Surface treatment device for lithium battery copper foil production

By designing the pressing and protection device of the surface treatment device for lithium battery copper foil production, the problem of insufficient contact between lithium battery copper foil and antioxidant liquid is solved, and more efficient antioxidant treatment and dust prevention effects are achieved, and the practicality of the production process is improved. and protective.

CN222064666UInactive Publication Date: 2024-11-26SHENZHEN JIAXINTONG ELECTRONICS CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420592553.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-26
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The lithium battery copper foil is not in sufficient contact with the antioxidant liquid during the production process, making it difficult to achieve antioxidant effect.

Method used

A surface treatment device for the production of lithium battery copper foil was designed, including a pressing device and a protective device. The pressing device presses the copper foil through components such as adjustment plates, connecting blocks, L-shaped frames and springs to ensure full contact with the antioxidant liquid; The guard device prevents dust from entering through a protective plate, a drive rod and a block.

Benefits of technology

The problem of insufficient contact between copper foil and antioxidant liquid is effectively avoided, the antioxidant effect is improved, and dust pollution is prevented through protective devices, which improves the practicality and protection of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222064666U_ABST
    Figure CN222064666U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of copper foil production, in particular to a surface treatment device for lithium battery copper foil production. The device comprises a processor, a liquid box is installed on the surface of the processor, a pressing device is arranged on one side of the liquid box, the pressing device comprises an adjusting plate, the adjusting plate is fixedly connected with one side of the liquid box, a sliding hole is formed in the surface of the adjusting plate, and a connecting block is slidably connected to the inner surface of the sliding hole of the adjusting plate. A sliding block is fixedly connected to one side of the connecting block, an L-shaped frame is fixedly connected to the side, away from the sliding block, of the connecting block, a pressing plate is fixedly connected to the lower surface of the L-shaped frame, a fixing rod is fixedly connected to the side, away from the connecting block, of the sliding block, and an operation plate is slidably connected to the arc surface of the fixing rod. The problem that when copper foil is subjected to anti-oxidation treatment through a liquid box, the copper foil makes insufficient contact with anti-oxidation liquid in the liquid box, and consequently the copper foil is difficult to achieve the anti-oxidation effect is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of copper foil production, in particular to a surface treatment device for lithium battery copper foil production. Background Art

[0002] Lithium battery copper foil, as the negative electrode current collector of lithium batteries, accounts for 5%-8% of the cost of lithium batteries and is an important lithium battery material. Lithium battery copper foil needs to be treated with anti-oxidation during the production process.

[0003] The inventors believe that the following defects often exist: lithium battery copper foil needs to be treated with anti-oxidation during the production process. When the copper foil passes through a liquid tank for anti-oxidation treatment, the copper foil is not in sufficient contact with the antioxidant liquid in the liquid tank, which makes it difficult for the copper foil to achieve the antioxidant effect. Therefore, a surface treatment device for lithium battery copper foil production is proposed to address the above problems. Utility Model Content

[0004] The utility model aims to solve the problem in the prior art that the copper foil is not in sufficient contact with the antioxidant liquid in the liquid box, which makes it difficult for the copper foil to achieve the antioxidant effect, and proposes a surface treatment device for lithium battery copper foil production.

[0005] In order to achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a surface treatment device for lithium battery copper foil production, comprising a processing machine, a liquid box is installed on the surface of the processing machine, a pressing device is provided on one side of the liquid box, the pressing device comprises an adjustment plate, the adjustment plate is fixedly connected to one side of the liquid box, a sliding hole is opened on the surface of the adjustment plate, a connecting block is slidably connected to the inner surface of the sliding hole of the adjustment plate, a sliding block is fixedly connected to one side of the connecting block, an L-shaped frame is fixedly connected to the side of the connecting block away from the sliding block, and the pressing plate is fixedly connected to the lower surface of the L-shaped frame.

[0006] The effect achieved by the above-mentioned components is: by setting up a pressing device, the effect of pressing the copper foil that is undergoing antioxidant treatment through a liquid box is achieved, thereby avoiding the situation where the copper foil is not in sufficient contact with the antioxidant liquid in the liquid box when the copper foil is undergoing antioxidant treatment through the liquid box, resulting in the copper foil being difficult to achieve the antioxidant effect, thereby improving the practicability of the device.

[0007] Preferably, the sliding block is fixedly connected to a fixing rod on one side away from the connecting block, an operating plate is slidably connected to the arc surface of the fixing rod, an insert rod is fixedly connected to the side of the operating plate close to the sliding block, and a plurality of slots are provided on the surface of the adjustment plate.

[0008] The effect achieved by the above components is: the effect of adjusting the height of the pressing plate is achieved, avoiding the situation where after the antioxidant liquid in the liquid tank is reduced, the height of the pressing plate is difficult to press the copper foil completely into the antioxidant liquid at the current height, thereby resulting in insufficient contact between the copper foil and the antioxidant liquid in the liquid tank.

[0009] Preferably, one end of the fixing rod away from the adjustment plate is fixedly connected to a limiting plate, and the size of the insertion rod is adapted to the size of the adjustment plate slot.

[0010] The effect achieved by the above components is: the limit plate limits the maximum sliding distance of the operating plate on the fixed rod, thereby preventing the operating plate from detaching from the arc surface of the fixed rod due to excessive pulling force when the staff pulls the operating plate.

[0011] Preferably, the arc surface of the fixing rod is sleeved with a first spring, and two ends of the first spring are fixedly connected to the operating plate and the sliding block respectively.

[0012] The effects achieved by the above components are as follows: the first spring improves the stability of the insertion rod when limiting the sliding block, thereby improving the stability of the insertion rod when limiting the pressing plate.

[0013] Preferably, a protective device is provided on the surface of the processing machine, and the protective device includes a fixed plate, which is fixedly connected to the surface of the processing machine, a protective plate is slidably inserted in the fixed plate, a support plate is fixedly connected to the surface of the fixed plate, a driving rod is threadedly inserted in the support plate, one end of the driving rod is rotatably connected to a connecting block, and a connecting hole is opened on the surface of the protective plate.

[0014] The effect achieved by the above components is: by setting up a protective device, the idle liquid tank is dust-proofed, which avoids the situation where the liquid tank is idle when the processor is not processing copper foil, causing dust to enter the liquid tank, thereby affecting the effect of the antioxidant liquid in the liquid tank, thereby improving the protectiveness of the device.

[0015] Preferably, a positioning rod is fixedly connected to one side of the connection block close to the driving rod, and the arc surface of the positioning rod is slidably connected to the support plate.

[0016] The effect achieved by the above components is that the positioning rod achieves the effect of limiting the connection block from rotating following the driving rod, so as to reduce the operating steps of the device for the staff and improve the work efficiency of the staff.

[0017] Preferably, a blocking block is fixedly connected to the surface of the protective plate, and the size of the protective plate is adapted to the size of the liquid tank.

[0018] The effect achieved by the above components is that the blocking block achieves the effect of limiting the protection plate from being separated from the fixing plate.

[0019] In summary, the beneficial effects of the utility model are:

[0020] 1. In the utility model, by providing a pressing device, the effect of pressing the copper foil that is subjected to antioxidant treatment through a liquid box is achieved, thereby avoiding the situation in which the copper foil is unable to achieve the antioxidant effect due to insufficient contact between the copper foil and the antioxidant liquid in the liquid box when the copper foil is subjected to antioxidant treatment through the liquid box, thereby improving the practicability of the device.

[0021] 2. In the utility model, by setting a protective device, the effect of dust prevention is achieved for the idle liquid box, which avoids the situation where the liquid box is idle when the processor is not processing copper foil, causing dust to enter the liquid box, thereby affecting the effect of the antioxidant liquid in the liquid box, thereby improving the protectiveness of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a three-dimensional structural schematic diagram of the utility model;

[0023] Figure 2 It is a structural schematic diagram of the pressing device in the utility model;

[0024] Figure 3 For the utility model Figure 2 A magnified image of point A;

[0025] Figure 4 It is a structural schematic diagram of the protective device in the utility model;

[0026] Figure 5 For the utility model Figure 4 Enlarged view of point B.

[0027] Legend: 1. Processor; 2. Liquid tank; 3. Pressing device; 4. Protective device; 301. Adjusting plate; 302. Connecting block; 303. Sliding block; 304. L-shaped frame; 305. Pressing plate; 306. Fixing rod; 307. Operating panel; 308. Inserting rod; 309. Limiting plate; 310. First spring; 41. Fixing plate; 42. Protective plate; 43. Support plate; 44. Driving rod; 45. Connecting block; 46. Positioning rod; 47. Stopping block. DETAILED DESCRIPTION

[0028] Reference Figure 1As shown, the utility model provides a technical solution: a surface treatment device for lithium battery copper foil production, comprising a processor 1, a liquid tank 2 is installed on the surface of the processor 1, and a pressing device 3 is provided on one side of the liquid tank 2. By setting the pressing device 3, the copper foil that passes through the liquid tank 2 for antioxidant treatment is pressed, thereby avoiding the situation that when the copper foil passes through the liquid tank 2 for antioxidant treatment, the copper foil is not in sufficient contact with the antioxidant liquid in the liquid tank 2, resulting in the copper foil having difficulty in achieving the antioxidant effect, thereby improving the practicability of the device. A protective device 4 is provided on the surface of the processor 1. By setting the protective device 4, the effect of dust prevention is achieved for the idle liquid tank 2, thereby avoiding the situation that when the processor 1 does not process the copper foil, the liquid tank 2 is idle, resulting in dust entering the liquid tank 2, thereby affecting the effect of the antioxidant liquid in the liquid tank 2, thereby improving the protectiveness of the device.

[0029] The specific configuration and functions of the pressing device 3 and the protective device 4 are described in detail below.

[0030] Reference Figure 2 and Figure 3As shown, in this embodiment: the pressing device 3 includes an adjusting plate 301, the adjusting plate 301 is fixedly connected to one side of the liquid tank 2, a sliding hole is opened on the surface of the adjusting plate 301, and the inner surface of the sliding hole of the adjusting plate 301 is slidably connected to a connecting block 302, one side of the connecting block 302 is fixedly connected to a sliding block 303, a side of the connecting block 302 away from the sliding block 303 is fixedly connected to an L-shaped frame 304, a lower surface of the L-shaped frame 304 is fixedly connected to a pressing plate 305, a side of the sliding block 303 away from the connecting block 302 is fixedly connected to a fixing rod 306, an arc surface of the fixing rod 306 is slidably connected to an operating plate 307, a side of the operating plate 307 close to the sliding block 303 is fixedly connected to an insertion rod 308, and the surface of the adjusting plate 301 Several slots are provided. When the staff needs to adjust the pressing height of the pressing plate 305, the operating plate 307 is pulled to make the operating plate 307 slide on the arc surface of the fixing rod 306. At the same time, the operating plate 307 drives the insertion rod 308 to move until the insertion rod 308 is disengaged from the slot of the adjustment plate 301. At this time, the sliding block 303 is pulled, and the sliding block 303 drives the connecting block 302 to slide in the sliding hole of the adjustment plate 301. At the same time, the connecting block 302 drives the L-shaped frame 304 to move, and the L-shaped frame 304 drives the pressing plate 305 to move until the pressing plate 305 is adjusted to a suitable position. At this time, the operating plate 307 is pushed to make the operating plate 307 slide on the arc surface of the fixing rod 306. At the same time, the operating plate 307 drives the insertion rod 308 to move , until the insertion rod 308 is inserted into the slot of the adjustment plate 301, at this time, the effect of adjusting the height of the pressing plate 305 is achieved, and it is avoided that after the antioxidant liquid in the liquid box 2 is reduced, the height of the pressing plate 305 is difficult to fully press the copper foil into the antioxidant liquid at the current height, thereby causing the copper foil to be insufficiently in contact with the antioxidant liquid in the liquid box 2. The end of the fixing rod 306 away from the adjustment plate 301 is fixedly connected to the limiting plate 309, and the size of the insertion rod 308 is adapted to the size of the slot of the adjustment plate 301. When the staff pulls the operating plate 307, the operating plate 307 slides on the arc surface of the fixing rod 306. At this time, the limiting plate 309 achieves the effect of limiting the maximum sliding distance of the operating plate 307 on the fixing rod 306, avoiding When the staff pulls the operating plate 307, the pulling force is too great, causing the operating plate 307 to detach from the arc surface of the fixed rod 306. The arc surface of the fixed rod 306 is sleeved with a first spring 310, and the two ends of the first spring 310 are respectively fixedly connected to the operating plate 307 and the sliding block 303. When the staff releases the operating plate 307, the rebound force of the first spring 310 drives the operating plate 307 to slide on the arc surface of the fixed rod 306. At the same time, the operating plate 307 drives the insertion rod 308 to move until the insertion rod 308 is inserted into the slot of the adjustment plate 301. At this time, the first spring 310 improves the stability of the insertion rod 308 when limiting the sliding block 303, thereby improving the stability of the insertion rod 308 when limiting the pressing plate 305.

[0031] Reference Figure 4 and Figure 5 As shown, specifically, the protective device 4 includes a fixed plate 41, which is fixedly connected to the surface of the processing machine 1, and a protective plate 42 is slidably inserted in the fixed plate 41. A support plate 43 is fixedly connected to the surface of the fixed plate 41, and a driving rod 44 is inserted into the inner thread of the support plate 43. One end of the driving rod 44 is rotatably connected to a connecting block 45, and a connecting hole is provided on the surface of the protective plate 42. A positioning rod 46 is fixedly connected to the side of the connecting block 45 close to the driving rod 44. The arc surface of the positioning rod 46 is slidably connected to the support plate 43. When the staff rotates the driving rod 44, the driving rod 44 moves in the inner thread of the support plate 43, and at the same time, the driving rod 44 drives the connecting block 45 to move, and the connecting block 45 drives the positioning rod 46 to slide in the support plate 43. At this time, the positioning rod 46 achieves the effect of limiting the connecting block 45 from rotating with the driving rod 44 In order to reduce the operating steps of the device for the staff and improve the work efficiency of the staff, a blocking block 47 is fixedly connected to the surface of the protective plate 42. The size of the protective plate 42 is adapted to the size of the liquid tank 2. When the staff needs to release the protection of the protective plate 42 on the liquid tank 2, the driving rod 44 is rotated, and the driving rod 44 rotates in the inner thread of the support plate 43. At the same time, the driving rod 44 drives the connecting block 45 to move, and the connecting block 45 drives the positioning rod 46 to slide in the support plate 43 until the connecting block 45 is disengaged from the connecting hole of the protective plate 42. At this time, the protective plate 42 is pulled to make the protective plate 42 slide in the fixed plate 41. At the same time, the protective plate 42 slides on the surface of the liquid tank 2, and the protective plate 42 drives the blocking block 47 to move. At this time, the blocking block 47 achieves the effect of limiting the separation of the protective plate 42 from the fixed plate 41.

[0032] Working principle: when the staff needs to press the copper foil that has been subjected to the antioxidant treatment through the liquid box 2, the operating plate 307 is pulled to make the operating plate 307 slide on the arc surface of the fixed rod 306, and the first spring 310 is stretched. At the same time, the operating plate 307 drives the insertion rod 308 to move until the insertion rod 308 is disengaged from the slot of the adjustment plate 301. At this time, the sliding block 303 is pulled, and the sliding block 303 drives the connecting block 302 to slide in the sliding hole of the adjustment plate 301. At the same time, the connecting block 302 drives the L-shaped frame 304 to move, and the L-shaped frame 304 drives the pressing plate 305 to move until the pressing plate 305 is pressed. The pressure plate 305 is adjusted to a suitable position, and the operating plate 307 is released at this time. The resilience of the first spring 310 drives the operating plate 307 to slide on the arc surface of the fixed rod 306. At the same time, the operating plate 307 drives the insertion rod 308 to move until the insertion rod 308 is inserted into the slot of the adjustment plate 301. At this time, the copper foil that has been subjected to antioxidant treatment through the liquid tank 2 is pressed, thereby avoiding the situation in which the copper foil is insufficiently in contact with the antioxidant liquid in the liquid tank 2 when the copper foil is subjected to antioxidant treatment through the liquid tank 2, resulting in the copper foil having difficulty in achieving the antioxidant effect, thereby improving the practicability of the device.

[0033] When the staff needs to prevent dust from the idle liquid tank 2, they push the protective plate 42 to make the protective plate 42 slide in the fixed plate 41, and at the same time, the protective plate 42 slides on the surface of the liquid tank 2 until the protective plate 42 completely covers the liquid tank 2. At this time, the driving rod 44 is rotated to make the driving rod 44 rotate in the thread of the support plate 43. At the same time, the driving rod 44 drives the connecting block 45 to move, and the connecting block 45 drives the positioning rod 46 to slide in the support plate 43 until the connecting block 45 is inserted into the connecting hole of the protective plate 42. At this time, the effect of preventing dust from the idle liquid tank 2 is achieved, and the liquid tank 2 is prevented from being idle when the processing machine 1 is not processing copper foil, resulting in dust entering the liquid tank 2, thereby affecting the effect of the antioxidant liquid in the liquid tank 2, thereby improving the protection of the device.

[0034] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.

Claims

1. A surface treatment device for lithium battery copper foil production, comprising a treatment machine (1), characterized in that: A liquid box (2) is installed on the surface of the processing machine (1); a pressing device (3) is provided on one side of the liquid box (2); the pressing device (3) comprises an adjusting plate (301); the adjusting plate (301) is fixedly connected to one side of the liquid box (2); a sliding hole is provided on the surface of the adjusting plate (301); a connecting block (302) is slidably connected to the inner surface of the sliding hole of the adjusting plate (301); a sliding block (303) is fixedly connected to one side of the connecting block (302); an L-shaped frame (304) is fixedly connected to the side of the connecting block (302) away from the sliding block (303); and a pressing plate (305) is fixedly connected to the lower surface of the L-shaped frame (304).

2. A surface treatment device for lithium battery copper foil production according to claim 1, characterized in that: A fixed rod (306) is fixedly connected to the side of the sliding block (303) away from the connecting block (302); an operating plate (307) is slidably connected to the arc surface of the fixed rod (306); an inserting rod (308) is fixedly connected to the side of the operating plate (307) close to the sliding block (303); and a plurality of slots are provided on the surface of the adjusting plate (301).

3. A surface treatment device for lithium battery copper foil production according to claim 2, characterized in that: One end of the fixing rod (306) away from the adjusting plate (301) is fixedly connected to the limiting plate (309), and the size of the inserting rod (308) is adapted to the size of the slot of the adjusting plate (301).

4. A surface treatment device for lithium battery copper foil production according to claim 2, characterized in that: The arc surface of the fixed rod (306) is sleeved with a first spring (310), and the two ends of the first spring (310) are respectively fixedly connected to the operating plate (307) and the sliding block (303).

5. The surface treatment device for lithium battery copper foil production according to claim 1, characterized in that: The surface of the processing machine (1) is provided with a protective device (4), and the protective device (4) comprises a fixed plate (41), the fixed plate (41) is fixedly connected to the surface of the processing machine (1), a protective plate (42) is slidably inserted in the fixed plate (41), a support plate (43) is fixedly connected to the surface of the fixed plate (41), a driving rod (44) is inserted into the internal thread of the support plate (43), one end of the driving rod (44) is rotatably connected to a connecting block (45), and a connecting hole is opened on the surface of the protective plate (42).

6. A surface treatment device for lithium battery copper foil production according to claim 5, characterized in that: A positioning rod (46) is fixedly connected to one side of the connection block (45) close to the driving rod (44), and the arc surface of the positioning rod (46) is slidably connected to the support plate (43).

7. A surface treatment device for lithium battery copper foil production according to claim 5, characterized in that: A blocking block (47) is fixedly connected to the surface of the protection plate (42), and the size of the protection plate (42) is adapted to the size of the liquid tank (2).

Citation Information

Cited By

  • Electrolytic copper foil anti-oxidation liquid insect prevention device and method

    CN119972654A