Systems and methods for performing laser-induced breakdown spectroscopy measurements on molten metal samples - Patents.com
The LIBS system addresses inaccuracies in molten metal analysis by temperature-controlled, passive cooling and rapid measurement initiation, providing efficient and accurate chemical analysis in industrial settings.
Patent Information
- Application Number
- JP2024515088
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-08
- Filing Date
- 2022-09-07
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2042-09-07
AI Technical Summary
Current methods for chemical analysis of molten metals, such as spark atomic emission spectroscopy, are prone to errors due to sample preparation issues and require extensive time for analysis, making them inaccurate and inefficient for real-time monitoring in industrial settings like primary aluminum smelters.
A LIBS system that monitors the temperature of molten metal samples during passive cooling and initiates measurements when temperature criteria are met, using a portable setup with integrated calibration, ensuring consistent and rapid chemical analysis without active heating, thus reducing measurement errors.
The system enables accurate, real-time, and in-situ chemical analysis of molten metals with reduced errors, facilitating fast and consistent results across multiple samples, suitable for battery-powered implementations in challenging industrial environments.
Smart Images

Figure 2024536735000001 
Figure 2024536735000002 
Figure 2024536735000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to chemical analysis of liquid metals and alloys. More specifically, the present disclosure relates to the use of laser-induced breakdown spectroscopy for chemical composition analysis of liquid metals and alloys. [Background technology]
[0002] In metal production, it is very important to monitor the chemical composition of the produced metal. For example, in the primary production of aluminum using continuous electrolysis by the Hall-Heroult process, samples of the metal from the individual reduction cells are periodically collected for chemical analysis. This is done to monitor the level of impurities in the metal, which also serves as an indicator of the operating conditions of each cell.
[0003] A typical primary aluminum smelter contains hundreds of reduction cells from which samples are collected constantly (up to daily) during normal operation. Current standard practice involves extracting a sample of liquid metal from the reduction cell and casting a solid sample using, for example, a standard sample mold conforming to ASTM standard E716. The solid sample is then analyzed to determine its chemical composition.
[0004] For decades, the standard method for the analysis of solid samples in the aluminum industry has been spark atomic emission spectroscopy (also known as spark optical emission spectroscopy or spark OES), e.g. according to ASTM standard E1251. Before performing a spark OES analysis, the sample needs to be appropriately prepared, e.g. by mechanically rolling to a specific depth within the cast sample. All of the sample preparation steps are important to ensure accurate analytical results. Summary of the Invention
[0005] A LIBS measurement system is disclosed that is configured to monitor the temperature of the molten metal sample during cooling of the molten metal sample in the crucible and to initiate a LIBS measurement after the temperature of the molten metal sample meets a measurement temperature criterion. The system may also monitor the temperature of an empty crucible to assist in ensuring that the crucible temperature is (i) high enough to ensure that a sufficiently low cooling rate of the molten metal sample occurs during the LIBS measurement after the molten metal sample is delivered to the crucible and cooled to meet the measurement temperature criterion, and (ii) optionally low enough to meet the measurement temperature criterion and avoid unnecessarily long cooling times of the molten metal sample before the start of the LIBS measurement. The LIBS measurement system may be mobile and battery powered and may include an integrated calibration section.
[0006] Accordingly, in one aspect, there is provided a method of performing laser-induced breakdown spectroscopy (LIBS) on a molten sample while the molten sample is cooling, the method comprising: monitoring a temperature of the molten sample during cooling of the molten sample in the crucible and comparing the temperature of the molten sample to a measured temperature criterion; determining that a temperature of the molten sample meets a measurement temperature criterion and initiating a LIBS measurement on the molten sample is provided.
[0007] The method comprises the steps of: measuring the temperature of the crucible while the crucible is in a preheated state and without a molten sample present at one or more times and comparing the temperature of the crucible to a crucible temperature criterion; determining that the temperature of the crucible meets a crucible temperature criterion to provide an indication that the crucible is ready to receive a molten sample; The crucible temperature criteria are configured such that the molten sample cools by less than 50° C. during the LIBS measurement.
[0008] In some exemplary embodiments of the method, the crucible temperature criterion includes a minimum crucible temperature such that the crucible temperature criterion is met when the minimum crucible temperature is exceeded. The minimum crucible temperature can be between 100° C. and 60% of the melting point temperature of the molten sample, in degrees C. The minimum crucible temperature can be between 15% of the melting point temperature of the molten sample and 60% of the melting point temperature, in degrees C.
[0009] In some exemplary embodiments of the method, the crucible temperature criterion is met when the temperature of the crucible is within the crucible temperature range. The maximum crucible temperature of the crucible temperature range can be defined such that when the temperature of the crucible is equal to the maximum crucible temperature and the molten sample is added to the crucible, the temperature of the molten sample meets the measurement temperature criterion within one minute. The maximum crucible temperature of the crucible temperature range can be defined such that when the temperature of the crucible is equal to the maximum crucible temperature and the molten sample is added to the crucible, the temperature of the molten sample meets the measurement temperature criterion within 30 seconds. The maximum crucible temperature can be between 50% of the melting point temperature of the molten sample and 90% of the melting point temperature in degrees Celsius.
[0010] In some exemplary implementations of the method, the measurement temperature criteria is selected such that the LIBS measurement is performed within a preselected measurement temperature range.
[0011] In some exemplary embodiments of the method, the measurement temperature criteria includes a preselected measurement temperature, and the LIBS measurement is initiated immediately after (i) determining that the temperature of the molten sample is equal to the preselected measurement temperature, and (ii) positioning the LIBS measurement head over the crucible.
[0012] In some exemplary embodiments of the method, the measurement temperature criteria includes a preselected measurement temperature, and the LIBS measurement is performed after determining that the temperature of the molten sample is equal to the preselected measurement temperature. The preselected measurement temperature may exceed the melting point temperature of the molten sample by an amount in the range of 5% to 25% of the melting point temperature in degrees Celsius.
[0013] In some exemplary embodiments of the method, the measurement temperature criteria includes a preselected measurement temperature range, and the LIBS measurement is performed while the temperature of the molten sample is within the preselected measurement temperature range.
[0014] In some exemplary implementations of the method, the measurement temperature criterion is configured such that when the crucible temperature criterion is met, the temperature of the molten sample during the LIBS measurement exceeds the temperature of the crucible.
[0015] In some exemplary embodiments of the method, the crucible is preheated with a pre-measured molten sample, and the pre-measured molten sample is discarded prior to measuring the temperature of the crucible.
[0016] In some exemplary embodiments of the method, the molten sample comprises aluminum and the crucible is preheated by contact with a crust of cryolite that has formed on the top of the reduction cell.
[0017] In some exemplary embodiments of the method, the temperature of the crucible and the temperature of the molten sample are measured using a common temperature sensor.
[0018] In some exemplary embodiments of the method, the temperature of the crucible and the temperature of the molten sample are measured without contact.
[0019] In some exemplary embodiments of the method, the crucible is supported by a crucible support during the LIBS measurement, the LIBS measurement is performed by a LIBS subsystem, a measurement head of the LIBS subsystem is movable from a parked position to an operating position in which the measurement head is above the crucible support, and a heat shield is positioned to insulate the measurement head from heat emitted from the crucible when the measurement head is in the parked position.
[0020] In some exemplary embodiments of the method, the crucible is a metallic crucible. The crucible may be formed from structural steel.
[0021] In some exemplary embodiments of the method, the heat capacity of the crucible is between 400 J / K and 500 J / K.
[0022] In some exemplary embodiments of the method, the thermal conductivity of the crucible is between 40 W / mK and 50 W / mK.
[0023] In some exemplary embodiments of the method, the crucible is a first crucible, the molten sample is a first molten sample, and the method comprises: discarding the first molten sample from the first crucible; Measuring a temperature of the first crucible; determining that the temperature of the first crucible does not meet a crucible temperature criterion due to an excessively high temperature; replacing the first crucible with a second crucible having a temperature less than the temperature of the first crucible; The method further includes performing LIBS measurements on the second molten sample using the second crucible while the first crucible is cooling.
[0024] A first crucible may be supported by a primary crucible support during LIBS measurements performed on the first molten sample, and after replacing the first crucible with the second crucible, the first crucible is placed on the secondary crucible support for cooling.
[0025] In some exemplary embodiments, the method includes, prior to replacing the first crucible with the second crucible: preheating a second crucible; monitoring the temperature of the second crucible; and indicating when the second crucible meets the crucible temperature criterion.
[0026] In some exemplary embodiments, the method comprises: Optionally, performing LIBS measurements on one or more additional molten samples using a second crucible; and Emptying the second crucible; Measuring the temperature of the second crucible; determining that the temperature of the second crucible does not meet a crucible temperature criterion due to an excessively high temperature; The second crucible, A first crucible, and replacing the selected crucible with a third crucible; and and performing LIBS measurements on another additional molten sample using the selected crucible.
[0027] In some exemplary embodiments of the present methods, the LIBS measurements are performed by a LIBS system that resides on a portable support structure, and the LIBS system is powered by a battery.
[0028] In another aspect, a method of performing laser induced breakdown spectroscopy (LIBS) on a molten sample while the molten sample is cooling includes the steps of: Preheating the crucible; Introducing a molten sample into a crucible; monitoring a temperature of the molten sample during cooling of the molten sample in the crucible and comparing the temperature of the molten sample to a measured temperature criterion; determining that a temperature of the molten sample meets a measurement temperature criterion and initiating a LIBS measurement on the molten sample is provided.
[0029] In certain exemplary embodiments, the method includes, after pre-heating the crucible and prior to introducing the molten sample into the crucible: measuring the temperature of the crucible at one or more times and comparing the temperature of the crucible to a crucible temperature criterion; determining that the temperature of the crucible satisfies the crucible temperature criterion and providing a molten sample to the crucible; The crucible temperature criteria are configured such that the molten sample cools by less than 50° C. during the LIBS measurement.
[0030] In another aspect, a system for performing laser induced breakdown spectroscopy (LIBS) is provided, the system comprising: A temperature sensor; a laser-induced breakdown spectroscopy (LIBS) subsystem; A processing circuit operably coupled to the temperature sensor and the LIBS subsystem, the processing circuit comprising at least one processor and associated memory, the memory including instructions executable by the processor to perform operations, the operations including: monitoring a temperature of the molten sample during cooling of the molten sample in the crucible with a temperature sensor; and processing circuitry to determine that the molten sample meets a measurement temperature criterion and control the LIBS subsystem to initiate a LIBS measurement on the molten sample.
[0031] Prior to introducing the molten sample into the crucible, the processing circuitry Measuring the temperature of the crucible using a temperature sensor, the crucible being preheated; providing an indication that the crucible is ready to receive a molten sample after determining that the temperature of the crucible satisfies the crucible temperature criterion; The crucible temperature criteria are configured such that the molten sample cools by less than 50° C. during the LIBS measurement.
[0032] In another aspect, a portable system for performing laser induced breakdown spectroscopy (LIBS), the portable system comprising: a laser induced breakdown spectroscopy (LIBS) subsystem comprising a measurement head, the LIBS subsystem being connectable to a battery; a primary crucible support, the measurement head of the LIBS subsystem being movable from a parked position to an operating position, the measurement head residing on the primary crucible support in the operating position to perform LIBS measurements on a molten sample residing in a crucible supported by the primary crucible support; a secondary crucible support capable of supporting and cooling an additional crucible; A portable system is provided that includes a LIBS subsystem, a primary crucible support, and a moveable support structure configured to support a secondary crucible support.
[0033] In some exemplary embodiments, the system comprises: a temperature sensor configured to monitor a temperature of a crucible present within the primary crucible support when the measurement head is in a parked position; A processing circuit operably coupled to a temperature sensor, the processing circuit comprising at least one processor and associated memory, the memory including instructions executable by the processor to perform operations, the operations including: measuring a temperature of a crucible supported by the primary crucible support with a temperature sensor; and processing circuitry that, after determining that the temperature of the crucible does not meet the crucible temperature criterion due to an excessively high temperature, provides an indication that the crucible should be cooled in the secondary crucible support prior to use.
[0034] In some exemplary embodiments, the system further comprises a crucible and an additional crucible, wherein the crucible and the additional crucible are made of metal. The crucible and the additional crucible may be formed of structural steel.
[0035] In some exemplary embodiments, the system further comprises a crucible and an additional crucible, wherein the heat capacity of the crucible and the additional crucible is between 400 J / K and 500 J / K.
[0036] In some exemplary embodiments, the system further comprises a crucible and an additional crucible, wherein the thermal conductivity of the crucible and the additional crucible is between 40 W / mK and 50 W / mK.
[0037] In another aspect, a portable system for performing laser induced breakdown spectroscopy (LIBS), the portable system comprising: a laser induced breakdown spectroscopy (LIBS) subsystem comprising a measurement head, the LIBS subsystem being connectable to a battery; an integrated calibration device; a movable support structure configured to support the LIBS subsystem and the integrated calibration device; A portable system is provided in which a measurement head of the LIBS subsystem is movable from an operating position above a crucible support, where the measurement head performs LIBS measurements on a molten sample present in the crucible, to a calibration position suitable for performing calibration measurements suitable for calibrating at least one parameter of the LIBS subsystem.
[0038] In some exemplary implementations of the system, the integrated calibration device includes a LIBS calibration reference material suitable for calibrating the signal of the LIBS subsystem when the measurement head is in the calibration position. The integrated calibration device may comprise a support frame, and the LIBS calibration reference material is movable relative to the support frame such that when the measurement head is repositioned in the calibration position to perform a subsequent calibration measurement, different regions of the LIBS calibration reference material can be optically interrogated by the measurement head, thereby facilitating reuse of the LIBS calibration reference material during multiple calibration measurements.
[0039] In some exemplary implementations of the system, the measurement head comprises a distance sensor and the integrated calibration device is an integrated distance sensor calibration device, the integrated distance sensor calibration device includes a contact location and a target location, the contact location being located on the integrated calibration device such that when the measurement head is in the calibration position and in contact with the contact location after lowering the measurement head along a direction parallel to the optical axis of the measurement head, a known spatial offset is between the distance sensor and the target location, thereby facilitating calibration of the distance sensor. The integrated distance sensor calibration device may be resiliently biased such that the known spatial offset is maintained when the measurement head is moved along the direction after contacting the contact location.
[0040] In some exemplary embodiments, the system comprises: a primary crucible support for supporting the crucible during LIBS measurements; and a secondary crucible support capable of supporting and cooling an additional crucible.
[0041] A further understanding of the functional and advantageous aspects of the present disclosure may be realized by reference to the following detailed description and drawings.
[0042] Embodiments will now be described, by way of example only, with reference to the following drawings: [Brief description of the drawings]
[0043] [Figure 1] FIG. 1 illustrates an exemplary system for performing LIBS measurements on a molten metal sample. [Figure 2A-2C] Shown are the initiation of the LIBS measurement (Figure 2A), the initiation of the LIBS measurement after determining that the temperature of the molten metal sample meets the measurement temperature criterion (Figure 2B), and monitoring of the temperature of the molten metal sample before measurement of an empty crucible prior to the introduction of the molten metal sample. [Diagram 3] 1 is a flow chart illustrating an exemplary method for performing LIBS measurements on a molten metal sample utilizing passive cooling and temperature monitoring of the molten metal sample prior to initiation of the LIBS measurement. [Figure 5A-5B] FIG. 13 shows a schematic diagram of a crucible replacement when the temperature of a given crucible is deemed too high for use in further measurements. [Figure 6] FIG. 13 illustrates an exemplary embodiment in which a heat shield is used to protect the LIBS measurement head when the LIBS measurement head is parked to the side of the crucible support. [Figure 7A-7C] FIG. 2 illustrates an example calibration subsystem for performing calibration operations on a LIBS measurement head between measurements. [Figure 8] FIG. 1 illustrates an exemplary mobile LIBS measurement system including a battery power source. [Figure 9] FIG. 1 illustrates an exemplary mobile LIBS metrology system including a calibration portion. [Figure 10] FIG. 1 illustrates the correspondence between elemental impurity analyses performed on (i) liquid aluminum samples using a portable LIBS system and (ii) solid aluminum samples using a laboratory-based spark OES system. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0044] Various embodiments and aspects of the present disclosure will be described with reference to the details described below. The following description and drawings are illustrative of the present disclosure and should not be construed as limiting the present disclosure. Numerous specific details are described to achieve a thorough understanding of the various embodiments of the present disclosure. However, in certain instances, well-known or conventional details are not described to provide a concise description of the embodiments of the present disclosure.
[0045] As used herein, the term "comprise" should be interpreted as inclusive and open-ended, not exclusive. In particular, when used in the specification and claims, the terms "comprise" and variations thereof mean that the specified features, steps, or components are included. These terms should not be interpreted to exclude the presence of other features, steps, or components.
[0046] As used herein, the term "exemplary" means "serving as an example, instance, or illustration," and should not be construed as preferred or advantageous over other configurations disclosed herein.
[0047] As used herein, the terms "about" and "approximately" are meant to encompass variations that may exist within the upper and lower limits of a range of values, such as variations in properties, parameters, and dimensions. Unless otherwise specified, the terms "about" and "approximately" mean plus or minus 25 percent or less.
[0048] As used herein, percentage values related to temperature are intended to refer to temperatures in degrees Celsius.
[0049] Unless otherwise stated, any specified range or group is to be understood as a shorthand term referring to each and each element within the range or group individually, as well as each and each possible subrange or subgroup contained therein, and the same for subranges or subgroups therein. Unless otherwise stated, the present disclosure relates to and expressly incorporates each and each specific element and combination of subranges or subgroups.
[0050] As mentioned above, the conventional approach to chemical analysis in the aluminum industry employs the use of spark OES on solid samples. Unfortunately, this conventional approach is subject to a number of technical problems that can hinder the ability to achieve accurate chemical analysis.
[0051] In particular, the sample preparation process can introduce errors. For example, errors can occur during the sample preparation process due to a number of potential sources, including, but not limited to, (i) temperature variations in the melt or mold when the sample is taken, (ii) non-uniform pouring of the sample mold, (iii) segregation related to the cooling rate of the metal, (iv) porosity, cracks, or gaps in the sample, (v) excessive surface roughness or smoothness after rolling, and (vi) contamination of the surface prior to analysis.
[0052] Furthermore, traditional techniques for casting samples and performing subsequent analysis may lead to potential errors arising from confusion between individual samples. Yet another problem associated with traditional chemical analysis workflows is the safety hazards that may be caused by traffic inside the smelter resulting from transporting cast samples to the laboratory. Considering the steps of collecting the liquid metal, casting solid samples, transporting the samples to a central analysis facility, and performing machine preparation and chemical analysis, many hours may pass from the time the metal is sampled to the time the analytical results are available to plant operators to make process decisions.
[0053] Recognizing and carefully considering the technical and workflow challenges discussed above, the present inventors set out to develop a new modality of chemical analysis that overcomes the problems associated with conventional approaches to chemical analysis. In particular, the present inventors recognized that to overcome the above technical problems, a new chemical analysis modality is needed that facilitates robust, rapid, and accurate chemical testing in a real-time, in-situ manner.
[0054] Various attempts have been made to adapt different detection modalities for real-time monitoring of the status of reduction cells in primary aluminum smelters. Some of these approaches include analysis of cell temperature and bath chemistry, analysis of individual anode current signals, analysis of cell voltage noise, and optionally multiple additional parameters that affect the current efficiency, energy consumption, and operational life of the cell. For example, differential thermal analysis has been successfully applied to determine bath chemistry, i.e., bath ratio and alumina (Al2O3) content, within minutes using the commercially available STARprobe™ (X. Wang: “Alcoa STARprobeTM - Update in further development for measuring cryolite properties,” TMS Light Metals 2016, pp. 397-402), which replaces alternative time-consuming sample preparation and X-ray analysis in a central laboratory.
[0055] However, real-time and in situ measurement of chemical impurities in produced metals presents different challenges that are not addressed by the real-time monitoring methods mentioned above. Laser-induced breakdown spectroscopy (LIBS), an atomic emission spectroscopy applicable to the measurement of liquids and solids, has emerged as a promising technique for the chemical analysis of liquid metals. In particular, LIBS has previously been applied to measure the impurity content of liquid aluminum (AK Rai, F.-Y. Yueh, JP Singh: “Laser-induced breakdown spectroscopy of molten aluminum alloy,” Appl. Opt. 42 (2003) pp. 2078-2084; J. Herbert, et al.: “The Industrial Application of Molten Metal Analysis,” TMS Light Metals 2019, pp. 945-952; SH Gudmundsson, et al.: “Accurate Real-Time Elemental (LIBS) Analysis of Molten Aluminum and Aluminum Alloys,” TMS Light Metals 2020, pp. 860-864).
[0056] Attempting to adapt LIBS for real-time, in-situ testing in industrial environments has been fraught with difficulties. For example, the complex and hazardous environment inside a primary aluminum smelter presents many technical challenges for the use of LIBS systems due to high temperatures, dust, and fumes expelled from the cells when they are opened. In addition, strong magnetic fields present challenges for instrumentation operating in the vicinity of reduction cells (see, e.g., Sun et al., Spectrochimica Acta Part B 142 (2018) 29-36). Small, handheld LIBS analyzers are available from several vendors, but they are not suitable for analyzing liquid metals and do not provide the detection limits or accuracy required to monitor aluminum from reduction cells.
[0057] Thus, despite the promise of LIBS for improved chemical composition analysis, outstanding technical challenges remain to be resolved to facilitate the adaptation of LIBS into real-time and in situ implementations that are sufficiently robust to provide fast and accurate chemical analysis of molten metals.
[0058] One problem the inventors faced when attempting to adapt a LIBS measurement system in a portable configuration is the need to ensure a stable measurement of the temperature of the molten metal sample during the LIBS measurement. Specifically, the relative intensities of the LIBS emission lines can depend on the sample temperature, and as a result, changes in sample temperature between successive LIBS measurements can lead to significant errors in the reported concentrations of impurities.
[0059] Such issues can in some cases be addressed by actively controlling the temperature of the molten metal sample prior to or during the LIBS measurement, however, such an approach can be problematic for portable implementations due to the high power consumption of active heat sources, which can hinder the ability to power portable systems using batteries.
[0060] The inventors sought to overcome the above technical problems by developing a LIBS system that uses passive cooling of the molten metal sample, thereby avoiding active heating before or during the LIBS measurement. It was further determined that such an embodiment may be adapted to facilitate accurate and repeatable LIBS measurements of the subsequently measured sample without significant measurement errors from changes in sample temperature by monitoring the temperature of the molten metal sample during cooling of the molten metal sample and initiating the LIBS measurement when or after the monitored temperature meets a preselected measurement temperature criterion. Such an embodiment may be particularly beneficial in a mobile configuration due to not requiring active heating of the molten metal sample before and during the LIBS measurement process, greatly simplifying the system and facilitating battery-powered configurations. Furthermore, this embodiment avoids introducing additional complexities into the spectral analysis to detect and correct for the effects of temperature changes in the melt.
[0061] Monitoring the temperature of the molten metal sample and initiating the LIBS measurement only when the measurement temperature criteria is met ensures that LIBS measurements made on different molten metal samples (e.g., different samples from a common cell or different samples from different cells) that may have different initial temperatures or different cooling rates due to different temperatures of the measurement crucibles are nevertheless performed at or near a common temperature during the LIBS measurement, such exemplary embodiments thereby avoid, prevent or mitigate measurement errors due to changes in sample temperature.
[0062] As described below, the exemplary embodiment may be beneficial in reducing sources of error in analysis by analyzing metal in the liquid state and facilitating very close, direct and unequivocal correlation of chemical analysis results to each reduction cell. The exemplary system and method further facilitates a consistent and fast workflow when measuring samples from multiple pots in succession. Similarly, the exemplary system and method may be used to facilitate the fast measurement of a series of samples drawn from a single reduction cell, or in a similar manner when multiple samples of liquid metal from a single source or multiple sources need to be analyzed quickly and accurately.
[0063] Thus, in certain exemplary embodiments, a portable chemical analysis system includes a LIBS metrology subsystem and a temperature sensor configured to monitor a temperature of the molten metal sample during passive cooling of the molten metal sample, and the portable metrology system controls the LIBS metrology subsystem to compare the measured temperatures of the molten metal sample and initiate a LIBS measurement after a preselected measurement temperature criterion is met.
[0064] An exemplary embodiment of such a portable LIBS system is shown in FIG. 1. The exemplary system includes a LIBS subsystem including a LIBS measurement head 200. The LIBS subsystem is operatively connected or connectable to a control and processing circuit, shown at 100, as described in more detail below. The LIBS measurement head 200 includes an optical beam delivery subsystem for delivering a LIBS laser pulse onto the surface of the molten metal sample 10 and collecting optical emissions from a plasma plume generated in response to the interaction of the laser pulse with the target material. The LIBS measurement head 200 may include all subcomponents of the LIBS system, including the LIBS laser source and detector. Alternatively, some of the components of the LIBS system (e.g., the LIBS laser source and / or detector) may be provided within a housing in optical and / or electrical communication with the LIBS measurement head 200.
[0065] The molten metal sample 10 is passively cooled in a crucible 20 (e.g., a ladle) prior to performing a LIBS measurement while monitoring the temperature of the metal molten sample 10, for example, as shown in Figure 2A. As shown in Figure 1, the crucible may be supported by a crucible support 30. When (or after) the temperature of the molten metal sample meets a preselected measurement temperature criterion, the LIBS measurement is initiated, as shown in Figure 2B.
[0066] 1, the exemplary system includes a temperature sensor 210 positionable to enable interrogation of the surface of the molten metal sample 10. In some exemplary implementations, the temperature sensor may be a non-contact temperature sensor, such as, but not limited to, an infrared pyrometer or a thermal camera. Such a sensor response may be corrected for the emissivity of the respective material being measured. Alternatively, the temperature sensor may be a contact-based temperature sensor, such as, but not limited to, a thermocouple or a thermometer.
[0067] The measurement temperature criterion ensures that LIBS measurements made on different molten metal samples (e.g., different samples from a common cell or different samples from different cells) are performed at or near the same temperature, thereby avoiding, preventing, or reducing measurement errors due to changes in sample temperature, as described above. For example, the LIBS measurement head 200 may be controlled such that the LIBS measurement is initiated (i) immediately after the measurement temperature criterion is met, (ii) after a fixed delay after the measurement temperature criterion is met, or (iii) within a predetermined time interval after the measurement temperature criterion is met, where the time interval may be calculated based on an observed cooling rate.
[0068] In one exemplary embodiment, the measurement temperature criterion may be met when the measured temperature of the molten metal sample 10 reaches a measurement temperature, such as a measurement temperature that exceeds the melting point temperature of the molten sample by 5%, or such as 10%, or such as 15%, or such as 20%, or such as 25%. In the exemplary case of molten aluminum, the measurement temperature is selected from the range of 700-800°C, such as 750°C.
[0069] When the LIBS measurement head 200 is in a parked position (e.g., as shown at 201 in FIG. 1 ) during monitoring of the temperature of the molten metal sample 10 (e.g., to ensure sufficient line of sight for non-contact temperature sensing), initiation of the LIBS measurement may include repositioning the LIBS measurement head 200 over the molten metal sample 10 (e.g., as shown at 230 in FIG. 1 ), and optionally lowering the LIBS measurement head 200 to the surface of the molten metal sample 10, followed by delivery of a LIBS laser pulse to the molten metal sample 10. Alternatively, when the temperature of the molten metal surface is measurable with the LIBS measurement head in a measurement position above the molten metal sample 10, the LIBS measurement may be initiated after a preselected measurement temperature criterion is met by the measured temperature of the molten metal sample 10, without laterally moving the LIBS measurement head 200.
[0070] Prior to performing the LIBS analysis, the surface of the molten metal sample may be skimmed with an automated skimmer (not shown in FIG. 1 ) or a manual skimmer. This skimming step serves to remove dross or remaining bath material from the surface of the sample to expose the liquid metal for analysis, in the case of non-contact temperature measurement, as well as to ensure proper measurement of the temperature of the liquid metal, since dross formation affects the emissivity of the sample surface. After performing the LIBS measurement, the LIBS measurement head 200 may be retracted (e.g., automatically) and the measurement results may be displayed and recorded (e.g., logged to a database). After the LIBS analysis, the molten metal sample may be returned to the reduction cell, discarded elsewhere in a liquid state, or allowed to solidify and then discarded or stored for reference. In some exemplary embodiments, the mobile analysis system may include an integrated disposable container for discarded samples.
[0071] It has been found by the inventors that the cooling rate of the molten metal sample 10 during the LIBS measurement can affect the accuracy of the LIBS measurement. In particular, if the cooling rate is high enough, the resulting temperature changes during the LIBS measurement step (which may include several seconds, such as, for example, approximately 5 seconds) can lead to inaccuracies in the determination of the impurity concentration. Furthermore, large variations in temperature during the LIBS measurement step make the system susceptible to measurement errors if the timing of the LIBS measurement relative to the time of the determination that the measurement temperature criterion has been met is not precisely controlled. Similarly, high cooling rates can adversely affect the consistency of the measurement conditions for a series of measurements of different liquid metal samples.
[0072] This problem may be exacerbated when the crucible is made of a material that may lead to fast cooling of the molten metal sample. For example, it may be useful or necessary to contact the crucible with an impact surface to remove the solidified metal from the crucible so as to facilitate fast removal of the molten metal sample after LIBS measurement. In such cases, it may be beneficial to use a non-ceramic crucible that can withstand the impact without risk of breakage. One example of a suitable crucible is a metallic crucible, such as a crucible made from structural steel. For such metallic crucibles, which typically have high heat capacity and high thermal conductivity, the molten metal sample may cool quickly in the cold metal crucible. In some exemplary embodiments, the heat capacity of such a crucible may be between 400 J / K and 500 J / K, and the thermal conductivity of the crucible material may be between 40 W / mK and 50 W / mK.
[0073] To avoid or reduce errors induced by rapid cooling of the molten metal sample, the inventors have found that it may be beneficial to pre-heat the crucible 20 prior to delivery of the molten metal sample 10 to the crucible 20. Such pre-heating may be beneficial in reducing and / or controlling the cooling rate of the molten metal sample 10 after it is received by the crucible 20. In addition, pre-heating improves the safety of the liquid metal sampling process by ensuring that the crucible is free of moisture prior to the introduction of the liquid metal.
[0074] Pre-heating of the crucible can be performed according to a wide variety of methods. In some exemplary embodiments, pre-heating is performed outside the portable LIBS measurement system, such as by utilizing available heat from a reduction cell. For example, in an exemplary implementation involving an aluminum smelter, the crucible can be pre-heated by contacting it with a cryolite crust formed inside the reduction cell for a period of time long enough for the crucible to reach the desired temperature.
[0075] After pre-heating the crucible, a molten metal sample may be provided to the crucible (e.g., a metering ladle). For example, a sample of liquid molten metal is extracted using a method traditionally used to sample metal from a reduction cell, such as using a sampling ladle to collect the molten metal from the reduction cell. For example, a sample of molten metal may be manually introduced to the sample crucible, e.g., by a human operator using such a sampling ladle. In addition, samples may be manually or automatically extracted from other types of sources, such as mixing furnaces, holding furnaces, etc., where the sampling ladle may in some embodiments also be used as a sample crucible to hold the sample during measurement.
[0076] In some exemplary embodiments, it may be beneficial to ensure that the crucible 20 has been pre-heated a sufficient amount to ensure that the cooling rate is not too rapid during the LIBS measurement. For example, prior to introducing the molten metal sample 10 into the crucible 20, the temperature of the crucible 20 may be measured and compared to a crucible temperature criterion to assess whether the crucible 20 has been sufficiently pre-heated prior to receiving the molten metal sample 10. The measured temperature criterion may be configured such that when the crucible temperature criterion is met, the temperature of the molten sample during the LIBS measurement exceeds the temperature of the crucible.
[0077] In some exemplary embodiments, the temperature sensor 210 used to monitor the temperature of the molten metal sample 10 may also be used to measure the temperature of the empty crucible 20. Such an exemplary embodiment is shown in Figure 2C. Alternatively, separate temperature sensors may be used to monitor the temperature of the molten metal sample and to measure the temperature of the crucible 20 prior to delivery of the molten metal sample 10.
[0078] In some exemplary embodiments, the crucible temperature criterion may be defined to be met when the measured crucible temperature exceeds a preselected minimum temperature value, e.g., within a range of 100° C. to 60% of the melting point temperature of the molten metal, or, e.g., 15-60% of the melting point temperature (e.g., 100-400° C. for aluminum), thereby ensuring that the cooling rate of the molten metal sample 10 after it is delivered to the crucible 20 is within a particular range. For example, the crucible temperature criterion may be selected such that the molten metal sample cools by less than 50° C. during the LIBS measurement, or, e.g., cools by less than 20° C. during the LIBS measurement, or, e.g., cools by less than 10° C. during the LIBS measurement, or, e.g., cools by less than 5° C. during the LIBS measurement.
[0079] In the absence of an upper limit on the allowable initial temperature of the crucible 20, the crucible 20 may in some cases be preheated to such a high temperature that an excessive amount of time elapses before the molten metal sample 10 cools to a temperature that satisfies the measurement temperature criterion while still satisfying the crucible temperature criterion. In such cases, the time required to collect and analyze subsequent samples is correspondingly increased. Such cases may be avoided by defining the crucible temperature criterion such that it is not satisfied by a crucible temperature that exceeds the upper temperature limit. For example, the crucible temperature criterion may include a maximum crucible temperature selected to be within 50-90% of the melting point temperature (e.g., in the exemplary case of aluminum, approximately 330-600°C). In addition, the maximum crucible temperature limit ensures that the degree of contamination of the crucible material into the molten metal is minimized.
[0080] For example, the crucible temperature criterion may be met when the temperature of the crucible 20 (before receiving the molten metal sample 10) is in a predefined temperature range, e.g., between 100° C. and 60% of the melting point temperature of the molten sample, or, e.g., between 15% and 60% of the melting point temperature of the molten sample (e.g., between 100° C. and 400° C. in the exemplary case of aluminum), or, e.g., between 30% and 75% of the melting point temperature (e.g., between 200° C. and 500° C. in the exemplary case of aluminum). Thus, the predefined temperature range has the characteristics of a “Goldilocks” range such that when the molten metal sample 10 is delivered to a crucible that meets the crucible temperature criterion, the molten metal cools at a rate slow enough to enable accurate LIBS measurements (when the temperature of the molten metal sample meets the measurement temperature criterion) and the molten metal sample cools to a temperature that meets the measurement temperature criterion within a short enough time. For example, the maximum temperature permitted by the crucible metrology criteria may be defined such that a molten metal sample after being delivered to a crucible cools to a temperature that meets the metrology temperature criteria within 1 minute, or within 30 seconds, or within 15 seconds.
[0081] In some exemplary embodiments, an indication may be provided to an operator when the temperature of the empty crucible 20 meets the crucible temperature criteria. Non-limiting examples of suitable indications include a display message, symbol or color and an audible alarm or message. The indication may be used to inform the operator that the empty crucible 20 is ready to receive a molten metal sample. In other exemplary embodiments, the temperature of the empty crucible 20 may be displayed. In such a case, an operator with knowledge of the suitable crucible temperature criteria (e.g., minimum crucible temperature range or desired crucible temperature range) may deliver a metal molten sample to the crucible when the displayed temperature meets the known crucible temperature criteria.
[0082] 3, a flow chart is provided illustrating an exemplary method of performing LIBS analysis of a molten sample using a LIBS measurement system, such as the system shown in FIG. 1. A pre-heated, empty crucible (containing no molten metal sample) is first provided and its temperature is measured at step 300. The crucible temperature criteria is evaluated at step 310. If the crucible criteria is not met at 312 due to the crucible temperature being too low, an operator may heat the crucible as shown at 314 and the crucible temperature is remeasured and reevaluated at 300. If the crucible temperature is too high as shown at 310, the crucible is allowed to passively cool and the crucible temperature is remeasured and reevaluated at 300.
[0083] Once the crucible temperature criteria have been met, an indication may be provided that the crucible is ready to receive the molten metal sample at 320. After the molten metal sample is received within the crucible, the temperature of the molten metal sample is monitored during cooling, as shown at 330, and the measurement temperature criteria are evaluated, as shown at 340. When the measurement temperature criteria have been met, the LIBS measurement is initiated, as shown at 350.
[0084] In the exemplary method described above with reference to FIG. 3, an empty crucible is allowed to cool passively when its measured temperature does not meet the crucible temperature criteria in step 310. For example, when a crucible is used for multiple LIBS measurements, the crucible temperature may rise due to repeated exposures, heating the molten metal sample, and the temperature of the crucible after the previous molten metal sample is discarded may exceed the maximum temperature allowed by the crucible temperature criteria. Unfortunately, as described above, passively cooling such an overheated crucible may introduce undesirable delays into the measurement process, especially when it is desirable to measure many samples in succession with the minimum possible time delay between measurements.
[0085] Problems associated with delays in passively cooling an overheated crucible can be overcome by replacing the crucible with a different crucible that has been preheated to a lower temperature. This process is shown diagrammatically in Figure 5A, where the overheated crucible 20 is replaced with a second preheated crucible 22.
[0086] 4 provides a flow chart illustrating an exemplary method including replacing an overheated crucible to minimize inter-measurement delays in successive measurements. This exemplary flow chart begins at step 316 of FIG. 3 and corresponds to a determination that an empty crucible has a temperature that is too hot to meet the crucible temperature criteria, as shown at 400. As shown at 410, this crucible is replaced with a second, pre-heated crucible. The second crucible may have a temperature that meets the crucible temperature criteria (as shown in FIG. 5A) or may have a temperature that exceeds the maximum allowable temperature of the crucible criteria but is still below the temperature of the first crucible, thereby resulting in a shorter time delay before the second crucible cools to a temperature that meets the crucible temperature criteria.
[0087] The first (heated) crucible, after being replaced with the second crucible, may be supported on a crucible holder integral with the LIBS measurement system (e.g., integral with a common movable support). As shown in FIG. 5A, the first crucible 20 may be placed on a crucible support 32 (e.g., a ladle support bracket) that was previously used to support the second crucible. Alternatively, the first crucible 20 may be placed on a separate crucible support. The crucible support 32 may be configured such that its effective thermal mass dissipation rate and degree of thermal contact with the attached crucible promote suitable rapid cooling of the crucible.
[0088] The second crucible is then used to perform LIBS measurements on a new molten metal sample after steps 330-350 of Figure 3, as shown in step 420 of Figure 4. Furthermore, this process can be repeated one or more times on different samples, reusing the second crucible, as shown in step 424.
[0089] During use of the second crucible, the first crucible is supported by the additional crucible support 32 and passively cools from its initially heated state. Again, as shown in FIG. 5A, the temperature of the first crucible may be intermittently measured to determine when the first crucible meets the crucible temperature criteria. For example, the temperature sensor 210 may be fixed relative to the LIBS measurement head 200, which is translated to facilitate interrogation of the first crucible 20 present in the crucible support 32 between uses of the LIBS measurement head 200 for LIBS measurements. In an alternative exemplary embodiment, a separate temperature sensor may be provided to monitor the temperature of the crucible present in the additional crucible support 32. For example, a temperature sensor (such as, but not limited to, an infrared pyrometer or a thermocouple sensor) may be integrated with the additional crucible support 32 to monitor the temperature of the first crucible, as shown, for example, at 222 in FIG. 1. Again, an indication may be provided to the operator when the first crucible meets the crucible temperature measurement criteria. Alternatively, the temperature of the first crucible may be displayed to allow the operator to determine when the first crucible meets the predetermined crucible temperature criteria.
[0090] 4, after repeated uses of the second crucible, the temperature of the second crucible may no longer meet the crucible metrology criteria and the second crucible may need to be cooled before further use. In such a case, rather than allowing the second crucible to passively cool until its temperature meets the crucible temperature criterion, the second crucible may be replaced with another crucible.
[0091] Step 450 illustrates an exemplary scenario in which the second crucible is replaced with a pre-heated third crucible. Alternatively, as shown in step 460, the second crucible may be replaced with the first crucible because the first crucible has cooled during use of the second crucible for LIBS measurements. These options are illustrated diagrammatically in FIG. 5B, which shows that the second crucible 22 is replaced with either the first crucible 20 or the third crucible 24 (present on the third crucible support 34). The second crucible is then passively cooled, as shown at 445, while LIBS measurements are performed on additional molten metal samples using the first crucible and the third crucible, as shown at 455 and 465, respectively.
[0092] While the exemplary embodiments above use one or two additional crucible supports, three or more crucible supports may be included to provide additional locations for crucible cooling. The number of crucible supports required may depend on the analysis speed and the need to ensure continuous operation when measuring from multiple sampling points.
[0093] As described above, in some exemplary implementations, the LIBS measurement head 200 may be in a parked position prior to performing a LIBS analysis. For example, the LIBS measurement head may be laterally translated (e.g., robotically translated) to a parked position during monitoring of the molten metal sample to ensure line of sight for non-contact temperature sensing. The LIBS measurement head may also be translated to a parked position to perform one or more calibration steps, as described in more detail below.
[0094] 6 illustrates a system state in which the LIBS measurement head 200 is parked in a lateral position to enable non-contact temperature sensing of the molten metal sample by the temperature sensor 210. The LIBS measurement head 200 includes a heat shield 220 positioned to insulate the LIBS measurement head 200 from heat radiated by the crucible 20. FIG 6 illustrates a non-limiting exemplary embodiment in which the heat shield 220 is fixed to the LIBS measurement head 200 such that the heat shield 220 is between the LIBS measurement head 200 and the crucible 20 when the LIBS measurement head 200 is in the parked position.
[0095] In some exemplary embodiments, one or more calibration devices may be used to calibrate the LIBS measurement head 200 when the LIBS measurement head 200 is in the parked position. FIG. 1 illustrates an exemplary implementation in which the system includes a calibration section 500 accessible by the LIBS measurement head 200 in the parked position 201. As illustrated in FIG. 1, the calibration section 500 may be interfaced with (e.g., controlled by) the processing and control circuitry 100, as indicated at 502. When the support 50 is a mobile support and the mobile LIBS system is used in a non-laboratory environment, an integrated calibration section may be used to ensure accurate operation of the system even in the presence of difficult environmental conditions such as high temperatures and dust.
[0096] For example, during some implementations of a LIBS analysis, it may be beneficial to ensure that the distance between the liquid metal surface and the excitation and detection optics (e.g., distal regions of the LIBS measurement head 200) does not change. This distance may be controlled using any suitable type of distance sensor that provides feedback to the mechanical translation mechanism of the LIBS measurement head 200. However, during a measurement run, the LIBS measurement head may be subject to heating due to significant changes in ambient temperature and heat dissipation from the sample and measurement ladle, which may be exacerbated in non-laboratory environments such as aluminum smelter pot rooms. To ensure fast and repeatable measurements, a calibration section may be incorporated into the system (e.g., supported with the LIBS system by a common movable support structure), which allows the distance sensor to be calibrated prior to a given measurement (optionally each measurement), thus at least partially compensating for thermal drift in the system.
[0097] An exemplary embodiment of a calibration unit for calibrating the distance sensor is shown in FIG. 7A. The LIBS measurement head 200 includes a distance sensor 510, and the remainder of the LIBS measurement subsystem (including, for example, power and detection components) is shown generally at 205. The LIBS measurement head 200 is shown in a parked position remote from the crucible, and the distance sensor resides on a calibration reference surface 522 of the distance sensor calibration unit 520. The calibration reference surface 522 defines a fixed reference position that can be used to calibrate the distance sensor 510. For example, the LIBS measurement head 200 can be lowered (manually or robotically) in a direction parallel to the optical axis of the LIBS measurement head 200 until the LIBS measurement head 200 contacts a contact location 526 (which contact can be detected by a contact sensor, such as, for example, a conductive or mechanical contact sensor). Contact between the distal end of the LIBS measurement head 200 (or another suitable location within the distal region of the LIBS measurement head) and contact location 526 of the distance sensor calibration portion 520 ensures that the distance sensor 510 and the reference surface 522 are separated by a known distance, thereby facilitating calibration of the distance sensor 510 via interrogation of the reference surface by the distance sensor 510.
[0098] 7B shows an alternative exemplary embodiment, where distance sensor calibrator 530 is resiliently biased, for example by one or more springs 535 or other suitable resiliently deformable components that may be used to ensure that a known spatial offset is maintained between distance sensor 510 and reference surface 522 when LIBS measurement head 200 is further lowered after contacting contact surface 526, without having to rely on a separate contact sensor. One or more springs 535 may also beneficially ensure that reference surface 522 is at an accurately and repeatably uniform height relative to LIBS measurement head 200 when contact location 526 is provided as a contact surface, or as a plurality of contact locations defining a contact plane.
[0099] FIG. 7C illustrates an example of a calibration portion 540 for calibrating the optical response of the LIBS subsystem. The exemplary calibration portion 540 supports (e.g., by bracketing) a replaceable solid reference sample of a reference material 545 having a known chemical concentration to correct for drift in the signal response of the LIBS subsystem. For example, an analysis of the solid reference sample is compared to a previous analysis of the same reference sample, and the system is calibrated to adjust for observed differences in the concentration of the detected reference material. In some exemplary implementations, the calibration portion can beneficially facilitate translation and / or rotation functions to ensure that the reference material can be measured at a new location when a subsequent drift-correction measurement is performed. The rotation and / or translation functions can also be used to interrogate multiple reference materials mounted on the calibration portion. This rotation and / or translation of the calibration reference portion 540 can be autonomously controlled by the control and processing circuitry 100, for example, as shown at 502 in FIG. 1. FIG. 7C shows an exemplary embodiment in which motor 550 is controlled to rotate a solid reference sample about the LIBS interrogation location when performing subsequent calibrations.
[0100] In some exemplary embodiments, the calibration unit may facilitate multiple calibrations, including but not limited to, calibration of the distance sensor and the use of one or more reference materials to calibrate the response of the LIBS measurement system. In some exemplary implementations, one or more calibration steps may be performed autonomously when one or more conditions are met, such as, for example, after a selected number of samples are measured, after a detected change in the detection surrounding conditions, and / or after an elapsed time.
[0101] Referring again to FIG. 1 , the LIBS subsystem is supported on a support 50. As mentioned above, in some exemplary implementations, the support 50 can be a mobile (portable) support. For example, the support 50 can be a manually movable cart or a generator-powered vehicle (e.g., a cart with battery-powered translation), including a semi-autonomous (self-driving) vehicle. In some exemplary embodiments, the portable LIBS system can be battery-powered. As mentioned above, the present exemplary method, including passive cooling and temperature monitoring prior to the start of LIBS measurements, is well suited to battery-powered implementations due to the absence of an active heating source with high power requirements.
[0102] 8 shows an example of a mobile LIBS measurement system including a LIBS subsystem (200, 205), a primary crucible support 30 for supporting a crucible in a measurement position for performing a LIBS measurement, at least one additional crucible support (this exemplary system includes two additional crucible supports 32 and 34) for supporting an additional crucible during passive cooling before being used during a LIBS measurement, a battery power source 260, and a mobile support 55. FIG 9 shows the inclusion of a calibration portion 500 in a mobile configuration, with the calibration portion 500, the LIBS subsystem, and one or more crucible supports (e.g., crucible supports 30, 32, and 34) supported by the mobile support 55.
[0103] It should be noted that while many of the present exemplary embodiments relate to portable LIBS systems, in other exemplary embodiments, the support supporting the LIBS metrology subsystem may be a fixed support. For example, any of the present exemplary systems and methods may be adapted to a non-portable configuration, such as a system configuration suitable for implementation in a furnace, launder, or other fixed source of liquid metal in either a plant / refinery or laboratory environment. In such a setting, sampling may be beneficially automated (e.g., by using a robotic arm).
[0104] Furthermore, while many of the exemplary embodiments described above employ passive cooling of the molten metal sample prior to LIBS analysis and / or passive cooling of the overheated crucible prior to further use, it should be understood that some embodiments may employ active heating and / or active cooling. For example, in some exemplary embodiments, forced air may be used to cool the overheated empty crucible present on the crucible support. Feedback from a temperature sensor measuring the temperature of the crucible may be used to control a cooling device to bring the empty crucible to a temperature that meets the crucible temperature criteria. Active heating may also optionally employ one or more preheated crucibles. For example, in some exemplary embodiments, one or more crucible supports may include a heat source (e.g., an induction or resistance heating element, or a gas burner). Feedback from a temperature sensor measuring the temperature of the crucible may be used to control the heat source to bring the empty crucible to a temperature that meets the crucible temperature criteria. In some exemplary embodiments, the system may include both active heating and cooling devices to control the temperature of one or more crucibles.
[0105] In other exemplary embodiments, active heating (such as induction heating) and / or cooling (such as forced air cooling) may be used in combination with monitoring the temperature of the molten metal sample along with the crucible to stabilize the temperature of the molten metal sample prior to or during LIBS measurements.
[0106] Embodiments of the present disclosure may be applied to a wide variety of metals and metal alloys, such as, but not limited to, aluminum, steel, steel alloys, iron, iron alloys, copper, zinc, lead, and other metals and metal alloys in the liquid state, and may be useful in industrial environments and applications as mentioned above.
[0107] It will be understood that the present disclosure is not intended to be limited to the analysis of any particular element and may be used to determine both the concentration of major or trace components of a metal or alloy sample. Thus, in some embodiments, the method and / or apparatus is for determining the true bulk concentration of one or more elements selected from aluminum, silicon, phosphorus, sulfur, chloride, calcium, magnesium, sodium, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, zirconium, strontium, niobium, molybdenum, ruthenium, rhodium, palladium, silver, cadmium, tin, antimony, wolfram, rhenium, iridium, platinum, gold, mercury, lead, and bismuth in a liquid metal or alloy sample. The method is also suitable for quantifying very light impurity elements that are difficult to detect using certain other analytical methods, such as hydrogen, lithium, beryllium, boron, and carbon. Furthermore, it will be understood that trace impurities may be introduced into the liquid metal from the sampling equipment itself, such as, for example, the sampling ladle and the measuring crucible. The present disclosure is equally applicable to the measurement and identification of such contaminants.
[0108] 1, a LIBS system typically includes excitation and detection means for generating and receiving atomic emission from a sample, including, but not limited to, all variations of laser-induced plasma excitation methodologies known in the art, including, but not limited to, the use of conventional LIBS methods, LIBS with dual collinear or non-collinear pulses, combined LIBS / discharge methods, etc.
[0109] In some exemplary embodiments, the spectral analysis is based on the LIBS method, in which a series of one or more laser pulses are directed to the sample surface via excitation optics, and the light emitted from the sample is received via receiving optics and transmitted to a detector for recording the spectral information of the detected light. The light detection method and the subsequent processing of the detected emission are known per se to those skilled in the art. Thus, from the spectral information, one or more emission peaks are analyzed and typically compared to a calibration value to realize a quantitative determination of one or more elements.
[0110] The excitation optics and receiving optics of the LIBS metrology subsystem may be completely separate optical elements or may include partly the same optical elements. In a preferred embodiment, the excitation means and receiving optics may be accurately positioned at a predefined distance from the sample surface for each individual excitation event. The accuracy of this positioning over time during field operation is advantageously maintained using a distance calibration function, as described above.
[0111] The pulsed excitation lasers used in the various exemplary embodiments may be of a conventional type, such as those typically used in current LIBS configurations. In accordance with the present invention, stable excitation conditions may involve optical excitation configured such that a sufficiently large and reproducible amount of the liquid metal sample is ablated during excitation, and such that the chemical composition of the ablated portion of the sample is representative of the composition of the entire sample.
[0112] In some embodiments, to maintain an inert atmosphere during LIBS measurements, a flow of inert gas, such as argon, helium, or nitrogen, is supplied from a source, such as a pressurized canister mounted on the same portable support as the LIBS system, through one or more gas flow paths to near the sampling point.
[0113] In some exemplary embodiments, the receiving optics of the LIBS measurement head may include two or more lenses, which are optionally arranged radially around the contact point of the laser pulse and the sample surface. The light collected by one or more receiving optics may be transmitted to the same or different spectrometers (e.g., each lens of the multiple lenses, if the lens can transmit light to each spectrometer) via optical fiber or other optical transmission means. In some embodiments, such multiple spectrometers may be configured such that each spectrometer collects emission in a limited wavelength range, such that the multiple spectrometers together cover a desired wavelength range. In some embodiments, the detection by the spectrometer may also include detection of selected wavelength bands using one or more suitable bandpass filters and optical sensors.
[0114] Referring again to FIG. 1, control and processing circuitry 100 is shown including one or more processors 110 (e.g., CPU / microprocessor), a bus 105, memory 115 which may comprise random access memory (RAM) and / or read-only memory (ROM), a data acquisition interface 120, a display 125, external storage 130, one or more communication interfaces 135, a power source 140, and one or more input / output devices and / or interfaces 145 (e.g., user input devices such as a speaker, a set of push buttons, a joystick, a keyboard, a keypad, a mouse, a position tracking stylus, a position tracking probe, a foot switch, and / or an acoustic transducer for capturing voice commands).
[0115] The above exemplary methods may be performed autonomously in accordance with modules 155, 160, and 165 of control and processing circuitry 100. For example, measuring the temperature of the empty crucible, monitoring the temperature of the molten metal sample, and evaluating the crucible temperature criteria and the measurement temperature criteria may be performed in accordance with executable instructions executed by temperature monitoring module 155. Robotic control of the LIBS measurement head (and optionally one or more components of calibration portion 500) may be controlled in accordance with robotic actuation module 160, and LIBS measurement acquisition and data processing may be performed in accordance with LIBS measurement module 165.
[0116] It should be understood that the exemplary system shown in Figure 1 illustrates a non-limiting example embodiment and is not intended to be limited to the components shown. Additionally, one or more components of the control and processing circuitry 100 may be provided as external components interfaced to a processing device.
[0117] For example, the control and processing circuitry may include a local computing subsystem including a first set of components supported by the support 50, the local computing subsystem being connectable to one or more external computing devices via a network. The network may include local and / or external networks, one or more segments of the network may be wireless. For example, in some implementations, data acquired locally and optionally processed by the local computing subsystem may be transmitted to one or more external computing devices, such as an external control system or one or more mobile computing devices, such as mobile phones, laptops and tablet computing devices, located within or remote from the metal processing plant. Examples of such data include raw data, analysis results, and / or equipment status (which may include, for example, environmental variables, error messages, alerts, or other means or indications). Communication between the local computing subsystem and one or more external computing devices may be unidirectional (e.g., for autonomous uploading of data to a remote computing device) or bidirectional. In some exemplary implementations, the local computing subsystem may be configured to receive one or more portable computing devices in a "docked" configuration for transmitting data via a wired or wireless connection.
[0118] Although only one of each component is illustrated in FIG. 1, any number of each component may be included in the control and processing circuitry 100. For example, a computer typically includes several different data storage media. Furthermore, while the bus 105 is illustrated as a single connection between all of the components, it will be understood that the bus 105 may represent one or more circuits, devices, or communication channels (which may optionally include wireless communication channels) coupling two or more of the components. For example, in a personal computer, the bus 105 includes or is a motherboard. The control and processing circuitry 100 may include more or fewer components than are illustrated.
[0119] The control and processing circuitry 100 may be implemented as one or more physical devices coupled to the processor 110 via one of a number of communication channels or interfaces. For example, the control and processing circuitry 100 may be implemented using an application specific integrated circuit (ASIC). Alternatively, the control and processing circuitry 100 may be implemented as a combination of circuitry and software, where the software is loaded into the processor from a memory or via a network connection.
[0120] Some aspects of the present disclosure may be embodied at least partially in software. That is, the present technology may be executed in a computer system or other data processing system in response to a processor thereof, such as a microprocessor, executing sequences of instructions contained in a memory, such as a ROM, a volatile RAM, a non-volatile memory, a cache, a magnetic and optical disk, or a remote storage device. Furthermore, the instructions may be downloaded to a computing device over a data network in the form of a compiled and linked version. Alternatively, the logic for performing the above-described processes may be embodied in additional computer and / or machine-readable mediums, such as large scale integrated circuits (LSIs), application specific integrated circuits (ASICs), or discrete circuit components, such as firmware, such as electrically erasable programmable read-only memories (EEPROMs) and field programmable gate arrays (FPGAs).
[0121] A computer-readable medium may be used to store software and data that, when executed by a data processing system, causes the system to perform various methods. The executable software and data may be stored in various locations, including, for example, ROM, volatile RAM, non-volatile memory, and / or cache. Portions of this software and / or data may be stored in any one of these storage devices. In general, a machine-readable medium includes any mechanism that provides (i.e., stores and / or transmits) information in a form accessible by a machine (e.g., a computer, a network device, a personal digital assistant, a manufacturing tool, any device having a set of one or more processors, etc.).
[0122] Examples of computer-readable media include, but are not limited to, recordable and non-recordable types of media such as volatile and non-volatile memory devices, read-only memory (ROM), random access memory (RAM), flash memory devices, floppy and other removable disks, magnetic disk storage media, optical storage media (e.g., compact disks (CDs), digital versatile disks (DVDs), etc.), among others. The instructions may be embodied in digital and analog communication links for electrical, optical, acoustic, or other forms of propagated signals, such as carrier waves, infrared signals, digital signals, etc. As used herein, the terms "computer-readable material" and "computer-readable storage medium" refer essentially to all computer-readable media, except for transitory propagating signals. EXAMPLES
[0123] The following examples are presented to enable those skilled in the art to understand and practice embodiments of the present disclosure, and should not be construed as limitations on the scope of the disclosure, but merely as illustrative and representative thereof.
[0124] 10 shows results of an analysis of liquid aluminum samples from hundreds of reduction cells performed using passive cooling and automated initiation of LIBS measurements according to an embodiment of the present disclosure compared to results from a laboratory spark OES analysis of conventionally prepared solid samples. Data from several primary aluminum smelters are combined. The measurements were performed using a portable battery-powered LIBS analyzer mounted on an electric vehicle incorporating distance calibration capabilities and three interchangeable measurement ladles as described above.
[0125] Prior to introducing the molten aluminum sample into the measurement crucible, the measurement crucible was preheated to a temperature that satisfied the crucible temperature criteria. After introducing a given molten aluminum sample into the measurement crucible, the temperature of the molten aluminum sample was monitored using a non-contact pyrometer while passively cooling the molten aluminum sample without performing any active heating or cooling of the crucible. LIBS measurements were performed upon satisfaction of the measurement temperature criteria as explained above.
[0126] As shown in FIG. 10, the agreement (within one standard deviation) between the results from the portable LIBS measurements and the laboratory reference measurements was better than 90 ppm for Fe and better than 30 ppm for Si, as shown diagrammatically by the width of the grey line in the figure.
[0127] Measurements were typically collected continuously from up to 50 reduction cells, and the portable LIBS system features of this example allowed an average cycle time of approximately 90 seconds per cell, which included the time to sample the aluminum from the cells, cool the aluminum to meet the measurement temperature criteria, perform the LIBS measurement, and transport the analyzer between cells using an electric vehicle.
[0128] It should be understood that the particular embodiments described above are shown by way of example, and that these embodiments may be susceptible to various modifications and alternative forms. It should also be understood that the claims are not intended to be limited to the particular forms disclosed, but rather are intended to cover all modifications, equivalents, and alternatives falling within the spirit and scope of the disclosure.
Claims
1. 1. A method for performing laser-induced breakdown spectroscopy (LIBS) on a molten sample while the molten sample is cooling, comprising the steps of: monitoring a temperature of the molten sample during cooling of the molten sample in the crucible and comparing the temperature of the molten sample to a measured temperature criterion; determining that the temperature of the molten sample satisfies the measurement temperature criterion and initiating a LIBS measurement on the molten sample; A method comprising:
2. Prior to the introduction of the molten sample, measuring the temperature of the crucible while the crucible is in a pre-heated state and the molten sample is absent at one or more times and comparing the temperature of the crucible to a crucible temperature criterion; determining that the temperature of the crucible satisfies the crucible temperature criterion to provide an indication that the crucible is ready to receive the molten sample; the crucible temperature criterion is configured such that the molten sample cools by less than 50° C. during the LIBS measurement; The method of claim 1.
3. The method of claim 2 , wherein the crucible temperature criterion includes a minimum crucible temperature such that the crucible temperature criterion is satisfied when the minimum crucible temperature is exceeded.
4. 4. The method of claim 3, wherein the minimum crucible temperature is between 100° C. and 60% of the melting point temperature of the molten sample, in degrees Celsius.
5. 4. The method of claim 3, wherein the minimum crucible temperature is between 15% of the melting point temperature and 60% of the melting point temperature of the molten sample in degrees Celsius.
6. The method of claim 2 , wherein the crucible temperature criterion is met when the temperature of the crucible is within a crucible temperature range.
7. 7. The method of claim 6, wherein a maximum crucible temperature of the crucible temperature range is defined such that the temperature of the crucible is equal to the maximum crucible temperature and that when the molten sample is added to the crucible, the temperature of the molten sample meets the measurement temperature criterion within one minute.
8. 7. The method of claim 6, wherein a maximum crucible temperature of the crucible temperature range is defined such that the temperature of the crucible is equal to the maximum crucible temperature and that when the molten sample is added to the crucible, the temperature of the molten sample meets the measurement temperature criterion within 30 seconds.
9. 8. The method of claim 7, wherein the maximum crucible temperature is between 50% of the melting point temperature and 90% of the melting point temperature of the molten sample in degrees Celsius.
10. The method according to any one of claims 1 to 9, wherein the measurement temperature criterion is selected such that the LIBS measurement is performed within a preselected measurement temperature range.
11. 10. The method of claim 1, wherein the measurement temperature criteria includes a preselected measurement temperature, and the LIBS measurement is initiated immediately after (i) determining that the temperature of the molten sample is equal to the preselected measurement temperature, and (ii) positioning a LIBS measurement head over the crucible.
12. 10. The method of claim 1, wherein the measurement temperature criteria comprises a preselected measurement temperature, and the LIBS measurement is performed after determining that the temperature of the molten sample is equal to the preselected measurement temperature.
13. 13. The method of claim 12, wherein the preselected measurement temperature exceeds the melting point temperature of the molten sample by an amount in the range of 5% to 25% of the melting point temperature in degrees Celsius.
14. 10. The method of any one of claims 1 to 9, wherein the measurement temperature criteria comprises a preselected measurement temperature range, and the LIBS measurement is performed while the temperature of the molten sample is within the preselected measurement temperature range.
15. 10. The method of any one of claims 2 to 9, wherein the measurement temperature criterion is configured such that when the crucible temperature criterion is met, the temperature of the molten sample during the LIBS measurement exceeds the temperature of the crucible.
16. 16. The method of any one of claims 2 to 15, wherein the crucible is pre-heated by a pre-metered molten sample, and the pre-metered molten sample is discarded before measuring the temperature of the crucible.
17. 16. The method of any one of claims 2 to 15, wherein the molten sample comprises aluminium and the crucible is preheated by contact with a crust of cryolite formed on the top of a reduction cell.
18. The method according to any one of claims 2 to 17, wherein the temperature of the crucible and the temperature of the molten sample are measured using a common temperature sensor.
19. The method of any one of claims 2 to 18, wherein the temperature of the crucible and the temperature of the molten sample are measured without contact.
20. The method of any one of claims 2 to 19, wherein the crucible is supported by a crucible support during LIBS measurement.
21. 21. The method of claim 20, wherein LIBS metrology is performed by a LIBS subsystem, a metrology head of the LIBS subsystem is movable from a parked position to an operating position in which the metrology head is above the crucible support, and a heat shield is positioned to insulate the metrology head from heat emitted from the crucible when the metrology head is in the parked position.
22. The method according to any one of claims 2 to 21, wherein the crucible is a metallic crucible.
23. 23. The method of claim 22, wherein the crucible is formed from structural steel.
24. The method according to any one of claims 2 to 21, wherein the heat capacity of the crucible is between 400 J / K and 500 J / K.
25. The method according to any one of claims 2 to 21, wherein the thermal conductivity of the crucible is between 40 W / mK and 50 W / mK.
26. the crucible is a first crucible, the molten sample is a first molten sample, and the method comprises: discarding the first molten sample from the first crucible; and Measuring the temperature of the first crucible; determining that the temperature of the first crucible does not meet the crucible temperature criterion due to an excessively high temperature; replacing the first crucible with a second crucible having a temperature less than the temperature of the first crucible; The method of any one of claims 6 to 8, further comprising performing LIBS measurements on a second molten sample using the second crucible while cooling the first crucible.
27. the first crucible is supported by a primary crucible support during the LIBS measurements performed on the first molten sample; 27. The method of claim 26, wherein after exchanging the first crucible for the second crucible, the first crucible is placed on a secondary crucible support for cooling.
28. Before replacing the first crucible with the second crucible, preheating the second crucible; monitoring the temperature of the second crucible; and indicating when the second crucible meets the crucible temperature criterion; and 27. The method of claim 26, further comprising:
29. Optionally, performing LIBS measurements on one or more additional molten samples using the second crucible; and Emptying the second crucible; and Measuring the temperature of the second crucible; and determining that the temperature of the second crucible does not meet the crucible temperature criterion due to an excessively high temperature; and The second crucible is the first crucible, and replacing the selected crucible with a third crucible; and performing LIBS measurements on additional molten samples using the selected crucible; and The method of any one of claims 26 to 28, further comprising:
30. The method of any one of claims 1 to 29, wherein the LIBS measurements are performed by a LIBS system present on a portable support structure, the LIBS system being powered by a battery.
31. 1. A method for performing laser-induced breakdown spectroscopy (LIBS) on a molten sample while the molten sample is cooling, comprising the steps of: Preheating the crucible; Introducing a molten sample into the crucible; monitoring a temperature of the molten sample during cooling of the molten sample in the crucible and comparing the temperature of the molten sample to a measured temperature criterion; determining that the temperature of the molten sample meets the measurement temperature criterion and initiating a LIBS measurement on the molten sample.
32. After pre-heating the crucible and before introducing the molten sample into the crucible, measuring the temperature of the crucible at one or more times and comparing the temperature of the crucible to a crucible temperature criterion; determining that the temperature of the crucible satisfies the crucible temperature criterion and providing the molten sample to the crucible; 32. The method of claim 31 , wherein the crucible temperature criterion is configured such that the molten sample cools by less than 50° C. during the LIBS measurement.
33. 1. A system for performing laser-induced breakdown spectroscopy (LIBS), the system comprising: A temperature sensor; a laser-induced breakdown spectroscopy (LIBS) subsystem; and a processing circuit operatively coupled to the temperature sensor and the LIBS subsystem, the processing circuit comprising at least one processor and associated memory, the memory including instructions executable by the processor to perform operations, the operations including: monitoring a temperature of the molten sample during cooling of the molten sample in the crucible with the temperature sensor; determining that the molten sample meets a measurement temperature criterion and controlling the LIBS subsystem to initiate a LIBS measurement on the molten sample; and a processing circuit including:
34. Prior to introducing the molten sample into the crucible, the processing circuitry Measuring the temperature of the crucible with the temperature sensor, the crucible being pre-heated; providing an indication that the crucible is ready to receive the molten sample after determining that the temperature of the crucible satisfies a crucible temperature criterion; 34. The system of claim 33, wherein the crucible temperature criterion is configured such that the molten sample cools by less than 50° C. during the LIBS measurement.
35. 1. A portable system for performing laser-induced breakdown spectroscopy (LIBS), the portable system comprising: a laser-induced breakdown spectroscopy (LIBS) subsystem comprising a measurement head, the LIBS subsystem being connectable to a battery; a primary crucible support, the measurement head of the LIBS subsystem being movable from a parked position to an operating position, the measurement head residing on the primary crucible support in order to perform LIBS measurements on a molten sample residing in a crucible supported by the primary crucible support; a secondary crucible support capable of supporting and cooling an additional crucible; a movable support structure configured to support the LIBS subsystem, the primary crucible support, and the secondary crucible support; A portable system comprising:
36. a temperature sensor configured to monitor a temperature of the crucible present within the primary crucible support when the measurement head is in the parked position; A processing circuit operably coupled to the temperature sensor, the processing circuit comprising at least one processor and associated memory, the memory including instructions executable by the processor to perform operations, the operations including: measuring a temperature of the crucible supported by the primary crucible support with the temperature sensor; providing an indication that the crucible should be cooled within the secondary crucible support prior to use after determining that the temperature of the crucible does not meet a crucible temperature criterion due to an excessively high temperature; and 36. The portable system of claim 35, further comprising:
37. 37. The portable system of claim 35 or 36, further comprising the crucible and the additional crucible, wherein the crucible and the additional crucible are made of metal.
38. 38. The portable system of claim 37, wherein the crucible and the additional crucible are formed from structural steel.
39. 37. The portable system of claim 35 or 36, further comprising the crucible and the additional crucible, the heat capacity of the crucible and the additional crucible being between 400 J / K and 500 J / K.
40. 37. The portable system of claim 35 or 36, further comprising the crucible and the additional crucible, the thermal conductivity of the crucible and the additional crucible being between 40 W / m-K and 50 W / m-K.
41. 1. A portable system for performing laser-induced breakdown spectroscopy (LIBS), the portable system comprising: a laser-induced breakdown spectroscopy (LIBS) subsystem comprising a measurement head, the LIBS subsystem being connectable to a battery; an integrated calibration device; a movable support structure configured to support the LIBS subsystem and the integrated calibration device; A portable system, wherein the measurement head of the LIBS subsystem is movable from an operating position above a crucible support, where the measurement head performs LIBS measurements on a molten sample present in the crucible, to a calibration position suitable for performing calibration measurements suitable for calibrating at least one parameter of the LIBS subsystem.
42. 42. The portable system of claim 41, wherein the integrated calibration device includes a LIBS calibration reference material suitable for calibrating a signal of the LIBS subsystem when the measurement head is in the calibration position.
43. 43. The portable system of claim 42, wherein the integrated calibration device comprises a support frame, and the LIBS calibration reference material is movable relative to the support frame such that when the measurement head is repositioned at the calibration position to perform a subsequent calibration measurement, different regions of the LIBS calibration reference material can be optically interrogated by the measurement head, thereby facilitating reuse of the LIBS calibration reference material during multiple calibration measurements.
44. 42. The portable system of claim 41 , wherein the measurement head comprises a distance sensor, and the integrated calibration device is an integrated distance sensor calibration device, the integrated distance sensor calibration device including a contact location and a target location, the contact location being located on the integrated calibration device such that when the measurement head is in the calibration position and in contact with the contact location after lowering the measurement head along a direction parallel to an optical axis of the measurement head, there is a known spatial offset between the distance sensor and the target location, thereby facilitating calibration of the distance sensor.
45. 45. The portable system of claim 44, wherein the integrated distance sensor calibration device is resiliently biased such that the known spatial offset is maintained when the measurement head is moved along the direction after contacting the contact location.
46. a primary crucible support for supporting the crucible during the LIBS measurement; A portable system according to any one of claims 41 to 45, further comprising a secondary crucible support capable of supporting and cooling an additional crucible.
Citation Information
Patent Citations
Device and method for quickly detecting temperature and components of vacuum induction furnace
CN112525888A
Proximate analyzer and its application method
JP1983162840A
Plasma melting device and plasma melting method
JP2015068576A
Handheld laser induced breakdown spectroscopy device
US20150103334A1
Handheld LIBS spectrometer
US20160084709A1