Multi-beam deflection array device for maskless particle beam processing

The multi-beam deflection array device with integrated electrodes within depressions on a single plate addresses crosstalk and manufacturing complexity issues, achieving reduced size and improved accuracy in particle beam exposure systems.

DE102008010123B4Active Publication Date: 2024-11-28IMS NANOFABTION +1
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
DE102008010123
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2008-02-20
Publication Date
2024-11-28
Estimated Expiration
2028-02-20

AI Technical Summary

Technical Problem

Existing pattern definition devices in particle beam exposure systems face issues such as crosstalk between apertures, complex electrode formation processes, sensitivity to deformation, and restrictions on electric field strength due to electrode height, which affect the integration density and accuracy of beam shaping.

Method used

A multi-beam deflection array device with integrated electrodes within depressions on a single plate, using a semiconducting substrate like doped silicon, and a hidden insulating layer to minimize crosstalk and electrostatic field interference, allowing for reduced size and cost-effective production.

Benefits of technology

The solution effectively minimizes crosstalk and reduces the size of the pattern definition system while maintaining high integration density and accuracy, simplifying the manufacturing process and improving the electrostatic field control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Multi-beam deflection array device (502, 311, 321, 331, 700, 130) for use in a particle beam exposure device operating with a beam (lb) of charged particles, wherein the multi-beam deflection array device has an overall plate-like shape with a membrane region comprising: - a first side (504) facing the incoming particle beam (lb) and a second side (504) opposite it, - an array of apertures, each allowing the passage of a corresponding beam element formed from the particle beam, - a number of depressions (512), each formed in one of the sides of the membrane area and associated with at least one of the apertures, and - an array of electrodes (511), wherein each aperture is assigned to at least one of the electrodes (511) and each electrode is located in one of the recesses (512) and the electrode is spaced perpendicular to the beam (lb) from the material of the membrane region surrounding the respective recess (512), and the electrodes are configured to realize a non-deflection state in which the particles passing through the apertures can move forward along a desired path, and a deflection state in which the particles are deflected away from the desired path.
Need to check novelty before this filing date? Find Prior Art

Description

Field of the invention and prior art

[0001] The invention relates to a multi-beam deflection array device for a maskless particle beam exposure apparatus for forming a pattern on a surface of a substrate using a plurality of beams of high-energy charged particles. More specifically, the invention relates to a multi-beam deflection array device as part of a pattern definition means for use in a maskless particle beam exposure apparatus.

[0002] Furthermore, the invention relates to a method for producing this multi-beam deflection array device.

[0003] In a particle beam exposure device, a particle beam is generated by an illumination system. This particle beam illuminates a pattern-defining means with an array (regular arrangement) of apertures that define a beam pattern to be projected onto a target surface. An important application of a particle beam exposure device of this type is in the field of nanoscale structuring, with direct ion beam modification of materials or with electron- or ion-beam-induced etching and / or deposition, for the fabrication or functionalization of nanoscale devices. Another important application is in the field of maskless particle beam lithography, which is used in semiconductor technology; namely, a lithography device that processes a substrate, e.g., a silicon wafer covered with a layer of radiation-sensitive resist, to create a desired pattern on the substrate surface.A desired pattern is exposed onto the photoresist, which is then developed—in the case of a positive resist, by partial removal according to the pattern defined in the previous exposure step. The developed resist is used as a mask for further patterning processes, such as reactive etching.

[0004] A particle beam exposure device is described in US Pat. No. 5,369,282. Arai et al. discuss an electron beam exposure system that uses a blanking aperture array (BAA) to serve as the pattern defining means. The BAA carries a number of rows of apertures, and the images of the apertures are scanned across the surface of the substrate in a controlled, uniform motion perpendicular to the rows of apertures. The rows are aligned with each other in an interleaved manner so that the apertures form staggered lines as viewed in the direction of the scanning motion. Thus, as the staggered lines move relative to the substrate, they sweep uniform lines across the substrate without leaving gaps between them, thereby covering the entire surface of the substrate to be exposed.

[0005] Applicant's US 6,768,125 B2 presents a maskless multi-beam lithography concept, called PML2 ('Projection Mask-Less Lithography #2'), which employs a pattern definition device comprising a number of stacked plates, including an aperture array device (aperture plate) and a deflection array device (blanking plate). These individual plates are mounted together at defined intervals, for example, in a housing.

[0006] The aperture plate has an array of apertures that define a beam pattern consisting of partial beams to be projected onto a target surface. These apertures include corresponding blanking openings in the blanking plate. These blanking openings are arranged so that each of the partial beams passes through the blanking opening corresponding to the aperture defining the respective partial beam. Each blanking opening is equipped with a deflection means that can be controlled by a blanking signal between two blanking states: a first state ("on") in which the deflection means assumes a state in which particles passing through the opening can move forward along a desired path, and a second state ("off") in which the deflection means deflects particles passing through the opening away from this path.

[0007] The deflection means comprises a set of electrodes for beam blanking, basically a pair. Applicant's US 2005 / 0242302 A1 proposes forming the electrodes around the blanking apertures by vertical growth using prior art electroplating techniques. The document proposes designing one of the electrodes, the so-called ground electrode, to have a significant height above the blanking plate and the other electrode, the so-called blanking electrode. This serves to provide better shielding of the blanking apertures against crosstalk and other undesirable effects.

[0008] There are several problematic issues with using a pattern-defining device according to the state of the art. Shielding the blanking apertures against crosstalk, for example, and a simple method for producing this blanking agent are essential. In particular, forming the electrodes using perpendicular growth is a rather complicated process. Furthermore, such electrodes are very sensitive to deformation and strain.

[0009] Furthermore, electrodes with a significant height above the blanking plate impose a limitation on the permissible electric field strength in the vicinity of the blanking plate (this results from stray fields around the electrodes due to the boundary conditions for the field lines). This is particularly disadvantageous when the blanking plate is used as part of a grating lens (as described, for example, in US 5,801,388 and US 6,326,632, owned by the applicant), where the side of the blanking plate containing the electrodes is used to define an electrostatic potential of the electrostatic negative (scattering) and / or positive (collecting) lens.

[0010] US 2005 / 0087701 A1 describes a pattern definition device for use in a particle beam exposure apparatus, wherein a beam of electrically charged particles is structured through a plurality of apertures. The device comprises at least one deflection arrangement with a plurality of apertures surrounding the beams, wherein at least two deflection electrodes are provided for each aperture, to which different electrostatic potentials can be applied, thereby correcting the path of the beam(s) passing through the respective aperture according to a desired path through the device.

[0011] DE 689 18 144 T2 discloses a charged particle beam exposure system, wherein a series of individual blanking apertures is provided to form a series of beams which are individually blanked and shown by applying voltages to the electrodes within the blanking apertures.

[0012] EP 1 033 741 A2 describes a charged particle beam lithography system comprising a beam source, a blanking aperture, a deflection unit, a convergence unit, and an exposure control circuit. The blanking aperture consists of a plurality of apertures and electrodes arranged opposite one another in pairs. Using an on / off signal applied to a deflection electrode at each aperture, it can be determined whether a charged particle beam passing through each aperture in the blanking aperture arrangement is being irradiated onto a sample. The deflection unit deflects the charged particle beam passing through the blanking aperture.

[0013] In the prior art, the pattern definition means includes at least two different plates for the comparatively high integration density of the apertures and deflection devices: an aperture plate to shape the beams and absorb a large portion of the heat load introduced by the incoming beam, and a blanking plate serving as a deflection array plate. Highly precise alignment between the two or more plates and excellent alignment with the direction of the incoming beam are necessary. Brief description of the invention

[0014] The invention aims to overcome the aforementioned weaknesses of the prior art. In particular, the design of a pattern definition device is to be improved, resulting in a design that is suitable for manufacture using inexpensive prior art methods.

[0015] This object is achieved according to the invention by a multi-beam deflection array device for use in a particle beam exposure apparatus according to claim 1.

[0016] Thanks to this solution, the arrangement of the electrodes within the recesses offers the advantage of minimizing crosstalk between the apertures, as these are shielded by the substrate material of the multi-beam deflection array device—hereinafter referred to as deflector array plate or DAP. Furthermore, considering the unavoidable thermal load resulting from the electrical power consumption of integrated circuits operating at high frequencies, the critical cross-sectional area for heat conduction along the membrane to the thicker support frame supporting the membrane is significantly increased, since, according to a preferred embodiment of the invention, the space between the deflectors is filled with thermally conductive material.At least one electrode serves as an active deflection electrode, while the associated element for the electrical ground can be realized either by a second electrode or, in a preferred variant, by using the substrate material of the DAP as a ground electrode.

[0017] In a variant of the invention, the recesses are formed on the first side of the DAP, ie the side facing the beam source.

[0018] In an alternative variant of the invention, the depressions are formed on the second side of the DAP, i.e., on the side facing the target. By combining the aperture plate with the DAP into one plate, the size of the pattern definition system can be further reduced. This variant is made possible by the special property of the invention that no significant field extends into the space beyond the pattern definition system. This is because the electrodes excited for beam switching are located within the depressions and do not cause any significant changes in the electrostatic field outside the depressions. The electrostatic field in the space outside the pattern definition system is determined by the electrostatic potential applied to the membrane surface and the potentials of neighboring electrodes (e.g.,Ring electrodes), whereby the recesses and electrodes therein do not lead to any significant stray fields in this area. This is particularly important when (as in, for example, US 5,801,388 and US 6,326,632 of the applicant) the pattern-defining means is used in conjunction with an external electrostatic field as a grating lens mask.

[0019] In another variant of the invention, a beam-shaping layer is provided on the first side of the membrane region, wherein the beam-shaping layer contains a plurality of retrograde stencil openings, each of which coincides (spatially / laterally matches) with a subsequent aperture in the membrane region and has an inner width that is smaller than the inner width of the associated aperture. This means that the apertures in the membrane region contain retrograde stencil openings in the beam-shaping layer. "Retrograde" here means that the stencil openings in the beam-shaping layer have a smaller inner width than the inner width of the apertures in the membrane region.

[0020] The beam-shaping layer, if present, is used to define the shape of the partial beams from the incoming particle beam. This allows the pattern definition system to be implemented with a single plate. A separate cover plate and aperture plate, as in the prior art, can be eliminated. This allows both the dimensions and production costs to be reduced.

[0021] Advantageously, the membrane region of the DAP can be made of a semiconducting substrate material. In particular, the substrate material can be silicon. Semiconducting materials allow the use of CMOS technology for structuring the integrated circuits and other proven microstructuring techniques for processing the substrate material. In the electrode region, where electrostatic potentials must change rapidly and electric field strengths must build up to deflect the particles, doped silicon could be used, e.g., with a conductivity of approximately 5 mΩcm. Appropriate values ​​of the dielectric constant ε and the electrical conductivity σ are used to optimize the dynamic behavior and function of the multi-beam deflector array means according to the invention for the desired operating frequency.

[0022] In a preferred embodiment of the invention, a hidden insulating layer exists between the electrodes and a layer containing electronics for controlling the electrodes. This hidden insulating layer can preferably be made of silicon oxide (SiO2) and extend over the entire membrane area. The insulating layer is used to separate the doped silicon region (for conductive electrodes) from the integrated circuits (IC), e.g., a CMOS layer.

[0023] Preferably, but not necessarily, the electrodes are made of the same material as the substrate material of the membrane region. This simplifies the production of the DAP according to the invention. In contrast to the prior art, e.g., US 2005 / 0242302 A1, the electrodes do not have to be formed by vertical growth. Furthermore, the electrodes can be coated with a metallic material. In addition to the protective effect of such a coating, its good conductivity allows for the dissipation of electrical charges resulting from the beam of charged particles.

[0024] Preferably, the electrodes do not protrude above the surface level of the membrane region side in which the recesses are formed. This means that the electrodes have a height equal to or below this surface level. This can effectively reduce crosstalk between the apertures and the propagation of the electric field generated by the electrodes.

[0025] In an advantageous embodiment of the invention, the deflection electrodes are contacted from the membrane region side which is opposite to the membrane region side in which the depressions are formed.

[0026] Preferably, the recesses have a diameter (in the sense of an inner width) that is smaller than the distance between the first and second sides of the membrane region.

[0027] Because the substrate material of the DAP is configured to act as a ground electrode for the deflection electrode, the creation of individual ground electrodes providing a ground potential is eliminated, and the manufacturing process for said devices can be simplified. For this variant, it is advantageous to provide a hidden insulating layer between the deflection electrodes and the substrate material, such as SiO2 in an SOI (silicon on insulator) wafer.

[0028] In another variant of the invention, each aperture with at least one deflection electrode can be associated with at least one ground electrode located in the recess surrounding the aperture. In this case, it is preferred that the ground and deflection electrodes do not protrude above the surface level of the membrane side in which the recesses are formed. This allows for a reduction in the size of the pattern definition system and a minimization of crosstalk between the apertures.

[0029] The invention further includes a method for manufacturing a multi-beam deflection array device for use in a projection lithography system according to claim 17.

[0030] In addition, after step b), an insulating layer may be deposited on the top side of the SOI wafer blank, covering the top side of the SOI wafer blank.

[0031] Before step c), metallic vias can be applied to selected recesses created in step a) on the top side of the SOI wafer blank.

[0032] In a possible variant of the process, the backside of the SOI wafer blank can be thinned in the membrane area before step d), e.g., to a thickness of 50 µm. This can be done using well-known techniques such as chemical mechanical polishing (CMP).

[0033] After step d), a metallic protective layer can be deposited on the structures on top of the SOI wafer blank. This layer can serve to discharge the surfaces exposed to the charged particles of the particle beam exposure device.

[0034] Preferably, in step d), the buried insulator layer is undercut during lithography using plasma etching (RIE). This measure prevents the buried silicon oxide layer from accumulating an electrical charge when struck by electrically charged particles of the particle beam.

[0035] The invention also includes a further method for manufacturing a multi-beam deflection array device according to claim 23.

[0036] Step d) of this method can be implemented in such a way that an insulating layer is formed on the upper side in defined areas at least adjacent to the locations of the sub-areas, on which the electrical contact means are formed in the form of contact fields.

[0037] Preferably, in step e), the backside can be thinned in the membrane region, wherein even more preferably the insulator layer is removed during the thinning process. Brief description of the drawings

[0038] In the following, the invention is described in more detail with reference to the drawings, which schematically show: Fig. 1 shows, in a longitudinal section, the structure of a particle beam exposure device to which the invention applies; Fig. 2 is a longitudinal section detail of a prior art pattern definition system used for the lithography apparatus of Fig. 1 is suitable according to the state of the art; Fig. 3 to 5 Longitudinal section details of the lithography device of the Fig. 1 suitable embodiments of the pattern definition system according to the invention; Fig. 6 and Fig. 7 different realizations of the deflection electrodes; Fig. 8 is an enlarged sectional view of an aperture in a multi-beam deflection array device according to the invention; Fig. 9.1 to 9.16 a sequence of diagrams to explain the manufacture of a multi-beam deflection array device of the type described in Fig. 8 shown species; Fig. 10 is a longitudinal sectional view of a multi-beam deflection array device according to the invention; Fig. 11 is a plan view of a region with two apertures of the device of Fig. 10; Fig. 12 a section of the device of the Fig. 10 along line CC; Fig. 13 is a longitudinal section of a two-plate embodiment of a multi-beam deflection array device according to the invention; Fig. 14 a plan view of an opening of the deflection array device of the Fig. 13; Fig. 15.1 to 15.7 a sequence of diagrams to explain a manufacturing process of a multi-beam deflection array device of the type described in Fig. 13 and Fig. 14 shown species; Fig. 16 a C-shaped recess in plan view, which is used in the work step of Fig. 15.2 is formed; and Fig. 17 an A-shaped recess in plan view, as formed during a variant of the work process. Detailed description of the invention

[0039] The preferred embodiments of the invention discussed below relate to a PML2-type particle beam exposure device with a pattern definition device as disclosed in the applicant's US Pat. No. 6,768,125 (= GB 2 389 454 A) and with a high-reduction projection system. The following first presents the technical background of the device, as far as relevant to the invention, and then discusses embodiments of the invention in detail. It should be emphasized that the invention is neither limited to the following embodiments nor to a pattern definition system, which represents merely one of the possible implementations of the invention. PML2 system

[0040] Fig. Figure 1 shows an overview of a lithography device. For clarity, the components in Fig. 1 is not shown true to size. The main components of the device 100 are - according to the direction of the lithography beam lb, pb, which is Fig. 1 runs vertically downwards - an illumination system 101, a pattern definition system 102, a projection system 103 and a target station 104 with a target 17 on a wafer stage 18. The invention relates only to the pattern definition system 102. Nevertheless, the lithography apparatus will be described first in order to give an example of a possible application of the invention.

[0041] The entire device 100 is contained in a vacuum housing 105 maintained under high vacuum to ensure undisturbed propagation of the beam lb,pb along the optical axis cx of the device. In the illustrated embodiment, the particle-optical systems 101, 103 are largely implemented using electrostatic lenses; it should be noted that other implementations, such as electromagnetic lenses, may also be used.

[0042] The illumination system 101 comprises an electron source or an ion source 11 fed by a gas supply (not shown) and an extractor system 12. In one embodiment, helium ions (He +) is used. However, it should be noted that, in general, other electrically charged particles can also be used. In addition to electrons, these can be, for example, hydrogen ions or heavy ions; in the context of this disclosure, heavy ions refer to ions of elements heavier than C, such as O, N, or noble gases Ne, Ar, Kr, Xe. It is also possible to use negatively charged ions, such as negatively charged hydrogen ions or carbon fullerene ions.

[0043] The ion source 11 emits energetic ions, i.e., with a defined (kinetic) energy of typically a few keV, e.g., 10 keV. With the aid of an electro-optical condenser lens system 13, the ions emitted by the source 11 are formed into a broad, essentially telecentric ion beam, which serves as the lithography beam 1b. The lithography beam 1b then irradiates the pattern definition system 102, which is described in more detail below. The lithography beam 1b then illuminates a plurality of apertures in the pattern definition system 102. Certain of the apertures are "switched on" or "open," making them transparent to the incident beam; the other apertures are "switched off" or "closed," i.e., non-transparent to the beam, meaning that the partial beam does not reach the target.The pattern of the switched-on apertures is selected according to the pattern to be exposed on the substrate 17, since these apertures are the only areas of the pattern definition device that are transparent to the beam 1b; the beam is thus shaped into a shaped beam pb consisting of a plurality of sub-beams.

[0044] The pattern represented by the shaped beam pb is then projected onto the substrate 17 by a particle projection system 103, where it forms an image of the switched-on apertures of the pattern definition system 102. The projection system 103 achieves a reduction of, for example, 200x with two crossovers c1, c2. If a partial beam is deflected by the pattern definition system 102 from its switched-on path, it is absorbed, for example, by a stop plate 16.

[0045] The substrate 17 can be a silicon wafer coated with a photoresist sensitive to the particle beams. The wafer 17 is held and positioned by a wafer stage 18 of the target station 104. Image position and distortion can be corrected using multipole electrodes 14 and 15.

[0046] Fig. Figure 2 shows the operation of the pattern definition system 102 according to a prior art embodiment, such as described in US Pat. No. 6,768,125 of the applicant. Only details necessary to disclose the operation are given. It should be noted that the dimensions of the longitudinal axis in Fig. 2 to 5 are enlarged and not to scale. The pattern definition system 102 comprises a number of plates mounted in a stacked configuration, forming a composite device whose components each perform their own functions. Each of the plates is preferably formed as a semiconductor wafer (particularly a silicon wafer) in which the structures have been created using well-known microstructuring techniques. The lithography beam 1b penetrates the plates through an array of apertures. Each aperture corresponds to a set of successive openings defined in these plates.

[0047] The first plate in the direction of the incident beam is a cover plate 200. By absorbing a large part of the incoming lithography beam 1b, the cover plate 200 serves to protect the subsequent plates from radiation damage. For this purpose, it can be covered with a resistant layer 210. The lithography beam 1b passes through the cover plate through a plurality of apertures, of which only two are in Fig. 2 and the following figures.

[0048] The cover plate 200 is followed by an aperture array plate 201 with an array (regular arrangement) of openings that serve to define the shape of the partial beams. Each opening corresponds to an opening in the cover plate 200. The openings in the aperture array plate have a width that is smaller than the width of the corresponding openings in the cover plate 200.

[0049] Following the aperture array plate 201 in the direction of the particle beam is a DAP 202. This plate serves to shut off the passage of selected partial beams; it has a plurality of openings, each corresponding to an aperture of the aperture array plate 201 and each equipped with a deflection means that is individually controlled to deflect particles radiated through the openings away from their path. This deflection means can consist of a deflection electrode 230, 230' and a ground electrode 220, 220'. The electrodes are freestanding with respect to the DAP. In the embodiment of the Fig. 2, these electrodes can be produced by vertical growth using state-of-the-art techniques.

[0050] For example, partial beam A passes through the successive apertures of the pattern definition system 102 without being deflected because the associated deflection electrode 230 is not excited, meaning that no voltage is applied to the deflection electrode. This corresponds to the "on" state of the aperture. Partial beam A passes through the pattern definition system 102 unaffected and is focused by the first crossover c1 of the particle-optical system 103 ( Fig. 1).

[0051] In contrast, by exciting the deflection electrode 230' belonging to the partial beam B, ie applying a transverse voltage, a "switched off" state is implemented. In this state, the deflection electrode 230' deflects the partial beam B away from its path. The partial beam B is consequently deflected away from the first crossover c1 and thus absorbed at the stop plate 16. The beam deflection angles are in Fig. 2 to 5 are exaggerated and generally very small, typically 0.5 to 5 mrad.

[0052] The pattern of the switched-on apertures is selected according to a pattern to be exposed on the substrate 17, since these apertures are the only areas of the pattern definition device transparent to the beam lb, thereby shaping the beam into a shaped beam pb emerging from the device. DAP with single plate

[0053] Fig. 3 to 5 show various embodiments of a pattern definition system according to the invention with a DAP in the form of a single plate. In Fig. 3, the aperture array plate 310 is combined with the functions of the cover plate to form a "beam-shaping plate" arranged above the DAP 311. The aperture array plate 310 is thick enough to dissipate the thermal load caused by the incident particles of the particle beam 1b. The deflection means is implemented by only one deflection electrode 312, 312' per aperture. The substrate material of the DAP 311 is configured to act as a ground electrode to the deflection electrodes 312, 312'. In contrast to the prior art, the deflection electrodes 312, 312' are not freestanding, but are located within recesses 313, 313' formed around the apertures on the side of the DAP opposite the incoming particle beam. The electrodes do not protrude above the surface level of this side. Such an arrangement has the advantage of reducing the overall size of the pattern definition system.

[0054] Fig. 4, which has the same sequence of functional plates as Fig. 3 shows, differs in the design of the DAP 321: Here, the recesses around the apertures are formed on the side of the DAP facing the incoming particle beam. By placing the deflection electrodes 322, 322' in the recesses, deformation of the electric field gradient outside the gap between the aperture array plate 320 and the DAP 321 can be prevented.

[0055] In a Fig. In the variant of the invention illustrated in Figure 5, a modified DAP 331 is used as a pattern definition system, combining the functions of a cover plate, aperture plate, and deflection plate into one plate. A beam-shaping layer 330, provided on the first side of the DAP 331, is used to define the shape of the particle beams. The beam-shaping layer 330 can be part of the membrane or added in a subsequent process step, such as vapor deposition of a metal, electroplating, or bonding a separate layer to the DAP 331. The apertures of the DAP 331 contain retrograde stencil openings 333 in the beam-shaping layer 330. "Retrograde" in this context means that the inner width in the stencil openings 333 of the beam-shaping layer 330 is smaller than the inner width in the following aperture of the DAP 331.The inner width of the stencil openings 333 can either be constant across the entire stencil opening or increase in the direction of the beam, widening toward the side facing away from the incoming beam. The term "retrograde" is used here to indicate that the inner width of the apertures of the DAP 331 is smaller in the stencil openings in the beam-shaping layer 330 than in the adjacent aperture. The partial beams are deflected by deflection electrodes 332, 332' located in the recesses formed in the DAP 331 on the side opposite the incoming particle beam.

[0056] The Fig. The embodiments of the invention shown in Figures 3 to 5 have a deflection electrode per aperture, which interacts with the substrate material of the DAP to act as associated ground electrodes. For the sake of completeness, two alternative arrangements of deflection and ground electrodes will be briefly presented.

[0057] Fig. Figure 6 shows a cross-section of a DAP 441 with an aperture through which a beam of charged particles is to pass. Located in a recess 410, two deflection electrodes 411, 412 of equal height are provided for deflecting said beam. The recess can be formed on one or the other side of the DAP 441. With such an arrangement, bipolar deflection can be achieved by exciting one or the other of the deflection electrodes 411, 412 with the substrate material of the DAP 441 configured to act as the corresponding ground electrodes.

[0058] Fig. Figure 7 shows an arrangement with a deflection electrode 415 and a ground electrode 414 formed in a recess 413, which arrangement can be located on either side of the DAP 441. The ground electrode 414 exceeds the deflection electrode 415 in height, with neither electrode extending above the surface level of the side on which the recess is located.

[0059] Furthermore, as for example in the design of the Fig. As shown in Figure 7, one or both types of electrodes 414, 415 may be coated with a metallic material.

[0060] Fig. Figure 8 shows a more detailed section of an aperture plate 501 and a DAP 502 according to the invention, corresponding to the embodiment of Fig. 3; only one aperture is shown for clarity. On the side facing the incoming beam 1b, the aperture plate 501 is covered with a resistant layer 500 to protect against radiation damage. The DAP 502 has a basic plate-like shape. Its first side 504 faces the incoming particle beam, the second side 503 faces it.

[0061] The DAP has a bulk layer 505 made of a semiconductor, preferably doped silicon with a conductivity of approximately 5 mΩcm. This layer defines the ground potential and serves as the substrate material for the DAP in the membrane region. The bulk material layer also allows any thermal load to be dissipated, which is associated with the electrical power consumption of integrated circuits operating at high frequencies for the electronic operation of the DAP 502. An insulating layer 506, e.g., silicon oxide, is located above the bulk material layer 505 on the side facing the incoming particle beam. Another silicon layer 507 is located above this insulating layer 506. The thickness of the bulk material layer 505 is approximately 50 µm. The thickness of the insulating layer 506 is approximately 300 nm; the silicon layer 507 typically measures 2 to 3 µm.

[0062] A CMOS circuit layer 508 is formed on the side of the silicon layer 507 facing the incoming particle beam. This CMOS circuit layer 508 contains the electronic components (not shown) that ensure the electronic operation of the DAP 502. The insulating layer 506 shields the silicon layer 507 and the CMOS circuit layer 508 from the bulk layer 505.

[0063] The CMOS circuit layer 508 is covered with an insulating protective layer 509, which may be made of silicon oxide, for example. A metal protective layer 510 is placed over the insulating layer 509 to prevent charging.

[0064] In the Fig. In the embodiment of the invention illustrated in Figure 8, the deflection electrode 511 is located in a recess 512 formed on the second side 503 of the DAP 502. Alternatively, this recess may be formed in the first side 504. Both implementations are within the scope of the invention.

[0065] Deflection electrode 511 is made of the same material as bulk layer 505. The electrode is formed from the substrate material of DAP 502 using lithographic techniques. A metal via 513 connects deflection electrode 511 to CMOS layer 508, which contains the electrical supply lines and control circuitry of the electrode. In the present embodiment, bulk layer 505 of DAP 502 serves as the ground electrode for deflection electrode 511. Manufacturing process

[0066] In the following, a possible way to produce a DAP according to the invention is presented.

[0067] Fig. 9.1 to 9.16 explain an exemplary manufacturing process for producing the DAP 502 of the Fig. 8. Cross-sections of the processed wafer are shown according to the sequential steps 1 to 16 of the method. For clarity, the manufacturing process is explained using a recess and its associated deflection electrode. Of course, a DAP 502 consists of a plurality of recesses and electrodes, so the following explanations do not represent any limitation of the invention.

[0068] A SOI wafer blank 600 is the starting material of the Fig. 9. The wafer blank 600 has a thickness of 650 µm, for example - Fig. 9.1. It comprises a bulk layer 601, a buried silicon oxide layer 602, for example, 300 nm thick, and a silicon layer 603, for example, 2 µm thick. Hereinafter, the silicon layer 603 is referred to as the top side TS of the SOI wafer 600, while the opposite side is referred to as the back side BS.

[0069] The top side TS and back side BS of the SOI wafer 600 contain alignment marks (in Fig. 9 to 9.14 not shown, cf. Fig. 10) to enable precise alignment of the structures created on both sides. The alignment marks are produced using standard double-sided photolithography and etching techniques. The alignment marks on the top side TS of the SOI wafer extend through the silicon layer 603 into the buried silicon oxide layer 602. The depth of the alignment marks on the back side BS of the SOI wafer must be such that precise operation of the alignment marks is possible throughout the entire manufacturing process. The alignment precision between the alignment marks on the top side TS and the bottom side BS of the SOI wafer 600 is approximately 0.1 µm using state-of-the-art techniques. Advanced systems allow for higher front / back alignment accuracy. The number of alignment marks is user-defined; at least two marks per DAP should be provided.

[0070] In a first step of the manufacturing process, recesses 604, 605 are created on the top side TS of the wafer 600 using plasma etching processes (RIE) - Fig. 9.2. The recesses 604, 605 extend through the silicon layer 603 and the insulating layer 602 of silicon oxide into the bulk layer 601. The recess 605 is intended to accommodate the via between the deflection electrode and the CMOS layer 606 produced in the following step.

[0071] In a next step, a CMOS circuit layer 606 is created on the silicon layer 603 on the top side TS of the wafer 600. This layer contains all electronic components for controlling the DAP. Although the creation of the CMOS layer 606 involves a sequence of steps, this is Fig. 9.3 is shown as only one step because the creation of such a layer is a well-established technique. It is also possible to begin the manufacturing process with the creation of the CMOS circuit layer 606 and continue with the creation of recesses as mentioned above and the other manufacturing steps discussed below.

[0072] By means of oxide deposition, the top side TS of the wafer is covered with an insulating layer of silicon oxide - Fig. 9.4. The insulating layer is then removed by RIE ( Fig. 9.5), whereby this layer remains on the vertical parts of the top surface TS of the wafer due to the anisotropic characteristics of the RIE.

[0073] Then, a metal contact 607 is introduced into the recess 605 to provide a connection between the CMOS layer 606 and the future electrode - Fig. 9.6. The next manufacturing steps concern the backside BS of the wafer 600. Therefore, an insulating layer 608 is applied to the topside TS of the wafer to protect the surface - Fig. 9.7 From here on, the cross section of the treated wafer is Fig. 9.8 to 9.16 shown reversed.

[0074] By applying known techniques on the back side BS of the wafer 600, a membrane region is formed: The thickness of the base material layer 601 is reduced from 650 µm to e.g. 50 µm, for example by using standard wafer thinning techniques - Fig. 9.8. The individual steps for this standard process, for example, KOH wet etching, are not shown.

[0075] Then, the backside BS of the wafer 600 is structured using lithographic processes. First, a thin insulating oxide layer 619, e.g., SiO2, is formed on the backside BS by thermal oxidation. Fig. 9.9. This thin layer of insulating oxide 619 is then covered with a spray layer of photoresist 609 - Fig. 9.10. The thin layer of insulating oxide 619 could be omitted and the subsequent etching could be carried out with a resist mask, but this would not be advantageous because the subsequent lithography steps involve etching up to 50 µm of silicon.

[0076] The photoresist layer 609 is exposed, for example, using a laser beam writer. For this purpose, one of the alignment marks on the backside BS of the wafer 600 is measured, and with this reference point, the desired pattern is exposed in the resist-covered membrane area on the backside BS. The exposed pattern is well aligned with the previously created recesses 604, 605. After laser beam lithography, the photoresist layer 609 is developed. Fig. 9.11.

[0077] Using RIE, the pattern of the resist mask is transferred into the thin layer of insulating oxide 619 - Fig. 9.12. In a next step, the photoresist is removed and a recess 611 is formed in the bulk layer using etching techniques, e.g. RIE - Fig. 9.13. This recess 611 will later serve as the recess housing the deflection electrode. The recess surrounds at least a central portion 612 of the base material that will form the electrode.

[0078] The laser beam lithography process is then applied again to the backside BS of the SOI wafer. A photoresist layer is applied to the backside BS and exposed using laser beam lithography. After developing the photoresist layer, RIE is used again to pattern the backside BS of wafer 600. The recess 611 now extends from the backside BS of wafer 600 through the bulk layer 601 to the buried silicon oxide layer 602. Fig. 9.14 shows only the result of these process steps.

[0079] The second application of the laser beam lithography process can be omitted; in this case, the photoresist (and thus the thin layer of insulating oxide) would be patterned differently. Consequently, after the first application of RIE, the recess would extend to the buried silicon oxide layer 602, with the top surface of the electrode aligning with the surface level of the backside BS of the SOI wafer.

[0080] In a next step, the etching is continued until the aperture passes through the entire wafer 600 - Fig. 9.15. Etching can be performed from the top side TS or the back side BS. It should be noted that the silicon oxide layer 602 is undercut during this process step. This helps to prevent charging of the silicon oxide layer 602 by charged particles of the particle beam. The undercut structure is shown in Fig. 9.15 by circles 610. Finally, the structures on the top side TS are covered with a metallic protective layer 611 - Fig. 9.16.

[0081] Fig. 9.16 now shows the deflection electrode 612 located in the depression 613 and associated with the aperture 614. The electrode is connected to the CMOS layer 606 via the metal contact 607, which is accommodated in the recess 605, wherein the metal contact 607 traverses the silicon oxide layer 602.

[0082] A schematic longitudinal section view of an entire DAP 700 produced by the method discussed above is shown in Fig. 10. The DAP 700 has a top side 705, which can be directed towards the incoming beam of particles, and opposite it a back side 706. Since some layers of the DAP have a vanishing thickness compared to the bulk layer and in Fig. 10 cannot be reproduced with reasonable accuracy, they have been suppressed for clarity. However, this should not imply any limitation of the invention. Fig. Figure 10 shows a membrane region 701 containing the recesses with the apertures and the associated electrodes. In one possible variant, an SOI wafer blank with a diameter of 150 mm is used. Such a wafer can accommodate up to eight DAPs, each 30 mm square.

[0083] The membrane area 701 has a square shape and is surrounded by a frame of considerable thickness, e.g., 650 µm. The side length 702 is 20 mm. The thickness of the base material in the membrane area is approximately 50 µm. Only three of a multitude of actually existing apertures are shown in Fig. 10 for clarity. Depending on the particular design, a single deflection array means may have more than one membrane region separated by regions of greater thickness. Because manufacturing involves process steps on both sides of the DAP, alignment marks 703, 704 on the top side 705 of the DAP 700 and corresponding alignment marks 703', 704' on the back side 706 enable alignment of the structures on both sides. The presence of two pairs of alignment marks as here is merely exemplary; any reasonable number of alignment marks is possible.

[0084] In another possible manufacturing process, briefly discussed below, the membrane area extends across the entire wafer. Thus, the entire wafer is thinned to a thickness of, for example, 50 µm.

[0085] The first process steps are similar to those of the manufacturing process explained in detail above, shown in Fig. 9.1 - 9.7. Fig. Figure 9.7 describes the deposition of a protective layer 608 on the top side TS of an SOI wafer. In the process described here, the top side of the SOI wafer is then bonded to a carrier wafer. The entire wafer is then thinned to a thickness of approximately 50 µm. CMP is used to produce a smooth surface. The next process steps for structuring the back side of the SOI wafer are again similar to the steps described in Fig. 9.8 - 9.16 of the first manufacturing process. Any alignment marks provided on the backside of the SOI wafer to enable alignment of the top and bottom structures must be deep enough to extend beyond the wafer thinning. Typical dimensions

[0086] Fig. Figure 11 shows a plan view of an area of ​​the membrane region 701 of a DAP 800 such as that of Fig. 8, with two apertures 801, 801' and the associated deflection electrodes 802, 802', which are located in the recesses 803, 803'.

[0087] Fig. 12 shows a cross section along the line CC of the Fig. 11 and provides an overview of typical dimensions of a DAP. For the sake of clarity, only the shape of the DAP is shown, omitting internal structures. The width 901 of an aperture can be 5 µm. A typical value of the distance 902 between the edge of the aperture nearest the deflection electrode 802 and the side of the deflection electrode 802 facing the aperture is 2 µm. It may be possible to reduce this distance to 1 µm, but this value is limited by the tolerance of the top / back alignment. A smaller distance 902 would be advantageous because a smaller voltage would be required to control the partial beams. The periodicity 903, i.e., the distance between corresponding edges of adjacent depressions, is approximately 30 µm. The thickness 905 of the substrate is 50 to 60 µm.The height 904 of an electrode is preferably around 40 µm - the height 904 can also correspond to the thickness of the substrate as long as the electrode does not protrude beyond the surface of the substrate. DAP with two plates

[0088] Fig. Figure 13 shows another embodiment 130 of a DAP. This consists of two plates 131, 132, which are produced from silicon wafers and connected by wafer bonding at bonding pads 133. The DAP 130 is connected to an aperture array plate of the type shown in Fig. 3 or Fig. 4 shown type combined.

[0089] The plates 131, 132 serve specific tasks in the DAP 130. The plate 131 has the deflection electrodes for each of the openings 140, whereas the plate 132 contains an electronics layer 142 (e.g., CMOS layer) with all the electrical circuitry required for processing and buffering the pattern data, which is then passed to the deflection plate 131 via the bonding pad contacts. (The internal structure of the electronics layer 142 is suppressed in the figures.) The plates 131, 132 are shown separately in the figure for clarity; for operation, they are permanently connected by bonding, and the bonding pads 133 provide not only a mechanical connection of the plates 131, 132, but also defined electrical contacts between the electronic components of the plates 131, 132, as explained in more detail below.The openings formed in plate 132 are significantly wider than the openings in plate 131 to allow for alignment tolerances and to reduce unwanted interference between the particle beam and the electronics of layer 142.

[0090] An advantageous design of the openings will now be described with reference to Fig. 13 and Fig. 14 discussed. Fig. Figure 14 shows a plan view of an opening 140 in the plate 131, wherein the Fig. 13 shown section along line NN of the Fig. 14. At each opening 140, a deflection electrode 135 is provided, while the surface 134 opposite the deflection electrode serves as a counter electrode. The counter electrode surface 134 can advantageously be shaped such that it projects into the opening 140, preferably with a concave surface to allow a defined electric field configuration. While the deflection electrode 135 is arranged opposite the surrounding bulk material 144 of the wafer membrane region (e.g., the membrane region in Fig. 10) is electrically insulated, the counter electrode surface 134 may be formed directly on the base material 144, and in this case, all deflection electrodes of the plate 131 operate with respect to a common ground potential of the base material 144. The ground potential is maintained via ground contact surfaces 143 formed outside the diaphragm region; additional ground contact surfaces may be present between the apertures to enhance the stability of the ground potential across the aperture array (reducing stray inductances).

[0091] The deflection electrodes 135 are connected to the base material 144 via a support material 145, which either has self-insulating properties (e.g., silicon oxide or nitride) or is adjacent to the material of the deflection electrode 135 and / or the base material 144 via an insulating intermediate layer (e.g., produced by surface oxidation). As already mentioned, each deflection electrode 135 is assigned a contact surface 133, which serves as an electrical feed for the electrical potential to be applied to the electrode. The contact surfaces 133 are electrically separated from the base material 144 by an insulating layer 141. As shown, the insulating layer can be provided only in certain areas of the membrane region as a carrier layer of the surfaces 133, which is only perforated at certain locations, namely to form electrical connections between the surfaces 133 and the respectively associated electrodes 135.In one variant, it may extend over the entire membrane area, with the exception of the aforementioned openings for electrical connections and windows for the openings 140.

[0092] A typical value for the distance between the deflection electrode 135 and the counter electrode surface 134 is approximately 5 to 6 µm. The plate 131 has a membrane with a thickness of approximately 20 to 80 µm, while the CMOS plate 132 can have a thickness of approximately 25 to 40 µm. The width of the openings in the CMOS plate can vary, as long as it leaves the openings 140 free; for example, 9 µm or more can be measured. The required accuracy of the bonding position is approximately ±2 µm. Of course, with regard to the aperture array plate according to Fig. 3 and Fig. 4 the apertures are embedded in the openings 140 of the DAP 130 with respect to the lateral directions; their position is shown in Fig. 14 is symbolically shown as a broken square. The width of an aperture can be, for example, 3.75 µm, with an aperture array plate thickness of approximately 10 to 20 µm. Manufacturing process of the two-plate DAP

[0093] An exemplary manufacturing process for plate 131 of the Fig. 13 and Fig. 14 is explained below using the Fig. 15.1 ff (cutting details illustrating the creation of two of the many openings). The process begins with an SOI wafer blank 650 - Fig. 15.1 - which has a bulk layer 651, the surface side of which is again referred to as the backside BS', a buried silicon oxide layer, e.g., 300 nm thick, serving as an etch stop layer 652, and a silicon layer 653, e.g., 50 µm thick, on the top side TS'. If available top-side silicon layers have a thickness less than the desired starting thickness, in this case 50 µm, a silicon layer 653 of the desired thickness can be created by epitaxial growth of silicon on the initial top-side layer.

[0094] At the location of the future openings 140, recesses 656 are defined on the top side of the wafer 650, for example by means of well-known lithographic methods, and etched by means of anisotropic etching such as RIE - Fig. 15.2. The recesses preferably end at the etch stop layer 652. The recess 656 has a C-like shape as in the top view of the Fig. 16. Each recess 656 surrounds and thus defines a projection 655 of the top layer, which will later become the deflection electrode 135 (see also Fig. 14).

[0095] In a next step, the flanks of the recesses 656 are provided with an insulating covering layer, e.g., by means of an oxidation process. (The oxide layers thus created are shown as thick vertical lines.) Then, the recess is filled with material, for example, with a-silicon or polysilicon. This step provides the support material 145, which will later provide the mechanical attachment of the electrode 135. The result of this step is shown in Fig. 15.3 shown.

[0096] As an alternative during the step of Fig. 15.3, the step of insulating the sides of the recess 656 can be omitted if, as in Fig. 15.3a an insulating support material is added.

[0097] Then, recesses 657, which form the openings 140 as in Fig. 14 are formed on the top side of the wafer. For this purpose, each recess 657 has a shape that meets the support material filled in the respective previous recesses 656 at two locations, so that the partial region 655 (the precursor of the electrode 135) is separated from the layer 653. The recesses are etched using the layer 652 as an etch stop layer; in a variant of the process (not shown), the recesses could be etched such that they extend through the oxide layer 652 into the bulk layer 651. The process methods for creating the recesses, in particular anisotropic etching, are well-known methods from the prior art. The result of this step is shown in Fig. 15.4 shown.

[0098] The amount of support material 145 can be selected so that it is just sufficient to mechanically connect the electrode 135 to the base material 144 and to support it during the subsequent processing sequence and during operation, while ensuring reliable electrical insulation from the top layer 653.

[0099] In the next step, electrical contacts are formed for the electrode regions 655. Areas of an insulator layer 141 and contact areas 133 thereon are deposited and connected so that they form electrical contacts for the future electrodes. It is important that the contact areas can be located at a location that is significantly offset laterally from the location of the electrodes. At the same time, the ground contact areas 143 ( Fig. 13). The result of this stage of the process shows Fig. 15.5.

[0100] Thereafter, the back side 651 is thinned down to the etch stop layer 652. Fig. 15.6 agrees with Fig. 15.5, but reversed since the back side BS' is now being processed. Thinning is preferably carried out only in membrane areas. At the same time, the recesses 657 are opened to the back side (since the etch stop layer is removed there), creating the openings 140. This step, shown in Fig. 15.7, the finished plate 131 results (the components of plate 131 are shown with different dimensions than in Fig. 13 shown).

[0101] The corresponding plate 132 can be produced using known CMOS processing techniques. The design of the electronic circuits is not part of the invention; the reader is referred to the previously mentioned publications for details on the DAP electronics. The plate 132 is provided with a plurality of holes corresponding to the openings in the plate 131 and also has matching bonding pads to provide the electrical contacts for the plate 131.

[0102] The alignment between the plate 131 and the CMOS plate 132 is achieved by means of alignment marks 160, which are created at the same time as the openings 130; otherwise, the alignment is achieved according to prior art methods.

[0103] Finally, plate 131 is bonded to plate 132, for example, using the eutectic bonding technique. Thinning of plate 132 can occur before or after the bonding process.

[0104] Of course, in addition to the modifications already mentioned, further variations of the process described above are possible. For example, instead of an SOI wafer 650, other wafer types with a hidden layer that can serve as an etch stop layer can be used. If the etch stop layer is not insulating, an additional step to create an insulator layer can be added after the thin etching step on the backside. Furthermore, in an additional etching step, added before or after the step of filling the support material, the size of the electrodes 135 can be reduced to create electrodes 135 whose height is smaller than the thickness of the surrounding material 144.

[0105] In a remarkable variation of the manufacturing process with regard to the steps of Fig. 15.2 to 15.3, the recess etched into the top layer 653 may have an annular or preferably A-shaped configuration, as shown in the top view of Fig. 17 with the reference number 654 (instead of the form 656 of the Fig. 16). Thus, the shape of the electrode 135 is already defined in this step, as an island 655' of the surface layer. Then, as above for Fig. As explained in Figure 15.3, the sides of the recesses 654 are provided with an insulating cover layer, and the recess is filled with the support material. The process flow then continues exactly as explained above (the recess for the opening 140 is created, etc.). If methods for partially filling a space with a material are available, these methods could be used to deliver the support material without displacing the recess, which would eliminate the need for re-etching the recess 140.

[0106] Of course, the two manufacturing processes can also be combined in a suitable manner; the main steps of the manufacturing process are the formation of the recesses on the top side, with the creation of structures in the surface layer at the locations of the apertures, forming the depression with the electrode structures located therein, and the treatment of the back side, which opens the apertures that extend through to the previously structured, corresponding recesses. For example, the first manufacturing process ( Fig. 9) for a two-plate DAP by omitting the process steps for producing the CMOS layer on the SOI wafer blank and instead performing process steps for producing contact pads as in the second manufacturing process ( Fig. 15.5) should be inserted.

Claims

[1] Multi-beam deflection array device (502, 311, 321, 331, 700, 130) for use in a particle beam exposure device operating with a beam (lb) of charged particles, the multi-beam deflection array device having an overall plate-like shape with a membrane region comprising: - a first side (504) facing the incoming particle beam (lb) and a second side (504) opposite thereto, - an array of apertures, each of which allows the passage of a corresponding beam element formed from the particle beam, - a number of recesses (512), each formed in one of the sides of the membrane region and associated with at least one of the apertures, and - an array of electrodes (511), each aperture being associated with at least one of the electrodes (511) and each electrode being located in one of the depressions (512) and the electrode being spaced perpendicularly to the beam (lb) from the material of the membrane region surrounding the respective depression (512), and the electrodes being configured to realize a non-deflecting state in which the particles passing through the apertures can advance along a desired path, and a deflecting state in which the particles are deflected away from the desired path. [2] Multi-beam deflection array device according to claim 1, characterized by that the recesses are formed on the first side (504). [3] Multi-beam deflection array device according to claim 1, characterized by that the recesses are formed on the second side (503). [4] Multi-beam deflection array device according to claim 3, characterized bya beam-shaping layer (330) provided on the first side of the membrane region, in which a plurality of retrograde stencil openings (333) are formed, each coinciding with a subsequent aperture and each having an inner width that is smaller than the inner width of the associated aperture. [5] Multi-beam deflection array device according to one of claims 1 to 4, characterized by that the membrane region consists of a semiconducting substrate material (505, 507), preferably silicon. [6] Multi-beam deflection array device according to one of claims 1 to 5, characterized by a hidden insulating layer (506) between the electrodes (511) and a layer (508) containing electronics for controlling the electrodes (511). [7] Multi-beam deflection array device according to claim 6, characterized by that the hidden insulating layer (506) extends over the entire membrane area. [8] Multi-beam deflection array device according to claim 6 or 7, characterized by that the membrane region consists of a semiconducting substrate material, as well as with a hidden insulating layer (506) of silicon oxide between the electrodes (511) and a layer (508) containing electronics for controlling the electrodes (511). [9] Multi-beam deflection array device according to one of claims 1 to 8, characterized by that the electrodes (511) are made of the same material as the substrate material of the membrane region. [10] Multi-beam deflection array device according to one of claims 1 to 9, characterized by that the electrodes (511) are surrounded by a metallic material (440). [11] Multi-beam deflection array device according to one of claims 1 to 10, characterized by that the electrodes (511) do not protrude from the surface level of the membrane region side (503, 504) in which the depressions (512) are formed. [12] Multi-beam deflection array device according to one of claims 1 to 11, characterized by that the deflection electrodes (511) are contacted from the membrane area side (503, 504) which is opposite to the membrane area side in which the depressions (512) are formed. [13] Multi-beam deflection array device according to one of claims 1 to 12, characterized by that the recesses (512) have a diameter which is smaller than the distance between the first (504) and second side (503) of the membrane region. [14] Multi-beam deflection array device according to one of claims 1 to 13, characterized by that the substrate material (505) is adapted to act as a ground electrode for the deflection electrode (511). [15] Multi-beam deflection array device according to one of claims 1 to 14, characterized bythat each aperture with its at least one deflection electrode (415) is associated with at least one ground electrode (414) which is located in the recess (413) surrounding the aperture. [16] Multi-beam deflection array device according to claim 15, characterized by that the ground electrode (415) and the deflection electrode (414) do not protrude from the surface level of the side of the membrane region in which the depressions are formed. [17] A method for producing a multi-beam deflection array device for use in a projection lithography system, namely a particle beam exposure device, from an SOI wafer blank (600) having a base material layer (601), a buried insulator layer (602) covered by a silicon layer (603) on a top side (TS) of the SOI wafer blank, opposite a back side (BS) of the wafer blank (600), characterized by following steps: a) structuring recesses (604, 605) on the top side (TS) of the SOI wafer blank (600), extending through the silicon layer (603) and the hidden insulator layer (602) into the base material layer (601), b) producing a CMOS layer (606) on the top side (TS) of the SOI wafer blank (600) over the silicon layer (603), c) depositing an insulating protective layer (608) on the top side (TS) of the SOI wafer blank (600), d) Structuring the back side (BS) of the SOI wafer blank (600) using lithographic processes and forming electrodes (612) spaced apart from surrounding material perpendicular to the beam (lb) and apertures (614) extending through to the corresponding recesses (604, 605) on the top side (TS) structured in a previous step. [18] Method according to claim 17, characterized bythat after step b) an insulating layer is deposited on the top side (TS) which covers the top side (TS) of the SOI wafer blank (600). [19] Method according to claim 18, characterized by that prior to step c), metallic through-contacts (607) are applied to the upper side (TS) in selected recesses (605) produced in step a). [20] Method according to one of claims 17 to 19, characterized by that before step d) the back side (BS) of the SOI wafer blank (600) is thinned in the membrane area. [21] Method according to one of claims 17 to 20, characterized by that after step d) a metallic protective layer (611) is deposited on the structures on the upper side (TS). [22] Method according to one of claims 17 to 21, characterized by that in step d) the hidden insulator layer (602) is undercut (610) during the use of lithographic processes. [23] A method for producing a multi-beam deflection array device for use in a projection lithography system, namely a particle beam exposure device, from an SOI wafer blank (650) having a base material layer (651), a buried insulator layer (652) covered by a silicon layer (653) on a top side (TS') of the SOI wafer blank, opposite a back side (BS') of the wafer blank (650), characterized by following steps: a) structuring recesses (656) on the upper side (TS') of the SOI wafer blank (650), extending through the silicon layer (653) at least to the hidden insulator layer (652), wherein the recesses each at least partially surround a partial region in the silicon layer, b) at least partially filling the recesses (656) with a support material (145), c) re-structuring the recesses (657) on the top side (TS), through the silicon layer (653) extending at least to the hidden insulator layer (652), wherein each recess (657) is formed into a shape in which the resulting recess - including sub-regions filled with support material (145) - surrounds the respective sub-region (655) in the silicon layer, whereby these sub-regions are electrically separated from the remaining silicon layer (653), d) producing electrical contact means for said partial regions (655), wherein the electrical contact means are electrically insulated from the remaining silicon layer, and e) Structuring the back side (BS) of the SOI wafer blank (650) by forming electrodes (612) spaced apart from surrounding material perpendicular to the beam (lb) and apertures (140) extending through to the corresponding recesses (657) on the top side (TS') structured in a previous step. [24] Method according to claim 23, characterized by that in step d) an insulating layer (655) is formed on the upper side in defined regions at least adjacent to the locations of the sub-regions, on which insulating layer the electrical contact means in the form of contact fields (133) are formed. [25] Method according to claim 23 or 24, characterized by that in step e) the back side (BS') is thinned in the membrane area. [26] Method according to claim 25, characterized by that when thinning the back side the insulator layer (652) is removed.

Citation Information

Patent Citations

  • Maskless particle beam system for exposing pattern on a substrate

    GB2389454A

  • Electron beam exposure method and system for exposing a pattern on a substrate with an improved accuracy and throughput

    US5369282A

  • Particle beam, in particular ionic optic imaging system

    US5801388A

  • Particle-optical imaging system for lithography purposes

    US6326632B1

  • Maskless particle-beam system for exposing a pattern on a substrate

    US6768125B2