PERMANENTLY EXCEEDED DYNAMOELECTRIC MACHINE
Patent Information
- Application Number
- DE502022002016
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-09-16
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2042-09-16
AI Technical Summary
Existing permanently excited dynamoelectric machines face challenges in achieving high dynamics while balancing small magnet volume and material costs, with expensive neodymium iron boron magnets being required for dynamic behavior.
The use of CeFeB magnets with a special motor structure, where permanent magnets have a north and north direction facing the gap, and a magnet dimension between 1/10 to 1/3 of the rotor diameter, combined with a material composition and production methods that include powder metallurgy and rapid solidification, to achieve cost-effective high dynamics.
This configuration results in a motor with lower inductance, allowing quick current buildup and high torques, shifting the voltage limit characteristic to high torques, thereby enhancing motor dynamics and productivity, particularly in machine tools and robots.
Description
[0001] The invention relates to a permanently excited dynamoelectric machine, in particular a motor, with a stator and a rotor mounted so as to be rotatable about a longitudinal axis, wherein the stator has a winding system, wherein permanent magnets are arranged on the rotor, wherein the magnetic material of the permanent magnets has a preferred direction for the magnetization, so that paths through the permanent magnet can be defined in the direction of the respective local preferred direction, wherein a magnet dimension in the preferred direction assigned to a point on a pole face is defined as the path length from this point to a corresponding point on the other pole face along the preferred direction through the permanent magnet, wherein a gap is formed between the rotor and the stator, wherein the winding system is designed and arranged such that it interacts electromagnetically with the permanent magnets of the rotor via the gap.
[0002] From US 2004 / 150283 A1, a permanent magnet dynamo-electric machine is known, having a stator and a rotor, with a winding system and with permanent magnets on the rotor, wherein the permanent magnets on the rotor have a north and a south pole on the side facing the air gap.
[0003] A permanent magnet dynamoelectric machine of the type mentioned above is already known from WO 2006 / 064589 A1.
[0004] It is already known from DE 10 2012 211960 A1 to form permanent magnets based on CeFeB. This is also stated in the publication by SIEMENS AG: "Particularly fine-crystalline, sustainable permanent magnets for motor and generator applications, PRIOR ART PUBLISHING GMBH, PRIOR ART PUBLISHING GMBH, MANFRED-VON-RICHTHOFEN-STR. 9, 12101 BERLIN GERMANY, Vol. Prior Art Journal 2022 #12, June 15, 2022 (2022-06-15), pages 41-43, XP007024723." A permanent-magnet dynamoelectric machine of the type mentioned above is already known from DE 10 2019 131456 A1.
[0005] From JP 5 860654 B2, electrical machines are already known having a rotor with permanent magnets, each of which has a north pole and a south pole on the side facing the gap.
[0006] Background information on electrical machines having a rotor with permanent magnets can be found in JP 2018 038162 A.
[0007] In relevant permanent-magnet dynamoelectric machines, or PM motors, the dynamics are influenced by various factors. In addition to the inherent polar moment of inertia, the thermally permissible torque, the electrical time constant, the torque limit imposed by the motor voltage, and the saturation behavior of the magnetic circuit also have limiting effects.
[0008] The resulting dynamics are usually a design compromise between small magnet volume and material costs. By using expensive neodymium-iron-boron (NdFeB) magnets, which are characterized by their small volume, a dynamic motor behavior can be achieved.
[0009] Based on the problems and disadvantages of the prior art, the invention aims to create a more cost-effective solution for high dynamics.
[0010] To achieve the object according to the invention, a permanent-magnet dynamoelectric machine of the type defined above is proposed with the additional features of the characterizing part of independent claim 1. The respective dependent subclaims contain advantageous developments of the invention.
[0011] In the context of the invention, magnetic anisotropy describes the fact that magnetic materials can exhibit a preferred direction or plane of magnetization. A measure of magnetic anisotropy is the magnetic anisotropy energy, i.e., the work required to rotate the magnetization away from the preferred direction.
[0012] According to the invention, magnetic remanence – or remanence for short – describes the residual magnetism retained by the permanent magnet after removal of an external magnetic field. In this case, remanence describes precisely the residual magnetism when the permanent magnet has been exposed to the saturation flux density.
[0013] In the terminology of the invention, the magnetic coercive field strength refers to the magnetic field strength required to completely and permanently demagnetize a ferromagnetic substance previously charged to the saturation flux density, so that the resulting total flux or local flux density is zero. This field strength is usually denoted by the abbreviation jHc.
[0014] The invention solves the problem by combining the use of CeFeB magnets and a special motor design.
[0015] In detail, it is proposed according to the invention that the permanent magnets are designed as CeFeB-based magnets, wherein the permanent magnets extending at least in sections along the longitudinal axis are designed and arranged such that the individual permanent magnets each have a north and a south pole on the side facing the gap and the magnet dimension in the preferred direction, starting from the center of gravity of the north pole, is between 1 / 10 and 1 / 3 of the rotor diameter there.
[0016] A preferred embodiment provides for the rotor to have a diameter of, for example, 45 mm (+ / - 10%) in the area of the magnets, including the magnets. This results in the magnet dimensions in the preferred direction, based on the centroid of the north pole, between 4.5 mm and 15 mm. With a diameter of 90 mm (+ / - 10%), the magnet thickness, based on the centroid of the north pole, is between 9 mm and 30 mm.
[0017] Mischmetal, also known as cerium mischmetal, is a metal alloy made up of rare earth metals. Standard grades typically consist of at least 98% rare earth metals, 1% iron, and 0.8% magnesium. Since rare earth metals are very difficult to separate due to their close chemical similarity, it is more economical to use a mischmetal.
[0018] Iron-mischmetal alloys with an iron content of 15% to 50% are called cerium-iron or by the trade name Auermetall.
[0019] The percentage distribution of rare earth metals in the classic mischmetal results directly from that of the parent mineral monazite: it contains about 45 to 52% cerium, 20 to 27% lanthanum, 15 to 18% neodymium, 3 to 5% praseodymium, 1 to 3% samarium, terbium and yttrium, and traces of other rare earth metals.
[0020] A preferred development of the invention provides that the permanent magnets, in addition to technically unavoidable impurities, have a material composition based on the basic composition CeFeB+X+Z. The material contains between 20 wt.% and 35 wt.% cerium. The elements Nd, Pr, La, Y, Dy, Tb, Gd, Ho are each present in an amount of less than 10 wt.% and a total of less than <15 wt.%. In this case, the sum of the components Nd, Pr, La, Y, Dy, Tb, Gd, Ho and Ce is between 25 wt.% and 35 wt.%. Component Z is present in an amount of up to 6 wt.% and represents at least one of Al, Co, Cu, Ga, Si, Ge, each in an amount of a maximum of 3 wt.%. The element boron is present in an amount of between 0.85 wt.% and 1.1 wt.%. The element Fe is present in an amount of between 59 wt.% and 75 wt.% or forms the remainder of the composition.
[0021] According to an advantageous development of the invention, there are essentially two variants for producing the magnets.
[0022] A first variant - production via the "powder metallurgy route" or the "sintered magnet" involves the following process steps: Melting an alloy, pouring and solidifying the melt to a solid, preferably as a cast strip (or strip cast), so that the solid results in a strip, comminuting the solid to a particle size <10pm, preferably <5pm, aligning the particles in a magnetic field in order to set a preferred direction or a magnetic anisotropy, pressing, preferably so that shells or lenses with magnetic anisotropy are formed, sintering, heat treatment.
[0023] A second variant - production via the "rapid solidification route" or the "hot-press magnet" involves the following process steps: Melt the alloy, rapidly solidify by means of melt centrifugation to form a solid, hot press the solid, hot form the compact to adjust the preferential direction.
[0024] Rapid solidification is preferably carried out using a rapidly rotating copper wheel ("melt spinning"), which dissipates the heat quickly.
[0025] Optionally, both variants can be post-treated via grain boundary diffusion with at least one element from the group Nd, Pr, La, Y, Dy, Tb, Gd, Ho, Bo or alloys thereof.
[0026] Hot pressing, or hot isostatic pressing (HIP), is a development in manufacturing technology in which powder and, if necessary, other solid materials are simultaneously hot-pressed and sintered. It involves shaping by pressing and sintering ceramics in a single process.
[0027] In the second variant, hot forming of the compact is a forming step above the recrystallization temperature of the metals involved. The hardening that occurs during forming can be accompanied by recovery and softening processes that occur during and after the forming step. These processes include, in particular, rolling or pressing the workpiece.
[0028] It is particularly useful if the winding system of the machine is at least partially embedded in a material that forms a magnetic return path.
[0029] According to an advantageous development of the invention, the rotor can be designed as an internal rotor and the permanent magnets can be mounted radially on the outside of the rotor.
[0030] According to another advantageous development of the invention, the rotor can be designed as an external rotor and the permanent magnets can be arranged on an inner surface of the rotor facing the gap.
[0031] The advantages of the invention are particularly effective when the number of poles of the rotor magnets is less than or equal to 16. It is particularly preferred when the number of poles is less than or equal to 8. This can be verified by simulations.
[0032] An advantageous development of the invention provides that the permanent magnets have at least one of the following properties: the remanence is between 0.7T and 1.0T at room temperature, the magnetic coercive field strength (jHC) is between -450kA / m and -750kA / m at room temperature.
[0033] An advantageous development of the invention provides that the machine is designed and the permanent magnets are dimensioned and arranged in such a way that during operation of the machine the B-field amplitude of the fundamental wave in the gap is between 0.7T and 0.85T.
[0034] Another advantageous development of the invention provides that the permanent magnets, each of which has a north and a south pole on the side facing the gap, have a horseshoe-shaped, trapezoidal, or lens-shaped cross-sectional shape. If the permanent magnets are lens-shaped or bowl-shaped, it is ensured that, regardless of the number of poles of the rotor, the section of the permanent magnet facing away from the gap essentially follows the preferred magnetic direction. The lens shape achieves a constant cross-section of the permanent magnet for the field line path without having to use superfluous magnetic material. This helps to save mass, on the one hand to reduce mass inertia and improve dynamics, and on the other hand to keep the costs of magnets low.
[0035] An advantageous development of the invention further provides for the magnets to be segmented or assembled axially and / or radially and / or circumferentially—preferably at least partially glued together. This option, due to its modularity, offers considerable design flexibility and facilitates manufacturing. Alternatively, the permanent magnets can be formed integrally, at least radially and / or circumferentially, resulting in improved magnetic properties and reduced joints, eliminating mechanical weak points.
[0036] In the case of the option which provides that the permanent magnets each have a north and a south pole on the side facing the gap, it is expedient if the permanent magnets are each designed and attached to the rotor in such a way that the magnetic lines enter the rotor on the side of the gap at a first circumferential position, are deflected in such a way that they run tangentially in sections and the magnetic lines exit the rotor at a second circumferential position.
[0037] A preferred embodiment of the motor provides for the magnets that the magnets are preferably divided into axial segments of 3mm to 5mm and / or the magnet dimension in the preferred direction in the center of the pole is between 5mm and 12mm for bowl-shaped magnets and between 10mm and 25mm for lens-shaped, horseshoe-shaped (see Figure 2) magnets.
[0038] A preferred embodiment of the engine also provides for the engine design that: the number of poles is at most 16, particularly preferably 8 and / or the distance between the iron teeth of the stator and the rotor is 0.6mm to 1mm and / or the stator laminations preferably have a lamination thickness of less than 150µm and / or the slotted grooves between the teeth are present on all laminations.
[0039] The invention and the described further developments result in a permanent-magnet dynamoelectric machine with lower inductance. This allows the current to build up quickly, resulting in high dynamics. Furthermore, the voltage limit characteristic is shifted to high torques, which also increases the dynamics of the motor. The selected air gap induction enables high torques with the thermally permissible stator current. This also makes it possible to utilize the high dynamics over a long period of time. The stator current generates low armature reaction, so that the relationship between current and torque is linear up to high torques. This results in an improvement in the dynamics of the motor. The design according to the invention leads to a motor that increases the productivity of the application machine. This applies in particular to machine tools, robots, and production machines.
[0040] The invention is described in more detail below using specific embodiments for clarity. They show: Figure 1 a schematic, simplified cross-sectional view of a permanent magnet dynamoelectric machine, where Figure 1 only serves to facilitate understanding of the invention, Figure 2 is a schematic, simplified cross-sectional view of a first variant of a permanent magnet dynamoelectric machine according to the invention, Figure 3 is a schematic view of a first manufacturing method for the permanent magnets, Figure 4 is a schematic view of a second manufacturing method for the permanent magnets, Figure 5 is a schematic view of a simulation of the operation of a machine according to the invention, running on a computer - not according to the patent claim, computer program product.
[0041] Figures 1 and 2Each shows a schematic cross-sectional view of a permanent-magnet dynamoelectric machine PDM, with a stator STT and a rotor RTR mounted for rotation about a longitudinal axis X. The stator STT has a winding system WND. Permanent magnets PMG are arranged on the rotor RTR. A gap RGP is formed between the rotor RTR and the stator STT. The winding system WND is designed and arranged such that it interacts electromagnetically with the permanent magnets PMG of the rotor RTR via the gap RGP.
[0042] The PMG permanent magnets are designed as CeFeB-based magnets. They extend, at least in sections, along the longitudinal axis X. In this case, the PMG permanent magnets have a substantially constant cross-section along their axial extent.
[0043] The magnetic material of the permanent magnets PMG exhibits a preferred direction PFD for magnetization, so that paths through the permanent magnet PMG can be defined in the direction of the respective local preferred direction PFD. A magnet thickness MTH assigned to a point on a pole face PAR is thus defined as the path length from this point to a corresponding point on the other pole face along the preferred direction PFD through the permanent magnet PMG.
[0044] The WND winding system is embedded in a MTR material that forms a magnetic return path.
[0045] The rotor RTR is designed as an internal rotor, and the permanent magnets PMG are mounted radially on the outside of the rotor RTR. Alternatively, the rotor RTR can also be designed as an external rotor, in which case the permanent magnets PMG would be arranged on an inner surface of the rotor RTR facing the gap.
[0046] In Figure 1, which shows an example intended solely to facilitate understanding of the invention, the permanent magnets PMG enclose the rotor RTR opposite the gap RGP in a shell-like manner. The magnet thickness MTH in the preferred direction, starting from the centroid of the north pole, is between 1 / 10 and 1 / 5 of the rotor diameter there.
[0047] In Figure 2 The permanent magnets PMG each have a north pole NPL and a south pole SPL on the side facing the gap RGP. The magnet thickness MTH in the preferred direction, starting from the centroid of the north pole NPL, is between 1 / 10 and 1 / 3 of the rotor diameter at that location.
[0048] The PMG permanent magnets have the following properties: the remanence is between 0.7T and 1.0T at room temperature, the magnetic coercive field strength jHC is between -450kA / m and -750kA / m at room temperature.
[0049] The number of poles of the permanent magnets PMG on the rotor RTR facing the gap RGP is in the embodiment of the Figure 1 and in the Figure 2 eight each. Each North Pole NPL or South Pole SPL is bounded by the other pole. The poles are in the Figure 2 Each rotor is formed by two adjacent permanent magnets arranged in opposite directions. There are eight permanent magnets (PMGs) on the rotor.
[0050] During operation of the PDM machine, the B-field amplitude of the fundamental wave in the RGP gap is between 0.7T and 0.85T.
[0051] In addition to technically unavoidable impurities, the PMG permanent magnets consist of a material composition according to the pattern CeFeB+X+Z, consisting in detail of: ingredient Weight fraction Ce 20 wt% to 35 wt% where X consists of at least one element of Nd, Pr, La, Y, Dy, Tb, Gd, Ho each <10 wt% and in total <15 wt% where Ce+X 25 wt% to 35 wt% Z at least one element of Al, Co, Cu, Ga, Si, Ge each <3 wt% and total <6 wt% B 0.85 wt% to 1.1 wt% Fe rest
[0052] One in Figure 3The schematically illustrated first manufacturing process for permanent magnets PMG includes the following process steps: S1 melting an alloy, S2 pouring and solidifying the melt to a solid, preferably as a cast strip, so that the solid results in a ribbon, S3 crushing the solid to a particle size <10pm, preferably <5pm, S4 aligning the particles in a magnetic field to set a preferred direction, S5 pressing, S6 sintering, S7 heat treatment, S8 post-treatment via grain boundary diffusion with at least one element from the group Nd, Pr, La, Y, Dy, Tb, Gd, Ho, B or alloys thereof.
[0053] One in Figure 4 The schematically illustrated alternative second manufacturing process for permanent magnets PMG includes the following process steps: S1 melting the alloy, S2 rapid solidification by means of melt centrifugation to form a solid, S3 hot pressing of the solid, S4 hot forming of the compact to adjust the preferred direction, S5 post-treatment via grain boundary diffusion with at least one element from the group Nd, Pr, La, Y, Dy, Tb, Gd, Ho, B or alloys thereof.
[0054] Figure 5shows a schematic representation - not according to the patent claim - of a simulation SIM of a permanent-magnet dynamoelectric machine PDM according to the invention running on a computer CMP - here on several computers CMP of a network WWB comprising a cloud CLD. The software installed on the computers CMP is a computer program product CPP which, when executed on at least one computer CMP, enables the user to influence or configure and gain knowledge based on the executed simulation SIM via interfaces, e.g., via screen and keyboard, so that, in particular, technical design decisions can be supported and verified using the simulation. The simulation method and the computer program product are not part of the claimed invention.
[0055] Although the invention has been illustrated and described in detail by the preferred embodiment, the invention is not limited to the disclosed examples. Variations may be derived by those skilled in the art without departing from the scope of the invention as defined by the following claims.
Claims
1. Permanent-magnet dynamoelectric machine (PDM), comprising a stator (STT) and a rotor (RTR) mounted rotatably about a longitudinal axis (X), wherein the stator (STT) has a winding system (WND), wherein permanent magnets (PMG) are arranged on the rotor (RTR), wherein the magnetic material of the permanent magnets (PMG) has a preferred direction (PFD) for the magnetization, so that paths through the permanent magnet (PMG) can be defined in the direction of the local preferred direction (PFD) in each case, wherein a magnet dimension (MTH) in the preferred direction (PFD) assigned to a point on a pole face (PAR) is defined as the path length from this point to a corresponding point on the other pole face along the preferred direction (PFD) through the permanent magnet (PMG), wherein a gap (RGP) is formed between the rotor (RTR) and the stator (STT), wherein the winding system (WND) is designed and arranged such that it interacts electromagnetically with the permanent magnets (PMG) of the rotor (RTR) via the gap (RGP), wherein the permanent magnets (PMG) are designed as CeFeB-based magnets, wherein the permanent magnets (PMG) extending at least in portions along the longitudinal axis (X) are designed and arranged in such a way that the permanent magnets (PMG) each have a north pole (NPL) and a south pole (SPL) on the side facing the gap (RGP), characterized in that the magnet dimension (MTH) in the preferred direction (PFD), proceeding from the area centroid of the north pole, is between 1 / 10 and 1 / 3 of the rotor diameter there.
2. Machine (PDM) according to Claim 1, wherein the permanent magnets (PMG) have at least one of the following properties: - the remanence at room temperature is between 0.7 T and 1.0 T, - the magnetic coercive field strength (jHC) at room temperature is between -450 kA / m and -850 kA / m.
3. Machine (PDM) according to Claim 1 or 2, wherein during operation of the machine (PDM), the B-field amplitude of the fundamental wave in the gap (RGP) is between 0.7 T and 0.85 T.
4. Machine (PDM) according to at least one of the preceding claims, wherein the pole number of the permanent magnets (PMG) on the rotor (RTR) at the gap (RGP) is less than or equal to 16.
5. Machine (PDM) according to at least one of the preceding claims, wherein the permanent magnets (PMG) each having a north pole and a south pole on the side facing the gap (RGP) have a horseshoe-shaped, trapezium-shaped or lens-shaped crosssectional shape.
6. Machine (PDM) according to at least one of the preceding claims, wherein the permanent magnets (PMG) have, besides technically unavoidable impurities, a substance composition according to the pattern CeFeB+X+Z, consisting of: ConstituentProportion by weightCe20% by weight to 35% by weightwhere X consists at least of an element from Nd, Pr, La, Y, Dy, Tb, Gd, Hoin each case <10% by weight and in total <15% by weightwhere Ce+X25% by weight to 35% by weightZ is at least one element from Al, Co, Cu, Ga, Si, Gein each case <3% by weight and total <6% by weightB0.85% by weight to 1.1% by weightFeremainder7. Machine (PDM) according to at least one of the preceding claims, wherein the permanent magnets (PMG) are produced by means of the method steps of: - melting an alloy, - casting and solidifying the melt to form a solid body, preferably as Castrip, such that the resulting solid body is a strip, - comminuting the solid body to a particle size of <10 um, preferably <5 um, - aligning the particles in a magnetic field in order to set a preferred direction, - pressing, - sintering, - heat treatment.
8. Machine (PDM) according to at least one of the preceding Claims 1 - 6, wherein the permanent magnets (PMG) are produced by means of: - melting of alloy, - rapid solidification by means of melt spinning to form a solid body, - hot pressing of the solid body, - hot forming of the compact in order to set the preferred direction.
9. Machine (PDM) according to Claim 7 or 8, wherein the permanent magnets (PMG) are produced by means of the additional subsequent method step of: - aftertreatment by way of grain boundary diffusion with at least one element from the group Nd, Pr, La, Y, Dy, Tb, Gd, Ho, B or alloys thereof.