Powder for thermal spraying
The thermal spray powder with a double oxide and specific particle size distribution, formed into secondary particles, addresses the challenges of density, surface roughness, and phase separation in thermal spray coatings by enhancing bonding and controlling particle sizes.
Patent Information
- Application Number
- JP2023058418
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
AI Technical Summary
Existing thermal spray powders containing double oxides face challenges in achieving high density, low surface roughness, and reducing phase separation ratios in the resulting coatings.
The thermal spray powder is composed of a double oxide with specific particle size distribution and composition, including metal oxides with a boiling point difference of 500°C or more, and is formed into secondary particles through granulation and sintering to enhance bonding, thereby reducing phase separation and surface roughness.
This configuration results in thermal spray coatings with improved density, reduced surface roughness, and decreased phase separation ratios, achieved through controlled particle sizes and enhanced bonding of primary particles.
Smart Images

Figure 2024145870000003 
Figure 2024145870000004 
Figure 2024145870000005
Abstract
Description
[Technical field]
[0001] The present disclosure relates to thermal spray powders. [Background technology]
[0002] The thermal spray powder disclosed in Patent Document 1 contains a granulated and sintered powder of a double oxide containing yttrium and aluminum. The granulated and sintered powder is composed of secondary particles obtained by granulating and sintering primary particles. The crushing strength of the secondary particles is 15 MPa or more. The 10% particle size of the thermal spray powder is 6 μm or more. When the X-ray diffraction of the thermal spray powder is measured, the ratio of the intensity of the X-ray diffraction peak derived from the (222) plane of yttria to the intensity of the maximum peak among the X-ray diffraction peak derived from the (420) plane of the garnet phase in the double oxide, the X-ray diffraction peak derived from the (420) plane of the perovskite phase in the double oxide, and the X-ray diffraction peak derived from the (-122) plane of the monoclinic phase in the double oxide is 20% or less. The publication states that by using such a thermal spray powder, a thermal spray coating of a double oxide containing yttrium and aluminum can be formed well. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 4560387 Summary of the Invention [Problem to be solved by the invention]
[0004] When using a thermal spray powder containing a double oxide, it is required to obtain a thermal spray coating that is highly dense and has low surface roughness, and to reduce the proportion of phase separation in the thermal spray coating.
[0005] In view of these circumstances, an object of the present invention is to provide a technique for increasing the density, reducing the surface roughness, and decreasing the proportion of phase separation in a thermal spray coating. [Means for solving the problem]
[0006] The thermal spray powder disclosed herein is a thermal spray powder containing a composite oxide including a plurality of metal oxides. The thermal spray powder is determined based on a particle size distribution based on a volumetric cumulative particle size distribution measured by a laser diffraction / scattering type particle size distribution measurement method, and the particle size distribution is determined based on a particle size distribution distribution measured by a laser diffraction / scattering type particle size distribution measurement method, and the particle size distribution distribution distribution measurement method is determined based on a particle size distribution distribution distribution measured by a laser diffraction / scattering type particle size distribution measurement method, and the particle size distribution distribution distribution distribution measurement method is determined based on a particle size distribution distribution distribution measurement method, and the particle size distribution distribution distribution distribution distribution measurement method is determined based on a particle size distribution distribution distribution distribution measurement method, and the particle size distribution distribution distribution distribution distribution distribution distribution measurement method is determined based on a particle size distribution distribution distribution distribution distribution measurement method. 10 ") is 10 μm or more, and the particle size at which the cumulative particle volume from the small particle size side is 50% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method (hereinafter referred to as "particle size D 50 The particle size (sometimes referred to as "particle size distribution") of the thermal spray powder is 40 μm or less. Under a condition of 1 atmosphere, the difference between the maximum and minimum boiling points among the plurality of metal oxides is 500° C. or more. By using a thermal spray powder of this composition, it is possible to increase the density of the thermal spray coating, reduce the surface roughness, and decrease the rate of phase separation.
[0007] In a preferred embodiment of the thermal spray powder disclosed herein, the double oxide contains at least two selected from the group consisting of lanthanoid elements La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu, metalloid elements Si and Ge, typical elements Al and Ga, and transition elements Sc, Y, Ti, Zr, Hf, Nb, Ta, Mo, and W. According to this configuration, the effect of the technology disclosed herein can be appropriately achieved by using a thermal spray powder containing at least two of the above-mentioned elements.
[0008] In a preferred embodiment, the thermal spray powder disclosed herein contains at least two selected from the group consisting of Al, Si, Y, Zr, and Yb. With this configuration, the effects of the technology disclosed herein can be appropriately achieved by using a thermal spray powder containing at least two of the above-mentioned elements.
[0009] In a preferred embodiment of the thermal spray powder disclosed herein, the multiple metal oxides include at least two of Al2O3, SiO2, Y2O3, ZrO2, and Yb2O3. With this configuration, the thermal spray powder is a composite oxide including at least two of the above metal oxides, and thereby the effects of the technology disclosed herein can be appropriately achieved.
[0010] In another preferred embodiment, the thermal spray powder disclosed herein contains a double oxide of Y2O3 and Al2O3, a double oxide of Yb2O3 and SiO2, or a double oxide of SiO2 and Al2O3. By using a thermal spray powder of a double oxide containing the above double oxides, the effects of the technology disclosed herein can be appropriately achieved.
[0011] Preferably, the thermal spray powders disclosed herein are YAlO3, Y4Al2O9, Y3Al5O 12 , Yb2Si2O7, or 3Al2O3·2SiO2. By using a thermal spray powder of a double oxide containing the above double oxides, the effects of the technology disclosed herein can be adequately achieved.
[0012] In another preferred embodiment, the particle diameter D of the thermal spray powder disclosed herein 50 is 23 μm or more and 38 μm or less. With this configuration, the effect of reducing the rate of phase separation in the thermal spray coating can be further enhanced. In addition, an increase in the surface roughness of the thermal spray coating can be suppressed.
[0013] In another preferred embodiment, the particle diameter D of the thermal spray powder disclosed herein 10is 12 μm or more and 21 μm or less. With this configuration, an increase in the surface roughness of the thermal spray coating can be suppressed. In addition, an increase in the surface roughness of the thermal spray coating can be suppressed.
[0014] In another preferred embodiment, the thermal spray powder disclosed herein is composed of secondary particles in which primary particles of the double oxide are bonded to each other. With this composition, the occurrence of phase separation in the thermal spray coating tends to be further suppressed.
[0015] Preferably, the secondary particles are granulated and sintered particles. With this configuration, the occurrence of phase separation in the thermal spray coating tends to be further suppressed.
[0016] In another preferred embodiment, the thermal spray powder disclosed herein is composed of a fused and pulverized powder of a double oxide. With this configuration, the effects of the technology disclosed herein are appropriately achieved. Also, the thermal spray powder can be obtained more easily. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1 is a cross-sectional SEM image of the thermal spray coating of Example 1. [Diagram 2] FIG. 2 is a cross-sectional SEM image of the thermal spray coating of Example 2. [Diagram 3] FIG. 3 is a cross-sectional SEM image of the thermal spray coating of Example 3. [Figure 4] FIG. 4 is a cross-sectional SEM image of the thermal spray coating of Example 4. [Diagram 5] FIG. 5 is a cross-sectional SEM image of the thermal spray coating of Example 5. [Figure 6] FIG. 6 is a cross-sectional SEM image of the thermal spray coating of Example 6. [Figure 7] FIG. 7 is a cross-sectional SEM image of the thermal spray coating of Example 7. [Figure 8] FIG. 8 is a cross-sectional SEM image of the thermal spray coating of Example 8. [Figure 9] FIG. 9 is a cross-sectional SEM image of the thermal spray coating of Example 9. [Figure 10] FIG. 10 is a cross-sectional SEM image of the thermal spray coating of Example 10. [Figure 11] FIG. 11 is a cross-sectional SEM image of the thermal spray coating of Example 11. [Figure 12] FIG. 12 is a cross-sectional SEM image of the thermal spray coating of Example 12. [Figure 13] FIG. 13 is a cross-sectional SEM image of the thermal spray coating of Example 13. [Figure 14] FIG. 14 is a cross-sectional SEM image of the thermal spray coating of Example 14. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] A preferred embodiment of the technology disclosed herein will be described below. Matters other than those specifically mentioned in this specification and necessary for implementing the present invention can be understood as design matters for a person skilled in the art based on the prior art in the relevant field. The technology disclosed herein can be implemented based on the contents disclosed in this specification and the technical common sense in the relevant field. In the specification, the expression "X to Y" indicating a numerical range means "X or more and Y or less" unless otherwise specified, and also means a range "greater than X and less than Y", a range "greater than X and less than Y", and a range "greater than X and less than Y".
[0019] <Definition> In this specification, the term "thermal spray powder" refers to a powdered material used for thermal spraying. In addition, in this specification, the term "composite particle" refers to a particulate matter (in the form of a particle) that is composed of a plurality of different materials, and the plurality of materials are bonded together to behave as a single particle. Examples of the composite particle include granulated particles and granulated sintered particles composed of at least two or more types of materials. In addition, in this specification, the term "primary particle" refers to the smallest unit that can be identified as a granular matter from the appearance among the morphological components that make up the thermal spray powder. Therefore, when the composite particle that makes up the thermal spray powder disclosed here includes a secondary particle, for example, the particle that makes up the secondary particle is called a primary particle. Here, the term "secondary particle" refers to a particulate matter in which the primary particles are bonded three-dimensionally to behave as a single particle. Examples of the "secondary particle" referred to here include granulated particles and particles sintered after granulation (granulated sintered particles).
[0020] The term "bonding" as used herein refers to the direct or indirect bonding of two or more primary particles. Examples of "bonding" include bonding between primary particles by chemical reaction, bonding between primary particles attracting each other by simple adsorption, bonding using the anchor effect of allowing an adhesive or the like to penetrate into the unevenness of the primary particle surface, bonding between primary particles using the effect of attraction due to static electricity, and bonding in which the surfaces of primary particles are melted and integrated. In addition, with respect to secondary particles composed of two or more materials, "bonding" includes bonding in which one material constitutes the primary particles and the other material is melted and integrated with the primary particles. In addition, in this specification, the term "raw material particles" refers to particles that constitute the powder in the raw material stage used to prepare the thermal spray powder disclosed herein.
[0021] <Method of measuring particle size> In this specification, "particle diameter D 10 " refers to the particle size at which the cumulative particle volume from the small particle size side is 10% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method. 50" refers to the particle size at which the cumulative particle volume from the small particle size side is 50% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method. For example, a commercially available measuring device is used to measure the particle size.
[0022] When a thermal spray powder containing a double oxide containing a plurality of metal oxides is sprayed, for example, a difference in composition occurs between splats (melted and flattened particles), and a thermal spray coating having a non-uniform composition may be formed. For example, among the plurality of metal oxides contained in the double oxide, a metal oxide having a relatively low boiling point may be vaporized during spraying, and an altered phase may be locally formed in the thermal spray coating in addition to the main phase consisting of the double oxide. The altered phase may be a phase consisting of a metal oxide having a relatively high boiling point, or a phase containing a larger amount of a metal oxide having a relatively high boiling point. The present inventors wanted to reduce the proportion of phase separation (i.e., the proportion of altered phase) in the thermal spray coating when producing a thermal spray coating by spraying such a double oxide. For this reason, the present inventors investigated the composition of the thermal spray powder.
[0023] <Composition of thermal spray powder> The thermal spray powder disclosed herein contains, for example, a double oxide. The thermal spray powder is preferably made of a double oxide powder, but may contain unavoidable impurities resulting from the manufacturing process of the double oxide powder, etc. The content of the unavoidable impurities in the entire thermal spray powder is generally 5 mass% or less, preferably 3 mass% or less, more preferably 1 mass% or less, even more preferably 0.5 mass% or less, particularly preferably 0.1 mass% or less, and the closer to 0 mass%, the better.
[0024] The composite oxide includes, for example, a plurality of metal oxides. Here, under a condition of 1 atmosphere, the difference between the maximum and minimum boiling points among the plurality of metal oxides is 500°C or more. It can be said that the greater the difference between the maximum and minimum boiling points of the plurality of metal oxides included in the composite oxide, the more likely phase separation occurs in the formed thermal spray coating. Therefore, from the viewpoint of better realizing the effects of the technology disclosed herein, the difference between the maximum and minimum boiling points described above is, for example, 700°C or more, preferably 1000°C or more, more preferably 1100°C or more, and even more preferably 1200°C or more or 1300°C or more. On the other hand, from the same viewpoint, the difference between the maximum and minimum boiling points described above is preferably about 3000°C or less, and may be, for example, 2500°C or less, or 2300°C or less.
[0025] The plurality of metal oxides may include at least two metal oxides selected from various metal oxides, the difference between the maximum and minimum boiling points of which is 500° C. or more under a condition of 1 atmosphere. Examples of metal oxides include semimetal elements such as silicon (Si), germanium (Ge), antimony (Sb), and bismuth (Bi); typical elements such as magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), zinc (Zn), aluminum (Al), gallium (Ga), indium (In), tin (Sn), and lead (Pb); scandium (Sc), yttrium (Y), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), and the like. Examples of oxides include transition elements such as molybdenum (Mo), tungsten (W), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), copper (Cu), silver (Ag), and gold (Au); and lanthanide elements such as lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), samarium (Sm), terbium (Tb), europium (Er), gadolinium (Gd), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), and lutetium (Lu).
[0026] Examples of metal oxides include alumina, zirconia, yttria, chromia, titania, cobalt oxide, magnesia, silica, calcia, ceria, iron oxide, nickel oxide, silver oxide, copper oxide, zinc oxide, gallium oxide, germanium oxide, strontium oxide, scandium oxide, samarium oxide, bismuth oxide, lanthanum oxide, lutetium oxide, hafnium oxide, vanadium oxide, niobium oxide, tungsten oxide, manganese oxide, tantalum oxide, terbium oxide, europium oxide, gadolinium oxide, dysprosium oxide, holmium oxide, erbium oxide, thulium oxide, praseodymium oxide, ytterbium oxide, neodymium oxide, tin oxide, antimony oxide, and molybdenum oxide.
[0027] Regarding the boiling points of metal oxides, for example, the following documents 1 to 3 can be referred to. ·Reference 1: G. Vesamsonov. The Latest Handbook of Oxides -Physical and Chemical Properties-, 2nd revised and expanded edition. Japan-Soviet Press, 1979, 209. ·Reference 2: Ginya Adachi. Science of rare earths. Kagaku Doujin, 1999, 198. (Source: HAIRE, RG, et al. Handbook on the Physics and Chemistry of Rare Earth, vol. 18: Lanthanide / Actinide Chemistry. 1994.) ·Reference 3: Chemical Society of Japan. Basic Chemistry Handbook (Revised 6th Edition). 2021.
[0028] For example, the boiling points of Ga2O3, GeO2, and Ta2O5 can be found in the above-mentioned reference 1 (G. Vesamsonov. The Latest Handbook of Oxides - Physical and Chemical Properties, 2nd Revised and Expanded Edition. Nisso Tsushinsha, 1979, 209.). The boiling points of Yb2O3, CeO2, Nd2O3, Sm2O3, Eu2O3, Gd2O3, Dy2O3, Ho2O3, Er2O3, Tm2O3, Lu2O3, and Pr2O3 can be found in the above-mentioned reference 2 (G. Adachi. Science of Rare Earths. Kagaku Dojin, 1999, 198. (Source: HAIRE, RG, et al. Handbook on the Physics and Chemistry of Rare Earth, vol. 18: Lanthanide / Actinide Chemistry. 1994.)). For the boiling points of Y2O3, Al2O3, SiO2, ZrO2, WO3, and La2O3, please refer to the boiling points listed in the above-mentioned reference 3 (Chemical Society of Japan. Basic Chemistry Handbook (Revised 6th Edition). 2021.). For the boiling point of SiO2, please refer to the boiling point of tridymite (2230 ° C).
[0029] From the viewpoint of preferably achieving the effects of the technology disclosed herein, it is preferable that the composite oxide contains at least two of the following: lanthanoid elements, such as La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu; semi-metal elements, such as Si and Ge; typical elements, such as Al and Ga; and transition elements, such as Sc, Y, Ti, Zr, Hf, Nb, Ta, Mo, and W.
[0030] From the viewpoint of preferably achieving the effects of the technology disclosed herein, the thermal spray powder preferably contains at least two elements selected from the group consisting of Al, Si, Y, Zr, and Yb. The thermal spray powder preferably contains a double oxide containing at least two elements out of these five elements. The metal oxide contained in the double oxide preferably contains at least one or two of alumina (Al2O3), silica (SiO2), yttria (Y2O3), zirconia (ZrO2), and ytterbium oxide (Yb2O3). The double oxide is preferably, for example, a double oxide of yttria (Y2O3) and alumina (Al2O3), a double oxide of ytterbium oxide (Yb2O3) and silica (SiO2), or a double oxide of silica (SiO2) and alumina (Al2O3).
[0031] In this case, the double oxide is, for example, YAlO3 (yttrium aluminum perovskite; YAP), Y4Al2O9 (yttrium aluminum monoclinic; YAM), Y3Al5O 12 The double oxide may contain yttrium aluminum garnet (YAG), Yb2Si2O7 (ytterbium disilicate; YbDS), or 3Al2O3·2SiO2 (mullite). By containing such a compound, the double oxide can better reduce the rate of phase separation in the thermal spray coating. Alternatively, the double oxide may contain, for example, a double oxide of zirconia (ZrO2) and alumina (Al2O3), a double oxide of zirconia (ZrO2) and silica (SiO2), a double oxide of ytterbium oxide (Yb2O3) and alumina (Al2O3), or a double oxide of yttria (Y2O3) and silica (SiO2). Alternatively, the double oxide may contain a double oxide containing three or more components, such as a double oxide of yttria (Y2O3), alumina (Al2O3), and silica (SiO2).
[0032] The double oxide is not limited to the above. The double oxide may include, for example, a double oxide of hafnium oxide (HfO2) and alumina (Al2O3), a double oxide of hafnium oxide (HfO2) and silica (SiO2), a double oxide of titania (TiO2) and silica (SiO2), a double oxide of lanthanum oxide (La2O3) and silica (SiO2), and a double oxide of lanthanum oxide (La2O3) and alumina (Al2O3).
[0033] However, the inventors' investigations have revealed that as the proportion of small particles in a thermal spray powder containing a double oxide increases, metal oxides with relatively low boiling points vaporize during thermal spraying, making it easier for phase separation to occur in the thermal spray coating. The inventors have also found that as the proportion of large particles in a thermal spray powder increases, the porosity of the thermal spray coating tends to increase and the surface roughness tends to increase. As a result of the inventors' intensive investigations, it has been found that by using a thermal spray powder having a predetermined particle size distribution, it is possible to increase the density, reduce the surface roughness, and reduce the proportion of phase separation in a thermal spray coating made of a thermal spray powder containing a double oxide.
[0034] The thermal spray powder disclosed herein has a particle diameter D 10 It is preferable that the particle size D is 10 μm or more. 10 As the particle diameter D increases, for example, the proportion of small particles in the particle size distribution of the entire thermal spray powder decreases. 10 The larger the particle diameter D 10 is preferably 11 μm or more, more preferably 12 μm or more, more preferably 15 μm or more, and even more preferably 20 μm or more. On the other hand, from the viewpoint of suppressing an increase in the surface roughness of the thermal spray coating, the particle diameter D 10 is, for example, 40 μm or less, preferably 35 μm or less, more preferably 33 μm or less, more preferably 30 μm or less, more preferably 27.5 μm or less, and even more preferably 21 μm or less. 10 is 12 μm to 21 μm.
[0035] The thermal spray powder disclosed herein has a particle diameter D 50 The particle size D is preferably 40 μm or less. 50 The smaller the particle diameter D, the denser the thermal spray coating becomes and the smaller the surface roughness tends to be. 50 On the other hand, from the viewpoint of suppressing an increase in the rate of phase separation in the thermal spray coating, the particle diameter D 50 is preferably 15 μm or more, more preferably 20 μm or more, and even more preferably 23 μm or more. 50 is 23μm to 38μm.
[0036] The thermal spray powder disclosed herein may be composed of composite particles produced by mixing, for example, multiple types of metal oxide particles (metal oxide powder) contained in a multiple oxide. Composite particles are particles containing different materials, namely multiple types of metal oxide particles, which are integrated with each other and behave as a single particle. The thermal spray powder may be composed of, for example, secondary particles (composite particles) in which primary particles of a multiple oxide are bonded to each other. By forming the thermal spray powder from secondary particles (composite particles) of a multiple oxide, it is possible to reduce the risk of metal oxides with relatively low boiling points vaporizing during thermal spraying. This makes it possible to reduce the proportion of phase separation in the thermal spray coating.
[0037] The form of the secondary particles (composite particles) is not limited, so long as, for example, primary particles of the double oxide are integrated and the effect of the technology disclosed herein can be realized. The thermal spray powder disclosed herein preferably includes, for example, granulated sintered particles. In other words, the secondary particles are preferably granulated sintered particles. In this case, it is preferable that granulated particles are produced first. In this case, the granulated particles can be produced, for example, by combining and mixing multiple types of metal oxide particles (primary particles) contained in the double oxide with any other component (for example, a binder, a solvent, etc.) and granulating the mixture. Alternatively, the granulated particles can also be produced by combining and mixing primary particles of the double oxide with any other component (for example, a binder, a solvent, etc.) and granulating the mixture.
[0038] In the granulated and sintered particles, the primary particles of the double oxide are integrated by sintering. Such bonding is achieved, for example, by sintering at least a portion of the primary particles of the double oxide. Therefore, in the granulated and sintered particles, the primary particles are bonded more firmly to each other by sintering, and the secondary particles are less likely to break during the thermal spraying process. This makes it difficult for metal oxides with relatively low boiling points to vaporize, and the proportion of phase separation in the thermal spray coating can be reduced. In addition, by making the boiling point difference between the oxides contained in each double oxide a predetermined value or more, it is possible to suppress the vaporization of metal oxides with relatively low boiling points, and ultimately to reduce the proportion of phase separation in the thermal spray coating.
[0039] <Method of manufacturing thermal spray powder> The thermal spray powder disclosed herein can be prepared, for example, by mixing, as raw material particles (raw material powder), multiple types of metal oxide particles (metal oxide powders) contained in a double oxide that is the material of the thermal spray powder together with other optional components, compounding, and sintering. The thermal spray powder may be, for example, a thermal spray powder constituted of granulated and sintered particles as secondary particles in which the primary particles are three-dimensionally bonded with gaps between them, the primary particles being formed by mixing, granulating, and sintering the raw material particles (primary particles).
[0040] When the thermal spray powder disclosed herein is composed of granulated and sintered particles, a method for producing the thermal spray powder can include, for example, a granulation step, a firing step, a crushing step, and a classification step.
[0041] The granulation process is, for example, a process of granulating raw material particles. In this process, for example, multiple types of metal oxide particles are prepared so that a desired composition ratio can be achieved for the composite oxide contained in the thermal spray powder, and the surfaces of the particles are stabilized with a protective agent or the like as necessary. Next, the stabilized raw material particles are dispersed in an appropriate solvent together with a binder as an optional component added as necessary, various additives (e.g., dispersants), and the like to prepare a dispersion. For example, a mixer such as a homogenizer or a blade stirrer, a disperser, or the like is used to disperse the raw material particles in the solvent. Next, granulated particles are produced using the obtained dispersion by using a granulation method such as wet granulation.
[0042] Examples of the granulation method include rolling granulation, fluidized bed granulation, stirring frame granulation, crushing granulation, melt granulation, spray granulation, and microemulsion granulation. Among them, the spray granulation method is a preferred granulation method. According to the spray granulation method, droplets are formed from the dispersion (spray liquid) obtained as described above. The droplets are carried by an air flow and passed through a spray drying device (spray dryer), thereby producing granulated particles.
[0043] The concentration of the raw material particles in the spray liquid is preferably, for example, 10% by mass to 80% by mass. Examples of the binder to be added include binding agents (e.g., polyvinyl butyral resin (PVB), polyvinyl alcohol resin (PVA), polyvinyl acetate resin, polyacrylic resin, etc.). For example, water can be used as the solvent. The amount of binder to be added is preferably adjusted to a ratio of 0.05% by mass to 10% by mass (e.g., 1% by mass to 5% by mass) relative to the mass of the raw material particles.
[0044] The firing step is, for example, a step of firing the granulated particles. In the firing step, the granulated particles are fired at a predetermined temperature (approximately 1000° C. to 2000° C.) for 1 hour to 10 hours in an air atmosphere; an inert atmosphere such as a nitrogen atmosphere or a rare gas atmosphere; or in a vacuum. The predetermined temperature may be, for example, the set temperature of a firing furnace. The temperature and time when firing the granulated particles can be appropriately set so as to achieve the desired composition, etc. of the thermal spray powder.
[0045] The crushing step is, for example, a step of crushing the fired product obtained in the firing step. The fired product may be crushed, for example, by a crusher. As the crusher, for example, a jaw crusher, a cone crusher, a hammer crusher, a roll crusher, a stone mill type crusher, etc. are preferably used. The crushing step can produce granulated sintered particles in the form of secondary particles in which primary particles are bonded (sintered) with gaps. The degree of crushing the fired product in this step can be appropriately set so as to achieve, for example, a desired particle size distribution of the secondary particles.
[0046] The classification step is, for example, a step of classifying the secondary particles obtained in the crushing step. This allows the particle size distribution of the secondary particles to be adjusted as desired. For the classification step, for example, in addition to classification using a sieve, a classifier such as an air classifier utilizing the Coanda effect, a swirling air classifier, a forced vortex centrifugal classifier, or a semi-free vortex centrifugal classifier is used.
[0047] As described above, the method for producing a thermal spray powder has been described with reference to a case in which the thermal spray powder is composed of granulated and sintered particles. However, the thermal spray powder does not necessarily have to be composed of granulated and sintered particles. The thermal spray powder may be composed of a molten and pulverized powder of a double oxide in another form. In producing the molten and pulverized powder, for example, first, a double oxide powder is prepared as a raw material. Next, the double oxide powder is heated and melted in an electric furnace or the like to obtain a molten liquid of the double oxide. Next, the molten liquid of the double oxide is rapidly cooled and solidified to obtain a solidified product. Next, the solidified product is crushed and classified, whereby a molten and pulverized powder of the double oxide as the thermal spray powder can be produced. By forming the thermal spray powder from a molten and pulverized powder of the double oxide, the thermal spray powder can be obtained more easily.
[0048] <Applications of thermal spray powder> By spraying the thermal spray powder disclosed herein by various thermal spraying methods, thermal spray coatings can be produced on various substrates. The thermal spray powder can be particularly preferably used to produce thermal spray coatings by plasma spraying methods such as atmospheric plasma spraying (APS), low pressure plasma spraying (LPS), and high pressure plasma spraying. The thermal spray powder can also be suitably used for high velocity flame spraying such as high velocity oxygen flame (HVOF) thermal spraying, warm spray thermal spraying, and high velocity air flame (HVAF) thermal spraying. The thermal spray powder may be supplied to a thermal spraying device in a powder state, or may be supplied to a thermal spraying device in a slurry state in which the powder is dispersed in a suitable dispersion medium.
[0049] The type of substrate used to produce the thermal spray coating is not particularly limited. Examples of substrates include aluminum, aluminum alloys, iron, steel, copper, copper alloys, nickel, nickel alloys, gold, silver, bismuth, manganese, zinc, and zinc alloys. Among these, preferred examples of substrates include steels, such as various SUS materials (which may be so-called stainless steels), which are used as corrosion-resistant structural steels among commonly used metal materials, aluminum alloys, such as 1000 series to 7000 series aluminum alloys, which are useful as lightweight structural materials, and Ni-based, Co-based, and Fe-based corrosion-resistant alloys, such as Hastelloy, Inconel, Stellite, and Invar.
[0050] As described above, the thermal spray powder disclosed herein contains a composite oxide containing a plurality of metal oxides. The thermal spray powder has a particle diameter D at which the cumulative particle volume from the small particle diameter side is 10% of the total particle volume in a volume-based cumulative particle diameter distribution based on a laser diffraction / scattering particle size distribution measurement method. 10 The particle diameter D is 10 μm or more, and the particle diameter D is the particle diameter at which the cumulative particle volume from the small particle side is 50% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method. 50 Under a condition of 1 atmospheric pressure, the difference between the maximum and minimum boiling points among the plurality of metal oxides is 500° C. or more.
[0051] Thermal spray powder contains a complex oxide that contains multiple metal oxides, which makes it possible to produce a thermal spray coating composed of complex oxides. Thermal spray powder has a particle diameter D of 10 μm or more in the volume-based particle size distribution based on the laser diffraction scattering method. 10 This reduces the proportion of small particles. This makes it difficult for metal oxides with relatively low boiling points to vaporize during the thermal spraying process, and reduces the proportion of phase separation in the thermal spray coating. In addition, the thermal spray powder has a particle diameter D of 40 μm or less. 50As a result, the particle size distribution of the thermal spray powder is generally sharp. This makes it possible to reduce the porosity of the thermal spray coating. Also, it is possible to reduce the surface roughness of the thermal spray coating.
[0052] Test examples relating to the present invention will be described below, but it is not intended that the present invention be limited to those shown in the following test examples.
[0053] <Production Example 1. Thermal spray powder containing a double oxide of Y2O3 and Al2O3> (Example 1) The raw powder has an average particle size of D 50 Yttrium oxide powder (primary particles) with an average particle diameter of 1 μm and 50 The aluminum oxide powder (primary particles) having a diameter of 0.5 μm was mixed with the aluminum oxide powder and dispersed in an aqueous solution containing 2 mass % of a binder (PVA) to prepare a slurry. This slurry was sprayed into an air stream using a spray granulator and dried to produce granulated particles. The obtained granulated particles were subjected to a firing process at 1600° C. for 6 hours in an air atmosphere to sinter the primary particles and produce a fired product. The fired product was crushed. Then, sieve classification and air stream classification were performed to obtain a thermal spray powder composed of granulated and sintered particles (secondary particles) with a uniform particle size. This thermal spray powder was used as the thermal spray powder of this example. The particle diameter D in this example was 1.0 μm. 10 is 11.4 μm, and the particle diameter D 50 The composition and particle size distribution of the thermal spray powder of this example are shown in the corresponding columns of Table 1.
[0054] (Example 2 to Example 11) The mixing ratio (mass ratio) of the yttrium oxide powder and the aluminum oxide powder in the raw material powder, the firing conditions, and the classification conditions were appropriately changed in producing the thermal spray powder of Example 1. In this way, the thermal spray powder of each example was produced, which was composed of granulated and sintered particles of a double oxide having the composition and particle size distribution shown in the corresponding column of Table 1.
[0055] <Production Example 2. Thermal spray powder containing a double oxide of Yb2O3 and SiO2> (Example 12 to Example 14) The raw powder is a fused and crushed powder with an average particle size of D 50 Ytterbium silicate powder with a particle size of 23 μm was prepared. The raw powder was subjected to sieve classification and air flow classification. As a result, thermal spray powders composed of fused pulverized powder with a uniform particle size distribution were produced. The classification conditions were changed appropriately to produce the thermal spray powders of each example. The composition and particle size distribution of the thermal spray powders of each example are shown in the corresponding columns of Table 2.
[0056] <Evaluation 1. Particle size distribution> For each example of thermal spray powder, a volumetric particle size distribution was measured using a laser diffraction particle size distribution analyzer (Malvern Panalytical, Mastersizer 3000). In this particle size distribution, the cumulative value from the fine particle side was 3%. The particle sizes at 5%, 10%, 50%, and 90% were obtained. The results are shown in the corresponding columns of "Dx(3)", "Dx(5)", "Dx(10)", "Dx(50)", and "Dx(90)" in Tables 1 and 2. In addition, the percentages (%) of particles having particle sizes of less than 25 μm, 20 μm or less, 15 μm or less, 10 μm or less, and 5 μm or less were obtained in the above particle size distribution. The results are shown in the corresponding columns of Tables 1 and 2 under "%-lower (25) μm," "%-lower (20) μm," "%-lower (15) μm," "%-lower (10) μm," and "%-lower (5) μm."
[0057] <Preparation of thermal spray coating> Using the thermal spray powder of each example, a thermal spray coating was produced by atmospheric pressure plasma spraying. The substrate used was an aluminum alloy (Al6061) plate (70 mm x 50 mm x 2.3 mm) whose surface was roughened by blasting with brown alumina abrasive (A#40). The thermal spraying conditions were as follows: Thermal spray machine: SG-100 (Praxair) Powder feeder: Model 1264 (Praxair) Plasma working gas: Argon (Ar) gas (50 psi (0.34 MPa)); and Helium (He) gas (50 psi (0.34 MPa)) Plasma power: 36kW Plasma generation voltage: 40V Plasma generation current: 900A Spray powder supply rate: 20g / min Spray distance (distance from spray gun to substrate): 120mm
[0058] <Evaluation 2. Surface roughness (Ra)> The surface roughness (arithmetic mean roughness) Ra of the thermal spray coating produced using each example of the thermal spray powder was measured in accordance with JIS B0601:2013. The surface roughness Ra was measured at five arbitrary points on each thermal spray coating using a surface roughness measuring device (SV-3000S CNC, manufactured by Mitutoyo Corporation), and the arithmetic mean value of these values was obtained as the surface roughness Ra. The results are shown in the "Ra" column of Tables 1 and 2.
[0059] <Evaluation 3. Cross-sectional structure of thermal spray coating> For the thermal spray coatings produced using the thermal spray powders of each example, the ratios of pores / altered phases / main phases of each thermal spray coating were measured by using images obtained by observing the surface (cross section of the thermal spray coating) perpendicular to the surface when the coating was viewed in plan view with an SEM. Specifically, the thermal spray coating was first cut perpendicularly to the substrate surface together with the substrate, and the surface to be observed (cross section of the thermal spray coating) was cut out. The cross section was observed with an SEM to obtain a cross-sectional SEM observation image. The cross-sectional SEM observation image was analyzed using image analysis software (Image-Pro Plus, manufactured by Nippon Roper Co., Ltd.) to calculate the ratios of pores / altered phases / main phases to the total cross-sectional area. Here, a binarization process was performed to separate pores from other parts (altered phase and main phase), and the pore ratio (porosity) (%) defined as the ratio of the area of pores to the total cross-sectional area was calculated. Next, a binarization process was performed in the same manner to separate the altered phase from other parts (pores and main phase), and the altered phase ratio (%), which is defined as the ratio of the area of the altered phase to the total cross-sectional area, was calculated using the following formula (A): Pore ratio (%) + altered phase ratio (%) + main phase ratio (%) = 100 (%) (A) Based on this, the main phase ratio (%) was calculated by subtracting the pore ratio (porosity) and altered phase ratio from the total cross-sectional area. The results are shown in the "Porosity (%)", "Altered phase (%)", and "Main phase (%)" columns in Tables 1 and 2.
[0060] For reference, cross-sectional SEM images of the thermal spray coating of each example are shown in Figs. 1 to 14. The scale bar in each figure indicates 100 µm. Fig. 1 is a cross-sectional SEM image of the thermal spray coating of Example 1. Fig. 2 is a cross-sectional SEM image of the thermal spray coating of Example 2. Fig. 3 is a cross-sectional SEM image of the thermal spray coating of Example 3. Fig. 4 is a cross-sectional SEM image of the thermal spray coating of Example 4. Fig. 5 is a cross-sectional SEM image of the thermal spray coating of Example 5. Fig. 6 is a cross-sectional SEM image of the thermal spray coating of Example 6. Fig. 7 is a cross-sectional SEM image of the thermal spray coating of Example 7. Fig. 8 is a cross-sectional SEM image of the thermal spray coating of Example 8. Fig. 9 is a cross-sectional SEM image of the thermal spray coating of Example 9. Fig. 10 is a cross-sectional SEM image of the thermal spray coating of Example 10. Fig. 11 is a cross-sectional SEM image of the thermal sprayed coating of Example 11. Fig. 12 is a cross-sectional SEM image of the thermal sprayed coating of Example 12. Fig. 13 is a cross-sectional SEM image of the thermal sprayed coating of Example 13. Fig. 14 is a cross-sectional SEM image of the thermal sprayed coating of Example 14.
[0061] [Table 1]
[0062] Regarding Examples 1 to 11, in the cases where Ra was less than 7 μm, the porosity was less than 7%, and the altered phase was less than 5%, it was evaluated that the proportion of phase separation in the thermal spray coating was reduced, the density was improved, and the increase in surface roughness was suppressed. As shown in Table 1, the composite oxide containing yttrium oxide and aluminum oxide (here, YAG: Y3Al5O 12 , YAP: YAlO3, or YAM: Y4Al2O9) for thermal spray powders with particle diameter D 10 is 10 μm or more, and the particle diameter D 50It was found that the thermal spray powders of Examples 1 to 7, in which the particle size is 40 μm or less and the difference between the maximum and minimum boiling points among multiple metal oxides (here, yttrium oxide and aluminum oxide) is 500° C. or more under a condition of 1 atmosphere, can form a thermal spray coating in which phase separation is suppressed, density is improved, and an increase in surface roughness is suppressed.
[0063] [Table 2]
[0064] Regarding Examples 12 to 14, in the cases where Ra was less than 7 μm, the porosity was less than 7%, and the altered phase was less than 8%, it was evaluated that the proportion of phase separation in the thermal spray coating was reduced, the density was improved, and the increase in surface roughness was suppressed. As shown in Table 2, for the thermal spray powder containing a double oxide containing ytterbium oxide and silica (here, YbDS:Yb2Si2O7), the particle diameter D 10 is 10 μm or more, and the particle diameter D 50 It was found that the thermal spray powder of Example 12, in which the particle size was 40 μm or less and the difference between the maximum and minimum boiling points among the multiple metal oxides (here, ytterbium oxide and silica) was 500° C. or more under a condition of 1 atmosphere, made it possible to form a thermal spray coating in which phase separation was suppressed, density was improved, and an increase in surface roughness was suppressed.
[0065] Although specific examples of the technology disclosed herein have been described above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and alterations of the specific examples exemplified above.
[0066] The technology disclosed herein includes the inventions relating to items 1 to 11 below. [Item 1] A thermal spray powder containing a double oxide including a plurality of metal oxides, The particle diameter D at which the cumulative particle volume from the small particle size side becomes 10% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method 10 is 10 μm or more, and The particle diameter D at which the cumulative particle volume from the small particle size side becomes 50% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method 50 is 40 μm or less, The thermal spray powder has a difference between the maximum and minimum boiling points of the plurality of metal oxides of 500° C. or more under a condition of 1 atmospheric pressure. [Item 2] 2. The thermal spray powder according to Item 1, wherein the double oxide contains at least two of the lanthanoid elements La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu, the semimetal elements Si and Ge, the typical elements Al and Ga, and the transition elements Sc, Y, Ti, Zr, Hf, Nb, Ta, Mo, and W. [Item 3] 3. The thermal spray powder according to item 1 or 2, containing at least two selected from the group consisting of Al, Si, Y, Zr, and Yb. [Item 4] 4. The thermal spray powder according to any one of items 1 to 3, wherein the plurality of metal oxides include at least two of Al2O3, SiO2, Y2O3, ZrO2, and Yb2O3. [Item 5] 5. The thermal spray powder according to any one of items 1 to 4, comprising a double oxide of Y2O3 and Al2O3, a double oxide of Yb2O3 and SiO2, or a double oxide of SiO2 and Al2O3. [Item 6] YAlO3, Y4Al2O9, Y3Al5O 12 6. The thermal spray powder according to any one of items 1 to 5, comprising: [Item 7] The particle diameter D 50 7. The thermal spray powder according to any one of items 1 to 6, wherein the particle size is 23 μm or more and 38 μm or less. [Item 8] The particle diameter D 10 8. The thermal spray powder according to any one of items 1 to 7, wherein the particle size is 12 μm or more and 21 μm or less. [Item 9] 9. The thermal spray powder according to any one of items 1 to 8, wherein primary particles of the double oxide are composed of secondary particles bonded to each other. [Item 10] Item 10. The thermal spray powder according to item 9, wherein the secondary particles are granulated and sintered particles. [Item 11] 9. The thermal spray powder according to any one of items 1 to 8, which is constituted by a fused and pulverized powder of the double oxide.
Claims
1. A thermal spray powder containing a double oxide including a plurality of metal oxides, The particle diameter D at which the cumulative particle volume from the small particle size side becomes 10% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method. 10 is 10 μm or more, and The particle diameter D at which the cumulative particle volume from the small particle size side becomes 50% of the total particle volume in the volume-based cumulative particle size distribution based on the laser diffraction scattering particle size distribution measurement method. 50 is 40 μm or less, The thermal spray powder has a difference between the maximum and minimum boiling points of the plurality of metal oxides of 500° C. or more under a condition of 1 atmospheric pressure.
2. 2. The thermal spray powder according to claim 1, wherein the double oxide contains at least two of the following: lanthanoid elements: La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu; semi-metal elements: Si and Ge; typical elements: Al and Ga; and transition elements: Sc, Y, Ti, Zr, Hf, Nb, Ta, Mo, and W.
3. The thermal spray powder according to claim 1 or 2, which contains at least two selected from the group consisting of Al, Si, Y, Zr, and Yb.
4. The plurality of metal oxides are Al 2 O 3 , SiO 2 , Y 2 O 3 , ZrO 2 , and Yb 2 O 3 The thermal spray powder according to claim 1 , comprising at least two of:
5. Y 2 O 3 and Al 2 O 3 and Yb 2 O 3 and SiO 2 or SiO 2 and Al 2 O 3 The thermal spray powder according to claim 1 or 2, which contains a double oxide of
6. YAlO 3 , Y 4 A 2 O 9 , Y 3 A 5 O 12 , Yb 2 S 2 O 7 , or 3Al 2 O 3 2SiO 2 The thermal spray powder of claim 5 , comprising:
7. The particle diameter D 50 The thermal spray powder according to claim 1 or 2, wherein the average particle size is 23 μm or more and 38 μm or less.
8. The particle diameter D 10 The thermal spray powder according to claim 1 or 2, wherein the average particle size is 12 μm or more and 21 μm or less.
9. 3. The thermal spray powder according to claim 1, wherein the primary particles of the double oxide are composed of secondary particles bonded to each other.
10. The thermal spray powder according to claim 9 , wherein the secondary particles are granulated and sintered particles.
11. 3. The thermal spray powder according to claim 1, which is constituted by a fused and pulverized powder of the double oxide.
Citation Information
Patent Citations
Thermal-spraying powder and thermal-sprayed film
JP2002080954A
Spherical particle for thermal spraying and thermal spraying member
JP2002363724A
BSAS powder
JP2011514872A
Spinel powder and manufacturing process therefor, and process for producing thermal sprayed film and gas sensor element
JP2012232871A
Rare earth oxide thermal spray material, method for manufacturing the same, rare earth oxide thermal spray coating and method for forming the same
JP2022098519A