Printable ultra-violet light emitting diode curable electrolyte for thin-film battery
Patent Information
- Application Number
- JP2021183115
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-11-11
- Filing Date
- 2021-11-10
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2041-11-10
AI Technical Summary
Existing thin film batteries face issues with leakage, reduced flexibility, and poor sealing due to solution-based electrolyte layers, and require an inert atmosphere for curing, which complicates the manufacturing process.
The use of a UV LED curable electrolyte layer formulation that forms a solid gel, allowing curing in air and eliminating the need for an inert environment, while also curing much faster than traditional methods.
The UV LED curable electrolyte layer addresses leakage and sealing issues, enabling faster manufacturing and flexibility in thin film batteries without the need for additional atmospheric controls.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical Field
[0001] The present disclosure generally relates to printed thin film batteries, and more specifically to printable ultraviolet (UV) light emitting diode (LED) curable electrolytes for thin film batteries.
Background Art
[0002] Batteries are used to power portable devices. Batteries generally include a cathode, an anode, and a liquid electrolyte. Batteries can be of various shapes, sizes, and voltages.
[0003] Thin film batteries are a recent development in battery technology. Thin film batteries use a series of layers deposited with high fidelity and precision. Printable thin film batteries enable new form factors and power sources for applications such as, for example, the Internet of Things (IoT), wearables, and sensors.
Summary of the Invention
Problems to be Solved by the Invention
[0004] According to aspects shown herein, an electrolyte for a printed thin film battery, a battery with the electrolyte, and a method for manufacturing a battery using the electrolyte are provided. One disclosed feature of an embodiment is a composition comprising an ultraviolet (UV) curable mixture of water, an acid, a phosphine oxide with one or more photoinitiators, a water-miscible polymer, a salt, and a neutralizing agent.
[0005] Another disclosed feature of an embodiment is a battery. The battery includes a cathode layer, an anode layer, and an electrolyte layer coupled to the cathode layer and the anode layer, and the electrolyte layer includes a crosslinked polymer and a phosphine oxide.
[0006] Another feature of the embodiment is a method. The method comprises printing a cathode layer, distributing an electrolyte layer precursor composition onto the cathode layer, wherein the electrolyte layer precursor composition comprises water, an acid, a phosphine oxide with one or more photoinitiators, a water-miscible polymer, a salt, a neutralizing agent, and a crosslinking agent, ultraviolet curing the electrolyte layer precursor composition in the presence of air to form an electrolyte layer, printing an anode layer, and bonding the anode layer to the electrolyte layer. [Brief explanation of the drawing]
[0007] The teachings of this disclosure can be easily understood by considering the embodiments for carrying out the following invention in conjunction with the following accompanying drawings.
[0008] [Figure 1] Figure 1 shows a block diagram of an exemplary thin-film battery of the present disclosure.
[0009] [Figure 2] Figure 2 shows a block diagram of another example of the thin-film battery of this disclosure.
[0010] [Figure 3] Figure 3 shows exemplary compounds used to formulate the exemplary electrolytes of this disclosure.
[0011] [Figure 4] Figure 4 shows an exemplary process flow diagram for manufacturing a thin-film battery using the electrolyte of this disclosure.
[0012] [Figure 5] Figure 5 shows a flowchart illustrating an exemplary method for manufacturing a thin-film battery using the electrolyte of this disclosure.
[0013] To facilitate understanding, whenever possible, the same reference number is used to indicate the same element common to the drawings. [Modes for carrying out the invention]
[0014] This disclosure broadly discloses a printable UV LED-curable electrolyte for thin-film batteries and a method for manufacturing the same. As mentioned above, thin-film batteries are a recent development in battery technology. Thin-film batteries use a series of layers deposited with high fidelity and precision. Some thin-film batteries use paper layers immersed in a liquid electrolyte as the electrolyte layer. However, this can introduce complexity and further challenges when manufacturing a fully printed battery. Leakage, reduced flexibility, and poor sealing are problems with liquid electrolyte layers.
[0015] This disclosure provides formulations for curable gel electrolyte layers. The printable UV LED curable electrolyte layer is a gel form that can eliminate problems associated with leakage, reduced flexibility, and decreased sealing performance associated with the above-mentioned liquid electrolyte layers. Furthermore, the solid gel form of the cured electrolyte can eliminate the need for physical separators when liquid electrolytes are used.
[0016] Some UV-curable materials suffer from oxygen inhibition during curing. Oxygen inhibition can limit the effectiveness of curing, and more complex systems such as an inert blanket atmosphere (e.g., a nitrogen gas (N2) blanket) may be required. The UV LED-curable electrolyte layer formulations of this disclosure can be cured in air. Therefore, the need for an inert environment is eliminated.
[0017] Furthermore, the UV LED curable electrolyte layer of this disclosure can cure much faster than other electrolyte layer formulations. For example, the UV LED curable electrolyte layer of this disclosure can cure in seconds rather than minutes. This can also improve the speed of the manufacturing process.
[0018] Figure 1 shows an exemplary thin-film printed battery 100 (also referred to herein as battery 100) of the present disclosure. In one embodiment, each layer of battery 100 may be printed (e.g., via a three-dimensional (3D) printer). Battery 100 may be made of a material or in dimensions that allows battery 100 to be flexible.
[0019] In one embodiment, the battery 100 may include a cathode current collector 102, a cathode layer 104, an electrolyte layer 106 of the present disclosure, an anode layer 108, and an anode current collector 110. In one embodiment, the electrolyte layer 106 may be located between the cathode layer 104 and the anode layer 108. In other words, the battery 100 may be manufactured such that the electrolyte layer 106 is formed on top of the cathode layer 104 and the anode layer 108 is formed on top of the electrolyte layer 106, or vice versa.
[0020] In one embodiment, the cathode current collector 102 and the anode current collector 110 may be manufactured from a conductive metal that can also be used as a material for 3D printing. For example, the cathode current collector 102 and the anode current collector 110 may be manufactured from silver (Ag).
[0021] In one embodiment, the cathode layer 104 and the anode layer 108 may also be printed using materials or compounds suitable for 3D printing. For example, the cathode layer 104 may be made using manganese oxide (MnO2), and the anode layer 108 may be made using zinc (Zn).
[0022] In one embodiment, the electrolyte layer 106 may be printed using a formulation capable of forming a curable gel electrolyte layer. The formulation may be printable in the presence of air and UV curable. In other words, the formulation of the electrolyte layer 106 can be cured in the presence of oxygen or ambient conditions. To put it another way, the formulation of the electrolyte layer 106 may be insensitive to oxygen inhibition or may not require the presence of an inert blanket atmosphere (e.g., nitrogen (N2) gas, argon, helium, etc.).
[0023] In addition, the formulation of the electrolyte layer 106 can cure much faster than previous electrolyte formulations. For example, the formulation of the electrolyte layer 106 can cure within seconds, as compared to other electrolyte formulations that cure in minutes. An example of the formulation of the electrolyte layer 106 is shown in FIG. 3 and is described in more detail below.
[0024] FIG. 2 shows another embodiment of an exemplary thin film printed battery 200 (also referred to herein as battery 200). In one embodiment, each layer of the battery 200 can be printed (e.g., via a 3D printer). The battery 200 can be made of a material or dimensions that allow the battery 200 to be flexible.
[0025] In one embodiment, the battery 200 can include a cathode current collector 202, a cathode layer 204, the electrolyte layer 206 of the present disclosure, an anode layer 208, and an anode current collector 210. In one embodiment, the cathode layer 204 and the anode layer 208 can be positioned in parallel. For example, the electrolyte layer 206 can be positioned above both the cathode layer 204 and the anode layer 208. Stated another way, the cathode layer 204 and the anode layer 208 can be bonded on the same side of the electrolyte layer 206 and positioned in parallel or adjacent to each other.
[0026] In one embodiment, the cathode current collector 202 and the anode current collector 210 can be manufactured from a conductive metal that can also be used as a material for 3D printing. For example, the cathode current collector 202 and the anode current collector 210 can be manufactured using silver (Ag).
[0027] In one embodiment, the cathode layer 204 and the anode layer 208 can also be printed using a material or compound that is compatible with a 3D printer. For example, the cathode layer 204 can be manufactured using manganese dioxide (MnO2), and the anode layer 208 can be manufactured using zinc (Zn).
[0028] In one embodiment, the electrolyte layer 206 may be printed using a formulation capable of forming a curable gel electrolyte layer. The formulation may be printable in the presence of air and may be UV curable. In other words, the formulation for the electrolyte layer 206 may be curable in the presence of oxygen or ambient conditions. To put it another way, the formulation for the electrolyte layer 206 may be insensitive to oxygen inhibition or may not require the presence of an inert blanket atmosphere (e.g., nitrogen (N2) gas, argon, helium, etc.).
[0029] In addition, the electrolyte layer 206 formulation can cure much faster than previous electrolyte formulations. For example, the electrolyte layer 206 formulation can cure within seconds, compared to other electrolyte formulations that cure in minutes. An example of a formulation for the electrolyte layer 206 is shown in Figure 3 and will be described in more detail below.
[0030] In one embodiment, the electrolyte layer 206 may be formed from an electrolyte layer precursor composition. The electrolyte layer precursor composition may include a UV-curable mixture of water, an acid, a phosphine oxide, a water-miscible polymer, a salt, and a neutralizing agent. In one embodiment, the formulation 300 may also include a crosslinking agent.
[0031] In one embodiment, examples of water-miscible polymers include polyethylene oxide (PEO), polyvinylpyrrolidone (PVP), polyvinyl alcohol (PVA), polyacrylamide, poly(2-alkyl-2-oxazoline), and polyphosphates. The water-miscible polymer used should have specific properties, such as good ion transport with a large amount of oxygen.
[0032] In one embodiment, the salt may be any type of ionic salt. In one embodiment, the ionic salt may be a chlorate or a bromate. For example, the salt may be ammonium chloride (NH4Cl), potassium chloride, sodium chloride, lithium chloride, ammonium bromide, potassium bromide, sodium bromide, and lithium bromide.
[0033] In one embodiment, examples of neutralizing agents include potassium hydroxide, lithium hydroxide, pyridine, and trimethylamine. The neutralizing agent may also be a base that produces a salt of the acid. For example, if the acid is acrylic acid and the neutralizing agent is potassium hydroxide, the neutralizing agent may produce a potassium salt of acrylic acid.
[0034] Figure 3 shows an exemplary formulation 300 of an electrolyte layer precursor composition that can be used to form the electrolyte layers 106 and 206 of the present disclosure. In one embodiment, formulation 300 may comprise water, acrylic acid 304, phosphine oxide 306 with one or more photoinitiators, polyethylene oxide (PEO) 312, ammonium chloride (NH4Cl) salt 308, potassium hydroxide (KOH) 310, and a crosslinking agent 314.
[0035] In one embodiment, the crosslinking agent 314 may be triethylene glycol divinyl ether (TEGDVE). In one embodiment, different variations of PEO 312 may be used depending on the formulation 300. For example, 10% by weight (10 wt%) of 600,000 molar volume of PEO, 5% by weight of 4,000,000 molar volume of PEO, or 12% by weight of 4,000,000 molar volume may be used in formulation 300.
[0036] In one embodiment, phosphine oxide 306 may be a long-wavelength UV absorbing photoinitiator that is typically oxygen-sensitive and does not exhibit good surface curing on its own. However, formulation 300 of the present disclosure comprises an additional compound with phosphine oxide 306, thereby enabling formulation 300 to cure rapidly (e.g., within a few seconds) under UV light-emitting diode light (e.g., wavelengths of about 395 nanometers (nm) to 405 nm) without surface inhibition.
[0037] In one embodiment, phosphine oxide 306 may be bisacylphosphine oxide (BAPO) or monoacylphosphine oxide (MAPO). Examples of BAPO 306 may be compounds identified by their trademark names Omnirad819 or Irgacure819. MAPO may be Lucrin TPO (trimethylbenzoylphosphine oxide, CAS number 75980-60-8), Lucrin TPO-L (ethyl(2,4,6-trimethylbenzoyl)phenylphosphineate, CAS number 84434-11-7), etc.
[0038] In one embodiment, the formulation 300 may vary in the amounts of water 302, acrylic acid 304, BAPO 306, PEO 312, NH4Cl salt 308, KOH 310, and crosslinking agent 314. The amount of formulation 300 distributed as the electrolyte layer 106 of battery 100 or 200 may vary in weight from about 16 grams (g) to 100 g. In one embodiment, water 302 may constitute 31% to 37% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, acrylic acid 304 may constitute about 8% to 11% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, BAPO 306 may constitute 7% to 15% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, NH4Cl salt 308 may constitute 2% to 20% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, KOH310 may constitute 6% to 9% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, PEO312 may constitute 20% to 25% by weight of the total weight of the UV-curable mixture or formulation 300. In one embodiment, the crosslinking agent 314 may constitute 2% to 4% by weight of the total weight of the UV-curable mixture or formulation 300.
[0039] An exemplary composition of formulation 300 is provided below. The example was prepared by mixing the reagents in a glass vial with magnetic stirring. PEO312 was pre-dissolved in water 302 before addition. The mixture was stirred overnight and degassed for 15 minutes with a stream of N2 gas before use.
[0040] Example 1: [Table 1]
[0041] Example 2: [Table 2]
[0042] Example 3: [Table 3]
[0043] Example 4: [Table 4]
[0044] Example 5: [Table 5]
[0045] Example 6: [Table 6]
[0046] Example 7: [Table 7]
[0047] Figure 4 shows an exemplary process flow 400 for manufacturing the battery 100 of the present disclosure. However, it should be noted that the battery 200 can be similarly manufactured by printing the cathode layer 204 and the anode layer 208 in parallel on the electrolyte layer 206. The process flow 400 can be executed by various devices in a manufacturing environment under the control of a central control unit or processor. For example, the process flow 400 may use a 3D printer, UV LED curing equipment, and other devices to execute the various blocks of the process flow 400.
[0048] In block 402, the cathode current collector 102 can be printed. The cathode current collector 102 can be printed from a conductive metal such as Ag using a 3D printer.
[0049] In block 404, in one embodiment, the cathode layer 104 can be printed on the cathode current collector 102. The cathode current collector 104 can be printed from MnO2 using a 3D printer.
[0050] In block 406, the formulation 300 can be distributed onto the cathode layer 104. In one embodiment, the formulation 300 can be distributed via a 3D printer to a desired location on the cathode layer 104. In one embodiment, a well 420 can be placed (or formed) on the cathode layer 104 so as to contain the formulation 300 at a desired location on the cathode layer 104. The well 420 may consist of a glass spacer fastened around the cathode layer 104. The well 420 may then be covered with cellophane tape.
[0051] In one embodiment, the well 420 may be a stencil or may be manufactured in a specific shape. A rectangular well 420 is shown in Figure 4, but it should be noted that the well 420 may have any desired shape depending on the shape of the battery.
[0052] In one embodiment, a screen 422 may be used instead of the well 420. The formulation 300 is poured onto the screen 422 and flattened by a squeegee. The screen 422 can direct the formulation 300 to a desired position in the cathode layer 104.
[0053] In block 408, the electrolyte layer 106 may be formed by curing the formulation 300 deposited in block 406 through the well 420 or the screen 422. The formulation 300 may be cured using a UV LED 450. In one embodiment, the formulation 300 may be cured using a 14-watt (W) 395 nm LED light source. The formulation can be cured within 30 seconds using an exemplary UV LED light source with the well 420, or within 1 second using the screen 422. In one embodiment, block 408 may be repeated for multiple passes to cure the formulation 300.
[0054] In block 410, the anode layer 108 can be printed on top of the electrolyte layer 106. The anode layer 108 can be printed from Zn using a 3D printer.
[0055] In block 412, the anode current collector 110 can be printed. The anode current collector 110 can be printed using a 3D printer from a conductive material such as Ag.
[0056] While process flow 400 shows a specific sequence, it should be noted that process flow 400 can be executed in a different order. For example, the anode current collector 110 may be printed first, followed by the anode layer 108, and then blocks 406 and 408 may be executed. Subsequently, the cathode layer 104 may be printed, followed by the cathode current collector 102.
[0057] Figure 5 shows a flowchart of an exemplary method 500 for manufacturing a thin-film battery with the electrolyte of the present disclosure. In one embodiment, one or more blocks of method 500 may be executed by various tools or devices under the control of a central control unit or processor.
[0058] In block 502, method 500 begins. In block 504, method 500 prints an electrode layer. The electrode layer may be a cathode layer or an anode layer. In one embodiment, the cathode layer may be printed from manganese dioxide (MnO2). For example, a 3D printer may print a cathode layer on top of a cathode current collector printed from a conductive metal such as Ag. Any type of additional printing process or 3D printer may be used. For example, any type of 3D printing process such as fused deposition modeling (FDM), selective laser sintering (SLS), selective laser melting (SLM), or binder spraying may be used.
[0059] In one embodiment, the anode layer may be printed from zinc (Zn). For example, a 3D printer may print the anode layer on top of an anode current collector printed from a conductive metal such as Ag.
[0060] In block 506, method 500 distributes the electrolyte layer precursor composition onto a substrate. In one embodiment, the electrolyte layer precursor composition may comprise water, acid, phosphine oxide, water-miscible polymer, salt, neutralizing agent, and crosslinking agent. In one embodiment, the electrolyte precursor composition may comprise a mixture of water, acrylic acid, bisacylphosphine oxide (BAPO), polyethylene oxide (PEO), ammonium chloride (NH4Cl) salt, potassium hydroxide (KOH), and triethylene glycol divinyl ether (TEGDVE). In one embodiment, different variations of PEO may be used depending on the formulation 300. For example, 10% by weight (10 wt%) of 600,000 molar volume of PEO, 5% by weight of 4,000,000 molar volume of PEO, or 12% by weight of 4,000,000 molar volume may be used in the UV-curable mixture.
[0061] In one embodiment, BAPO may be a long-wavelength UV-absorbing photoinitiator that is typically oxygen-sensitive and does not exhibit good surface curing on its own. However, the UV-curable mixtures of the present disclosure include additional compounds with BAPO, thereby enabling the UV-curable mixture to cure rapidly (e.g., within a few seconds) under UV light-emitting diodes (e.g., at a wavelength of about 395 nanometers (nm)) without surface inhibition. In addition, sufficient loading of BAPO may be present to overcome the oxygen inhibition phenomenon. Examples of BAPO may be compounds identified by their trade names Omnirad819 or Irgacure819.
[0062] In one embodiment, the UV-curable mixture may vary in the amounts of water, acrylic acid, BAPO, PEO, NH4Cl salt, KOH, and crosslinking agent. The weight of the UV-curable mixture may vary from about 16 grams (g) to 100 g. In one embodiment, water may constitute 31% to 37% by weight of the total weight of the UV-curable mixture. In one embodiment, acrylic acid may constitute about 8% to 11% by weight of the total weight of the UV-curable mixture. In one embodiment, BAPO may constitute 7% to 15% by weight of the total weight of the UV-curable mixture. In one embodiment, NH4Cl salt may constitute 2% to 20% by weight of the total weight of the UV-curable mixture. In one embodiment, KOH may constitute 6% to 9% by weight of the total weight of the UV-curable mixture. In one embodiment, PEO may constitute 20% to 25% by weight of the total weight of the UV-curable mixture. In one embodiment, the crosslinking agent may constitute 2% to 4% by weight of the total weight of the UV-curable mixture. Examples of different mixtures are provided in Examples 1-7 above.
[0063] In block 508, method 500 cures the electrolyte layer precursor composition with ultraviolet (UV) light in the presence of air. For example, the electrolyte layer can be cured using a 14-watt (W) 395 nm LED light source. In addition, the electrolyte layer can be cured under ambient conditions in the presence of air or oxygen. In other words, curing does not use oxygen inhibition or curing in the presence of inert N2 gas. As a result, the curing process can be simplified.
[0064] In addition, the mixture forming the electrolyte layer can harden relatively quickly (for example, within a few seconds, within 30 seconds, or in less than a minute). As a result, the manufacturing speed can also be improved.
[0065] In one embodiment, UV light may also contribute to the polymerization of an acid (e.g., acrylic acid). Monomers of the acid (e.g., acrylic acid) are present in the electrolyte layer precursor composition and can then be polymerized to form an acid polymer (e.g., polyacrylic acid) during UV curing.
[0066] After the electrolyte layer is formed, the anode layer and cathode layer may be bonded to the electrolyte layer. For example, the electrode layer may be the cathode layer, and the anode layer may be bonded to the cathode layer, or vice versa. For example, the anode layer may be bonded to the top of the electrolyte layer such that the electrolyte layer is located between the anode layer and the cathode layer (e.g., battery 100).
[0067] In one embodiment, the anode layer may be coupled to the electrolyte layer on the same side as the cathode layer is coupled to the electrolyte layer. In other words, the anode layer may be coupled to the electrolyte layer in parallel with the cathode layer (e.g., battery 200). In block 510, method 500 ends.
[0068] It will be understood that variations of those disclosed above, as well as other features and functions, or substitutes thereof, may be combined into many other different systems or applications. Various currently unforeseen or unprecedented substitutes, modifications, variations, or improvements may subsequently be made by those skilled in the art, and these are also intended to be covered by the following claims.
Claims
1. 1. A composition comprising: an ultraviolet (UV) curable mixture comprising water, an acid, a phosphine oxide, a water-miscible polymer, a salt, and a neutralizing agent; and a crosslinker comprising triethylene glycol divinyl ether (TEGDVE).
2. The composition of claim 1, wherein the crosslinker comprises from 2% to 4% by weight of the total weight of the UV curable mixture.
3. The composition of claim 1 , wherein the water-miscible polymer comprises polyethylene oxide (PEO).
4. 4. The composition of claim 3, wherein the PEO comprises at least one of ten percent by weight (10 wt%) of the 600,000 molar volume PEO, five percent by weight of the 4,000,000 molar volume PEO, or twelve percent by weight of the 4,000,000 molar volume PEO.
5. The composition of claim 1 , wherein the water comprises from 31% to 37% by weight of the total weight of the UV curable mixture.
6. The composition of claim 1 , wherein the acid comprises from 8% to 11% by weight of the total weight of the UV curable mixture.
7. 2. The composition of claim 1, wherein the phosphine oxide comprises one or more photoinitiators and comprises a bisacylphosphine oxide (BAPO) or a monoacylphosphine oxide (MAPO).
8. 8. The composition of claim 7, wherein the phosphine oxide comprises BAPO in an amount of 7% to 15% by weight of the total weight of the UV curable mixture.
9. The composition of claim 1, wherein the water-miscible polymer comprises 20% to 25% by weight of the total weight of the UV curable mixture.
10. The salt is ammonium chloride (NH 4 The composition of claim 1 comprising a salt of 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 2
11. The composition of claim 1, wherein the neutralizing agent comprises potassium hydroxide (KOH) in an amount of 6% to 9% by weight of the total weight of the UV curable mixture.
12. A battery, A cathode layer; and an anode layer; and an electrolyte layer coupled to the cathode layer and the anode layer, the electrolyte layer comprising a crosslinked polymer and a phosphine oxide, the crosslinked polymer being formed from a mixture of water, an acid, the phosphine oxide with one or more photoinitiators, a water-miscible polymer, a salt, a neutralizing agent, and a crosslinker comprising triethylene glycol divinyl ether (TEGDVE) that is consumed during curing under UV light to form the electrolyte layer.
13. 13. The battery of claim 12, wherein the electrolyte layer is located between the cathode layer and the anode layer.
14. 13. The battery of claim 12, wherein the cathode layer and the anode layer are positioned side-by-side on the electrolyte layer.
15. 13. The battery of claim 12, wherein the phosphine oxide comprises a bisacylphosphine oxide (BAPO) or a monoacylphosphine oxide (MAPO).
16. 1. A method comprising: Printing an electrode layer; dispensing an electrolyte layer precursor composition onto the electrode layer, the electrolyte layer precursor composition comprising water, an acid, a phosphine oxide, a water-miscible polymer, a salt, a neutralizing agent, and a crosslinker comprising triethylene glycol divinyl ether (TEGDVE); and UV curing the electrolyte layer precursor composition in the presence of air to form an electrolyte layer.
17. The method of claim 15 , wherein the electrode layer comprises a printed cathode layer or anode layer, and the anode layer is laminated onto the electrode layer.
18. 16. The method of claim 15, wherein the electrode layer includes a printed cathode layer and a printed anode layer is bonded to the electrolyte layer on the same side of the electrolyte layer that is bonded to the cathode layer.