Display device

By employing a microcrystalline semiconductor structure with an amorphous buffer layer in a thin film transistor, the liquid crystal display device achieves enhanced aperture ratio and reduced leakage current, improving display brightness and efficiency.

JP2024153898AInactive Publication Date: 2024-10-29SEMICON ENERGY LAB CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024129135
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2007-07-27
Filing Date
2024-08-05
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing liquid crystal display devices face challenges in achieving high aperture ratio due to issues with current drive capability, leakage current, and increased capacitance when using amorphous or polycrystalline semiconductors, which affect display quality and efficiency.

Method used

The use of a microcrystalline semiconductor structure in a stacked configuration with an amorphous semiconductor as a buffer layer to form a thin film transistor, optimizing channel width and length ratios to enhance current drive capability and reduce leakage current, thereby improving aperture ratio.

Benefits of technology

This configuration results in a liquid crystal display device with improved aperture ratio, reduced off-state current, and minimized transistor variations, leading to higher brightness and efficiency with reduced backlight requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153898000001_ABST
    Figure 2024153898000001_ABST
Patent Text Reader

Abstract

To provide a liquid crystal display device having an improved aperture ratio, and to provide an electronic device.SOLUTION: A liquid crystal display device comprises: a substrate having an insulating surface; a transistor formed on the substrate; and a pixel electrode electrically connected to the transistor. The transistor comprises: a gate electrode; a gate insulating layer on the gate electrode; a semiconductor layer having a microcrystalline structure on the gate insulating layer; and a buffer layer on the semiconductor layer having the microcrystalline structure. Channel width W of the transistor and channel length L of the transistor satisfy the relation of 0.1≤W / L≤1.7.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a liquid crystal display device and an electronic device. [Background technology]

[0002] In recent years, a semiconductor thin film has been formed on a substrate having an insulating surface, and the semiconductor thin film is used to fabricate a semiconductor device. The technology for fabricating semiconductor devices using the aforementioned semiconductor thin films is being widely researched. Among other things, it is used as a switching element in image display devices. This is often the case.

[0003] Amorphous semiconductors and polycrystalline semiconductors are used as switching elements of the image display device. When using amorphous semiconductors, the number of steps can be minimized by eliminating the steps required for crystallization, etc. This allows the switching elements to be manufactured at low cost. In addition, when using polycrystalline semiconductors, it is possible to create high-performance switching elements. It has the advantage of being able to manufacture

[0004] Examples of image display devices using switching elements include liquid crystal display devices and electroluminescent devices. Liquid crystal display devices have a structure in which a voltage is applied between a pixel electrode and a counter electrode. By applying a potential difference, the orientation of the liquid crystal molecules is changed to produce a display. In order to hold the potential difference required for display for a certain period of time, a storage capacitor is generally provided in the pixel. Electroluminescent displays provide electrical charges to a light-emitting material between electrodes, The display is achieved by inducing radiative recombination of carriers.

[0005] In LCDs, the pixel aperture ratio is one of the important parameters that determine the display quality. The improved aperture ratio improves the brightness and enables high-contrast display. Furthermore, the improved aperture ratio makes it possible to reduce the output of the backlight. As a method for improving the aperture ratio, for example, a method for forming a storage capacitor using a light-shielding film is available. (See, for example, Patent Document 1).

[0006] By the way, in addition to amorphous and polycrystalline semiconductors, there are also microcrystalline semiconductors. For example, microcrystalline silicon, like amorphous silicon, is a material that has been known for a long time. Field-effect transistors using microcrystalline silicon date back to the 1980s. However, to date, microcrystalline systems have not been reported. The silicon-based transistors are different from the amorphous silicon transistors and the polycrystalline silicon transistors. The practical application of this technology was delayed due to being overwhelmed by transistors using (See, for example, Non-Patent Document 1). [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 10-170961 [Patent Document 2] U.S. Patent No. 5,591,987 [Non-patent literature]

[0008] [Non-Patent Document 1] Toshiaki Arai et al., SID 07 DIGEST, 2007, p.1370-1373 Summary of the Invention [Problem to be solved by the invention]

[0009] In a liquid crystal display device, a transistor in a pixel portion (hereinafter also referred to as a "pixel transistor") High current drive capability and low leakage current characteristics are required for the This is because the storage capacitance needs to be charged and discharged quickly. The current characteristic is required in order to prevent the charge stored in the storage capacitor from escaping.

[0010] When an amorphous semiconductor is used as a pixel transistor, it can be manufactured inexpensively as described above. On the other hand, amorphous semiconductors have low carrier mobility, so The current driving capability of the transistors is also low. It is possible to improve the current driving capability by increasing This causes a problem that the size becomes large and the aperture ratio of the pixel decreases.

[0011] Increasing the size of transistors has other drawbacks. For example, The gate wiring (also called the gate electrode) is formed between the source region or drain region of the The problem is that the capacitance (hereafter referred to as coupling capacitance) increases. In the circuit diagram, the coupling capacitance 2301 and the storage capacitance 2302 are connected to the gate wiring 2303. and the liquid crystal element 2304. When the potential of the line 2303 fluctuates, the potential of the storage capacitor 2302 also fluctuates. In order to keep the quality constant, it is necessary that the potential fluctuation of the storage capacitor 2302 is sufficiently small. Therefore, the ratio of the storage capacitance 2302 to the binding capacitance 2301 must be increased. If the amount 2302 is increased, the aperture ratio will decrease. When the capacitance becomes large, the coupling capacitance 2305 also becomes large at the same time, so the Mari etc. are also a problem.

[0012] As described above, when an amorphous semiconductor is used as a pixel transistor, the desired performance can be obtained. It is very difficult to increase the aperture ratio while maintaining the same level of contrast.

[0013] On the other hand, when a polycrystalline semiconductor is used as a pixel transistor, the mobility is low as described above. However, the problem caused by the exposure equipment used in the manufacture of liquid crystal displays is solved. The resolution of the device is only a few micrometers, and it cannot be said that the characteristics of polycrystalline semiconductors are fully utilized. On the contrary, the leakage current is increased due to the channel width being larger than the optimal size. If the leakage current is large, the storage capacitance becomes large. In order to reduce leakage current, the aperture ratio must be reduced. In some cases, a method such as connecting several transistors in series is used. The resolution is lower in LCDs than in LSIs. This is because the substrates used in the devices (typically glass substrates) have a bending of several tens of micrometers. For this reason, when exposing a large area at once, it is necessary to increase the focal depth of the exposure device. do.

[0014] Furthermore, when using polycrystalline semiconductors, the process becomes complicated and productivity decreases. There is a problem.

[0015] In view of the above problems, the present invention provides a liquid crystal display device and an electronic device with an improved aperture ratio. The objective of the project is to provide [Means for solving the problem]

[0016] In the present invention, a semiconductor having a microcrystalline structure (hereinafter also referred to as a "microcrystalline semiconductor") and an amorphous semiconductor are A transistor is manufactured using a stacked structure of conductors. More specifically, A bottom-gate type in which a microcrystalline semiconductor is used and an amorphous semiconductor is stacked on the microcrystalline semiconductor This allows the fabrication of thin film transistors with high current driving capability and low leakage current characteristics. In other words, it is possible to provide a transistor having both the above-mentioned transistors. By using the same as the etching element, it is possible to provide a liquid crystal display device with an improved aperture ratio. can.

[0017] A liquid crystal display device according to the present invention includes a substrate having an insulating surface and a transistor formed on the substrate. a pixel electrode electrically connected to the transistor, a gate electrode, a gate insulating layer on the gate electrode, and a semiconductor having a microcrystalline structure on the gate insulating layer. a buffer layer on the semiconductor layer having a microcrystalline structure, The channel width W and the channel length L of the transistor must satisfy the relationship 0.1≦W / L≦1.7. It is characterized by the following:

[0018] Another aspect of the liquid crystal display device of the present invention is a liquid crystal display device comprising a substrate having an insulating surface and a transistor formed on the substrate. a pixel electrode electrically connected to the transistor, A gate electrode, a gate insulating layer on the gate electrode, and a semiconductor having a microcrystalline structure on the gate insulating layer. A semiconductor layer having a microcrystalline structure and a buffer layer on the semiconductor layer, The channel width W is 1 μm or more and 10 μm or less (preferably 1 μm or more and 5 μm or less). It is characterized by the following:

[0019] Another aspect of the liquid crystal display device of the present invention is a liquid crystal display device comprising a substrate having an insulating surface and a and a pixel electrode electrically connected to the transistor. The gate electrode has a gate insulating layer on the gate electrode, and the gate insulating layer has a microcrystalline structure. and a buffer layer on the semiconductor layer having a microcrystalline structure. The channel width W of the transistor is the minimum processing dimension d of the transistor, and the current The channel width W of transistors with the same driving capability a For d≦W≦W a Relationship In the above, the channel width (W a ) other parameters The transistor is equivalent to the transistor of the present invention.

[0020] Another aspect of the liquid crystal display device of the present invention is a liquid crystal display device comprising a substrate having an insulating surface and a and a pixel electrode electrically connected to the transistor. The gate electrode has a gate insulating layer on the gate electrode, and the gate insulating layer has a microcrystalline structure. and a buffer layer on the semiconductor layer having a microcrystalline structure. The relationship between the channel width W and the channel length L of the transistor is 0.1≦W / L≦1.7. A semiconductor having a microcrystalline structure that satisfies the above and serves as at least a channel formation region of a transistor. The present invention is characterized in that a buffer layer remains on the layer.

[0021] Another aspect of the liquid crystal display device of the present invention is a liquid crystal display device comprising a substrate having an insulating surface and a and a pixel electrode electrically connected to the transistor. The gate electrode has a gate insulating layer on the gate electrode, and the gate insulating layer has a microcrystalline structure. and a buffer layer on the semiconductor layer having a microcrystalline structure. The channel width W of the capacitor is 1 μm or more and 10 μm or less (preferably 1 μm or more and 5 μm or less). on a semiconductor layer having a microcrystalline structure which is to become at least a channel formation region of a transistor, is characterized in that the buffer layer remains.

[0022] Another aspect of the liquid crystal display device of the present invention is a liquid crystal display device comprising a substrate having an insulating surface and a and a pixel electrode electrically connected to the transistor. The gate electrode has a gate insulating layer on the gate electrode, and the gate insulating layer has a microcrystalline structure. and a buffer layer on the semiconductor layer having a microcrystalline structure. The channel width W of the transistor is the minimum processing dimension d of the transistor, and the current The channel width W of transistors with the same driving capability a For d≦W≦W a Relationship A semiconductor having a microcrystalline structure that satisfies the above and serves as at least a channel formation region of a transistor. The present invention is characterized in that a buffer layer remains on the layer. Channel Width (W a ) other parameters are the same as those of the transistor of the present invention.

[0023] In the above structure, the buffer layer is formed using an amorphous semiconductor. The present invention also features a semiconductor having a microcrystalline structure that serves as a channel formation region of a transistor. The buffer layer is characterized in that a groove is formed on the body layer.

[0024] Moreover, various electronic devices can be provided using the above liquid crystal display device.

[0025] In this specification, unless otherwise specified, a microcrystalline semiconductor has a microcrystalline structure. In other words, a microcrystalline semiconductor is a semiconductor that includes components other than a microcrystalline structure. For example, depending on the film formation conditions, the film may contain an amorphous structure.

[0026] In this specification, "connection" includes "electrical connection".

[0027] In addition, the display device in this specification includes display devices such as image display devices, lighting devices, etc. Also, FPC (Flexible Printed Circuit) circuit) and TAB (Tape Automated Bonding) tape , TCP (Tape Carrier Package) and other connectors are attached. modules with printed wiring boards on the ends of TAB tape or TCP; The display element is equipped with an IC (integrated circuit) using the COG (Chip On Glass) method. All such modules are included in the display device. Effect of the Invention

[0028] According to the present invention, it is possible to provide a liquid crystal display device having an improved aperture ratio. By using the above, high quality electronic devices can be provided. [Brief description of the drawings]

[0029] [Figure 1]1A to 1C are diagrams illustrating a manufacturing process of a display device according to the present invention. [Diagram 2] 1A to 1C are diagrams illustrating a manufacturing process of a display device according to the present invention. [Diagram 3] 1A to 1C are diagrams illustrating a manufacturing process of a display device according to the present invention. [Figure 4] FIG. 1 is a plan view of a display device according to the present invention. [Diagram 5] FIG. 1 is a plan view of a display device according to the present invention. [Figure 6] FIG. 1 is a diagram showing an example of a display device of the present invention. [Figure 7] 1A to 1C are diagrams illustrating a process for producing a display device according to the present invention. [Figure 8] FIG. 1 is a cross-sectional view of a display device according to the present invention. [Figure 9] FIG. 1 is a plan view of a display device according to the present invention. [Figure 10] FIG. 1 is a plan view of a display device according to the present invention. [Figure 11] FIG. 1 is a circuit diagram of a display device according to the present invention. [Figure 12] FIG. 1 is a cross-sectional view of a display device according to the present invention. [Figure 13] FIG. 1 is a plan view of a display device according to the present invention. [Figure 14] FIG. 1 is a plan view of a display device according to the present invention. [Figure 15] FIG. 1 is a circuit diagram of a display device according to the present invention. [Figure 16] FIG. 1 is a cross-sectional view of a display device according to the present invention. [Figure 17] FIG. 1 is a plan view of a display device according to the present invention. [Figure 18] FIG. 1 is a cross-sectional view of a display device according to the present invention. [Figure 19] FIG. 1 is a plan view of a display device according to the present invention. [Figure 20] FIG. 1 is a cross-sectional view of a display device according to the present invention. [Figure 21] FIG. 1 is a plan view of a display device according to the present invention. [Figure 22] 1A and 1B are diagrams illustrating electronic devices using a display device of the present invention. [Diagram 23] FIG. 1 is a circuit diagram of a conventional display device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] The present invention will be described below with reference to the drawings. The present invention is not limited to the above embodiment, and various modifications and variations in form and detail are possible without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made thereto. The present invention is not limited to the description of the embodiments. In the configuration, the same reference numerals will be used in common between different drawings to indicate the same parts.

[0031] (Embodiment 1) In this embodiment, a manufacturing process of a liquid crystal display device of the present invention, particularly, a manufacturing process of a thin film transistor The process will be described with reference to FIGS. 1 to 6. FIGS. 1 to 3 are cross-sectional views of the manufacturing process. 4 and 5 are plan views of a thin film transistor and a connection region of a pixel electrode in one pixel. 6 is a cross-sectional view and a plan view of the completed liquid crystal display device.

[0032] Although various configurations of the plan view are possible, the following is a representative configuration in this embodiment. In the case of a structure in which the channel formation region, source region, and drain region are arranged linearly (see Figure 4) ), and when either the channel formation region or the source or drain region has a U-shaped structure ( As shown in FIG. 5, the present invention is not limited to these. By adopting this configuration, it is possible to ensure a constant channel width without reducing the aperture ratio. In addition, in the present invention, the channel width can be made sufficiently small, By using a linear structure as shown in FIG. 4, a liquid crystal display device with a very high aperture ratio can be fabricated. 1 to 3 correspond to the line segment AB in FIGS.

[0033] In thin-film transistors using microcrystalline semiconductors, the current drive is n-channel rather than p-channel. For this reason, n-channel transistors are suitable for the pixel area. The present invention is not limited to this. In this embodiment, an n-channel thin film transistor is used. He explains.

[0034] First, a gate electrode 102 is formed on a substrate 100 (FIGS. 1(A) and 4(A)). See FIG. 5(A). The substrate 100 is made of barium borosilicate glass, aluminoborosilicate glass, etc. Uses non-alkali glass substrates such as aluminosilicate glass, ceramic substrates, etc. If heat resistance allows, a plastic substrate or the like may be used. A substrate having an insulating layer on the surface of a metal substrate such as an alloy may be used. There are no particular limitations, and the sizes are 320mm x 400mm, 370mm x 470mm, and 550mm. m×650mm, 600mm×720mm, 680mm×880mm, 730mm×92 0mm, 1000mm×1200mm, 1100mm×1250mm, 1150mm×1 300mm, 1500mm×1800mm, 1900mm×2200mm, 2160mm x 2460mm, 2400mm x 2800mm, 2850mm x 3050mm etc. It can be used appropriately.

[0035] The gate electrode 102 may be made of titanium, molybdenum, chromium, tantalum, tungsten, or aluminum. The gate electrode 102 is formed of a metal material such as sapphire or an alloy material thereof. A conductive layer formed by a tarpaulin deposition method or a vacuum deposition method is etched using a mask. In addition, conductive nanopastes such as gold, silver, and copper can be applied by inkjet printing. Alternatively, the above-mentioned metal materials may be discharged by a casting method and then sintered. A nitride layer may be provided between the substrate 100 and the gate electrode 102. The adhesion of the electrode 102 can be improved. In addition, the diffusion of the metal material into the semiconductor layer can be suppressed. It can also be prevented.

[0036] It is preferable that the gate electrode 102 is processed so that its end portion has a tapered shape. This prevents breakage when forming a semiconductor layer, wiring, etc. on the gate electrode 102. In addition, other wirings can be formed in the same process as the formation of the gate electrode 102. In this embodiment, the gate electrode 102 has a single-layer structure. However, it may have a laminated structure of two or more layers. For example, a laminated structure of aluminum and molybdenum. Alternatively, a laminated structure of copper and molybdenum may be used. Alternatively, titanium nitride or tantalum nitride may be used. By covering the resistance material with a barrier metal, metal that is a source of contamination in the semiconductor layer is prevented. The elements can be prevented from diffusing.

[0037] Next, a gate insulating layer 104a and a gate insulating layer 104b are formed on the gate electrode 102. The gate insulating layer 104a and the gate insulating layer 104b are formed by CVD. Silicon oxide film, silicon nitride film, silicon oxynitride film formed by a deposition method, a sputtering method, or the like In this embodiment, the gate insulating layer 104a and the gate insulating layer 104b are formed of a silicon nitride oxide film or the like. Silicon nitride or silicon nitride oxide is used as the gate insulating layer 104b, and silicon oxide or silicon nitride oxide is used as the gate insulating layer 104c. The gate insulating layer has a two-layer structure, but this is not the case in the present invention. It may be a single layer or a laminated structure of three or more layers.

[0038] Here, silicon oxynitride is a material having a higher oxygen content (number of atoms) than nitrogen in its composition. For example, oxygen is 50 atomic % or more and 70 atomic % or less, and nitrogen is 0.5 atomic % or less. 15 atomic % or less, silicon is 25 atomic % to 35 atomic %, hydrogen is 0.1 atomic % to 10 The content of silicon oxide in the composition is in the range of 1 atomic % or less. This refers to a material that contains more nitrogen (atomic number) than oxygen. For example, oxygen is 5 atomic % or more and 30 atomic % or less. atomic % or less, nitrogen is 20 atomic % to 55 atomic % or less, silicon is 25 atomic % to 35 atomic % or less The hydrogen content is in the range of 10 atomic % to 25 atomic %. Rutherford Backscattering (RBS) Hydrogen Forward Scattering Spectrometry (HFS) The measurements were taken using forward scattering. The total content of the constituent elements does not exceed 100 atomic %.

[0039] Note that hydrogen plasma treatment may be performed when the gate insulating layer 104b is formed. By subjecting the edge layer to hydrogen plasma treatment, crystal growth of the microcrystalline semiconductor layer can be promoted. This is because the dangling bonds in the gate insulating layer are eliminated by hydrogen plasma treatment. In this way, when the gate insulating layer 104b is formed, By performing the plasma treatment, the characteristics of the obtained microcrystalline semiconductor layer can be improved.

[0040] Then, a microcrystalline semiconductor layer 106, a buffer layer 108, and a A semiconductor layer 110 to which an impurity element that imparts a conductivity type is added is formed in sequence (see FIG. 1(C)). see).

[0041] The microcrystalline semiconductor layer 106 has an intermediate structure between an amorphous structure and a crystalline structure (including a single crystal structure and a polycrystalline structure). It is a layer containing a semiconductor, and the crystal grain size is approximately 2 nm or more and 100 nm or less. Microcrystalline silicon, a typical example of a crystalline semiconductor, has a peak in its Raman spectrum that corresponds to that of a single crystal. Recon shows 521cm -1 In other words, the single crystal silicon is shifted to the lower wave number side. Showing 521cm -1 and 480 cm, which indicates amorphous silicon. -1 Between the microcrystalline silica In addition, water is added to terminate the dangling bonds. It may contain 1 atomic % or more of elements or halogens. By incorporating rare gas elements such as argon, krypton, and neon, lattice distortion is promoted. As a result, a good microcrystalline semiconductor with improved stability can be obtained.

[0042] The microcrystalline semiconductor layer 106 is, for example, a high-frequency wave having a frequency of several tens of MHz to several hundreds of MHz. Plasma CVD, formed using microwave plasma CVD with a frequency of 1 GHz or more The source gases are SiH4, Si2H6, SiH2Cl2, and SiHCl3. Silicon compounds such as SiCl4 and SiF4 diluted with hydrogen are used. The silicon compounds and hydrogen mentioned above can be combined with helium, argon, krypton, or neon. One or more of rare gas elements such as those mentioned above may be added to the microcrystalline semiconductor layer 106. The thickness is set to 2 nm or more and 50 nm or less, and preferably 10 nm or more and 30 nm or less.

[0043] Note that the microcrystalline semiconductor layer 106 has a weak n-type conductivity when an impurity element is not intentionally added. Therefore, even if the threshold voltage is controlled by adding an impurity element that gives the p-type, When boron is used as an impurity element to impart p-type, for example, the concentration of boron is 1×10 14 atoms / cm 3 More than 6×10 16 atoms / cm 3 So that it becomes as follows: It may be added.

[0044] The buffer layer 108 is a layer containing an amorphous semiconductor, such as SiH4, Si2H6, or SiH2 Using gaseous silicon compounds such as Cl2, SiHCl3, SiCl4, and SiF4, plasma The silicon compound gas can be formed by the CVD method. It is diluted with one or more rare gas elements selected from the group consisting of argon, krypton, and neon. Furthermore, hydrogen may be added to form an amorphous semiconductor layer containing hydrogen, or nitrogen may be added to form an amorphous semiconductor layer containing nitrogen. An amorphous semiconductor layer containing nitrogen may be formed by adding fluorine, chloride, or ammonia. Gases containing fluorine, bromine, or iodine (F2, Cl2, Br2, I2, HF, HCl, HB r, HI, etc.) to form an amorphous semiconductor layer containing fluorine, chlorine, bromine, or iodine. You can do that.

[0045] The buffer layer 108 is formed by a sputtering method using an amorphous semiconductor as a target. The sputtering atmosphere may be a hydrogen atmosphere or a rare gas atmosphere. Ammonia, nitrogen, or N2O atmosphere is preferred, but is not limited to this. By adding fluorine, an amorphous semiconductor layer containing nitrogen can be formed. , gases containing chlorine, bromine, or iodine (F2, Cl2, Br2, I2, HF, HCl, By adding an alkaline ion (HBr, HI, etc.), amorphous materials containing fluorine, chlorine, bromine, or iodine are produced. A semiconductor layer can also be formed.

[0046] After forming an amorphous semiconductor layer as a buffer layer 108 on the surface of the microcrystalline semiconductor layer 106, The surface of the amorphous semiconductor layer is treated with hydrogen plasma, nitrogen plasma, halogen plasma, or the like. The surface of the amorphous semiconductor layer may be hydrogenated, nitrided, or halogenated by treatment.

[0047] The thickness of the buffer layer 108 is 100 nm or more and 500 nm or less, preferably 150 nm or less. m or more and 400 nm or less, more preferably 200 nm or more and 300 nm or less. The reason for forming the insulating layer 108 thick is to prevent the formation of a source region and a drain region in the subsequent process (e.g., the process of forming the source region and the drain region). This is because a part of the buffer layer 108 is left in the etching process. This reduces the leakage current (also called "off current") of the thin film transistor. In addition, the buffer layer is formed on the microcrystalline semiconductor layer, and a part of the buffer layer is formed in the channel. The microcrystalline semiconductor layer 106 which functions as a hole formation region is prevented from being oxidized, and good characteristics are obtained. Note that a barrier layer in a region overlapping with the microcrystalline semiconductor layer and the source region or the drain region can be formed. The buffer layer has the above-mentioned thickness (100 nm or more and 500 nm or less, preferably 150 nm or less). and preferably 200 nm to 300 nm), and Contribute to improvement.

[0048] In order to fully obtain the effect of reducing the off-current, the buffer layer 108 should contain n-type impurities such as phosphorus. A region in which the impurity element that gives the n-type and the impurity element that gives the p-type, such as boron, do not exist at the same time. When these impurity elements are present at the same time, recombination centers are formed. This is because a leakage current occurs due to the formation of a gate electrode. When forming a MOS transistor, an impurity element that imparts n-type conductivity is added to the buffer layer 108. The microcrystalline semiconductor layer 106 is provided with a semiconductor layer 110 having a thickness of 100 nm to control the threshold voltage. In order to prevent this, impurity elements that give p-type conductivity may be added. Care must be taken to avoid creating areas that do not exist.

[0049] When forming an n-channel thin film transistor, an impurity element that imparts one conductivity type is As an impurity element to be added to the semiconductor layer 110 to which phosphorus is added, for example, phosphorus can be used. In addition, when a p-channel thin film transistor is formed, For example, boron can be used. The conductor layer 110 has a thickness of about 2 nm to 50 nm (preferably 10 nm to 30 nm). The method for manufacturing the semiconductor device is to use a gas containing an impurity element. A plasma CVD method using gases (e.g., PH3 or B2H6) can be used. .

[0050] Next, a mask 112 is formed on the semiconductor layer 110 to which an impurity element that imparts one conductivity type is added. The gate insulating layer 104a, the gate insulating layer 104b, and the micro-insulating layer 104c are formed (see FIG. 1D). The crystalline semiconductor layer 106 and the buffer layer 108 may be formed in succession, or a gate insulating layer may be formed. layer 104a, a gate insulating layer 104b, a microcrystalline semiconductor layer 106, a buffer layer 108, and The semiconductor layer 110 to which an impurity element that imparts one conductivity type is added may be formed continuously. At least the gate insulating layer 104a, the gate insulating layer 104b, the microcrystalline semiconductor layer 106, and By successively forming the buffer layer 108 and the substrate 102 without exposing them to the air, each interface is kept clean. The mask 112 can be formed by photolithography or inkjet printing. It can be formed by using a jet method.

[0051] Next, the microcrystalline semiconductor layer 106, the buffer layer 108, and the one-conductivity type The semiconductor layer 110 to which the impurity element that imparts the conductivity is added is etched to form a microcrystalline semiconductor layer 1 14, a buffer layer 116, and a semiconductor layer 118 doped with an impurity element that imparts one conductivity type (See FIG. 1(E)). Note that FIG. 1(B) is a diagram showing the line segment of FIG. 4(B) or FIG. 5(B). It corresponds to the cross section of AB.

[0052] Here, the microcrystalline semiconductor layer 114, the buffer layer 116, and the impurity layer imparting one conductivity type The end of the semiconductor layer 118 to which the element is added is etched into a tapered shape. The semiconductor layer 118 to which an impurity element that imparts an electric type is added and the microcrystalline semiconductor layer 114 are in contact with each other. In the present invention, the semiconductor layer 1 to which an impurity element that imparts one conductivity type is added is When the buffer layer 116 contacts the microcrystalline semiconductor layer 114, the buffer layer 116 loses its effect. Therefore, the above measures are very effective. The taper angle of the shape is set to 30° or more and 90° or less, and preferably 45° or more and 80° or less.

[0053] Next, a semiconductor layer 118 to which an impurity element that imparts one conductivity type is added and a gate insulating layer 1 A conductive layer 120a, a conductive layer 120b, and a conductive layer 120c are sequentially laminated on the substrate 04b. (See FIG. 2(A)). Note that in this embodiment mode, a conductive layer having a three-layer structure is formed. The present invention is not limited to this. It may be a single layer or two-layer structure, or a laminated structure of four or more layers. is also good.

[0054] Materials that can be used for the conductive layers 120a, 120b, and 120c include , Tantalum (Ta), Tungsten (W), Titanium (Ti), Molybdenum (Mo), Al Aluminum (Al), gold (Au), silver (Ag), copper (Cu), chromium (Cr), neodymium ( Nd), or alloy materials or compound materials mainly composed of the above elements Semiconductors such as polycrystalline silicon doped with impurity elements such as phosphorus The material may be AgPdCu alloy. Examples of the method include a vacuum deposition method and a plasma CVD method. In this embodiment, the conductive layer 120 1A shows a case where the conductive layer 120c is made of molybdenum and the conductive layer 120b is made of aluminum. For example, the conductive layers 120a and 120c may be made of titanium, and the conductive layers Aluminum may be used for 120b.

[0055] The conductive layers 120a, 120b, and 120c are made of a conductive nanopaste. It is also possible to form the insulating film by using the screen printing method or the ink jet method described above.

[0056] Thereafter, a mask 122 is formed on the conductive layer 120a, the conductive layer 120b, and the conductive layer 120c. The mask 122 can be formed similarly to the mask 112.

[0057] Next, the conductive layer 120a, the conductive layer 120b, and the conductive layer 120c are etched using the mask 122. The conductive layer 124a and the conductive layer 124b function as a source electrode and a drain electrode, respectively. b. the conductive layer 124c and the conductive layer 126a serving as a source electrode or a drain electrode; The conductive layers 126b and 126c are formed (see FIG. 2B). The conductive layers 124a, 124b, 124c, and 126 are removed by hot etching. a. Conductive layer 126b and conductive layer 126c are formed. Wet etching is not performed using dry etching. The etching is isotropic compared to the etching, and the edge 128a of the mask 122 and the conductive layer 12 4a, the ends 128b of the conductive layers 124b and 124c do not coincide, and the mask 122 and the ends 130a of the conductive layers 126a, 126b, and 126c. No match.

[0058] Next, a mask 122 is used to form a semiconductor layer 11 doped with an impurity element that imparts one conductivity type. 8 and the buffer layer 116 are etched to form source or drain regions 132, Then, a source region or drain region 134 and a buffer layer 136 are formed (see FIG. 2(C)). Then, the mask 122 is removed. 6 is a partly etched film, and covers the surface of the microcrystalline semiconductor layer 114 .

[0059] The buffer layer 136 formed by etching has a groove, the end of which is a saw. The groove 132 forms a surface that is almost continuous with the end of the source region or drain region 132. is formed in a region roughly coinciding with the opening of the mask 122.

[0060] As described above, by providing the buffer layer 136, the lead of the thin film transistor This reduces the carrier current (also called the "off current") during the off-state. This is because the main part of the MOSFET path is formed in the buffer layer 136. In the first embodiment, only the microcrystalline semiconductor layer functions as a channel, and the carriers pass through the buffer layer 136. By providing a groove in the buffer layer 136, the thickness of the buffer layer 136 is not increased. This is because the leakage current is reduced by forming the trench. In addition, the semiconductor layer 1 to which an impurity element that imparts one conductivity type is added is By completely removing 18, leakage current caused by impurity elements contained in the residue is reduced. In addition, hydrogen, fluorine, etc., present in the grooves of the buffer layer can It is possible to prevent impurity elements such as a buffer. The layer 136 exists over the microcrystalline semiconductor layer 114 and functions as a channel formation region. This makes it possible to prevent the microcrystalline semiconductor layer 114 from being oxidized and obtain favorable characteristics.

[0061] The buffer layer 136 also has the effect of preventing parasitic channels. In addition, the thickness of the semiconductor layer 118 is increased when the semiconductor layer 118 is etched. In the case where the buffer layer 136 is not provided, the etching The microcrystalline semiconductor layer 114 is oxidized by the radical reaction, and the mobility is reduced and the subthreshold This results in an increase in the saturation threshold (S value) and other problems. When using hydrogenated amorphous semiconductor materials, especially a-Si:H (hydrogenated amorphous silicon), It is preferable to use silicon (SiC) because the surface is terminated with hydrogen, which makes it difficult to react with oxygen. This is because it is possible to suppress the degradation.

[0062] In addition, the end 138 of the source or drain region 132, the conductive layer 124a, and the conductive layer 1 24b, the ends 128b of the conductive layer 124c are not coincident, and the source or drain regions 134 and the ends 130b of the conductive layers 126a, 126b, and 126c. They do not match. Ends 138 and 140 are located inside end 128b and end 130b. This results in the following:

[0063] FIG. 2C corresponds to a cross-sectional view taken along line AB in FIG. 4C or FIG. 5C. 4(C) and 5(C), the ends 128b and 130b are the ends 138 and It can be seen that the source electrode or the drain electrode is located outside the semiconductor device 140. It also functions as a source wiring or a drain wiring.

[0064] Through the above steps, the microcrystalline semiconductor layer 114 is formed as a channel formation region. A thin film transistor 142 having a buffer layer 136 is formed on the conductor layer 114. can.

[0065] Next, an insulating layer 144 is formed so as to cover the thin film transistor 142 (see FIG. 3(A)). The insulating layer 144 is formed in the same manner as the gate insulating layer 104a and the gate insulating layer 104b. The insulating layer 144 is resistant to the intrusion of impurities such as organic matter, metals, and water suspended in the air. Since the purpose of the film is to prevent infiltration, it is preferable to form a dense film.

[0066] Next, a contact hole is formed in the insulating layer 144, and a conductive layer is A pixel electrode 146 is formed in contact with the pixel electrode 124c (see FIG. 3B). This corresponds to a cross-sectional view taken along line AB in FIG. 4(D) or FIG. 5(D).

[0067] The pixel electrode 146 is made of indium oxide containing tungsten oxide, Indium zinc oxide containing titanium oxide, indium oxide containing titanium oxide Indium tin oxide, indium tin oxide (hereinafter referred to as "ITO"), indium zinc oxide In addition, a conductive material having light transmitting properties, such as indium tin oxide doped with silicon oxide, is used. This can be done.

[0068] In addition, the pixel electrode 146 is made of a conductive material including a conductive polymer. A conductive composition having a sheet resistance of 1000 in a thin film can also be used. It is preferable that the thickness of the pixel electrode layer is 0 Ω / sq. or less. In the case of forming a film, the transmittance of light at a wavelength of 550 nm is preferably 70% or more. In addition, it is preferable that the resistivity of the conductive polymer contained therein is 0.1 Ω cm or less. .

[0069] As the conductive polymer, a so-called π-electron conjugated conductive polymer can be used. For example, polyaniline and its derivatives, polypyrrole and its derivatives, polythiophene Examples of the polymerizable compound include polyaniline and its derivatives, and copolymers thereof.

[0070] In this embodiment, the ends 128b and 138, and the ends 130b and 14 Although transistors with a configuration in which the 0s do not match have been fabricated, a configuration in which the 0s match may also be used. FIG. 3(C) shows a cross section of a thin-film transistor with these edges aligned. In order to make the end shapes match, it is necessary to use highly anisotropic dry etching. The conductive layer 124a and the conductive layer 124b function as a source electrode and a drain electrode, respectively. a conductive layer 124c serving as a source electrode or a drain electrode, and a conductive layer 126b, a conductive layer 126c is used as a mask to add an impurity element that imparts one conductivity type. The end portions can also be made flush by etching the semiconductor layer.

[0071] After that, alignment films and other materials are applied, and then the opposing substrate is attached, liquid crystal is sealed in, and various driving circuits are The liquid crystal display device is completed by carrying out mounting and the like (see FIG. 6). FIG. 6(A) shows the liquid crystal display device. 6(B) is a cross-sectional view taken along line CD in FIG. For simplicity, in FIG. 6, the laminated structure of the transistors and the like are partially omitted.

[0072] In the liquid crystal display device shown in FIG. 6, a pixel portion 602 on a substrate 600 and a scanning line driver circuit 604 A sealant 606 is provided so as to surround the pixel portion 602. A counter substrate 608 is provided on the driving circuit 604. The line driver circuit 604 and the liquid crystal 610 are disposed between the substrate 600, the sealant 606, and the counter substrate 608. The region surrounded by the sealant 606 on the substrate 600 is In a different region, a signal line driver circuit formed of a separately prepared single crystal semiconductor or polycrystalline semiconductor is In FIG. 6B, a transistor included in the signal line driver circuit 612 is mounted. 614 is shown as an example.

[0073] A pixel portion 602 and a scanning line driver circuit 604 on a substrate 600 have a plurality of thin film transistors. In FIG. 6B, a thin film transistor 616 included in a pixel portion 602 is shown as an example. The thin film transistor 616 corresponds to a thin film transistor using a microcrystalline semiconductor. It can be produced by the process of:

[0074] In order to control the distance (cell gap) between the pixel electrode 618 and the counter electrode 620, A spherical spacer 622 is provided. Instead of the spherical spacer, an insulating layer is selectively provided. Alternatively, a spacer obtained by etching may be used.

[0075] Various signals provided to the scanning line driver circuit 604 and the signal line driver circuit 612 are routed through wiring. 624 and is supplied from the FPC 628 via the wiring 626. A connection terminal 630 is formed on the wiring 626, and the FPC 628 and the connection terminal 630 are The electrical connection is made via anisotropic conductive material 632. The connection terminal 630 is formed from the same conductive layer as the pixel electrode 618. The wiring 624 and the lead wiring 626 are formed from the same conductive layer as the wiring 634. This is not limited to this.

[0076] Although not shown in FIG. 6, the liquid crystal display device of the present invention further includes an alignment film and a polarizing plate. The transparent substrate 1 may have a color filter (hereinafter, also referred to as a colored film), a light-shielding film, or the like.

[0077] In addition, FIG. 6 shows an example in which a signal line driver circuit 612 is formed separately and mounted on a substrate 600. However, the present invention is not limited to this. Depending on the characteristics of the transistor, it may be possible to integrate a signal line driver circuit. Of course, a structure in which a scanning line driver circuit is separately formed may be used. A part of the signal line driver circuit and a part of the scanning line driver circuit may be separately formed and mounted.

[0078] As described above, according to the present invention, a microcrystalline semiconductor is used as a channel formation region of a pixel transistor. The transistor and the liquid crystal display device are configured as follows: This is merely an example, and the present invention is not limited to this.

[0079] The transistor used in the liquid crystal display device of the present invention has a channel width (W) of at least The minimum processing dimension (d) is the minimum processing dimension of the This refers to the minimum of the width of the contact part, the channel length, the wiring width, etc. The transistors used in the liquid crystal display device are formed so as to satisfy the relationship d≦W. The channel width of a transistor using a microcrystalline semiconductor is limited by the resolution of an exposure device. By not receiving it.

[0080] The upper limit of the channel width (W) is the same as that of the current driving capability formed using an amorphous semiconductor. The channel width (W a ) can be referred to. The width of the channel (W) a ) and W≦W a This is defined as amorphous. The mobility of carriers in microcrystalline semiconductors is higher than that in semiconductors, and the electric field When the current driving ability is the same, the channel width is smaller than that of the amorphous semiconductor. This is because the channel of a transistor using an amorphous semiconductor, which is the subject of comparison, Width (W a ) The parameters other than the above are set equal to those of the transistor of the present invention. Attention should be paid to the following.

[0081] In addition, in the transistor used in the liquid crystal display device of the present invention, The channel length (L) is 0.1≦W / L≦2.0 (or 0.1≦W / L<2.0), preferably The relationship of 0.1≦W / L≦1.5, more preferably 0.1≦W / L≦1.0 is satisfied. In the case where a transistor using an amorphous semiconductor is used for a pixel of a liquid crystal display device, Width (W a ) and channel length (L a ) is 20≦W a ≦100, 3≦L a ≦10 (unit is In other words, 2.0≦W a / L a ≦33.3. In the case where a transistor using a microcrystalline semiconductor of the present invention is used for a pixel of a liquid crystal display device, For example, it is about 1≦W≦5, 3≦L≦10 (both units are μm). W / L is approximately 1.7 or less.

[0082] Note that when a transistor using a polycrystalline semiconductor is used for a pixel of a liquid crystal display device, The channel width (W p ) is significantly restricted. It is difficult to fabricate pixel transistors that fully utilize the performance of crystalline semiconductors. Considering the degree of thermal expansion, the channel length (L p ) and amorphous The channel length of the semiconductor transistor is the same (3≦L p Under the condition of ≦10) is W p ≦0.5 is an appropriate condition, and W p / L p ≦0.6, but in this way Met W p / L p The value of is not realistic and does not have much meaning.

[0083] In the transistor used in the liquid crystal display device of the present invention, the channel width (W) is To be more specific, it is 1 μm or more and 10 μm or less (more preferably 1 μm or less and 5 μm or less). The lower limit should be the resolution limit of the exposure device, and the lower limit should be the resolution limit of the exposure device + 5 It is also possible to specify the channel width with an upper limit of about 1 μm.

[0084] Generally, when a transistor using an amorphous semiconductor is used in a liquid crystal display device, the transistor The channel width is fabricated to be 20 μm or more and 100 μm or less. The reason for making is large is that the mobility of carriers in amorphous semiconductors is low. However, When a large channel width is adopted, the size of the transistor also becomes large, and the coupling capacitance In this respect, the amount of light emitted from the light source increases, which causes the problem of a decrease in the aperture ratio as described above. Recently, transistors have been developed using microcrystalline semiconductors, which have higher carrier mobility than amorphous semiconductors. In order to fabricate a GaN-GaN GaN CMOS ... In other words, the problem of the coupling capacitance can be solved and the aperture ratio can be improved.

[0085] In addition, a transistor using a polycrystalline semiconductor is different from a transistor using a microcrystalline semiconductor. In comparison, the carrier mobility is high, so the channel width can theoretically be made smaller than that of microcrystalline semiconductors. However, the exposure apparatus used in manufacturing the liquid crystal display device The resolution of the FT-IR is about several μm (e.g., 3 μm), and in reality, the channels are smaller than the resolution. Therefore, the polycrystalline semiconductor cannot be used as a pixel transistor for a liquid crystal display device. There is little merit in using polycrystalline semiconductors in semiconductors. For this reason, transistors using polycrystalline semiconductors have a large leakage current when off, so In order to hold the required charge for a given period of time, the storage capacitance must be increased. Therefore, even when a polycrystalline semiconductor is used, the aperture ratio is reduced. The aperture ratio also decreases when transistors are connected in series to reduce the current.

[0086] In this regard, in a transistor using a microcrystalline semiconductor, the relationship between the required current and the channel width is The present invention provides a liquid crystal display device having an optimum relationship for the liquid crystal display device and a maximum aperture ratio. It is possible to do this.

[0087] Note that a transistor using a microcrystalline semiconductor of the present invention has a microcrystalline semiconductor A buffer layer (amorphous semiconductor layer) is laminated on the semiconductor layer. This reduces the main leakage current. Since the lead is formed on the buffer layer (amorphous semiconductor layer) side, which has low electrical conductivity, the lead In other words, the storage capacitance can be further reduced. This leads to an improvement in the aperture ratio.

[0088] The buffer layer has several other effects. For example, it reduces the crystallinity of the channel formation region. One example is the effect of preventing the oxidation of the semiconductor. These effects include preventing the intrusion of elements. Since the variation in the characteristics of the transistors can be reduced, the variation in the characteristics of the transistors can be reduced when manufacturing a liquid crystal display device. This reduces the need to consider the effect of transistor variations. From the viewpoint of charge retention, this means that a design with a margin is no longer necessary. Even in situations where storage capacity was secured by having the device hold the battery, the extra capacity is no longer needed. This allows the storage capacitance to be reduced, making it possible to improve the aperture ratio. It is Noh.

[0089] In terms of reducing variations in transistors, the characteristics of microcrystalline semiconductors are Polycrystalline semiconductors are highly preferred. The size of each crystal grain varies. The channel formation region of a transistor made using this material is formed by a small number of crystal grains. However, the characteristics of each transistor tend to vary greatly. The grain size is uniform, and the channel formation region of the transistor is formed by many crystal grains. Therefore, the variation in the characteristics of the transistors can be reduced.

[0090] (Embodiment 2) In this embodiment mode, a transistor in which crystallinity is improved by irradiating a microcrystalline semiconductor layer with laser light is fabricated. A method for producing the star will be described with reference to FIG.

[0091] First, a gate electrode is formed on a substrate in the same manner as in the first embodiment. A gate insulating layer (not shown) is formed to cover the electrodes. A microcrystalline semiconductor layer is formed on the first insulating film (see FIG. 7A).

[0092] As described above, a microcrystalline semiconductor layer is formed on the gate insulating layer 700 by using a plasma CVD method or the like. During the formation, an amorphous layer is formed near the interface between the gate insulating layer 700 and the semiconductor layer 702. It is found that a region rich in ZnO (herein referred to as "interface region 704") is formed. In addition, a very thin microcrystalline semiconductor layer with a thickness of 10 nm or less may be formed by a plasma CVD method or the like. In such a case, it is difficult to obtain a semiconductor layer with uniform crystal grains. The treatment of irradiating the laser beam shown in FIG.

[0093] After the semiconductor layer 702 is formed, a laser having an energy density that does not melt the semiconductor layer 702 is used. Light is applied from above the semiconductor layer 702 (in the direction of the surface opposite to the interface region 704) (FIG. 7(B) ) The laser process (hereinafter referred to as "LP") is as follows: Solid-phase crystal growth is performed without melting the semiconductor layer 702 by radiant heating. That is, it is a crystal growth method that utilizes a critical region where the deposited semiconductor layer 702 does not become liquid. In that sense, it can also be called "critical growth."

[0094] The cross section after irradiation with laser light is shown in FIG. Excimer laser light below nm, or second harmonics of YAG laser or YVO4 laser It is preferable to use a wavelength of 532 nm to the fourth harmonic (wavelength 266 nm). Other laser beams can be used if they are of the same quality, but we have decided to use a laser beam that will improve productivity. For this purpose, it is preferable to use a high-output laser as described above. The light is focused into a line or spot shape using an optical system, and the energy is adjusted so that the semiconductor layer 702 does not melt. The laser light is irradiated at an energy density ( Since the laser beam is focused at a low energy density, the irradiation area of ​​the laser beam can be increased. In other words, even a large-area substrate can be processed in a short time.

[0095] The laser light can reach the interface region 704. 2 (the upper surface in the figure) as a seed, and the crystals are grown from the surface to the interface region 704. Solid-phase crystal growth proceeds toward the crystalline structure, and roughly columnar crystals grow. Crystal growth does not increase the grain size, but rather increases the crystal grain size through the thickness of the semiconductor layer. This can be said to be for the purpose of improving the crystallinity and adjusting the crystal grain size.

[0096] In this case, by making the shape of the irradiated beam a long rectangular shape (linear shape), for example, 730 mm It is possible to process a semiconductor layer on a glass substrate measuring 920 mm x 920 mm in size with a single scan. When using a pulsed laser such as a sigma laser, the linear laser beam is overlapped. The overlap rate should be between 0% and 90% (preferably between 0% and 67%). This reduces the processing time per substrate, improving productivity. The shape of the beam is not limited to a linear shape, and a planar shape can be used for the same processing. In addition, the LP process of this embodiment is not limited to the above-mentioned size of the glass substrate, Can be applied to a variety of sizes.

[0097] In the above-mentioned critical growth, polycrystalline semiconductors (so-called low-temperature The surface irregularities (protruding bodies called ridges) seen in polysilicon are not formed. Another feature is that the smoothness of the semiconductor surface remains excellent before and after LP treatment. A crystalline semiconductor obtained by irradiating a microcrystalline semiconductor layer after film formation with laser light as in the embodiment. The layer 706 has a different film quality from a microcrystalline semiconductor layer obtained by film formation. The growth mechanism and film quality of the microcrystalline semiconductor modified by CVD are different from those of the microcrystalline semiconductor modified by CVD.

[0098] In this specification, a crystalline semiconductor obtained by performing LP treatment on a microcrystalline semiconductor layer after film formation is Among these, the case where silicon is used is called LPSAS (Laser Process Semiconductor). LPSAS is a new type of silicon that uses a 32-bit LPSAS chip. It is a semiconductor with better properties than microcrystalline silicon, but microcrystalline silicon Therefore, in this specification, the term "microcrystalline silicon" is used. refers to both conventional microcrystalline silicon and LPSAS, and "conventional" is used only when a distinction is required. Similarly, the terms "microcrystalline silicon" and "LPSAS" are used interchangeably. In the case of "conductors," both conventional microcrystalline semiconductors and crystalline semiconductors that have undergone LP processing are included. This includes:

[0099] Next, a buffer layer 708 is formed on the crystalline semiconductor layer 706. When forming layer 708 as a-Si:H (hydrogenated amorphous silicon), hydrogen Since the crystalline semiconductor layer 706 is supplied with the crystalline semiconductor layer 706, the same effect as that in the case where the crystalline semiconductor layer 706 is crystallized is obtained. In other words, by forming an a-Si:H layer on the crystalline semiconductor layer 706, By forming the crystalline semiconductor layer 706, hydrogen is diffused into the crystalline semiconductor layer 706 to terminate the dangling bonds. The a-Si:H layer can be grown at temperatures of 300°C or higher using the plasma CVD method. It is preferable to form the film at a temperature of 400° C. or less.

[0100] The subsequent steps are the same as those in the first embodiment, and therefore will not be repeated here.

[0101] By using the semiconductor that has been subjected to LP processing such as LPSAS formed in this embodiment, This can further improve the electrical characteristics of the transistor.

[0102] This embodiment mode can be used in appropriate combination with Embodiment Mode 1.

[0103] (Embodiment 3) In this embodiment, the thin film transistor (hereinafter referred to as "TFT") shown in the first and second embodiments is The details of a liquid crystal display device having a liquid crystal display (also referred to as a liquid crystal display device) will be described with reference to FIGS. The thin film transistors used in the liquid crystal display devices of the first to ninth embodiments are the same as those shown in the first and second embodiments. It can be manufactured in the same manner as a thin film transistor.

[0104] First, about VA (Vertical Alignment) type LCD devices The VA method is a method for controlling the alignment of liquid crystal molecules in a liquid crystal display panel. In VA type LCDs, when no voltage is applied, the long axis of the liquid crystal molecules is aligned along the panel. In this embodiment, the pixels are arranged perpendicular to the surface. The pixel is divided into several regions (subpixels) and reacts in several different ways when a voltage is applied. This is called multi-domain or multi-domain. In the following explanation, we will focus on a multi-domain VA-type liquid crystal display device. I will explain it below.

[0105] 8 to 10 show an example of a multi-domain VA liquid crystal display device. FIG. 9 is a plan view of the substrate on which the pixel electrodes are formed, and FIG. 10 is a schematic diagram of the substrate. 8 is a plan view of the substrate side on which the counter electrode is formed. Note that FIG. 8 corresponds to the cross section of line EF in FIG. The following description makes reference to these drawings.

[0106] FIG. 8 shows a TFT 828, a pixel electrode 824 connected thereto, and a storage capacitor 830. The substrate 800 and a counter substrate 801 on which a counter electrode 840 and the like are formed are overlapped. , the liquid crystal is injected.

[0107] In the position where the spacer 842 is formed on the opposing substrate 801, a light-shielding film 832 and a first A first colored film 834, a second colored film 836, a third colored film 838, and a counter electrode 840 are formed. This structure allows the height of the protrusions 844 and the spacers 842 to be adjusted to control the alignment of the liquid crystal. An alignment film 848 is formed on the pixel electrode 824, and a counter electrode 8 An alignment film 846 is also formed on the substrate 40. A liquid crystal layer 850 is formed therebetween.

[0108] Although a columnar spacer is shown here as the spacer 842, a spherical bead spacer may also be used. Furthermore, the spacers 842 may be disposed between the pixels formed on the substrate 800. It may be formed on the electrode 824 .

[0109] On the substrate 800, a TFT 828, a pixel electrode 824 connected thereto, and a storage capacitor 8 The pixel electrode 824 is formed by a first insulating film 820 and a second insulating film 822. Each of the TFTs is connected to the wiring 818 via a contact hole 823 that penetrates the TFTs. The thin film transistor shown in the embodiment mode 1 or 2 can be appropriately used for the storage capacitor 8. The capacitance section 830 is formed by a capacitance wiring 804 formed in the same manner as the gate wiring 802 of the TFT 828 and a gate The gate insulating film 806 and the wiring 816, 818 are formed in the same manner as the capacitance electrode 817. .

[0110] The pixel electrode 824, the liquid crystal layer 850, and the counter electrode 840 are overlapped to form a liquid crystal element. It has been made.

[0111] 9 shows a structure on a substrate 800. The pixel electrode 824 is the same as that shown in the first embodiment. The pixel electrode 824 is provided with a slit 825. The bit 825 is for controlling the alignment of the liquid crystal.

[0112] The TFT 829 and the pixel electrode 826 and storage capacitor 831 connected thereto shown in FIG. The TFT 828 and the pixel electrode 824 and the storage capacitor 830 connected thereto are formed in the same manner. Both the TFT 828 and the TFT 829 are electrically connected to the wiring 816. The pixel of the liquid crystal display device is composed of a pixel electrode 824 and a pixel electrode 826. The pixel electrode 824 and the pixel electrode 826 are sub-pixels.

[0113] 10 shows the structure on the opposing substrate side. An opposing electrode 840 is formed on a light-shielding film 832. The counter electrode 840 is preferably formed using the same material as the pixel electrode 824. A protrusion 844 for controlling the alignment of the liquid crystal is formed on the counter electrode 840. A spacer 842 is formed in accordance with the position of 32.

[0114] The equivalent circuit of the pixel structure is shown in FIG. The line 802 is connected to the wiring 816. In this case, the capacitance wiring 804 and the capacitance wiring 805 are connected to each other. By making the positions different, the operation of the liquid crystal element 851 and the liquid crystal element 852 can be made different. That is, the potentials of the capacitance wiring 804 and the capacitance wiring 805 are individually controlled. The orientation of the liquid crystal can be precisely controlled to widen the viewing angle.

[0115] When a voltage is applied to a pixel electrode 824 having a slit 825, The slit 825 and the protrusion on the opposing substrate 801 side cause distortion of the electric field (diagonal electric field). By arranging the 844 and 846 so that they interdigitate with each other, a diagonal electric field is generated, which allows the liquid crystal to be aligned. This makes it possible to widen the viewing angle of the LCD panel. can be done.

[0116] Next, a VA type liquid crystal display device different from the above will be described with reference to FIGS. do.

[0117] 12 and 13 show an example of a VA type liquid crystal display device. FIG. 13 is a plan view of the substrate side on which the pixel electrodes are formed, and FIG. 14 is a plan view of the substrate side on which the counter electrode is formed. 12 corresponds to the cross section of line GH in FIG. The following description will be given with reference to both figures.

[0118] In the liquid crystal display device described here, a single pixel has a plurality of pixel electrodes. The structure has a TFT connected to the element electrode. Each TFT is driven by a different gate signal. That is, in a multi-domain pixel, each pixel is The signal applied to the element electrodes is independently controlled.

[0119] The structure on the substrate 1200 will be described. The pixel electrode 1224 is formed in the contact hole 1223. The pixel electrode 1226 is connected to the wiring 1218 of the TFT 1228. The pixel electrode is connected to the wiring 1219 of the TFT 1229 through a contact hole 1227. An alignment film 1248 is formed on the TFT 1224 and the pixel electrode 1226. The gate wiring 1202 of the TFT 28 and the gate wiring 1203 of the TFT 1229 have different gate signals. On the other hand, the wiring 12 which functions as a data line is separated so that a signal can be given to the 16 is commonly used in TFT1228 and TFT1229. For FT1229, the thin film transistor shown in embodiment 1 or 2 can be used as appropriate. In addition, a capacitance line 1290 is formed in the same layer as the gate line 1202 and the gate line 1203. It has been made.

[0120] The pixel electrodes 1224 and 1226 have different shapes and are separated by a slit. A pixel electrode 1226 is formed so as to surround the outside of the pixel electrode 1224 that spreads in a V shape. The timing of the voltages applied to the pixel electrodes 1224 and 1226 is TF The alignment of the liquid crystal is controlled by varying the T1228 and TFT1229.

[0121] The equivalent circuit of this pixel structure is shown in Figure 15. The TFT 1228 is connected to the gate wiring 1202. The TFT 1229 is connected to the gate wiring 1203. By applying different gate signals to the wiring 1203, the operation of the TFT 1228 and the TFT 1229 is controlled. The timing of the operation can be varied.

[0122] The counter substrate 1201 is provided with a light-shielding film 1232, a colored film 1236, a counter electrode 1240, and an alignment film. A flattening film 1246 is formed between the colored film 1236 and the counter electrode 1240. The counter electrode 1240 is formed between different pixels to prevent the alignment of the liquid crystal from being disturbed. Although it is a common electrode, a slit 1241 is formed. The liquid crystal layer 1250 and the counter electrode 1240 are overlapped to form a liquid crystal element. In addition, the pixel electrode 1226, the liquid crystal layer 1250, and the counter electrode 1240 are overlapped with each other, An element is formed.

[0123] The slits 1241 and the slits on the pixel electrode 1224 and pixel electrode 1226 sides are alternately arranged. By arranging them so that they interdigitate with each other and generating a diagonal electric field, the orientation of the liquid crystal can be changed in each location. (See FIG. 14.) This makes it possible to widen the viewing angle of the liquid crystal display panel. can.

[0124] Next, a liquid crystal display device of the in-plane switching type will be described. This method uses a horizontal electric field to drive the liquid crystal and express gradation. If this is done, the viewing angle can be expanded to approximately 180 degrees. A liquid crystal display device to be used will be described.

[0125] FIG. 16 shows a substrate on which a TFT 1628 and a second pixel electrode 1624 connected thereto are formed. The figure shows a state in which the liquid crystal display panel 1600 and the counter substrate 1601 are overlapped and liquid crystal is injected. The plate 1601 is provided with a light-shielding film 1632, a coloring film 1636, a flattening film 1637, an alignment film 1660, etc. The first pixel electrode 1607 and the second pixel electrode 1624 are formed on the substrate 160. Since the second pixel electrode is located on the 0 side, there is no need to provide an electrode on the opposing substrate 1601 side. An alignment film 1661 is formed on the substrate 1624. A liquid crystal layer 1650 is formed on the substrate 1610.

[0126] On the substrate 1600, a first pixel electrode 1607 and a second pixel electrode 1608 connected to the first pixel electrode 1607 are provided. A capacitance wiring 1604 and a TFT 1628 are formed. The same material as that of the pixel electrode shown in the embodiment mode 1 can be used. The electrode 1607 is formed in a shape that generally matches the shape of the pixel. A gate insulating film 1606 is formed on the electrode 1607 and the capacitance wiring 1604 .

[0127] The wiring 1616 and the wiring 1618 of the TFT 1628 are formed on the gate insulating film 1606 The wiring 1616 is a data line that transmits a video signal in the liquid crystal display panel. At the same time, it is connected to the source region 1610 and serves as either a source electrode or a drain electrode. The wiring 1618 serves as the other of the source electrode and the drain electrode, and is connected to the TFT 1628 and the second pixel. It also functions as a wiring for connecting to the element electrode 1624 .

[0128] An insulating film 1620 is formed on the wiring 1616 and the wiring 1618. On the insulating film 1620, a contact hole is formed in the insulating film 1620, and the wiring 1618 is connected to the contact hole. A second pixel electrode 1624 is formed to connect the second pixel electrode 1624. The same material as the pixel electrode shown in the first embodiment can be used.

[0129] In this manner, the TFT 1628 and the second pixel electrode 1 connected thereto are formed on the substrate 1600. A storage capacitor is formed between the first pixel electrode 1607 and the second pixel electrode 162. 4, a gate insulating film 1606 and an insulating film 1620 are formed.

[0130] FIG. 17 is a plan view showing the configuration of pixel electrodes, etc. The second pixel electrode 1624 is provided with a slit 1625. The pixel 1625 is for controlling the alignment of the liquid crystal. In this case, the electric field is the first pixel voltage. The first pixel electrode 1607 and the second pixel electrode 1624 are connected to each other. A gate insulating film 1606 and the like are formed between the pixel electrodes 1624. Since the layer is sufficiently thin compared to the substrate 1600, the electric field is substantially parallel to the substrate 1600 (horizontal direction). This electric field is used to rotate the liquid crystal molecules horizontally. In this case, the liquid crystal molecules rotate horizontally. Since the display is arranged in a direction, there is little problem with contrast reduction depending on the viewing angle, and the viewing angle is The corners are widened. In addition, the first pixel electrode 1607 and the second pixel electrode 1624 are both Since the electrode is light-transmitting, the aperture ratio can be improved.

[0131] Next, another example of a liquid crystal display device of the lateral electric field type will be described.

[0132] 18 and 19 show another structure of a liquid crystal display device of the in-plane switching mode. FIG. 18 corresponds to the KL cross section of FIG. 19. The explanation will be given with reference to these two figures.

[0133] FIG. 18 shows a substrate on which a TFT 1828 and a second pixel electrode 1824 connected thereto are formed. The figure shows a state in which the opposing substrate 1800 and the opposing substrate 1801 are overlapped and liquid crystal is injected. The plate 1801 is provided with a light-shielding film 1832, a coloring film 1836, a flattening film 1837, an alignment film 1860, etc. The first pixel electrode (common potential line 1809) and the second pixel electrode 18 Since 24 is on the substrate 1800 side, there is no need to provide an electrode on the opposing substrate 1801 side. An alignment film 1861 is formed on the second pixel electrode 1824. A liquid crystal layer 1850 is formed between the substrates 1801 .

[0134] On the substrate 1800, a common potential line 1809 and a TFT 1828 are formed. The common potential line 1809 can be formed simultaneously with the gate wiring 1802 of the TFT 1828. In this case, the first pixel electrode is synonymous with the common potential line 1809. In the pixel area, the electric potential line 1809 is formed in a shape that generally matches the shape of the pixel.

[0135] The wiring 1816 and the wiring 1818 of the TFT 1828 are formed on the gate insulating film 1806. The wiring 1816 is a data line that transmits a video signal in a liquid crystal display device. At the same time, the source region or drain region is connected, and the source electrode or drain electrode The wiring 1818 becomes the other of the source electrode and the drain electrode, and the second pixel electrode This is the wiring that connects to 1824.

[0136] An insulating film 1820 is formed on the wiring 1816 and the wiring 1818. A second pixel electrode 1824 is formed on the insulating film 1820. A contact hole 1823 is formed in the second pixel electrode 1824. The second pixel electrode 1824 is made of the same material as the pixel electrode shown in the embodiment mode 1. As shown in FIG. 19, the first pixel electrode (common potential line 1809) The first pixel electrode (common potential line) is connected to the second pixel electrode 1824 so that a horizontal electric field is generated between the first pixel electrode (common potential line) and the second pixel electrode 1824. 1809) and the second electrode are formed. Also, the slit portion of the second pixel electrode 1824 The portion is formed so as to be engaged with the electrode portion of the first pixel electrode (common potential line 1809).

[0137] A potential difference occurs between the first pixel electrode (common potential line 1809) and the second pixel electrode 1824. As a result, an electric field is generated between the first pixel electrode (common potential line 1809) and the second pixel electrode 1824. This electric field is used to rotate the liquid crystal molecules horizontally. Since the display is arranged horizontally, there is little problem with contrast reduction depending on the viewing angle. The field will become wider.

[0138] The storage capacitor is a gate between the first pixel electrode (common potential line 1809) and the capacitor electrode 1815. The gate insulating film 1806 is provided. The electrode 1824 is connected via a contact hole 1833 .

[0139] Next, a TN type liquid crystal display device will be described.

[0140] 20 and 21 show the pixel structure of a TN type liquid crystal display device. 21 is a plan view. Note that FIG. 20 is a cross-sectional view taken along line MN in FIG. The following description will be given with reference to both figures.

[0141] The pixel electrode 2024 is connected to the TFT 2028 via the wiring 2018 through the contact hole 2023. The wiring 2016, which functions as a data line, is connected to the TFT 2028. The TFT shown in the first or second embodiment can be used as the TFT 2028.

[0142] The pixel electrode 2024 may be made of the same material as the pixel electrode shown in the first embodiment. can.

[0143] The counter substrate 2001 is provided with a light-shielding film 2032, a colored film 2036, a counter electrode 2040, and an alignment film. 2060, etc. are formed. In addition, a flat layer is formed between the colored film 2036 and the counter electrode 2040. An alignment film 2037 is formed on the pixel electrode 2024 to prevent the alignment of the liquid crystal from being disturbed. The liquid crystal layer 2050 is formed between the pixel electrode 2024 and the counter electrode 2040. It is provided in.

[0144] In addition, the substrate 2000 or the counter substrate 2001 may be provided with a colored film (color filter) or a A shielding film (black matrix) may be formed to prevent screening. In addition, a polarizing plate is attached to the surface of the substrate 2000 opposite to the surface on which the TFT 2028 is formed. Also, a polarizing plate is formed on the surface of the counter substrate 2001 opposite to the surface on which the counter electrode 2040 is formed. The counter electrode 2040 is the same as the pixel electrode shown in the first embodiment. The above materials can be used appropriately.

[0145] The storage capacitor is connected to a capacitance wiring 2004 formed in the same layer as the gate electrode 2002. The pixel electrode 2015 is formed of a photoresist insulating film 2006 and a capacitance electrode 2015. The electrode 2024 is connected via a contact hole 2033 .

[0146] As described above, various methods using a microcrystalline semiconductor as a channel formation region of a pixel transistor have been developed. It is possible to provide a liquid crystal display device of this type.

[0147] The liquid crystal display device of the present invention uses thin film transistors with small off-current and small variation. The aperture ratio can be improved by using a OLED, which improves the brightness and provides excellent image quality. It is also possible to reduce the brightness of the backlight. This brings about an effect of improving the life span of the backlight.

[0148] Note that this embodiment mode can be used in appropriate combination with embodiment mode 1 or 2.

[0149] (Embodiment 4) In this embodiment, an electronic device using a liquid crystal display device of the present invention will be described with reference to FIG. He explains.

[0150] Examples of electronic devices manufactured using the semiconductor device of the present invention include video cameras, digital cameras, and the like. , goggle-type displays (head-mounted displays), navigation systems , audio playback devices (car audio components, etc.), computers, game devices, mobile information terminals (Mobile computers, mobile phones, portable game consoles, e-books, etc.), equipped with recording media Image playback devices that incorporate the Digital Versatile Disc (DVD) ) and a device equipped with a display that can play back recording media such as a DVD player and display the images. can be done.

[0151] FIG. 22A shows a television receiver or a monitor of a personal computer. 1, support base 2202, display unit 2203, speaker unit 2204, video input terminal 2205 The display unit 2203 uses a liquid crystal display device according to the present invention. A television receiver or a monitor of a personal computer having an improved aperture ratio and improved brightness is provided. can be provided.

[0152] Figure 22(B) shows a digital camera. The front part of the main body 2211 has an image receiving unit 2213. A shutter button 2216 is provided on the top surface of the main body 2211. In addition, on the rear surface of the main body 2211, a display unit 2212, operation keys 2214, and an external A connection port 2215 is provided. The liquid crystal display device of the present invention is used in the display unit 2212. The present invention provides a digital camera with improved aperture ratio and improved brightness. It is possible.

[0153] FIG. 22C shows a notebook type personal computer. The main body 2221 has a keyboard. A keyboard 2224, an external connection port 2225, and a pointing device 2226 are provided. In addition, a housing 2222 having a display unit 2223 is attached to the main body 2221. The display unit 2223 uses a liquid crystal display device according to the present invention. It is possible to provide a notebook personal computer with improved display efficiency and brightness.

[0154] FIG. 22(D) shows a mobile computer, which includes a main body 2231, a display unit 2232, a switch, The display unit 2232 includes an input / output port 2233, an operation key 2234, an infrared port 2235, etc. The display unit 2232 is provided with a liquid crystal display device according to the present invention. The present invention provides a mobile computer with improved aperture ratio and brightness. A computer can be provided.

[0155] FIG. 22E shows an image reproducing device. A main body 2241 is provided with a display unit 2244, a recording medium reader / writer, and a The main body 2241 is provided with a slide-in portion 2245 and an operation key 2246. A housing 2242 having a speaker unit 2247 and a display unit 2243 is attached. The liquid crystal display device of the present invention is used for each of the display portion 2243 and the display portion 2244. The present invention provides an image reproducing device with improved aperture ratio and improved brightness. can be done.

[0156] 22(F) shows an electronic book. A main body 2251 is provided with operation keys 2253. In addition, a plurality of display units 2252 are attached to the main body 2251. The liquid crystal display device of the present invention is used in the following applications. Improved electronic books can be provided.

[0157] FIG. 22(G) shows a video camera. The main body 2261 has an external connection port 2264 and a remote control. A computer receiving unit 2265, an image receiving unit 2266, a battery 2267, an audio input unit 2268, and an operation The main body 2261 is provided with a housing having a display unit 2262. The display unit 2262 is equipped with a liquid crystal display device according to the present invention. The present invention provides a video camera with improved aperture ratio and improved brightness. can.

[0158] FIG. 22H shows a mobile phone, which includes a main body 2271, a housing 2272, a display unit 2273, and an audio An input unit 2274, an audio output unit 2275, an operation key 2276, an external connection port 2277, The display unit 2273 includes a liquid crystal display device according to the present invention. According to the present invention, it is possible to provide a mobile phone having an improved aperture ratio and improved brightness.

[0159] As described above, the scope of application of the present invention is extremely wide, and it can be used in electronic devices in a wide range of fields. It is possible. Note that this embodiment mode can be used in appropriate combination with any of the first to third embodiments. can be done. [Explanation of symbols]

[0160] 100 Substrates 102 Gate electrode 104a Gate insulating layer 104b Gate insulating layer 106 Microcrystalline semiconductor layer 108 Buffer Layer 110 Semiconductor layer doped with impurity elements 112 Mask 114 Microcrystalline semiconductor layer 116 Buffer Layer 118 Semiconductor layer doped with impurity elements 120a Conductive layer 120b conductive layer 120c conductive layer 122 Mask 124a conductive layer 124b Conductive layer 124c conductive layer 126a conductive layer 126b Conductive layer 126c conductive layer 128a End 128b End 130a end 130b end 132 Source or drain region 134 Source or drain region 136 Buffer Layer 138 End 140 End 142 Thin-film transistor 144 Insulating Layer 146 Pixel electrode 600 Substrates 602 Pixel section 604 Scanning line driver circuit 606 Sealing material 608 Opposing Substrate 610 Liquid crystal 612 Signal Line Driver Circuit 614 Transistor 616 Thin Film Transistor 618 Pixel electrode 620 Counter Electrode 622 Spacer 624 Wiring 626 Wiring 628 FPC 630 Connection terminal 632 Anisotropic Conductive Materials 634 Wiring 640 Counter Electrode

Claims

[Claim 1] A pixel electrode electrically connected to a substrate having an insulating surface, a transistor formed on the substrate, The transistor is a gate electrode, a gate insulating layer on the gate electrode, a semiconductor layer having a microcrystalline structure on the gate insulating layer, and a buffer layer on the semiconductor layer having a microcrystalline structure; The display device according to the present invention is characterized in that a channel width W of the transistor and a channel length L of the transistor satisfy the relationship: 0.1≦W / L≦1.7.

Citation Information

Patent Citations

  • Electrode substrate and plane display apparatus

    JP1996201853A

  • Manufacture of field-effect thin film transistor

    JP1997092841A

  • Liquid crystal display device and its manufacturing method

    JP1998170961A

  • Semiconductor MIS field effect transistor with semi-amorphous semiconductor material

    US5591987A