METHOD FOR PRODUCING LIQUID POWDER FROM A DRI PRODUCT
Patent Information
- Application Number
- DE502021005479
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-04-30
- Filing Date
- 2021-03-02
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2041-03-02
AI Technical Summary
Existing methods for producing liquid pig iron from directly reduced iron products are not optimized for energy efficiency and slag management, leading to suboptimal processes and environmental impacts.
A method involving the use of directly reduced iron products with specific iron and carbon content, combined with slag formers, in an electrically operated melting unit to produce a liquid pig iron phase and a granulable slag phase with adjusted basicity and viscosity, allowing for industrial application and reduced CO2 emissions.
The method enables the production of granulable slags that can be used in cement production, reducing fuel use and CO2 emissions, while maintaining the existing steel production route and allowing partial or complete replacement of blast furnace capacity without altering core metallurgical processes.
Description
[0001] The present invention relates to a method for producing liquid pig iron, in particular from a directly reduced iron product (DRI product) in a melting unit, a granulated slag and a plant for producing liquid pig iron.
[0002] Such processes and systems are generally known from the prior art. For example, WO 2017 / 207472 A1 discloses a process and a system for producing liquid pig iron from a directly reduced iron product (DRI) that is melted in an electric arc furnace (EAF). The DRI used has a high carbon content, which is present in the form of iron carbide and has a beneficial energetic effect on the molten bath. Furthermore, European patent applications EP 1 160 338 A1 and EP 1 160 337 A1 disclose a highly energy-efficient process for preheating and final reduction of a directly reduced iron product (DRI). This product is melted in an electric arc furnace (EAF), with the CO2-containing offgas generated during the melting process being reused in the process.
[0003] European patent application EP 1 298 224 A1 also discloses a process for producing liquid pig iron in which a directly reduced iron product is melted by arc heating. The arc heating primarily comprises radiant heating, which leads to an improved service life of the refractory material of the melting furnace. EP 1 437 420 A1 also discloses a process for producing liquid pig iron.
[0004] Another process for producing liquid pig iron is known from US Pat. No. 5,810,905. In this process, an iron-containing fine ore is first converted into iron carbide in a fluidized-bed reactor in the presence of hydrogen. This iron carbide is then fed into an electric arc furnace (SAF) and melted and liquefied to produce liquid pig iron.
[0005] Although various processes and plants for producing liquid pig iron from a directly reduced iron product are known from the state of the art, there is still a need for improved processes and plants.
[0006] Against this background, the present invention is therefore based on the object of specifying a method and a plant for producing liquid pig iron that is improved compared to the prior art.
[0007] According to the invention, the object is achieved by a method having the features of patent claim 1.
[0008] Further advantageous embodiments of the invention are specified in the dependent claims. The features listed individually in the dependent claims can be combined with one another in a technologically expedient manner and can define further embodiments of the invention. Furthermore, the features specified in the claims are further specified and explained in the description, where further preferred embodiments of the invention are presented.
[0009] According to a first aspect, the present invention relates to a process for producing liquid pig iron, comprising the steps: i) Providing a directly reduced iron product (DRI product) with an iron content of at least 75.0 wt.%, a carbon content of at least 0.10 wt.% and a content of acidic and basic slag components selected from the group comprising CaO, SiO 2 , MgO and Al 2 O 3 of a maximum of 15.0 wt.%, ii) Feeding the DRI product with the addition of slag formers into an electrically operated melting unit, iii) Feeding further iron and / or carbon components up to a proportion of 30 wt.% based on the amount of DRI product into the electrically operated melting unit, iv) Melting the DRI product and, if appropriate, the further iron and / or carbon components in the presence of the slag formers, so that a liquid pig iron phase and a liquid slag phase are formed, v) Adjusting the slag phase such that it has a basicity of (CaO+MgO / SiO 2 ) from 0.95 to 1.50, vi) tapping the liquid pig iron phase, and vii) tapping and granulating the slag phase. .
[0010] Surprisingly, it has been shown that by applying a slag analysis that is unusual for electrically operated melting units, such as EAF, SAF, or IF units, with a chemical composition similar to that of a blast furnace, granulatable slags can be obtained that are industrially usable. For example, these slags are a preferred product in cement production, as they reduce the use of fuels in cement production and thus significantly reduce CO2 emissions. The slags therefore do not require complex processing or even landfilling, but instead provide a market value that has an economically beneficial effect on the production process.
[0011] By producing liquid pig iron from the DRI product used and pursuing the desired slag operation, the existing process route for crude steel production in an integrated steelworks with blast furnace, hot metal desulfurization, and LD converter can be maintained. The particular advantage lies in the fact that the existing blast furnace capacity can be successively supplemented, partially, or completely replaced by the process according to the invention, with neither the core metallurgical processes nor the processes for treating by-products, such as blast furnace, desulfurization, and steelworks slag, requiring significant changes.
[0012] The DRI product can comprise directly reduced iron in the form of so-called premium "DR-grade pellets," or alternatively, iron from so-called blast furnace pellets with higher slag content, and / or mixtures thereof. Increasing the slag content increases the amount of slag in the melting unit. In a preferred embodiment, the directly reduced iron product (DRI product) has an iron content of at least 80.0 wt.%, more preferably at least 85.0 wt.%.
[0013] The slag constituents can vary depending on the ore quality and therefore constitute a maximum of 15.0 wt.%, preferably a maximum of 12.0 wt.%, in the DRI product used. However, the DRI product is not free of the slag constituents and preferably comprises them in a proportion of at least 2.0 wt.%, more preferably in a proportion of at least 4.0 wt.% in the DRI product used.
[0014] To obtain a granulatable slag, it must have the ability to vitrify, with vitrification generally being represented as a function of basicity and composition. According to the invention, the slag phase is therefore adjusted such that it has a basicity B3 of (CaO+MgO / SiO 2 ) of 0.95 to 1.50, preferably a basicity B3 of (CaO+MgO / SiO 2 ) of 1.0 to 1.40, more preferably a basicity B3 of (CaO+MgO / SiO 2 ) of 1.0 to 1.25.
[0015] To facilitate the granulation of the slag phase, the slag phase should advantageously exhibit specific flow behavior. It has proven preferable for the slag phase to be adjusted to a viscosity of 0.10 to 0.80 Pa*s, preferably a viscosity of 0.30 to 0.50 Pa*s. Viscosity can generally be described as a function of composition and temperature. In this context, it is therefore particularly preferred that the slag phase is tapped at a tapping temperature in the range of 1300°C to 1600°C, more preferably at a tapping temperature in the range of 1350°C to 1550°C, and most preferably at a tapping temperature in the range of 1400°C to 1500°C.
[0016] In a particularly preferred embodiment, the granulation is carried out as wet or dry granulation.
[0017] In a further advantageous embodiment, the slag-forming agents are added automatically via a process model integrated into a plant automation system, based on which the amount of slag-forming agents added is calculated and determined as a function of process parameters. The process model is advantageously based on mass and energy balances for the melt and slag. The automated addition ensures the necessary settings of the desired metal and / or slag parameters. For the complex slag system CaO, SiO 2 , MgO, Al 2 O 3 with its numerous crystalline mixed oxides, the process model can also include a suitable model for the thermodynamic description of the liquid slag phase, which describes the saturation limits with regard to the oxides and mixed oxides as a function of composition and temperature.
[0018] Advantageously, the slag formers are added to the melting process in quantities such that the flow properties and vitrification capacity required for successful granulation are achieved in the liquid slag phase. Particularly preferably, the slag formers according to step ii) can be added to the melting process in a proportion of up to a maximum of 15.0 wt.%, and very particularly preferably up to a maximum of 10.0 wt.%, based on the amount of DRI product added. The slag formers are preferably selected from the group comprising CaO, SiO 2 , MgO and / or Al 2 O 3 . If necessary, further mixed oxides, such as CaSiO 5 , Ca 2 Si 2 O 5 , Mg 2 SiO 4 , CaAl 2 O 4 , etc., can be added.
[0019] A particularly granulatable slag phase comprises a composition consisting of at least 70.0% by weight of the components CaO, MgO and SiO 2 .
[0020] In principle, the process is carried out with a mass fraction of 100% of the DRI product based on a batch. Alternatively, further iron and / or carbon components can be added to the process according to the invention per batch. If the addition of further iron and / or carbon components is provided, they are added according to step iii) up to a maximum proportion of 30.0 wt.%, preferably of a maximum of 25.0 wt.%, more preferably of a maximum of 20.0 wt.%, based on the amount of DRI product added. The further iron and / or carbon components are selected from the group comprising cold pig iron, batch coal, and / or steel scrap.
[0021] The directly reduced iron product (DRI product) can be added to the smelting unit in various forms. The directly reduced iron product (DRI product) is preferably fed to the smelting unit in hot form as a HDRI product (so-called hot DRI), in cold form as a CDRI product (so-called cold DRI), in hot briquette form as a HBI product (so-called hot briquetted DRI), and / or in particulate form, preferably with a maximum average particle diameter of 10.0 mm, more preferably with a maximum average particle diameter of 5.0 mm.
[0022] The DRI product produced in the direct reduction process typically has a carbon content between 0.50 and 6.0 wt.%. To achieve a pig iron-like analysis in the liquid pig iron phase, it may be necessary to carburize the liquid pig iron phase formed in step iv) to a carbon content of at least 2.50 wt.%. This can be achieved by adding cold pig iron or another carbon carrier to the smelting process. The liquid pig iron phase produced in the process is to be introduced into a conventional process route in the further process, for example, by feeding it to a pig iron desulfurization plant or a converter for further processing. Therefore, the carbon content must not exceed a maximum of 6.0 wt.%, more preferably a maximum of 4.50 wt.%.
[0023] The pig iron phase produced according to the process of the invention preferably has the following composition in wt.%: - Carbon content 2.50 - 5.0, more preferably 3.50 - 4.50, - Silicon 0.10 - 0.80, more preferably 0.20 - 0.50, - Manganese 0.50 - 5.0, more preferably 0.50 - 1.50, - and unavoidable impurities of sulphur and phosphorus of not more than 0.06 each, more preferably not more than 0.04 each.
[0024] The DRI product is preferably produced in a direct reduction plant as part of low-CO2 steel production and fed via a conveyor system to the melting unit and / or a thermally insulated bunker reservoir under a protective atmosphere. Both conventional natural gas-based reformer gas and hydrogen-enriched reformer gas with a hydrogen content of up to 100% can be used as the reducing gas. The hydrogen required for enrichment is preferably produced using green electricity, thus being CO2-neutral.
[0025] In a particularly preferred embodiment, the DRI product and / or the slag formers are fed to the melting unit from a preferably thermally insulated bunker reservoir. The DRI product temporarily stored in the bunker reservoir is stored in a protective gas atmosphere. Alternatively, the DRI product can be fed directly from the direct reduction plant via a conveyor system with metal conveyor belts to the melting unit and / or a thermally insulated bunker reservoir under a protective gas atmosphere. The DRI product has a temperature of 750 to 800 °C.
[0026] In a further unclaimed aspect, the present invention also relates to a granulated slag obtained by the process according to the invention. This slag has the following composition in wt. %: - SiO2 30.0 - 50.0, preferably 35.0 - 40.0 - CaO 25.0 - 50.0, preferably 30.0 - 43.0 - Al2O3 5.0 - 15.0, preferably 8.0 - 12.0 - MgO 2.0 - 15.0, preferably 4.0 - 12.0, - as well as unavoidable impurities selected from the group comprising iron (Fe), MnO 2 and / or sulfur (S).
[0027] Preferably, the iron content in the unavoidable impurities is a maximum of 2.0 wt%, more preferably 1.0 wt%.
[0028] Particularly preferably, the total proportion of the components SiO 2 , CaO and MgO in the granulated slag is at least 70.0 wt.%, more preferably 75.0 wt.%, even more preferably 80.0 wt.% and most preferably 85.0 wt.%.
[0029] The granulated slag produced according to the process of the invention is characterized by a glassy solidification content of at least 70.0 wt.%, preferably at least 90.0 wt.%, and more preferably at least 95.0 wt.%. A glass content of more than 90.0 wt.% is preferably achieved by wet granulation.
[0030] Advantageously, the granulated slag also has a total iron content (Fe) of a maximum of 2.0 wt%, preferably a total iron content (Fe) of a maximum of 1.0 wt%.
[0031] Depending on the application of the granulated slag, any minor components present in the eluates (chloride, sulfate, heavy metals, etc.) may also be important, as they are found in the environmental testing of suitability for use. In a preferred design variant, the granulated slag can therefore have an eluate classification parameter of 0 (unrestricted installation) or 1 (restricted open installation) according to the applicable legal guidelines (NGS - TR Soil of LAGA M20 from May 2013).
[0032] According to a further unclaimed aspect, the present invention also relates to a plant for producing liquid pig iron, comprising a direct reduction plant for producing a directly reduced iron product (DRI product), an electrically operated melting unit in which the directly reduced iron product (DRI product) can be melted, and a conveyor device via which the directly reduced iron product (DRI product) can be transported from the direct reduction plant to the melting unit.
[0033] The melting unit is preferably designed in the form of an electric arc furnace (EAF), a submerged arc furnace (SAF) or an induction furnace (IF).
[0034] The conveying device is preferably designed in the form of a metal conveyor belt and has a protective gas atmosphere.
[0035] Furthermore, the system advantageously has a thermally insulated bunker reservoir.
[0036] The invention and the technical environment are explained in more detail below with reference to the figures. It should be noted that the invention is not intended to be limited by the exemplary embodiments shown. In particular, unless explicitly stated otherwise, it is also possible to extract partial aspects of the facts explained in the figures and combine them with other components and findings from the present description and / or figures. In particular, it should be noted that the figures and in particular the illustrated proportions are only schematic. The same reference numerals denote the same objects, so that explanations from other figures can be used as a supplement if necessary. They show: Fig. 1 a schematic representation of a flow chart by means of which the method according to the invention is explained, Fig. 2a schematically simplified representation of a system according to a first embodiment, and Fig. 3 a schematically simplified representation of a system according to a second embodiment.
[0037] According to Figure 1 The method according to the invention is explained in a possible embodiment using a flow chart.
[0038] To produce liquid pig iron, a directly reduced iron product 1 (DRI product) is first provided, which in the embodiment shown here has an iron content of 80.0 wt.%, a carbon content of 3.0 wt.% and a content of acidic and basic slag components selected from the group comprising CaO, SiO 2 , MgO and Al 2 O 3 of a maximum of 12.0 wt.% and is in the form of a hot DRI product with a temperature of approx. 750 - 800 °C.
[0039] The DRI product 1 can, for example, be produced in a low-CO 2 steel production process in a direct reduction plant 11, as described in the Figures 2 and 3 is shown.
[0040] In a next step, the DRI product 1 is fed to an electrically operated melting unit 3 with the addition of slag formers 2. In the presently illustrated embodiment, the slag formers 2 are selected from the group comprising CaO, SiO 2 , MgO, and Al 2 O 3 and are added to the melting unit 3 in an amount of up to 10.0 wt.% based on the amount of DRI product fed in. The melting unit 3 is presently designed in the form of an electric arc furnace (EAF) and comprises at least one electrode 4, such as a carbon electrode.
[0041] The Figure 1The process described can, in principle, be carried out with a mass fraction of 100% of the DRI product based on a batch. However, in the illustrated embodiment, additional iron and / or carbon components 5 in the form of coal and steel scrap are added to the melting unit 3. In the present example, the mass fraction of the iron and carbon components 5 is 20.0 wt.% based on the amount of DRI product added.
[0042] The mixture of DRI product 1, slag former 2 and the iron and carbon components 5 is then melted using electric current to form a liquid pig iron phase 6 and a liquid slag phase 7.
[0043] By adding the slag formers 5, the slag phase 7 is adjusted such that, in the presently presented embodiment, it has a basicity B3 of (CaO+MgO / SiO 2 ) of 0.95 to 1.25 and a viscosity of 0.30 to 0.50 Pa*s. If these slag parameters are achieved, the slag phase 7 is tapped at a tapping temperature in the range of 1350 °C to 1550 °C and then granulated. In a final step, the liquid pig iron phase 6 is tapped and fed, for example, to a converter steelworks for further processing.
[0044] The tapped pig iron phase 6 has the following composition in wt.%: - Carbon content 3.50, - Silicon 0.3, - Manganese 0.50, - Remaining iron and unavoidable impurities of sulphur and phosphorus of maximum 0.04 each.
[0045] The tapped slag phase 7 is processed by wet granulation into a granulated slag 8, which has the following composition in wt.%: - SiO2 45.0, - CaO 40.0 - Al2O3 8.0, - MgO 5.0, - as well as unavoidable impurities including iron, MnO 2 and sulphur (S) totalling less than 2.0.
[0046] The granulated slag is characterized by a glassy solidification content of 95.0 wt.% and a total iron content (Fe) of less than 1.0 wt.%.
[0047] Figure 2 shows a schematically simplified representation of a system 10 according to a first embodiment variant.
[0048] The plant 10 for producing liquid pig iron comprises a direct reduction plant 11 for producing the directly reduced iron product 1. The direct reduction plant 11 comprises a first upper section, which forms a reduction shaft 12, and a second lower section, which forms a cooling section 13. Conventional reformer gas based on natural gas, coke gas, or other metallurgical gases, as well as hydrogen-enriched reformer gas with a maximum hydrogen content of up to 100%, can be used as the reducing gas. The required hydrogen is advantageously produced in a CO2-neutral manner from green electricity.
[0049] The DRI product 1 produced in the present direct reduction plant 11 can have a variable carbon content depending on the hydrogen content in the reduction gas. To achieve a pig iron-like analysis, the carbon content can be increased by deliberately injecting natural gas for cooling purposes into the lower cooling section 13.
[0050] Furthermore, the plant 10 comprises an electrically operated melting unit 3 in which the directly reduced iron product 1 (DRI product) can be melted, as well as a conveyor device 14 via which the directly reduced iron product 1 can be transported from the direct reduction plant 11 to the melting unit 3.
[0051] The melting unit 3 is in the form of an electric arc furnace (EAF).
[0052] The DRI product 1 produced in the direct reduction plant 11 can be fed directly to the melting unit 3 via the conveyor device 14, which in this case is designed in the form of a metal conveyor belt and has a protective gas atmosphere, as shown by the dashed line. Preferably, the DRI product 1 is first fed via the conveyor device 14 to a thermally insulated bunker reservoir 15 under a protective atmosphere, from which it is then fed, preferably automatically, to the melting unit 3.
[0053] In Figure 3 A schematically simplified representation of the system 10 in a second embodiment is shown. In contrast to the Figure 2In the embodiment shown, the melting unit 3 is designed in the form of a submerged arc furnace (SAF). This process is characterized in this case by the presence of a foamed slag phase 16 in the melting unit 3, which surrounds the electrode 4. List of reference symbols
[0054] 1Directly reduced iron product / DRI product 2Slag former 3Smelting unit 4Electrode 5Iron and / or carbon components 6Liquid pig iron phase 7Liquid slag phase 8Granulated slag 10Plant 11Direct reduction plant 12Reduction shaft 13Cooling section 14Conveying system 15Bunker reservoir 16Foamed slag
Claims
1. Method of producing liquid pig iron, comprising the steps: i) preparing a direct reduced iron product (1) (DRI product) with an iron content of at least 75.0 weight %, a carbon content of at least 0.10 weight % and a content of acidic and basic slag constituents, which is selected from the group comprising CaO, SiO2, MgO and Al2O3, of at most 15.0 weight %, ii) feeding the DRI product (1) with addition of slag formers (2) into an electrically operated smelting unit (3), iii) feeding further iron and / or carbon components (5) up to a proportion of 30 weight % referred to the DRI product quantity into the electrically operated smelting unit (3), iv) smelting the DRI product (1) as well as optionally the further iron and / or carbon components (5) in the presence of the slag formers (2) so that a liquid pig iron phase (6) and a liquid slag phase (7) are formed, v) setting the slag phase (7) in such a way that this has a basicity of (CaO + MgO / SiO2) of 0.95 to 1.5, vi) tapping the liquid pig iron phase (6) and vii) tapping and granulating the slag phase (7).
2. Method according to claim 1, wherein the slag phase (7) is set so that this has a basicity of (CaO + MgO / SiO2) of 1.0 to 1.40, preferably a basicity of (CaO + MgO / SiO2) of 1.0 to 1.25.
3. Method according to any one of the preceding claims, wherein the slag phase (7) is tapped at a tap temperature in range of 1300° C to 1600° C.
4. Method according to any one of the preceding claims, wherein the slag formers (2) are selected from the group comprising CaO, SiO2, MgO, Al2O3 and / or mixed oxides thereof.
5. Method according to any one of the preceding claims, wherein the slag formers (2) are fed according to step ii) up to a proportion of at most 15.0 weight %, preferably at most 10.0 weight %, referred to the fed DRI product quantity.
6. Method according to any one of the preceding claims, wherein the iron and / or carbon components (5) are fed according to step iii) up to a proportion of at most 30.0 weight %, preferably at most 25.0 weight %, more preferably at most 20.0 weight %, referred to the fed DRI product quantity.
7. Method according to any one of the preceding claims, wherein the granulation is undertaken as wet granulation or dry granulation.
8. Method according to any one of the preceding claims, wherein the addition of the slag formers (2) is carried out automatically by way of a process model which is integrated in a plant automation system and on the basis of which the addition quantity of the slag formers (2) is calculated and is fixed as a function of process parameters.
9. Method according to any one of the preceding claims, wherein the direct reduced iron product (1) is fed to the smelting unit (3) in hot form as HDRI product, in cold form as CDRI product, in hot briquette form as HBI product and / or in particulate form, preferably with a mean particle diameter of at most 10.0 mm.
10. Method according to any one of the preceding claims, wherein the liquid pig iron phase (6) formed in accordance with step iv) is carburised to a carbon content of at least 2.50 weight %.
11. Method according to any one of the preceding claims, wherein the DRI product (1) and / or the slag formers (2) is or are fed to the smelting unit (3) from a bunker reservoir (15), which is preferably thermally insulated.
12. Method according to any one of the preceding claims, wherein the DRI product (1) is produced in a direct reduction plant (11) and fed by way of a conveyor device (14) to the smelting unit (3) and / or to the bunker reservoir (15) under a protective atmosphere.