Electrolytic capacitor
The innovative electrolytic capacitor design addresses short circuits and sealing issues by using a lead terminal with a thinning flat plate and secure crimping, enhancing vibration resistance and maintaining sealing performance while reducing height.
Patent Information
- Application Number
- JP2023065624
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-13
- Publication Date
- 2024-10-25
AI Technical Summary
Conventional electrolytic capacitors face issues with short circuits due to misalignment or burrs on electrode foils, reduced vibration resistance, increased height, and compromised sealing performance, leading to potential electrolyte leakage and reduced lifespan.
The electrolytic capacitor design features a lead terminal with a cylindrical columnar part and a thin, gradually thinning flat plate part, where the flat plate thickness decreases with distance from the columnar part, and the inclination angle of the end surface is larger than the flat plate's thickness direction, along with multiple crimping points for secure connection, eliminating the need for a reinforcing portion.
This design enhances vibration resistance, prevents short circuits, maintains sealing integrity, and allows for a lower profile, thereby improving the capacitor's durability and lifespan.
Smart Images

Figure 2024151869000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an electrolytic capacitor having lead terminals connected to a pair of electrode foils. [Background technology]
[0002] A conventional electrolytic capacitor is disclosed in Patent Document 1. In this electrolytic capacitor, a capacitor element is housed in a cylindrical main case with a bottom, and the opening of the main case is sealed with a rubber seal. The capacitor element is formed by winding a pair of electrode foils consisting of a cathode foil and an anode foil facing each other with a separator interposed between them, and a lead terminal is connected to each of the electrode foils. The lead terminals pass through through holes provided in the seal and are drawn out of the main case, and are soldered to a circuit board.
[0003] The lead terminal has a cylindrical columnar portion press-fitted into the through hole of the sealing body, and a thin plate-like plate portion to which the electrode foil is connected by crimping. The columnar portion has an inclined end face inclined with respect to the axial direction, and a reinforcing portion having a smaller inclination angle with respect to the axial direction than the inclined end face is provided across the inclined end face and the plate portion. The reinforcing portion can prevent cracks from occurring between the plate portion and the columnar portion due to the plate portion swinging like a pendulum due to vibrations, etc., when the vehicle is mounted. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2021-158184 A (pages 4 to 10, Figure 5) Summary of the Invention [Problem to be solved by the invention]
[0005] However, in the conventional electrolytic capacitor, since the reinforcing portion is provided, one end of the electrode foil on the sealing body side faces the inclined reinforcing portion with the separator sandwiched therebetween, and therefore, if the electrode foil is misaligned during winding or if burrs are generated on the edge of the electrode foil, the electrode foil may come into contact with the reinforcing portion, which may cause a short circuit.
[0006] On the other hand, if the flat plate portion is formed long and the electrode foil is placed farther away from the reinforcing portion, the flat plate portion will be subject to greater vibration when it is mounted on a vehicle, resulting in problems such as insufficient vibration resistance and the occurrence of cracks. In addition, the height of the electrolytic capacitor will increase, making it impossible to meet the market demand for a lower height.
[0007] In addition, if the vibration of the flat plate portion is suppressed by fitting the reinforcing portion into the through hole of the sealing body, the columnar portion penetrating the sealing body becomes shorter, which reduces the sealing performance of the electrolytic capacitor, which may lead to contamination of the circuit board due to leakage of electrolyte and cause a short circuit, and also leads to a problem of shortening the life of the electrolytic capacitor due to an increased evaporation rate of the electrolyte.
[0008] An object of the present invention is to provide an electrolytic capacitor capable of preventing damage to the lead terminals due to vibration without deteriorating the sealing performance in response to a reduction in height. [Means for solving the problem]
[0009] In order to achieve the above object, the present invention provides an electrolytic capacitor comprising: a cylindrical main case having one axial end closed by a closing surface and the other end having an opening; a capacitor element housed in the main case and formed by winding a pair of electrode foils made of a cathode foil and an anode foil facing each other via a separator and connected to respective lead terminals; and a sealing body having a pair of through holes and sealing the opening, The extraction terminal has a cylindrical columnar portion that is inserted into the through hole and a thin flat portion that is joined to the electrode foil by a crimping portion, and is characterized in that the thickness of the flat portion becomes thinner as it moves away from the columnar portion.
[0010] The present invention is also characterized in that, in the electrolytic capacitor of the above configuration, the radial length of the capacitor element decreases from the opening side toward the blocked surface side, and the rate of decrease in the radial length of the capacitor element in the axial direction is greater than the rate of decrease in the thickness of the flat plate portion.
[0011] Furthermore, the present invention is characterized in that, in the electrolytic capacitor having the above-mentioned configuration, the lead-out terminal is joined to the electrode foil by a plurality of the crimping portions arranged in the axial direction, and the length of the crimping portions in the axial direction and the length of the crimping portions along the winding direction of the electrode foil are made smaller with increasing distance from the columnar portion.
[0012] In the electrolytic capacitor of the present invention having the above-mentioned configuration, the width of the flat portion along the winding direction of the electrode foil is made smaller with increasing distance from the columnar portion.
[0013] Furthermore, in the electrolytic capacitor of the present invention having the above-described configuration, the columnar portion has an inclined end face inclined with respect to the axial direction, and the inclination angle of the inclined end face with respect to the axial direction is greater than the inclination angle of a plane intersecting the thickness direction of the flat portion. Effect of the Invention
[0014] According to the present invention, the thickness of the thin plate portion of the lead terminal is made thinner as it moves away from the columnar portion. Therefore, the shape change at the base of the flat portion is gradual, and the concentration of stress due to vibration near the base of the flat portion is alleviated. In addition, the plate thickness of the flat portion is increased near the base, so that the strength of the flat portion is improved. In addition, the radial gap between the capacitor element, which is wound with electrode foil and is joined to the flat portion, and the main body case is narrowed on the opening side, so that the oscillation of the capacitor element is suppressed. In addition, the center of gravity of the capacitor element is brought closer to the columnar portion fixed to the sealing body, so that the oscillation of the capacitor element is further suppressed. As a result, the vibration resistance of the electrolytic capacitor is improved, and damage to the lead terminal due to vibration when mounted on a vehicle can be prevented.
[0015] Furthermore, as a result of the above, there is no need to provide a reinforcing portion as in the conventional example, which makes it possible to prevent short circuits and deterioration of the sealing performance of the sealing body due to contact between the reinforcing portion and the electrode foil, and also makes it possible to accommodate a reduction in the height of the electrolytic capacitor. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a vertical cross-sectional view showing an electrolytic capacitor according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a perspective view showing a capacitor element of an electrolytic capacitor according to a first embodiment of the present invention; [Diagram 3] FIG. 1 is a front view showing a lead-out terminal of an electrolytic capacitor according to a first embodiment of the present invention; [Figure 4] FIG. 1 is a side view showing a lead-out terminal of an electrolytic capacitor according to a first embodiment of the present invention; [Diagram 5] FIG. 1 is a side view showing a crimped portion of an electrode foil of an electrolytic capacitor according to a first embodiment of the present invention. [Figure 6] FIG. 1 is a schematic top view showing a capacitor element of an electrolytic capacitor according to a first embodiment of the present invention. [Figure 7] FIG. 1 is a schematic front cross-sectional view showing a capacitor element of an electrolytic capacitor according to a first embodiment of the present invention. [Figure 8] FIG. 11 is a side view showing a lead-out terminal of the electrolytic capacitor according to the second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] First Embodiment DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will now be described with reference to the accompanying drawings, in which: FIG 1 is a longitudinal sectional view of an electrolytic capacitor 1 according to a first embodiment;
[0018] The main case 2 is made of a metal such as aluminum or resin and is formed into a cylindrical shape with a circular cross section and a bottom, with one axial end closed by a blocking surface 2a and the other end having an opening 2b. From the standpoint of workability and sealing performance, it is preferable to form the main case 2 from aluminum. The capacitor element 10 is housed inside the main case 2, and the opening 2b is sealed by a sealing body 5. The main case 2 can be provided with an explosion-proof valve or a thin-walled portion for explosion prevention in case the internal pressure increases due to gas generation.
[0019] 2 shows a perspective view of capacitor element 10. Capacitor element 10 has cathode foil 11, anode foil 12, and separator 13 formed in a long strip shape. Capacitor element 10 is formed by winding a pair of electrode foils consisting of cathode foil 11 and anode foil 12 facing each other with separator 13 interposed therebetween into a substantially cylindrical shape. An end of cathode foil 11 or separator 13 is fixed with adhesive tape 14.
[0020] The width of separator 13 in the short side direction (axial direction) is formed to be larger than the width of cathode foil 11 and anode foil 12 in the short side direction. As a result, separator 13 protrudes toward closed surface 2a and opening 2b with respect to cathode foil 11 and anode foil 12, thereby preventing short-circuiting between cathode foil 11 and anode foil 12.
[0021] Cathode foil 11 is made of a metal such as aluminum, and its surface is roughened by etching. An inorganic coating layer of carbon, titanium, or the like may be formed on the surface of cathode foil 11. In addition, a natural oxide film or a chemical oxide film formed by applying a voltage in a chemical solution may be formed on the surface of cathode foil 11.
[0022] The anode foil 12 is made of a valve metal such as aluminum, tantalum, niobium, or titanium, and its surface is roughened by etching. A chemical oxide film that becomes a dielectric layer is formed on the anode foil 12 by applying a voltage in a chemical solution.
[0023] Separator 13 is made of paper or nonwoven fabric made of natural cellulose fiber, or chemical fiber such as rayon, polyethylene terephthalate, or polyamide. Separator 13 is porous and can hold an electrolyte in the internal voids. Separator 13 is preferably thicker than the size of protrusions such as burrs on cathode foil 11 and anode foil 12, and is formed to a thickness of, for example, 20 μm to 60 μm.
[0024] An electrolyte is provided between the cathode foil 11 and the anode foil 12. The electrolyte may be one or both of an electrolytic solution and a solid electrolyte. The electrolyte covers at least a portion of the cathode foil 11 and the anode foil 12, and a portion of the electrolyte is also held by the separator 13.
[0025] The electrolyte is a solution in which a solute is dissolved in a high boiling point polar solvent such as γ-butyrolactone, sulfolane, ethylene glycol, or diethylene glycol. The solute may be an inorganic acid (phosphoric acid, boric acid, etc.), an organic acid (phthalic acid, fumaric acid, maleic acid, salicylic acid, adipic acid, etc.), or a composite compound of an inorganic acid and an organic acid (borodiglycolic acid, borodisalicylic acid, etc.). An ionic liquid that is liquid at room temperature may also be used as the electrolyte. The electrolyte covers at least a portion of the cathode foil 11 and the anode foil 12, and is present in a state of being impregnated in the separator 13.
[0026] A conductive polymer can be used for the solid electrolyte. Polypyrrole, polythiophene, polyaniline, and derivatives thereof can be used for the conductive polymer, and p-toluenesulfonic acid, polystyrenesulfonic acid, etc. can be used as a dopant. The conductive polymer can be formed by a polymerization reaction within the capacitor element 10. The conductive polymer may be retained within the capacitor element 10 by dispersing a conductive polymer that has been polymerized in advance in water to form a dispersion, which is then impregnated into the capacitor element 10 and dried.
[0027] The polythiophene derivative using polyethylenedioxythiophene and the dopant using polystyrenesulfonic acid are preferably used as dispersions with excellent conductivity and stability. In addition, when a sulfonic acid group is provided in the molecule of the polythiophene derivative, it can be used as a self-doped conductive polymer that is soluble in a solvent such as water.
[0028] Also, a hybrid electrolytic capacitor 1 can be formed by forming a solid electrolyte in the capacitor element 10 and further impregnating it with an electrolytic solution. Alternatively, an electrolytic capacitor 1 can be formed by forming a solid electrolyte in the capacitor element 10 and further impregnating it with a room temperature solid electrolyte such as a functional liquid such as ethylene glycol or polyethylene glycol, or a polymeric polyethylene glycol in which a solute containing an acid has been dissolved.
[0029] A lead-out terminal 7 is connected to the cathode foil 11, and a lead-out terminal 8 is connected to the anode foil 12. The lead-out terminals 7, 8 are formed to be the same shape. Figs. 3 and 4 show a front view and a side view of the lead-out terminals 7, 8. The lead-out terminals 7, 8 each have a first member 21 having a columnar portion 23 and a flat portion 25, and a second member 22 connected to the first member 21. The first member 21 is made of aluminum, for example, and the second member 22 is made of CP wire with a copper layer provided on the outer surface of an iron wire, for example.
[0030] The second member 22 is inserted into the hole 21a provided in the columnar portion 23 of the first member 21 and welded. This mechanically and electrically fixes the first member 21 and the second member 22. The open end of the second member 22 forms a connection terminal to be soldered to a circuit board. A resin seat plate that supports the main case 2 may be provided, and the second member 22 may be bent on the bottom surface of the seat plate to form the connection terminal.
[0031] The columnar portion 23 of the first member 21 is formed in a cylindrical shape, and has an inclined end face 24 at one end on the flat plate portion 25 side. The columnar portion 23 is formed by utilizing the shape of the round bar (e.g., cylindrical aluminum material) that forms the first member 21. As described later, the columnar portion 23 is press-fitted into the through hole 5a (see FIG. 1 ) of the sealing body 5. This causes the second member 22 to be drawn out of the main body case 2.
[0032] The flat plate portion 25 is formed in a long, thin plate shape, and the width W of the flat plate portion 25 is constant from the columnar portion 23 to the tip. The flat plate portion 25 is formed by pressing one end of the round bar that forms the first member 21 and cutting off unnecessary portions. The inclined end face 24 of the columnar portion 23 is also formed at the same time during the press process. The thickness of the flat plate portion 25 is made continuously thinner as it moves away from the columnar portion 23 by a press mold. The thickness of the flat plate portion 25 may be made continuously thinner by cutting or the like after the press process.
[0033] Since the thickness of the flat portion 25 becomes thinner with increasing distance from the columnar portion 23, the shape of the base of the flat portion 25 changes more gently, and the concentration of stress due to vibration near the base of the flat portion 25 is alleviated. In addition, since the thickness of the flat portion 25 increases near the base, the strength of the flat portion 25 is improved.
[0034] At this time, the inclination angle θ2 of the inclined end surface 24 with respect to the axial direction is formed to be larger than the inclination angle θ1 of the surface intersecting the plate thickness direction of the flat plate portion 25. This makes it possible to move the electrode foil away from the inclined end surface 24 in the axial direction while keeping the flat plate portion 25 close to the columnar portion 23. Therefore, even if the electrode foil is misaligned during winding or burrs are generated on the edge of the electrode foil, it is possible to prevent a short circuit caused by contact between the electrode foil and the inclined end surface 24.
[0035] Cathode foil 11 or anode foil 12 is mechanically and electrically connected and fixed to flat portion 25 by crimping portion 15. Fig. 5 shows a side view of crimping portion 15. Flat portion 25 is provided with a plurality of crimping portions 15 aligned in the axial direction. Crimping portion 15 is formed by overlapping cathode foil 11 or anode foil 12 and flat portion 25 of lead terminals 7, 8, and performing pin crimping or punch hole crimping.
[0036] In the pin crimping process, a piercing needle with a pyramidal tip is inserted to form a burr in the electrode foil and the flat plate portion 25, and the burr is then cold-pressed onto the electrode foil by pressing. In the punch hole crimping process, a hole is made in the electrode foil, and then the flat plate portion 25 is overlapped and a piercing needle is inserted to form a burr in the flat plate portion 25, and the burr is then cold-pressed onto the electrode foil by pressing.
[0037] 5, the pressed burrs form the crimping portion 15 into a petal shape, and the electrode foil and the flat portion 25 are mechanically connected. The chemical oxide film or natural oxide film of the electrode foil and the flat portion 25 is destroyed by the punching process with the needle and the pressing process, and the electrode foil and the flat portion 25 are electrically connected.
[0038] The size of the petal-shaped crimping portion 15 is proportional to the thickness of the flat portion 25 when a piercing needle of the same size is used. That is, the length of the crimping portion 15 in the axial direction and the length of the crimping portion 15 along the winding direction of the electrode foil are proportional to the thickness of the flat portion 25. For this reason, the size of the crimping portion 15 is larger on the columnar portion 23 side and becomes smaller toward the tip side.
[0039] The larger the crimped portion 15, the smaller the contact resistance of the connection between the electrode foil and the lead terminals 7, 8, and the higher the mechanical strength and the more stable the joint. Since the crimped portion 15 is formed large at a position close to the columnar portion 23 where strong stress is applied during vibration, it is possible to reduce the likelihood of breakage due to peeling between the electrode foil and the lead terminals 7, 8 caused by vibration. Therefore, it is possible to prevent the lead terminals 7, 8 from coming off the cathode foil 11 or the anode foil 12 even when subjected to strong vibration.
[0040] In addition, because the fixing strength of the crimping portion 15 located near the columnar portion 23 is strong and stable, the number of crimping portions 15 provided on the flat portion 25 can be minimized. This makes it possible to reduce the generation of burrs and foil powder during the crimping process, which are likely to adversely affect the characteristics of the electrolytic capacitor 1. This makes it possible to obtain an electrolytic capacitor 1 with stable characteristics. Furthermore, since work hardening and metal fatigue caused by the crimping process can be suppressed, vibration resistance is improved and damage to the lead-out terminals 7, 8 can be prevented.
[0041] Moreover, by reducing the number of crimping portions 15, the length of flat plate portion 25 can also be shortened. This increases the area of cathode foil 11 and anode foil 12 that face each other via separator 13, allowing the capacitance to be increased. Furthermore, the distance between the tip of flat plate portion 25 and the foil end of cathode foil 11 or anode foil 12 can be increased. This reduces interference between flat plate portion 25 and the electrode foil end, preventing the cathode foil 11 or anode foil 12 from cracking or breaking.
[0042] 1, sealing body 5 is formed into a disk shape by molding an insulating elastic body such as butyl rubber or ethylene propylene rubber, and has a pair of through holes 5a into which lead terminals 7, 8 of capacitor element 10 are inserted by press-fitting.
[0043] With the sealing body 5 placed in the opening 2b of the main case 2, the main case 2 is subjected to a drawing process that presses the outer circumferential surface. As a result, a drawn portion 2c that protrudes toward the inner surface of the main case 2 is formed. The drawn portion 2c compresses the outer circumferential surface of the sealing body 5 in the inward direction, so that it adheres closely to the inner circumferential surface of the main case 2. Furthermore, the compression of the sealing body 5 causes the inner surface of the through hole 5a to adhere closely to the lead-out terminals 7, 8. As a result, the opening 2b of the main case 2 is sealed by the sealing body 5.
[0044] The end of the main case 2 on the opening 2b side is curved and folded to form a folded portion 2d towards the sealing body 5. The folded portion 2d and the drawn portion 2c prevent the sealing body 5 from slipping out of the main case 2.
[0045] 6 and 7 show a schematic top view and a schematic front cross-sectional view of capacitor element 10. In these figures, cathode foil 11 is shown by a thick solid line, anode foil 12 is shown by a medium solid line, and separator 13 is shown by a dashed line. As described above, flat portions 25 of lead terminals 7 and 8 are connected to cathode foil 11 and anode foil 12, respectively, by crimping portion 15 (see FIG. 5). Cathode foil 11 and anode foil 12, which face each other with separator 13 interposed therebetween, are wound into a substantially cylindrical shape using a winding core. Capacitor element 10 around which the electrode foils are wound is removed from the winding core by hooking it onto a blanking plate.
[0046] The thickness of flat portion 25 of lead-out terminals 7, 8 is continuously reduced from columnar portion 23 toward the tip. Therefore, the radial length of capacitor element 10 decreases from the lead-out side (opening 2b side) of lead-out terminals 7, 8 toward blocking surface 2a (see FIG. 1).
[0047] This narrows the radial gap between capacitor element 10 and main case 2 near sealing body 5, reducing the range of movement of capacitor element 10 within main case 2. As a result, the oscillation of capacitor element 10 is suppressed when electrolytic capacitor 1 vibrates, improving the vibration resistance of electrolytic capacitor 1 and preventing damage to lead-out terminals 7, 8.
[0048] In addition, by applying a pulling force while fixing the position of the winding core and winding the cathode foil 11 and the anode foil 12, the winding tension on the tip side of the flat portion is increased. This allows the rate of decrease in the radial length of the capacitor element 10 to be greater than the rate of decrease in the plate thickness of the flat portion 25. This allows the radial gap on the opening 2b side between the capacitor element 10 and the main case 2 to be narrowed further, and the vibration resistance of the electrolytic capacitor 1 to be improved further.
[0049] In addition, a large space is secured between the peripheral wall surface of the main case 2 and the capacitor element 10 on the closed surface 2a side. Therefore, when the main case 2 with the opening 2b facing upward is filled with an electrolyte and the capacitor element 10 is immersed therein, a large amount of electrolyte can be filled. This allows a large amount of electrolyte to be impregnated into the capacitor element 10, and the life of the electrolytic capacitor 1 can be extended.
[0050] In addition, since the gap between the cathode foil 11 and the anode foil 12 is narrower on the opposite side than on the lead-out side of the lead-out terminals 7, 8, the electrolyte is more likely to move to the lead-out side of the lead-out terminals 7, 8 when it is impregnated. Therefore, when the opening 2b is placed downward in the aging process, the electrolyte that has accumulated in the space on the blocking surface 2a side flows to the sealing body 5 side so as to be familiar with the entire capacitor element 10, and is heated so that the electrolyte fills the etching pits as well. This makes it possible to repair defects in the chemical oxide film of the anode foil 12 evenly from the center of the capacitor element 10 to the entire surface.
[0051] In addition, since the plate thickness of flat portion 25 is large on the side of columnar portion 23, the center of gravity of capacitor element 10 is brought closer to columnar portion 23 which is fixed in close contact with sealing body 5. This reduces the vibration of capacitor element 10 and improves the vibration resistance of electrolytic capacitor 1. In particular, when a room temperature solid electrolyte is used as the electrolyte, the effect of improving vibration resistance is significant.
[0052] According to this embodiment, the thickness of the thin plate-like flat plate portion 25 of the lead terminals 7, 8 is made thinner as it moves away from the columnar portion 23. Therefore, the shape change at the base of the flat plate portion 25 becomes gentle, and the concentration of stress due to vibration near the base of the flat plate portion 25 is alleviated. In addition, the plate thickness of the flat plate portion 25 is increased near the base, so that the strength of the flat plate portion 25 is improved. Furthermore, the radial gap between the capacitor element 10, which is wound with an electrode foil joined to the flat plate portion 25, and the main body case 2 is narrowed on the opening 2b side, so that the oscillation of the capacitor element 10 is suppressed. In addition, the center of gravity of the capacitor element 10 is brought closer to the columnar portion 23, so that the oscillation of the capacitor element 10 is further suppressed. As a result, the vibration resistance of the electrolytic capacitor 1 is improved, and damage to the lead terminals 7, 8 due to vibration when mounted on a vehicle can be prevented.
[0053] In addition, because of the improved vibration resistance, there is no need to provide a reinforcing portion as in the conventional example, which prevents short circuits caused by contact between the reinforcing portion and the electrode foil and a decrease in the sealing performance of the sealing body 5, and also enables the electrolytic capacitor 1 to be made thinner.
[0054] Furthermore, by making the rate of decrease in the radial length of capacitor element 10 in the axial direction larger than the rate of decrease in the thickness of flat plate portion 25, the radial gap on the opening 2b side between capacitor element 10 and main body case 2 can be made narrower, thereby further improving the vibration resistance of electrolytic capacitor 1.
[0055] Furthermore, lead-out terminals 7, 8 are joined to the electrode foil by a plurality of crimping portions 15 arranged in the axial direction, and the length of crimping portions 15 in the axial direction and the length of crimping portions 15 along the winding direction of the electrode foil are made smaller with increasing distance from columnar portion 23. This allows crimping portions 15 closer to columnar portion 23 to be formed larger, preventing lead-out terminals 7, 8 from coming off cathode foil 11 or anode foil 12 even under strong vibration. Furthermore, the number of crimping portions 15 can be reduced, increasing the capacitance of electrolytic capacitor 1 and preventing cracks and breakage of the electrode foil.
[0056] In addition, since the inclination angle θ2 of inclined end face 24 with respect to the axial direction is greater than the inclination angle θ1 of the surface intersecting the plate thickness direction of flat plate portion 25, the electrode foil can be separated in the axial direction from inclined end face 24. Therefore, even if the electrode foil is misaligned during winding or burrs occur on the edge of the electrode foil, a short circuit due to contact between the electrode foil and inclined end face 24 can be prevented.
[0057] <Second embodiment> Next, Fig. 8 is a side view showing lead-out terminals 7, 8 of an electrolytic capacitor 1 according to a second embodiment. The same parts as those in Fig. 4 above are denoted by the same reference numerals. This embodiment differs from the first embodiment in the shape of the flat plate portions 25 of the lead-out terminals 7, 8. The other parts of the electrolytic capacitor 1 are the same as those in the first embodiment.
[0058] The width W of flat portion 25 along the winding direction of the electrode foil is not constant, but is formed to become smaller as it moves away from columnar portion 23 toward the tip. This makes it possible to narrow the radial length of capacitor element 10 (see FIG. 1) from the lead-out side (opening 2b side) of lead-out terminals 7, 8 toward closed surface 2a. This further improves the vibration resistance of electrolytic capacitor 1, making it possible to prevent damage to lead-out terminals 7, 8. [Industrial Applicability]
[0059] The present invention can be used in automobiles, electronic devices, etc. in which electrolytic capacitors are mounted in circuits. [Explanation of symbols]
[0060] 1. Electrolytic capacitor 2 Main unit case 2a Occlusion surface 2b opening 2c Drawing section 2d bend part 5 Sealing body 5a through hole 7, 8 Output terminal 10 Capacitor element 11 Cathode foil 12 Anode foil 13 Separator 14 Adhesive Tape 15 Crimping part 21 First member 21a Hole 22 Second member 23 Columnar part 24 Slanted end face 25 Flat plate part W width θ1, θ2 Tilt angle
Claims
1. an electrolytic capacitor comprising: a cylindrical main case having one axial end closed by a closing surface and an opening at the other axial end; a capacitor element housed in the main case by winding a pair of electrode foils made of a cathode foil and an anode foil facing each other via a separator and connected to lead terminals, and a sealing body having a pair of through holes and sealing the opening, an electrolytic capacitor characterized in that the lead-out terminal has a cylindrical columnar portion that is inserted into the through hole and a thin plate-like portion that is joined to the electrode foil by a crimping portion, and the thickness of the flat portion is formed to become thinner as it moves away from the columnar portion.
2. 2. The electrolytic capacitor according to claim 1, characterized in that the radial length of the capacitor element decreases from the opening side toward the closed surface side, and the rate of decrease in the radial length of the capacitor element in the axial direction is greater than the rate of decrease in the thickness of the flat portion.
3. 3. The electrolytic capacitor according to claim 1, wherein the lead-out terminal is joined to the electrode foil by a plurality of the crimping portions arranged in an axial direction, and the length of the crimping portions in the axial direction and the length of the crimping portions along the winding direction of the electrode foil are made smaller with increasing distance from the columnar portion.
4. 3. The electrolytic capacitor according to claim 1, wherein a width of the flat portion along a winding direction of the electrode foil decreases with increasing distance from the columnar portion.
5. 3. The electrolytic capacitor according to claim 1, wherein the columnar portion has an inclined end face inclined with respect to the axial direction, and the inclination angle of the inclined end face with respect to the axial direction is greater than the inclination angle of a plane intersecting the thickness direction of the flat portion.