rear suspension of compound swing arms

ES3084042T3Undetermined Publication Date: 2026-11-10BENTELER AUTOMOBILTECHNIK GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
ES2024204235T
Authority / Receiving Office
ES · ES
Patent Type
Patents
Current Assignee / Owner
Priority Date
2023-10-12
Filing Date
2024-10-02
Publication Date
2026-11-10
Estimated Expiration
2044-10-02

AI Technical Summary

Technical Problem

Existing compound link axles face challenges in achieving deep weld penetration between torsion beams and side arms due to differences in wall thickness, leading to reduced service life and potential burn-through, without increasing weight or compromising driving dynamics.

Method used

A compound link axle design with a chamfered joining surface on the torsion profile, creating a V-shaped gap for deep weld penetration, ensuring the weld seam penetrates deeply into the torsion profile without causing burn-through, while maintaining the same weight and improving joint strength.

Benefits of technology

The design enhances the service life of the compound link axle by ensuring deep weld penetration and maintaining driving stability and comfort without increasing weight, thus improving load-bearing behavior.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000008_0000
    Figure 00000008_0000
  • Figure 00000008_0001
    Figure 00000008_0001
  • Figure 00000009_0000
    Figure 00000009_0000
Patent Text Reader

Abstract

The invention relates to a composite link shaft comprising two side arms 2 and a torsion profile 1. The torsion profile 1 is connected to each side arm 2 by a weld 8. At least in the weld area, the torsion profile 1 has a wall 3 with a thickness t1 greater than the thickness t2 of the wall 4 of the side arm 2. The torsion profile 1 has a joining surface 6 at each end 5, and each side arm 2 has a joining surface 7, wherein the torsion profile 1 and the side arms 3 are connected at their mutually facing joining surfaces 6 and 7 by a weld 8. The joining surface 6 at the end 5 of the torsion profile 1 has a chamfer 9. The joining space 11 formed between the joining surfaces 6 and 7 of the end 5 and the side arm 2 is V-shaped. This allows for a significantly increased penetration depth of the weld bead 8 in the torsion profile 1.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a compound link axle for motor vehicles according to the features in the preamble of claim 1.

[0002] A compound link axle features two torsionally and flexurally rigid side arms and a torsion profile extending transversely between them, which connects the side arms with torsional flexibility. A compound link axle is characterized by good lateral stability when cornering, as well as its compact size and low weight.

[0003] A compound link axle with a V-shaped torsion profile in cross-section is known, for example, from DE 27 359 39 C2 or EP 0 916 530 B1. The torsion profile is welded to the side arms.

[0004] Due to the high dynamic and static forces acting during operation, particularly longitudinal forces, the weld seam between the torsion profile and the side arms is subjected to high loads. Therefore, the strength and quality of the weld seams are of paramount importance. The penetration depth of a weld seam is closely related to the joint strength.

[0005] The torsion beam and the side arms often have different wall thicknesses. Typically, the torsion beam has a greater wall thickness than the side arms. When welding with a butt joint, it has been shown that, due to the difference in wall thickness between the torsion beam and the side arm, it is difficult to achieve deep weld penetration into the torsion beam without causing burn-through in the side arm. This reduced penetration can lead to a reduction in the service life of a compound link axle.

[0006] WO 2014 / 136261 A1 discloses a compound link axle according to the preamble of claim 1, which has two side arms and a torsion profile. The torsion profile has two side legs connected by a crown section. The torsion profile has a wall with a wall thickness of [missing value], and the side arms each have a wall with a wall thickness of [missing value], the wall thickness of the wall of the torsion profile being greater than the wall thickness of the wall of a side arm. The torsion profile has a joining surface at each end section. Likewise, the side arms each have a joining surface. The torsion profile and the side arms are each joined at their mutually facing joining surfaces by a weld.

[0007] According to WO 2021 / 170348 A1, a multi-point linkage for a motor vehicle chassis is considered state of the art. The multi-point linkage has at least a few straight profile sections that are spaced parallel to each other along their longitudinal extent and simultaneously decoupled from each other at their ends. Each profile section has an open cross-section that is at least substantially C-shaped or U-shaped. Each end of the profile section is connected to a hollow cylindrical joint via a weld, with the ends of the profile sections meeting the cylindrical outer circumferential surfaces of the hollow cylindrical joint in a manner that is at least substantially T-shaped. The weld is a fillet weld with a wedge-shaped cross-section.

[0008] The technological background of welding technology and the formation of weld seams includes the revelations in Fahrenwaldt Hans J.: In: "Praxiswissen Schweißtechnik: Werkstoffe, Prozesse, Fertigung", January 1, 2013, Springer Vieweg, XP093246871, page 499, as well as Beitz Wolfgang: "DUBBEL - Taschenbuch Für Den Maschinenbau" In: "DUBBEL - Taschenbuch Für Den Maschinenbau", December 31, 1997, Springer Berlin / Heidelberg, XP093246916.

[0009] Starting from the prior art, the invention is based on the objective of improving the load-bearing behavior and increasing the service life of a compound link axle without adversely increasing its weight.

[0010] According to the invention, the solution to this problem consists of a compound link axle according to the features of claim 1.

[0011] Advantageous embodiments and further developments of the compound link axle according to the invention are the subject of the dependent claims.

[0012] A compound link axle has two side arms and a torsion profile that connects the two side arms in a torsionally flexible manner. The torsion profile is connected to each side arm by a weld. The torsion profile has a wall with a specific thickness, and each side arm also has a wall with a specific thickness. The wall thickness of the torsion profile is greater than the wall thickness of a side arm in the weld area, at least in the area of ​​the weld. The torsion profile has a mating surface at each end section. Each side arm also has a mating surface. The torsion profile and the side arms are connected at their mating surfaces by a weld.

[0013] The joining surface has a chamfer at each end section of the torsion profile. This chamfer causes the end section to taper towards the end face of the torsion profile. The end sections of the torsion profile are prepared for welding. The joining surface is extended by the chamfered section and tapers towards the end of the end section. The chamfer on the joining surface of the end section results in a V-shaped gap between the joining surface at the end of the torsion profile and the joining surface on a side arm. The chamfer and the V-shaped gap allow for deep weld penetration in the torsion profile. "Penetration" refers to the depth of the molten zone in the base material, in this case, the steel of the torsion profile at the end section.

[0014] The penetration depth is typically between 2% and 10%. The invention also allows for higher penetration depths. The flank penetration length, i.e., the length of the molten area in which the welding filler material has bonded with the base material, is 70% to 90% of the wall thickness of the components, in particular the wall thickness of the torsion profile.

[0015] The invention creates a compound link axle with a longer service life without increasing the component weight. The advantageous driving dynamics characteristics, and thus the performance with maximum driving stability and comfort, are maintained.

[0016] The torsion profile and the side arms are aligned at an angle perpendicular to each other; in particular, the torsion profile abuts each side arm with a T-joint.

[0017] An advantageous embodiment provides that the end section of the torsion profile has a butt surface at its end face, wherein the butt surface runs essentially perpendicular to the longitudinal axis of the wall of the torsion profile. The butt surface at the end face forms part of the joining surface at the end section of the torsion profile. The torsion profile abuts the joining surface on the side arm with this butt surface.

[0018] The slope tapers off into the end face of the final section. The impact surface adjoins the slope.

[0019] The contact surface is significantly shorter than the length of the bevel. The contact surface extends parallel to the joining surface on a side arm.

[0020] The chamfer is particularly advantageous when created by machining. A torsion profile with its intended cross-section, such as a U-, V-, or round cross-section, can be used to manufacture the compound link axle. The end sections are then machined to create the chamfer.

[0021] In particular, the chamfer is provided in the areas of the impact edge where the greatest loads from external forces occur. In the case of the torsion profile of the compound link axle, the chamfer is provided, in particular, at the joining surfaces of the legs of the torsion profile. In the case of a U- or V-shaped torsion profile in cross-section, the chamfer is arranged on the inside of the cross-section, or on the outside of the cross-section, along the legs. The chamfer is provided on a partial section of the length of a leg of the torsion profile. According to the invention, the chamfer is provided in the lower longitudinal section of the leg and extends over 30% to a maximum of 75%, in particular approximately 50%, of the length of a leg.The tangential length of the ramp is measured in the cross-section of the torsion profile along its circumference and can extend over the entire circumference of the end face of the torsion profile. However, the tangential length of the ramp can also extend only over the length of one leg or be provided on a partial section of the length of a leg of a torsion profile.

[0022] In the areas or sections of the joining surface where no slope is provided, the joining surface of the torsion profile abuts the joining surface of a side arm.

[0023] The joining surface at the end section of the torsion profile is machined to create the chamfer. This involves removing material from the end section. This can be done, for example, by milling, turning, or grinding.

[0024] In particular, a wedge-shaped edge area is removed at the end of each end section of a torsion profile, creating the slope in the joining surface.

[0025] It is also possible to first process the end faces of a sheet steel blank and provide it with a bevel, after which the blank is then formed into a torsion profile and provided with its intended cross-section.

[0026] The slope runs at an angle to the longitudinal axis of the wall of the torsion profile; preferably, the angle is in a range between 25° and 60°. For practical purposes, an angle in the range of 30° to 45° is considered particularly advantageous.

[0027] The inclined section has an axial length greater than the wall thickness of the torsion profile at its end section. Specifically, the ratio of the inclined section's axial length to the wall thickness of the torsion profile is between 1:1 and 2:1. The axial length of the inclined section is measured along the longitudinal axis of the torsion profile wall.

[0028] The butt surface at the end face of the end section of an end profile has a width measured perpendicular to the longitudinal axis of the torsion profile wall. The width of the butt surface is significantly smaller than the wall thickness of the torsion profile wall; in particular, the wall thickness of the torsion profile wall is 3 to 6 times greater than the width of the butt surface. Accordingly, the ratio of the width of the butt surface to the wall thickness of the torsion profile wall in the end section is between 1:3 and 1:6.

[0029] Two side arms and a torsion beam are provided for the manufacture of the compound link axle. The components of the compound link axle are made of steel. The torsion beam and the side arms have different wall thicknesses, at least in the area of ​​the welded joint. This means, in particular, that the wall thickness of the torsion beam is greater than the wall thickness of one of the side arms. The torsion beam and the side arms are positioned at an angle to each other and joined by a weld.

[0030] To produce the torsion profile, a starting plate is provided, which has a wall with a specific thickness. A bevel is formed at the end section of the starting plate, and a butt surface is created on the end face of the end section.

[0031] The initial circuit board is formed into a torsion profile. During this forming step, the initial circuit board acquires, at least in certain areas, particularly along its length, a cross-sectional configuration of the torsion profile. Specifically, the initial circuit board is formed around its longitudinal axis and given the cross-section of the torsion profile, for example, a U- or V-shaped profile.

[0032] Furthermore, the two side arms are provided. The side arms have a wall with a thickness that differs from the wall thickness of the torsion profile.

[0033] The torsion profile and the side arms are aligned at an angle to each other, so that the joining surfaces of the torsion profile and the joining surfaces of the side arms face each other. The torsion profile and side arms are then joined by a weld seam at the joining surfaces.

[0034] The invention is explained in more detail below with reference to the drawings. These show: Figure 1 technically schematically and simplified a section of the wall of a torsion profile and a section of the wall of a side arm before a welding joint; Figure 2 the components according to the representation of the Figure 1 after the welding process; Figure 3 a compound link axle in a perspective view; Figure 4 a view of the front face of the end section of a torsion profile and Figure 5 a view of the front face of the end section of another embodiment of a torsion profile.

[0035] The Figures 1 and 2 The images show sections of components of a compound link axle for a motor vehicle. A compound link axle V in a perspective view is shown in the Figure 3A compound link axle V essentially comprises two wheel-guiding side arms 2 and a torsion profile 1 connecting the two side arms 2. The torsion profile is designated by reference numeral 1 and a side arm by reference numeral 2.

[0036] The torsion profile 1 has a wall 3 with a wall thickness t1. The side arm(s) 2 each have a wall 4 with a wall thickness t2. The wall thickness t1 of the wall 3 of the torsion profile 1 is greater than the wall thickness t2 of the wall 4 of the side arm 2.

[0037] The torsion profile 1 has a joining surface 6 at each end section 5. The side arms 2 also each have a joining surface 7. The torsion profile 1 and the side arms 2 are each connected at their mutually facing joining surfaces 6, 7 by a weld 8. The weld connection with the weld 8 is in the Figure 2 depicted.

[0038] The joining surface 6 at the end section 5 of the torsion profile 1 has a chamfer 9. The chamfer 9 is created by machining the end section 5. Due to the chamfer 9, the end section 5 tapers towards the end face 10 of the torsion profile 1.

[0039] To create the welded joint, the torsion profile 1 and the side arm(s) 2 are positioned relative to each other. This is shown in the illustration of the Figure 1 The joining surfaces 6, 7 face each other. A V-shaped joining gap 11 is formed between the joining surface 5 of the torsion profile 1 and the joining surface 6 of a side arm 2. The material-bonded connection is made via a weld seam, as in the Figure 2 The inclined plane 9 makes the weld seam 8 significantly more efficient; in particular, a component-optimized penetration in the torsion profile 1 can be achieved.

[0040] The end section 5 of the torsion profile 1 has a butt surface 12 at its end face. The butt surface 12 runs essentially perpendicular to the longitudinal axis L of the wall 3 of the torsion profile 1. The butt surface 12 is oriented parallel to the joining surface 6 of a side arm 2. At the deepest point of the V-shaped joining gap 11, a gap section parallel to and between the butt surface 12 and the joining surface 6 is formed.

[0041] The inclined plane 9 causes the end section 5 to taper at an acute angle α towards the end face 10. The inclined plane 9 ends at the end face 10. The contact surface 12 adjoins the inclined plane 9 at an obtuse angle.

[0042] The inclined plane 9 runs at an angle α to the longitudinal axis L of the wall 3 of the torsion profile 1. In the illustrated embodiment, the angle α is approximately 30°.

[0043] The inclined surface has an axial length l. The axial length l is greater than the wall thickness t1 of wall 3 of the torsion profile 1. The ratio of the axial length l of the inclined surface 9 to the wall thickness t1 of wall 3 of the torsion profile 1 can be between 1:1 and 2:1.

[0044] The impact surface 12 has a significantly smaller width b compared to the wall thickness t1 of the wall 3 of the torsion profile 1. The width b of the impact surface 12 is measured perpendicular to the longitudinal axis L of the wall 3 of the torsion profile 1. The ratio of the width b of the impact surface 12 to the wall thickness t1 of the wall 3 of the torsion profile 1 can be between 1:3 and 1:6. In a particularly advantageous practical embodiment of the compound link axle according to the invention, the width b of the impact surface 12 is 1 mm to 3 mm, inclusive.

[0045] The weld preparation and the formation of the chamfer 9 in the joining surface 6 at the end section 5 of the torsion profile 1, as well as the V-shaped configuration of the joining gap 11, result in a welded joint between the torsion profile 1 and the side arm 2 with a quality that meets the requirements. The penetration depth of the weld 8 on the torsion profile 1 can be significantly increased without causing burn-through on the side arm 2. The weld 8 meets the highest strength requirements, with the result that the service life of the compound link axle can be increased without any adverse increase in weight.

[0046] The Figure 3 Figure 1 shows a compound link axle V. The torsion profile 1 abuts a side arm 2 at a T-joint. The torsion profile 1 has a wall 3 (see Figure 3). Figures 1 and 2) and has a U-shaped cross-sectional profile with two side legs 13, which are connected via a vertex section 14. The end section 5 of the torsion profile 1 abuts the wall 4 of a side arm 2. The joining surface 6 at the end section 5 of the torsion profile 1 is adapted to the outer contour of the side arm 2 and is curved in an arc.

[0047] Arrow P1 schematically illustrates the tangential length of a side leg 13 with which the end section 5 of the torsion profile 1 abuts the outer circumference of the side arm 2. This length, relative to the circumference of the side arm 2, which has a round cross-section, is approximately 180° + / - 15°.

[0048] Arrow P2 indicates the length of the longitudinal section 15 in which the bevel 9 is provided on the inside of a leg 13 of the torsion profile 1. The bevel 9 is located in the lower longitudinal section 15 of the side leg 13. The bevel 9 extends over 30% to 75%, specifically approximately half the length of a side leg 13. With respect to the cross-section of a side arm 2, the bevel 9 extends over a circumferential section of approximately 90° ± 15°. The bevel 9 is located in the lower longitudinal section 15 of a side leg 13, starting from the free end of the leg.

[0049] The Figure 4 Figure 1 shows a front view of the joining surface 6 at an end section 5 of a torsion profile 1. The torsion profile 1 has a wall 3 with a wall thickness t1. A chamfer 9 is provided in the joining surface 6 at the end section 5 of the torsion profile 1. The chamfer 9 runs on the inside of the side leg 13 of the torsion profile 1.

[0050] The inclined plane 9 is provided in the lower longitudinal section 15 of the side leg 13 extending from the free leg end. The tangential length of the longitudinal section 15 is indicated by the arrow P2. In the illustrated embodiment, the inclined plane 9 extends approximately over half the length of a side leg 13.

[0051] The Figure 5 Figure 1 shows a front view of the joining surface 6 in an alternative embodiment on the end section 5 of a torsion profile 1. Unlike the embodiment according to the Figure 4 Here, the inclined plane 9 is arranged on the outside of the side legs 13 of the torsion profile. As in the other embodiments, the inclined plane 9 is produced by machining. The inclined plane 9 extends along a lower longitudinal section 15 of each side leg 13, starting from the free end of the leg. Otherwise, the embodiment corresponds to that of Figure 4 and the accompanying description. Reference symbol:

[0052] 1 - Torsion profile 2 - Side arm 3 - Wall of the torsion profile 4 - Wall of the side arm 5 - End section 6 - Joining surface 7 - Joining surface 8 - Weld seam 9 - Bevel 10 - End face 11 - Joining gap 12 - Butt surface 13 - Side leg 14 - Apex section 15 - Longitudinal section of 13 b -width L -longitudinal axis l -length t1 -wall thickness to 3 t2 -wall thickness to 4 α -angle P1 -arrow P2 -arrow

Claims

1. Torsion-beam rear axle comprising two side arms (2) and a torsion profile (1), wherein the torsion profile (1) has a wall (3) with a wall thickness (t1), and the side arms (2) each have a wall (4) with a wall thickness (t2), wherein the wall thickness (t1) of the wall (3) of the torsion profile (1) is greater than the wall thickness (t2) of the wall (4) of a side arm (2), and the torsion profile (1) has a joining surface (6) at each end section (5), and the side arms (2) each have a joining surface (7), wherein the torsion profile (1) and the side arms (2) are each connected at their mutually facing joining surfaces (6, 7) by a weld seam (8), and the torsion profile (1) has two side legs (13) which are connected by a vertex section (14), characterized in that the joining surface (6) at the end section (5) of the torsion profile (1) has an inclined portion (9), wherein the inclined portion (9) is provided in the lower longitudinal section (15) of a side leg (13) and extends over 30% to a maximum of 75% of the length of a side leg (13).

2. Torsion-beam rear axle according to claim 1, characterized in that the end section (5) of the torsion profile (1) has an end-face abutment surface (12), wherein the abutment surface (12) extends substantially at right angles to the longitudinal axis (L) of the wall (3) of the torsion profile (1).

3. Torsion-beam rear axle according to claim 2, characterized in that the abutment surface (12) adjoins the inclined portion (9).

4. Torsion-beam rear axle according to any one of claims 1 to 3, characterized in that the inclined portion (9) is produced by machining.

5. Torsion-beam rear axle according to any one of claims 1 to 4, characterized in that the inclined portion (9) extends at an angle (α) of 25° to 60°, in particular 30° to 45°, relative to the longitudinal axis (L) of the wall (3) of the torsion profile (1).

6. Torsion-beam rear axle according to any one of claims 1 to 5, characterized in that the inclined portion (9) has an axial length (I), and the ratio of the axial length (l) of the inclined portion (9) to the wall thickness (t1) of the wall (3) of the torsion profile (1) is between 1:1 and 2:1.

7. Torsion-beam rear axle according to any one of claims 2 to 6, characterized in that the abutment surface (12) has a width (b) measured perpendicular to the longitudinal axis (L) of the wall (3) of the torsion profile (1), and the ratio of the width (b) of the abutment surface (12) to the wall thickness (t1) of the wall (3) of the torsion profile (1) is between 1:3 and 1:6.

8. Torsion-beam rear axle according to any one of claims 1 to 7, characterized in that the inclined portion (9) is provided in a longitudinal section (15) extending from the free leg end of a leg (13) of the torsion profile (1).