Lens part, display body and display method
The lens unit in VR goggles, with a polarizing member and λ/4 members, addresses weight and visibility issues by optimizing optical configurations and adhesive layers, achieving a lightweight and clear display.
Patent Information
- Application Number
- JP2024146098
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-12-28
AI Technical Summary
Existing VR goggles are heavy and hinder visibility due to the use of conventional optical members, necessitating a lightweight and high-visibility solution.
A lens unit comprising a polarizing member, reflective polarizing member, half mirror, and λ/4 members with specific optical configurations and adhesive layers to reduce weight and improve visibility, achieving an ISC value of 100 or less.
The lens unit significantly reduces the weight of VR goggles while enhancing visibility by minimizing diffused light and maintaining image clarity.
Smart Images

Figure 2024161601000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a lens portion, a display, and a display method. [Background technology]
[0002] Image display devices, such as liquid crystal display devices and electroluminescence (EL) display devices (e.g., organic EL display devices), are rapidly becoming widespread. In image display devices, optical members such as polarizing members and phase difference members are generally used to realize image display and to improve the performance of the image display (see, for example, Patent Document 1).
[0003] In recent years, new applications for image display devices have been developed. For example, goggles with displays (VR goggles) for realizing virtual reality (VR) have begun to be commercialized. Since the use of VR goggles in various situations is being considered, there is a demand for them to be lightweight and have improved visibility. Weight reduction can be achieved, for example, by thinning the lenses used in the VR goggles. On the other hand, there is also a demand for the development of optical members suitable for display systems using thin lenses. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2021-103286 A Summary of the Invention [Problem to be solved by the invention]
[0005] In view of the above, a primary object of the present invention is to provide a lens portion that can reduce the weight of VR goggles and improve visibility. [Means for solving the problem]
[0006] 1. A lens unit according to an embodiment of the present invention is a lens unit used in a display system that displays an image to a user, and comprises: a reflective polarizing element that reflects light that is emitted forward from a display surface of a display element that displays an image and has passed through a polarizing element and a first λ / 4 element; a first lens unit arranged on an optical path between the display element and the reflective polarizing element; a half mirror that is arranged between the display element and the first lens unit and transmits the light emitted from the display element and reflects the light reflected by the reflective polarizing element toward the reflective polarizing element; a second lens unit arranged in front of the reflective polarizing element; and a second λ / 4 element arranged on the optical path between the half mirror and the reflective polarizing element, and the ISC value of an assembly formed by arranging three first laminated units each including the second λ / 4 element and at least one adhesive layer is 100 or less. 2. The lens portion according to 1 above may have a second laminated portion including the reflective polarizing member. 3. In the lens portion described in 2 above, the first laminated portion and the second laminated portion may be disposed apart from each other. 4. In the lens portion according to 2 or 3 above, the second stacked portion may include an absorptive polarizing member disposed between the reflective polarizing member and the second lens portion. 5. In the lens portion described in any one of 2 to 4 above, the second stacked portion may include a third λ / 4 member disposed between the reflective polarizing member and the second lens portion. 6. In the lens portion described in any one of 1 to 5 above, the first laminated portion may include a first protective member disposed in front of the second λ / 4 member. 7. In the lens portion according to any one of the above items 1 to 6, the first laminated portion may include three or less pressure-sensitive adhesive layers. 8. In the lens portion according to any one of 1 to 7 above, the thickness of each of the pressure-sensitive adhesive layers included in the first laminate portion may be 20 μm or less. 9. In the lens portion according to any one of the above items 1 to 8, the surface roughness Ra of each of the pressure-sensitive adhesive layers included in the first laminate portion may be 20 nm or less. 10. In the lens portion according to any one of the above items 1 to 9, each of the pressure-sensitive adhesive layers included in the first laminate portion may be a single layer. 11. In the lens portion as described in any one of 1 to 10 above, the first lens portion and the half mirror may be integral with each other. 12. A display according to an embodiment of the present invention has a lens portion as described in any one of 1 to 11 above.
[0007] 13. A display method according to an embodiment of the present invention includes the steps of: passing light representing an image emitted through a polarizing element and a first λ / 4 element through a half mirror and a first lens unit; passing the light that has passed through the half mirror and the first lens unit through a second λ / 4 element; reflecting the light that has passed through the second λ / 4 element toward the half mirror with a reflective polarizing element; making the light reflected by the reflective polarizing element and the half mirror transmittable through the reflective polarizing element by the second λ / 4 element; and passing the light that has transmitted through the reflective polarizing element through a second lens unit, wherein the ISC value of an assembly formed by arranging three first laminate units each including the second λ / 4 element and at least one adhesive layer is 100 or less. Effect of the Invention
[0008] The lens portion according to the embodiment of the present invention can reduce the weight of the VR goggles and improve visibility. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic diagram showing a general configuration of a display system according to an embodiment of the present invention. [Diagram 2] 2 is a schematic cross-sectional view showing an example of details of a lens portion of the display system shown in FIG. 1. [Diagram 3] FIG. 2 is a schematic perspective view showing an example of a multilayer structure included in a reflective polarizing film. [Figure 4] FIG. 1 is a diagram for explaining a method for measuring an ISC value. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the embodiments of the present invention will be described with reference to the drawings, but the present invention is not limited to these embodiments. In addition, in order to clarify the description, the width, thickness, shape, etc. of each part may be shown more diagrammatically than in the embodiment, but these are merely examples and do not limit the interpretation of the present invention.
[0011] (Definition of terms and symbols) The definitions of terms and symbols used in this specification are as follows. (1) Refractive index (nx, ny, nz) "nx" is the refractive index in the direction in which the in-plane refractive index is maximum (i.e., the slow axis direction), "ny" is the refractive index in the direction perpendicular to the slow axis in the plane (i.e., the fast axis direction), and "nz" is the refractive index in the thickness direction. (2) In-plane phase difference (Re) "Re(λ)" is the in-plane retardation measured with light of wavelength λ nm at 23° C. For example, "Re(550)" is the in-plane retardation measured with light of wavelength 550 nm at 23° C. Re(λ) is calculated by the formula: Re(λ)=(nx-ny)×d, where d(nm) is the thickness of the layer (film). (3) Retardation in the thickness direction (Rth) "Rth(λ)" is the retardation in the thickness direction measured with light of wavelength λ nm at 23° C. For example, "Rth(550)" is the retardation in the thickness direction measured with light of wavelength 550 nm at 23° C. Rth(λ) is calculated by the formula: Rth(λ)=(nx-nz)×d, where d(nm) is the thickness of the layer (film). (4) Nz coefficient The Nz coefficient is calculated by Nz=Rth / Re. (5)Angle When angles are referred to herein, the angles include both clockwise and counterclockwise angles relative to a reference direction, so for example, "45°" means ±45°.
[0012] FIG. 1 is a schematic diagram showing a schematic configuration of a display system according to one embodiment of the present invention. In FIG. 1, the arrangement and shape of each component of a display system 2 are illustrated. The display system 2 includes a display element 12, a reflective polarizing member 14, a first lens unit 16, a half mirror 18, a first phase difference member 20, a second phase difference member 22, and a second lens unit 24. The reflective polarizing member 14 is disposed in front of the display surface 12a side of the display element 12, and can reflect light emitted from the display element 12. The first lens unit 16 is disposed on the optical path between the display element 12 and the reflective polarizing member 14, and the half mirror 18 is disposed between the display element 12 and the first lens unit 16. The first phase difference member 20 is disposed on the optical path between the display element 12 and the half mirror 18, and the second phase difference member 22 is disposed on the optical path between the half mirror 18 and the reflective polarizing member 14.
[0013] The components arranged in front of the half mirror (in the illustrated example, the half mirror 18, the first lens section 16, the second phase difference member 22, the reflective polarizing member 14, and the second lens section 24) may be collectively referred to as the lens section (lens section 4).
[0014] The display element 12 is, for example, a liquid crystal display or an organic EL display, and has a display surface 12a for displaying an image. The light emitted from the display surface 12a passes through, for example, a polarizing member (typically, a polarizing film) that may be included in the display element 12, and is converted into a first linearly polarized light.
[0015] The first phase difference member 20 includes a first λ / 4 member that can convert a first linearly polarized light incident on the first phase difference member 20 into a first circularly polarized light. When the first phase difference member does not include a member other than the first λ / 4 member, the first phase difference member may correspond to the first λ / 4 member. The first phase difference member 20 may be provided integrally with the display element 12.
[0016] The half mirror 18 transmits the light emitted from the display element 12 and reflects the light reflected by the reflective polarizing member 14 toward the reflective polarizing member 14. The half mirror 18 is provided integrally with the first lens portion 16.
[0017] The second phase difference member 22 includes a second λ / 4 member that can transmit light reflected by the reflective polarizing member 14 and the half mirror 18 through the reflective polarizing member 14. When the second phase difference member does not include any member other than the second λ / 4 member, the second phase difference member may correspond to the second λ / 4 member. The second phase difference member 22 may be provided integrally with the first lens portion 16.
[0018] The first circularly polarized light output from the first λ / 4 member included in the first phase difference member 20 passes through the half mirror 18 and the first lens unit 16, and is converted into the second linearly polarized light by the second λ / 4 member included in the second phase difference member 22. The second linearly polarized light output from the second λ / 4 member is reflected toward the half mirror 18 without passing through the reflective polarizing member 14. At this time, the polarization direction of the second linearly polarized light incident on the reflective polarizing member 14 is the same as the reflection axis of the reflective polarizing member 14. Therefore, the second linearly polarized light incident on the reflective polarizing member 14 is reflected by the reflective polarizing member 14.
[0019] The second linearly polarized light reflected by the reflective polarizing member 14 is converted into the second circularly polarized light by the second λ / 4 member included in the second phase difference member 22, and the second circularly polarized light output from the second λ / 4 member passes through the first lens unit 16 and is reflected by the half mirror 18. The second circularly polarized light reflected by the half mirror 18 passes through the first lens unit 16 and is converted into the third linearly polarized light by the second λ / 4 member included in the second phase difference member 22. The third linearly polarized light passes through the reflective polarizing member 14. At this time, the polarization direction of the third linearly polarized light incident on the reflective polarizing member 14 is the same as the transmission axis of the reflective polarizing member 14. Therefore, the third linearly polarized light incident on the reflective polarizing member 14 passes through the reflective polarizing member 14.
[0020] The light transmitted through the reflective polarizing member 14 passes through the second lens portion 24 and enters the eye 26 of the user.
[0021] For example, the absorption axis of the polarizing member included in the display element 12 and the reflection axis of the reflective polarizing member 14 may be disposed approximately parallel to each other or approximately perpendicular to each other. The angle between the absorption axis of the polarizing member included in the display element 12 and the slow axis of the first λ / 4 member included in the first phase difference member 20 is, for example, 40° to 50°, may be 42° to 48°, or may be about 45°. The angle between the absorption axis of the polarizing member included in the display element 12 and the slow axis of the second λ / 4 member included in the second phase difference member 22 is, for example, 40° to 50°, may be 42° to 48°, or may be about 45°.
[0022] The in-plane retardation Re(550) of the first λ / 4 member is, for example, 100 nm to 190 nm, and may be 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The first λ / 4 member preferably exhibits an inverse dispersion wavelength characteristic in which the retardation value increases according to the wavelength of the measurement light. The Re(450) / Re(550) of the first λ / 4 member may be, for example, 0.75 or more and less than 1, or 0.8 or more and 0.95 or less.
[0023] The in-plane retardation Re(550) of the second λ / 4 member is, for example, 100 nm to 190 nm, and may be 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The second λ / 4 member preferably exhibits an inverse dispersion wavelength characteristic in which the retardation value increases according to the wavelength of the measurement light. The Re(450) / Re(550) of the second λ / 4 member may be, for example, 0.75 or more and less than 1, or 0.8 or more and 0.95 or less.
[0024] In the lens portion 4, a space may be formed between the first lens portion 16 and the second lens portion 24. In this case, it is preferable that the member disposed between the first lens portion 16 and the second lens portion 24 is integrally provided with either the first lens portion 16 or the second lens portion 24. For example, it is preferable that the member disposed between the first lens portion 16 and the second lens portion 24 is integrated with either the first lens portion 16 or the second lens portion 24 via an adhesive layer. According to such a form, for example, the handling of each member may be excellent. The adhesive layer may be formed of an adhesive or a pressure-sensitive adhesive. Specifically, the adhesive layer may be an adhesive layer or a pressure-sensitive adhesive layer. The thickness of the adhesive layer is, for example, 0.05 μm to 30 μm.
[0025] Fig. 2 is a schematic cross-sectional view showing an example of the details of the lens unit of the display system shown in Fig. 1. Specifically, Fig. 2 shows a first lens unit, a second lens unit, and members disposed between them. The lens unit 4 includes a first lens unit 16, a first stack unit 100 provided adjacent to the first lens unit 16, a second lens unit 24, and a second stack unit 200 provided adjacent to the second lens unit 24. In the example shown in Fig. 2, the first stack unit 100 and the second stack unit 200 are disposed apart from each other. Although not shown, a half mirror may be provided integrally with the first lens unit 16.
[0026] The first laminated unit 100 includes a second phase difference member 22 and a pressure-sensitive adhesive layer 41 disposed between the first lens unit 16 and the second phase difference member 22, and is integrally provided with the first lens unit 16 by the pressure-sensitive adhesive layer 41. The first laminated unit 100 further includes a first protective member 31 disposed in front of the second phase difference member 22. The first protective member 31 is laminated on the second phase difference member 22 via the pressure-sensitive adhesive layer 42. The first protective member 31 can be located on the outermost surface of the first laminated unit 100.
[0027] In the example shown in Fig. 2, the second retardation member 22 includes, in addition to the second λ / 4 member 22a, a member (so-called positive C-plate) 22b that can exhibit a refractive index characteristic of nz > nx = ny. The second retardation member 22 has a laminated structure of the second λ / 4 member 22a and the positive C-plate 22b. As shown in Fig. 2, in the second retardation member 22, it is preferable that the second λ / 4 member 22a is positioned more forward than the positive C-plate 22b. The second λ / 4 member 22a and the positive C-plate 22b are laminated via, for example, an adhesive layer (not shown).
[0028] The above second λ / 4 member preferably exhibits a refractive index characteristic of nx > ny ≥ nz. Here, "ny = nz" includes not only the case where ny and nz are exactly equal but also the case where they are substantially equal. Therefore, within a range that does not impair the effects of the present invention, ny < nz may occur. The Nz coefficient of the second λ / 4 member is preferably 0.9 to 3, more preferably 0.9 to 2.5, still more preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0029] The second λ / 4 member is formed of any suitable material that can satisfy the above characteristics. The second λ / 4 member can be, for example, a stretched film of a resin film or an alignment cured layer of a liquid crystal compound.
[0030] Examples of the resin contained in the resin film include polycarbonate resins, polyester carbonate resins, polyester resins, polyvinyl acetal resins, polyarylate resins, cyclic olefin resins, cellulose resins, polyvinyl alcohol resins, polyamide resins, polyimide resins, polyether resins, polystyrene resins, acrylic resins, etc. These resins may be used alone or in combination. Examples of the combination methods include blending and copolymerization. When the second λ / 4 member exhibits reverse dispersion wavelength characteristics, a resin film containing a polycarbonate resin or a polyester carbonate resin (hereinafter sometimes simply referred to as a polycarbonate resin) can be preferably used.
[0031] Any suitable polycarbonate-based resin can be used as the polycarbonate-based resin. For example, the polycarbonate-based resin contains a structural unit derived from a fluorene-based dihydroxy compound, a structural unit derived from an isosorbide-based dihydroxy compound, and a structural unit derived from at least one dihydroxy compound selected from the group consisting of alicyclic diol, alicyclic dimethanol, di-, tri- or polyethylene glycol, and alkylene glycol or spiro glycol. Preferably, the polycarbonate-based resin contains a structural unit derived from a fluorene-based dihydroxy compound, a structural unit derived from an isosorbide-based dihydroxy compound, a structural unit derived from an alicyclic dimethanol and / or a structural unit derived from a di-, tri- or polyethylene glycol; more preferably, it contains a structural unit derived from a fluorene-based dihydroxy compound, a structural unit derived from an isosorbide-based dihydroxy compound, and a structural unit derived from a di-, tri- or polyethylene glycol. The polycarbonate-based resin may contain a structural unit derived from another dihydroxy compound as necessary. Details of polycarbonate-based resins that can be suitably used for the second λ / 4 member and methods for forming the second λ / 4 member are described, for example, in JP 2014-10291 A, JP 2014-26266 A, JP 2015-212816 A, JP 2015-212817 A, and JP 2015-212818 A, and the descriptions in these publications are incorporated herein by reference.
[0032] The thickness of the second λ / 4 member made of a stretched resin film is, for example, 10 μm to 100 μm, preferably 10 μm to 70 μm, and more preferably 20 μm to 60 μm.
[0033] The above-mentioned liquid crystal compound alignment solidified layer is a layer in which the liquid crystal compound is aligned in a predetermined direction within the layer, and the alignment state is fixed. The "alignment solidified layer" is a concept that includes an alignment solidified layer obtained by hardening a liquid crystal monomer as described later. In the second λ / 4 member, typically, rod-shaped liquid crystal compounds are aligned in the slow axis direction of the second λ / 4 member (homogeneous alignment). Examples of rod-shaped liquid crystal compounds include liquid crystal polymers and liquid crystal monomers. The liquid crystal compound is preferably polymerizable. If the liquid crystal compound is polymerizable, the alignment state of the liquid crystal compound can be fixed by aligning the liquid crystal compound and then polymerizing it.
[0034] The alignment solidified layer of the liquid crystal compound (liquid crystal alignment solidified layer) can be formed by performing an alignment treatment on the surface of a predetermined substrate, applying a coating liquid containing a liquid crystal compound to the surface to align the liquid crystal compound in a direction corresponding to the alignment treatment, and fixing the alignment state. Any appropriate alignment treatment can be adopted as the alignment treatment. Specifically, mechanical alignment treatment, physical alignment treatment, and chemical alignment treatment can be mentioned. Specific examples of mechanical alignment treatment include rubbing treatment and stretching treatment. Specific examples of physical alignment treatment include magnetic field alignment treatment and electric field alignment treatment. Specific examples of chemical alignment treatment include oblique deposition method and photoalignment treatment. As the treatment conditions of various alignment treatments, any appropriate conditions can be adopted depending on the purpose.
[0035] The alignment of the liquid crystal compound is performed by treating the liquid crystal compound at a temperature at which the liquid crystal compound exhibits a liquid crystal phase according to the type of liquid crystal compound. By performing such temperature treatment, the liquid crystal compound takes on a liquid crystal state and is aligned according to the alignment treatment direction of the substrate surface.
[0036] In one embodiment, the alignment state is fixed by cooling the liquid crystal compound aligned as described above. When the liquid crystal compound is polymerizable or crosslinkable, the alignment state is fixed by subjecting the liquid crystal compound aligned as described above to a polymerization treatment or crosslinking treatment.
[0037] As the liquid crystal compound, any suitable liquid crystal polymer and / or liquid crystal monomer is used. The liquid crystal polymer and the liquid crystal monomer may be used alone or in combination. Specific examples of the liquid crystal compound and the method for producing the liquid crystal alignment solidified layer are described in, for example, JP 2006-163343 A, JP 2006-178389 A, and WO 2018 / 123551 A. The descriptions in these publications are incorporated herein by reference.
[0038] The thickness of the second λ / 4 member constituted by the liquid crystal alignment solidified layer is, for example, 1 μm to 10 μm, preferably 1 μm to 8 μm, more preferably 1 μm to 6 μm, and further preferably 1 μm to 4 μm.
[0039] The thickness direction retardation Rth(550) of the positive C plate is preferably -50nm to -300nm, more preferably -70nm to -250nm, further preferably -90nm to -200nm, and particularly preferably -100nm to -180nm. Here, "nx=ny" includes not only the case where nx and ny are strictly equal, but also the case where nx and ny are substantially equal. The in-plane retardation Re(550) of the positive C plate is, for example, less than 10nm.
[0040] The positive C plate may be formed of any suitable material, but is preferably composed of a film containing a liquid crystal material fixed in homeotropic alignment. The liquid crystal material (liquid crystal compound) that can be homeotropically aligned may be a liquid crystal monomer or a liquid crystal polymer. Specific examples of such liquid crystal compounds and methods for forming a positive C plate include the liquid crystal compounds and methods for forming the retardation layer described in
[0020] to
[0028] of JP-A-2002-333642. In this case, the thickness of the positive C plate is preferably 0.5 μm to 5 μm.
[0041] The first protective member typically includes a substrate. The thickness of the substrate is preferably 5 μm to 80 μm, more preferably 10 μm to 50 μm, and further preferably 15 μm to 40 μm. The substrate may be made of any appropriate film. Examples of materials that are the main components of the film constituting the substrate include cellulose-based resins such as triacetyl cellulose (TAC), polyester-based, polyvinyl alcohol-based, polycarbonate-based, polyamide-based, polyimide-based, polyethersulfone-based, polysulfone-based, polystyrene-based, cycloolefin-based such as polynorbornene, polyolefin-based, (meth)acrylic, acetate-based, and other resins. Here, (meth)acrylic refers to acrylic and / or methacrylic. In one embodiment, the substrate is preferably made of a (meth)acrylic resin. By using a (meth)acrylic resin, a substrate having excellent smoothness can be formed by extrusion molding. Then, a protective member having excellent smoothness can be obtained.
[0042] The first protective member preferably has a substrate and a surface treatment layer formed on the substrate. The first protective member having the surface treatment layer may be disposed so that the surface treatment layer is located on the front side. Specifically, the surface treatment layer may be located on the outermost surface of the first laminated portion. The surface treatment layer may have any appropriate function. For example, from the viewpoint of improving visibility, the surface treatment layer preferably has an anti-reflection function. The thickness of the surface treatment layer is preferably 0.5 μm to 10 μm, more preferably 1 μm to 7 μm, and further preferably 2 μm to 5 μm.
[0043] The second laminated section 200 includes a reflective polarizing member 14 and an adhesive layer disposed between the reflective polarizing member 14 and the second lens section 24. For example, from the viewpoint of improving visibility, the second laminated section 200 further includes an absorbing polarizing member 28 disposed between the reflective polarizing member 14 and the second lens section 24. The absorbing polarizing member 28 is laminated in front of the reflective polarizing member 14 via an adhesive layer 44. The reflection axis of the reflective polarizing member 14 and the absorption axis of the absorbing polarizing member 28 can be disposed approximately parallel to each other, and the transmission axis of the reflective polarizing member 14 and the transmission axis of the absorbing polarizing member 28 can be disposed approximately parallel to each other. By laminating them via an adhesive layer, the reflective polarizing member 14 and the absorbing polarizing member 28 are fixed, and it is possible to prevent the axial arrangement of the reflection axis and the absorption axis (the transmission axis and the transmission axis) from being misaligned. In addition, it is possible to suppress the adverse effects of an air layer that may be formed between the reflective polarizing member 14 and the absorbing polarizing member 28.
[0044] The second laminated section 200 further includes a second protective member 32 disposed behind the reflective polarizing member 14. The second protective member 32 is laminated to the reflective polarizing member 14 via an adhesive layer 43. The second protective member 32 may be located on the outermost surface of the second laminated section 200. The second protective member may include a substrate, similar to the first protective member. The second protective member preferably includes a substrate and a surface treatment layer formed on the substrate. In this case, the surface treatment layer may be located on the outermost surface of the second laminated section. For details of the substrate and the surface treatment layer, the same explanation as for the first protective member can be applied.
[0045] As shown in FIG. 2, the second laminated section 200 may further include a third phase difference member 30 disposed between the absorptive polarizing member 28 and the second lens section 24. The third phase difference member 30 is laminated to the absorptive polarizing member 28 via an adhesive layer 45. The third phase difference member 30 is laminated to the second lens section 24 via an adhesive layer 46, and the second laminated section 200 is provided integrally with the second lens section 24. The third phase difference member 30 includes, for example, a third λ / 4 member. The angle between the absorption axis of the absorptive polarizing member 28 and the slow axis of the third λ / 4 member included in the third phase difference member 30 is, for example, 40° to 50°, may be 42° to 48°, or may be about 45°. By providing such a member, for example, reflection of external light from the second lens section 16 side can be prevented. When the third phase difference member does not include a member other than the third λ / 4 member, the third phase difference member may correspond to the third λ / 4 member.
[0046] The reflective polarizing element transmits polarized light (typically, linearly polarized light) parallel to its transmission axis while maintaining its polarization state, and can reflect light in other polarization states. The reflective polarizing element is typically composed of a film having a multilayer structure (sometimes referred to as a reflective polarizing film). In this case, the thickness of the reflective polarizing element is, for example, 10 μm to 150 μm, preferably 20 μm to 100 μm, and more preferably 30 μm to 60 μm.
[0047] FIG. 3 is a schematic perspective view showing an example of a multilayer structure included in a reflective polarizing film. The multilayer structure 14a has a layer A having birefringence and a layer B having substantially no birefringence alternately. The total number of layers constituting the multilayer structure may be 50 to 1000. For example, the refractive index nx in the x-axis direction of the A layer is larger than the refractive index ny in the y-axis direction, the refractive index nx in the x-axis direction of the B layer is substantially the same as the refractive index ny in the y-axis direction, and the refractive index difference between the A layer and the B layer is large in the x-axis direction and substantially zero in the y-axis direction. As a result, the x-axis direction can be the reflection axis, and the y-axis direction can be the transmission axis. The refractive index difference between the A layer and the B layer in the x-axis direction is preferably 0.2 to 0.3.
[0048] The A layer is typically made of a material that develops birefringence through stretching. Examples of such materials include naphthalene dicarboxylic acid polyesters (e.g., polyethylene naphthalate), polycarbonates, and acrylic resins (e.g., polymethyl methacrylate). The B layer is typically made of a material that does not substantially develop birefringence even when stretched. Examples of such materials include copolyesters of naphthalene dicarboxylic acid and terephthalic acid. The multilayer structure can be formed by combining coextrusion and stretching. For example, the material constituting the A layer and the material constituting the B layer are extruded, and then multilayered (e.g., using a multiplier). The resulting multilayer laminate is then stretched. The x-axis direction in the illustrated example can correspond to the stretching direction.
[0049] Commercially available reflective polarizing films include, for example, products manufactured by 3M under the trade names "DBEF" and "APF" and products manufactured by Nitto Denko Corporation under the trade name "APCF."
[0050] The crossed transmittance (Tc) of the reflective polarizing member (reflective polarizing film) may be, for example, 0.01% to 3%. The single transmittance (Ts) of the reflective polarizing member (reflective polarizing film) may be, for example, 43% to 49%, and preferably 45% to 47%. The degree of polarization (P) of the reflective polarizing member (reflective polarizing film) may be, for example, 92% to 99.99%.
[0051] The crossed transmittance, single transmittance and degree of polarization can be measured, for example, using an ultraviolet-visible spectrophotometer. The degree of polarization P can be calculated from the obtained Tp and Tc by measuring the single transmittance Ts, parallel transmittance Tp and crossed transmittance Tc using an ultraviolet-visible spectrophotometer, using the following formula. Note that Ts, Tp and Tc are Y values measured using a 2-degree visual field (C light source) according to JIS Z 8701 and corrected for visibility. Polarization degree P(%)={(Tp-Tc) / (Tp+Tc)} 1 / 2 ×100
[0052] The absorptive polarizing member may typically include a resin film (sometimes referred to as an absorptive polarizing film) containing a dichroic material. The thickness of the absorptive polarizing film is, for example, 1 μm or more and 20 μm or less, and may be 2 μm or more and 15 μm or less, 12 μm or less, 10 μm or less, 8 μm or less, or 5 μm or less.
[0053] The absorptive polarizing film may be prepared from a single layer of resin film, or may be prepared using a laminate of two or more layers.
[0054] When preparing from a single-layer resin film, for example, an absorptive polarizing film can be obtained by subjecting a hydrophilic polymer film such as a polyvinyl alcohol (PVA)-based film, a partially formalized PVA-based film, or an ethylene-vinyl acetate copolymer-based partially saponified film to a dyeing treatment with a dichroic substance such as iodine or a dichroic dye, a stretching treatment, etc. Among them, an absorptive polarizing film obtained by dyeing a PVA-based film with iodine and uniaxially stretching it is preferable.
[0055] The dyeing with iodine is carried out, for example, by immersing the PVA film in an aqueous iodine solution. The stretching ratio of the uniaxial stretching is preferably 3 to 7 times. The stretching may be carried out after the dyeing treatment or while the dyeing is being carried out. Alternatively, the stretching may be followed by dyeing. If necessary, the PVA film is subjected to a swelling treatment, a crosslinking treatment, a washing treatment, a drying treatment, or the like.
[0056] Examples of the laminate produced using the laminate of two or more layers include a laminate of a resin substrate and a PVA-based resin layer (PVA-based resin film) laminated on the resin substrate, or a laminate of a resin substrate and a PVA-based resin layer formed by coating on the resin substrate. The absorptive polarizing film obtained using a laminate of a resin substrate and a PVA-based resin layer formed by coating on the resin substrate can be produced, for example, by coating a PVA-based resin solution on the resin substrate and drying the resin substrate to form a PVA-based resin layer on the resin substrate to obtain a laminate of the resin substrate and the PVA-based resin layer; and stretching and dyeing the laminate to make the PVA-based resin layer into an absorptive polarizing film. In this embodiment, preferably, a polyvinyl alcohol-based resin layer containing a halide and a polyvinyl alcohol-based resin is formed on one side of the resin substrate. The stretching typically includes immersing the laminate in an aqueous boric acid solution to stretch it. Furthermore, the stretching may further include, as necessary, stretching the laminate in air at a high temperature (for example, 95° C. or higher) before stretching in the aqueous boric acid solution. In addition, in this embodiment, the laminate is preferably subjected to a drying shrinkage treatment in which the laminate is heated while being transported in the longitudinal direction, thereby shrinking the laminate by 2% or more in the width direction. Typically, the manufacturing method of this embodiment includes subjecting the laminate to an air-assisted stretching treatment, a dyeing treatment, an underwater stretching treatment, and a drying shrinkage treatment in this order. By introducing the auxiliary stretching, even when PVA is applied onto a thermoplastic resin, it is possible to increase the crystallinity of PVA, and to achieve high optical properties. At the same time, by increasing the orientation of PVA in advance, problems such as a decrease in the orientation or dissolution of PVA when immersed in water in the subsequent dyeing and stretching steps can be prevented, and high optical properties can be achieved. Furthermore, when the PVA-based resin layer is immersed in a liquid, the disorder of the orientation of polyvinyl alcohol molecules and the decrease in the orientation can be suppressed compared to when the PVA-based resin layer does not contain a halide. This can improve the optical properties of the absorptive polarizing film obtained through treatment steps in which the laminate is immersed in a liquid, such as a dyeing treatment and an underwater stretching treatment. Furthermore, the optical properties can be improved by shrinking the laminate in the width direction through drying shrinkage treatment.The obtained laminate of resin substrate / absorptive polarizing film may be used as it is (i.e., the resin substrate may be used as a protective layer for the absorptive polarizing film), or any suitable protective layer may be laminated on the peeled surface of the resin substrate / absorptive polarizing film laminate after peeling the resin substrate from the laminate, or on the surface opposite to the peeled surface, depending on the purpose. Details of the method for producing such an absorptive polarizing film are described in, for example, JP2012-73580A and JP6470455A. The entire disclosures of these publications are incorporated herein by reference.
[0057] The crossed transmittance (Tc) of the absorptive polarizing member (absorptive polarizing film) is preferably 0.5% or less, more preferably 0.1% or less, and even more preferably 0.05% or less. The single transmittance (Ts) of the absorptive polarizing member (absorptive polarizing film) is, for example, 41.0% to 45.0%, and preferably 42.0% or more. The polarization degree (P) of the absorptive polarizing member (absorptive polarizing film) is, for example, 99.0% to 99.997%, and preferably 99.9% or more.
[0058] The in-plane retardation Re(550) of the third λ / 4 member is, for example, 100 nm to 190 nm, and may be 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The third λ / 4 member preferably exhibits an inverse dispersion wavelength characteristic in which the retardation value increases according to the wavelength of the measurement light. The third λ / 4 member may have Re(450) / Re(550) of, for example, 0.75 or more and less than 1, or 0.8 or more and 0.95 or less. The third λ / 4 member preferably has a refractive index characteristic that satisfies the relationship nx>ny≧nz. The Nz coefficient of the third λ / 4 member is preferably 0.9 to 3, more preferably 0.9 to 2.5, even more preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0059] The third λ / 4 member is formed of any appropriate material that can satisfy the above characteristics. The third λ / 4 member can be, for example, a stretched resin film or an oriented and solidified layer of a liquid crystal compound. The same explanation as for the second λ / 4 member can be applied to the third λ / 4 member composed of a stretched resin film or an oriented and solidified layer of a liquid crystal compound. The second λ / 4 member and the third λ / 4 member may be members having the same configuration (e.g., forming material, thickness, optical properties, etc.) or may be members having different configurations.
[0060] In the lens unit 4, the ISC value of an assembly formed by arranging three first laminates from a member located in front of the first lens unit 16 to a member located behind the reflective polarizing member 14 is 100 or less, preferably 90 or less, more preferably 80 or less, and even more preferably 70 or less. By satisfying such an ISC value, a display system with extremely excellent visibility can be realized. Specifically, by satisfying such an ISC value, it is possible to suppress the generation of diffused light in the lens unit and suppress the image from becoming unclear. The ISC value can be an index of smoothness or unevenness. In addition, the ISC value of an assembly in which three first laminates are arranged can be an index of the visibility of the entire display system. Since light can pass through the first laminate three times in the display system, the first laminate can be greatly involved in the visibility of the display system. In the example shown in FIG. 2, for example, from the viewpoint of convenience of evaluation, the first laminate 100 includes a member located behind the space formed between the first lens unit 16 and the reflective polarizing member 14. Specifically, the first laminate unit 100 includes an adhesive layer 41, a second retardation member 22 including a second λ / 4 member 22a, an adhesive layer 42, and a first protective member 31. In practice, the lower limit of the ISC value of an assembly formed by arranging three first laminate units is about 5.
[0061] In the example shown in FIG. 2, six pressure-sensitive adhesive layers 41 to 46 are used to integrally provide each member disposed between the first lens portion 16 and the second lens portion 24 with the first lens portion 16 or the second lens portion 24. In the example shown in FIG. 2, the first laminated portion 100 includes two pressure-sensitive adhesive layers. For example, the number of pressure-sensitive adhesive layers included in the first laminated portion 100 varies depending on the number of members disposed between the first lens portion 16 and the reflective polarizing member 14. The first laminated portion includes preferably three or less pressure-sensitive adhesive layers, more preferably two or less pressure-sensitive adhesive layers. According to this embodiment, the first laminated portion can achieve the above ISC value satisfactorily.
[0062] The thickness of the adhesive layer used for laminating each of the above members can be set to any appropriate thickness. The thickness of each of the adhesive layers used for laminating each of the above members is preferably 20 μm or less, may be 15 μm or less, may be 10 μm or less, or may be 7 μm or less. With such a thickness, the degree of unevenness of the adhesive layer surface can be suppressed, and the ISC value can be satisfactorily achieved in the first lamination part. On the other hand, the thickness of the adhesive layer is, for example, 3 μm or more.
[0063] The surface roughness Ra of each of the pressure-sensitive adhesive layers used for laminating the above-mentioned members is preferably 20 nm or less, more preferably 15 nm or less. With such a thickness, the above-mentioned ISC value can be satisfactorily achieved in the first laminated portion.
[0064] The adhesive layer may be made of any suitable adhesive. Specific examples include acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives. By adjusting the type, number, combination, and compounding ratio of the monomers forming the base resin of the adhesive, as well as the compounding amount of the crosslinking agent, reaction temperature, reaction time, etc., an adhesive having desired properties according to the purpose can be prepared. The base resin of the adhesive may be used alone or in combination of two or more. An acrylic resin is preferably used as the base resin. Specifically, the adhesive layer is preferably made of an acrylic adhesive.
[0065] For example, the pressure-sensitive adhesive layer can be formed by coating and drying a pressure-sensitive adhesive composition containing a base resin, additives such as a crosslinking agent, and a solvent. The pressure-sensitive adhesive composition may be directly coated on the adherend, or may be coated on a substrate such as a separately prepared base film. Drying is typically performed by heating.
[0066] For example, the surface roughness Ra can be satisfied by adjusting the thickness of the coating film of the pressure-sensitive adhesive composition. If the film thickness is too thick, liquid flow due to temperature difference may occur in the coating film upon heating, and a pressure-sensitive adhesive layer with a large degree of surface unevenness may be formed.
[0067] For example, the surface roughness Ra can be satisfied by controlling the drying conditions of the coating film of the pressure-sensitive adhesive composition. Specifically, the surface roughness Ra can be satisfied by adjusting the volume and speed of the air blown onto the coating film during drying. If the volume and speed of the air blown onto the coating film are too large, waves may occur in the coating film, and a pressure-sensitive adhesive layer with a large degree of surface unevenness may be formed. In one embodiment, the coating film is preferably dried in a temperature environment of 65°C to 110°C with an air speed adjusted to within a range of 2m / min to 15m / min, and more preferably adjusted to 2m / min to 8m / min. For example, it is preferable that the temperature and air speed are adjusted to such values near the entrance of the oven in which drying is performed after coating. Specifically, the temperature and air speed can be adjusted to such values from the entrance of the oven to the center of the oven.
[0068] The pressure-sensitive adhesive layers used for laminating the above-mentioned members are preferably each composed of a single layer. For example, it is preferable that each pressure-sensitive adhesive layer does not have a multi-layer structure formed by applying the pressure-sensitive adhesive composition two or more times. By making the pressure-sensitive adhesive layer a single layer, for example, the above-mentioned surface roughness Ra can be satisfied. EXAMPLES
[0069] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples. The thickness, surface roughness Ra, and retardation value are values measured by the following measuring methods. <Thickness> The thickness of 10 μm or less was measured using a scanning electron microscope (manufactured by JEOL, product name "JSM-7100F"), and the thickness of more than 10 μm was measured using a digital micrometer (manufactured by Anritsu, product name "KC-351C"). <Surface roughness Ra> The arithmetic mean surface roughness Ra (μm) was measured according to JIS B 0601 (1994 edition). The adhesive layer to be measured was attached to a glass plate (MICRO SLIDE GLASS, manufactured by MATSUNAMI, product number S, thickness 1.3 mm, 45 mm x 50 mm) to prepare a measurement sample. The adhesive layer was attached by transferring the adhesive layer formed on the substrate film from the substrate film to the glass plate. The obtained measurement sample was measured using a scanning white light interferometer (manufactured by Zygo, product name "Newview7300"). Specifically, the measurement sample was placed on a measurement table with a vibration-proof table, interference fringes were generated using a single white LED light, and an interference objective lens (2.5x) with a reference surface was scanned in the Z direction (thickness direction) to selectively obtain the smoothness (surface smoothness) of the outermost surface of the adhesive layer in a 2 mm square field of view. Based on this measurement, the arithmetic average surface roughness Ra was calculated. <Phase difference value> The phase difference value at each wavelength at 23°C was measured using a Mueller matrix polarimeter (Axometrics, product name "Axoscan").
[0070] [Example 1] (Formation of adhesive layer) A monomer mixture containing 92 parts by weight of butyl acrylate, 2.9 parts by weight of acrylic acid, 0.1 parts by weight of 2-hydroxyethyl acrylate, and 5 parts by weight of N-acryloylmorpholine was charged into a four-neck flask equipped with a stirring blade, a thermometer, a nitrogen gas inlet tube, and a condenser. Furthermore, 0.1 parts by weight of 2,2'-azobisisobutyronitrile as a polymerization initiator was charged together with 200 parts by weight of ethyl acetate per 100 parts by weight of this monomer mixture, and nitrogen gas was introduced while gently stirring to replace the atmosphere in the flask with nitrogen. The liquid temperature in the flask was kept at around 55°C, and a polymerization reaction was carried out for 8 hours to prepare a solution of an acrylic polymer with a weight average molecular weight (Mw) of 1.78 million. The acrylic polymer solution was applied to the substrate film, and the resulting coating film on the substrate film was dried in an oven to form an adhesive layer having a thickness of 5 μm and a surface roughness Ra of 12 nm. The drying was performed by adjusting the air speed in the oven from the oven entrance to the center of the oven to a range of 15 m / min or less. The air speed was measured by an anemometer installed in the oven.
[0071] (Fabrication of λ / 4 components) Polymerization was carried out using a batch polymerization apparatus consisting of two vertical reactors equipped with stirring blades and a reflux condenser controlled at 100° C. Bis[9-(2-phenoxycarbonylethyl)fluoren-9-yl]methane 29.60 parts by mass (0.046 mol), isosorbide (ISB) 29.21 parts by mass (0.200 mol), spiroglycol (SPG) 42.28 parts by mass (0.139 mol), diphenyl carbonate (DPC) 63.77 parts by mass (0.298 mol), and calcium acetate monohydrate 1.19×10 as a catalyst. -2 Part of mass (6.78×10 -5 mol) was charged. After the inside of the reactor was purged with nitrogen under reduced pressure, heating was performed with a heat medium, and stirring was started when the inside temperature reached 100 ° C. 40 minutes after the start of the temperature increase, the inside temperature was reached 220 ° C., and while controlling to maintain this temperature, the pressure was reduced and 90 minutes after reaching 220 ° C., the pressure was reduced to 13.3 kPa. Phenol vapor by-produced with the polymerization reaction was led to a reflux condenser at 100 ° C., a small amount of monomer components contained in the phenol vapor were returned to the reactor, and the uncondensed phenol vapor was led to a condenser at 45 ° C. and recovered. Nitrogen was introduced into the first reactor to restore the pressure to atmospheric pressure, and the oligomerized reaction liquid in the first reactor was transferred to the second reactor. Next, the temperature increase and pressure reduction in the second reactor were started, and the inside temperature was set to 240 ° C. and the pressure to 0.2 kPa in 50 minutes. Thereafter, polymerization was allowed to proceed until the specified stirring power was reached. When the predetermined power was reached, nitrogen was introduced into the reactor to restore pressure, and the produced polyester carbonate resin was extruded into water and the strands were cut to obtain pellets.
[0072] The obtained polyester carbonate resin (pellets) was vacuum-dried at 80°C for 5 hours, and then a long resin film having a thickness of 135μm was produced using a film-forming device equipped with a single-screw extruder (manufactured by Toshiba Machine Co., Ltd., cylinder setting temperature: 250°C), a T-die (width 200mm, setting temperature: 250°C), a chill roll (setting temperature: 120-130°C) and a winder. The obtained long resin film was stretched in the width direction at a stretching temperature of 143°C and a stretching ratio of 2.8 times to obtain a stretched film having a thickness of 47μm. The Re(550) of the obtained stretched film was 143nm, Re(450) / Re(550) was 0.86, and the Nz coefficient was 1.2.
[0073] (Positive C-plate formation) A liquid crystal coating solution was prepared by dissolving 20 parts by weight of a side-chain liquid crystal polymer represented by the following chemical formula (1) (the numbers 65 and 35 in the formula indicate the mole percent of the monomer unit, and are conveniently represented as a block polymer: weight average molecular weight 5000), 80 parts by weight of a polymerizable liquid crystal exhibiting a nematic liquid crystal phase (manufactured by BASF: trade name Paliocolor LC242), and 5 parts by weight of a photopolymerization initiator (manufactured by Ciba Specialty Chemicals: trade name Irgacure 907) in 200 parts by weight of cyclopentanone. The coating solution was then applied to a PET substrate that had been subjected to a vertical alignment treatment using a bar coater, and the liquid crystal was aligned by heating and drying at 80°C for 4 minutes. The liquid crystal layer was irradiated with ultraviolet light to harden the liquid crystal layer, thereby forming a positive C plate with a thickness of 4 μm and an Rth(550) of -100 nm on the substrate. [ka]
[0074] (Creating protective materials) The following hard coat layer forming material was applied to an acrylic film (thickness 40 μm) having a lactone ring structure and heated at 90° C. for 1 minute. After heating, the coating layer was irradiated with a high-pressure mercury lamp with an integrated light intensity of 300 mJ / cm. 2 The coating layer was cured by irradiation with ultraviolet light of 1000 .mu.m to prepare an acrylic film (thickness 44 .mu.m) on which a hard coat layer with a thickness of 4 .mu.m was formed. Next, the following coating solution A for forming an anti-reflection layer was applied onto the hard coat layer using a wire bar, and the applied coating solution was heated at 80°C for 1 minute and dried to form a coating film. The dried coating film was then irradiated with a high-pressure mercury lamp with an integrated light quantity of 300 mJ / cm2. 2 The coating was cured by irradiation with ultraviolet light of 1500 nm to form an antireflection layer A having a thickness of 140 nm. Next, the following coating solution B for forming an antireflection layer was applied onto the antireflection layer A using a wire bar, and the applied coating solution was heated at 80°C for 1 minute and dried to form a coating film. The dried coating film was irradiated with a high-pressure mercury lamp with an integrated light amount of 300 mJ / cm 2 The coating was cured by irradiation with ultraviolet light of 1000 ohms to form an antireflection layer B having a thickness of 105 nm. In this way, a protective member (thickness: 44 μm) was obtained.
[0075] (Hard Coat Layer Forming Material) A hard coat layer forming material was prepared by mixing 50 parts of a urethane acrylic oligomer (manufactured by Shin-Nakamura Chemical Co., Ltd., "NK Oligo UA-53H"), 30 parts of a multifunctional acrylate mainly composed of pentaerythritol triacrylate (manufactured by Osaka Organic Chemical Industry Co., Ltd., product name "Viscoat #300"), 20 parts of 4-hydroxybutyl acrylate (manufactured by Osaka Organic Chemical Industry Co., Ltd.), 1 part of a leveling agent (manufactured by DIC Corporation, "GRANDIC PC4100") and 3 parts of a photopolymerization initiator (manufactured by Ciba Japan, "Irgacure 907") and diluting with methyl isobutyl ketone to a solids concentration of 50%.
[0076] (Anti-reflection layer forming coating solution A) 100 parts by weight of a multifunctional acrylate (manufactured by Arakawa Chemical Industries, Ltd., product name "Opstar KZ6728", solid content 20% by weight), 3 parts by weight of a leveling agent (manufactured by DIC Corporation, "GRANDIC PC4100"), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF, product name "OMNIRAD907", solid content 100% by weight) were mixed. The mixture was diluted with butyl acetate as a diluting solvent to a solid content of 12% by weight, and the mixture was stirred to prepare coating solution A for forming an anti-reflection layer.
[0077] (Anti-reflection layer forming coating solution B) 100 parts by weight of a polyfunctional acrylate mainly composed of pentaerythritol triacrylate (manufactured by Osaka Organic Chemical Industry Co., Ltd., trade name "Viscoat #300", solid content 100% by weight), 150 parts by weight of hollow nanosilica particles (manufactured by JGC Catalysts and Chemicals Co., Ltd., trade name "Surulia 5320", solid content 20% by weight, weight average particle diameter 75 nm), 50 parts by weight of solid nanosilica particles (manufactured by Nissan Chemical Industries, Ltd., trade name "MEK-2140Z-AC", solid content 30% by weight, weight average particle diameter 10 nm), 12 parts by weight of a fluorine-containing additive (manufactured by Shin-Etsu Chemical Co., Ltd., trade name "KY-1203", solid content 20% by weight), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF, trade name "OMNIRAD907", solid content 100% by weight) were mixed. To the mixture was added a mixed solvent of TBA (tertiary butyl alcohol), MIBK (methyl isobutyl ketone) and PMA (propylene glycol monomethyl ether acetate) in a weight ratio of 60:25:15 as a dilution solvent until the total solids content was 4% by weight, and the mixture was stirred to prepare coating solution B for forming an anti-reflection layer.
[0078] (First laminated part) The above-mentioned positive C plate was attached to the above-mentioned λ / 4 member (stretched film) via an ultraviolet-curing adhesive (thickness after curing: 1 μm) to obtain a retardation member. The obtained retardation member was attached to a glass plate (MICRO SLIDE GLASS, product number S, thickness 1.3 mm, 180 mm x 250 mm, manufactured by MATSUNAMI Co., Ltd.) via the above-mentioned 5 μm thick adhesive layer. Here, the retardation member was attached so that the positive C plate was located on the glass plate side. Next, the protective member was attached to the retardation member via the 5 μm-thick adhesive layer to obtain a first laminated portion on the glass plate. Here, the acrylic film of the protective member was attached to the retardation member side.
[0079] (Preparation of absorptive polarizing film) The thermoplastic resin substrate was a long amorphous isophthalic copolymerized polyethylene terephthalate film (thickness: 100 μm) having a water absorption rate of 0.75% and a Tg of about 75° C. One side of the resin substrate was subjected to a corona treatment. A PVA aqueous solution (coating liquid) was prepared by adding 13 parts by weight of potassium iodide to 100 parts by weight of a PVA-based resin made by mixing polyvinyl alcohol (polymerization degree 4200, saponification degree 99.2 mol%) and acetoacetyl-modified PVA (manufactured by Mitsubishi Chemical Corporation, product name "GOHSENEX Z410") in a ratio of 9:1, and dissolving the mixture in water. The above PVA aqueous solution was applied to the corona-treated surface of a resin substrate and dried at 60° C. to form a PVA-based resin layer with a thickness of 13 μm, thereby producing a laminate. The obtained laminate was uniaxially stretched at its free end to 2.4 times its original size in the machine direction (longitudinal direction) between rolls with different peripheral speeds in an oven at 130° C. (auxiliary air stretching treatment). Next, the laminate was immersed in an insolubilizing bath (a boric acid aqueous solution obtained by mixing 4 parts by weight of boric acid with 100 parts by weight of water) at a liquid temperature of 40° C. for 30 seconds (insolubilizing treatment). Next, the film was immersed in a dye bath (an aqueous iodine solution obtained by mixing iodine and potassium iodide in a weight ratio of 1:7 with 100 parts by weight of water) at a liquid temperature of 30°C for 60 seconds while adjusting the concentration so that the single transmittance (Ts) of the final polarizing film would be 42.0% or more (dyeing process). Next, the piece was immersed in a crosslinking bath (a boric acid aqueous solution obtained by mixing 3 parts by weight of potassium iodide and 5 parts by weight of boric acid with respect to 100 parts by weight of water) at a liquid temperature of 40° C. for 30 seconds (crosslinking treatment). Thereafter, the laminate was immersed in an aqueous boric acid solution (boric acid concentration: 4% by weight, potassium iodide concentration: 5% by weight) at a liquid temperature of 70°C and uniaxially stretched in the longitudinal direction (longitudinal direction) between rolls with different peripheral speeds to a total stretch ratio of 5.5 times (underwater stretching treatment). Thereafter, the laminate was immersed in a cleaning bath (an aqueous solution obtained by mixing 4 parts by weight of potassium iodide with 100 parts by weight of water) at a liquid temperature of 20° C. (cleaning treatment). Thereafter, while drying in an oven maintained at 90°C, the laminate was brought into contact with a SUS heated roll whose surface temperature was maintained at 75°C for approximately 2 seconds (drying shrinkage treatment). The shrinkage rate of the laminate in the width direction due to the drying shrinkage treatment was 5.2%. In this manner, a polarizing film (absorption type polarizing film) having a thickness of 5 μm was formed on the resin substrate.
[0080] (Second laminated part) The absorptive polarizing film was attached to a glass plate (MICRO SLIDE GLASS, product number S, thickness 1.3 mm, 180 mm×250 mm, manufactured by MATSUNAMI Co., Ltd.) via the above-mentioned adhesive layer having a thickness of 5 μm. Next, a reflective polarizing film ("APCF" manufactured by Nitto Denko Corporation) was attached to the absorptive polarizing film via the above-mentioned 5 μm-thick adhesive layer so that the reflection axis of the reflective polarizing film and the absorption axis of the absorptive polarizing film were arranged parallel to each other. Next, the protective member was attached to the reflective polarizing film to obtain a second laminate on the glass plate, with the acrylic film of the protective member facing the reflective polarizing film.
[0081] [Example 2] A first laminate part and a second laminate part were obtained in the same manner as in Example 1, except that the pressure-sensitive adhesive layer shown below was used. (Formation of adhesive layer) A monomer mixture containing 94.9 parts by weight of butyl acrylate, 5 parts by weight of acrylic acid, and 0.1 parts by weight of 2-hydroxyethyl acrylate was charged into a four-neck flask equipped with a stirring blade, a thermometer, a nitrogen gas inlet tube, and a condenser. Furthermore, 0.3 parts by weight of dibenzoyl peroxide as a polymerization initiator was charged together with ethyl acetate for 100 parts by weight of this monomer mixture, and nitrogen gas was introduced while gently stirring to replace the atmosphere in the flask with nitrogen. The liquid temperature in the flask was kept at 60°C and a polymerization reaction was carried out for 7 hours. Next, ethyl acetate was added to the resulting reaction liquid to adjust the solid concentration to 30% by weight, and a solution of an acrylic polymer with a weight average molecular weight (Mw) of 2.2 million was prepared. An acrylic adhesive was prepared by blending 100 parts by weight of the solid content of the obtained acrylic polymer solution with 0.6 parts by weight of a trimethylolpropane / tolylene diisocyanate adduct (product name: Coronate L, manufactured by Tosoh Corporation) and 0.075 parts by weight of a silane coupling agent (product name: KBM403, manufactured by Shin-Etsu Chemical Co., Ltd.). The obtained acrylic adhesive was applied to a substrate film, and the coating film on the substrate film was dried in an oven to form an adhesive layer having a thickness of 15 μm and a surface roughness Ra of 16 nm. The drying was performed by adjusting the air speed in the oven from the oven entrance to the center of the oven to a range of 15 m / min or less.
[0082] [Comparative Example 1] The first laminate part and the second laminate part were obtained in the same manner as in Example 2, except that in forming the adhesive layer, the air speed in the oven was adjusted to within a range of 15 m / min or less, and an adhesive layer having a thickness of 15 μm and a surface roughness Ra of 22 nm was formed.
[0083] [Comparative Example 2] The first laminate part and the second laminate part were obtained in the same manner as in Example 2, except that in forming the adhesive layer, the coating thickness of the acrylic adhesive was changed and the air speed in the oven was adjusted to within a range of 15 m / min or less to form an adhesive layer with a thickness of 23 μm and a surface roughness Ra of 29 nm.
[0084] The ISC values of the first laminated parts of the examples and comparative examples were measured using EyeScale-4W manufactured by Eye System Co., Ltd. Specifically, based on the specifications of the measuring device, the in-plane unevenness of the first laminated part and the second laminated part was calculated as the ISC value in the ISC measurement mode of the 3CCD image sensor. Fig. 4 is a diagram for explaining a method for measuring the ISC value, and is a schematic diagram showing the arrangement of a light source, a measurement sample, a screen, and a CCD camera as viewed from above. As shown in Fig. 4, a light source L, three first laminates 100, and a screen S were arranged in this order, and a transmitted image projected onto the screen S was measured by a CCD camera C. The measurement sample was an assembly of three first laminated units 100 arranged side by side. The three first laminated units 100 were arranged with an interval of 0.001 to 3 mm between them. As shown in FIG. 4, the first laminated unit 100 located closest to the light source L was arranged so that the adjacent glass plate G was located on the light source L side. The first laminated unit 100 located in the middle was arranged so that the adjacent glass plate G was located on the screen S side. The first laminated unit 100 located closest to the screen S was arranged so that the adjacent glass plate G was located on the light source L side. The distance from the light source L to the measurement sample in the X-axis direction was set to 10 to 60 cm. The distance from the light source L to the screen S in the X-axis direction was set to 70 to 130 cm. The distance from the CCD camera C to the measurement sample in the Y-axis direction was set to 3 to 30 cm. The distance from the CCD camera C to the screen S in the X-axis direction was set to 70 to 130 cm. For ease of understanding, the details of the first laminated portion are omitted in Fig. 4. The measurement results are shown in Table 1.
[0085] For the examples and comparative examples, appearance (light transmitted through the lens) was evaluated using an optical lens (manufactured by Thorabs, product name "LA1145") and a point light source (manufactured by Hamamatsu Photonics, model number "L8425-01"). Specifically, the first laminated part and the second laminated part cut into a circle of 45 mmφ were laminated in this order on the flat side of the optical lens while being lightly pressed with a hand roller so as not to introduce foreign matter, air bubbles, or deformation streaks into the surface. Next, in order to remove the influence of minute air bubbles, degassing was performed using a pressurized degassing device (autoclave). The degassing conditions were 50°C, 0.5 MPa, and 30 minutes. After degassing, the sample was left to cool at room temperature for 30 minutes or more to obtain a measurement sample. A point light source, an optical lens (measurement sample), and a screen were placed in this order, and the light from the point light source through the optical lens was projected onto the screen to evaluate its appearance. Here, the lens was held by a holder at a position where the light from the point light source was incident on the convex side of the optical lens. The distance from the point light source to the screen was 1050 mm, and the distance from the optical lens to the screen was 130 mm. The light reflected on the screen through the optical lens was visually observed, and the appearance was evaluated according to the following evaluation criteria. The measurement results are shown in Table 1. (Evaluation Criteria) Good: No visible wrinkles or ripples - Defective: Wrinkles and ripples are visible
[0086] [Table 1]
[0087] The present invention is not limited to the above-described embodiment, and various modifications are possible. For example, the above-described embodiment may be replaced with a configuration that is substantially the same as the configuration shown in the above-described embodiment, a configuration that provides the same effect, or a configuration that can achieve the same purpose. [Industrial Applicability]
[0088] The lens portion according to the embodiment of the present invention can be used in a display such as VR goggles. [Explanation of symbols]
[0089] 2 display system, 4 lens portion, 12 display element, 14 reflective polarizing member, 16 first lens portion, 18 half mirror, 20 first phase difference member, 22 second phase difference member, 24 second lens portion, 28 absorptive polarizing member, 30 third phase difference member, 31 first protective member, 32 second protective member, 41 adhesive layer, 42 adhesive layer, 43 adhesive layer, 44 adhesive layer, 45 adhesive layer, 46 adhesive layer, 100 first laminate portion, 200 second laminate portion.
Claims
1. An optical member set having a first laminated portion including a polarizing member, a first λ / 4 member, a second λ / 4 member, and at least one pressure-sensitive adhesive layer, and a reflective polarizing member, The respective members included in the optical member set are arranged such that light emitted forward from the display element passes through the polarizing member, the first λ / 4 member, the first lens unit, and the first stacked unit in this order, is reflected by the reflective polarizing member, passes through the first stacked unit, is reflected toward the front side, and passes through the first stacked unit, the reflective polarizing member, and the second lens unit in this order; The ISC value of an assembly formed by arranging three of the first laminated units is 100 or less. Optical component set.
2. The optical member set according to claim 1 , further comprising a second stack including the reflective polarizing member.
3. The optical member set according to claim 2 , wherein the first laminated portion and the second laminated portion are disposed apart from each other.
4. The optical member set according to claim 2 , wherein the second stack portion includes an absorptive polarizing member disposed between the reflective polarizing member and the second lens portion.
5. The optical member set according to claim 2 , wherein the second stacked portion includes a third λ / 4 member disposed between the reflective polarizing member and the second lens portion.
6. The optical member set according to claim 1 , wherein the first stacked portion includes a first protective member disposed in front of the second λ / 4 member.
7. The optical member set according to claim 1 , wherein the first laminated portion includes three or less pressure-sensitive adhesive layers.
8. The optical member set according to claim 1 , wherein each of the pressure-sensitive adhesive layers included in the first laminated portion has a thickness of 20 μm or less.
9. The optical member set according to claim 1 , wherein each of the pressure-sensitive adhesive layers included in the first laminate portion has a surface roughness Ra of 20 nm or less.
10. The optical member set according to claim 1 , wherein each of the pressure-sensitive adhesive layers included in the first laminated portion is a single layer.
Citation Information
Patent Citations
Display optical system for reducing ghosting and head-mounted display device
CN112305763A
Optical system of miniature head-mounted display
CN211826725U
Optical system for head-mounted displays
JP2019526075A
Compact collimator for polarized light with high contrast
JP2022540833A
Method for manufacturing optical system for head-mounted display
WO2022075264A1