Thermal recording material
The heat-sensitive recording material with specific urea and N,N'-diarylurea compounds addresses the lack of light and acid resistance in conventional materials, ensuring enhanced durability under environmental stress.
Patent Information
- Application Number
- JP2023079707
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional heat-sensitive recording materials lack sufficient light resistance and acid resistance, particularly when exposed to lighting and acidic conditions due to environmental factors and substances.
A heat-sensitive recording material comprising a support with a heat-sensitive recording layer containing specific urea compounds and N,N'-diarylurea compounds, represented by defined chemical formulas, which enhance the material's light and acid resistance.
The material exhibits improved light resistance and acid resistance, maintaining image quality under various environmental conditions.
Smart Images

Figure 2024163807000001 
Figure 2024163807000002 
Figure 2024163807000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a heat-sensitive recording material, and more particularly to a heat-sensitive recording material having excellent light resistance and acid resistance in the image area. [Background technology]
[0002] Thermal recording materials are already well known. Thermal recording materials generally have a thermal recording layer mainly composed of an electron-donating dye precursor and an electron-accepting developer on a support. The thermal recording material develops color and forms an image by heating using a thermal head, a thermal pen, a laser beam, or the like. Thermal recording materials are used as output media for measurement recorders, facsimiles, ATM statements of financial institutions, computer printing terminals, label printers, ticket issuing machines, POS systems, ticket issuing machines, portable terminals, and the like.
[0003] As the applications of thermal recording materials have expanded to a wide variety, there is a trend for thermal recording materials to be required to have not only color development but also greater resistance than ever before. The resistance includes, for example, light resistance and acid resistance. The reason for this is that printed matter used as output media tends to be left under lighting, and acidic water tends to increase due to the effects of not only acidic substances contained in food but also COx, NOx, and SOx present in the living environment.
[0004] For example, a known example of a heat-sensitive recording material having excellent oil resistance is a heat-sensitive recording medium having a heat-sensitive recording layer containing a colorless or light-colored electron-donating leuco dye and an electron-accepting developer on a support, the heat-sensitive recording layer containing N-[2-(3-phenylureido)phenyl]benzenesulfonamide and a urea compound as the electron-accepting developer (see, for example, Patent Document 1). Further, as a thermal recording material having improved acid resistance and water resistance against, for example, vinegar, a thermal recording material is known which has, on a support, a filler, an undercoat layer mainly composed of a resin, a thermal color developing layer mainly composed of a leuco dye and a developer which causes the leuco dye to develop color when heated, and a protective layer mainly composed of diacetone-modified polyvinyl alcohol and a crosslinking agent, in which the undercoat layer contains diacetone-modified polyvinyl alcohol as a resin and the thermal color developing layer contains N-aminopolyacrylamide as a crosslinking agent (see, for example, Patent Document 2). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent No. 6960562 [Patent Document 2] JP 2011-056894 A DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]
[0006] The thermosensitive recording material described in Patent Document 2 has a technical idea of achieving acid resistance and the like by the action and effect of a crosslinking agent contained in the thermosensitive recording layer and the protective layer. Therefore, Patent Document 2 does not disclose any color developer related to acid resistance. An object of the present invention is to provide a heat-sensitive recording material in which the light resistance and acid resistance of a heat-sensitively recorded image are improved compared to conventional materials. [Means for solving the problem]
[0007] As a result of intensive research, the present inventors have arrived at the following invention. [1] A thermal recording material having a support having a front surface and a back surface, and a thermal recording layer containing a dye precursor and a color developer on at least the front surface of the support, wherein the color developer contains one or more urea-based compounds represented by the following general formula (Chemical Formula 1) and one or more N,N'-diaryl urea-based compounds represented by the following general formula (Chemical Formula 3).
[0008] [ka] Here, R1 represents the following general formula (Chemical Formula 2).
[0009] [ka] Here, R2 represents a hydrogen atom or an alkyl group having 1 to 6 carbon atoms.
[0010] [ka] Here, R3 represents a substituted or unsubstituted branched or alicyclic alkyl group having 3 to 12 carbon atoms, a substituted or unsubstituted alkyl group having 1 to 12 carbon atoms, a substituted or unsubstituted alkoxy group having 1 to 12 carbon atoms, a substituted or unsubstituted aryl group having 6 to 12 carbon atoms, or an aralkyl group having 7 to 12 carbon atoms substituted with a halogen atom. Note that multiple R3s may be the same or different. In the general formula (Chemical Formula 3), multiple substituents "-OSO2-R3" are at the same or different positions in each benzene ring.
[0011] In some embodiments, the present invention is the following. [2] The heat-sensitive recording material according to the above [1], wherein the compound represented by the above general formula (Chemical Formula 1) contains at least N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea.
[0012] In some embodiments, the present invention is the following. [3] The heat-sensitive recording material according to the above [1], wherein the compound represented by the above general formula (Chemical Formula 3) contains at least N,N'-di[3-(p-toluenesulfonyloxy)phenyl]urea.
[0013] In some embodiments, the present invention is the following. [4] The heat-sensitive recording material according to the above [1], wherein the compound represented by the above general formula (Chemical Formula 1) contains at least N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, and the compound represented by the above general formula (Chemical Formula 3) contains at least N,N'-di[3-(p-toluenesulfonyloxy)phenyl]urea. Effect of the Invention
[0014] The heat-sensitive recording material of the present invention has improved light resistance and acid resistance in the heat-recorded image area compared to conventional materials. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The present invention will now be described in more detail. The thermal recording material has a support having a front and a back surface, and a thermal recording layer containing a dye precursor and a color developer on at least the front surface of the support. The color developer contains one or more urea compounds represented by the above general formula (Chemical Formula 1) and one or more N,N'-diaryl urea compounds represented by the above general formula (Chemical Formula 3). Here, the front and back surfaces of the support are expressions for convenience in distinguishing between surfaces, and do not mean the front and back surfaces of the support based on a specific difference.
[0016] In some embodiments, the heat-sensitive recording material contains 30 parts by mass or more and 50 parts by mass or less of the dye precursor per 100 parts by mass of the color developer in the heat-sensitive recording layer, because this allows better compatibility between prevention of background discoloration of the heat-sensitive recording material and sensitivity to heat.
[0017] The dye precursor is a dye that is colorless or light-colored under normal conditions, has a partial skeleton such as lactone, lactam, sultone, spiropyran, ester, or amide, and develops color by donating electrons or accepting protons from acids or the like. In a thermal recording material with good color development, the dye precursor develops color by reacting with a color developer upon heating. In some embodiments, the dye precursor is one or more types selected from those conventionally known in the thermal recording field.
[0018] In some embodiments, the dye precursor is a leuco dye, because they are commercially available and available in a variety of types. Examples of leuco dyes include triarylmethane compounds, diphenylmethane compounds, xanthene compounds, thiazine compounds, and spiro compounds. In some embodiments, the dye precursor is one or more selected from the group consisting of leuco dyes. Leuco dyes include, for example, 3,3-bis(p-dimethylaminophenyl)-6-dimethylaminophthalide (crystal violet lactone), 3,3-bis(p-dimethylaminophenyl)phthalide, 3-(p-dimethylaminophenyl)-3-(1,2-dimethylindol-3-yl)phthalide, 3-(p-dimethylaminophenyl)-3-(2-methylindol-3-yl)phthalide, 3-(p-dimethylaminophenyl)-3-(2-phenylindol-3-yl)phthalide, 3,3-bis(1,2-dimethylindol-3-yl)-5-dimethylaminophthalide, 3,3-bis(1,2-dimethylindol-3-yl)-6-dimethylaminophthalide, 3,3-bis(9-ethylcarbazol-3-yl)-5 ... bis(2-phenylindol-3-yl)-5-dimethylaminophthalide, and 3-p-dimethylaminophenyl-3-(1-methylpyrrol-2-yl)-6-dimethylaminophthalide, as well as 4,4'-bis(dimethylaminophenyl)benzhydryl benzyl ether, N-chlorophenylleucoauramine, and N-2,4,5-trichlorophenylleucoauramine, as well as rhodamine B anilinolactam, rhodamine B p-chloroanilinolactam, 3-diethylamino-7-dibenzylaminofluoran, 3-diethylamino-7-octylaminofluoran, 3-diethylamino-7-phenylfluoran, 3-diethylamino-7-chlorofluoran, 3-diethylamino-6-chloro-7-methylfluoran, 3-diethylamino-7-(3,4-dichloroanilino)fluoran, 3-diethylamino-7-(2-chloroanilino)fluoran, 3-dibutylamino-7-(2-chloroanilino)fluoran, 3-diethylamino-6-methyl-7-anilinofluoran, 3-dipentylamino-6-methyl-7-anilinofluoran, 3-(N-ethyl-N-tolyl)amino-6-methyl-7-anilinofluoran, 3-piperidinyl dino-6-methyl-7-anilinofluoran, 3-(N-ethyl-N-tolyl)amino-6-methyl-7-phenethylfluoran, 3-diethylamino-7-(4-nitroanilino)fluoran, 3-(N-methyl-N-propyl)amino-6-methyl-7-anilinofluoran, 3-(N-ethyl-N-isoamyl)amino-6-methyl-7-anilinofluoran, 3-(N-methyl- N-cyclohexyl)amino-6-methyl-7-anilinofluoran, 3-(N-ethyl-N-tetrahydrofurfuryl)amino-6-methyl-7-anilinofluoran, 3-diethylamino-6-methyl-7-(3-trifluoromethylanilino)fluoran, 2-anilino-3-diethylamino-6-methylfluoran, and 2-anilino-6-dibutylamino-3-methylfluoran, as well as benzoyl leucomethylene blue and p-nitrobenzoyl leucomethylene blue, and further 3-methylspirodinaphthopyran, 3-ethylspirodinaphthopyran, 3,3′-dichlorospirodinaphthopyran, 3-benzylspirodinaphthopyran, 3-methylnaphtho-(3-methoxybenzo)spiropyran, and 3-propylspirobenzopyran. In some embodiments, the dye precursor is one or more selected from the group consisting of fluoran-based compounds in xanthene-based compounds. In at least one embodiment, the dye precursor is one or two selected from 2-anilino-6-dibutylamino-3-methylfluoran, 3-dipentylamino-6-methyl-7-anilinofluoran, and 3-(N-ethyl-N-isoamyl)amino-6-methyl-7-anilinofluoran. The reason for this is that they have excellent color development properties.
[0019] The developer is a combination of at least two types of developers, including a urea compound represented by the above general formula (Chemical Formula 1) and an N,N'-diaryl urea compound represented by the above general formula (Chemical Formula 3). Here, R1 in the above general formula (Chemical Formula 1) represents a benzenesulfonyloxy group represented by the above general formula (Chemical Formula 2). R2 in the above general formula (Chemical Formula 2) represents a hydrogen atom or an alkyl group having 1 to 6 carbon atoms. R3 in the above general formula (Chemical Formula 3) represents a substituted or unsubstituted branched or alicyclic alkyl group having 3 to 12 carbon atoms, a substituted or unsubstituted alkyl group having 1 to 12 carbon atoms, a substituted or unsubstituted alkoxy group having 1 to 12 carbon atoms, a substituted or unsubstituted aryl group having 6 to 12 carbon atoms, or an aralkyl group having 7 to 12 carbon atoms substituted with a halogen atom. Note that multiple R3s may be the same or different from each other. In the general formula (Chemical Formula 3), multiple substituents "-OSO2-R3" are in the same positional relationship or different positions in each benzene ring.
[0020] Examples of the color developer represented by the general formula (Chemical Formula 1) include N-3-(phenylsulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, N-4-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, N-3-(t-butylphenylsulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, and N-3-(n-hexylphenylsulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea. In some embodiments, the color developer represented by the general formula (Chemical Formula 1) is one or more selected from the group consisting of these. In at least one embodiment, the color developer represented by the general formula (Chemical Formula 1) is N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea. This is because the light resistance of the thermal recording material is improved.
[0021] Examples of R3 in the above general formula (Chemical Formula 3) include the following. Examples of the alkyl group include a methyl group, an ethyl group, an n-propyl group, an i-propyl group, an n-butyl group, an i-butyl group, a t-butyl group, a cyclopentyl group, a hexyl group, a cyclohexyl group, a 2-ethylhexyl group, and a lauryl group. Examples of aryl groups include a phenyl group, a p-tolyl group, a m-tolyl group, an o-tolyl group, a 2,5-dimethylphenyl group, a 2,4-dimethylphenyl group, a 3,5-dimethylphenyl group, a 2,3-dimethylphenyl group, a 3,4-dimethylphenyl group, a mesitylene group, a p-ethylphenyl group, a p-propylphenyl group, a p-butylphenyl group, a p-methoxyphenyl group, a 3,4-dimethoxyphenyl group, a p-ethoxyphenyl group, a p-chlorophenyl group, a 1-naphthyl group, a 2-naphthyl group, and a methylated naphthyl group. Examples of aralkyl groups include benzyl, 1-phenylethyl, 2-phenylethyl, 3-phenylpropyl, p-methylbenzyl, m-methylbenzyl, m-ethylbenzyl, p-ethylbenzyl, pi-propylbenzyl, pt-butylbenzyl, p-methoxybenzyl, m-methoxybenzyl, o-methoxybenzyl, m,p-di-methoxybenzyl, p-ethoxy-m-methoxybenzyl, and p-chlorobenzyl groups.
[0022] The color developer represented by the above general formula (Chemical Formula 3) is, for example, N,N'-di-[3-(benzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(o-toluenesulfonyloxy)phenyl]urea, N,N'-di-[3-(m-toluenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-toluenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-toluenesulfonyloxy)-4-methyl-phenyl]urea, N,N'-di-[3-(p-xylenesulfonyloxy) ... phenyl]urea, N,N'-di-[3-(m-xylenesulfonyloxy)phenyl]urea, N,N'-di-[3-(mesitylenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-ethylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-propylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-isopropylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(pt-butylbenzenesulfonyloxy)phenyl]urea , N,N'-di-[3-(p-methoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(m-methoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(o-methoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(m,p-dimethoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-ethoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-propoxybenzenesulfonyloxy)phenyl]urea phenyl]urea, N,N'-di-[3-(p-butoxybenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(o-phenylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-phenylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-phenylbenzenesulfonyloxy)phenyl]urea, N,N'-di-[3-(p-chlorobenzenesulfonyloxy)phenyl]urea, N,N'-di-[4-(benzenesulfonyloxy)phenyl]urea, N,N'-di-[4-(p-toluenesulfonyloxy)phenyl]urea, N,N'-di-[3-(ethanesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(p-toluenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(m-toluenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(o-toluenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N' -[3-(p-xylenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(mesitylenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(p-ethylbenzenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(p-methoxybenzenesulfonyloxy)phenyl]urea, N-[3-(benzenesulfonyloxy)phenyl]-N'-[3-(p-methoxybenzenesulfonyloxy)phenyl]urea, N-[3-(ethanesulfonyloxy)phenyl]urea, N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(m-toluenesulfonyloxy)phenyl]urea, N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(o-toluenesulfonyloxy)phenyl]urea, N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(p-ethylbenzenesulfonyloxy)phenyl]urea, N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(p-ethylbenzenesulfonyloxy)phenyl]urea, Examples of the phenyl urea include N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(methanesulfonyloxy)phenyl]urea, N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(propanesulfonyloxy)phenyl]urea, and N-[3-(p-toluenesulfonyloxy)phenyl]-N'-[3-(t-butanesulfonyloxy)phenyl]urea. In some embodiments, the color developer represented by the general formula (Chemical Formula 3) is one or more selected from the group consisting of these. In at least one embodiment, the color developer represented by the general formula (Chemical Formula 3) is N,N'-di-[3-(p-toluenesulfonyloxy)phenyl]urea. This is because the acid resistance of the thermal recording material is improved.
[0023] In some embodiments, the thermosensitive recording layer may contain, in addition to the color developers represented by the general formulae (Chemical Formula 1) and (Chemical Formula 3), a color developer conventionally known in the field of thermosensitive recording, within a range that does not impair the effects of the present invention. In at least one embodiment, the thermosensitive recording layer contains 80% by mass or more and 100% by mass or less of the color developers represented by the general formulae (Chemical Formula 1) and (Chemical Formula 3) relative to the total color developers contained in the thermosensitive recording layer. The reason for this is that the acid resistance of the thermosensitive recording material is improved.
[0024] In some embodiments, the content mass ratio of the color developers represented by the general formula (Chemical Formula 1) and the general formula (Chemical Formula 3) in the thermosensitive recording layer is General Formula (Chemical Formula 1):General Formula (Chemical Formula 3)=10:90 to 50:50. In at least one embodiment, the content mass ratio of the color developers represented by the general formula (Chemical Formula 1) and the general formula (Chemical Formula 3) in the thermosensitive recording layer is General Formula (Chemical Formula 1):General Formula (Chemical Formula 3)=10:90 to 50:50, where the color developer represented by the general formula (Chemical Formula 1) is N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea and the color developer represented by the general formula (Chemical Formula 3) is N,N'-di-[3-(p-toluenesulfonyloxy)phenyl]urea. The reason for this is that the light resistance and acid resistance of the thermosensitive recording material are improved.
[0025] The thermal recording material can be obtained by applying a coating liquid for a thermal recording layer, in which each component such as a dye precursor and a color developer is dispersed or dissolved in water, to the surface of a support and drying the coating liquid. The thermal recording layer may be either a single layer or a multilayer. The concept of water includes distilled water and ion-exchanged water. Coating may be performed using a coating device or printing device conventionally known in the field of coated paper. Examples of coating devices include a film press coater, a rod coater, an air knife coater, a rod blade coater, a bar coater, a blade coater, a gravure coater, a curtain coater, an E-bar coater, and a film transfer coater. Examples of printing devices include various printing machines such as lithographic, letterpress, intaglio, flexographic, gravure, and screen. The drying may be performed by a method using a drying device conventionally known in the field of coated paper, such as a hot air dryer such as a straight tunnel dryer, an arch dryer, an air loop dryer, or a sine curve air float dryer, an infrared heating dryer, or a dryer using microwaves or the like. In order to improve the smoothness of the heat-sensitive recording layer, a machine calender, a super calender, a gloss calender, a brushing device or the like can be applied to the heat-sensitive recording layer. In some embodiments, the solid coating amount of the thermosensitive recording layer is 2 g / m2 on the surface of the support. 2 More than 15g / m 2 The reason is that the light resistance and acid resistance are improved, or the productivity is improved.
[0026] In addition to the dye precursor and the color developer, the thermal recording layer may contain one or more additives selected from the group of additives conventionally known in the thermal recording field, such as dispersants, binders, sensitizers, lubricants, storage stability improvers, and pigments, as necessary. In some embodiments, the thermal recording material contains a dispersant, binder, and pigment in addition to the dye precursor and color developer in the thermal recording layer. This is because the production of the thermal recording material is stable. In some embodiments, the thermal recording material contains a sensitizer in addition to the dye precursor and color developer in the thermal recording layer. This is because the sensitivity of the thermal recording material to heat is improved. In at least one embodiment, the thermal recording material contains a dispersant, binder, pigment, and sensitizer in addition to the dye precursor and color developer in the thermal recording layer.
[0027] The above dispersing agents are conventionally known in the field of thermal recording. Examples of the dispersing agent include polyvinyl alcohols such as fully saponified polyvinyl alcohol, partially saponified polyvinyl alcohol, sulfonic acid modified polyvinyl alcohol, silanol modified polyvinyl alcohol, carboxyl modified polyvinyl alcohol, diacetone modified polyvinyl alcohol, acetoacetyl modified polyvinyl alcohol, phosphoric acid modified polyvinyl alcohol, butyral modified polyvinyl alcohol, and epoxy modified polyvinyl alcohol; starch and its modifications; cellulose derivatives such as hydroxyethyl cellulose, methyl cellulose, hydroxypropyl cellulose, ethyl cellulose, and carboxymethyl cellulose; proteins such as gelatin and casein; and chitosan in an acid solution. Examples of the dispersant include hydrates, sodium alginate, polyvinylpyrrolidone, diisobutylene maleic anhydride copolymers, styrene isobutylene maleic anhydride copolymers, styrene maleic anhydride copolymers, ethylene acrylic acid copolymers, styrene acrylic acid copolymers, styrene acrylic acid ester copolymers, polycarboxylic acids such as polyacrylic acid, water-soluble polymer compounds such as polyacrylic acid esters and polyacrylsulfonic acid, anionic low-molecular surfactants such as dodecylbenzenesulfonates, dialkylsulfosuccinates, alkylnaphthalenesulfonates, alkyldiphenyletherdisulfonates and fatty acid metal salts, and nonionic surfactants such as acetylene glycol. In some embodiments, the dispersant is one or more selected from the group consisting of the above.
[0028] The binders are those conventionally known in the thermal recording field. Examples of the binder include water-soluble binders such as starches, hydroxymethylcellulose, methylcellulose, ethylcellulose, carboxymethylcellulose, gelatin, casein, polyvinyl alcohol, modified polyvinyl alcohol, sodium alginate, polyvinylpyrrolidone, polyacrylamide, acrylamide acrylate copolymers, acrylamide acrylate ester methacrylate copolymers, polyacrylates, polymaleates, styrene maleic acid copolymers, ethylene maleic acid copolymers, and isobutylene maleic acid copolymers, and water-dispersible binders such as styrene butadiene copolymers, acrylonitrile butadiene copolymers, methyl acrylate butadiene copolymers, acrylonitrile butadiene styrene copolymers, polyvinyl acetate, vinyl acetate acrylate copolymers, ethylene vinyl acetate copolymers, polyacrylates, styrene acrylate copolymers, and polyurethanes. In some embodiments, the binder is one or more selected from the group consisting of the above.
[0029] The above pigments are conventionally known in the field of thermal recording. Examples of the pigment include inorganic pigments such as diatomaceous earth, talc, kaolin, calcined kaolin, ground calcium carbonate, light calcium carbonate, magnesium carbonate, zinc oxide, amorphous silica, colloidal silica, alumina, alumina hydrate, aluminum hydroxide, magnesium hydroxide, titanium dioxide, barium sulfate, zinc sulfate, and amorphous calcium silicate, as well as organic pigments such as various resin particles. In some embodiments, the pigment is one or more selected from the group consisting of the above.
[0030] The above sensitizers are conventionally known in the field of thermal recording. Examples of the sensitizer include fatty acid monoamides such as palmitic acid monoamide and stearic acid monoamide, diphenyl sulfone, N-hydroxymethylstearic acid amide, N-stearylstearic acid amide, ethylene bisstearic acid amide, methylene bisstearic acid amide, methylolstearic acid amide, N-stearyl urea, benzyl-2-naphthyl ether, p-toluenesulfonamide, m-terphenyl, 4-benzylbiphenyl, 2,2′-bis(4-methoxyphenoxy)diethyl ether, α,α′- Examples of the sensitizer include diphenoxy-o-xylene, bis(4-methoxyphenyl)ether, diphenyl adipate, dibenzyl oxalate, bis(4-methylbenzyl)oxalate, bis(4-chlorobenzyl)oxalate, dimethyl terephthalate, dibenzyl terephthalate, phenyl benzenesulfonate, bis(4-allyloxyphenyl)sulfone, 1,2-bis(3-methylphenoxy)ethane, 1,2-diphenoxyethane, 4-acetylacetophenone, acetoacetic anilides, fatty acid anilides, etc. In some embodiments, the sensitizer is one or more selected from the group consisting of the above.
[0031] In addition to the dye precursor and the color developer, the thermal recording layer may contain, as necessary, one or more auxiliary agents selected from the group consisting of hindered phenol compounds, hindered amine compounds, phosphate derivatives, and benzotriazole derivatives, which are conventionally known in the thermal recording field, in order to improve the storage stability of images, higher fatty acid metal salts such as zinc stearate and calcium stearate, waxes such as paraffin, oxidized paraffin, polyethylene, oxidized polyethylene, and castor wax, in order to improve sticking resistance, hardeners and crosslinking agents in order to improve water resistance, and further surfactants, fluorescent dyes, coloring dyes, and bluing agents.
[0032] The support may be any of transparent support, semi-transparent support and opaque support, and is not particularly limited.The support may be, for example, paper, various nonwoven fabrics, woven fabrics, synthetic resin films, synthetic resin laminated paper, synthetic paper, metal foil, ceramic paper, etc., and composite sheets of these.In some embodiments, from the viewpoint of environmental issues, the support is paper.
[0033] In some embodiments, the thermal recording material has an undercoat layer between the support and the thermal recording layer, which is conventionally known in the thermal recording field.The reason for this is that the adhesion between the support and the thermal recording layer and / or the dimensional stability of the thermal recording material are improved.The undercoat layer can contain various additives such as pigments and binders, as well as surfactants, coloring dyes, fluorescent dyes, lubricants and ultraviolet absorbers.
[0034] In some embodiments, the thermal recording material has a backcoat layer, which is conventionally known in the field of coated paper, on the back side of the support, or is subjected to a water-coating treatment. This is because it can suppress curling of the thermal recording material. The backcoat layer can contain various additives such as pigments and binders, as well as surfactants, coloring dyes, fluorescent dyes, lubricants, and ultraviolet absorbers.
[0035] In some embodiments, the thermal recording material has a protective layer on the thermal recording layer, which is conventionally known in the thermal recording field. This is because the thermal recording material can obtain scratch resistance, water resistance, etc. The protective layer can contain pigments and binders, as well as various additives such as lubricants, hardeners, crosslinking agents, and ultraviolet absorbers.
[0036] The method of forming the undercoat layer, backcoat layer and protective layer on the thermal recording material may be a method using a coating device or printing device conventionally known in the field of coated paper. Examples of the coating device include a film press coater, a rod coater, an air knife coater, a rod blade coater, a bar coater, a blade coater, a gravure coater, a curtain coater, an E-bar coater and a film transfer coater. Examples of the printing device include various printing machines such as lithographic, letterpress, intaglio, flexographic, gravure and screen. EXAMPLES
[0037] The present invention will be described in more detail below with reference to examples. However, the present invention is not limited to these examples. Here, "parts by mass" and "% by mass" refer to the amount of dry solids or the amount of substantial components, respectively. The amount of coating refers to the amount of dry solids.
[0038] The paper supports and the thermal recording materials of the respective Examples and Comparative Examples were prepared according to the following procedures.
[0039] <Thermal recording material paper support> The paper stock was prepared as follows: Pulp (LBKP with CSF freeness of 420 ml) 1000 parts by mass Filler (light calcium carbonate) 100 parts by mass Aluminum sulfate 10 parts by mass Paper strength agent (cationized starch) 10 parts by weight AKD sizing agent 1 part by weight
[0040] The above-mentioned paper stock was made into paper using a fourdrinier paper machine. The obtained paper was machine calendered to a basis weight of 90 g / m 2 Both sides of the obtained base paper were subjected to a size press treatment using a sizing liquid containing starch as a surface sizing agent. The amount of starch attached was 1 g / m per side. 2 The paper obtained by the size press treatment was used as a support for a thermal recording material.
[0041] <Coating fluid for undercoat layer> The following materials were mixed with water to prepare a coating liquid for the undercoat layer. Pigment (calcined kaolin) 1000 parts by weight Dispersant (ammonium polyacrylate) 1 part by weight Dispersant (sodium hexametaphosphate) 1 part by mass Binder (styrene butadiene copolymer) 120 parts by weight Binder (urea modified starch phosphate) 60 parts by weight
[0042] <Undercoat layer> The coating solution for the undercoat layer was applied to the surface of the support at a coating amount of 9 g / m 2 The coating was then performed so that an undercoat layer was provided on the surface of the support and then dried.
[0043] <Dispersion of dye precursor> The following ingredients were mixed in water as a medium, and wet-pulverized in a bead mill until the volume average particle size became 0.7 μm, to obtain a dispersion with a concentration of 30% by mass. Dye precursor (types listed in Table 1) / 40 parts by weight Dispersant (fully saponified polyvinyl alcohol) 10 parts by weight Acetylene glycol surfactant 0.2 parts by mass Here, 2-anilino-6-dibutylamino-3-methylfluoran was used for dye precursor A described in Table 1, 3-dipentylamino-6-methyl-7-anilinofluoran was used for dye precursor B described in Table 1, and 3-(N-ethyl-N-isoamyl)amino-6-methyl-7-anilinofluoran was used for dye precursor C described in Table 1.
[0044] <Dispersion of color developer and sensitizer> The following components were dispersed and dissolved in water as a medium, and mixed. The developer and sensitizer were wet-pulverized in a bead mill until the volume average particle size became 0.7 μm, to obtain a dispersion with a concentration of 30% by mass. Developer type and combination are listed in Table 1 / 100 parts by weight Sensitizer (1,2-diphenoxyethane) 50 parts by mass Sensitizer (stearic acid monoamide) 30 parts by weight Dispersant (fully saponified polyvinyl alcohol) 4 parts by weight Dispersant (styrene-maleic acid copolymer) 7 parts by weight Zinc stearate 20 parts by weight Surfactant (diethylhexyl sodium sulfosuccinate) 5 parts by weight Paraffin (paraffin wax) 10 parts by weight Here, N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea was used as developer A in Table 1, N,N'-di-[3-(p-toluenesulfonyloxy)phenyl]urea was used as developer B in Table 1, N-3-(phenylsulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea was used as developer C in Table 1, N,N'-di-[3-(ethanesulfonyloxy)phenyl]urea was used as developer D in Table 1, and conventionally known 4,4'-dihydroxydiphenylsulfone was used as developer E in Table 1. Conventionally known 4-hydroxy-4'-isopropoxydiphenylsulfone was used as developer F in Table 1.
[0045] <Pigment dispersion> The following ingredients were mixed and stirred in water as a medium to obtain a dispersion with a concentration of 15% by mass. Aluminum hydroxide 80 parts by weight Amorphous silica 20 parts by weight Dispersant (ammonium polyacrylate) 0.4 parts by weight Dispersant (polyvinyl alcohol) 35 parts by weight Binder (polyacrylate) 12 parts by weight
[0046] <Coating solution for thermal recording layer> The dye precursor dispersion, the developer and sensitizer dispersion, and the pigment dispersion were mixed and dispersed so that the final dye precursor, developer, and white pigment had the following mass ratios. Parts by weight of dye precursor: parts by weight of color developer: parts by weight of white pigment = 40:100:80
[0047] <Thermal recording materials> The coating amount of the heat-sensitive recording layer coating liquid was 3 g / m2 on the surface side of the support having the undercoat layer. 2 The coating was performed using an air knife coater and dried using a dryer so that the coating became a thickness of 100 μm. Thereafter, a calendar treatment was performed to obtain a heat-sensitive recording material.
[0048] <Thermal recording> For each of the thermal recording materials of the Examples and Comparative Examples, a printing test machine (OHKURA ELECTRIC CO., LTD., TH-PMD) was used to print a solid black gradation image by gradually changing the applied energy from 0.00 mJ / dot to 0.58 mJ / dot.
[0049] The light resistance and acid resistance of the thermal recording materials of each of the Examples and Comparative Examples were evaluated. The evaluation results are shown in Table 1.
[0050] [Table 1]
[0051] <Light resistance> The light resistance of the thermal recording material was evaluated by the following method. The printed thermal recording material was measured using a xenon arc weatherometer (Atlas Co., Ltd.) to determine the irradiance at 340 nm was 0.39 W / m 2 The materials were irradiated with light of this formula for three times, 8 hours, 24 hours, and 144 hours, under conditions of 40°C and 55% relative humidity. After irradiation, the optical color density of the black solid area where the applied energy was 0.58 mJ / dot was measured for each thermal recording material using a reflection densitometer (Videojet X-Rite KK, MACBETH (registered trademark) RD-918). The measured values were evaluated according to the following criteria. In the present invention, if a thermal recording material is rated A or B, it is considered to have improved light resistance compared to conventional materials. A: The density after 8 hours of irradiation is 1.00 or more. And the concentration value after 144 hours of irradiation is 0.85 or more and less than 1.00. B: Density after 8 hours of irradiation is 1.00 or more; And the concentration value after 144 hours of irradiation is 0.70 or more and less than 0.85. C: Density after 8 hours of irradiation is less than 1.00; and / or the concentration value after 144 hours of irradiation is less than 0.70.
[0052] <Acid resistance> The acid resistance of the heat-sensitive recording material was evaluated by the following method. The printed thermal recording materials were immersed in an aqueous solution of acetic acid at 35°C and a concentration of 4% by mass for 24 hours. After immersion, the optical color density of the solid black area of each thermal recording material where the applied energy was 0.58 mJ / dot was measured using a reflection densitometer (Videojet X-Rite KK, MACBETH RD-918). The measured values were evaluated according to the following criteria. In the present invention, thermal recording materials that are rated A, B, or C are considered to have improved acid resistance compared to conventional materials. A: Concentration after immersion is 1.20 or more. B: Concentration after immersion is 1.10 or more and less than 1.20. C: Concentration after immersion is 1.00 or more and less than 1.10. D: Concentration after immersion is less than 1.00.
[0053] From the results in Table 1, it is clear that Examples 1 to 14, which correspond to the present invention, are heat-sensitive recording materials that have improved light fastness and acid fastness compared to conventional materials. On the other hand, it is clear that Comparative Examples 1 to 10, which do not satisfy the constitution of the present invention, do not satisfy light fastness and / or acid fastness.
[0054] Mainly, by comparing Examples 7, 13 and 14, it can be seen that the developer represented by the general formula (Chemical Formula 1) is preferably N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, and the developer represented by the general formula (Chemical Formula 3) is preferably N,N'-di-[3-(p-toluenesulfonyloxy)phenyl]urea.
Claims
1. A thermal recording material having a support having a front surface and a back surface, and a thermal recording layer containing a dye precursor and a color developer on at least the front surface of the support, wherein the color developer contains one or more urea compounds represented by the following general formula (Chemical Formula 1) and one or more N,N'-diaryl urea compounds represented by the following general formula (Chemical Formula 3). 【Chemistry 1】 Here, R 1 represents the following general formula (Chemical Formula 2). 【Chemistry 2】 Here, R 2 represents a hydrogen atom or an alkyl group having 1 to 6 carbon atoms. 【Chemistry 3】 Here, R 3 represents a substituted or unsubstituted branched or alicyclic alkyl group having from 3 to 12 carbon atoms, a substituted or unsubstituted alkyl group having from 1 to 12 carbon atoms, a substituted or unsubstituted alkoxy group having from 1 to 12 carbon atoms, a substituted or unsubstituted aryl group having from 6 to 12 carbon atoms, or an aralkyl group having from 7 to 12 carbon atoms and substituted with a halogen atom. 3 may be the same or different. In the general formula (Chemical formula 3), the multiple substituents "-OSO 2 -R 3 " are at the same or different positions in each benzene ring.
2. 2. The heat-sensitive recording material according to claim 1, wherein the compound represented by the general formula (Chemical Formula 1) contains at least N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea.
3. 2. The heat-sensitive recording material according to claim 1, wherein the compound represented by the general formula (Chemical Formula 3) contains at least N,N'-di[3-(p-toluenesulfonyloxy)phenyl]urea.
4. The heat-sensitive recording material according to claim 1, wherein the compound represented by the general formula (Chemical Formula 1) contains at least N-3-(p-toluenesulfonyloxy)phenyl-N'-(p-toluenesulfonyl)urea, and the compound represented by the general formula (Chemical Formula 3) contains at least N,N'-di[3-(p-toluenesulfonyloxy)phenyl]urea.
Citation Information
Patent Citations
Thermal recording material
JP2011056894A
Thermal recording medium
JP6960562B2