Solid-state battery and fiber

By integrating fibers coated with a solid electrolyte at the interfaces of solid electrolyte and electrode layers, the bonding strength and ionic conductivity are enhanced, addressing the limitations of van der Waals forces and reducing material costs in solid batteries.

JP2024134669APending Publication Date: 2024-10-04HONDA MOTOR CO LTD

Patent Information

Application Number
JP2023044984
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

The bonding force at the interface between the solid electrolyte layer and the electrode layers in solid batteries is low, leading to challenges in increasing energy density, durability, and cost, due to reliance on van der Waals forces and the need for high restraining forces.

Method used

Incorporating fibers coated with a solid electrolyte at the interfaces between the solid electrolyte and electrode layers, which enhances bonding strength and ionic conductivity through mechanical anchoring and improved compatibility.

Benefits of technology

The use of coated fibers improves bonding strength and ionic conductivity at the interfaces, allowing for higher energy density and reduced material costs while maintaining durability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134669000001_ABST
    Figure 2024134669000001_ABST
Patent Text Reader

Abstract

To provide a solid-state battery which can improve the adhesion of an interface between a solid electrolyte layer and an electrode layer, and ion conductivity.SOLUTION: There is provided a solid-state battery which includes a positive electrode layer containing a positive electrode active material, a negative electrode layer, and a solid electrolyte layer containing a solid electrolyte and disposed between the positive electrode layer and the negative electrode layer. At least either of an interface between the positive electrode layer and the solid electrolyte layer, and an interface between the negative electrode layer and the solid electrolyte layer has a fiber coated by the solid electrolyte.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a solid-state battery and a fiber. [Background technology]

[0002] In recent years, research and development into secondary batteries that contribute to energy efficiency has been conducted in order to ensure that more people have access to affordable, reliable, sustainable and advanced energy.

[0003] As such secondary batteries, solid-state batteries such as lithium ion secondary batteries in which a solid electrolyte layer is disposed between a positive electrode layer and a negative electrode layer are known.

[0004] As a solid-state battery, a technology has been disclosed in which, in a battery having a gelled or solid electrolyte, the electrolyte contains inorganic particles having oxidation resistance and heat resistance, thereby improving the oxidation resistance and heat resistance of a surface layer facing a positive electrode member (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent No. 6683259 Summary of the Invention [Problem to be solved by the invention]

[0006] However, the bonding strength of the interface between the solid electrolyte layer and the positive electrode layer or negative electrode layer (electrode layer) of a solid battery is relatively low because it depends almost entirely on van der Waals forces. This makes it difficult to increase the energy density of the battery by increasing the area, or the battery has low durability. Alternatively, a holding mechanism with high binding force is required, which increases the cost of the components and reduces the volumetric energy efficiency of the battery.

[0007] The present invention has been made in view of the above, and has an object to provide a solid-state battery capable of improving the bonding strength and ion conductivity at the interface between a solid electrolyte layer and an electrode layer. [Means for solving the problem]

[0008] (1) The present invention relates to a solid-state battery having a cathode layer containing a cathode active material, an anode layer, and a solid electrolyte layer containing a solid electrolyte and disposed between the cathode layer and the anode layer, wherein at least one of an interface between the cathode layer and the solid electrolyte layer and an interface between the anode layer and the solid electrolyte layer has fibers coated with a solid electrolyte.

[0009] According to the invention (1), a solid-state battery can be provided that can improve the bonding strength and ion conductivity at the interface between the solid electrolyte layer and the electrode layer.

[0010] (2) The solid-state battery according to (1), wherein the solid electrolyte covering the fibers is made of the same material as the solid electrolyte contained in the solid electrolyte layer.

[0011] According to the invention of (2), the compatibility between the fibers coated with the solid electrolyte and the solid electrolyte in the solid electrolyte layer is improved, and the dispersibility is improved, so that the bonding strength and ionic conductivity of the layers at the interface between the layers can be further improved.

[0012] (3) The solid-state battery according to (1), wherein the solid electrolyte covering the fibers has a higher Young's modulus than the solid electrolyte contained in the solid electrolyte layer.

[0013] According to the third aspect of the present invention, when a solid-state battery is formed, the solid electrolyte-coated fibers have an improved anchoring effect when penetrating into other layers through the interfaces of the layers, and therefore the bonding strength and ionic conductivity of the layers at the interfaces can be improved.

[0014] (4) The solid-state battery according to any one of (1) to (3), wherein the fibers have a higher Young's modulus than a solid electrolyte contained in the solid electrolyte layer.

[0015] According to the invention of (4), when forming a solid-state battery, the anchor effect when the fibers coated with the solid electrolyte penetrate into other layers through the interface between the layers is improved, and therefore the bonding strength and ionic conductivity of the layers at the interface between the layers can be further improved.

[0016] (5) The solid state battery according to any one of (1) to (4), wherein the solid electrolyte covering the fibers has an average particle size of 1 nm to 500 nm.

[0017] According to the invention of (5), the fibers can be covered more suitably than the solid electrolyte of the solid electrolyte layer.

[0018] (6) The solid-state battery according to claim 1 or 2, wherein the fibers penetrate into a plurality of layers adjacent to the interface.

[0019] According to the sixth aspect of the present invention, the fibers coated with the solid electrolyte penetrate into the adjacent layers through the interfaces of the layers, thereby exerting an anchor effect, thereby making it possible to further improve the bonding strength and ionic conductivity of the layers at the interfaces.

[0020] (7) The present invention also relates to a fiber coated with a solid electrolyte, which is used in a solid-state battery having a positive electrode layer containing a positive electrode active material, a negative electrode layer, and a solid electrolyte layer containing a solid electrolyte and disposed between the positive electrode layer and the negative electrode layer, for joining the positive electrode layer and the solid electrolyte layer, or the negative electrode layer and the solid electrolyte layer.

[0021] According to the seventh aspect of the present invention, a solid-state battery can be manufactured that can improve the bonding strength and ion conductivity at the interface between the solid electrolyte layer and the electrode layer. [Brief description of the drawings]

[0022] [Figure 1] 1 is a diagram showing a configuration of a solid-state battery according to an embodiment of the present invention; [Diagram 2]FIG. 2 is a diagram showing a fiber configuration according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] <Solid battery> Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a cross-sectional view showing a schematic configuration of a solid-state battery 1 according to this embodiment. As shown in Fig. 1, the solid-state battery 1 has an anode layer 10, a cathode layer 20, and a solid electrolyte layer 30 disposed between the anode layer 10 and the cathode layer 20. Fig. 1 shows a configuration in which each layer is stacked one by one, but the number of layers is not particularly limited.

[0024] The solid-state battery 1 may be, for example, an all-solid-state lithium ion battery having a solid electrolyte. As the solid-state battery 1, in particular, an all-solid-state lithium metal battery using lithium metal in the anode or an all-solid-state silicon anode lithium ion battery using silicon is preferable. Since these batteries are relatively large in expansion and contraction due to charging and discharging, the configuration of the present invention capable of improving the bonding strength between the solid electrolyte layer and the electrode layer is more effective.

[0025] (Negative electrode layer) The negative electrode layer 10 includes a negative electrode active material layer that essentially contains a negative electrode active material 11 and optionally contains a solid electrolyte 13, a conductive assistant 14, and the like, and a negative electrode current collector 12. In addition to the above, the negative electrode active material layer may contain a material known as an electrode material for a solid-state battery, such as a binder.

[0026] The negative electrode active material 11 is not particularly limited, but may be, for example, lithium titanate (Li4Ti5O 12 transition metal oxides such as TiO2, Nb2O3, and WO3; metal sulfides, metal nitrides, carbon materials such as graphite, soft carbon, and hard carbon; silicon-based materials such as silicon elemental, silicon alloys, and silicon compounds; and lithium metal, lithium alloys, and metallic indium.

[0027] The negative electrode current collector 12 is not particularly limited, and any known material can be used as a negative electrode current collector for solid-state batteries. and the like metal foils.

[0028] The solid electrolyte 13 is not particularly limited as long as it is a material capable of conducting lithium ions, and examples thereof include a sulfide-based solid electrolyte material, an oxide-based solid electrolyte material, a nitride-based solid electrolyte material, and a halide-based solid electrolyte material.

[0029] The conductive assistant 14 is a material known as an electrode material for solid-state batteries, and is not particularly limited as long as it has electronic conductivity. Examples of the conductive assistant 14 include carbon materials such as acetylene black, and metal materials.

[0030] (Positive electrode layer) The positive electrode layer 20 includes a positive electrode active material layer that essentially contains a positive electrode active material 21 and optionally contains a solid electrolyte 23, a conductive assistant 24, and the like, and a positive electrode current collector 22. In addition to the above, the positive electrode active material layer may contain a material known as an electrode material for a solid-state battery, such as a binder.

[0031] The positive electrode active material 21 is not particularly limited, but may be, for example, LiCoO2, Li(Ni 5 / 10 Co 2 / 10 Mn 3 / 10 )O 2、 Li(Ni) 6 / 10 Co 2 / 10 Mn 2 / 10 )O 2、 Li(Ni) 8 / 10 Co 1 / 10 Mn 1 / 10 )O 2、 Li(Ni) 0.8 Co 0.15 Al 0.05 )O 2、 Li(Ni) 1 / 6 Co 4 / 6 Mn 1 / 6 )O 2、 Li(Ni) 1 / 3 Co 1 / 3 Mn 1 / 3 )O 2、Examples include LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, and sulfur.

[0032] The positive electrode current collector 22 is not particularly limited, but examples thereof include aluminum (Al) foil, stainless steel (SUS) foil, and the like.

[0033] The solid electrolyte 23 and the conductive assistant 24 may have the same configurations as the solid electrolyte 13 and the conductive assistant 14, respectively.

[0034] (solid electrolyte layer) The solid electrolyte layer 30 essentially contains a solid electrolyte 31. The solid electrolyte layer 30 may contain a binder and the like in addition to the above.

[0035] As the solid electrolyte 31, a configuration similar to that of the solid electrolytes 13 and 23 described above can be adopted.

[0036] The solid electrolyte 31 preferably has a lower Young's modulus (rigidity) than the fibers 41 described below. The solid electrolyte 31 preferably has a lower Young's modulus (rigidity) than the solid electrolyte 42 described below.

[0037] The solid electrolyte 31 may be, for example, Li3PS4 (Young's modulus: 18 to 25 GPa), Li 10 GeP2S 12 (Young's modulus: 21 GPa or less), Li3PO4 (Young's modulus: 50 GPa or less), Li 2.9 PO 3.3 N 0.46 (Young's modulus: 50 GPa or less), etc. The solid electrolyte 31 having a lower Young's modulus than the fibers 41 and / or the solid electrolyte can be appropriately selected depending on the Young's modulus of the selected fibers 41 and solid electrolyte .

[0038] <Coated fiber> In the solid-state battery 1, at least one of the interface I1 between the anode layer 10 and the solid electrolyte layer 30 and the interface I2 between the cathode layer 20 and the solid electrolyte layer 30 has a coated fiber 4 as a fiber coated with a solid electrolyte. The presence of the coated fiber 4 at the interface I1 or the interface I2 produces not only van der Waals forces but also an anchor effect, and the anode layer 10 and / or the cathode layer 20 and the solid electrolyte layer 30 are mechanically bonded together. This improves the bonding strength between the anode layer 10 and / or the cathode layer 20 and the solid electrolyte layer 30. This reduces the amount of binder contained in the electrode layer and the solid electrolyte layer, thereby improving ion conductivity.

[0039] 2 shows an outline of the structure of the coated fiber 4. The coated fiber 4 is formed by coating a fiber 41 with a solid electrolyte .

[0040] The fibers 41 preferably have a higher Young's modulus (rigidity) than the solid electrolyte 31 contained in the solid electrolyte layer 30. This improves the anchor effect when the coated fibers 4 penetrate into other layers through the interface I1 or I2 when forming the solid battery 1. This can further improve the bonding strength between the negative electrode layer 10 and / or the positive electrode layer 20 and the solid electrolyte layer 30.

[0041] Examples of the fibers 41 include non-electron-conductive ceramic fibers. Specifically, alumina (Young's modulus: 360 to 470 GPa), zirconia (Young's modulus: 200 GPa), silicon nitride (Young's modulus: 300 GPa), silicon carbide (α type, Young's modulus: 440 GPa), aluminum nitride (Young's modulus: 320 GPa), Li7La3Zr2O 12 (LLZ, Young's modulus: 130-150 GPa), Li3PO4 (Young's modulus: 50 GPa or less), Li3PO4N, which is lithium phosphate with nitrogen added X (LIPON, Young's modulus: 50 GPa or less), etc. The fibers 41 having a Young's modulus equal to or greater than that of the solid electrolyte 31 can be appropriately selected according to the Young's modulus of the selected solid electrolyte 31.

[0042] The diameter of the fibers 41 is preferably, for example, 1 / 5 or less of the diameter of the solid electrolyte 42. This improves the bonding strength between the fibers 41 and the solid electrolyte 42, and reduces the loss of the solid electrolyte 42 from the surfaces of the fibers 41 when the fibers 41 are anchored to the positive electrode layer or the negative electrode layer.

[0043] The length of the fibers 41 is preferably equal to or less than the total thickness of the negative electrode active material layer, the solid electrolyte layer 30, and the positive electrode active material layer, for example. This makes it possible to prevent damage to the current collector caused by the fibers 41.

[0044] The aspect ratio of the fibers 41 is preferably, for example, equal to or greater than 5. This allows the amount of penetration into the positive electrode layer or negative electrode layer to be increased, thereby achieving a greater anchor effect.

[0045] The solid electrolyte 42 coats the surfaces of the fibers 41. Coating the surfaces of the fibers 41 with the solid electrolyte 42 improves the ionic conductivity of the coated fibers 4. This can further improve the ionic conductivity of each layer at the interface I1 and the interface I2. The solid electrolyte 42 can have a structure similar to that of the solid electrolytes 13, 23, and 31.

[0046] The solid electrolyte 42 is preferably the same type of solid electrolyte as the solid electrolyte 31. This improves the compatibility between the coated fiber 4 and the solid electrolyte 31, improving the dispersibility of the coated fiber 4. This can further improve the bonding strength and ion conductivity between the negative electrode layer 10 and / or the positive electrode layer 20 and the solid electrolyte layer 30 at the interface I1 and / or the interface I2.

[0047] On the other hand, it is also preferable that the solid electrolyte 42 has a Young's modulus (rigidity) equal to or greater than that of the solid electrolyte 31. This improves the anchor effect when the coated fiber 4 penetrates into another layer through the interface I1 or I2 when forming the solid battery 1. This can further improve the bonding strength between the negative electrode layer 10 and / or the positive electrode layer 20 and the solid electrolyte layer 30.

[0048] As the solid electrolyte 42 having a Young's modulus (rigidity) equal to or higher than that of the solid electrolyte 31, for example, Li7La3Zr2O 12 (LLZ, Young's modulus: 130-150 GPa), Li3PO4 (Young's modulus: 50 GPa or less), Li 2.9 PO 3.3 N 0.46 (Young's modulus: 50 GPa or less), etc. The solid electrolyte 42 can be appropriately selected depending on the Young's modulus of the selected solid electrolyte 31.

[0049] The solid electrolyte 42 preferably has an average particle size (D50) of, for example, 1 nm to 500 nm, which allows the fibers 41 to be appropriately coated.

[0050] [Solid-state battery manufacturing method] The manufacturing method of the solid battery 1 is not particularly limited, and a known method can be applied. For example, a method for forming the positive electrode layer and the negative electrode layer includes a method in which a material constituting the electrode active material layer, such as an electrode active material, is dissolved or dispersed in a solvent to prepare an electrode mixture slurry, which is then applied to the surface of a current collector and dried. For example, a method for forming a solid electrolyte layer includes a method in which a solid electrolyte slurry prepared by dissolving or dispersing a solid electrolyte in a solvent is applied to an arbitrary target and dried. The above-mentioned coating means is not particularly limited, and examples thereof include an inkjet method, a screen printing method, and a doctor blade method. In order to have the coated fiber 4 present at the interface I1 or I2 of the solid battery 1, a method in which the coated fiber 4 is mixed with either the electrode mixture slurry or the solid electrolyte slurry can be used.

[0051] The layers thus formed are stacked and optionally pressed to produce a solid-state battery 1 (laminate). The pressing method may be uniaxial compression bonding, but a roll press method is preferred. This is because roll press moves the coated fiber 4 so as to be oriented in the feed direction of the laminate, making it easier for the coated fiber to be positioned at the interface I1 or I2.

[0052] [Method of manufacturing covered fibers] The method for producing the coated fiber 4 includes, for example, a solution method. In the solution method, the solid electrolyte 42 is a sulfur-based solid electrolyte, such as Li3PS4 or Li 10 GeP2S 12 In the solution method, first, a solution of the solid electrolyte 42 (e.g., Li3PS4) is mixed and dissolved in a solvent (e.g., N-methylformamide) to prepare a solution of the solid electrolyte 42. Fibers 41 (e.g., alumina) are mixed with the solution and vacuum dried to produce fibers 41 coated with the solid electrolyte 42 (coated fibers 4). The average particle size of the solid electrolyte 42 can be adjusted by the concentration of the solid electrolyte 42 when the solution is prepared or the temperature during vacuum drying.

[0053] In addition to the above, the method for producing the coated fiber 4 includes a sputtering deposition method and a laser ablation method. In the sputtering deposition method and the laser ablation method, the solid electrolyte 42 is an oxide solid electrolyte, Li7La3Zr2O 12 , Li3PO4, Li 2.9 PO 3.3 N 0.46 In the sputtering deposition method and the laser ablation method, first, a solid electrolyte 42 (e.g., Li7La3Zr2O 12 ) is compressed at a predetermined pressure and molded to obtain a green compact (bulk body). Next, in the sputtering deposition method, a rare gas (argon, etc.) is bombarded in a vacuum with the green compact (bulk body) as a target to produce a fiber 41 (coated fiber 4) coated with a solid electrolyte 42. In the laser ablation method, a pulsed laser is irradiated instead of the rare gas.

[0054] The method for producing the coated fiber 4 is not limited to the above, and an alkoxide solution method using a composite alkoxide solution made of lithium alkoxide, lanthanum alkoxide, and zirconium alkoxide can also be used.

[0055] Although the preferred embodiments of the present invention have been described above, the present invention is not limited to the above-mentioned embodiments, and the present invention includes modifications and improvements within the scope of the present invention that can achieve the object of the present invention. [Explanation of symbols]

[0056] 1 solid state battery 10 Negative electrode layer 20 Positive electrode layer 21 Cathode active material 30 Solid electrolyte layer 31 Solid electrolyte 4. Coated fibers (fibers coated with solid electrolyte) 41 Textiles 42 Solid electrolyte I1, I2 interface

Claims

1. A solid-state battery having a positive electrode layer including a positive electrode active material, a negative electrode layer, and a solid electrolyte layer including a solid electrolyte and disposed between the positive electrode layer and the negative electrode layer, A solid-state battery comprising: a fiber coated with a solid electrolyte at at least one of an interface between the positive electrode layer and the solid electrolyte layer and an interface between the negative electrode layer and the solid electrolyte layer.

2. 2. The solid-state battery according to claim 1, wherein the solid electrolyte covering the fibers is made of the same material as the solid electrolyte contained in the solid electrolyte layer.

3. 2. The solid-state battery according to claim 1, wherein the solid electrolyte covering the fibers has a higher Young's modulus than the solid electrolyte contained in the solid electrolyte layer.

4. The solid-state battery according to claim 1 , wherein the fibers have a higher Young's modulus than a solid electrolyte contained in the solid electrolyte layer.

5. 3. The solid-state battery according to claim 1, wherein the average particle size of the solid electrolyte coating the fibers is 1 nm to 500 nm.

6. The solid-state battery of claim 1 or 2, wherein the fibers penetrate into a plurality of layers adjacent to the interface.

7. 1. A solid-state battery having a positive electrode layer containing a positive electrode active material, a negative electrode layer, and a solid electrolyte layer containing a solid electrolyte and disposed between the positive electrode layer and the negative electrode layer.

2. A fiber coated with a solid electrolyte, the fiber being used for joining the positive electrode layer and the solid electrolyte layer, or the negative electrode layer and the solid electrolyte layer.

Citation Information

Patent Citations

  • Manufacture of solid-electrolyte sheet and solid-electrolyte secondary battery

    JP1991017965A

  • Solid electrolyte sheet, electrode sheet, and all solid secondary battery

    JP2014096311A

  • Electrolyte sheet, solid-electrolyte-coated fiber, and lithium-ion battery

    WO2021241402A1

  • Batteries and electronic devices

    JP6683259B2

Cited By

  • High young's modulus solid electrolyte, all-solid-state lithium battery, and method for producing the

    JP2026073917A

  • solid-state batteries

    JP2026163392A

  • High Young's modulus solid electrolyte, all-solid-state lithium battery, and method for manufacturing the same.

    JP7905022B2