Battery module
The battery module design addresses sealing issues by using a fixing member to distribute stress and protect the current collector and lead tabs, maintaining module integrity despite pressure changes.
Patent Information
- Application Number
- JP2023045144
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Existing battery modules face issues with sealing performance deterioration due to gas generation, which can lead to breakage of the joint between the current collector and lead tab under torsional stress from uneven expansion or distortion of the exterior body.
A battery module design with a fixing member that covers the welded portion and extends beyond the joint, suppressing stress concentration by positioning closer to the electrode laminate, and using a combination of fixing members made of different materials to maintain sealing and protect the current collector and lead tabs.
The design effectively maintains sealing properties and prevents breakage of the current collector and lead tabs by distributing stress, ensuring the module's integrity under pressure fluctuations.
Smart Images

Figure 2024134783000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a battery module. [Background technology]
[0002] In recent years, research and development into secondary batteries that contribute to energy efficiency has been conducted in order to ensure that more people have access to affordable, reliable, sustainable and advanced energy.
[0003] A secondary battery has an exterior body such as a laminate film that houses an electrode stack. There is a problem that the sealing property at the welded part of the exterior body is deteriorated due to gas generation from the electrolyte inside the exterior body. In response to the above problem, a technology has been disclosed relating to a battery pack having a pressure contact member with a contact surface for pressing the heat-welded part of the exterior case (for example, see Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2004-103258 A Summary of the Invention [Problem to be solved by the invention]
[0005] In the technology disclosed in Patent Document 1, the heat-sealed portion of the outer case is evenly pressed by a pressure member. However, simply pressing and fixing the heat-sealed portion may cause the joint between the current collector and the lead tab to break if, for example, torsional stress occurs due to uneven expansion of the outer case or distortion of the heat-sealed portion.
[0006] The present invention has been made in view of the above, and has an object to provide a battery module that can maintain the sealing performance of an exterior body and protect a current collector and a lead tab. [Means for solving the problem]
[0007] (1) The present invention relates to a battery module in which battery cells are stacked, each having an electrode laminate, an exterior body that houses the electrode laminate, and a lead tab to which a current collector of the electrode laminate is connected, wherein the lead tab has an extension portion that extends from the exterior body, the battery module includes a fixing member that is arranged in contact with a welding portion provided on the outer periphery of the exterior body in the stacking direction and fixes the battery cells, the width of the fixing member is greater than the width of the welding portion, and the end of the fixing member on the electrode laminate side is arranged on the electrode laminate side of the end of the lead tab on the electrode laminate side in the joining region where the current collector and the lead tab are joined.
[0008] According to the invention of (1), it is possible to provide a battery module that can maintain the sealing performance of the exterior body and protect the current collectors and the lead tabs.
[0009] (2) A battery module as described in (1), wherein the current collector has a joint portion to be joined to the lead tab, and the fixing member is positioned outside the electrode laminate further than the end portion of the joint portion in the joining area that is on the electrode laminate side.
[0010] According to the invention of (2), stress concentration at the joints of the current collector can be suppressed, so that breakage of the current collector can be suppressed.
[0011] (3) The battery module according to (1) or (2), wherein the fixing member has an R-shaped surface facing the current collector in the joining region.
[0012] According to the invention of (3), stress concentration at the joints of the current collector can be further suppressed, so that breakage of the current collector can be further suppressed.
[0013] (4) A battery module as described in (1) or (2), in which the fixing member is provided in contact with a location of the outer casing where the extension portion is provided, and is used in combination with a second fixing member provided in contact with a location of the outer casing where the extension portion is not provided, and the fixing member and the second fixing member are made of different materials.
[0014] According to the invention (4), the fixing member and the second fixing member can be made of appropriate materials according to the functions required of each of them. [Brief description of the drawings]
[0015] [Figure 1] 1 is a perspective view showing a configuration of a battery module according to a first embodiment. FIG. [Diagram 2] 1 is an exploded perspective view showing a configuration of a battery module according to a first embodiment. FIG. [Diagram 3] FIG. 2 is an exploded perspective view showing a state in which a plurality of battery modules according to the first embodiment are stacked. [Figure 4] 2 is a cross-sectional view taken along line AA showing a main part of the battery module according to the first embodiment. FIG. [Diagram 5] 11 is a cross-sectional view showing a main part of a battery module according to a second embodiment. FIG. [Figure 6] FIG. 11 is a perspective view showing a configuration of a first member according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] <Battery module> First Embodiment Hereinafter, a first embodiment of the present invention will be described with reference to the drawings. As shown in Figures 1 and 2, a battery module 1 has battery cells 10 and a fixing member 21 that fixes the battery cells 10. The fixing member 21 is preferably used as a fixing frame 20 in combination with a second fixing member 22.
[0017] 1 has one set of battery cells 10 and a fixing frame 20, but the number of stacked battery cells 10 is not particularly limited. As shown in FIG. 3, the battery module may be formed by stacking a plurality of sets of battery modules 1 in FIG. 1 as stacking units in stacking direction Z. In such a case, the plurality of battery modules 1 are integrated by inserting fasteners f into a plurality of holes h formed in the fixing frame 20 and fastening them together. Also, as shown in FIG. 3, a cushioning material 30 may be disposed between the battery modules 1.
[0018] (Battery cell) 1 etc., the battery cell 10 has an electrode laminate 11, a pair of lead tabs 12, 13 to which a current collector of the electrode laminate 11 is connected, and an exterior body 14 that houses the electrode laminate 11. The battery cell 10 has a rectangular shape when viewed from above (stacking direction Z).
[0019] The battery cell 10 is not particularly limited, but examples thereof include a semi-solid lithium ion battery cell having a gel electrolyte as an electrolyte, a liquid battery cell having an electrolyte solution in which the electrolyte is dissolved in a solvent, etc. In the above-mentioned battery cells, the internal pressure of the exterior body 14 may increase due to gas generated from the electrolyte or the electrolyte solution, but the battery module 1 of the present embodiment can maintain the sealing performance of the exterior body and protect the current collector and the lead tab even when the internal pressure of the exterior body 14 increases.
[0020] The battery cell 10 is preferably a semi-solid lithium metal battery cell that uses lithium metal in the negative electrode, or a semi-solid lithium ion battery cell that uses a silicon compound in the negative electrode, because these semi-solid batteries undergo relatively large expansion and contraction during charging and discharging.
[0021] The electrode laminate 11 is formed by laminating a pair of negative and positive electrodes and an electrolyte layer disposed between the negative and positive electrodes in an arbitrary number of layers. The lamination direction is the direction Z in each drawing. The negative electrode includes, for example, a negative electrode active material layer and a negative electrode current collector. The positive electrode includes, for example, a positive electrode active material layer and a positive electrode current collector.
[0022] The negative electrode active material layer is a layer that essentially contains a negative electrode active material. The negative electrode active material is not particularly limited, and examples thereof include lithium titanate (Li4Ti5O 12 transition metal oxides such as TiO2, Nb2O3, and WO3; metal sulfides, metal nitrides, carbon materials such as graphite, soft carbon, and hard carbon; silicon-based materials such as silicon elemental, silicon alloys, and silicon compounds; and lithium metal, lithium alloys, and metallic indium.
[0023] The negative electrode current collector is not particularly limited, and examples thereof include metal foils such as copper (Cu) foil, stainless steel (SUS) foil, and aluminum (Al) foil.
[0024] The positive electrode active material layer is a layer that essentially contains a positive electrode active material. The positive electrode active material is not particularly limited, and examples thereof include LiCoO2, Li(Ni 5 / 10 Co 2 / 10 Mn 3 / 10 )O 2、 Li(Ni) 6 / 10 Co 2 / 10 Mn 2 / 10 )O 2、 Li(Ni) 8 / 10 Co 1 / 10 Mn 1 / 10 )O 2、 Li(Ni) 0.8 Co 0.15 Al 0.05 )O 2、 Li(Ni) 1 / 6 Co 4 / 6 Mn 1 / 6 )O 2、 Li(Ni) 1 / 3 Co 1 / 3 Mn 1 / 3 )O 2、 Examples include LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, and sulfur.
[0025] The positive electrode current collector is not particularly limited, and examples thereof include aluminum foil.
[0026] The pair of lead tabs 12, 13 each have an extension portion 121, 131 extending from the exterior body 14. In the following explanation, the configuration of the negative electrode lead tab 12 and the negative electrode current collector 111 will be explained, but a similar configuration can be applied to the positive electrode lead tab 13 and the positive electrode current collector (not shown). As shown in Fig. 4, the lead tab 12 is joined to the multiple negative electrode current collectors 111 gathered inside the exterior body 14 in a joining region R1 by a method such as ultrasonic welding. The direction in which the lead tab 12 extends from the exterior body 14 is the direction X in each drawing.
[0027] The exterior body 14 is made of a laminate film or the like, and houses the electrode stack 11 therein. A welding portion (welding portion 142 in FIG. 4) is provided on the outer periphery of the battery cell 10, i.e., the outer periphery 141 of the exterior body 14, for overlapping and welding the exterior bodies together. The welding portion is provided on at least two sides of the outer periphery 141 where the extension portions 121, 131 are arranged. In addition to the above, the welding portion may also be provided on two sides of the outer periphery 141 where the extension portions 121, 131 are not arranged.
[0028] 4, the exterior body 14 has a gas reservoir portion 14a between the stacking end portion of the electrode stack 11 and an outer circumferential portion 141. Gas generated from the electrolyte or electrolytic solution can flow into and be retained in the gas reservoir portion 14a.
[0029] (Fixing member) 4, fixing member 21 is disposed in contact with welded portion 142 in the stacking direction Z at a location of outer circumferential portion 141 where extension portions 121, 131 are provided. In this embodiment, a pair of fixing members 21 are disposed above and below extension portions 121, 131 in the stacking direction Z, respectively. The pair of fixing members 21 clamp and fix the short side of outer circumferential portion 141 together with lead tabs 12, 13 via welded portion 142. Fixing member 21 can maintain the sealing performance of exterior body 14 and can protect lead tabs 12, 13, and current collectors connected to the lead tabs from stresses such as torsional stress due to uneven expansion of exterior body 14 and distortion of heat-welded portions.
[0030] FIG. 4 is an enlarged cross-sectional view of the extension portion 121 and its vicinity taken along line AA in FIG. 1. As shown in FIG. 4, the length L1 of the fixing member 21 in the extension direction of the lead tab 12 of the fixing member 21 (direction X in FIG. 4), which is the width of the fixing member 21, is greater than the length L2 of the welding portion 142 in the direction X, which is the width of the welding portion 142. In addition, the end 21a of the fixing member 21 on the electrode laminate 11 side is disposed closer to the electrode laminate 11 side than the end 12a of the lead tab 12 on the electrode laminate 11 side in the joining region R1 (note that in FIG. 4 and FIG. 5, the laminated structure of the electrode laminate 11 is omitted and only the configuration of the negative electrode current collector 111 is shown in schematic form). This makes it possible to suppress the application of stress to the negative electrode current collector 111 due to the lead tab 12 being pulled when the battery cell 10 expands and contracts or when the gas reservoir portion 14a of the exterior body 14 expands and contracts. This makes it possible to maintain the sealing performance of the exterior body 14 and protect the current collector and the lead tab.
[0031] It is preferable that fixing member 21 completely covers the end of welded portion 142 on the electrode stack 11 side when viewed from above. This makes it possible to prevent stress from being applied to welded portion 142 when gas reservoir portion 14a of exterior body 14 expands and contracts, which would impair the sealing performance of exterior body 14. Fixing member 21 may completely cover welded portion 142 when viewed from above.
[0032] As shown in FIG. 4, the end 21a of the fixing member 21 on the electrode laminate 11 side is preferably disposed outside the electrode laminate 11 relative to the end R1a of the joint 11a of the negative electrode current collector 111 on the electrode laminate 11 side with the lead tab 12 in the joint region R1. As a result, the end R1a of the negative electrode current collector 111 is not fixed, and the bent portion when the gas reservoir 14a of the exterior body 14 expands and contracts becomes the end 21a of the fixing member 21. As a result, the end R1a can move freely to some extent following the expansion and contraction of the gas reservoir 14a, so that stress is less likely to concentrate on the end R1a when the gas reservoir 14a expands than when the end R1a is fixed. Therefore, the breakage of the negative electrode current collector 111 can be suppressed.
[0033] Fixing member 21 functions as a seat for the bus bar in addition to suppressing stress concentration on welded portion 142. Also, extending portion 121 may be bent for joining to the bus bar, but fixing member 21 makes it easy to bend extending portion 121. There is no particular limitation on the material of fixing member 21 suitable for the above function, but for example, a resin material is used.
[0034] The pressure at which outer periphery 141 is clamped by the pair of fixing members 21 is preferably equal to or greater than the rising internal pressure for gas generated inside exterior body 14, and more preferably equal to or greater than the sealing pressure resistance of exterior body 14. Specifically, the clamping pressure is preferably equal to or greater than 0.05 MPa, and more preferably equal to or greater than 0.5 MPa.
[0035] (Fixed frame) The pair of fixing members 21 are preferably combined with a pair of second fixing members 22 to constitute the fixing frame 20 formed in a frame shape. The fixing frame 20 is arranged to sandwich the outer periphery 141. In this embodiment, the fixing frames 20 are respectively arranged above and below the stacking direction Z of the battery cell 10, and are fixed by sandwiching a part including the outer edge of the outer periphery 141. The fixing frame 20 sandwiches four sides of the battery cell 10 in a top view, and fixes the electrode stack 11 and exterior body 14 of the battery cell 10 together with the pair of lead tabs 12, 13.
[0036] For example, when a material with large expansion and contraction, such as lithium metal or a silicon-based material, is used as the negative electrode active material, it is preferable to place the cushioning material 30 between the battery modules 1. However, when the cushioning material 30 is used, there is a possibility that a torsional stress acts on the lead tabs 12, 13. With the above-mentioned configuration, the lead tabs 12, 13 and the current collectors connected to the lead tabs can be more preferably protected from the torsional stress and the like.
[0037] In the fixed frame 20, the pair of fixed members 21 and the pair of second fixed members 22 are preferably joined together. The fixed frame 20 may be integrally formed, but it is preferable that the fixed members 21 and the second fixed members 22 are formed separately. This allows the fixed members 21 and the second fixed members 22 to be made of different materials according to the performance required of each of them.
[0038] (Second fixing member) The second fixing members 22 are disposed in contact with portions of the outer circumferential portion 141 where the extending portions 121, 131 are not provided, in the stacking direction Z. In this embodiment, the pair of second fixing members 22 are disposed above and below the outer circumferential portion 141, respectively, in the stacking direction Z. The pair of second fixing members 22 clamp and fix the long side sides of the outer circumferential portion 141.
[0039] As shown in FIG. 1, the second fixing member 22 has a hole h penetrating in the stacking direction Z. As shown in FIG. 3, a fastener f for stacking a plurality of battery modules 1 may be inserted into the hole h, or a coolant for cooling the battery module 1 may be disposed therein. An example of the coolant is a chiller hose. This allows efficient temperature adjustment of the battery module 1. The fixing member 21 may also have a hole h similar to that of the second fixing member 22.
[0040] The second fixing member 22 that fulfills the above functions is not particularly limited, but is preferably made of a material that has a certain degree of rigidity and heat dissipation properties, for example, a metal material such as aluminum steel.
[0041] Second Embodiment Next, a battery module 1a according to a second embodiment will be described with reference to Figures 5 and 6. Note that the same components as those in the battery module 1 of the first embodiment described above will be denoted by the same reference numerals, and the description thereof may be omitted.
[0042] The battery module 1a has a fixing member 211. Like the fixing member 21, the fixing member 211 is arranged in contact with the welding portion 142 at the location of the outer circumferential portion 141 where the extending portions 121, 131 are provided, in the stacking direction Z. In this embodiment, the pair of fixing members 211 are arranged above and below the extending portions 121, 131, respectively, in the stacking direction Z.
[0043] The fixing member 211 has an R-shaped surface 21b that faces the electrode stack 11 and the negative electrode current collector 111 in the joining region R1. Since the fixing member 211 has the R-shaped surface 21b, the end portion R1a is less likely to come into contact with the fixing member 211 when the gas reservoir portion 14a of the exterior body 14 expands and contracts. This makes it difficult for stress to be concentrated on the end portion R1a when the gas reservoir portion 14a expands. Therefore, breakage of the negative electrode current collector 111 can be further suppressed.
[0044] 6, the fixing member 211 preferably has a recess 21c formed on the surface that comes into contact with the outer circumferential portion 141. The recess 21c is a recess in which the joint portion between the lead tab 12 and the negative electrode current collector 111 in the joint region R1 can be disposed. The recess 21c allows the fixing member 211 to have a shape corresponding to the shape of the joint portion between the lead tab 12 and the negative electrode current collector 111, so that the outer circumferential portion 141 can be fixed by the fixing member 211 more preferably.
[0045] Although the embodiments of the present invention have been described above, the present invention is not limited to the above-mentioned embodiments and can be modified as appropriate. For example, it is possible to combine the configuration of the first embodiment with the configuration of the second embodiment. [Explanation of symbols]
[0046] 1, 1a battery module 11 Electrode laminate 111 Negative electrode collector (current collector) 11a Joint 12, 13 Lead tab 121, 131 extension part 14 Exterior body 141 Outer periphery 142 Welded area 21 Fixing member 22 Second fixing member R joint area Z stacking direction
Claims
1. A battery module in which battery cells are stacked, the battery cells having an electrode laminate, an exterior body that houses the electrode laminate, and lead tabs to which current collectors of the electrode laminate are connected, the lead tab has an extension portion extending from the exterior body, the battery module includes a fixing member that is disposed in contact with a welding portion provided on an outer periphery of the exterior body in a stacking direction and fixes the battery cell; The width of the fixing member is greater than the width of the welded portion, a battery module, wherein an end of the fixing member on the electrode stack side is positioned closer to the electrode stack than an end of the lead tab on the electrode stack side in a joining region where the current collector and the lead tab are joined.
2. the current collector has a joint portion to be joined to the lead tab, The battery module according to claim 1 , wherein the fixing member is disposed outside the electrode stack relative to an end of the joint portion in the joint region that is on the electrode stack side.
3. The battery module according to claim 1 , wherein the fixing member has an R-shaped surface facing the current collector in the joining region.
4. the fixing member is provided in contact with a portion of the exterior body where the extension portion is provided, and is used in combination with a second fixing member provided in contact with a portion of the exterior body where the extension portion is not provided, The battery module according to claim 1 , wherein the fixing member and the second fixing member are made of different materials.
Citation Information
Patent Citations
Battery pack
JP2004103258A
Housing for battery cell
JP2005302502A
Battery cell, battery module including the battery cell, and battery pack including the battery module
JP2022545204A
Thin battery, assembled cells, and method of producing thin battery
WO2006038697A1
Electric device with outer film cover
WO2007105541A1
Cited By
Storage battery module and manufacturing method thereof
CN122843645A
Battery module and method for manufacturing the same
JP2026164369A