tea bag
The tea bag uses a water-swellable material with differential expansion to manage tea component extraction, ensuring optimal flavor and aroma by blocking further water flow after a set time, addressing the issue of flavor loss in traditional tea bags.
Patent Information
- Application Number
- JP2023520174
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-28
- Filing Date
- 2021-09-28
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2041-09-28
AI Technical Summary
Existing tea bags allow tea components to seep into hot water for an indefinite period, leading to a loss of flavor and aroma over time, resulting in a bitter taste.
A tea bag made from a water-swellable material that expands differently in different directions when exposed to water, allowing controlled extraction of tea components for a predetermined time before blocking further water flow.
Maintains optimal flavor and aroma by controlling the extraction period, preventing unwanted tea components from dissolving for too long, thus enhancing the tea-drinking experience.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a tea bag, and more particularly to a tea bag that allows tea ingredients to be extracted for a specific period of time so that a user can enjoy the optimal taste and aroma. [Background technology]
[0002] Generally, a typical tea bag is composed of a packaging tea bag that contains a certain amount of tea ingredients such as various tea leaves or extracts, such as powdered regular coffee, green tea, Polygonatum odoratum tea, and black tea, a string connected to the tea bag so that the tea bag can be put into or taken out of a container containing water, and a tag connected to the tea bag string to function as a handle so that the tea bag string can be pulled.
[0003] When such a tea bag is placed in a container containing hot water, the tea ingredients will seep into the hot water and the user will drink the solution containing the tea ingredients. Here, the taste and aroma of the tea depend on how long it takes for the contents of the tea bag to seep into the hot water. If the tea bag is allowed to seep for more than a certain amount of time, the tea will taste bitter and lose its aroma, making it impossible to enjoy the best taste and aroma of the tea contained in the tea bag.
[0004] In order to solve this problem, the applicant proposed in Korean Patent Publication No. 10-2022-0043888 a tea bag including a tea bag containing tea ingredients inside so that tea can be easily drunk, characterized in that the tea bag is equipped with a water-expanding material that expands to seal the tea ingredients contained inside so that they are not released to the outside when the tea bag is left in water for a certain period of time.
[0005] The present application is a more specific improvement over Applicant's earlier application.
[0006] As a related patent document, WO2017 / 137399 discloses that a tea bag folded into a disk or circle expands when it absorbs water. However, this patent does not disclose the structure and function of preventing water absorption after a certain time has passed. Korean Patent Publication No. 10-2019-0127978 discloses a cellulose nonwoven fabric that swells with water, but the difference in pore size is already determined when the fiber is manufactured, and does not disclose the structure and function of initially absorbing water and blocking water penetration after a certain time has passed. Japanese Patent Publication No. 2009-114569 discloses a mesh that expands when it absorbs water. However, this patent does not disclose the mesh size decreasing when it absorbs water. Summary of the Invention [Problem to be solved by the invention]
[0007] Therefore, the present invention aims to provide a tea bag that is made of a water-swelling material and that can preserve the inherent flavor and aroma of tea by blocking the flow of water through the tea bag after a predetermined time has passed since tea is immersed in water and exposed to the water, thereby maintaining the inherent flavor and aroma of tea. [Means for solving the problem]
[0008] In order to achieve the above-mentioned object, the present invention provides a tea bag containing tea therein, the tea bag being made of a water-expandable material that, when in contact with water, has a greater expansion rate in a first direction than in a second direction perpendicular to the first direction, and the water-expandable material has respective expansion rates such that, after a predetermined time has elapsed, the portion in the first direction expands more than the portion in the second direction to impede the flow of water.
[0009] The water-swellable material may be a fiber, the first direction may be a thickness (machine) direction, and the second direction may be a length (transverse) direction.
[0010] The present invention also provides a tea bag containing tea therein, the tea bag being made of a water-swelling material that, when in contact with water, has a contraction rate in a second direction greater than a contraction rate in a first direction perpendicular to the second direction, and the water-swelling material has respective contraction rates such that, after a predetermined time has elapsed, the portion in the second direction contracts more than the portion in the first direction, thereby impeding the flow of water.
[0011] The water-swellable material may be a fiber, the first direction may be a thickness (machine) direction, and the second direction may be a length (transverse) direction.
[0012] The present invention also provides a tea bag containing tea therein, the tea bag having a composite structure consisting of one or more lattice-shaped partitions and a water-expandable material arranged in the spaces between the partitions, the partitions each having a line in the horizontal direction, extending generally parallel to one another, and each having a predetermined interval in the vertical direction, and the partitions each having a line in the vertical direction, extending generally parallel to one another, and each having a predetermined interval in the horizontal direction, the partitions being made of a material that does not expand or contract when in contact with water and does not change in shape or structure.
[0013] The water-swellable material may comprise a fiber that swells when in contact with water.
[0014] The water-swellable material may be formed by stitching a material which, when in contact with water, expands in a first direction greater than it expands in a second direction perpendicular to the first direction, or by stitching a material which, when in contact with water, contracts in a second direction greater than it contracts in a first direction perpendicular to the second direction.
[0015] The present invention also provides a tea bag containing tea therein, the tea bag including a water-expanding material that is deformed by plastic processing to allow water to flow and that prevents water from flowing by restoring to its original shape when in contact with water for a predetermined period of time or more.
[0016] The present invention also provides a tea bag containing tea therein, the tea bag including a water-swelling material, the water-swelling material having a multi-layer structure in which a core is formed from a material having a low expansion rate due to water, and at least one outer periphery having a high expansion rate is formed on the outer periphery surrounding the core.
[0017] The present invention also provides a tea bag containing tea therein, the tea bag having a composite structure in which a water-swelling substance is layered or coated on all or part of a fabric material through which water can freely flow, the water-swelling substance having a structure in which, when contacted with water, the expansion rate in a first direction is greater than the expansion rate in a second direction perpendicular to the first direction, or a structure in which, when contacted with water, the contraction rate in the second direction is greater than the contraction rate in the first direction perpendicular to the second direction.
[0018] The present invention also provides a tea bag containing tea therein, the tea bag having a composite structure in which a water-expanding substance is layered or coated on all or part of a fabric material through which water can freely flow, the water-expanding substance having a structure in which, when contacted with water, the expansion rate in a first direction, i.e., the thickness direction, is greater than the expansion rate in a second direction perpendicular to the first direction, or a structure in which, when contacted with water, the contraction rate in the second direction, i.e., the longitudinal direction, is greater than the contraction rate in the first direction perpendicular to the second direction.
[0019] The present invention also provides a tea bag containing tea therein, the tea bag including a water-expanding substance, the water-expanding substance having a multi-layer structure in which, when in contact with water, a second portion expands more than a first portion after a predetermined time has elapsed, thereby impeding the flow of water, the first portion forming a core of the water-expanding substance, and the second portion forming an outer periphery surrounding the core.
[0020] The present invention also provides a tea bag containing tea therein, the tea bag including a water-expanding substance, the water-expanding substance having a multi-layer structure in which, when contacted with water, a first portion shrinks more than a second portion after a predetermined time has elapsed, thereby reducing the cross-sectional area of the passage through which the water passes and impeding the flow of water, the first portion forming a core of the water-expanding substance, and the second portion forming an outer periphery surrounding the core portion.
[0021] The water-swellable material may include a fibrous material.
[0022] The outer periphery formed by the second portion may have a structure of two or more layers. Effect of the Invention
[0023] The present invention has the effect of satisfying various consumer preferences and improving marketability by allowing the user to brew tea for a certain period of time so that the user can enjoy the optimal taste and aroma. [Brief description of the drawings]
[0024] [Figure 1] FIG. 2 is a diagram for explaining the structure and principle of the water-swelling material that characterizes the tea bag of the present invention in terms of expansion rate. [Diagram 2] FIG. 2 is a diagram showing the expansion process of a fabric woven with warp and weft yarns when exposed to water based on the principle of FIG. 1. [Diagram 3] FIG. 2 is a diagram for explaining the structure and principle of the water-swelling material that characterizes the tea bag of the present invention in terms of shrinkage rate. [Figure 4] FIG. 4 is a diagram showing the shrinkage process of a fabric woven with warp and weft yarns when exposed to water based on the principle of FIG. 3. [Diagram 5] FIG. 1 shows an embodiment of a tea bag containing a water-expandable material of the present invention. [Figure 6] FIG. 2 shows another embodiment of a tea bag containing a water-expandable material of the present invention. [Figure 7] FIG. 2 shows yet another embodiment of a tea bag containing a water-swellable material of the present invention. [Figure 8] FIG. 8 is a diagram showing yet another embodiment of a tea bag containing a water-swellable substance according to the present invention, using the principle of FIG. [Figure 9] FIG. 2 shows yet another embodiment of a tea bag containing a water-swellable material of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] The structure and principle of the water-swellable material 10, which is a feature of the tea bag 1 of the present invention, will be described below. The water-swellable material 10 will be described as being made of fiber as a representative example, but it should be noted that the material is not necessarily limited to fiber.
[0026] [Mode for carrying out the invention]
[0027] The objects and effects of the present invention, as well as the technical configuration for achieving the same, will become apparent from the following detailed description of the embodiments based on the accompanying drawings. In the description of the present invention, if it is determined that the detailed description of known functions or configurations may unnecessarily obscure the gist of the present invention, the detailed description will be omitted.
[0028] Throughout the specification, when a part "includes" a certain element, this does not mean excluding other elements, but means that other elements may be further included, unless otherwise specified. Meanwhile, in the embodiments of the present invention, each element, functional block, or means may be composed of one or more sub-elements.
[0029] First, the structure and principle of the water-swelling material 10 that characterizes the tea bag 1 of the present invention will be described. Although the water-swelling material 10 will be described as a representative example of fiber, it should be noted that the material is not necessarily limited to fiber.
[0030] FIG. 1a shows a portion of a fiber having an initial length Lo and an initial thickness Do.
[0031] If the expansion rate of the fiber in the longitudinal direction is α, the length L of the fiber after a certain time (t) is L = L O (1+αΔt) (α>0).
[0032] Fiber length was excluded here, since temperature, in addition to time, acts as an important variable, but is considered to be a factor that equally affects the change in length and thickness.
[0033] Next, if the expansion rate of the fiber in the thickness direction is β, the fiber thickness D after a certain time (t) is D = D O (1+βΔt) (β>0).
[0034] If the expansion coefficient α in the longitudinal direction and the expansion coefficient β in the thickness direction are the same, the change in length and thickness rateHowever, when the expansion rate in the thickness direction β is greater than the expansion rate in the longitudinal direction α, the fiber expands more in the thickness direction and less in the longitudinal direction, or the length of expansion is very small, as shown in Figure 1b.
[0035] FIG. 2 is a diagram showing the expansion process of a fabric woven with warp and weft yarns when exposed to water in the cases of α=β and β>α based on the principle of FIG.
[0036] As shown, in the initial state without water, the fabric is in the state shown in FIG. 2a.
[0037] When α = β, when the fabric is exposed to water, the length and thickness of the fibers expand at the same rate (Figure 2b), thus increasing the size of the cavities between the fibers (cross-sectional area of the grid), allowing water to naturally flow in and out (Figure 2c).
[0038] However, when β>α, when the fabric is exposed to water, the thickness of the fibers expands more than their length (Figure 2d), and the width of the cavity formed by the four fibers (cross-sectional area of the grid) is narrowed by the expanding thickness from all sides, slowing or blocking the flow of water (Figure 2e).
[0039] Therefore, the first requirement for the water-swellable material 10 of the present invention is that it must be a material (fiber) whose expansion rate in the thickness direction is greater than its expansion rate in the longitudinal direction after a certain period of time.
[0040] Next, the above principle will be explained from the viewpoint of shrinkage rate.
[0041] FIG. 3a shows a portion of a fiber having an initial length Lo and an initial thickness Do.
[0042] In Figure 3a, the shrinkage rate of the fiber in the longitudinal direction is |α’| Then, the length of the fiber after a certain time (t) is L = L O (1+α'Δt) (α'<0).
[0043] Next, the shrinkage rate in the thickness direction of the fiber is|β’| Then, the fiber thickness D after a certain time (t) is D = D O (1+β'Δt) (β'<0).
[0044] Here, if the shrinkage rate in the longitudinal direction is |α’| and shrinkage rate in thickness direction |β’| If it is the same, the change in length and thickness rate However, the shrinkage rate in the longitudinal direction is |α’| is the shrinkage rate in the thickness direction |β’| If the shrinkage is larger than 100%, the fiber will shrink more in the longitudinal direction and less in the thickness direction or the shrinkage length will be very small, as shown in FIG. 3b.
[0045] Figure 4 is based on the principle of Figure 3. |α’| = |β’| 1A and 1B are diagrams showing the shrinkage process of a fabric woven with warp and weft yarns when exposed to water in the cases of |α'| >|β'| and |α'| >|β'|, respectively.
[0046] As shown, in the absence of water the fabric is in the state shown in FIG. 4a.
[0047] |α’| = |β’| In the case of , when the fabric is exposed to water, the length and thickness of the fibers shrink at the same rate (Figure 4b), and therefore the extent of the cavities between the fibers relative to the total area Ratio of Since there is no change, the flow of water in and out is maintained naturally (Figure 4c).
[0048] However, when |α'|>|β'|, when the fabric is exposed to water, the length of the fibers shrinks more than the thickness (Figure 4d), and the width of the cavity formed by the four fibers is narrowed from all sides by the shrinking lengths, slowing or blocking the flow of water (Figure 4e).
[0049] Therefore, another alternative condition for the water-swellable material 10 of the present invention is that it must be a material (fiber) whose shrinkage rate in the longitudinal direction after a certain period of time is greater than its shrinkage rate in the thickness direction.
[0050] In summary, the water-expandable material 10 constituting the tea bag 1 of the present invention has an expansion rate in the first direction of (a) is the expansion rate in the second direction perpendicular to the first direction (b) or shrinkage in the second direction is greater than |α’| is the shrinkage rate in the first direction perpendicular to the second direction |β’| It can be seen that the condition that is greater than must be satisfied.
[0051] Based on the above description, an embodiment of a tea bag 1 containing a water-expandable substance 10 of the present invention will now be described with reference to FIG.
[0052] In this embodiment, the water expansion material 10 of the tea bag 1 is knitted or woven in the horizontal and vertical directions to immediately form the tea bag 1. If the expansion rate in the thickness direction is greater than that in the length direction, the flow of water slows down or is blocked after a certain time has passed, as shown in Figure 2, so that undesired tea ingredients do not dissolve or disperse in the water, and the original taste of the tea can be maintained. The water expansion material 10 must not expand suddenly the moment it comes into contact with water, but must first allow time for the tea ingredients to fully dissolve in the water. In other words, the lattice space formed by the horizontal and vertical fibers becomes gradually narrower over time, and is manufactured so that when it becomes less than the critical area, the flow of water molecules is blocked, inhibited, or slowed down. Taking these points into full consideration, length Direction and Thickness The expansion rates in the directions, the difference between the expansion rates and a predetermined time, i.e., the contact time with water, are appropriately determined.
[0053] The above-mentioned effect can be obtained even when the shrinkage rate in the length direction is larger than the shrinkage rate in the thickness direction. This is a matter that is obvious to those skilled in the art, so a detailed description will be omitted.
[0054] Next, as another embodiment of the present invention, another structure of the tea bag 1 containing the water-swelling substance 10 will be described with reference to FIG.
[0055] In FIG. 6, the tea bag 1 is a composite structure consisting of a number of lattice-shaped compartments 20 and a water-swellable material 10 woven into a sheet in each compartment 20 .
[0056] The partitions 20 are made up of rows 22, each of which is a line in the horizontal direction, extends generally in parallel, and is formed at a predetermined interval in the vertical direction, and columns 24, each of which is a line in the vertical direction, extends generally in parallel, and is formed at a predetermined interval in the horizontal direction. A large number of partitions 20 are formed throughout the tea bag 1, and each partition 20 provides a space A, for example, in the shape of a square grid. The partitions 20 of the present invention are made of a material with very small expansion and contraction rates, so that even when in contact with water, their shape and structure hardly change, their volume does not increase, and the size of the space A is constant. The partitions 20 can be made of a fiber material or a clean plastic material that is harmless to the human body.
[0057] The water-swelling substance 10 of the present invention can be stitched in a sheet form into the space A formed by the partitions 20. Alternatively, a bag through which water can pass can be formed for each partition 20, and the water-swelling substance 10 can be filled in the bag.
[0058] As shown in the enlarged view, the water-swellable material 10 is composed of a number of fiber particles 10A that expand when they come into contact with water. When the fiber particles 10A come into contact with water, their volume increases and their size becomes larger. When the fiber particles 10A come into contact with water, the fiber particles, i.e., the water-swellable material 10, expand, but the skeleton and shape of the compartments 20 do not change, so they cannot expand beyond the adjacent compartments 20. Therefore, each fiber expands within a given compartment 20, narrowing the gap between the fibers and impeding the flow of water.
[0059] The fiber material 10A functions like agar, which expands in volume when it comes into contact with water, and may expand in any direction, but it goes without saying that the same effect can be achieved by forming the space of the partition 20 by knitting and stitching materials with different expansion or contraction rates in the horizontal and vertical directions, as described with reference to Figures 1 to 5.
[0060] Fig. 7 is a diagram illustrating the principle of another embodiment of the present invention, in which when a film or sheet made of an artificial or natural material is plastically deformed by an external force such as punching or other methods, the material returns to its original state when wetted with water or at a certain temperature or higher while maintaining the physical or chemical deformation of the deformed portion. This is similar to a kind of shape memory effect.
[0061] Paper and natural fibrous materials have a swelling and shrinking phenomenon, and when permanently deformed by an external force, they return to their pre-plastic state in water. A sheet includes an aggregate of threads or fibrous elements, and can be embodied as a textile or paper. Plastic deformation includes not only breaking and separating from the sheet, but also the plastic deformation of the fibers or fibrous elements that are components of the textile.
[0062] As shown in Fig. 7, the water-expandable material 10 has a multi-layer structure of a first layer A1, a second layer B1, and a third layer C1, and the plastic deformation rate is first layer>second layer>third layer, and the water-expandable material 10 is in a state deformed by an external force. When the water-expandable material 10 is exposed to water and heated to a temperature above a certain temperature, it returns to its original position, thereby closing the water passage and preventing the passage of water. In addition, in Fig. 7, the first layer A1, the second layer B1, and the third layer C1 may be different materials from each other, or may be a single material but the physical properties may change during the plastic deformation process.
[0063] When a fiber having a certain length in a woven fabric is plastically deformed by an external force, the end of the fiber may protrude as shown in Fig. 7. When exposed to water or at a certain temperature, the fiber returns to its pre-plastic state and inhibits the movement of water.
[0064] FIG. 8 is a diagram showing another embodiment using the principle of FIG.
[0065] If the water-expandable material 10 is made of a plastically deformed material as shown in Fig. 8a before the tea bag 1 comes into contact with water, the water flow will return to a natural state before a certain time has passed while the tea bag is in contact with water. After that, as shown in Fig. 8b, the water-expandable material 10 will return to its original state after a certain time has passed, blocking the passage of water and suppressing the movement of water. In Fig. 8, the water-expandable material 10 can be made of multiple layers as shown in Fig. 7 or a single layer.
[0066] FIG. 9 shows yet another embodiment of the present invention, and FIG. 9a shows a cross section of a fiber in which a water-expandable material 10 is formed by forming a core portion 10b out of a material having a low expansion rate in water and forming an outer periphery 10c having a high expansion rate on the outer periphery surrounding the core portion 10b.
[0067] 9b shows a water-expandable material 10 whose thermal expansion coefficient increases gradually toward the periphery. In a single fiber element, fibers with different expansion coefficients can be realized in multiple stages in the radial direction from the center of the fiber during spinning and weaving.
[0068] In the embodiment of FIG. 9, the thermal expansion coefficient of the outer periphery of the fiber can be made larger than that of the center naturally or artificially through physicochemical treatment during the spinning and weaving process, so it is easy to manufacture the water-expandable material 10. When the water-expandable material 10 forms a tea bag 1, it is greatly affected by the temperature of the water used to dissolve the tea. This allows the outer periphery of the fiber to heat up faster and absorb more water. That is why.
[0069] Alternatively, the first portion may be configured to shrink more than the second portion, because if the thermal shrinkage rate of the core material, which is the first portion, due to the water temperature is made larger than that of the second portion, the cross-sectional area of the hole through which water passes can be reduced as a result, based on the principle described in FIG.
[0070] In the case of FIG. 9, even if the core and outer periphery are made of the same material, the core and outer periphery can be embodied to have different physical properties during the fiber manufacturing process or when exposed to water and high temperatures, so the core and outer periphery can be made of the same material or different materials.
[0071] Although several embodiments of the present invention have been described above, various modifications of the present invention are possible. For example, the tea bag 1 may be made of an existing fabric material through which water can freely flow, and the water-swelling material of the present invention may be layered or coated on the entire or part of the fabric to form a composite structure.
[0072] Needless to say, the scope of the present invention extends to the same or equivalent areas as the claims set forth below.
Claims
1. A tea bag containing tea therein, The tea bag includes a water-swelling material that is deformed by plastic processing to allow the flow of water, and that prevents the flow of water by restoring its original shape when in contact with water for a predetermined period of time or more.
2. A tea bag containing tea therein, The tea bag comprises a water-swellable material; The water-expandable substance has a multi-layer structure such that when it comes into contact with water, after a predetermined time, the second portion expands more than the first portion to impede the flow of water, the first portion forming a core of the water-expandable substance, and the second portion forming an outer periphery surrounding the core.
3. A tea bag containing tea therein, The tea bag includes a water-swelling material, the water-swelling material having a multi-layer structure in which, when contacted with water, a first portion shrinks more than a second portion after a predetermined time, reducing the cross-sectional area of a passage through which water passes and impeding the flow of water, the first portion forming a core of the water-swelling material, and the second portion forming an outer periphery surrounding the core.
4. A tea bag as described in claim 2 or 3, wherein the water-expandable material includes a fibrous material.
5. A tea bag as described in claim 2 or 3, wherein the outer periphery formed by the second part has a structure of two or more layers.