Active matrix substrate, liquid crystal display device including the same, and manufacturing method for active matrix substrate
The active matrix substrate with a reflection suppressing layer and notch design addresses alignment disorder and burn-in issues in ultra-high-definition liquid crystal displays, ensuring high-quality images without additional manufacturing steps.
Patent Information
- Application Number
- JP2023068674
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-31
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In ultra-high-definition liquid crystal display devices with a COA structure, the alignment disorder of the liquid crystal layer occurs at the ends of slits in the transparent electrodes, leading to burn-in and afterimages due to overlapping structures with metal layers, which degrade display quality.
An active matrix substrate design featuring a reflection suppressing layer with a notch to avoid overlapping with the ends of slits, comprising laminated metal layers and an inorganic protective film, ensuring alignment order and suppressing reflections.
The solution effectively prevents burn-in and afterimages while maintaining ultra-high-definition pixel sizes, such as 1000 to 1200 ppi, by aligning the reflection suppressing layer to avoid slit ends, enhancing display quality and suitability for head-mounted displays.
Smart Images

Figure 2024154702000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an active matrix substrate, a liquid crystal display device including the active matrix substrate, and a method for manufacturing the active matrix substrate. [Background technology]
[0002] In recent years, liquid crystal display devices often use a color filter on array (hereinafter also referred to as COA) structure in which a color filter is provided on an active matrix substrate (array substrate) and alignment with an opposing substrate is not required.
[0003] For example, Patent Document 1 discloses a liquid crystal display device in which a pixel electrode and a common electrode are provided on a substrate having a COA structure, and which utilizes a FFS (Fringe Field Switching) mode, which is one of the in-plane switching driving methods. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2017-116821 A Summary of the Invention [Problem to be solved by the invention]
[0005] Incidentally, in a horizontal electric field driving type liquid crystal display device having an active matrix substrate with a COA structure in which a slit for liquid crystal alignment is formed in a pixel electrode or a common electrode, when the pixel size is ultra-high resolution of 1000 to 1200 ppi (pixel per inch) or more for head mounted display applications, for example, the end of the slit formed in the transparent electrode of the pixel electrode or the common electrode often overlaps with a reflection suppressing layer including a metal layer disposed between each colored layer of a color filter. In this case, in the portion where the electrically floating reflection suppressing layer and the end of the slit overlap, the alignment of the liquid crystal layer is disturbed, causing burn-in and residual images, resulting in a decrease in display quality.
[0006] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to suppress the occurrence of burn-in and afterimages at the ends of a slit formed in a transparent electrode. [Means for solving the problem]
[0007] In order to achieve the above-mentioned object, the active matrix substrate of the present invention comprises a base substrate, a plurality of thin film transistors provided on the base substrate corresponding to a plurality of sub-pixels, a color filter provided on each of the thin film transistors, with a colored layer of a predetermined color arranged corresponding to each of the sub-pixels, a first transparent electrode provided on the upper side of the color filter, a second transparent electrode provided on the first transparent electrode via an inorganic protective film made of an inorganic insulating film, and having a strip-shaped slit formed therein, and a reflection suppression layer provided in a strip shape on the inorganic protective film at the boundary portion of the colored layers of different colors, and in which a first metal layer, an intermediate layer and a second metal layer are laminated in this order, and is characterized in that the reflection suppression layer has a cutout portion so as not to overlap with an end of the slit.
[0008] Furthermore, a liquid crystal display device according to the present invention is characterized in comprising the above-mentioned active matrix substrate, a counter substrate provided opposite to the active matrix substrate, and a liquid crystal layer provided between the active matrix substrate and the counter substrate.
[0009] Also, a method for manufacturing an active matrix substrate according to the present invention includes a thin film transistor forming step of forming a plurality of thin film transistors on a base substrate corresponding to a plurality of sub-pixels, a color filter forming step of forming a color filter on each of the thin film transistors, the color filter having a colored layer of a predetermined color arranged thereon corresponding to each of the sub-pixels, a first transparent electrode forming step of forming a first transparent conductive film on an upper side of the color filter, and then patterning the first transparent conductive film to form a first transparent electrode, and a first insulating film, a first metal film, an intermediate film, and a second metal film so as to cover the first transparent electrode, and then patterning the first metal film, the intermediate film, and the second metal film to form a first metal layer, an intermediate layer, and a second metal layer, respectively, and The method includes a reflection-suppressing layer forming step of forming a reflection-suppressing layer having a metal layer, an intermediate layer, and a second metal layer stacked in this order in a strip-like shape so as to overlap the boundary portions of the colored layers of different colors; an inorganic protective film forming step of patterning the inorganic insulating film exposed from the reflection-suppressing layer to form an inorganic protective film; and a second transparent electrode forming step of forming a second transparent conductive film so as to cover the reflection-suppressing layer on the inorganic protective film, and then patterning the second transparent conductive film to form a second transparent electrode having a strip-like slit whose end portion overlaps with the reflection-suppressing layer, wherein in the second transparent electrode forming step, the reflection-suppressing layer exposed from the slit is removed to form a reflection-suppressing layer having a notch portion. Effect of the Invention
[0010] According to the present invention, it is possible to suppress the occurrence of burn-in or afterimages at the ends of a slit formed in a transparent electrode. [Brief description of the drawings]
[0011] [Figure 1] 1 is a plan view of an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. [Diagram 2] 2 is a cross-sectional view of the active matrix substrate and a liquid crystal display device including the same, taken along line II-II in FIG. [Diagram 3]3 is a cross-sectional view of the active matrix substrate and a liquid crystal display device including the same, taken along line III-III in FIG. [Figure 4] 4 is a cross-sectional view of the active matrix substrate and a liquid crystal display device including the same, taken along line IV-IV in FIG. [Diagram 5] 1 is a first cross-sectional view illustrating a part of a manufacturing process of an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. [Figure 6] 5 showing a second cross-sectional view subsequent to FIG. 5 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. [Figure 7] 7 is a third cross-sectional view following FIG. 6 showing a part of the manufacturing process of the active matrix substrate constituting the liquid crystal display device according to the first embodiment of the present invention. FIG. [Figure 8] 7 showing a fourth cross-sectional view following FIG. 7 illustrating a part of a manufacturing process of the active matrix substrate constituting the liquid crystal display device according to the first embodiment of the present invention. FIG. [Figure 9] 8 showing a fifth cross-sectional view following FIG. 8 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. [Figure 10] 9 showing a sixth cross-sectional view continuing from FIG. 9 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. FIG. [Figure 11] 10 showing a seventh cross-sectional view continuing from FIG. 10 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. FIG. [Figure 12] 11 showing a part of a manufacturing process of an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. FIG. [Figure 13] 12 showing a part of a manufacturing process of the active matrix substrate constituting the liquid crystal display device according to the first embodiment of the present invention. FIG. [Figure 14]13 showing a part of a manufacturing process of an active matrix substrate constituting a liquid crystal display device according to a first embodiment of the present invention. FIG. [Figure 15] FIG. 11 is a plan view of an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. [Figure 16] 16 is a cross-sectional view of the active matrix substrate taken along line XVI-XVI in FIG. 15. [Figure 17] 17 is a cross-sectional view of the active matrix substrate taken along line XVII-XVII in FIG. 15. [Figure 18] 18 is a cross-sectional view of the active matrix substrate taken along line XVIII-XVIII in FIG. 15. [Figure 19] FIG. 11 is a plan view of a modified example of an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. [Figure 20] 10A to 10C are first cross-sectional views illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. [Figure 21] 20 showing a second cross-sectional view following FIG. 20 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. [Figure 22] 21 showing a third cross-sectional view following FIG. 21 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. FIG. [Figure 23] 22 showing a fourth cross-sectional view following FIG. 22 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. FIG. [Figure 24] 23 showing a fifth cross-sectional view continuing from FIG. 23 illustrating a part of a manufacturing process for an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. FIG. [Diagram 25] 25 is a sixth cross-sectional view continuing from FIG. 24 and showing a part of a manufacturing process of an active matrix substrate constituting a liquid crystal display device according to a second embodiment of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to the following embodiments.
[0013] First Embodiment 1 to 14 show a first embodiment of an active matrix substrate, a liquid crystal display device including the same, and a method for manufacturing the active matrix substrate according to the present invention. Here, Fig. 1 is a plan view of an active matrix substrate 30a constituting the liquid crystal display device of the present embodiment. Also, Figs. 2, 3, and 4 are cross-sectional views of a liquid crystal display device 50 taken along lines II-II, III-III, and IV-IV in Fig. 1.
[0014] As shown in Figs. 2 to 4, the liquid crystal display device 50 includes an active matrix substrate 30a having a COA structure, a counter substrate 40 provided to face the active matrix substrate 30a, and a liquid crystal layer 45 provided between the active matrix substrate 30a and the counter substrate 40. In the liquid crystal display device 50, a plurality of sub-pixels P (see Fig. 1) are provided in a matrix in a display region for displaying an image. Here, as shown in Figs. 2 to 4, the display region includes a sub-pixel P having a red layer 16r for performing red gradation display, a sub-pixel P having a green layer 16g for performing green gradation display, and a sub-pixel P having a blue layer (not shown) for performing blue gradation display, which are provided adjacent to each other. In the display region, one pixel is formed by three adjacent sub-pixels P for performing red, green, and blue gradation display.
[0015] As shown in Figures 2 to 4, the active matrix substrate 30a includes a base substrate 10a such as a glass substrate, a plurality of thin film transistors (hereinafter also referred to as TFTs) 5 provided on the base substrate 10a corresponding to a plurality of sub-pixels P, a color filter 16 provided on each TFT 5, an organic protective film 17 provided on the color filter 16, a plurality of pixel electrodes 18a each provided as a first transparent electrode on the organic protective film 17, an inorganic protective film 19a provided on each pixel electrode 18a, a common electrode 23a provided as a second transparent electrode on the inorganic protective film 19a, a surface protective film 25 provided on the common electrode 23a, and an alignment film 26 provided on the surface protective film 25. As shown in FIG. 1, the active matrix substrate 30a includes a base substrate 10a and a plurality of gate lines 11 arranged in the display region so as to extend parallel to each other in the Y direction in the figure, and a plurality of source lines 14 arranged so as to extend parallel to each other in the X direction in the figure and to intersect with each gate line 11 via a gate insulating film 12.
[0016] 2, the TFT 5 includes a gate electrode 11a provided on a base substrate 10a, a gate insulating film 12 provided so as to cover the gate electrode 11a, a semiconductor layer 13 provided on the gate insulating film 12 in an island shape so as to overlap the gate electrode 11a, and a source electrode 14a and a drain electrode 14b provided on the semiconductor layer 13 so as to be spaced apart from each other. The TFT 5 is provided for each intersection of the gate line 11 and the source line 14, that is, for each sub-pixel P. Here, the gate electrode 11a is a wide portion of the gate line 11 as shown in FIG. 1. The semiconductor layer 13 includes, for example, an intrinsic amorphous silicon layer provided on the gate insulating film 12 side, and a pair of n-type electrodes provided on the intrinsic amorphous silicon layer so as to expose the channel region of the intrinsic amorphous silicon layer and to be spaced apart from each other. + 1, the source electrode 14a is a portion that protrudes in an L-shape to the side of the source line 14, and is disposed on one n-type side of the semiconductor layer 13. +The drain electrode 14b is disposed in contact with the other n-type amorphous silicon layer of the semiconductor layer 13. + 2, the semiconductor layer 13 is electrically connected to the pixel electrode 18a via a contact hole H formed in the color filter 16 and the organic protective film 17. Note that, although the semiconductor layer 13 including an intrinsic amorphous silicon layer is exemplified in this embodiment, the semiconductor layer 13 may be composed of, for example, polysilicon of LTPS (low temperature polysilicon), an In-Ga-Zn-O-based oxide semiconductor, or the like.
[0017] The color filter 16 is provided so that a colored layer of a predetermined color is arranged corresponding to each sub-pixel P, and specifically, as shown in Figs. 2 to 4, the color filter 16 includes a red layer 16r provided as a colored layer in the sub-pixel P for displaying red gradations, a green layer 16g provided as a colored layer in the sub-pixel P for displaying green gradations, and a blue layer (not shown) provided as a colored layer in the sub-pixel P for displaying blue gradations. An interlayer insulating film 15 is provided between the TFT 5 and the color filter 16. Here, the gate insulating film 12, the interlayer insulating film 15, the inorganic protective film 19a, and the surface protective film 25 are each formed of a single layer or a multilayer film of an inorganic insulating film such as silicon nitride, silicon oxide, or silicon oxynitride.
[0018] The organic protective film 17 is made of a transparent organic resin material such as an acrylic resin.
[0019] 1 to 4, the pixel electrode 18a is provided in a rectangular shape on the organic protective film 17. Here, as shown in Fig. 1, the multiple pixel electrodes 18a are provided in a matrix shape corresponding to the multiple sub-pixels P. The pixel electrode 18a, together with the common electrode 23a and the inorganic protective film 19a provided between the common electrode 23a, constitutes an auxiliary capacitance of each sub-pixel P.
[0020] As shown in FIG. 1, the common electrode 23a is provided in common to a plurality of sub-pixels P. In addition, as shown in FIG. 1 and FIG. 4, the common electrode 23a is provided with a strip-shaped slit Sa for aligning the liquid crystal layer 45 so as to penetrate the common electrode 23a. Here, as shown in FIG. 1, both ends of the slit Sa are provided so as to intersect with the reflection suppression forming layer Bp described later. In addition, as shown in FIG. 1 and FIG. 2, the common electrode 23a is provided with a rectangular opening M penetrating the common electrode 23a so as to overlap with the contact hole H. Furthermore, inside the opening M of the common electrode 23a, as shown in FIG. 1 and FIG. 2, a transparent conductive layer 23b formed in the same layer as the common electrode 23a by the same material is provided in a concave shape separated from the common electrode 23a so as to overlap the bottom and side surfaces of the contact hole H. In addition, as shown in FIG. 2, a resin filling layer 24 is provided between the transparent conductive layer 23b and the surface protective film 25. Furthermore, between the common electrode 23a and the inorganic protective film 19a, an anti-reflection layer B is provided on the inorganic protective film 19a so as to overlap the boundary portion L of the colored layers of different colors, as shown in Figures 1, 3, and 4.
[0021] As shown in Fig. 1, the reflection suppressing layer B is provided in a strip shape across the display area so as to overlap each source line 14. As shown in Figs. 3 and 4, the reflection suppressing layer B includes a first metal layer 20a, an intermediate layer 21a, and a second metal layer 22a, which are laminated in this order on an inorganic protective film 19a, and is configured to reflect light incident from the liquid crystal layer 45 side by the second metal layer 22a, reflect light transmitted through the second metal layer 22a without being reflected by the second metal layer 22a by the first metal layer 20a, and suppress reflection of light incident from the liquid crystal layer 45 side by canceling out the light reflected by the second metal layer 22a and the light reflected by the first metal layer 20a. Here, the first metal layer 20a is configured of a metal film such as a tungsten film, a molybdenum film, or a molybdenum-tungsten alloy having a thickness of about 60 nm or more. The intermediate layer 21a is made of, for example, an inorganic insulating film such as a silicon nitride film having a refractive index of about 1.8 to 2.1 and a thickness of about 40 nm to 90 nm, or a transparent conductive film such as an ITO (Indium Tin Oxide) film or an IZO (Indium Zinc Oxide) film. The second metal layer 22a is made of, for example, a metal film such as a tungsten film or a molybdenum film having a thickness of about 2 nm to 15 nm.
[0022] 1 and 4, the antireflection layer B has a cutout C so as not to overlap both ends of the slit Sa. Here, the end face of the cutout C and the end face of the end of the slit Sa corresponding to the cutout C are provided flush with each other. In this specification, the end faces being flush with each other does not only refer to the case where the two end faces are aligned with each other strictly without any step, but also includes the case where there is a slight step of, for example, about 0.8 μm or less.
[0023] The alignment film 26 and an alignment film 31 described later are made of, for example, a polyimide resin whose surface has been subjected to a rubbing treatment.
[0024] As shown in FIGS. 2 to 4, the counter substrate 40 includes a base substrate 10b such as a glass substrate, and an alignment film 31 provided on the base substrate 10b.
[0025] The liquid crystal layer 45 is made of, for example, a nematic liquid crystal material having electro-optical properties. Here, the liquid crystal layer 45 is sealed between the active matrix substrate 30a and the counter substrate 40 by a frame-shaped sealant that bonds the active matrix substrate 30a and the counter substrate 40 to each other in a frame region around the display area.
[0026] The liquid crystal display device 50 having the above-described configuration applies a predetermined voltage to the liquid crystal layer 45 and auxiliary capacitance disposed between each pixel electrode 18a and the common electrode 23a, and changes the orientation state of the liquid crystal layer 45 due to an electric field generated in a direction along the substrate surface, i.e., in the horizontal direction, thereby adjusting the transmittance of light passing through the panel of each sub-pixel P, thereby displaying an image.
[0027] Next, a method for manufacturing the liquid crystal display device 50 of this embodiment will be described, focusing on a method for manufacturing the active matrix substrate 30a. Here, Figs. 5 to 14 are first to tenth cross-sectional views successively showing a part of the manufacturing process of the active matrix substrate 30a. In each of the cross-sectional views of Figs. 5 to 14, the right side, center, and left side of the broken line in the figure respectively show the parts corresponding to the cross-sectional views of Figs. 2, 3, and 4. The manufacturing process of the active matrix substrate 30a includes a TFT forming step, a color filter forming step, a first transparent electrode forming step, a reflection suppressing layer forming step, an inorganic protective film forming step, and a second transparent electrode forming step.
[0028] First, an aluminum film (about 300 nm thick) and a molybdenum niobium film (about 50 nm thick) are sequentially formed on a base substrate 10a such as a glass substrate, for example, by a sputtering method to form a metal laminate film, and then the metal laminate film is subjected to photolithography, etching, and resist stripping and cleaning to form a gate line 11 including a gate electrode 11a.
[0029] Next, on the surface of the substrate on which the gate lines 11 are formed, an inorganic insulating film (about 350 nm thick) such as a silicon nitride film or a silicon oxide film, an intrinsic amorphous silicon film (about 120 nm thick) and a phosphorus-doped n + After forming an amorphous silicon film (approximately 30 nm thick), a true amorphous silicon film and a n + The laminated film of the amorphous silicon film is subjected to photolithography, etching, and resist stripping and cleaning to form a gate insulating film 12 and a semiconductor formation layer.
[0030] Thereafter, on the substrate surface on which the gate insulating film 12 and the semiconductor formation layer are formed, a titanium film (about 30 nm thick), an aluminum film (about 300 nm thick), and a titanium film (about 50 nm thick) are successively formed by, for example, a sputtering method to form a metal laminate film, and then the metal laminate film is subjected to photolithography, etching, and resist stripping and cleaning to form the source line 14, the source electrode 14a, and the drain electrode 14b.
[0031] Furthermore, the source electrode 14a and the drain electrode 14b are used as a mask to form the n-type semiconductor layer. + The amorphous silicon film is removed by etching to form the semiconductor layer 13 and the TFT 5 including the semiconductor layer 13 (TFT formation step).
[0032] Next, on the substrate surface on which the TFTs 5 are formed, an inorganic insulating film (about 750 nm thick) such as a silicon nitride film or a silicon oxide film is formed by, for example, a plasma CVD method to form an interlayer insulating film 15, and then, for example, a spin coat method or a slit coat method is used to apply an acrylic photosensitive resin (about 1.6 μm thick) colored in red, green, or blue, and the applied photosensitive resin is partially exposed to light and then developed for patterning to form a colored layer of the selected color (for example, a red layer 16r). Furthermore, the same process is repeated for the other two colors to form colored layers of the other two colors (for example, a green layer 16g and a blue layer), and a color filter 16 having contact holes H is formed as shown in FIG. 5 (color filter formation process).
[0033] Thereafter, an acrylic photosensitive resin (about 2.0 μm thick) is applied to the surface of the substrate on which the color filter 16 is formed, for example, by spin coating or slit coating, and the applied photosensitive resin is partially exposed to light and then developed for patterning, thereby forming an organic protective film 17 having a contact hole H, as shown in FIG. 6.
[0034] Furthermore, the interlayer insulating film 15 exposed from the contact hole H is etched to form the contact hole H in the interlayer insulating film 15 as shown in FIG.
[0035] Next, a first transparent conductive film 18 of an ITO film or IZO film having a thickness of about 70 nm is formed, for example, by a sputtering method on the substrate surface on which the contact hole H is formed in the interlayer insulating film 15, as shown in FIG. 8, and then the first transparent conductive film 18 is subjected to photolithography, etching, and resist stripping and cleaning to form a pixel electrode 18a, as shown in FIG. 9 (first transparent electrode formation process).
[0036] Thereafter, an inorganic insulating film 19 such as a silicon nitride film having a thickness of about 100 nm is formed on the substrate surface on which the pixel electrodes 18a are formed, for example, by a plasma CVD method, and a first metal film 20 such as a molybdenum-tungsten alloy film having a thickness of about 60 nm, an intermediate film 21 such as an IZO film having a thickness of about 60 nm, and a second metal film 22 such as a molybdenum film having a thickness of about 6 nm are formed by a sputtering method, and then, as shown in FIG. 10, a resist Ra is formed on the substrate surface by photolithography.
[0037] Furthermore, the first metal film 20, the intermediate film 21 and the second metal film 22 exposed from the resist Ra are wet etched using a mixed acid solution of phosphoric acid, nitric acid and acetic acid to form an anti-reflection forming layer Bp in which the first metal layer 20ap, the intermediate layer 21ap and the second metal layer 22ap are stacked, as shown in FIG. 11 (anti-reflection forming layer forming process).
[0038] Next, after the resist Ra is stripped and washed, the inorganic insulating film 19 is subjected to photolithography, etching, and the resist is stripped and washed to form an inorganic protective film 19a as shown in FIG. 12 (inorganic protective film forming step).
[0039] Then, a second transparent conductive film 23, which is an ITO film or an IZO film and has a thickness of about 70 nm, is formed on the substrate surface on which the inorganic protective film 19a is formed, for example, by a sputtering method, and then a resist Rb is formed on the substrate surface by photolithography, as shown in FIG. 13.
[0040] Furthermore, the second transparent conductive film 23 and the anti-reflection forming layer Bp exposed from the resist Ra are wet etched using a mixed acid solution of phosphoric acid, nitric acid and acetic acid, so that a common electrode 23a having a slit Sa and an opening M, a transparent conductive layer 23b, a first metal layer 20a, an intermediate layer 21a and a second metal layer 22a are stacked to form an anti-reflection layer B having a cutout portion C, as shown in FIG. 14 (second transparent electrode forming process).
[0041] Next, an acrylic photosensitive resin (about 2.5 μm thick) is applied, for example, by spin coating or slit coating, to the substrate surface on which the common electrode 23a etc. are formed, and the applied photosensitive resin is partially exposed to light and then developed for patterning to form a filling resin layer 24.
[0042] Furthermore, on the substrate surface on which the filled resin layer 24 has been formed, an inorganic insulating film (with a thickness of about 30 nm) such as a silicon nitride film is formed by, for example, a plasma CVD method, thereby forming a surface protective film 25.
[0043] Finally, a polyimide resin film is applied by, for example, a printing method to the entire substrate on which the surface protection film 25 has been formed, and then the resin film is subjected to baking and rubbing treatments to form an alignment film 26.
[0044] In this manner, the active matrix substrate 30a can be manufactured.
[0045] Furthermore, the active matrix substrate 30a and the counter substrate 40 manufactured as described above are bonded together via a sealant, and a liquid crystal material is sealed between the active matrix substrate 30a and the counter substrate 40 to form a liquid crystal layer 45, thereby manufacturing the liquid crystal display device 50.
[0046] As described above, according to the active matrix substrate 30a of the present embodiment, the liquid crystal display device 50 including the active matrix substrate 30a, and the method for manufacturing the active matrix substrate 30a, in the second transparent electrode formation step, the anti-reflection formation layer Bp exposed from the slits Sa of the common electrode 23a is removed, and the anti-reflection layer B having the cutout portions C provided so as not to overlap with both ends of the slits Sa is formed. As a result, the anti-reflection layer B is not exposed from the slits Sa of the common electrode 23a, so that alignment disturbance of the liquid crystal layer 45 is suppressed, and the occurrence of burn-in or afterimages at the ends of the slits Sa formed in the common electrode 23a can be suppressed.
[0047] Furthermore, according to the active matrix substrate 30a of the present embodiment, the liquid crystal display device 50 including the active matrix substrate 30a, and the method for manufacturing the active matrix substrate 30a, both ends of the slit Sa of the common electrode 23a overlap with the anti-reflection formation layer Bp which becomes the anti-reflection layer B, so that it is possible to realize an ultra-high definition pixel size of 1000 to 1200 ppi or more for use in head mounted displays, for example.
[0048] Furthermore, according to the active matrix substrate 30a of the present embodiment, the liquid crystal display device 50 including the active matrix substrate 30a, and the manufacturing method for the active matrix substrate 30a, the common electrode 23a is provided on the reflection suppressing layer B in which the first metal layer 20a, the intermediate layer 21a, and the second metal layer 22a are laminated in this order, so that it is possible to effectively suppress reflection of light incident from the liquid crystal layer 45 side without adding any manufacturing process.
[0049] Second Embodiment 15 to 25 show a second embodiment of an active matrix substrate, a liquid crystal display device including the same, and a method for manufacturing the active matrix substrate according to the present invention. Here, FIG. 15 is a plan view of an active matrix substrate 30b constituting the liquid crystal display device of this embodiment. Also, FIGS. 16, 17, and 18 are cross-sectional views of the active matrix substrate 30b taken along lines XVI-XVI, XVII-XVII, and XVIII-XVIII in FIG. 15. Also, FIG. 19 is a plan view of an active matrix substrate 30c which is a modified example of the active matrix substrate 30b. In the following embodiments, the same parts as those in FIGS. 1 to 14 are denoted by the same reference numerals, and detailed description thereof will be omitted.
[0050] In the above-described first embodiment, a liquid crystal display device 50 is illustrated that includes an active matrix substrate 30a in which a common electrode 23a is provided above a pixel electrode 18a and a slit Sa is formed in the common electrode 23a. In contrast, in the present embodiment, a liquid crystal display device is illustrated that includes an active matrix substrate 30b in which a pixel electrode 23b is provided above a common electrode 18ba and a slit Sb is formed in the pixel electrode 23b.
[0051] The liquid crystal display device of this embodiment includes an active matrix substrate 30b having a COA structure, a counter substrate 40 (see FIGS. 2 to 4) provided to face the active matrix substrate 30b, and a liquid crystal layer 45 (see FIGS. 2 to 4) provided between the active matrix substrate 30b and the counter substrate 40. In the liquid crystal display device of this embodiment, a plurality of sub-pixels P are provided in a matrix in the display region, similar to the liquid crystal display device 50 of the first embodiment. In the display region, a sub-pixel P in which a red layer 16r is arranged, a sub-pixel P in which a green layer 16g is arranged, and a sub-pixel P in which a blue layer is arranged are provided adjacent to each other, similar to the liquid crystal display device 50 of the first embodiment.
[0052] 16 to 18, the active matrix substrate 30b includes a base substrate 10a such as a glass substrate, a plurality of TFTs 5 provided on the base substrate 10a corresponding to a plurality of sub-pixels P, a color filter 16 provided on each TFT 5, an organic protective film 17 provided on the color filter 16, a common electrode 18ba provided as a first transparent electrode on the organic protective film 17, an inorganic protective film 19b provided on the common electrode 18ba, a plurality of pixel electrodes 23b provided as second transparent electrodes on the inorganic protective film 19b, a surface protective film 25 provided on each pixel electrode 23b, and an alignment film 26 provided on the surface protective film 25. Similarly to the active matrix substrate 30a of the first embodiment, the active matrix substrate 30b includes a plurality of gate lines 11 and a plurality of source lines 14.
[0053] As shown in Fig. 15, the common electrode 18ba is provided on the organic protective film 17 in common to a plurality of sub-pixels P. Furthermore, as shown in Fig. 15 and Fig. 16, the common electrode 18ba is provided with a rectangular opening M penetrating the common electrode 18ba so as to overlap with the contact hole H. Furthermore, inside the opening M of the common electrode 18ba, a transparent conductive layer 18bb, which is formed in the same layer and of the same material as the common electrode 18ba, is provided in a concave shape spaced apart from the common electrode 18ba so as to overlap with the bottom and side surfaces of the contact hole H, as shown in Fig. 15 and Fig. 16.
[0054] The pixel electrode 23b is provided in a rectangular shape as shown in FIG. 15. Here, the pixel electrodes 23b are provided in a matrix shape corresponding to the sub-pixels P. The pixel electrode 23b, together with the common electrode 18ba and the inorganic protective film 19b provided between the common electrode 18ba, constitutes an auxiliary capacitance of each sub-pixel P. The pixel electrode 23b is electrically connected to the drain electrode 14b of the TFT 5 through the transparent conductive layer 18bb provided in the contact hole H as shown in FIG. 16. The pixel electrode 23b is provided with a strip-shaped slit Sb for orienting the liquid crystal layer 45 so as to penetrate the pixel electrode 23b as shown in FIG. 15 and FIG. 18. One end of the slit Sb (lower left side in FIG. 15) is provided so as to intersect with the reflection suppression forming layer Bp described later. Between the pixel electrode 23b and the surface protective film 25, a resin filling layer 24 is provided as shown in FIG. 16. Furthermore, between the pixel electrode 23b and the inorganic protective film 19b, an anti-reflection layer B is provided on the inorganic protective film 19b so as to overlap the boundary portion L of the colored layers of different colors, as shown in Figures 15, 17, and 18.
[0055] As shown in Fig. 15, the reflection suppression layer B is provided in a discontinuous strip shape for each sub-pixel P so as to overlap each source line 14. As shown in Figs. 17 and 18, the reflection suppression layer B includes a first metal layer 20b, an intermediate layer 21b, and a second metal layer 22b which are laminated in this order on an inorganic protective film 19b, and is configured to reflect light incident from the liquid crystal layer 45 side by the second metal layer 22b, reflect light transmitted through the second metal layer 22b without being reflected by the second metal layer 22b by the first metal layer 20b, and suppress reflection of light incident from the liquid crystal layer 45 side by canceling out the light reflected by the second metal layer 22b and the light reflected by the first metal layer 20b. Here, the first metal layer 20b is configured of a metal film such as a tungsten film, a molybdenum film, or a molybdenum-tungsten alloy having a thickness of about 60 nm or more. The intermediate layer 21b is, for example, made of an inorganic insulating film such as a silicon nitride film having a refractive index of about 1.8 to 2.1 and a thickness of about 40 nm to 90 nm, or a transparent conductive film such as an ITO film or an IZO film. The second metal layer 22b is, for example, made of a metal film such as a tungsten film or a molybdenum film having a thickness of about 2 nm to 15 nm. As shown in Figs. 15 and 18, the antireflection layer B is provided with a notch C so as not to overlap one end of the slit Sb (the lower left side in Fig. 15). Here, the end face of the notch C and the end face of the end of the slit Sa corresponding to the notch C are provided flush with each other.
[0056] In the present embodiment, the active matrix substrate 30b is exemplified in which both end faces in the length direction (X direction in FIG. 15) of the reflection antireflection layer B are disposed inside both end faces in the length direction (X direction in FIG. 15) of the pixel electrode 23b in each subpixel P, but the active matrix substrate 30c shown in FIG. 19 may be used. Specifically, in the active matrix substrate 30c, as shown in FIG. 19, both end faces in the length direction (X direction in FIG. 15) of the reflection antireflection layer B are flush with both end faces in the length direction (X direction in FIG. 15) of the pixel electrode 23b.
[0057] The liquid crystal display device of this embodiment, like the liquid crystal display device 50 of the first embodiment described above, is configured to display images by applying a predetermined voltage to the liquid crystal layer 45 and auxiliary capacitance arranged between each pixel electrode 23b and the common electrode 18ba, and changing the orientation state of the liquid crystal layer 45 due to an electric field generated in a direction along the substrate surface, i.e., in the horizontal direction, thereby adjusting the transmittance of light passing through the panel of each sub-pixel P.
[0058] Next, a method for manufacturing the liquid crystal display device of this embodiment will be described, focusing on a method for manufacturing the active matrix substrate 30b. Here, Figs. 20 to 25 are first to sixth cross-sectional views successively showing a part of the manufacturing process of the active matrix substrate 30b. Note that in the cross-sectional views of Figs. 20 to 25, the right side, center, and left side of the broken lines correspond to the cross-sectional views of Figs. 16, 17, and 18, respectively.
[0059] First, in the manufacturing method of the active matrix substrate 30a of the first embodiment, a first transparent conductive film 18 (see FIG. 8) made of an ITO film or an IZO film is formed, for example, by a sputtering method on a substrate surface having a contact hole H formed in an interlayer insulating film 15. Then, the first transparent conductive film 18 is subjected to photolithography, etching, and resist stripping and cleaning to form a common electrode 18ba having an opening M and a transparent conductive layer 18bb, as shown in FIG. 20 (first transparent electrode formation process).
[0060] Next, on the substrate surface on which the common electrode 18ba etc. are formed, for example, by plasma CVD method, an inorganic insulating film 19 such as a silicon nitride film having a thickness of about 100 nm is formed, and a first metal film 20 such as a molybdenum-tungsten alloy film having a thickness of about 60 nm, an intermediate film 21 such as a silicon nitride film having a thickness of about 60 nm, and a second metal film 22 such as a molybdenum film having a thickness of about 6 nm are formed by sputtering method, and then a resist Rc is formed on the substrate surface by photolithography, as shown in FIG. 21.
[0061] Thereafter, the first metal film 20, the intermediate film 21 and the second metal film 22 exposed from the resist Rc are dry etched using a fluorine-based gas to form an anti-reflection forming layer Bp in which the first metal layer 20bp, the intermediate layer 21bp and the second metal layer 22bp are stacked, as shown in FIG. 22 (anti-reflection forming layer formation process).
[0062] Furthermore, after the resist Rc is stripped and washed, the inorganic insulating film 19 is subjected to photolithography, etching, and the resist is stripped and washed to form an inorganic protective film 19b as shown in FIG. 23 (inorganic protective film forming step).
[0063] Next, a second transparent conductive film 23, which is an ITO film or an IZO film and has a thickness of about 70 nm, is formed on the substrate surface on which the inorganic protective film 19b is formed, for example, by a sputtering method, and then a resist Rd is formed on the substrate surface by photolithography, as shown in FIG. 24.
[0064] Furthermore, the second transparent conductive film 23 and the anti-reflection forming layer Bp exposed from the resist Rd are dry etched using a fluorine-based gas to form a pixel electrode 23b having a slit Sb, a first metal layer 20b, an intermediate layer 21b and a second metal layer 22b, as shown in FIG. 25, and a anti-reflection layer B having a cutout portion C is formed (second transparent electrode forming process).
[0065] Next, an acrylic photosensitive resin (about 2.5 μm thick) is applied to the substrate surface on which the pixel electrodes 23b etc. are formed, for example, by spin coating or slit coating, and the applied photosensitive resin is partially exposed to light and then developed to pattern it, thereby forming a filling resin layer 24.
[0066] Furthermore, on the substrate surface on which the filled resin layer 24 has been formed, an inorganic insulating film (with a thickness of about 30 nm) such as a silicon nitride film is formed by, for example, a plasma CVD method, thereby forming a surface protective film 25.
[0067] Finally, a polyimide resin film is applied by, for example, a printing method to the entire substrate on which the surface protection film 25 has been formed, and then the resin film is subjected to baking and rubbing treatments to form an alignment film 26.
[0068] In this manner, the active matrix substrate 30b can be manufactured.
[0069] Furthermore, the active matrix substrate 30b and the counter substrate 40 manufactured as described above are bonded together via a sealant, and a liquid crystal material is filled between the active matrix substrate 30b and the counter substrate 40 to form a liquid crystal layer 45, thereby manufacturing the liquid crystal display device of this embodiment.
[0070] As described above, according to the active matrix substrate 30b of the present embodiment, the liquid crystal display device including the active matrix substrate 30b, and the method for manufacturing the active matrix substrate 30b, in the second transparent electrode formation step, the anti-reflection layer Bp exposed from the slits Sb of the pixel electrode 23b is removed, and the anti-reflection layer B having the cutout portion C provided so as not to overlap one end of the slits Sb is formed. As a result, the anti-reflection layer B is not exposed from the slits Sb of the pixel electrode 23b, so that alignment disturbance of the liquid crystal layer 45 is suppressed, and the occurrence of burn-in or afterimages at the end of the slits Sb formed in the pixel electrode 23b can be suppressed.
[0071] Furthermore, according to the active matrix substrate 30b of the present embodiment, the liquid crystal display device including the same, and the method for manufacturing the active matrix substrate 30b, one end of the slit Sb of the pixel electrode 23b overlaps with the antireflection formation layer Bp which becomes the antireflection layer B, so that it is possible to realize an ultra-high definition pixel size of 1000 to 1200 ppi or more for use in, for example, a head mounted display.
[0072] Furthermore, according to the active matrix substrate 30b of the present embodiment, the liquid crystal display device including the active matrix substrate 30b, and the method for manufacturing the active matrix substrate 30b, the pixel electrode 23b is provided on the reflection suppressing layer B in which the first metal layer 20b, the intermediate layer 21b, and the second metal layer 22b are laminated in this order, so that it is possible to effectively suppress the reflection of light incident from the liquid crystal layer 45 side without adding any manufacturing process.
[0073] Other Embodiments In each of the above embodiments, a liquid crystal display device including an active matrix substrate in which an electrode of a TFT connected to a pixel electrode is used as a drain electrode has been exemplified. However, the present invention can also be applied to a liquid crystal display device including an active matrix substrate in which an electrode of a TFT connected to a pixel electrode is called a source electrode. [Industrial Applicability]
[0074] As described above, the present invention is useful for a liquid crystal display device of the in-plane switching driving type that includes an active matrix substrate having a color filter on-array structure. [Explanation of symbols]
[0075] B Reflection suppression layer Bp reflection suppressing layer C Cutout H Contact Hole L boundary part P subpixel Sa,Sb slit 5 TFT (Thin Film Transistor) 10a Base board 16 Color Filters 16g green layer (colored layer) 16r Red layer (colored layer) 17 Organic protective film 18 First transparent conductive film 18a Pixel electrode (first transparent electrode) 18ba common electrode (first transparent electrode) 19 Inorganic insulating film 19a,19b Inorganic protective film 20 First metal film 20a,20ap,20b,20bp 1st metal layer 21 Interlayer 21a,20ap,21b,21bp middle layer 22 Second metal film 22a,22ap,22b,22bp 2nd metal layer 23 Second transparent conductive film 23a Common electrode (second transparent electrode) 23b Pixel electrode (second transparent electrode) 30a, 30b, 30c Active matrix substrate 40 Opposing substrate 45 Liquid crystal layer 50 LCD display device
Claims
1. A base substrate; a plurality of thin film transistors provided on the base substrate corresponding to a plurality of sub-pixels; a color filter provided on each of the thin film transistors, the color filter including a colored layer of a predetermined color arranged corresponding to each of the sub-pixels; A first transparent electrode provided on the upper side of the color filter; a second transparent electrode provided on the first transparent electrode via an inorganic protective film made of an inorganic insulating film, the second transparent electrode having strip-shaped slits; a reflection suppressing layer provided in a strip shape on the inorganic protective film at a boundary portion of the colored layers having different colors, the reflection suppressing layer including a first metal layer, an intermediate layer, and a second metal layer laminated in this order; The active matrix substrate according to claim 1, wherein the antireflection layer is provided with a notch portion so as not to overlap an end portion of the slit.
2. 2. The active matrix substrate according to claim 1, an end face of the cutout portion and an end face of an end of the slit corresponding to the cutout portion are provided flush with each other.
3. 3. The active matrix substrate according to claim 1, the first transparent electrodes are pixel electrodes provided corresponding to the sub-pixels and electrically connected to the thin film transistors; The active matrix substrate, wherein the second transparent electrode is a common electrode provided in common to the plurality of sub-pixels.
4. 3. The active matrix substrate according to claim 1, the first transparent electrode is a common electrode provided in common to the plurality of sub-pixels, the second transparent electrodes are pixel electrodes provided corresponding to the sub-pixels and electrically connected to the thin film transistors,
5. 3. The active matrix substrate according to claim 1, The active matrix substrate, wherein the intermediate layer is formed of a transparent conductive film.
6. 3. The active matrix substrate according to claim 1, The active matrix substrate, wherein the intermediate layer is formed of an inorganic insulating film.
7. An active matrix substrate according to claim 1 or 2; an opposing substrate provided opposite the active matrix substrate; a liquid crystal layer provided between the active matrix substrate and the counter substrate;
8. a thin film transistor forming step of forming a plurality of thin film transistors on a base substrate corresponding to a plurality of sub-pixels; a color filter forming step of forming a color filter on each of the thin film transistors, the color filter having a colored layer of a predetermined color arranged corresponding to each of the sub-pixels; a first transparent electrode forming step of forming a first transparent conductive film on the upper side of the color filter and then patterning the first transparent conductive film to form a first transparent electrode; a reflection-suppressing layer forming step of forming an inorganic insulating film, a first metal film, an intermediate film and a second metal film so as to cover the first transparent electrode, and then patterning the first metal film, the intermediate film and the second metal film to form a first metal layer, an intermediate layer and a second metal layer, respectively, and forming a reflection-suppressing layer in which the first metal layer, the intermediate layer and the second metal layer are laminated in this order in a strip shape so as to overlap a boundary portion of the colored layers of different colors; an inorganic protective film forming step of patterning the inorganic insulating film exposed from the antireflection layer to form an inorganic protective film; a second transparent electrode forming step of forming a second transparent conductive film so as to cover the anti-reflection forming layer on the inorganic protective film, and then patterning the second transparent conductive film to form a second transparent electrode having a strip-shaped slit whose end portion overlaps with the anti-reflection forming layer; A method for manufacturing an active matrix substrate, wherein in the second transparent electrode forming step, the reflection-suppressing layer exposed from the slit is removed to form a reflection-suppressing layer having a cutout portion.
9. 9. The method for manufacturing an active matrix substrate according to claim 8, the first transparent electrodes are pixel electrodes provided corresponding to the sub-pixels and electrically connected to the thin film transistors; a second transparent electrode provided in a common electrode area of the plurality of sub-pixels;
10. 9. The method for manufacturing an active matrix substrate according to claim 8, the first transparent electrode is a common electrode provided in common to the plurality of sub-pixels, the second transparent electrodes are pixel electrodes provided corresponding to the sub-pixels and electrically connected to the thin film transistors,
11. The method for manufacturing an active matrix substrate according to any one of claims 8 to 10, The method for producing an active matrix substrate, wherein the intermediate film is formed of a transparent conductive film.
12. The method for manufacturing an active matrix substrate according to any one of claims 8 to 10, The method for producing an active matrix substrate, wherein the intermediate film is formed of an inorganic insulating film.
13. The method for manufacturing an active matrix substrate according to any one of claims 8 to 10, The method for manufacturing an active matrix substrate, wherein the color filter forming step forms the color filter having contact holes for electrical connection to each of the thin film transistors.
14. The method for manufacturing an active matrix substrate according to claim 13, The method for manufacturing an active matrix substrate, wherein the color filter forming step forms an organic protective film made of an organic insulating film having the contact holes on the color filter.
Citation Information
Patent Citations
Liquid crystal display device
JP2017116821A