Training procedure for protective element

The training process for protective elements on wafers uses ultrasound vibration and controlled heating/cooling to confirm complete melting of thermoplastic plastic, addressing uneven distribution and wafer damage issues, achieving uniform thickness and protection.

DE102020213864B4Active Publication Date: 2024-10-24DISCO CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
DE102020213864
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-11-06
Filing Date
2020-11-04
Publication Date
2024-10-24
Estimated Expiration
2040-11-04

AI Technical Summary

Technical Problem

Existing methods for forming protective elements on wafers using solid granular plastic face challenges in determining if the plastic has fully melted, leading to uneven distribution and potential damage to the wafer due to insufficiently melted plastic.

Method used

A training process involving a plastic intake, detection, distribution, and hardening steps, utilizing ultrasound vibration to confirm complete melting of thermoplastic plastic on a wafer, and a Peltier element for controlled heating and cooling to ensure uniform thickness and prevent wafer damage.

Benefits of technology

Ensures uniform distribution of melted thermoplastic plastic over the wafer surface, preventing damage and ensuring consistent thickness of the protective element by confirming complete melting before distribution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A training method for a protective element for forming a protective element on a surface on one side (Wb) of a wafer (W) by melting a thermoplastic polymer (P), wherein the training method for a protective element comprises: a plastic feed step for arranging several grains of the thermoplastic polymer (P) on a plastic placement surface (23) of a platform (20); a wafer holding step for holding a surface on another side (Wa) of the wafer (W) by a wafer holding surface (13) of a wafer holding unit (10); a contact step to move the wafer holding unit (10) and the platform (20) relative to each other in one direction so that they approach each other, using a vertical movement mechanism (30) to bring the surface of one side (Wb) of the wafer (W) held by the wafer holding unit (10) into contact with the grains of the thermoplastic polymer (P); a detection step for a plastic state for heating the granules of the thermoplastic polymer (P) in contact with the surface of one side (Wb) of the wafer (W) while an ultrasonic vibration propagates between the polymer placement surface (23) and the wafer holding surface (13), and detecting whether the thermoplastic polymer (P) that is clamped between the surface on one side (Wb) of the wafer (W), which is held at the wafer holding surface (13), and the polymer placement surface (23) has been joined or not; a distribution step for distributing the thermoplastic polymer (P), which was recognized as united in the recognition step for a polymer state, over an entire surface area on one side (Wb) of the wafer (W) through the wafer (W); and a curing step to cool the thermoplastic polymer (P) that was distributed to cure the thermoplastic polymer (P), wherein the protective element, which protects the entire surface area on one side (Wb) of the wafer (W), is formed.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION Technical field

[0001] The present invention relates to a training method for a protective element. Description of the state of the art

[0002] The technology disclosed in Japanese patent application JP 2017-168 565 A involves forming a protective element on a surface on one side of a wafer using a plastic material. The wafer is held by a clamping table through the protective element, and a surface on the opposite side of the wafer is ground. As a result, irregularities on the wafer are removed, and the wafer thickness is made uniform.

[0003] Forming the protective element is carried out, for example, as follows. First, a film is placed on a platform. A liquid plastic is applied to the film. The liquid plastic is spread across a surface on one side of the wafer. As a result, the liquid plastic is distributed over the entire surface area on that side of the wafer. The liquid plastic is then cured.

[0004] The liquid plastic is drawn from a tank filled with liquid plastic by a pump and applied to the platform's film. Since the liquid plastic tank is heavy, replacing it is strenuous for the operator. To address this problem, a technology exists that uses a solid granular plastic.

[0005] In this technology, the granular plastic is melted into a liquid plastic at a single stage and spread into a sheet shape through a surface on one side of a wafer. The plastic is then cured by cooling. As a result, a sheet-shaped element can be formed on the surface of one side of the wafer. JP 2017-168565A concerns a training device for a protective element. PRESENTATION OF THE INVENTION

[0006] In the above-described formation process for a protective element using solid granular plastic, the plastic to be melted is clamped between the platform and the wafer. It is difficult to determine whether the solid plastic has melted or not. As a result, insufficient liquid plastic, containing the incompletely melted plastic, may be distributed throughout the wafer. In this case, it is difficult to form a protective element of uniform thickness, and the granular plastic and the time required for liquefaction can be wasted.

[0007] Accordingly, an objective of the present invention is to provide a formation method for a protective element by which it can preferably be detected that a plastic has become liquid when forming a protective element by converting a solid plastic into a liquid.

[0008] In accordance with one aspect of the present invention, a formation method for a protective element is provided for forming a protective element on a surface on one side of a wafer, wherein the formation method for a protective element comprises: a plastic feeding step for arranging several grains of a thermoplastic polymer on a plastic placement surface of a platform, a wafer holding step for holding a surface on another side of the wafer by a wafer holding surface of a wafer holding unit, a contact step for moving the wafer holding unit and the platform relative to each other in one direction so that they approach each other, using a vertical movement mechanism to bring the surface on one side of the wafer, which is held on the wafer holding unit, into contact with the grains of the thermoplastic polymer.A detection step for a plastic state to heat the granules of the thermoplastic polymer in contact with the surface on one side of the wafer while an ultrasonic vibration is propagated between the polymer placement surface and the wafer holding surface, and to detect whether the thermoplastic polymer that has been bonded between the surface on one side of the wafer, which is held by the wafer holding surface, and the plastic placement surface has been bonded; a distribution step to distribute the thermoplastic polymer that has been detected as bonded, in the detection step for a plastic state over an entire area of ​​the surface on one side of the wafer through the wafer; and a curing step to cool the distributed thermoplastic polymer to cure the thermoplastic polymer. The protective element that protects the entire area of ​​the surface on one side of the wafer,is trained.

[0009] In the plastic state detection step of the formation process for a protective element of the present invention, it is detected whether the thermoplastic material, which is clamped between a surface on one side of the wafer and the plastic placement surface, is sufficiently melted and merged. If it is detected that the thermoplastic material is merged, the distribution step is carried out to distribute the thermoplastic material across the entire surface on one side of the wafer through the wafer. Therefore, in this formation process, the pressure and distribution of the thermoplastic material, which is not sufficiently melted, through the wafer can be prevented. Additionally, the pressure of the thermoplastic material, which is not sufficiently melted, through the wafer, and thus damage the wafer, can be prevented.Consequently, the thickness of the protective element, which includes the thermoplastic material formed on the surface on one side of the wafer, can be designed to be essentially uniform.

[0010] The above and further aims, features and advantages of the present invention and the way in which they are realized will become more apparent, and the invention itself will best be understood by studying the following description and the attached claims with reference to the attached drawings, which show a preferred embodiment of the invention. BRIEF DESCRIPTION OF THE FIGURES Fig. Figure 1 is a sectional view showing a configuration of a training device for a plastic protective element; Fig. 2 is a sectional view showing a plastic feeding step being carried out in the training device for a plastic protective element; Fig. 3 is a sectional view showing a wafer holding step being performed in the training device for a plastic protective element; Fig. 4 is a sectional view showing a wafer contact step being performed in the training device for a plastic protective element; Fig. Figure 5 is a sectional view showing a heating step and a detection step for a plastic condition in the training device for a plastic protective element; Fig. Figure 6 is a graph that represents an example of an ultrasonic vibration received by an ultrasonic wave receiver; Fig. Figure 7 is a sectional view showing a distribution step being carried out in the training device for a plastic protective element; Fig. Figure 8 is a sectional view showing a cooling (curing) process being carried out in the training device for a plastic protective element; Fig. Figure 9 is a sectional view showing a spacing step being performed in the training device for a plastic protective element; and Fig. Figure 10 is a sectional view showing a wafer removal step being performed in the training device for a plastic protective element. DETAILED DESCRIPTION OF THE PREFERRED VERSION

[0011] A training device 1 for a plastic protective element according to the present embodiment, which is in Fig. The process shown in Figure 1 serves to melt solid grains of a thermoplastic polymer P placed on a polymer placement surface 23 of a platform 20, to distribute the molten thermoplastic polymer P over the entire area of ​​a surface on one side of a wafer W, and to cure the distributed thermoplastic polymer P to form a protective element. The thermoplastic polymer P is, for example, a polyolefin. The polymer placement surface 23 has, for example, been coated with a fluorine coating, making it easy to remove the placed thermoplastic polymer P.

[0012] The training device 1 for a plastic protective element includes in a vacuum training chamber 2 a wafer holding unit 10 which holds the wafer W by means of a holding surface 13, wherein the platform 20 has the plastic placement surface 23 for placing the grains of the thermoplastic plastic P on it, and a vertical movement mechanism (vertical actuation mechanism) 30.

[0013] The vacuum training chamber 2 serves to enclose the training device 1 for a plastic protective element, which can form a vacuum within itself, and includes an opening 4, a cover 3 suitable for covering the opening 4, a cover opening / closing mechanism 5 for opening / closing the cover 3, and a vacuum pump 7 for forming a vacuum in the vacuum training chamber 2.

[0014] The wafer holding unit 10 includes a support column 11 extending to penetrate an upper surface of the vacuum training chamber 2 and a wafer holding table 12 provided at a lower end of the support column 11 and located within the vacuum training chamber 2. A lower surface of the wafer holding table 12 is the wafer holding surface 13 for suction retention of the wafer W. Note that a vacuum seal 2a for maintaining the vacuum within the vacuum training chamber 2 is provided at a portion of the upper surface of the vacuum training chamber 2 that is penetrated by the support column 11.

[0015] The support column 11 and the wafer holding table 12 are provided with air passages 15, which are connected to an air supply source 14 and a suction source 16. The wafer holding surface 13 of the wafer holding table 12 is designed to be selectively connected to either the air supply source 14 or the suction source 16 via the air passage 15. The wafer holding unit 10 is suitable for holding the wafer W by suction through the wafer holding surface 13, which is brought into contact with the suction source 16.

[0016] Additionally, the wafer holding unit 10 is equipped with an ultrasonic wave oscillator 18 located near the wafer holding surface 13. The ultrasonic wave oscillator 18 is connected to an ultrasonic wave transmission section 17, which, for example, includes a high-frequency power source. The ultrasonic wave oscillator 18 oscillates an ultrasonic wave using high-frequency power from the ultrasonic wave transmission section 17.

[0017] The platform 20 includes a support column 21 that extends so that it penetrates a lower surface of the vacuum training chamber 2 and a plastic placement table 22, which is provided at an upper end of the support column 21 and is located inside the vacuum training chamber 2. Furthermore, an upper surface of the plastic placement table 22 is the plastic placement surface 23 for placing the thermoplastic material P on it.

[0018] The plastic placement surface 23 is arranged such that it faces the wafer holding surface 13 of the wafer holding unit 10. Additionally, a vacuum seal 2b for maintaining the vacuum in the vacuum training chamber 2 is provided on a portion of a lower surface of the vacuum training chamber 2, which is penetrated by the support column 21.

[0019] Furthermore, the plastic placement table 22 of the platform 20 is equipped with an ultrasonic wave receiver 33 located near the plastic placement surface 23. The ultrasonic wave receiver 33 receives an ultrasonic wave propagated to it, converts the ultrasonic wave into a voltage, and transmits the voltage to an ultrasonic wave receiving section 34.

[0020] Additionally, the training device 1 for a plastic protective element includes a wafer conveying mechanism 40 and a plastic conveying mechanism 50. The wafer conveying mechanism 40 and the plastic conveying mechanism 50 are conveying elements similar to robot hands. The wafer conveying mechanism 40 and the plastic conveying mechanism 50 can be separate elements or a single element.

[0021] The wafer conveying mechanism 40 conveys the wafer W from outside into the vacuum training chamber 2. The wafer conveying mechanism 40 is suitable for positioning the wafer W in such a way that it faces the wafer holding surface 13 of the wafer holding unit 10, through the opening 4 in the vacuum training chamber 2. In the wafer holding unit 10, the wafer W, which is arranged in this way, can be held by suction through the wafer holding surface 13, which is connected to the suction source 16.

[0022] The plastic conveying mechanism 50 conveys several granules of the thermoplastic material P from outside to the training device 1 for a plastic protective element. The plastic conveying mechanism 50 places the granules of the thermoplastic material P on the plastic placement surface 23 of the platform 20 in the vacuum training chamber 2 through the opening 4. Note that an annular protruding part may be formed on an outer circumference of the plastic placement surface 23 so that the granules of the thermoplastic material P do not fall off the plastic placement surface 23.

[0023] The vertical movement mechanism 30 is arranged on an upper surface of the vacuum training chamber 2 and is connected to the support column 11 of the wafer holding unit 10. The vertical movement mechanism 30 moves the wafer holding unit 10 and the platform 20 relative to each other in a Z-axis direction, which is the vertical direction perpendicular to the plastic placement surface 23. In the present embodiment, the vertical movement mechanism 30 moves the support column 11 of the wafer holding unit 10 in the Z-axis direction. In other words, the vertical movement mechanism 30 is configured to move the wafer holding unit 10 in the Z-axis direction relative to the platform 20, which is fixed in place.

[0024] More precisely, the vertical motion mechanism 30 comprises an arm 31, which is connected to the support column 11 and extends in a horizontal direction, a drive rod 32, which is connected to the arm 31 and extends along the Z-axis direction, and a sensor 35, which detects a travel path. When the drive rod 32 is moved vertically by a drive source (not shown), the arm 31 and the wafer holder 10 (support column 11), which is connected to the arm 31, are moved vertically along the Z-axis direction. The travel path of the wafer holder 10 is detected by the sensor 35.

[0025] Furthermore, the training device 1 for a plastic protective element includes a load detector 60. The load detector 60 is connected to the support column 11 of the wafer holding unit 10 by the vertical movement mechanism 30. The load detector 60 detects a load transmitted to the wafer holding unit 10 (i.e., a force with which the wafer W presses the thermoplastic material P) when the wafer holding unit 10 and the platform 20 come into contact with each other through the wafer W and the thermoplastic material P.

[0026] In addition, according to the present embodiment, the platform 20 has a Peltier element 24 inside it. The Peltier element 24 is an example of a temperature control device arranged in the platform 20. The Peltier element 24 has, for example, a flat plate shape and is arranged near the plastic placement surface 23 of the plastic placement table 22 of the platform 20, parallel to the plastic placement surface 23. The Peltier element 24 has an upper surface 24a parallel to and near the plastic placement surface 23 and a lower surface 24b away from the plastic placement surface 23.

[0027] Furthermore, the ends of one side of a first electrical power line 25 and a second electrical power line 26, which are routed in the support column 21 and the plastic placement table 22, are attached to both ends of the Peltier element 24. The other side ends of the first electrical power line 25 and the second electrical power line 26 are connected to direct current (DC) power sources 28 by means of switches 27.

[0028] The DC power source 28 is a power source that supplies the Peltier element 24 with a direct current. The switch 27 has a function for connecting the DC power source 28 to the Peltier element 24 via the first electrical power line 25 and the second electrical power line 26, and a function for switching the direction of the direct current from the DC power source 28 to the Peltier element 24 via the first electrical power line 25 and the second electrical power line 26.

[0029] In other words, the switch 27 is designed to reverse the direction of the direct current supplied to the Peltier element 24. This reverse direction is used to heat the upper surface 24a of the Peltier element 24 and cool it. Note that the lower surface 24b of the Peltier element 24 is cooled when the direct current flows in the first direction and heated when the direct current flows in the second direction.

[0030] Furthermore, the training device 1 for a plastic protective element includes a control unit 70, which contains a computer that controls elements of the execution device 1 for a plastic protective element. The control unit 70 controls the elements of the training device 1 for a plastic protective element described above in order to train a protective element on an entire surface on one side of the wafer W.

[0031] Next, an operation for training the protective element for the wafer W in the training device 1 for a plastic protective element is described below. First, the control unit 70 controls the cover opening / closing mechanism 5 to open the cover 3 of the vacuum training chamber 2, thereby exposing the opening 4. Then, the control unit 70 moves the plastic conveying mechanism 50, which holds the multiple grains of the thermoplastic material P, in an -X direction, thereby conveying the thermoplastic material P into the vacuum training chamber 2 through the exposed opening 4. Furthermore, the control unit 70 controls the plastic conveying mechanism 50 to arrange (place) the multiple grains of the thermoplastic material P on the plastic placement surface 23 of the platform 20, for example, in a flat shape at substantially uniform intervals (plastic feed step), as shown in Fig. 2 shown.

[0032] Next, the control unit 70 brings the suction source 16, which is in Fig. As shown in Figure 1, the wafer holding surface 13 of the wafer holding unit 10 is connected to the wafer holding surface 13. As a result, a negative pressure is applied to the wafer holding surface 13. Furthermore, the control unit 70 moves the wafer conveying mechanism 50, which holds the wafer W in the -X direction, thereby conveying the wafer W through the exposed opening 4 in the vacuum training chamber 2, and positioning the wafer W so that it faces the wafer holding surface 13. Additionally, the control unit 70 holds a first surface (a surface on the other side) Wa of the wafer W through the wafer holding surface 13, as shown in Figure 1. Fig. Figure 3 shows that, as a result, the wafer W is in a state in which a second surface (surface on one side) Wb is directed towards the thermoplastic polymer P, located on an upper side of the thermoplastic polymer P, which is placed on the polymer placement surface 23 (wafer holding step).

[0033] Subsequently, the control unit 70 controls the cover opening / closing mechanism 5, which is located in Fig. Figure 1 shows the mechanism for closing the cover 3 of the vacuum training chamber 2, thereby closing the opening 4. The control unit 70 controls the vertical movement mechanism 30 to move the wafer holding unit 10 downwards along the Z-axis direction. As a result, as shown in Fig. As shown in Figure 4, the second surface Wb of the wafer W, which is held on the wafer holding surface 13 of the wafer holding unit 10, is brought into contact with the multiple grains of the thermoplastic polymer P, which is held on the polymer placement surface 23 of the platform 20 (wafer contact step).

[0034] In this way, the control unit 70 moves the wafer holding unit 10 and the platform 20 relative to each other in one direction, bringing them closer together, using the vertical movement mechanism 30, and brings the second surface Wb of the wafer W, held by the wafer holding unit 10, into contact with the granules of the thermoplastic material P, which is held against the plastic placement surface 23 (pressing the granules of the thermoplastic material P with a comparatively weak force). In this state, the control unit 70 controls the vacuum pump 7 to create a vacuum in the vacuum formation chamber 2.

[0035] Furthermore, in this state, when the air pressure in the vacuum training chamber 2 is equal to or less than a predetermined value, the control unit 70 controls the switch 27, which is located in Fig. Figure 1 shows how to connect the DC power source 28 to the Peltier element 24 via the first electrical power line 25 and the second electrical power line 26. The control unit 70 then controls the switch 27 to direct the DC current from the DC power source 28 in a first direction to heat the upper surface 24a of the Peltier element 24, as indicated by arrow D1 in Figure 1. Fig. 5 is indicated.

[0036] In this way, while the thermoplastic polymer P is being forced through the second surface Wb of the wafer W, the control unit 70 causes the direct current to flow in the first direction, thereby heating the upper surface 24a of the Peltier element 24, the polymer placement surface 23 around the thermoplastic polymer P at the polymer placement surface 23, and melting the thermoplastic polymer P (heating step). Note that in this case, the lower surface 24b of the Peltier element 24 is cooled.

[0037] Furthermore, the control unit 70 controls the ultrasonic wave transmission section 17 to oscillate an ultrasonic wave from the ultrasonic wave oscillator 18. The ultrasonic wave oscillated by the ultrasonic wave oscillator 18 is propagated between the wafer holding surface 13 and the plastic placement surface 23 (i.e., the thermoplastic polymer P). The control unit 70 then receives, via the ultrasonic wave receiving section 34, a voltage corresponding to the amplitude of an ultrasonic vibration received by the ultrasonic wave receiver 33. From this received voltage, the control unit 70 derives a quantity of the amplitude of the ultrasonic vibration received by the ultrasonic wave receiver 33.Based on the amplitude of the ultrasonic vibration thus obtained, the control unit 70 determines whether the thermoplastic polymer P, which is clamped between the wafer holding surface 13 and the polymer placement surface 23, has become liquid and united (whether the thermoplastic polymer P has melted sufficiently) (removal step for polymer state).

[0038] Fig. Figure 6 shows a graph of an ultrasonic vibration received by the ultrasonic wave receiver 33. In this graph, the ordinate axis represents the amplitude (A), while the abscissa axis represents time (T). In a case where the thermoplastic material P has not become sufficiently liquid and has not been fully bonded, the ultrasonic vibration received by the ultrasonic wave receiver 33 has a comparatively small amplitude, as shown by the dashed line R0 in Figure 6. Fig. Figure 6 shows. On the other hand, in a case where the thermoplastic material P has been sufficiently liquefied and combined, the ultrasonic vibration received by the ultrasonic wave receiver 33 has a comparatively large amplitude, as shown by a solid line R1 in Fig. 6 is given.

[0039] Therefore, for example, in a case where the amplitude of the ultrasonic vibration received by the ultrasonic wave receiver 33 becomes equal to or greater than a predetermined value, the control unit 70 determines that the thermoplastic polymer P, which is clamped between the wafer holding surface 13 and the plastic placement surface 23, has melted and merged (liquefied).

[0040] In a case where it was determined that the thermoplastic polymer P, which was melted and merged between the wafer holding surface 13 and the polymer placement surface 23, is present, the control unit 70 controls the vertical movement mechanism 30 to press the merged thermoplastic polymer more firmly through the second surface Wb of the wafer W. As a result, as in Fig. Figure 7 shows that a molten plastic layer S of the molten and distributed thermoplastic polymer P is formed such that it covers the entire area of ​​the second surface Wb of the wafer W (distribution step).

[0041] The control unit 70 then controls the switch 27 (see Fig. 1) to cause the direct current from the direct current power source 28 to flow in the second direction in the opposite direction to the first direction in order to cool the upper surface 24a of the Peltier element 24, as indicated by an arrow D2 in Fig. 8. As a result, while the molten plastic layer S is forced through the second surface Wb of the wafer W, the control unit 70 cools the upper surface 24a of the Peltier element 24. By cooling the upper surface 24a in this way, the control unit 70 cools the plastic placement surface 23 and the molten plastic layer S at the plastic placement surface 23, thereby curing the molten plastic layer S. As a result, a protective element Sa (see Fig. 9), which contains the cured molten plastic layer S, is formed on the entire surface of the second surface Wb of the wafer W (cooling (curing) step). Note that in this case the lower surface 24b of the Peltier element 24 is heated.

[0042] Next, the control unit 70 controls the switch 27 to disconnect the DC power source 28 from the Peltier element 24. Then, the control unit 70 controls the vertical movement mechanism 30, which is located in Fig. Figure 1 shows how to move the wafer holding unit 10 upwards along the X-axis direction in order to distance the wafer holding unit 10 from the platform 20 (plastic placement surface 23), as shown in Fig. Figure 9 shows. In other words, the control unit 70 distances the protective element Sa, which is formed on the second surface Wb of the wafer W, away from the plastic placement surface 23. As a result, the control unit 70 is suitable for holding the wafer W, which has the protective element Sa on its second surface Wb, by the wafer holding surface 13 of the wafer holding unit 10 (distance step).

[0043] Subsequently, the control unit 70 holds the vacuum pump 7, which is located in Fig. As shown in Figure 1, the cover opening / closing mechanism 5 is activated and controls the cover opening / closing mechanism to open the cover 3 of the vacuum training chamber 2, thereby exposing the opening 4. As a result, the vacuum in the vacuum training chamber 2 will collapse.

[0044] Furthermore, the control unit 70 arranges the wafer conveying mechanism 40 so that it faces the wafer holding surface 13 of the wafer holding unit 10 and brings the wafer conveying mechanism 40 into contact with the protective element Sa, which covers the second surface Wb of the wafer W, as shown in Fig.Figure 10 is shown. Furthermore, the control unit 70 causes the wafer holding surface 13 of the wafer holding unit 10 to come into contact with the air supply source 14. As a result, the suction holding of the wafer W by the wafer holding surface 13 is released, and the wafer W is held by the wafer conveying mechanism 40.

[0045] The control unit 70 then moves the wafer in a +X direction, as indicated by an arrow E through the wafer conveying mechanism 40, to convey the wafer W out of the vacuum training chamber 2 through the opening 4 (wafer ejection step). Note that the wafer conveying mechanism 40 can hold the first surface Wa of the wafer W.

[0046] As described above, in the detection step for a plastic state of the present embodiment, ultrasonic vibration is propagated between the plastic placement surface 23 and the wafer holding surface 13, thereby detecting whether a thermoplastic P, clamped between the second surface Wb of the wafer W held by the wafer holding surface 13 and the plastic placement surface 23, has sufficiently melted and merged. Then, if it is detected that the thermoplastic P has merged, a distribution step is performed to spread the thermoplastic P over the entire area of ​​the second surface Wb of the wafer W by the wafer W. Therefore, in the present embodiment, distribution by pressing with the wafer W of the thermoplastic P, which has not been sufficiently melted, can be prevented.Additionally, pressure through the wafer W of the thermoplastic material P, which has not been sufficiently melted, and the resulting damage to the wafer W, can be suppressed. As a result, the thickness of the protective element Sa, which contains the thermoplastic material P formed on the second surface Wb of the wafer W, can be made essentially uniform.

[0047] Furthermore, in the heating step of the present embodiment, the upper surface 24a of the Peltier element 24 is heated, thereby heating the plastic placement surface 23 and the thermoplastic material P placed on it, in order to obtain the molten plastic layer S. In this case, the lower surface 24b of the Peltier element 24 is cooled, which improves the cooling effect of the plastic placement surface 23 in the subsequent cooling (curing) step. Therefore, the time required to form the protective element Sa on the second surface Wb of the wafer W by cooling and curing the molten plastic layer S (the time for the cooling (curing) step) can be reduced.

[0048] Note that in the heating and cooling steps of the present embodiment, the direct current is caused to flow through the Peltier element 24 to heat or cool the upper surface 24a of the Peltier element, thereby heating the granules of the thermoplastic P or cooling the molten plastic layer S. However, the configuration for such heating and cooling is not limited to the Peltier element 24. Instead of the Peltier element 24, another temperature adjustment device arranged on the platform 20 or the wafer holding unit 10 can be used.

[0049] Additionally, in the present embodiment, the load exerted on the wafer holding unit 10 when the wafer holding unit 10 and the platform 20 come into contact with each other through the wafer W and the molten plastic layer S is detected by the load detector 60, which is provided on the upper surface of the vacuum training chamber 2. Such a load detector can be provided in the wafer holding table 12 of the wafer holding unit 10 or in the plastic placement table 22 of the platform 20.

Claims

[1] A protective member forming method for forming a protective member on a surface on one side (Wb) of a wafer (W) by melting a thermoplastic resin (P), the protective member forming method comprising: a resin supplying step for arranging a plurality of grains of the thermoplastic resin (P) on a resin placing surface (23) of a platform (20); a wafer holding step of holding a surface on another side (Wa) of the wafer (W) by a wafer holding surface (13) of a wafer holding unit (10); a contact step of moving the wafer holding unit (10) and the platform (20) relative to each other in a direction so as to approach each other using a vertical moving mechanism (30) to bring the surface of one side (Wb) of the wafer (W) held by the wafer holding unit (10) into contact with the grains of the thermoplastic resin (P); a plastic state detecting step of heating the grains of the thermoplastic resin (P) in contact with the one-side surface (Wb) of the wafer (W) while propagating an ultrasonic vibration between the plastic placement surface (23) and the wafer holding surface (13), and detecting whether or not the thermoplastic resin (P) clamped between the one-side surface (Wb) of the wafer (W) held on the wafer holding surface (13) and the plastic placement surface (23) has been united; a distributing step of distributing the thermoplastic resin (P) detected as being combined in the resin state detecting step over an entire area of the surface on one side (Wb) of the wafer (W) through the wafer (W); and a curing step for cooling the thermoplastic material (P) which has been distributed in order to cure the thermoplastic material (P), wherein the protective member which protects the entire area of the surface on one side (Wb) of the wafer (W) is formed.

Citation Information

Patent Citations

  • Protection member formation device

    JP2017168565A

  • JP002017168565A