Secondary battery
The secondary battery design with circumferentially arranged welding protrusions on the sealing plate addresses unstable welding issues by preventing electrolyte adhesion, enhancing manufacturing stability and electrical connectivity.
Patent Information
- Application Number
- JP2023047752
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
Smart Images

Figure 2024136597000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a secondary battery. [Background technology]
[0002] Patent Document 1 discloses a battery and a manufacturing method thereof. In the technology of Patent Document 1, at least two protrusions are provided on the current collecting lead, thereby preventing explosion while maintaining low internal resistance and welding strength. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2005-268070 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, when protrusions are provided on the current collecting lead as in the technique of Patent Document 1, the current collecting lead is immersed in the electrolyte during the welding process, which causes explosions due to adhesion of the electrolyte, resulting in unstable welding.
[0005] Therefore, an object of the present invention is to provide a secondary battery that can be stably welded. [Means for solving the problem]
[0006] The present invention employs the following solutions. Note that the solutions below are merely examples, and the present invention is not limited thereto. The present invention can be an invention that includes at least one of the invention-specifying matters shown in the solutions below. Furthermore, each invention-specifying matter shown in the solutions below can be made into a subordinate concept by adding an element that limits the invention-specifying matter, and can also be made into a superordinate concept by deleting an element that limits the invention-specifying matter.
[0007] The conveying device of the solution is, for example, a secondary battery including an outer can having an opening, a sealing plate placed in the opening, an electrode group contained in the outer can, a current collecting lead having one end welded to the sealing plate and the other end connected to the electrode group, and a plurality of welding protrusions arranged circumferentially on the underside of the sealing plate. Effect of the Invention
[0008] According to the present invention, a secondary battery that can be stably welded can be provided. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a perspective view showing a battery 1. [Diagram 2] 2 is a diagram illustrating the structure of a sealing plate 42 and a sealing body 40. FIG. [Diagram 3] 4A to 4C are diagrams illustrating the structure of a sealing plate 42. [Figure 4] FIG. 13 is a conceptual diagram showing a problem that occurs in a sealing body welding process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, a nickel-metal hydride secondary battery (hereinafter, abbreviated as "battery") will be described as an embodiment of the secondary battery of the present invention with reference to the drawings. Note that the following embodiment is shown as a suitable example of the secondary battery of the present invention, and the embodiment is not limited to this example. The battery can be of any size (AA size, AAA size, etc.).
[0011] [Battery configuration] Fig. 1 is a perspective view showing a battery 1. In Fig. 1, the battery 1 is shown partially cut away to facilitate understanding of the structure. The battery 1 includes an outer can 10, an electrode group 20 housed in the outer can 10, a positive electrode lead 30 (a current collecting lead, a tab which is a metal lead of the positive electrode plate) connected to a part of the electrode group 20, and a sealing body 40 which is connected to the positive electrode lead 30 and seals the opening 11 of the outer can 10.
[0012] The outer can 10 is a bottomed cylindrical member having an opening 11 at the top, and is made of a conductive material (e.g., nickel-plated steel sheet). The electrode group 20 includes a strip-shaped positive electrode 22, a negative electrode 24, and a separator 26. The negative electrode 24 and the positive electrode 22 sandwiched between two separators 26 are stacked and wound in a spiral shape and are contained in the outer can 10 together with an alkaline electrolyte (not shown). The outermost periphery of the negative electrode 24 becomes the outermost periphery of the electrode group 20 and is in contact with the inner periphery of the outer can 10. This electrically connects the negative electrode 24 and the outer can 10, and the bottom wall 12 of the outer can 10 functions as a negative electrode terminal.
[0013] The positive electrode 22 is made of nickel oxide. The negative electrode 24 is made of a hydrogen storage alloy. The separator 26 may be, for example, a nonwoven fabric of polyolefin fibers to which a hydrophilic group has been added. The alkaline electrolyte may be, for example, an aqueous solution containing potassium hydroxide, sodium hydroxide, lithium hydroxide, or the like as a solute.
[0014] An upper insulating member 32 is disposed between the electrode group 20 and the sealing body 40, and a lower insulating member 36 is disposed between the electrode group 20 and the bottom wall 12. In addition, a positive electrode lead 30 is disposed through a slit 34 provided in the upper insulating member 32.
[0015] One end of the positive electrode lead 30 is welded to a sealing plate 42 included in the sealing body 40, and the other end is connected to a positive electrode 22 included in the electrode group 20. In the illustrated example, the positive electrode lead 30 is bent in an S-shape (the shape of a horizontal letter S), but it may be bent in an L-shape (the shape of a horizontal letter L) or may have another shape.
[0016] The sealing body 40 includes a sealing plate 42 that is disposed at the opening 11 of the outer can 10 and closes the opening 11, a projection 44 (welding protrusion, welding point) disposed on the lower surface of the sealing plate 42, an annular gasket 46 that closely contacts the opening edge 14 of the outer can 10 while holding the outer edge of the sealing plate 42, and a cylindrical positive electrode terminal 48 with a flange disposed in the center of the upper surface of the sealing plate 42, which together seal the opening 11 of the outer can 10. Note that in FIG. 1, due to the portion shown in cross section, only one projection 44 appears to be in contact with the positive electrode lead 30, but in reality, two projections 44 are in contact with the positive electrode lead 30.
[0017] The sealing plate 42 is formed of a steel plate. The positive electrode terminal 48 is formed of a conductive material. The positive electrode terminal 48 is connected to the sealing plate 42, and the positive electrode lead 30 is connected to the positive electrode 22 and the sealing plate 42 as described above. Therefore, the positive electrode 22 and the positive electrode terminal 48 are electrically connected via the positive electrode lead 30 and the sealing plate 42. The gasket 46 is formed of an insulating material (for example, nylon).
[0018] A first gas vent hole 50 is formed in the center of the sealing plate 42, and a rubber valve body 52 is arranged to close the first gas vent hole 50, which is pressed against the sealing plate 42 by the positive electrode terminal 48. Although not shown, a small second gas vent hole is formed in the lower part of the side wall of the positive electrode terminal 48. The valve body 52 normally closes the first gas vent hole 50 airtight, but when gas is generated inside the outer can 10 and the pressure rises, the valve body 52 is compressed to open the first gas vent hole 50. This allows the inside and outside of the outer can 10 to communicate with each other through the first gas vent hole 50 and the second gas vent hole, and the gas is released to the outside. As a result, the internal pressure drops and the valve body 52 returns to its original state, closing the first gas vent hole 50 again. In this way, the valve body 52 functions as a safety valve for the battery 1.
[0019] [Structure of sealing body] FIG. 2 is a diagram for explaining the structures of the sealing plate 42 and the sealing body 40. FIG. 2(A) shows a view of the sealing plate 42 as seen from the lower surface side (back surface side), and FIG. 2(B) shows a cross-sectional view near the sealing body 40.
[0020] As shown in FIG. 2(A), a plurality (for example, 14) of projections 44 are arranged on the lower surface of the sealing plate 42. The plurality of projections 44 are arranged in a circumferential shape on the lower surface of the sealing plate 42. Each projection 44 is a hemispherical or cylindrical protrusion.
[0021] The arrangement interval (length L1: for example, 1 mm) of the plurality of projections 44 is shorter than the width (length L2: for example, 3 mm) of the positive electrode lead 30 (L1 < L2). By adopting such an arrangement interval, at least two projections 44 can be brought into contact with the positive electrode lead 30. Further, the portion of the positive electrode lead 30 that is welded to the sealing plate 42 is a member having an elongated plate shape (rectangular shape). Note that the arrangement interval of the plurality of projections 44 is the length from the center of one projection 44 to the center of the adjacent projection 44. Also, the diameter of the projection 44 is, for example, about 0.1 to 1.0 mm.
[0022] As shown in FIG. 2(B), the left projection 44 (44L) is in contact with the positive electrode lead 30, but the right projection 44 (44R) is not in contact with the positive electrode lead 30. For this reason, welding is performed at the portion where the left projection 44 (44L) and the positive electrode lead 30 are in contact.
[0023] 〔Details of the sealing plate〕 FIG. 3 is a diagram for explaining the structure of the sealing plate 42. FIG. 3(A) shows the sealing plate 42 shown in FIG. 1 alone, and FIG. 3(B) shows another form of the sealing plate 42A. As shown in FIG. 3(A), the sealing plate 42 includes a first annular portion 61, a second annular portion 62, and a third annular portion 63. The first annular portion 61 is an annular member having a first gas vent hole 50 (opening) at the center. The second annular portion 62 is an annular member that is disposed outside the first annular portion 61 and is located lower than the first annular portion 61. The third annular portion 63 is an annular member that is disposed outside the second annular portion 62 and positioned above the second annular portion 62. The multiple projections 44 are disposed on the lower surface of the second annular portion 62 .
[0024] Furthermore, if the midpoint between the outer end X of the second annular portion 62 and the inner end Y of the second annular portion 62 is defined as an intermediate portion Z, the projection 44 is not disposed between the outer end X and the intermediate portion Z, but is disposed between the intermediate portion Z and the inner end Y (disposed at any position between the intermediate portion Z and the inner end Y). In other words, the projection 44 is disposed not on the outside of the second annular portion 62, but at a position closer to the inside of the second annular portion 62.
[0025] Thus, in this embodiment, the projections 44 for welding the positive electrode lead 30 are provided on a flat surface (the lower surface of the second annular portion 62) other than the outer circumferential portion (third annular portion 63) having the gasket 46 (see FIG. 1) and the innermost circumferential portion (first annular portion 61) having a hole portion for discharging gas (first gas vent hole 50) of the sealing plate 42 of a predetermined size (for example, AAA size of about 9.5 mm), and the projections 44 are arranged at intervals of 1 mm for the positive electrode lead 30 having a width of 3 mm, for example. Note that as long as at least two projections 44 and the positive electrode lead 30 are in contact with each other, the shapes and dimensions of the sealing plate 42 and the positive electrode lead 30 are not limited to these.
[0026] In order to withstand an internal pressure of approximately 3.5 MPa, the sealing plate 42 has two steps S (portions sandwiched between the first annular portion 61 and the third annular portion 63) on the left and right sides. For this reason, the welding area (the area of the underside of the second annular portion 62) is very small. In addition, there are R-machined portions (chamfered portions; see R in the figure) on the left and right sides of the second annular portion 62, but these R-machined portions tend to become larger over time due to wear of the mold (for example, R 0.2 mm → actual measured R 0.8 mm, etc.). Furthermore, since the welded surface is unstable, current shunting is likely to occur (without the projection 44, the positive electrode lead 30 may end up being welded to two places: the lower surface of the second annular portion 62 and the R-machined portion). Therefore, in this embodiment, by providing the projection 44 on the lower surface of the second annular portion 62, the problem of the narrow welding area and the problem of the occurrence of current shunting are solved.
[0027] As shown in Fig. 3(B), sealing plate 42A of another embodiment has a configuration basically similar to sealing plate 42 shown in Fig. 3(A), and therefore a description of parts that perform the same functions will be omitted. Differences include that the opening width of first gas vent hole 50A is wider, sealing plate 42A is thinner, the radial length of each annular portion is changed, and the heights of first annular portion 61A and third annular portion 63A are reversed.
[0028] In this way, sealing plates of various shapes can be adopted depending on the shape and size of the battery 1. The sealing plate may be a sealing plate that is flatter than the sealing plate shown in Figures 3(A) and (B) (a sealing plate having a shape that is nearly fully flat), or may be a sealing plate that has a larger step than the sealing plate shown in Figures 3(A) and (B).
[0029] [Contents regarding the sealing body welding process] FIG. 4 is a conceptual diagram showing a problem in the sealing body welding process. In the manufacturing method of the nickel-metal hydride secondary battery, a positive electrode lead 30 made of a metal lead is previously joined to a Ni sponge that is the base material of the positive electrode plate, and the electrode group 20 wound together with the negative electrode plate and the separator is inserted into an outer can 10, and then an electrolyte is poured in. Thereafter, the positive electrode lead 30 that becomes the positive electrode plate is resistance welded to a sealing body 40 that has a positive electrode terminal 48 (a sealing body welding process is performed), and the battery 1 is formed by sealing.
[0030] In the sealing body welding process, as shown in Fig. 4, the sealing body 40 and the positive electrode lead 30 are placed between the receiving electrode 100 and the push electrode 200 (electrode rod) and then welded. In this sealing body welding process, welding spatter (metallic pieces) is generated, and internal short circuit defects may occur due to the inclusion of welding spatter. The generation of welding spatter is caused by explosion during resistance welding. The welding spatter first occurs between the sealing body 40 and the positive electrode lead 30 (internal spatter 70), and then occurs in front of the positive electrode lead 30 (between the positive electrode lead 30 and the push electrode 200) (surface spatter 80).
[0031] Then, when an extraction was carried out of the high resistance areas during welding resulting from such explosions, the results of extraction of the components that affect welding were as follows. (1) The influence of explosions is small between the power source and the receiving electrode 100. (2) The sealing body 40 is less susceptible to explosions. (3) The positive electrode lead 30 is significantly affected by explosions at locations where the electrolyte is attached. (4) Between the push electrode 200 and the power source, the influence of explosion is large at the portion where the electrolyte is attached.
[0032] The reason for the results (3) and (4) above is that the sealing body welding process is performed after the electrolyte injection process, and therefore electrolyte adheres to the positive electrode lead 30. A liquid puddle occurs in the part where electrolyte adheres, and explosion occurs due to the adhesion of electrolyte, resulting in poor welding stability. That is, when the electrolyte is poured from the top of the exterior can 10, the electrolyte adheres to the positive electrode lead 30 to be welded, and when the sealing body 40 is welded, the electrolyte components (KOH, NaOH, LiOH, etc.) precipitate, making the welding unstable and causing explosions. Furthermore, the inclusion of welding spatters causes short circuit failures inside the battery.
[0033] Therefore, in this embodiment, in order to stably weld the sealing plate 42, a plurality of projections 44 are provided at regular intervals in a circumferential shape on the underside of the sealing plate 42. The sealing plate 42 and the positive electrode lead 30 are joined by resistance welding at these projections 44. Since there is no adhesion of electrolyte on the sealing body 40 side, welding can be stabilized, and the battery 1 can be produced more stably.
[0034] As described above, according to this embodiment, the following effects are obtained. (1) According to the present embodiment, the projection 44 is disposed on the sealing plate 42 side rather than on the positive electrode lead 30 side. This allows the sealing plate 42 to be welded without being affected by the electrolyte, thereby improving the occurrence of explosions during welding. As a result, a battery 1 that can be stably welded can be provided.
[0035] (2) According to this embodiment, the projections 44 are arranged circumferentially on the underside of the sealing plate 42, so that positioning is not required and stable welding is possible. Since the sealing plate 42 falls from top to bottom in the manufacturing process, the orientation in which it is welded is not determined. In this regard, in this embodiment, the projections 44 are arranged circumferentially on the underside of the sealing plate 42, so that it can be reliably welded regardless of the orientation in which the projections 44 are arranged. In addition, since the projections 44 are used as welding points, the R-processed portion and the positive electrode lead 30 are not welded, so there is no shunting of current, and it is easy to set welding conditions such as the location of welding.
[0036] (3) In this embodiment, the projections 44 other than the two projections 44 in contact with the positive electrode lead 30 are basically not used for welding. However, if the welding does not go well or if the welded portion is inadvertently cut, welding can be performed using the remaining projections 44 without replacing the sealing plate 42, and the yield can be improved.
[0037] (4) According to this embodiment, the arrangement interval of the projections 44 is shorter than the width of the positive electrode lead 30, so that at least two projections 44 can be welded to the positive electrode lead 30, and the welding can be stabilized. That is, by having two or more projections 44 contact each other with respect to the width of the positive electrode lead 30 (for example, 3 mm for AAA), welding defects can be reduced.
[0038] (5) According to the present embodiment, the portion of the positive electrode lead 30 that is welded to the sealing plate 42 is an elongated plate-like member, and therefore it is more difficult to align the positive electrode lead 30 with the sealing plate 42 than a circular member. In this regard, the projections 44 of the present embodiment are arranged circumferentially, and therefore even if the positive electrode lead 30 is an elongated plate-like member, it is possible to perform stable welding while easily positioning the positive electrode lead 30.
[0039] (6) According to this embodiment, the sealing plate 42 is a stepped member including the first annular portion 61, the second annular portion 62, and the third annular portion 63, and therefore is more susceptible to welding spatters than a sealing plate that is nearly flat. In this regard, in this embodiment, by arranging the projection 44 on the underside of the second annular portion 62, it is possible to further prevent welding spatters from occurring.
[0040] (7) According to this embodiment, the projection 44 is not disposed between the outer end X and the middle portion Z of the second annular portion 62, but is disposed between the middle portion Z and the inner end Y, which improves ease of welding. That is, since the gasket 46 is disposed on the outside of the second annular portion 62, depending on the shape of the gasket 46, disposing the projection 44 on the outside of the second annular portion 62 may make welding difficult. Therefore, by disposing the projection 44 on the lower surface of the second annular portion 62 at a position closer to the inside, ease of welding can be improved.
[0041] [Modifications] The present invention is not limited to the above-described embodiment, and can be practiced in various modified forms. (1) Although the sealing plate 42 has been described as a stepped member, it may be a flat member without any steps. (2) The number of projections 44 may be 13 or less, or 15 or more. (3) Although an example has been described in which two projections 44 are in contact with the positive electrode lead 30, three or more projections 44 may be in contact with the positive electrode lead 30 by shortening the spacing between the projections 44 or shortening the diameter of the projections 44.
[0042] (4) Although the projection 44 is formed on the lower surface of the second annular portion 62 in the above embodiment, it may be formed on the lower surface of the first annular portion 61 or on the lower surface of the third annular portion 63. (5) The arrangement interval of the multiple projections 44 may be a value smaller than 1 mm or a value larger than 1 mm. The width of the positive electrode lead 30 may be a value smaller than 3 mm or a value larger than 3 mm. (6) The shape of the battery 1 may be cylindrical or rectangular (prismatic). The type of battery 1 is not limited to a nickel-metal hydride secondary battery (sealed nickel-metal hydride secondary battery) and may be other alkaline secondary batteries, lithium ion secondary batteries, etc. [Explanation of symbols]
[0043] 1 battery 10 Outer can 11 Opening 20 electrode groups 30 Positive lead 40 Sealing body 42, 42A Sealing plate 44 Projection 46 Gasket 48 Positive terminal
Claims
1. an outer can having an opening; A sealing plate disposed at the opening; an electrode group accommodated in the outer can; a current collecting lead having one end welded to the sealing plate and the other end connected to the electrode group; A plurality of welding projections arranged circumferentially on the lower surface of the sealing plate; A secondary battery comprising:
2. 2. The secondary battery according to claim 1, A secondary battery, characterized in that the arrangement interval between the plurality of welding projections is shorter than the width of the current collecting lead.
3. 2. The secondary battery according to claim 1, The secondary battery, wherein the current collecting lead is a member having a long and narrow plate shape at a portion that is welded to the sealing plate.