Imprinting mold
By integrating a mask layer into the embossing mold, the problem of aligning the embossing mold and the mask is solved, improving the accuracy of pattern transfer and resistance to deformation, making it suitable for nanoimprinting technology.
Patent Information
- Application Number
- CN202420428985.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-06
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2034-03-06
AI Technical Summary
In existing nanoimprinting technology, the imprinting mold and mask need to be precisely aligned, and the alignment difficulty of the flexible mold increases when the temperature changes, which affects the accuracy of pattern transfer.
The mask is solidified and integrated into the embossing mold to form a non-transparent area that does not transmit UV light, eliminating the need for alignment and resisting deformation caused by temperature changes.
It eliminates the need for alignment during the printing process, improves the accuracy of pattern transfer, and overcomes the impact of temperature changes on pattern transfer.
Smart Images

Figure CN221946332U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of micro-machining, in particular to an imprinting mold integrated with a mask. Background Art
[0002] Nanoimprinting is a technology that transfers the pattern on the mold to other materials through contact imprinting. Compared with photolithography, nanoimprinting can overcome the resolution limit problem caused by the light diffraction phenomenon in optical exposure technology, showing ultra-high resolution and ultra-high efficiency. At the same time, the unique advantages of nanoimprinting, such as low cost and suitability for industrial production, have also made it widely favored in the field of 3D micro-pattern processing.
[0003] Figure 1 A schematic diagram of a conventional nanoimprinting process is shown. As an example, as shown in the figure, a columnar micro-pattern is engraved on one side of the mold surface as an imprinting pattern. When the imprinting pattern on the mold is to be transferred to a substrate, the mold can be pressed vertically on one side of the substrate coated with UV glue. By arranging a mask above the mold and irradiating it vertically with a UV lamp, the UV glue in the local area corresponding to the bright area of the mask (i.e., the light-colored square area in the mask) can be cured to form a microstructure as shown in the figure. At the same time, since UV light cannot penetrate the dark area of the mask (i.e., the black area as shown in the figure), the UV glue in the remaining areas corresponding to the dark area of the mask will not be cured, that is, no microstructure will be formed. Then, by removing the uncured UV glue using a chemical solvent, a substrate with a microstructure imprinted with a target pattern can be obtained.
[0004] In the conventional nanoimprint process as described above, the imprint mold and the mask are usually separated, which means that each time the imprint pattern is transferred to the substrate, the imprint mold and the mask need to be accurately aligned so that the desired pattern can be imprinted on the substrate. This requires a high-precision alignment device to align the imprint mold and the mask.
[0005] Furthermore, in some cases, the imprint mold may be a flexible mold based on materials such as PET, which is prone to expansion or contraction when the temperature changes, making high-precision alignment between the imprint mold and the mask more difficult. Utility Model Content
[0006] The utility model is made in view of the above problems. The utility model provides an imprint mold integrated with a mask. By solidifying and integrating the mask into the imprint mold, it is no longer necessary to align the imprint mold and the mask during the imprinting process, thereby being able to accurately transfer the pattern on the imprint mold to the substrate, and at the same time being able to effectively resist deformation problems caused by factors such as temperature changes.
[0007] The utility model provides an imprinting mold, which comprises: a transparent substrate; an array of micro-patterns arranged on a first surface of the transparent substrate; and a mask layer arranged in gaps between the micro-patterns on the first surface of the transparent substrate to form a non-light-transmitting area that does not transmit UV light.
[0008] In some embodiments, the mask layer is a metal layer.
[0009] In some embodiments, the masking layer is an ink layer.
[0010] In some embodiments, the transparent substrate is a rigid substrate made of quartz material.
[0011] In some embodiments, the transparent substrate is a flexible substrate made of a polymer material.
[0012] In some embodiments, each micropattern in the array of micropatterns includes a plurality of nanoscale microstructure units having a three-dimensional structure.
[0013] In some embodiments, each micropattern in the array of micropatterns includes a plurality of micrometer-scale microstructure units having a three-dimensional structure.
[0014] In some embodiments, each micropattern in the array of micropatterns includes a plurality of microstructure units having a rectangular, semicircular, or triangular cross-section. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 A schematic diagram showing the conventional nanoimprinting process.
[0016] Figure 2 A schematic diagram showing an example of an imprinting mold according to the present invention.
[0017] Figure 3 A schematic diagram showing an example of an imprinting mold according to the present invention is shown.
[0018] Figure 4 A schematic diagram showing an example of a method for manufacturing an imprinting mold according to the present invention.
[0019] Figure 5 A schematic diagram showing an example of a method for manufacturing an imprinting mold according to the present invention.
[0020] Figure 6 A schematic diagram showing an exemplary process of imprinting using the imprinting mold according to the present invention is shown. DETAILED DESCRIPTION
[0021] The embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although some embodiments of the present invention are shown in the accompanying drawings, it should be noted that the present invention can be implemented in various other forms and should not be construed as being limited to the embodiments described herein.
[0022] On the contrary, these embodiments are provided for a more thorough and complete understanding of the present invention. It should be noted that the drawings and embodiments of the present invention are only for illustrative purposes and are not intended to limit the scope of protection of the present invention.
[0023] It should be noted that the term "including" and its variations used in this document are open inclusions, that is, "including but not limited to". The term "based on" means "based at least in part on". The term "one embodiment" means "at least one embodiment"; the term "another embodiment" means "at least one other embodiment"; the term "some embodiments" means "at least some embodiments". The relevant definitions of other terms will be given in the following description.
[0024] It should also be noted that the concepts such as "first" and "second" mentioned in the present invention are only used to distinguish different devices, modules or units, and are not used to limit the order or interdependence of the functions performed by these devices, modules or units.
[0025] It should be noted that the modifications of "one" and "plurality" mentioned in the present invention are illustrative rather than restrictive, and those skilled in the art should understand that, unless otherwise clearly indicated in the context, it should be understood as "one or more".
[0026] The utility model provides an imprinting mold integrated with a mask. By solidifying and integrating the mask into the imprinting mold, it is no longer necessary to align the imprinting mold and the mask during the imprinting process, thereby accurately transferring the pattern on the imprinting mold to the substrate, and resisting deformation problems caused by factors such as temperature changes.
[0027] Figure 2 FIG. 1 is a schematic diagram showing an example of an imprinting mold 1000 according to the present invention. Figure 2 2 and 3 respectively show a cross-sectional view and a top view of the imprinting mold 1000 .
[0028] like Figure 2As shown in the cross-sectional view (a) in FIG. 1 , the imprint mold 1000 includes a transparent substrate 1100, an array of micropatterns 1110 arranged on a first surface (e.g., an upper surface as shown in the figure) of the transparent substrate 1100, and a mask layer 1200 arranged on the first surface of the transparent substrate 1100 and in the gaps between the micropatterns 1110. The area where the mask layer 1200 is located forms a non-light-transmitting area that does not transmit UV light, thereby preventing the UV glue in the non-light-transmitting area from being cured.
[0029] like Figure 2 As shown in the top view (b) in FIG. 1 , the array of micropatterns 1110 may be a 2×2 two-dimensional array of micropatterns 1110 , and each micropattern 1110 may include a plurality of microstructure units having a three-dimensional structure.
[0030] For example, Figure 2 Each of the micro patterns 1110 shown includes 3 rows and 4 columns, with a total of 12 micro structure units, and each micro structure unit is a protruding structure with a rectangular cross section.
[0031] It should be noted that the 2×2 two-dimensional array arrangement of the micropatterns 1110 described above is merely exemplary and not limiting. In other embodiments, the plurality of micropatterns 1110 may also form any form of one-dimensional array, annular array, etc.
[0032] In addition, as mentioned above Figure 2 The protrusion structure with a rectangular cross section is merely an exemplary embodiment of a microstructure unit in the micropattern 1110. In other embodiments, the microstructure unit in the micropattern 1110 may also be a three-dimensional structure with other cross-sectional shapes.
[0033] Figure 3 A schematic diagram of another example of an imprinting mold according to the utility model is shown. Figure 3 , examples of microstructure units having semicircular and triangular cross-sectional shapes are shown in (a) and (b), respectively.
[0034] For example, Figure 3 Each of the micro patterns 1110 shown in (a) may include a plurality (eg, 6) of columnar protrusions having a semicircular cross-section. Figure 3 Each of the micropatterns 1110 shown in (b) may include a plurality (eg, 5) of prism-shaped protrusions having a triangular cross-section.
[0035] Optionally, in other embodiments, Figure 3 The micro pattern 1110 shown in (a) may also be a two-dimensional (eg, 4×6) array composed of a plurality of hemispherical protrusions. Figure 3The micro pattern 1110 shown in (b) may also be a two-dimensional (eg, 3×5) array composed of a plurality of pyramidal (eg, triangular pyramids, quadrangular pyramids or circular pyramids) protrusions.
[0036] In other embodiments, the microstructure units in the micropattern 1110 may also have any other three-dimensional shapes, including but not limited to the above examples.
[0037] Typically, the microstructure units in the micropattern 1110 have the same material as the transparent substrate 1100 and are formed on the first surface of the transparent substrate 1100 by photolithography.
[0038] In some embodiments, the microstructure units in the micropattern 1110 may have a size of nanometer level, for example, between 2 nm and 9 nm. In other embodiments, the microstructure units in the micropattern 1110 may also have a size of micrometer level.
[0039] Back to Figure 2 There are gaps between the multiple micropatterns 1110 forming the array, and a mask layer formed of a light-shielding material is arranged in the gap (for example, shown by the black area), so that UV light can be blocked from passing through during the process of transferring the micropattern 1110 on the imprint mold 1000 to other substrates, so that the UV glue in the corresponding area is not cured, so that the uncured UV glue can be removed with a chemical solvent in the subsequent processing.
[0040] In some embodiments, the mask layer 1200 may be a metal layer, for example, a metal layer formed of nickel (Ni), chromium (Cr), etc. In other embodiments, the mask layer 1200 may also be an ink layer.
[0041] For ease of understanding, Figure 4 and Figure 5 Schematic diagrams of two examples of the method for manufacturing the imprinting mold according to the utility model are respectively shown.
[0042] like Figure 4 As shown, when a metal layer (eg, nickel, chromium) is used as a mask layer, a plurality of arrays of micro patterns 1110 may be firstly printed on a first surface of a transparent substrate 1100 using a photolithography technique, as shown in (a).
[0043] Then, a metal layer (as shown by the black lines in (b)) is disposed on the first surface of the transparent substrate 1100 by sputtering or deposition, so that the metal layer covers the plurality of micro patterns 1110 and the gaps therein.
[0044] Finally, the metal layer deposited on the surface of the micropattern 1110 can be removed by exposure and development techniques, and the metal layer in the gaps between the multiple micropatterns 1110 is retained as the mask layer 1200, thereby obtaining an imprint mold integrated with the mask layer 1200, as shown in (c).
[0045] like Figure 5 As shown, when an ink layer is used as a mask layer, the ink can be applied only in the gaps between the plurality of micro patterns 1110 by means of a screen printing technique with the aid of a template as shown in the figure, so as to serve as a mask layer 1200 .
[0046] In the various embodiments described above, the transparent substrate 1100 of the imprinting mold 1000 can be either a rigid substrate (for example, made of quartz material) or a flexible substrate (for example, made of polymer materials such as PET).
[0047] Figure 6 A schematic diagram showing an exemplary process of performing imprinting using the imprinting mold 1000 according to the present invention is shown.
[0048] like Figure 6 As shown, a UV glue layer 3000 of a certain thickness is coated on the substrate 2000. After the imprinting mold 1000 is vertically pressed onto the UV glue layer 3000 and cured using UV light, an imprinting pattern 3100 complementary to the micro pattern on the imprinting mold 1000 can be formed on the UV glue layer 3000. Since the mask layer is integrated in the imprinting mold 1000, the traditional alignment process is omitted during the imprinting process, and the mask layer integrated in the imprinting mold 1000 can prevent the UV glue in the non-light-transmitting area (i.e., the gap between the micro patterns) from being cured.
[0049] Note, for simplicity, Figure 6 The step of removing uncured UV glue with chemical solvents is omitted.
[0050] The specific structure of the imprinting mold of the utility model and various examples and embodiments of the manufacturing method thereof have been described above in conjunction with the accompanying drawings. It should be noted that the examples described above are only illustrations of some of the many specific examples and embodiments of the principles described herein. Obviously, those skilled in the art can easily design many other arrangements without departing from the scope as defined by the attached claims.
Claims
1. An imprinting mold, comprising: Transparent substrate; an array of micropatterns disposed on a first surface of the transparent substrate; as well as The mask layer is arranged in the gaps between the micro patterns on the first surface of the transparent substrate to form a non-light-transmitting area that does not transmit UV light.
2. The imprinting mold according to claim 1, characterized in that: The mask layer is a metal layer.
3. The imprinting mold according to claim 1, characterized in that: The mask layer is an ink layer.
4. The embossing mold according to any one of claims 1 to 3, characterized in that: The transparent substrate is a rigid substrate made of quartz material.
5. The embossing mold according to any one of claims 1 to 3, characterized in that: The transparent substrate is a flexible substrate made of polymer material.
6. The embossing mold according to any one of claims 1 to 3, characterized in that: Each micropattern in the array of micropatterns includes a plurality of nanoscale microstructure units having a three-dimensional structure.
7. The embossing mold according to any one of claims 1 to 3, characterized in that: Each micropattern in the array of micropatterns includes a plurality of micrometer-scale microstructure units having a three-dimensional structure.
8. The embossing mold according to any one of claims 1 to 3, characterized in that: Each micropattern in the array of micropatterns includes a plurality of microstructure units with a rectangular, semicircular, or triangular cross section.