Cake and method for producing cake

Incorporating carboxymethyl cellulose addresses the challenge of poor rise and stability in egg-free, milk-free cakes, achieving comparable texture and volume.

JP2024172018AInactive Publication Date: 2024-12-12NIPPON PAPER IND CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023089427
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Cakes without eggs and milk components face challenges in dough rise and stability, leading to poor volume and texture.

Method used

Incorporation of carboxymethyl cellulose (CMC) into cake recipes, specifically with defined viscosity, substitution degree, and particle size, to enhance dough stability and volume.

Benefits of technology

The cake achieves the same texture and flavor with a voluminous feel, even without eggs or milk, through the use of CMC, ensuring improved dough stability and volume.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024172018000003
    Figure 2024172018000003
  • Figure 2024172018000001
    Figure 2024172018000001
  • Figure 2024172018000002
    Figure 2024172018000002
Patent Text Reader

Abstract

To provide a cake that exhibits comparable texture and flavor profiles even when not containing egg or dairy components, and offers a substantial volume.SOLUTION: A cake contains saccharides, grain flour, soybean milk, and carboxymethyl cellulose.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a cake containing carboxymethyl cellulose and a method for producing a cake containing carboxymethyl cellulose. [Background technology]

[0002] In recent years, health consciousness has increased, and so-called plant-based foods, which use plant ingredients instead of animal ingredients, have come into the spotlight as a way to bring about healthier eating habits (e.g., Patent Document 1, etc.).

[0003] There is also a demand for plant-based cakes, a type of baked confectionery, that do not use milk, eggs, etc. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2023-56671 A Summary of the Invention [Problem to be solved by the invention]

[0005] The protein contained in egg whites has the property of easily foaming by trapping air (foaming ability), and the bubbles do not disappear easily (foam stability). In addition, the lecithin contained in egg yolks has the effect of promoting emulsification. Therefore, if the ingredients do not contain eggs, there are problems such as the dough not rising well and the risen dough lacking stability, resulting in a cake with less volume after baking.

[0006] Therefore, an object of the present invention is to provide a cake that has a voluminous feel and texture that is comparable to that of a cake containing no eggs or dairy ingredients, and a method for producing the cake. [Means for solving the problem]

[0007] As a result of extensive research into achieving this object, the present inventors have found that blending carboxymethylcellulose (CMC) is effective, and have completed the present invention.

[0008] The present invention provides the following: (1) A cake comprising sugar, cereal flour, soy milk, and carboxymethyl cellulose. (2) A cake as described in (1) above, characterized in that it does not contain eggs. (3) A cake according to (1) or (2), characterized in that it does not contain dairy ingredients. (4) The cake according to (1) or (2), wherein the carboxymethyl cellulose has a Brookfield viscosity (30 rpm / 25° C.) of 1 to 200 mPa s when dispersed in water at a solid content of 1% by mass. (5) The cake according to (1) or (2), wherein the carboxymethyl cellulose has a degree of carboxymethyl substitution in the range of 0.2 to 0.5. (6) The cake according to (1) or (2), wherein the carboxymethyl cellulose has an average particle size in the range of 10 to 70 μm. (7) The cake according to (1) or (2), wherein the amount of the carboxymethyl cellulose is 0.1 to 5 mass % in terms of solid content relative to the total amount of the raw materials. (8) A cake according to (1) or (2), characterized in that it is a pound cake. (9) A method for producing a cake, comprising: a mixing step of mixing ingredients including sugars, grain flours, soy milk, and powdered carboxymethyl cellulose; and a baking step of pouring the batter obtained in the mixing step into a mold and baking the batter. (10) The method for producing a cake according to (9), characterized in that the ingredients do not contain eggs. (11) The method for producing a cake according to (9) or (10), characterized in that the ingredients do not contain dairy components. (12) The method for producing a cake according to (9) or (10), characterized in that the cake is a pound cake. Effect of the Invention

[0009] According to the present invention, it is possible to provide a cake that is comparable in texture and flavor and has a voluminous feel even when it does not contain eggs or dairy components, and also to provide a method for producing this cake. [Brief description of the drawings]

[0010] [Figure 1] Photographs of cakes of Examples 1 to 3 and Comparative Example 1 (top: photograph from above, bottom: cross-sectional photograph). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The present invention will be described in detail below. In the present invention, "to" includes the end values. In other words, "X to Y" includes the values ​​X and Y at both ends.

[0012] (cake) The cake of the present invention comprises sugar, cereal flour, soy milk, and carboxymethyl cellulose.

[0013] (Sugars) The sugars used in the cake of the present invention are not particularly limited, and examples thereof include granulated sugar, white sugar, brown sugar, brown sugar, cane sugar, beet sugar, maple sugar, Wasanbon sugar, oligosaccharides, glucose, fructose, invert sugar, starch syrup, maltose, and lactose, and these can be used alone or in combination of two or more. The nature of the sugars is not particularly limited, and sugars in various forms such as powder and liquid can be used. In the present invention, the blending amount of sugars relative to the total amount of the ingredients of the cake is preferably 15 to 35% by mass, more preferably 20 to 30% by mass. These sugars may be used alone or in combination of two or more.

[0014] (cereal flour) The flour used in the cake of the present invention is not particularly limited, and examples thereof include flours such as wheat flour (weak flour, medium flour, semi-strong flour, strong flour, whole wheat flour, durum wheat flour, etc.), barley flour, soy flour, buckwheat flour, rye flour, rice flour, and corn flour; starches such as corn starch, potato starch, tapioca starch, sago starch, and processed starches obtained by subjecting these starches to physical or chemical processing alone or in combination. From the viewpoint of extensibility, it is preferable to use weak flour and starches, and it is more preferable to use weak flour. In the present invention, the amount of the flour to be blended with respect to the total amount of the raw materials of the cake is preferably 20 to 35% by mass, more preferably 25 to 30% by mass. These flours may be used alone or in combination of two or more types.

[0015] (Soy milk) In the present invention, soy milks refer to milky products obtained by soaking soybeans, red beans, or other beans in water, grinding them, heating them, and filtering them. More specifically, the above soy milks include 1) those obtained by soaking soybeans in water to swell them, grinding them, adding water, boiling them down, and filtering them to remove the okara, 2) those obtained by steaming soybeans, grinding them, filtering them to remove the okara, and 3) commercially available soy milks made from soybeans (so-called unadjusted soy milks). Other soy milks include those obtained by adjusting the unadjusted soy milks listed above to have an easy-to-drink taste and aroma (adjusted soy milks), and those obtained by adding fruit juice or other ingredients to unadjusted soy milk (soy milk beverages). There are no particular limitations on the soy milks used in the cake of the present invention, and any of unadjusted soy milks, adjusted soy milks, and soy milk beverages may be used. In the present invention, the amount of soy milks to be mixed with respect to the total amount of ingredients of the cake is preferably 10 to 30% by mass, more preferably 15 to 25% by mass. These soy milks may be used alone or in combination of two or more.

[0016] (Carboxymethylcellulose) Carboxymethylcellulose has a structure in which a part of the hydroxyl group in the glucose residue constituting cellulose is ether-bonded to a carboxymethyl group. Carboxymethylcellulose may take the form of a salt, and the carboxymethylcellulose used in the present invention also includes the salt of carboxymethylcellulose. Examples of the salt of carboxymethylcellulose include metal salts such as sodium carboxymethylcellulose.

[0017] (Degree of carboxymethyl substitution) The carboxymethyl cellulose used in the present invention preferably has a carboxymethyl substitution degree per anhydrous glucose unit of cellulose of 0.20 or more, more preferably 0.23 or more. If the carboxymethyl substitution degree is less than 0.20, it is difficult to disperse it uniformly in the cake dough when using a device with low stirring power such as a mixer, and it precipitates when added to the cake dough, and the desired thickening cannot be obtained. The upper limit of the carboxymethyl substitution degree is preferably 0.50 or less, more preferably 0.48 or less, and even more preferably 0.45 or less. If the carboxymethyl substitution degree exceeds 0.50, it is likely to dissolve in water or soy milk or other aqueous medium, and there is a risk of the dough becoming sticky in the container. Therefore, the carboxymethyl substitution degree is preferably in the range of 0.20 or more and 0.50 or less. The carboxymethyl substitution degree can be adjusted by controlling the amount of the carboxymethylating agent to be reacted, the amount of the mercerizing agent, the composition ratio of water to the organic solvent, etc.

[0018] In the present invention, the anhydroglucose unit means each anhydroglucose (glucose residue) constituting cellulose. The degree of carboxymethyl substitution (also called the degree of etherification) indicates the ratio of hydroxyl groups in the glucose residues constituting cellulose that are substituted with carboxymethyl ether groups (the number of carboxymethyl ether groups per glucose residue). The degree of carboxymethyl substitution may be abbreviated as DS.

[0019] The method for measuring the degree of carboxymethyl substitution is as follows: Weigh out approximately 2.0 g of the sample and place it in a 300 mL Erlenmeyer flask with a stopper. Add 100 mL of nitric acid methanol (a solution of 100 mL of concentrated nitric acid added to 1000 mL of methanol) and shake for 3 hours to convert the carboxymethylcellulose salt (CMC) to H-CMC (hydrogen-type carboxymethylcellulose). Weigh out 1.5 to 2.0 g of the bone-dry H-CMC and place it in a 300 mL Erlenmeyer flask with a stopper. Moisten the H-CMC with 15 mL of 80% methanol, add 100 mL of 0.1 N-NaOH, and shake at room temperature for 3 hours. Using phenolphthalein as an indicator, back-titrate the excess NaOH with 0.1 N-H2SO4, and calculate the degree of carboxymethyl substitution (DS value) using the following formula. A = [(100 × F'-0.1N-H2SO4 (mL) × F) × 0.1] / (bone dry mass of H-CMC (g)) Degree of carboxymethyl substitution = 0.162 x A / (1-0.058 x A) F': Factor of 0.1N-H2SO4 F: Factor of 0.1N NaOH.

[0020] (Crystallization degree of cellulose type I) The crystallinity of cellulose type I in the carboxymethyl cellulose used in the present invention is not particularly limited. The crystallinity of cellulose can be controlled by the concentration of the mercerizing agent, the temperature during treatment, and the degree of carboxymethylation. Since a high concentration of alkali is used in mercerization and carboxymethylation, the cellulose type I crystals are easily converted to type II, but the desired crystallinity can be maintained by adjusting the degree of modification, such as by adjusting the amount of alkali (mercerizing agent) used. The lower limit of the crystallinity of cellulose type I in the carboxymethyl cellulose used in the present invention is 0. The upper limit is not particularly limited. In reality, the upper limit is considered to be about 90%.

[0021] The method for measuring the crystallinity of cellulose type I of carboxymethyl cellulose is as follows: The sample is placed in a glass cell and measured using an X-ray diffraction measuring device (LabX XRD-6000, manufactured by Shimadzu Corporation). The degree of crystallinity is calculated using the method of Segal et al. The diffraction intensity at 2θ = 10° to 30° in the X-ray diffraction diagram is used as the baseline, and the degree of crystallinity is calculated from the diffraction intensity of the 002 plane at 2θ = 22.6° and the diffraction intensity of the amorphous part at 2θ = 18.5° using the following formula: Xc = (I002c - Ia) / I002c × 100 Xc = Crystallinity of cellulose type I (%) I002c: 2θ=22.6°, diffraction intensity of 002 plane Ia: 2θ=18.5°, diffraction intensity of the amorphous part.

[0022] (viscosity) The viscosity of the carboxymethyl cellulose used in the present invention is not particularly limited, but from the viewpoint of the handleability of the dough, the B-type viscosity (conditions: rotation speed 30 rpm, temperature 25°C) when made into an aqueous dispersion with a solid content of 1% by mass is preferably 1 to 400 mPa·s, more preferably 5 to 300 mPa·s, and even more preferably 10 to 200 mPa·s. If the B-type viscosity is too higher than the above upper limit, there is a risk that the dough will stick to the container, and if it is too lower than the above lower limit, there is a risk that the moldability will decrease.

[0023] (Average particle size) In the present invention, the carboxymethylcellulose blended in the cake is preferably in the form of a powder or fine powder, and has an average particle size of 10 to 70 μm, more preferably 12.5 to 65 μm, and even more preferably 15 to 60 μm, under conditions of a moisture content of less than 10% by mass. It is presumed that the average particle size within the above range keeps the fiber length and fiber diameter of the carboxymethylcellulose within a certain range without becoming too thin, and is likely to exhibit thickening (gelation) while having good dispersibility. If the average particle size is too large than the upper limit, there is a risk of deterioration in texture, and if it is too small than the lower limit, the powder is likely to fly up, making it difficult to handle.

[0024] The average particle size in the present invention is the particle size that includes 50% of the particles when calculated from the minimum value in the volume-based particle size distribution. The particle size distribution can be measured using a laser diffraction / scattering particle size distribution analyzer.

[0025] (Manufacturing method of carboxymethyl cellulose) Carboxymethylcellulose can generally be produced by treating cellulose with an alkali (mercerization), and then reacting the resulting mercerized cellulose (also called alkali cellulose) with a carboxymethylating agent (also called etherifying agent). Common methods for producing carboxymethylcellulose include the aqueous method, in which both mercerization and carboxymethylation are carried out using water as a solvent, and the solvent method, in which both mercerization and carboxymethylation are carried out in a solvent mainly composed of an organic solvent. From the viewpoint of the degree of carboxymethyl substitution and the degree of crystallinity, the carboxymethylcellulose used in the present invention is preferably produced, for example, by carrying out mercerization in a solvent mainly composed of water or in a mixed solvent of water and an organic solvent, and then carrying out carboxymethylation in a mixed solvent of water and an organic solvent.

[0026] (cellulose) In this specification, cellulose refers to a polysaccharide having a structure in which D-glucopyranose (also simply called "glucose residue" or "anhydroglucose") is linked together through β-1,4 bonds. Cellulose is generally classified into native cellulose, regenerated cellulose, fine cellulose, microcrystalline cellulose in which the amorphous region is removed, etc., based on the origin, production method, etc. In the present invention, any of these celluloses can be used as the raw material for mercerized cellulose.

[0027] Examples of natural cellulose include bleached pulp or unbleached pulp (bleached wood pulp or unbleached wood pulp), linters, refined linters, and cellulose produced by microorganisms such as acetic acid bacteria. The raw material for bleached pulp or unbleached pulp is not particularly limited, and examples thereof include wood, cotton, straw, bamboo, hemp, jute, kenaf, etc. The method for producing bleached pulp or unbleached pulp is also not particularly limited, and may be a mechanical method, a chemical method, or a method that is an intermediate combination of the two. Examples of bleached or unbleached pulp classified according to the production method include mechanical pulp (thermomechanical pulp (TMP), groundwood pulp), chemical pulp (sulfite pulp such as softwood unbleached sulfite pulp (NUSP) and softwood bleached sulfite pulp (NBSP), and kraft pulp such as softwood unbleached kraft pulp (NUKP), softwood bleached kraft pulp (NBKP), hardwood unbleached kraft pulp (LUKP), and hardwood bleached kraft pulp (LBKP)). Furthermore, in addition to papermaking pulp, dissolving pulp may be used. Dissolving pulp is chemically refined pulp that is mainly used by dissolving it in chemicals, and is the main raw material for artificial fibers, cellophane, etc.

[0028] Examples of regenerated cellulose include cellulose dissolved in some solvent such as cuprammonium solution, cellulose xanthate solution, morpholine derivative, etc., and spun again. Examples of fine cellulose include those obtained by depolymerizing the above-mentioned natural cellulose and regenerated cellulose and other cellulose-based materials (e.g., acid hydrolysis, alkali hydrolysis, enzymatic decomposition, explosive crushing, vibration ball mill treatment, etc.), and those obtained by mechanically treating the above-mentioned cellulose-based materials.

[0029] (Mercerization) Mercerized cellulose (also called alkali cellulose) is obtained by adding a mercerizing agent (alkali) to the above-mentioned cellulose as a raw material. By adjusting the composition of the solvent in the mercerization reaction and the composition of the solvent in the carboxymethylation reaction, it is possible to economically obtain carboxymethyl cellulose that has both a specific degree of carboxymethyl substitution and the crystallinity of cellulose type I.

[0030] For example, by using water as the main solvent in the mercerization reaction and using a mixed solvent of an organic solvent and water in the subsequent carboxymethylation, it is possible to obtain carboxymethylcellulose having a specific degree of carboxymethyl substitution and a crystallinity of 50% or more of cellulose type I. The term "water-based solvent" refers to a solvent containing water at a ratio of more than 50% by mass. The water content in the water-based solvent is preferably 55% by mass or more, more preferably 60% by mass or more, more preferably 70% by mass or more, more preferably 80% by mass or more, even more preferably 90% by mass or more, and even more preferably 95% by mass or more. Particularly preferably, the water-based solvent is 100% by mass (i.e., water). The higher the water content during mercerization, the more advantageously carboxymethyl groups are introduced into cellulose more uniformly. Examples of solvents other than water (used mixed with water) in the water-based solvent include organic solvents used as a solvent during the subsequent carboxymethylation. Examples of such solvents include alcohols such as methanol, ethanol, N-propyl alcohol, isopropyl alcohol, N-butanol, isobutanol, and tertiary butanol, ketones such as acetone, diethyl ketone, and methyl ethyl ketone, as well as dioxane, diethyl ether, benzene, and dichloromethane, and these can be added alone or in a mixture of two or more kinds to water in an amount of less than 50% by mass to be used as a solvent for mercerization. The organic solvent in the solvent mainly composed of water is preferably 45% by mass or less, more preferably 40% by mass or less, more preferably 30% by mass or less, more preferably 20% by mass or less, more preferably 10% by mass or less, more preferably 5% by mass or less, and more preferably 0% by mass.

[0031] Examples of the mercerizing agent include alkali metal hydroxides such as lithium hydroxide, sodium hydroxide, and potassium hydroxide, and any one or more of these can be used in combination. The mercerizing agent is not limited to these, but these alkali metal hydroxides can be added to the reactor as an aqueous solution of, for example, 1 to 60 mass %, preferably 2 to 45 mass %, and more preferably 3 to 25 mass %.

[0032] The amount of the mercerizing agent used is not particularly limited, but is preferably an amount that allows the degree of carboxymethyl substitution in the carboxymethyl cellulose to be 0.20 or more. In one embodiment, the amount is preferably 0.1 mol or more and 2.5 mol or less, more preferably 0.3 mol or more and 2.0 mol or less, and even more preferably 0.4 mol or more and 1.5 mol or less, per 100 g (bone dry) of cellulose.

[0033] The amount of the solvent during mercerization is not particularly limited as long as it allows stirring and mixing of the raw materials, but is preferably 1.5 to 20 times by mass, more preferably 2 to 10 times by mass, relative to the cellulose raw material.

[0034] The mercerization treatment is carried out by mixing the raw material (cellulose) with a solvent, adjusting the temperature of the reactor to 0 to 70°C, preferably 10 to 60°C, more preferably 10 to 40°C, adding an aqueous solution of a mercerizing agent, and stirring for 15 minutes to 8 hours, preferably 30 minutes to 7 hours, more preferably 30 minutes to 3 hours, to obtain mercerized cellulose (alkali cellulose).

[0035] The pH during mercerization is preferably 9 or more, which allows the mercerization reaction to proceed. The pH is more preferably 11 or more, further preferably 12 or more, and may be 13 or more. There is no particular upper limit to the pH.

[0036] The mercerization can be carried out using a reactor capable of mixing and stirring the above-mentioned components while controlling the temperature, and various reactors conventionally used for mercerization reactions can be used. For example, a batch-type stirring device having two shafts for stirring and mixing the above-mentioned components is preferred from the viewpoints of both uniform mixing ability and productivity.

[0037] (Carboxymethylation) Carboxymethyl cellulose is obtained by adding a carboxymethylating agent (also called an etherifying agent) to mercerized cellulose.

[0038] Examples of the carboxymethylating agent include monochloroacetic acid, sodium monochloroacetate, methyl monochloroacetate, ethyl monochloroacetate, isopropyl monochloroacetate, etc. Among these, monochloroacetic acid or sodium monochloroacetate is preferred in terms of availability of the raw material.

[0039] The amount of the carboxymethylating agent used is not particularly limited, but in one embodiment, from the viewpoint of effective utilization, it is preferable to add in the range of 0.5 to 1.5 mol per anhydrous glucose unit of cellulose. The lower limit of the above range is more preferably 0.6 mol or more, even more preferably 0.7 mol or more, and the upper limit is more preferably 1.3 mol or less, even more preferably 1.1 mol or less. The carboxymethylating agent can be added to the reactor as, for example, a 5 to 80 mass % aqueous solution, more preferably 30 to 60 mass %, but is not limited thereto, or can be added in a powder state without dissolving.

[0040] The molar ratio of the mercerizing agent to the carboxymethylating agent (mercerizing agent / carboxymethylating agent) is generally 0.90 to 2.45 when monochloroacetic acid or sodium monochloroacetate is used as the carboxymethylating agent. The reason is that if it is less than 0.90, the carboxymethylation reaction may be insufficient, and unreacted monochloroacetic acid or sodium monochloroacetate may remain and be wasted, and if it exceeds 2.45, a side reaction between the excess mercerizing agent and monochloroacetic acid or sodium monochloroacetate may proceed, resulting in the production of an alkali metal glycolate, which may be uneconomical.

[0041] The concentration of the cellulose raw material in the carboxymethylation reaction is not particularly limited, but is preferably 1 to 40% (w / v) from the viewpoint of increasing the effective utilization rate of the carboxymethylating agent. The effective utilization rate of the carboxymethylating agent refers to the ratio of the carboxymethyl groups introduced into cellulose among the carboxymethyl groups in the carboxymethylating agent.

[0042] Simultaneously with the addition of the carboxymethylating agent, or before or immediately after the addition of the carboxymethylating agent, an organic solvent or an aqueous solution of an organic solvent is appropriately added to the reactor, or the organic solvent other than water used in the mercerization treatment is appropriately reduced by reducing pressure or the like to form a mixed solvent of water and an organic solvent, and the carboxymethylation reaction is allowed to proceed in this mixed solvent of water and an organic solvent. The timing of the addition or reduction of the organic solvent may be any time between the end of the mercerization reaction and immediately after the addition of the carboxymethylating agent, and is not particularly limited, but is preferably within 30 minutes before or after the addition of the carboxymethylating agent, for example.

[0043] Examples of the organic solvent include alcohols such as methanol, ethanol, N-propyl alcohol, isopropyl alcohol, N-butanol, isobutanol, and tertiary butanol, ketones such as acetone, diethyl ketone, and methyl ethyl ketone, as well as dioxane, diethyl ether, benzene, and dichloromethane, and these can be used alone or in a mixture of two or more kinds as a solvent for carboxymethylation by adding them to water. Among these, monohydric alcohols having 1 to 4 carbon atoms are preferred because of their excellent compatibility with water, and monohydric alcohols having 1 to 3 carbon atoms are more preferred.

[0044] The ratio of the organic solvent in the mixed solvent during carboxymethylation is preferably 20% by mass or more, more preferably 30% by mass or more, even more preferably 40% by mass or more, even more preferably 45% by mass or more, and particularly preferably 50% by mass or more, based on the total of water and organic solvent. The higher the ratio of the organic solvent, the more likely it is that uniform carboxymethyl group substitution will occur, and the more advantageous it is that carboxymethyl cellulose with stable quality can be obtained. The upper limit of the ratio of the organic solvent is not limited, and may be, for example, 99% by mass or less. Considering the cost of the organic solvent to be added, it is preferably 90% by mass or less, more preferably 85% by mass or less, even more preferably 80% by mass or less, and even more preferably 70% by mass or less.

[0045] When the crystallinity of carboxymethylcellulose is to be a high value such as 50% or more, the reaction medium during carboxymethylation (a mixed solvent of water and an organic solvent, etc., not containing cellulose) preferably has a lower proportion of water (in other words, a higher proportion of organic solvent) than the reaction medium during mercerization. By satisfying this range, the crystallinity of the obtained carboxymethylcellulose is easily maintained. In addition, when the reaction medium during carboxymethylation has a lower proportion of water (a higher proportion of organic solvent) than the reaction medium during mercerization, when transferring from the mercerization reaction to the carboxymethylation reaction, a mixed solvent for the carboxymethylation reaction can be formed by a simple means of adding a desired amount of organic solvent to the reaction system after the mercerization reaction is completed.

[0046] A mixed solvent of water and an organic solvent is prepared, and a carboxymethylating agent is added to the mercerized cellulose, followed by stirring for 15 minutes to 4 hours, preferably 15 minutes to 1 hour, while maintaining a constant temperature, preferably in the range of 10 to 40°C. The liquid containing the mercerized cellulose and the carboxymethylating agent are preferably mixed in several batches or by dropwise addition, in order to prevent the reaction mixture from becoming too hot. After adding the carboxymethylating agent and stirring for a certain period of time, the temperature is raised if necessary to a reaction temperature of 30 to 90°C, preferably 40 to 90°C, more preferably 60 to 80°C, and an etherification (carboxymethylation) reaction is carried out for 30 minutes to 10 hours, preferably 1 hour to 4 hours, to obtain carboxymethyl cellulose. By raising the temperature during the carboxymethylation reaction, the etherification reaction can be advantageously carried out efficiently in a short time.

[0047] In the carboxymethylation, the reactor used in the mercerization may be used as it is, or a separate reactor capable of mixing and stirring the above-mentioned components while controlling the temperature may be used.

[0048] After the reaction is completed, the remaining alkali metal salt may be neutralized with a mineral acid or an organic acid. If necessary, by-products such as inorganic salts and organic acid salts may be removed by washing with aqueous methanol, and the product may be dried, pulverized, and classified to obtain carboxymethyl cellulose or a salt thereof. Examples of the apparatus used in dry pulverization include impact mills such as hammer mills and pin mills, media mills such as ball mills and tower mills, and jet mills. Examples of the apparatus used in wet pulverization include homogenizers, mass colloiders, pearl mills, and the like.

[0049] In the present invention, the amount of carboxymethylcellulose is preferably 0.1 to 5 mass% in terms of solid content relative to the total amount of the raw materials for the cake, more preferably 0.3 to 4.5 mass%, further preferably 0.5 to 4.0 mass%, and particularly preferably 0.7 to 3.5 mass%. When the amount of carboxymethylcellulose is within the above range, favorable workability and moldability are achieved. If the amount is more than the upper limit, the dough may be sticky to the container, and if it is less than the lower limit, the moldability may be reduced.

[0050] (eggs) The cake of the present invention may be configured to not contain eggs, and from the viewpoint of plant-based foods, it is preferable that the cake does not contain eggs. In the present application, eggs include whole eggs, egg yolks, and egg whites. The eggs of the present application may be either cracked eggs or liquid eggs, and may or may not be pretreated by sterilization, freezing, salting, sweetening, or the like.

[0051] (milk ingredient) The cake of the present invention may be configured to not contain dairy components, and from the viewpoint of plant-based foods, it is preferable that the cake does not contain dairy components. In the present application, dairy components refer to components derived from milk and dairy ingredients themselves, such as cow's milk, skim milk, skim milk powder, whole milk powder, sweetened milk powder, etc.

[0052] (Oils and fats) Fats and oils can be used in the cake of the present invention. There is no particular limitation on the type of fats and oils, and examples thereof include vegetable fats and oils such as corn oil, rapeseed oil, soybean oil, coconut oil, palm oil, etc., animal fats and oils such as lard, beef tallow, fish oil, milk fat, and hardened oils and interesterified oils thereof. In the present invention, from the viewpoint of plant-based foods, it is preferable to use vegetable fats and oils such as rapeseed oil, soybean oil, palm oil, corn oil, etc., or hardened oils and interesterified oils thereof. The blending amount of fats and oils with respect to the total amount of the raw materials of the cake is preferably 15 to 35% by mass, more preferably 20 to 30% by mass. These fats and oils may be used alone or in combination of two or more kinds.

[0053] The cake of the present invention may contain a leavening agent, an emulsifier, etc. as appropriate, so long as the effect of the present invention is not impaired.

[0054] (Leaving agent) In the present invention, the leavening agent refers to a substance that makes the cake dough porous and expands it, and examples of such leavening agents include ammonium bicarbonate, sodium bicarbonate, and baking powder. When a leavening agent is used in the cake of the present invention, the amount of the leavening agent is preferably 1.5% by mass or less, and more preferably 1.0% by mass or less, based on the total amount of the ingredients of the cake. These leavening agents may be used alone or in combination of two or more kinds.

[0055] (emulsifier) Examples of emulsifiers include emulsifiers used in foods, such as glycerin fatty acid esters, sucrose fatty acid esters, sorbitan fatty acid esters, propylene glycol fatty acid esters, plant sterols, lecithin, sodium stearoyl lactate, calcium stearoyl lactate, polysorbate, and Quillaja saponin. When an emulsifier is used in the cake of the present invention, the amount of the emulsifier is preferably 1.0% by mass or less, more preferably 0.5% by mass or less, based on the total amount of the ingredients of the cake. These emulsifiers may be used alone or in combination of two or more.

[0056] The cake of the present invention may contain, as necessary, suitable additives such as salt, thickening polysaccharides such as xanthan gum and carrageenan, other thickeners, flavorings, coloring agents, emulsion stabilizers, and the like.

[0057] (Cake manufacturing method) The method for producing a cake of the present invention includes a mixing step in which essential raw materials, namely sugars, cereal flours, soy milks, and powdered carboxymethyl cellulose, are mixed with raw materials that are used as necessary, such as a leavening agent, salt, fats and oils, and an emulsifier, and a baking step in which the batter obtained in the mixing step is poured into a mold and then baked.

[0058] Since the cake of the present invention contains carboxymethylcellulose, it has a texture and flavor comparable to those of cakes that do not contain eggs or dairy ingredients, and has a voluminous feel.

[0059] Examples of the cake of the present invention include sponge cake, roll cake, hot cake, bouquet, Baumkuchen, pound cake, snack cake, and the like. EXAMPLES

[0060] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these. In addition, unless the method of measurement / calculation of each value in each example is specifically stated, it is measured / calculated by the method described in the specification.

[0061] (viscosity) The viscosities of CMC1 to 3 used in the examples were measured as follows. First, CMC1 to 3 were each added to water to prepare an aqueous dispersion of carboxymethyl cellulose with a solid content of 1% by mass. The obtained aqueous dispersion of 1% by mass of solid content was stirred for 3 hours using a stirrer at a rotation speed of 600 rpm and a temperature of 25°C. Thereafter, the viscosity after 3 minutes was measured using a B-type viscometer (manufactured by Toki Sangyo Co., Ltd.) at a rotation speed of 30 rpm and a temperature of 25°C in accordance with the method of JIS Z 8803.

[0062] (Average particle size) The average particle sizes of CMC1 to 3 used in the examples were determined from the particle size distribution based on the volume average particle size.

[0063] The particle size distribution was measured using a laser diffraction / scattering particle size distribution analyzer (Mastersizer 2000E, manufactured by Spectris Co., Ltd.). For the measurement, the sample was dispersed in methanol and then subjected to ultrasonic treatment for at least one minute.

[0064] (Production Example 1) A solution of 68 parts of sodium hydroxide dissolved in a mixed solvent of 30 parts of water and 70 parts of isopropanol (IPA) was added to a twin-axis kneader with the rotation speed adjusted to 100 rpm, and 100 parts of hardwood pulp (LBKP, manufactured by Nippon Paper Industries Co., Ltd.) was added based on the dry mass when dried at 100°C for 60 minutes. The mixture was stirred and mixed at 30°C for 90 minutes to prepare mercerized cellulose. 230 parts of IPA and 80 parts of monochloroacetic acid were further added while stirring, and after stirring for 30 minutes, the mixture was heated to 70°C and allowed to carry out a carboxymethylation reaction for 90 minutes. The concentration of IPA in the reaction medium during the carboxymethylation reaction was 91%. After the reaction was completed, the mixture was neutralized with acetic acid to a pH of about 7, deliquored, dried, and pulverized to obtain a fine powder of carboxymethylcellulose sodium salt (CMC1) with a carboxymethyl substitution degree (DS) of 0.28, a crystallinity of cellulose type I of 0%, an average particle size of 20 μm, a 1% viscosity of 80 mPa·s, and a moisture content of less than 10%.

[0065] (Production Example 2) A powder of carboxymethylcellulose sodium salt (CMC2) was obtained in the same manner as in Production Example 1, except that the degree of pulverization was changed. The powder had a carboxymethyl substitution degree (DS) of 0.28, a crystallinity of cellulose type I of 0%, an average particle size of 50 μm, a 1% viscosity of 80 mPa s, and a moisture content of less than 10%.

[0066] (Production Example 3) A solution of 20 parts of sodium hydroxide in 100 parts of water was added to a twin-shaft kneader with the rotation speed adjusted to 100 rpm, and 100 parts of hardwood pulp (LBKP, manufactured by Nippon Paper Industries Co., Ltd.) was added based on the dry mass when it was dried at 100°C for 60 minutes. The mixture was stirred and mixed at 30°C for 90 minutes to prepare mercerized cellulose. 230 parts of IPA and 60 parts of sodium monochloroacetate were further added while stirring, and after stirring for 30 minutes, the mixture was heated to 70°C and carboxymethylation reaction was carried out for 90 minutes. The concentration of IPA in the reaction medium during the carboxymethylation reaction was 70%. After the reaction was completed, the mixture was neutralized with acetic acid to about pH 7, deliquored, dried, and pulverized to obtain a powder of carboxymethylcellulose sodium salt (CMC3) with a carboxymethyl substitution degree (DS) of 0.32, a crystallinity of cellulose I type 71%, an average particle size of 50 μm, a 1% viscosity of 30 mPa·s, and a moisture content of less than 10%.

[0067] (Cake making) Cakes of Examples 1 to 3 and Comparative Example 1 were produced with the composition shown in Table 1. Specifically, powders, i.e., weak flour, beet sugar, baking powder, salt, and CMC1 to 3 or modified starch (phosphate cross-linked starch) were sifted into a bowl. Next, margarine (derived from vegetable oils and fats) and an emulsifier, which had been previously heated and melted, were added to the bowl and thoroughly stirred. Furthermore, unsweetened soy milk was added to the bowl and thoroughly stirred to obtain a cake batter. The obtained cake batter was poured into a pound cake mold and baked at a temperature of 160°C for 50 minutes in an oven preheated to 160°C to produce a cake.

[0068] [Table 1]

[0069] (Sensory evaluation) A sensory evaluation was carried out by 14 panelists on the items of appearance, smell, taste, texture, and overall deliciousness of the cakes obtained in the Examples and Comparative Examples, using a 5-point scale (5 points to 1 point). A score equivalent to the cake of Comparative Example 1 was given as 3 points, and the cakes of Examples 1 to 3 were scored based on this. The evaluation criteria are shown below. The average scores were also calculated and are shown in Table 2. 5 points: Better than Comparative Example 1 4 points: slightly better than Comparative Example 1 3 points: equivalent to Comparative Example 1 2 points: slightly worse than Comparative Example 1 1 point: Worse than Comparative Example 1

[0070] [Table 2]

[0071] From Table 2, it can be seen that the cakes containing CMC in Examples 1 to 3 had excellent results, being equal to or better than the cake in Comparative Example 1, which did not contain CMC, in all items of the sensory evaluation. In particular, Examples 2 and 3, which used CMC2 and CMC3, had better results than Comparative Example 1 in all items.

[0072] Fig. 1 shows photographs of the cakes of Examples 1 to 3 and Comparative Example 1. The top photograph is a photograph of the cake taken from above, and the bottom photograph is a cross-sectional photograph of the cake. Fig. 1 shows that the cakes containing CMC of Examples 1 to 3 have a raised center and increased volume compared to the cake of Comparative Example 1, which does not contain CMC.

[0073] From the above, it was found that cakes containing sugars, cereal flours, soy milks, and carboxymethylcellulose had superior flavor and texture, and also had a volume-increasing effect, compared to cakes in which processed starch was used instead of carboxymethylcellulose.

Claims

1. A cake comprising sugar, cereal flour, soy milk, and carboxymethyl cellulose.

2. 2. The cake of claim 1, which does not contain eggs.

3. 3. A cake according to claim 1 or 2, characterized in that it does not contain any dairy ingredients.

4. 3. The cake according to claim 1, wherein the carboxymethyl cellulose has a Brookfield viscosity (30 rpm / 25° C.) of 1 to 200 mPa·s when dispersed in water with a solid content of 1% by mass.

5. 3. The cake according to claim 1, wherein the carboxymethyl cellulose has a degree of carboxymethyl substitution in the range of 0.2 to 0.

5.

6. 3. The cake according to claim 1, wherein the carboxymethyl cellulose has an average particle size in the range of 10 to 70 μm.

7. 3. The cake according to claim 1, wherein the amount of the carboxymethyl cellulose relative to the total amount of the raw materials is 0.1 to 5 mass % in terms of solid content.

8. 3. The cake according to claim 1 or 2, which is a pound cake.

9. A mixing step of mixing raw materials including sugars, grain flours, soy milk, and powdered carboxymethyl cellulose; and a baking step of pouring the batter obtained in the mixing step into a mold and baking the mixture.

10. The method for producing a cake according to claim 9, characterized in that the ingredients do not contain eggs.

11. The method for producing a cake according to claim 9 or 10, characterized in that the raw materials do not contain dairy ingredients.

12. The method for producing a cake according to claim 9 or 10, characterized in that the cake is a pound cake.

Citation Information