Secondary battery and manufacturing method of secondary battery
The secondary battery design with an airtight and peelable part effectively manages internal pressure to prevent bursting and electrolyte leakage by allowing controlled pressure release.
Patent Information
- Application Number
- JP2023051036
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
AI Technical Summary
Existing secondary batteries risk bursting due to unexpected increases in internal pressure, which can lead to electrolyte scattering.
A secondary battery design featuring a laminated electrode body enclosed in an exterior body with a thermally welded perimeter, including both an airtight maintenance part and an easily peelable part, where the peelable part has a lower peel strength than the airtight part, allowing controlled release of pressure when internal pressure rises.
Prevents the exterior body from bursting by allowing controlled release of pressure through the peelable part, preventing electrolyte leakage and ensuring safe operation.
Smart Images

Figure 2024140049000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a secondary battery and a method for manufacturing a secondary battery. [Background technology]
[0002] Patent Document 1 discloses a lithium ion secondary battery in which a battery group, in which a positive electrode, a negative electrode, and a separator layer are laminated, is sealed in a sheet-like exterior body. An opening on the outer periphery of the exterior body is closed by a heat seal part with high peel strength. Furthermore, inside the heat seal part of the exterior body, an easy peel seal part with a peel strength lower than that of the heat seal part is formed. When gas is generated inside the exterior body and the internal pressure of the exterior body increases, the easy peel seal part peels off, thereby increasing the volume of the exterior body and suppressing the increase in internal pressure. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2002-015713 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the above structure, if the internal pressure of the exterior body increases unexpectedly, there is a risk that the exterior body will burst and the electrolyte inside the exterior body will splash out.
[0005] The present disclosure has been completed in light of the above circumstances, and has an object to prevent rupture caused by an increase in internal pressure of an exterior body. [Means for solving the problem]
[0006] The secondary battery of the first disclosure is a laminated electrode body in which a positive electrode plate, a negative electrode plate, and a separator are laminated; and an exterior body that contains the laminated electrode body and has laminate sheets arranged to sandwich the laminated electrode body, A heat-sealed portion is formed on the outer periphery of the exterior body by applying pressure under heating to hermetically seal the mating surfaces of the laminate sheets, The heat-sealed portion includes an airtightness maintaining portion and an easily peelable portion having a peel strength lower than that of the airtightness maintaining portion, In at least one of a plurality of sides constituting the outer periphery of the exterior body, the airtightness maintaining portion and the easily peelable portion are arranged so as to be aligned along the side.
[0007] The method for producing a secondary battery according to the second disclosure includes the steps of: a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; A step of placing an inclusion on a mating surface of the laminate sheet in at least one of a plurality of side portions constituting an outer peripheral edge portion of the laminate sheet; The method includes a step of forming an airtightness maintaining portion that hermetically adheres the mating surfaces to each other by performing a thermal welding process in an area of the at least one side portion that includes the inclusion, and simultaneously with the formation of the airtightness maintaining portion, forming an easy-peel portion that hermetically adheres the mating surfaces to each other with a peel strength lower than that of the airtightness maintaining portion by performing a thermal welding process in an area of the at least one side portion that is adjacent to the inclusion.
[0008] The manufacturing method of the secondary battery according to the third disclosure includes: a heat sealer having a strong pressure surface and a weak pressure surface adjacent to the strong pressure surface and recessed in a stepped shape from the strong pressure surface, the heat sealer being capable of heating the strong pressure surface and the weak pressure surface; a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; The method includes a step of abutting the strong pressure surface against at least one of the multiple sides constituting the outer peripheral edge of the laminate sheet and performing a thermal welding process to form an airtight maintaining portion in which the mating surfaces are airtightly adhered to each other, and at the same time, abutting the weak pressure surface against the at least one side and performing a thermal welding process to form an easy peeling portion in which the mating surfaces are adhered to each other with a peel strength lower than that of the airtight maintaining portion. Effect of the Invention
[0009] When the internal pressure inside the exterior body rises to a certain level, the easily peelable portion peels off, causing the internal pressure to drop to atmospheric pressure, thereby preventing the exterior body from bursting due to an excessive increase in internal pressure. Since the easily peelable portion and the airtightness maintaining portion are arranged in line along the side portions, the portion where the laminate sheet peels off when the internal pressure rises can be set to a desired area. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a perspective view of a secondary battery according to a first embodiment; [Diagram 2] Exploded perspective view of a secondary battery [Diagram 3] Front view of secondary battery [Figure 4] FIG. 1 is a plan view showing a schematic state in which a step of forming a thermally welded portion is started in a manufacturing process of a secondary battery; [Diagram 5] A schematic plan view showing the state after the thermal welding process is completed [Figure 6] Schematic diagram showing the structure of inclusions [Figure 7] FIG. 1 is a perspective view showing a state in which an easily peelable portion of a laminate sheet has peeled off; [Figure 8] FIG. 11 is a front view of a secondary battery according to a second embodiment; [Figure 9] FIG. 11 is a perspective view showing a state in which an easily peelable portion of a laminate sheet is peeled off in a secondary battery according to a second embodiment; [Figure 10] FIG. 11 is a plan view showing a state where a step of forming a thermally welded portion is started in the manufacturing process of the secondary battery according to the third embodiment; [Figure 11]FIG. 11 is a plan view showing a state where a step of forming a thermally welded portion is completed in the manufacturing process of the secondary battery according to the third embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Here, preferred embodiment examples of the present disclosure will be described. Any combination of the following embodiment examples without causing any contradiction is also included in the embodiment for carrying out the present invention.
[0012] In the secondary battery of the first disclosure, the laminate sheet has a sheet-like base material and a sheet-like sealing material that is superimposed on the inner surface of the sheet-like base material to form the mating surface, and the heat-sealed portion is provided with an inclusion sandwiched between the mating surfaces, and the inclusion is preferably disposed only in an area of the airtightness maintaining portion adjacent to the easy peeling portion. According to this configuration, when the pressurizing surface of the heat-sealing machine to the heat-sealed portion is formed by a flat surface, the pressurizing force from the heat-sealing machine to the sealing material in the easy peeling portion is smaller than the pressurizing force to the sealing material in the airtightness maintaining portion. This difference in pressurizing force can cause a difference in the ease of peeling between the easy peeling portion and the airtightness maintaining portion. Therefore, the shape of the pressurizing surface of the heat-sealing machine can be simplified.
[0013] In the secondary battery of the first disclosure, the intermediate material preferably includes a sheet-like support having a communicating space for being impregnated with the molten sealing material and made of a material having a melting point higher than that of the sealing material. According to this configuration, the sheet-like support does not melt in the thermal welding process and is maintained in a state in which it exists between the sealing materials. The molten sealing material is impregnated into the communicating space of the sheet-like support, thereby ensuring sealing properties and increasing the bonding strength between the sheet-like base material and the intermediate material.
[0014] In the secondary battery of the first disclosure, the intermediate material is preferably made of a material having a melting point equal to or lower than that of the sealing material, and includes an adhesive layer superposed on the surface of the sheet-like holder facing the mating surface. According to this configuration, in the thermal welding process, the molten sealing material and the molten adhesive layer are integrated, and the sealing material and the adhesive layer are impregnated into the communicating space of the sheet-like holder, thereby increasing the bonding strength between the sheet-like base material and the intermediate material.
[0015] [Embodiment 1] A first embodiment of the present disclosure will be described with reference to Figs. 1 to 8. The present invention is not limited to these examples, but is defined by the claims, and includes all modifications within the meaning and scope equivalent to the claims. In this first embodiment, the F direction in Figs. 1, 2, 4, 5, and 7 is defined as the front with respect to the front-rear direction. The R direction in Figs. 1 to 5, and 7 is defined as the right with respect to the left-right direction. The left-right direction and the width direction are used synonymously. The H direction in Figs. 1 to 3, and 7 is defined as the up-down direction.
[0016] The laminated secondary battery A of the first embodiment has a configuration in which the entire laminated electrode body 30 and the base ends of the pair of tabs 34 are liquid-tightly enclosed by the exterior body 10. An electrolyte (not shown) is stored in the exterior body 10. As shown in FIG. 2, the laminated electrode body 30 is configured by alternately stacking a plurality of negative electrode plates 31 (electrode plates) and a plurality of positive electrode plates 32 (electrode plates) with a plurality of sheet-like separators (not shown) sandwiched therebetween. The negative electrode plates 31 and the positive electrode plates 32 are of a well-known configuration in which a slurry (not shown) made by kneading an active material, a binder, a conductive material, etc. is applied to both sides of a sheet-like base material (not shown) that is rectangular as a whole. A connection portion 33 made of an uncoated portion where the slurry is not applied is formed on the right edge portion of the negative electrode plate 31 and the left side portion of the positive electrode plate 32, respectively. The negative electrode plate 31 and the positive electrode plate 32 are stacked such that their respective connection parts 33 are positioned on opposite sides in the left-right direction. Metallic tabs 34 each having a flat plate shape are fixed to the left and right connection parts 33 in the stacked state so as to be conductive.
[0017] The exterior body 10 is formed by thermally welding two rectangular laminate sheets 11. The laminate sheet 11 has an aluminum sheet-like base material 12 and a seal material 13 made of PP or the like superimposed on the inner surface of the sheet-like base material 12. The seal material 13 forms a mating surface 14 between the laminate sheets 11. The seal material 13 is made of a thermoplastic resin such as polypropylene (PP) having a melting point of about 160°C, for example. The two laminate sheets 11 are arranged so that the seal material 13 faces the other laminate sheet 11 and sandwich the laminated electrode body 30 and the tab 34 in the front-rear direction. A heat-sealed portion 15 is formed around the entire periphery of the outer peripheral edge of the pair of laminate sheets 11. The heat-sealed portion 15 is arranged so as to surround the laminated electrode body 30 in a front-to-back direction.
[0018] The heat-sealed portion 15 has an airtightness maintaining portion 16 and an easily peelable portion 17. The airtightness maintaining portion 16 is a portion having a relatively high welding strength, and the easily peelable portion 17 is a portion having a lower welding strength than the airtightness maintaining portion 16. The outer peripheral edge portion of the laminate sheet 11 is composed of four sides 21, 22L, 22R, 23 on the top, bottom, left and right. In the lower side portion 21, the sealing materials 13 are directly welded to each other over the entire area. The heat-sealed portion 15 of the lower side portion 21 is composed only of the airtightness maintaining portion 16. In both the left and right side portions 22L, 22R, the base end portion of the tab 34 is sandwiched between the laminate sheets 11. The heat-sealed portion 15 of both the left and right side portions 22L, 22R is composed only of the airtightness maintaining portion 16.
[0019] The heat-sealed portion 15 of the upper side portion 23 is composed of two airtightness maintaining portions 16 and one easy peeling portion 17. The airtightness maintaining portions 16 are disposed only at the left and right ends of the upper side portion 23. The easy peeling portion 17 is disposed in the region between the two airtightness maintaining portions 16 of the upper side portion 23. As shown in Figs. 1, 3, and 7, an inclusion 25 is disposed in the airtightness maintaining portion 16. As shown in Figs. 4 to 6, the inclusion 25 is a three-layered sheet material in which one sheet-like holder 26 is sandwiched between two adhesive layers 27. In the drawings, the thicknesses of the sheet-like holder 26 and the adhesive layers 27 are exaggerated. The thickness of the sheet-like holder 26 is, for example, 200 µm, and the thickness of one adhesive layer 27 is, for example, 80 µm.
[0020] The sheet-like holder 26 is made of a nonwoven fabric. The nonwoven fabric is a fabric material having fine communicating spaces (not shown) that open on the surface of the nonwoven fabric and communicate with the inside of the nonwoven fabric. The material of the sheet-like holder 26 is a resin material having a higher melting point than the sealant 13. Specifically, fully aromatic polyethylene having a melting point of about 350°C, polyacrylonitrile (PAN) having a melting point of about 320°C, or the like is used. The material of the adhesive layer 27 is a thermoplastic resin having a melting point lower than the sealant 13. Specifically, modified polypropylene (modified PP) having a melting point of about 130°C to 140°C, or the like is used.
[0021] Next, the manufacturing process of the secondary battery A will be described. The laminated electrode body 30 and the tab 34 are sandwiched between two laminate sheets 11, and of the four sides 21, 22L, 22R, 23 of the outer periphery of the laminate sheet 11, the bottom side 21 and both left and right sides 22L, 22R are thermally welded. This process forms a bag-shaped exterior body 10 with the top side 23 unwelded. Next, electrolyte is injected into the exterior body 10 from the opening of the top side 23.
[0022] Thereafter, a heat-sealing process is performed on the upper side portion 23. For the heat-sealing process, a pair of heat-sealing machines 35 shown in Figures 4 and 5 are used. The heat-sealing machines 35 have a heating function and a pressurizing function. The opposing pressurizing surfaces 36 of the heat-sealing machines 35 are flat surfaces perpendicular to the opposing direction of the heat-sealing machines 35.
[0023] In the heat welding process, the inclusions 25 are placed between the mating surfaces 14 of the two laminate sheets 11 at both the left and right ends of the upper side portion 23, the upper side portion 23 is sandwiched between the heat sealers 35, and the entire area of the upper side portion 23 is heated while being pressed by the pressurizing surface 36. The heating temperature during heat welding is set to a temperature higher than the melting point of the resin material of the sealing material 13 and the adhesive layer 27 and lower than the melting point of the resin material of the sheet-like holder 26. In the heat welding process, the heated sealing material 13 and the adhesive layer 27 are melted, and in the area where the inclusions 25 are placed, the sealing material 13 and the adhesive layer 27 are integrated, and the mixture of the molten sealing material 13 and the adhesive layer 27 enters into the communication space (not shown) of the sheet-like holder 26. In the area where the inclusions 25 are not placed, the sealing materials 13 are integrated with each other.
[0024] In the heat welding process, the sealant 13 and the adhesive layer 27 are heated to a deformable molten state, but the sheet-like holder 26 remains in a solid state without melting or deforming. In the region where the inclusion 25 is arranged, the sealant 13 is crushed to a greater extent by the thickness of the sheet-like holder 26 and the adhesive layer 27. In addition, the molten adhesive layer 27 and the sealant 13 enter the fine communicating spaces of the sheet-like holder 26 from the front and rear sides, providing an anchor effect. As a result, the airtightness maintaining portion 16 with high welding strength is formed in the region of the upper side portion 23 where the inclusion 25 is arranged.
[0025] On the other hand, in the region where the intervening material 25 is not arranged, the amount of crushing of the sealing material 13 is smaller than that in the region where the intervening material 25 is arranged. In addition, the anchor effect of the sheet-like holder 26 is not generated. Therefore, in the region of the upper side portion 23 where the intervening material 25 is not arranged, the easily peelable portion 17 having a lower welding strength than the airtightness maintaining portion 16 is formed. The welding strength of the airtightness maintaining portion 16 formed on the lower side portion 21 and both the left and right side portions 22L, 22R is approximately the same as that of the airtightness maintaining portion 16 of the upper side portion 23. Therefore, the welding strength of the easily peelable portion 17 is lower than that of the airtightness maintaining portion 16 of the lower side portion 21 and both the left and right side portions 22L, 22R.
[0026] When the secondary battery A is used, part of the electrolyte becomes vaporized gas as the temperature rises. When the vaporized gas is generated, the pressure inside the exterior body 10 increases, and as shown in FIG. 7, peeling occurs between the laminate sheets 11 at the easily peelable parts 17 of the upper side part 23. As a result, the vaporized gas is released to the outside of the exterior body 10 from the openings 18 generated by the peeling, so there is no risk of the exterior body 10 bursting. Since the openings 18 are formed only in the upper side part 23, there is no risk of the electrolyte leaking out of the exterior body 10 even if the openings 18 are generated.
[0027] The secondary battery A of the first embodiment includes a laminated electrode body 30 in which a positive electrode plate 32, a negative electrode plate 31, and a separator are laminated, and an exterior body 10 that houses the laminated electrode body 30. The exterior body 10 has two laminate sheets 11 arranged to sandwich the laminated electrode body 30. A heat-sealed portion 15 is formed on the outer periphery of the exterior body 10 by pressurizing the laminated sheets 11 in a heated state to hermetically seal the mating surfaces 14 of the laminate sheets 11. The heat-sealed portion 15 includes an airtightness maintaining portion 16 and an easy peeling portion 17 whose peel strength is lower than that of the airtightness maintaining portion 16. Among the four sides 21, 22L, 22R, and 23 that constitute the outer periphery of the exterior body 10, the airtightness maintaining portion 16 and the easy peeling portion 17 are arranged in a line along the upper side 23.
[0028] According to this configuration, when the internal pressure inside the exterior body 10 rises to a certain level, the easily peelable portion 17 peels off, causing the internal pressure to drop to atmospheric pressure, thereby preventing the exterior body 10 from bursting due to an excessive rise in internal pressure. In addition, the electrolyte stored in the exterior body 10 can be prevented from scattering. Since the easily peelable portion 17 and the airtightness maintaining portion 16 are arranged to be aligned along the upper side portion 23, the portion from which the laminate sheet 11 peels off when the internal pressure rises can be set to a desired region (only the upper side portion 23). This makes it possible to avoid problems such as the electrolyte leaking into an unexpected region when the easily peelable portion 17 peels off.
[0029] The laminate sheet 11 has a sheet-like base material 12 and a sheet-like sealing material 13 that is superimposed on the inner surface of the sheet-like base material 12 to form a mating surface 14. The heat-sealed portion 15 includes an inclusion 25 sandwiched between the mating surfaces 14. The inclusion 25 is disposed only in the region of the airtightness maintaining portion 16 adjacent to the easy peeling portion 17. Since the pressure surface 36 of the heat-sealing machine 35 to the heat-sealed portion 15 is composed of a flat surface, the presence of the inclusion 25 causes the pressure force from the heat-sealing machine 35 to the sealing material 13 in the easy peeling portion 17 to be smaller than the pressure force to the sealing material 13 in the airtightness maintaining portion 16. This difference in pressure force causes a difference in the ease of peeling between the easy peeling portion 17 and the airtightness maintaining portion 16. According to this embodiment 1, the shape of the pressure surface 36 of the heat-sealing machine 35 is simplified.
[0030] The intermediate material 25 includes a sheet-like holder 26 made of a material having a higher melting point than the sealing material 13. The sheet-like holder 26 has communicating spaces that are impregnated with the molten sealing material 13. The sheet-like holder 26 does not melt in the heat welding process, and is therefore maintained in a state in which it exists between the sealing materials 13. The molten sealing material 13 is impregnated into the communicating spaces of the sheet-like holder 26, thereby ensuring the sealing performance and increasing the bonding strength between the sheet-like base material 12 and the intermediate material 25.
[0031] The intermediate material 25 includes an adhesive layer 27 superimposed on the surface of the sheet-like holder 26 facing the mating surface 14 of the laminate sheet 11. The adhesive layer 27 has a melting point lower than that of the sealing material 13. In the thermal welding process, the molten sealing material 13 and the molten adhesive layer 27 are integrated, and the sealing material 13 and the adhesive layer 27 are impregnated into the communicating spaces of the sheet-like holder 26, thereby increasing the bonding strength between the sheet-like base material 12 and the intermediate material 25.
[0032] The secondary battery A of the first embodiment is manufactured through the following first preparation step, second preparation step, and heat welding step. In the first preparation step, a laminated electrode body 30, in which a positive electrode plate 32, a negative electrode plate 31, and a separator are laminated, is sandwiched and surrounded by a laminate sheet 11 constituting an exterior body 10. In the second preparation step, an inclusion 25 is placed on a mating surface 14 of the laminate sheet 11 at an upper side 23 of four sides 21, 22L, 22R, and 23 constituting the outer periphery of the laminate sheet 11. In the heat welding process, a heat welding process is performed in the area of the upper edge portion 23 including the inclusion 25 to form an airtight maintaining portion 16 that hermetically adheres the mating surfaces 14 to each other, and simultaneously with the formation of the airtight maintaining portion 16, a heat welding process is performed in the area of the upper edge portion 23 adjacent to the inclusion 25 to form an easy-to-peel portion 17 that hermetically adheres the mating surfaces 14 to each other with a peel strength lower than that of the airtight maintaining portion 16.
[0033] <Embodiment 2> Next, a second embodiment of the present disclosure will be described with reference to Figs. 8 and 9. A secondary battery B of the second embodiment has a different configuration of the thermally welded portion 15 from that of the first embodiment. Since the other configurations are the same as those of the first embodiment, the same reference numerals are used for the same configurations, and the description of the structure, action, and effect will be omitted.
[0034] The heat-sealed portion 15 of the second embodiment differs from that of the first embodiment in the arrangement and number of the airtightness maintaining portion 16 and the easily peelable portion 17 in the upper side portion 23. The left and right ends of the upper side portion 23 are heat-sealed in the process of forming the airtightness maintaining portion 16 in the left and right side portions 22L, 22R, and therefore function as the airtightness maintaining portion 16 having high welding strength. The airtightness maintaining portion 16 is formed in the left-right center portion of the upper side portion 23 by arranging an inclusion 25 and performing heat welding. In the region of the upper side portion 23 other than the airtightness maintaining portion 16 at the left and right ends and the left-right center portion, the easily peelable portion 17 is formed by heat welding.
[0035] When the internal pressure of the vaporized gas in the exterior body 10 rises to a certain level, the laminate sheet 11 peels off at least one or both of the two easily peelable portions 17 spaced apart on the left and right sides of the upper side portion 23. The vaporized gas in the exterior body 10 is released to the outside from the opening 18 created by the peeling.
[0036] <Embodiment 3> Next, a third embodiment of the present disclosure will be described with reference to Figs. 10 to 11. In the third embodiment, a secondary battery C and a method for manufacturing the secondary battery C are configured differently from those in the first embodiment. Since the other configurations are the same as those in the first embodiment, the same reference numerals are used for the same configurations, and descriptions of the structures, functions, and effects will be omitted.
[0037] The secondary battery C of the present embodiment 3 has a configuration in which no intervening material 25 is disposed in the airtightness maintaining portion 16. The pressure application surface 41 of the heat sealer 40 used in the manufacturing method of the present embodiment 3 has a pair of strong pressure application surfaces 42 and one weak pressure application surface 43. The weak pressure application surface 43 is recessed from the strong pressure application surface 42 in a stepped shape, and is disposed adjacent to the strong pressure application surface 42. The strong pressure application surface 42 is disposed in a position where it applies pressure to both the left and right ends of the upper side portion 23. The weak pressure application surface 43 is disposed adjacent to the region between the pair of strong pressure application surfaces 42. The strong pressure application surface 42 and the weak pressure application surface 43 are heated to the same temperature.
[0038] The secondary battery C of the third embodiment is manufactured through the following preparation process and heat welding process. In the preparation process, a laminated electrode body 30, which is a laminate of a positive electrode plate 32, a negative electrode plate 31, and a separator (not shown), is sandwiched and surrounded by two laminate sheets 11 that constitute an exterior body 10. In the heat welding process, the airtightness maintaining portion 16 and the easily peelable portion 17 are simultaneously formed on the upper side portion 23 of the four side portions 21, 22L, 22R, and 23 that constitute the outer periphery of the laminate sheet 11. The airtightness maintaining portion 16 is formed by abutting the strong pressure surface 42 against the laminate sheet 11 and performing a heat welding process, thereby tightly adhering the mating surfaces 14 of the laminate sheets 11 to each other in an airtight manner. The easy peeling portion 17 is formed by bringing the weak pressure surface 43 into contact with the laminate sheet 11 and carrying out a heat welding process, thereby adhering the mating surfaces 14 together with a peel strength lower than that of the airtightness maintaining portion 16 .
[0039] <Other Examples> The present invention is not limited to the embodiments described above and illustrated in the drawings, and the following embodiments are also included within the technical scope of the present invention. In the first to third embodiments, the easily peelable portion is not limited to being formed on one side, but may be formed on a plurality of sides. In the first to third embodiments, the side portion forming the airtightness maintaining portion and the easy peeling portion is not limited to the upper side portion, and may be a side portion. In the first to third embodiments, the laminated electrode body may be sandwiched between a single laminate sheet folded in half. In this case, heat-sealed portions may be formed on three sides. In embodiments 1 to 3, the inclusion may be a single-layer part made of only nonwoven fabric without an adhesive layer, or may be a two-layer part in which an adhesive layer is laminated on only one side of the nonwoven fabric. In the first to third embodiments, the melting point of the adhesive layer may be the same as that of the sealing material, in which case the sealing material and the adhesive layer may be made of the same material. In the first to third embodiments, the melting point of the adhesive layer may be the same as the melting point of the sealing material. In the second embodiment, a plurality of inclusions may be arranged at intervals in an area other than both ends of one side portion. [Explanation of symbols]
[0040] A,B,C…Secondary battery 10…Exterior body 11...Laminate sheet 12...Sheet-shaped substrate 13...Sealing material 14…Mating surface 15...Heat welding part 16…Airtight section 17...Easy peeling part 23...Top side (at least one side) 21...Bottom side (multiple sides) 22L…Left side (multiple sides) 22R…Right side (multiple sides) 25...Inclusions 26...Sheet-shaped holder 27...adhesive layer 30...Laminated electrode body 31...Negative electrode plate 32…Positive electrode plate 40…Heat seal machine 42…Strong pressure surface 43...Light pressure surface
Claims
1. a laminated electrode body in which a positive electrode plate, a negative electrode plate, and a separator are laminated; and an exterior body that contains the laminated electrode body and has laminate sheets arranged to sandwich the laminated electrode body, A heat-sealed portion is formed on the outer periphery of the exterior body by applying pressure under heating to hermetically seal the mating surfaces of the laminate sheets, The heat-sealed portion includes an airtightness maintaining portion and an easily peelable portion having a peel strength lower than that of the airtightness maintaining portion, A secondary battery in which, in at least one of a plurality of sides constituting the outer peripheral edge of the exterior body, the airtightness maintaining portion and the easily peelable portion are arranged side by side along the side.
2. The laminate sheet has a sheet-like base material and a sheet-like sealing material that is superimposed on the inner surface of the sheet-like base material to form the mating surface, The heat-sealed portion is provided with an inclusion sandwiched between the mating surfaces, The secondary battery according to claim 1 , wherein the inclusion is disposed only in an area of the airtightness maintaining portion adjacent to the easily peelable portion.
3. 3. The secondary battery according to claim 2, wherein the intermediate material includes a sheet-like support having a communicating space for being impregnated with the molten sealing material and made of a material having a melting point higher than that of the sealing material.
4. 4. The secondary battery according to claim 3, wherein the intermediate material is made of a material having a melting point equal to or lower than that of the sealing material, and includes an adhesive layer superposed on a surface of the sheet-like supporting body facing the mating surface.
5. a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; A step of placing an inclusion on a mating surface of the laminate sheet in at least one of a plurality of side portions constituting an outer peripheral edge portion of the laminate sheet; a heat-sealing process is performed in an area of the at least one side portion that includes the inclusion to form an airtightness maintaining portion that hermetically adheres the mating surfaces to each other, and simultaneously with the formation of the airtightness maintaining portion, a heat-sealing process is performed in an area of the at least one side portion that is adjacent to the inclusion to form an easy-peel portion that hermetically adheres the mating surfaces to each other with a peel strength lower than that of the airtightness maintaining portion.
6. A heat sealer is used that has a strong pressure surface and a weak pressure surface adjacent to the strong pressure surface and recessed in a stepped shape from the strong pressure surface, and that can heat the strong pressure surface and the weak pressure surface; a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; A method for manufacturing a secondary battery includes a step of abutting the strong pressure surface against at least one of a plurality of sides constituting an outer peripheral edge portion of the laminate sheet and performing a thermal welding process to form an airtightness maintaining portion in which the mating surfaces are airtightly adhered to each other, and at the same time, abutting the weak pressure surface against the at least one of the sides and performing a thermal welding process to form an easy peeling portion in which the mating surfaces are adhered to each other with a peel strength lower than that of the airtightness maintaining portion.
Citation Information
Patent Citations
Battery cell with venting structure using taping
JP2018521481A
Secondary battery
JP2019087336A
Secondary battery and seal block
JP2023502614A
Adhesive film, electricity storage device, and method for producing electricity storage device
WO2022230951A1
Lithium ion secondary battery
JP2002015713A
Cited By
Non-aqueous electrolytic solution secondary battery and method for producing non-aqueous electrolytic solution secondary battery
WO2026211462A1