GaN HEMT device with high packaging power density
By forming an isolation region and a multi-layer isolation layer structure on the GaN HEMT device, the device flow capacity and packaging power density are improved without affecting the gate control capability, and the problem of low packaging power density in the prior art is solved.
Patent Information
- Application Number
- CN202323249174.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-30
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2033-11-30
AI Technical Summary
Existing GaN HEMT devices have low package power density under high power conditions, and methods to increase package power density such as increasing device length or closing devices can affect gate control capabilities or introduce parasitic inductances and resistors.
By forming n active regions on the GaN HEMT device, each active region is isolated from each other, the gate width of each active region is controlled to be 1 mm, and G, D, of each active region is controlled by interconnecting metals in the device. The S electrode is interconnected with the G, D, and S electrodes of the device, and adopts ISO isolation zones and multi-layer isolation layer structures to improve the device's flow capacity and packaging power density.
Without affecting the device gate control capability, the flow capacity and large-size package power density of a single device are improved, parasitic inductance and resistance are reduced, and the overall performance of the device is improved.
Smart Images

Figure CN222126534U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductors, in particular to a GaN HEMT device with high packaging power density. Background Art
[0002] In the field of power electronic device technology, third-generation semiconductors represented by GaN and SiC are increasingly valued. Among them, GaN has the advantages of large bandgap width, critical breakdown field strength and high electron mobility, and has great application potential in power device markets such as fast charging, data centers, OBCs, and solar inverters.
[0003] Currently, the main application form of GaN in power devices is GaN HEMT devices. Since Khan et al. produced the first AlGaN / GaN high electron mobility transistor (HEMT) in 1993, horizontally structured GaN HEMT devices have attracted widespread attention for their superior electrical performance and lower energy consumption than Si devices.
[0004] GaN HEMT devices have better performance than traditional Si devices, especially enhanced GaN HEMT devices, which are more popular in the market due to their wide range of applications. Traditional enhanced GaN HEMT devices generally have a gate width of 1mm, a pad area width of 250um, and a device width of about 1.5mm. The device generally adopts a common source and common drain interdigital structure. The current capacity of each pair of interdigital structures is determined. Increasing the current capacity of the device is generally achieved by increasing the length of the device and then increasing the number of interdigital structures of the device.
[0005] As GaN HEMT devices become more powerful, their current carrying capacity and length increase. To match the length of the devices, the device package size also increases. Currently, the mainstream packages are DFN5*6 and DFN8*8, but the width of GaN HEMT devices is still 1.5mm, which results in a large portion of space inside the DFN5*6 and DFN8*8 packages not being utilized, resulting in low device package power density. Currently, there are two main ways to improve the power density of DFN5*6 and DFN8*8 packages on the market, namely:
[0006] 1. Increasing the device gate width from 1mm to a size that matches the package width, but this will cause the gate control capability to weaken;
[0007] 2. Multiple GaN HEMT devices are sealed together, but this will cause larger parasitic inductance and parasitic resistance.
[0008] Therefore, how to improve the power density of large-size packages without affecting the electrical performance of GaN HEMT devices is an urgent problem that needs to be solved when GaN HEMT devices are used under high-power conditions. Utility Model Content
[0009] In view of the above problems, the utility model provides a GaN HEMT device with high package power density which improves the package power density.
[0010] The technical solution of the utility model is:
[0011] High package power density GaN HEMT devices, including:
[0012] Epitaxial wafer, an ISO isolation region is provided between the passive region and the n active regions;
[0013] A first isolation layer is deposited on the P-GaN layer of the epitaxial wafer; an S electrode and a D electrode are provided in the active region and extend downward from the top surface of the first isolation layer to the inside of the AlGaN barrier layer; and a D and S electrode pad metal interconnected with the S electrode and the D electrode is provided outside the active region;
[0014] A second isolation layer is deposited on the top surface of the first isolation layer, the S electrode and the D electrode; a G electrode is provided in the active area, extending downward from the top surface of the second isolation layer to the top surface of the P-GaN layer; a G electrode pad metal interconnected with the G electrode is provided outside the active area;
[0015] A third isolation layer is deposited on the top surface of the second isolation layer.
[0016] Specifically, the epitaxial wafer is a Si-based epitaxial wafer, a SiC-based epitaxial wafer or a GaN-based substrate epitaxial wafer.
[0017] Specifically, the epitaxial wafer includes a substrate, an AlN spacer layer, an Al composition gradient buffer AlGaN layer, a C-doped high-resistance GaN layer, a GaN channel layer, an AlN insertion layer, an AlGaN barrier layer and a P-GaN layer which are sequentially connected from bottom to top.
[0018] Specifically, the upper surface of the G electrode and the upper surface of the second isolation layer are in the same plane, and form a Schottky contact with the P-GaN layer.
[0019] Specifically, the top surface of the D electrode, the top surface of the S electrode and the top surface of the first isolation layer are in the same plane, and form an ohmic contact with the two-dimensional electron gas in the channel below.
[0020] Specifically, the top surface of the P-GaN layer is lower than the bottom surface of the first isolation layer above it.
[0021] The method for preparing a GaN HEMT device with high packaging power density proposed in the utility model has the following advantages:
[0022] n active areas are formed on the GaN HEMT device, each active area is isolated from each other, the gate width in each active area is controlled to be 1mm, and the G, D, and S electrodes of each active area are interconnected with the G, D, and S electrode Pads of the device through the interconnection metal in the device. This solution can improve the current carrying capacity of a single device and increase the power density of the device in large-size packaging without affecting the gate control capability of the device and without introducing additional parasitic inductance and parasitic resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a process flow chart of the utility model.
[0024] Figure 2 is a schematic diagram of the device surface structure in step S100,
[0025] Figure 3 is a schematic diagram of the cross-sectional structure after the P-GaN layer is etched in step S200,
[0026] Figure 4 is a schematic diagram of the cross-sectional structure after the first isolation layer is deposited in step S200,
[0027] Figure 5 is a schematic diagram of the cross-sectional structure of the D and S electrode grooves after preparation in step S300,
[0028] Figure 6 It is a schematic diagram of the cross-sectional structure of the S electrode and the D electrode.
[0029] Figure 7 This is a schematic diagram of the surface structure of the S electrode pad metal and the D electrode pad metal.
[0030] Figure 8 It is a schematic diagram of the surface structure in which the S electrode and the D electrode are interconnected with the S electrode pad metal and the D electrode pad metal respectively.
[0031] Fig. 9 is a schematic diagram of the cross-sectional structure after the second isolation layer is deposited.
[0032] Fig.10 This is a schematic diagram of the cross-sectional structure of the G electrode groove after preparation.
[0033] Fig.11 This is a schematic diagram of the cross-sectional structure of the G electrode after preparation in the G electrode groove.
[0034] Fig.12 This is a schematic diagram of the surface structure of the G electrode pad metal.
[0035] Fig.13 This is a schematic diagram of the surface structure of the metal interconnection between the G electrode and the G electrode pad.
[0036] Fig.14 is a schematic diagram of the cross-sectional structure after the third isolation layer is deposited.
[0037] Fig.15 This is a schematic diagram of the surface structure after the S electrode pad metal, D electrode pad metal, and G electrode pad metal windows are opened.
[0038] Fig.16 It is a schematic diagram of the length (L) and width (W) of the device of the utility model with two active regions,
[0039] Fig.17 This is a schematic diagram of the length (L) and width (W) of a traditional structure gate width 1mm device.
[0040] Fig.18 This is a schematic diagram of the length (L) and width (W) of a 2mm gate width device that matches the package width.
[0041] Fig.19 This is a schematic diagram of the length (L) and width (W) of two conventional structure 1mm gate width devices after sealing;
[0042] In the figure, 1 is a substrate, 2 is an AlN spacer layer, 3 is an Al composition gradient buffer AlGaN layer, 4 is a C-doped high-resistance GaN layer, 5 is a GaN channel layer, 6 is an AlN insertion layer, 7 is an AlGaN barrier layer, 8 is a P-GaN layer, 9 is an ISO isolation region, 10 is a schematic diagram of an active region, 11 is a first isolation layer, 12 is an S electrode groove, 13 is a D electrode groove, 14 is an S electrode, 15 is a D electrode, 16 is an S electrode and an S electrode pad metal interconnection metal, 17 is a D electrode and a D electrode pad metal interconnection metal, 18 is an S electrode pad metal, 19 is a D electrode pad metal, 20 is a second isolation layer, 21 is a G electrode groove, 22 is a G electrode, 23 is a G electrode and a G electrode pad metal interconnection metal, 24 is a G electrode pad metal, and 25 is a third isolation layer. DETAILED DESCRIPTION
[0043] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0044] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0045] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0046] The present invention is described below with reference to Figures 1-19;
[0047] A GaN HEMT device with high package power density and a method for preparing the same include the following steps:
[0048] Step S100, ion implantation is performed between the passive region and the n active regions 10 on the epitaxial wafer to form an ISO isolation region 9, referring to Figure 2 As shown;
[0049] Step S110, using a photoresist to protect the active area 10 of the epitaxial wafer through a photolithography process (cleaning, coating, photolithography, development, etc.);
[0050] Step S120, high-energy ion implantation is performed on the area outside the active region 10 to destroy the internal lattice structure of the GaN channel layer 5, the AlN insertion layer 6 and the AlGaN barrier layer 7 in the epitaxial wafer outside the active region 10, so that the GaN channel layer 5, the AlN insertion layer 6 and the AlGaN barrier layer 7 become high-resistance state, play a role in electrical isolation, and form the ISO isolation region 9;
[0051] Accordingly, light ions such as H and F can be used to implant the epitaxial wafer outside the active region 10 to perform an ISO isolation process. The length L1 of the active region 10 ( Figure 2 The width W1 of the active region 10 (shown in the x-axis direction) depends on the number of common-source and common-drain interdigitation structures. Figure 2The number n of active regions 10 depends on the design width of the device. The width of the isolation region satisfies the electrical isolation function of the active region 10 and the wiring and electrical isolation requirements of the D and S electrode interconnection metals 17 and 16. The width range is set to 1-1000um.
[0052] In this case, Si-based epitaxial wafers were used and high-energy ion F was implanted. The implantation angle was 7 degrees and the implantation was divided into three times. The energy and dose of the three implantations were 140 KeV and 1.2e respectively. 14 cm -3 , 80 KeV and 0.6e 14 cm -3 , 40 KeV and 0.4e 14 cm -3 The length L1 of the active area 10 is set to 0.5 mm, including 8 common source and common drain finger structures, the width W1 of the active area 10 is set to 1 mm, the corresponding gate width of the active area 10 is 1 mm, the number of active areas n=2, and the width of the ISO isolation area between the two active areas is 100 um, ensuring that the electrical isolation of the active area 10 is met and the wiring and electrical isolation requirements of the D and S electrode interconnection metals 17 and 16 are met. Figure 2 A schematic diagram of the surface of the device after ISO isolation 9 is performed between the passive area and the active area 10 is shown, wherein y1-y2 is the range of an interdigitated structure of the device, and x1 and x2 are the cross-sectional positions of the device along the x-axis in the two active areas, respectively.
[0053] Step S200, refer to Figure 3 , 4 As shown, the P-GaN layer 8 on the epitaxial wafer outside the G electrode region is removed, and a first isolation layer 11 is deposited;
[0054] Step S210, using a photolithography process (including epitaxial wafer cleaning, gluing, photolithography, and development) to protect the G electrode region of the device with photoresist, and using ICP dry etching to etch the P-GaN layer 8 in the region outside the G electrode region that is not protected by the photoresist, and then cleaning off the photoresist;
[0055] Step S220, depositing a first isolation layer 11;
[0056] Accordingly, the etching depth is equal to the thickness of the P-GaN layer 8. The first isolation layer 11 mainly plays a protective role. The thickness satisfies the condition that the first isolation layer 11 exerts little additional stress on the epitaxial wafer. The thickness range is set to 10-10000nm.
[0057] In this case, the width of the G electrode region is set to 2um, and Cl2 is used for ICP dry etching. The etching rate is 10nm / min to ensure the accuracy of etching. The thickness of the P-GaN layer 8 is 80nm, so the etching time is 8min and the etching depth is 80nm. Si3N4 is used as the first isolation layer 11 for isolation and protection, and the thickness is 100nm;
[0058] Figure 3 It shows that after removing the P-GaN layer 8 outside the G electrode area, the device Figure 2 Schematic diagram of the cross sections x1 and x2 in the y1-y2 region shown; Figure 4 It shows that after the first isolation layer 11 is deposited, the device Figure 2 Schematic diagram of the cross sections x1 and x2 in the y1-y2 region shown.
[0059] Step S300, in each active area 10 on the epitaxial wafer, a D electrode groove 13 is prepared in the D electrode area, and an S electrode groove 12 is prepared in the S electrode area, referring to Figure 5 As shown;
[0060] Step S310, using a photolithography process (including epitaxial wafer cleaning, glue coating, photolithography, and development) to protect the areas outside the D and S electrode regions with a photoresist;
[0061] Step S320, etching the D and S electrode regions by using ICP dry etching to form D electrode grooves 13 and S electrode grooves 12 in each active region 10, and then cleaning off the photoresist;
[0062] Accordingly, the etching depth is greater than the thickness of the first isolation layer 11 and less than the sum of the thicknesses of the first isolation layer 11 and the AlGaN barrier layer 7. The widths of the D and S electrode grooves 13 and 12 ( Figure 5 The width of the D and S electrode regions is consistent with that of the X-axis.
[0063] In this case, the width of the D and S electrode regions is 5um. CF4 is used for ICP dry etching. The etching rate is 10nm / min to ensure the accuracy of etching. The thickness of the Si3N4 layer 10 is 100nm, and the thickness of the AlGaN barrier layer 7 is 20nm. Therefore, the selected etching time is 11min and the etching depth is 110nm. Figure 5 It shows that after preparing the D and S electrode grooves 13 and 12 in each active area 10, the device Figure 2 Schematic diagram of the cross sections x1 and x2 in the y1-y2 region shown.
[0064] Step S400, prepare a D electrode 15 in the D electrode groove 13, prepare an S electrode 14 in the S electrode groove 12, prepare D and S electrode pad metals 19 and 18 interconnected with the D and S electrodes 15 and 14 outside the active area 10, and deposit a second isolation layer 20, refer to Figure 6 , 7 , 8, 9;
[0065] S410, optionally, a metal stripping process can be used to protect the D and S electrode grooves 13 and 12 regions in each active area 10 and the D and S electrode pad metal 19 and 18 regions outside the active area and the interconnection metal 17 and 16 regions by using photoresist through epitaxial wafer cleaning, glue coating, photolithography, and development. The D and S electrode grooves 13 and 12 regions in each active area 10 and the D and S electrode pad metal 19 and 18 regions outside the active area and the interconnection metal 17 and 16 regions are deposited with an ohmic contact metal of a corresponding thickness. The D electrode 15 and S electrode 14 are prepared in each active area 10, and the D and S electrode pad metal 19 and 18 interconnected with the D and S electrodes 15 and 14 are prepared outside the active area 10. Then, the photoresist is cleaned off, and a second isolation layer 20 is deposited.
[0066] S420, optionally, a metal etching process can be used to first deposit an ohmic contact metal of a corresponding thickness, and then the D and S electrode grooves 13 and 12 regions in each active area 10 and the D and S electrode pad metal 19 and 18 regions and the interconnection metal 17 and 16 regions outside the active area are protected by photoresist, and then the D and S electrode grooves 13 and 12 regions in each active area 10 and the D and S electrode pad metal 19 and 18 regions and the interconnection metal 17 and 16 regions outside the active area are protected by ICP dry etching. 6. The metal outside the region is etched away, and the etching depth is not less than the corresponding thickness of the deposited ohmic contact metal, ensuring that the D and S electrode grooves 13 and 12 regions in each active region 10 and the D and S electrode pad metal 19 and 18 regions outside the active region and the metal outside the interconnection metal 17 and 16 regions are completely etched, and D electrodes 15 and S electrodes 14 are prepared in each active region 10, and D and S electrode pad metals 19 and 18 interconnected with the D and S electrodes 15 and 14 are prepared outside the active region 10, and then the photoresist is cleaned off, and a second isolation layer 20 is deposited;
[0067] Correspondingly, the D electrode 15, the S electrode 14 in each active area 10 form a good ohmic contact with the two-dimensional electron gas below, the upper surfaces of the D electrodes 15 and the S electrodes 14 are level with the upper surface of the first isolation layer 11, the width of the S electrode and the S electrode pad metal interconnection metal 16 and the D electrode and the D electrode pad metal interconnection metal 17 meet the requirements of electrical conduction, and the width range is set to 1-100um, the distance between the two meets the requirements of electrical isolation, and the distance range is set to 1-100um, the width of the D and S electrode pad metals 19 and 18 meets the requirements of WB wiring, and the width range is set to 50-1000um, the second isolation layer 20 mainly plays a protective role, and the thickness meets the condition that the second isolation layer 20 has little additional stress on the epitaxial wafer, and the thickness range is set to 10-10000nm.
[0068] In this case, a metal lift-off process is used to protect the D and S electrode grooves 13 and 12 in each active area 10, the D and S electrode pad metal 19 and 18 areas outside the active area, and the interconnection metal 17 and 16 areas. 10nmTi+100nmAl are deposited as ohmic contact metal in the D and S electrode grooves 13 and 12 areas in each active area 10, the D and S electrode pad metal 19 and 18 areas outside the active area, and the interconnection metal 17 and 16 areas. D electrodes 15 and S electrodes 14 are prepared in each active area 10, and D and S electrode pad metals 19 and 18 interconnected with the D and S electrodes 15 and 14 are prepared outside the active area 10. Then, the photoresist is washed off, and high-temperature annealing is performed at 850°C for 30s to connect the D and S electrode ohmic contact metals with the two-dimensional electron gas below to form a good Ohmic contact, at this time, the upper surface of the D electrode 15 and the S electrode 14 in each active area 10 is level with the upper surface of the isolation layer 11, the width of the S electrode and the S electrode pad metal interconnection metal 16 and the D electrode and the D electrode pad metal interconnection metal 17 is set to 20um, which meets the electrical conduction requirements of the device, and the distance between the two is set to 40um. The subsequently deposited Si3N4 meets the electrical isolation requirements of the device, and the width of the D and S electrode pad metals 19 and 18 are both set to 250um, which meets the WB wiring requirements of the device. Si3N4 is used as the second isolation layer 20 for isolation and protection, and the thickness is 100nm; after preparing the D electrode 15 and the S electrode 14 in each active area 10, and preparing the D and S electrode pad metals 19 and 18 interconnected with the D and S electrodes 15 and 14 outside the active area 10, Figure 6 The device is shown in Figure 2 The schematic diagram of the x1 and x2 sections in the y1-y2 region is shown below. Figure 7 The surface schematic diagram shows the common source and common drain interdigitation structure in the active area 10, and the interconnection metals 17 and 16 and the D and S electrode pad metals 19 and 18 outside the active area 10. Figure 8 Further details show the device Figure 2 The surface schematic diagram of the D and S electrodes of the common source and common drain interdigitation structure in the active region 10 in the y1-y2 region and the interconnection metals 17 and 16 outside the active region 10 is shown. After the second isolation layer 20 is deposited, Fig. 9 The device is shown in Figure 2 Shown is a schematic diagram of the x1 and x2 sections in the y1-y2 region.
[0069] Step S500, a G electrode groove 21 is prepared in the G electrode region of the active region 10, referring to Fig.10 As shown;
[0070] Through epitaxial wafer cleaning, gluing, photolithography, and development, a photoresist is used to protect the outside of the G electrode area, and the G electrode area is etched by ICP dry etching to form a G electrode groove 21 in each active area 10, and then the photoresist is washed off;
[0071] Correspondingly, the etching depth of the G electrode groove 21 is the same as the sum of the thicknesses of the first isolation layer 11 and the second isolation layer 20 , and the width of the G electrode groove 21 in each active area 10 is consistent with the width of the G electrode region.
[0072] In this embodiment, CF4 is used for ICP dry etching, and the etching rate is 10nm / min to ensure the accuracy of etching. The sum of the thickness of the first isolation layer 11 and the second isolation layer 20 is 200nm, so the selected etching time is 20min, the etching depth is 200nm, and the width of the G electrode groove 16 in each active area 10 is 2um. Fig.10 It shows that after forming the G electrode groove 21 in each active area 10, the device Figure 2 Schematic diagram of the cross sections x1 and x2 in the y1-y2 region shown.
[0073] Step S600, prepare a G electrode 22 in the G electrode groove 21, prepare a G electrode pad metal 24 interconnected with the G electrode 22 outside the active area 10, and deposit a third isolation layer 25, referring to Fig.11 , 12 , 13, 14;
[0074] S610, using a metal lift-off process, through epitaxial wafer cleaning, gluing, photolithography, and development, the G electrode groove 21 area and the G electrode pad metal 24 area outside the active area 10 and the interconnection metal 23 area are protected with photoresist, Schottky contact metal of corresponding thickness is deposited in the G electrode groove 21 area in each active area 10 and the G electrode pad metal 24 area outside the active area 10 and the interconnection metal 23 area, a G electrode 22 is prepared in each active area 10, and a G electrode pad metal 24 interconnected with the G electrode 22 is prepared outside the active area 10, then the photoresist is cleaned off, and a third isolation layer 25 is deposited;
[0075] S620, optionally, a metal etching process may be used to first deposit a Schottky contact metal of a corresponding thickness, and then, through epitaxial wafer coating, photolithography, and development, the G electrode groove 21 region in each active region 10 and the G electrode pad metal 24 region and the interconnection metal 23 region are protected with photoresist, and the G electrode groove 21 region in each active region 10 and the G electrode pad metal 24 region and the metal outside the interconnection metal 23 region are etched away by ICP dry etching, and the etching depth is not less than the Schottky contact metal of the corresponding thickness deposited, ensuring that the G electrode groove 21 region in each active region 10 and the G electrode pad metal 24 region and the metal outside the interconnection metal 23 region are completely etched, and a G electrode 22 is prepared in each active region 10, and a G electrode pad metal 24 interconnected with the G electrode 22 is prepared outside the active region 10, and then the photoresist is cleaned off, and a third isolation layer 25 is deposited;
[0076] Correspondingly, the G electrode 22 in each active area 10 forms a good Schottky contact with the P-GaN layer 8, the upper surface of the G electrode 22 is level with the upper surface of the second isolation layer 20, the width of the G electrode and the G electrode pad metal interconnection metal 23 meets the electrical conduction requirement, and the width range is set to 1-100um, the distance between the G electrode and the G electrode pad metal interconnection metal 23 and the D electrode and the D electrode pad metal interconnection metal 17 meets the electrical isolation requirement, and the distance range is set to 1-100um, the width of the G electrode pad metal 24 meets the WB wiring requirement, and the width range is set to 50-1000um, the third isolation layer 25 mainly plays a protective role, and the thickness meets the condition that the third isolation layer 25 has little additional stress on the epitaxial wafer, and the thickness range is set to 10-10000nm.
[0077] In this case, a metal stripping process is used. Through epitaxial wafer cleaning, gluing, photolithography, and development, a photoresist is used to protect the G electrode groove 21 area in each active area 10 and the G electrode pad metal 24 area and the interconnection metal 23 area outside the active area 10. 10nmAu+40nmNi+70nmAl are deposited as Schottky contact metal in the G electrode groove 21 area in each active area 10 and the G electrode pad metal 24 area and the interconnection metal 23 area outside the active area 10. A G electrode 22 is prepared in each active area 10, and a G electrode pad metal 24 interconnected with the G electrode 22 is prepared outside the active area 10. Then, the photoresist is washed off. At this time, the upper surface of the G electrode 17 and the second insulation layer are connected. The upper surface of the separation layer 20 is horizontal, the width of the G electrode and the D electrode pad metal interconnection metal 23 is set to 20um, which meets the electrical conduction requirements of the device, the distance between the G electrode and the G electrode pad metal interconnection metal 23 and the D electrode and the D electrode pad metal interconnection metal 17 is set to 40um, and the subsequently deposited Si3N4 meets the electrical isolation requirements, the width of the G electrode pad metal 24 is set to 220um, which meets the WB wiring requirements of the device, and Si3N4 is used as the third isolation layer 25 for isolation and protection, with a thickness of 100nm; after preparing the G electrode 22 in each active area 10, and preparing the G electrode pad metal 24 interconnected with the G electrode 22 outside the active area 10, Fig.11 The device is shown in Figure 2 The schematic diagram of the x1 and x2 sections in the y1-y2 region is shown below. Fig.12 The surface schematic diagram shows the common source and common drain interdigitation structure in the active region 10, and the interconnection metal 23 and the G electrode pad metal 24 outside the active region 10. Fig.13 Further details show the device Figure 2 The schematic diagram of the surface of the G electrode 22 in the common source and common drain finger structure in the active region 10 and the interconnection metal 23 outside the active region 10 in the y1-y2 region is shown. After the third isolation layer 25 is deposited, Fig.14 The device is shown in Figure 2 Schematic diagram of the cross sections x1 and x2 in the y1-y2 region shown.
[0078] Step S700, open windows on the metal 19, 18, 24 regions of the D, S, and G electrode pads, refer to Fig.15 As shown;
[0079] S710, by cleaning, gluing, photolithography, and developing the epitaxial wafer, the areas outside the D, S, and G electrode pad metal 19, 18, and 24 are protected with photoresist, and the D, S, and G electrode pad metal 19, 18, and 24 areas in the active area 10 are etched with ICP dry etching, and then the photoresist is cleaned;
[0080] Accordingly, the etching depth is equal to the sum of the thickness of the third isolation layer 25 and the second isolation layer 20, ensuring that the D, S, G electrode Pad metals 19, 18, 24 in the active area 10 are successfully opened;
[0081] In this case, CF4 is used for ICP dry etching, and the etching rate is 10nm / min to ensure the accuracy of etching. The sum of the thickness of the third isolation layer 25 and the second isolation layer 20 is 200nm, so the selected etching time is 20min. Fig.15 The schematic diagram of the device surface after the D, S, G electrode Pad metals 19, 18, 24 in the active area 10 are opened is shown;
[0082] Step S800: the entire device is prepared.
[0083] Further description of the structural plan of this case:
[0084] High package power density GaN HEMT devices, including:
[0085] Epitaxial wafer, an ISO isolation region 9 is provided between the passive region and n active regions 10;
[0086] A first isolation layer 11 is deposited on the P-GaN layer 8 of the epitaxial wafer (only the P-GaN layer 8 in the G electrode region in each active region 10 is retained); an S electrode 14 and a D electrode 15 extending downward from the top surface of the first isolation layer 11 to the inside of the AlGaN barrier layer 7 are provided in the active region 10; and D and S electrode pad metals 19 and 18 interconnected with the S electrode 14 and the D electrode 15 are provided outside the active region 10;
[0087] A second isolation layer 20 is deposited on the top surface of the first isolation layer 11, the S electrode 14 and the D electrode 15; a G electrode 22 is provided in the active area 10, extending downward from the top surface of the second isolation layer 20 to the top surface of the P-GaN layer 8; a G electrode pad metal 24 interconnected with the G electrode 22 is provided outside the active area 10;
[0088] The third isolation layer 25 is deposited on the top surface of the second isolation layer 20 to play a protective and passivation role.
[0089] The epitaxial wafer is further defined as being a Si-based epitaxial wafer, a SiC-based epitaxial wafer or a GaN-based substrate epitaxial wafer.
[0090] The epitaxial wafer comprises a substrate 1, an AlN spacer layer 2, an Al composition gradient buffer AlGaN layer 3, a C-doped high-resistance GaN layer 4, a GaN channel layer 5, an AlN insertion layer 6, an AlGaN barrier layer 7 and a P-GaN layer 8, which are sequentially connected from bottom to top. Fig.14 shown.
[0091] It is further defined that the upper surface of the G electrode 22 and the upper surface of the second isolation layer 20 are in the same plane, and form a good Schottky contact with the P-GaN layer 8 .
[0092] It is further defined that the top surface of the D electrode 15 , the top surface of the S electrode 14 and the top surface of the first isolation layer 11 are in the same plane, forming a good ohmic contact with the two-dimensional electron gas in the channel below.
[0093] It is further defined that the top surface of the P-GaN layer 8 is lower than the bottom surface of the first isolation layer 11 thereon.
[0094] The utility model has the following advantages:
[0095] n active areas are formed on the GaN HEMT device, each active area is isolated from each other, the gate width in each active area is controlled to be 1mm, and the G, D, and S electrodes of each active area are interconnected with the G, D, and S electrode Pads of the device through the interconnection metal in the device. This solution can improve the current carrying capacity of a single device and increase the power density of the device in large-size packaging without affecting the gate control capability of the device and without introducing additional parasitic inductance and parasitic resistance.
[0096] Under the same process and the condition of determining the 8-pair interdigitation structure, the above-mentioned devices are packaged in DFN5*6, and the device of the utility model (Sample 4) with two active areas is as follows Fig.16 As shown in the figure, the conventional structure gate width 1mm device (Sample1) Fig.17 As shown in Figure 2, the gate width increases from 1mm to 2mm to match the package width size of the device (Sample2). Fig.18 As shown in Figure 2, two sealed devices with a gate width of 1 mm (Sample 3) are Fig.19As shown in Table 1, taking Sample 1 as an anchor, the size, package power density, gate control capability and parasitic parameters of the four devices are compared. It can be seen that in the DFN5*6 package, for Sample1, 2, 3, and 4, under the condition of determining the device length L, the package power density of Sample2, 3, and 4 is twice that of the traditional structure 1mm gate width device Sample1, but the gate width of the device Sample2 with the size of the package width increased from 1mm to 2mm is weak in gate control ability, and the parasitic resistance and parasitic inductance of the two 1mm gate width devices Sample3 are large, which will affect the normal use of the device and reduce the electrical performance quality of the device. The device Sample4 with two active areas has the advantages of high package power density, strong gate control ability, and small parasitic parameters. In terms of the overall size of the device, it can be seen that Sample4 has an additional 100um wide active area isolation area, and the device width is 0.1mm larger than Sample2, but Sample4 also has the advantages of high package power density, strong gate control ability, and small parasitic parameters. The slight disadvantage of the device in size compared with Sample2 is insignificant.
[0097] Table 1:
[0098] No W (mm) L (mm) Package power density Gate control capability Parasitic parameters Sample1 1.7 0.7 1 powerful Small Sample2 2.7 0.7 2 weak Small Sample3 3.4 0.7 2 powerful big Sample4 2.8 0.7 2 powerful Small
[0099] Regarding the contents disclosed in this case, there are a few points that need to be explained:
[0100] (1) The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case. Other structures can refer to the general design;
[0101] (2) In the absence of conflict, the embodiments and features of the embodiments disclosed in this case may be combined with each other to obtain new embodiments;
[0102] The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case should be based on the protection scope of the claims.
Claims
1. GaN HEMT devices with high package power density, It is characterized in that include: Epitaxial wafer; A first isolation layer (11) is deposited on the P-GaN layer (8) and the AlGaN barrier layer (7) of the epitaxial wafer; an S electrode (14) and a D electrode (15) are provided in the active region (10) and extend downward from the top surface of the first isolation layer (11) to the inside of the AlGaN barrier layer (7); and D and S electrode pad metals (19, 18) interconnected with the S electrode (14) and the D electrode (15) are provided outside the active region (10); A second isolation layer (20) is deposited on the top surfaces of the first isolation layer (11), the S electrode (14) and the D electrode (15); a G electrode (22) is provided in the active region (10), and extends downward from the top surface of the second isolation layer (20) to the top surface of the P-GaN layer (8); and a G electrode pad metal (24) interconnected with the G electrode (22) is provided outside the active region (10); A third isolation layer (25) is deposited on the top surface of the second isolation layer (20).
2. The high package power density GaN HEMT device according to claim 1, It is characterized in that The epitaxial wafer is a Si-based epitaxial wafer, a SiC-based epitaxial wafer or a GaN-based substrate epitaxial wafer.
3. The high package power density GaN HEMT device according to claim 1, It is characterized in that The epitaxial wafer comprises a substrate (1), an AlN spacer layer (2), an Al composition gradient buffer AlGaN layer (3), a C-doped high-resistance GaN layer (4), a GaN channel layer (5), an AlN insertion layer (6), an AlGaN barrier layer (7) and a P-GaN layer (8) which are connected in sequence from bottom to top.
4. The high package power density GaN HEMT device according to claim 1, It is characterized in that The upper surface of the G electrode (22) and the upper surface of the second isolation layer (20) are in the same plane, and form a Schottky contact with the P-GaN layer (8).
5. The high package power density GaN HEMT device according to claim 1, It is characterized in that The top surface of the D electrode (15), the top surface of the S electrode (14) and the top surface of the first isolation layer (11) are on the same plane and form an ohmic contact with the two-dimensional electron gas in the channel below.
6. The high package power density GaN HEMT device according to claim 1, It is characterized in that The top surface of the P-GaN layer (8) is lower than the bottom surface of the first isolation layer (11) above it.
Citation Information
Cited By
GaN HEMT device with high packaging power density and preparation method thereof
CN117637475A