Optical Sensors
A TSPP-DAR coating with optional PSS layers and polytetrafluoroethylene membranes enhances the stability and reliability of optical sensors for ammonia detection, addressing instability issues in existing sensors.
Patent Information
- Application Number
- JP2024516367
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-13
- Filing Date
- 2022-09-09
- Publication Date
- 2024-10-16
AI Technical Summary
Existing optical sensors for ammonia detection suffer from instability due to the hydrophilic nature of porphyrins, leading to swelling and sensitivity to humidity, which affects their performance and reliability.
A coating comprising tetrakis(4-sulfophenyl)porphine (TSPP) crosslinked with diazo resin (DAR) is applied to optical sensors, optionally with poly(styrene sulfonate) (PSS), forming alternating layers to enhance stability, and protected by expanded polytetrafluoroethylene membranes.
The coating significantly improves the stability and reliability of optical sensors for ammonia detection by reducing swelling and humidity sensitivity, enabling accurate and reproducible measurements.
Smart Images

Figure 2024537658000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to coatings for optical sensors, optical sensors, and methods of making optical sensors. [Background technology]
[0002] A description of optical fiber chemical sensors is given in Pospisilova, M.; Kuncova, G.; Trogl, J. “Fiber-optic chemical sensors and fiber-optic bio-sensors”, Sensors 2015, 15, 25208-25259, doi: 10.3390 / S151025208. Due to their unique properties, such as small size, resistance to electromagnetic interference and biocompatibility, they facilitate remote real-time measurements with high sensitivity and selectivity. Most importantly, optical fiber sensors (OFS) can be deployed in harsh and corrosive environments due to the chemical inertness of the silica matrix of the fibers. See Kharaz, A; Jones, BE “A distributed optical-fibre sensing system for multi-point humidity measurement.” Sens. Actuators A Phys. 1995, 47, 491-493, doi.org / 10.1016 / 0924-4247(94)00948-H.
[0003] Various geometric shapes of optical fibers are possible. US Pat. Nos. 7,263,246 B1 and 8,703,505 B2 describe U-shaped fibers that have several advantages. First, they have a high sensitivity to the absorption of the evanescent wave, since lower modes are converted to higher modes. Second, they are less prone to breakage than other shapes. Third, the probes are easy to manufacture and suitable for repetition.
[0004] Japanese Patent No. 5388309B2 describes an optical fiber sensor having a composite thin film including at least one layer of silica particles and at least one organic compound film, in which the organic compound film is polyacrylic acid or polyglutamic acid when detecting amine gases such as ammonia and pyridine.
[0005] "Korposh, S.; Kodaira, S.; Selyanchyn, R.; Ledezma, FH; James, SW; Lee, S.-W. "Porphyrin-nanoassembled fiber-optic gas sensor fabrication: Optimization of parameters for sensitive ammonia gas detection." Opt. Laser Technol. 2018, 101, 1-10, doi.org / 10.1016 / j.optlastec.2017.10.027" describes an ammonia gas sensor. A layer of poly(diallyldimethylammonium chloride) (PDDA) and tetrakis(4-sulfophenyl)porphine (TSPP) was deposited on the surface of the core of a hard-clad multimode fiber from which the polymer cladding was removed. The sensor was able to detect ammonia at the limit of 0.5 ppm. However, it was sensitive to humidity because the porphyrin is hydrophilic, and the immobilized polymer swelled. Summary of the Invention
[0006] It is an object of the present invention to provide an optical sensor for detecting ammonia and similar analytes with improved stability.
[0007] In a first aspect, the present invention provides a coating for a transmissive optic of an optical sensor, the coating comprising a TSPP crosslinked with a diazo resin (DAR).
[0008] The present inventors have found that DAR surprisingly improves the stability of TSPP.
[0009] The coating may include alternating layers, each of which includes either a DAR or a TSPP.
[0010] For even greater stability, the coating may include poly(styrene sulfonate) (PSS) and may include alternating layers of (a) a diazo resin and (b) a mixture of TSPP and PSS.
[0011] The DAR may have the formula: [ka] R 1 is hydrogen or an alkyl group, R 2 is hydrogen, 2-SO 3 H or 3-OCH 3 It is.
[0012] For example, the DAR may have the following formula: [ka]
[0013] In a second aspect, the present invention provides an optical sensor for detecting an analyte that modulates the absorption spectrum of tetrakis(4-sulfophenyl)porphine (TSPP), the sensor comprising a transmissive optic, a light source at an input side of the optic, and a detector for detecting at least one frequency of light at an output side of the optic, the optic having a coating as described above.
[0014] To detect ammonia dissolved in water, the sensor may include at least one gas-permeable waterproof membrane that protects the coating of the optical component. The membrane may be expanded polytetrafluoroethylene. An embodiment includes two such membranes in two respective planes between which is the working part of the optical component.
[0015] In certain embodiments, the transmissive optical component comprises an optical fiber, for example a U-shaped optical fiber, however alternative optical components such as prisms or planar waveguides are within the scope of the invention.
[0016] The optical fiber may be housed in a holder for manual use, and a working portion of the optical fiber may extend from the holder. The holder may have an opening through which the optical fiber extends. The membrane may be fastened around the opening.
[0017] In one example, the sensor includes a temperature sensor and is positioned to compensate for temperature dependent variations in the analyte measurement.
[0018] In a third aspect, the present invention provides a method of making an optical sensor comprising immersing at least a portion of a transmissive optical component in a TSPP and a DAR, and crosslinking the TSPP and the diazo resin to form a coating.
[0019] The immersion may include separate immersions in aqueous solutions of the diazo resin and TSPP, e.g., repeated alternating immersions in the separate solutions, hi some embodiments, the solution of TSPP also includes PSS.
[0020] Crosslinking may be carried out using ultraviolet light.
[0021] The method of the present invention may include a subsequent step of protecting a portion of the optical component having a coating with at least one waterproof, gas-permeable membrane.
[0022] In one embodiment of the invention, the transmissive optical component comprises an optical fiber. The immersed portion may be a U-shaped bend in the optical fiber, and the method may include a prior step of forming a U-shaped bend in the optical fiber. [Brief description of the drawings]
[0023] Embodiments of the invention will now be described in more detail, by way of example only, with reference to the accompanying drawings, in which:
[0024] [Figure 1] FIG. 1 shows a schematic diagram of an optical fiber coating according to the invention.
[0025] [Diagram 2] FIG. 2 shows a sensor according to the present invention, including its internal components.
[0026] [Diagram 3] FIG. 3 is a partial view of the distal end of the sensor of FIG. 2, including internal components.
[0027] [Figure 4] FIG. 4 is a cutaway view of the distal end shown in FIG. 3, including the internal components.
[0028] [Diagram 5] FIG. 5 is a simplified diagram of the sensor's printed circuit board.
[0029] [Figure 6] FIG. 6 shows the optical transmission spectrum obtained when the optical fiber of a sensor according to the invention is used to detect ammonia in a solution.
[0030] [Figure 7] FIG. 7 shows the normalized light absorption spectrum obtained when the optical fiber of a sensor according to the invention is used to detect ammonia in solution. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] In accordance with the present invention, the coating of the optical component includes a DAR synthesized, for example, as described in "Zhao, C.; Chen, JY; Cao, WX "Synthesis and characterization of diphenylamine diazonium salts and diazoresins." Angew. Makromol. Chem. 1998, 259, 77-82."
[0032] In this particular embodiment, a suitable length of multimode optical fiber, such as 40 cm, can be used to construct a sensor according to the invention. A short section of the plastic cladding of the optical fiber, for example 1 cm, is removed, for example by burning. This section is then bent into a U-shape, for example using a burner. The exposed portion of the silica core is prepared, for example by rinsing several times in ethanol and DI water, and treating with a desiccant, such as 1 wt% ethanol KOH (ethanol / water=3:2, v / v). This creates a negatively charged evanescent field.
[0033] Next, an aqueous solution of positively charged DAR (e.g., 1 wt%) and TSPP (e.g., H 2 1 mM in HO) and optionally PSS (e.g., 2 Electrostatic films are deposited by immersing the negatively charged activated core of the optical fiber alternately in mixtures of 0, 0.025, and 0.1 wt% in O for 15 min each in this example. Each cycle results in a DAR / TSPP or DAR / TSPP+PSS bilayer. Between immersions, the optical fiber may be washed with water and dried by flushing with nitrogen gas. Multilayer assemblies can be formed by cyclic repetition of these two steps. Figure 1 shows only 3.5 bilayers containing DAR (100) and TSPP+PSS (102). However, it is possible to form 5, 8.5, or more than 8.5 bilayers. To avoid decomposition of the DAR, the films are deposited in the dark.
[0034] The deposited bilayer is cured by exposing the optical fiber to UV light. In one embodiment, the wavelength is not more than 365 nm, and the exposure is for 15 minutes at a distance of 10 cm. As a result, the ionic bonds between the diazonium cation ions in the DAR and the sulfonate anion residues in the TSPP (and PSS) are converted to cross-linked covalent bonds by UV light irradiation.
[0035] 2-5 show a sensor incorporating an optical fiber prepared as described above. This sensor is suitable for handheld use. However, sensors of various shapes and sizes can be made in accordance with the present invention using any reasonable length of optical fiber.
[0036] The first cladding portion (10) and the second cladding portion (12) of the optical fiber are partially contained within the handle portion (14) of the sensor and extend through the neck portion (15). The exposed portion (16) of the optical fiber is housed in the head portion (18) of the sensor.
[0037] In the head portion (18), the U-shaped exposed portion (16) extends into a window (20), which in this embodiment is circular. The window is defined by a first frame (22) and a second frame (24) on either side of the head portion (18). A first gas-permeable waterproof membrane (26) and a second gas-permeable waterproof membrane (28) are provided in each frame (22), (24) to prevent water from entering the window (20) and contacting the DAR / TSPP+PSS. The membranes may be expanded polytetrafluoroethylene, such as Gore-Tex®.
[0038] FIG. 5 shows a PCB (2) housed in the base of the sensor, omitting components not described herein. The PCB comprises a cluster (4) of LEDs of different specific wavelengths, all coupled to a first cladding portion (10), and at least one photodetector (6) coupled to a second cladding portion (12). Each LED is individually activated to transmit its light through the first cladding portion (10) to the exposed portion (16) and into the optical fiber. The PCB may also have a microcontroller configured to activate each of the LEDs and record the operation of the photodetector.
[0039] A temperature sensor (29), such as a thermocouple, may be included in the sensor to measure the temperature of the head. Connection of the temperature sensor to the PCB is per item (30) in Figure 2.
[0040] When ammonia comes into contact with the exposed area, the TSPP attenuates the light in the optical fiber at a specific frequency. Figure 6 shows the transmission spectra of ammonia at different concentrations. Figure 7 shows the normalized absorption spectrum (i.e., the spectrum of the sensor itself has been subtracted).
[0041] These spectra show (a) frequencies where the effect of ammonia is significant and (b) frequencies where it has essentially no effect. It is possible to manufacture a sensor according to the invention with a single LED at one of the (a) frequencies and calibrate the sensor with known ammonia concentrations. However, for reproducibility and to account for LED wavelength spread and manufacturing tolerances, a PCB may include LEDs emitting at two or more of the (a) frequencies. The PCB may also include one or more LEDs emitting at at least one of the (b) frequencies for use as a reference.
[0042] To measure the concentration of ammonia in a solution, such as seawater, the head of the sensor is immersed in the solution, so that gaseous ammonia enters the window. To measure the concentration of ammonia in, for example, atmosphere, the head of the sensor is exposed to the atmosphere. Therefore, for sensors used in purely dry atmosphere environments, the waterproof membrane can be omitted.
[0043] The LEDs are operated in sequence and the response at the photodetector is monitored for each LED. A microcontroller, or connected computer, calculates the concentration of ammonia and compensates for the temperature changes sensed by the temperature sensor. The sensor may have its own small display to show the results.
Claims
1. A coating for a transmissive optic of an optical sensor, the coating comprising tetrakis(4-sulfophenyl)porphine (TSPP) crosslinked with a diazo resin (DAR).
2. The coating of claim 1 comprising alternating layers each comprising a DAR and a TSPP.
3. 10. The coating of claim 1 comprising poly(styrene sulfonate) (PSS).
4. 4. The coating of claim 3 comprising alternating layers of (a) a diazo resin and (b) a mixture of TSPP and PSS.
5. The DAR has the formula: 【Chemistry 3】 R 1 is hydrogen or an alkyl group; R 2 is hydrogen, 2-SO 3 H or 3-OCH 3 5. The coating of claim 1 , wherein
6. The DAR has the formula: 【Chemistry 4】 The coating of claim 5.
7. 1. An optical sensor for detecting an analyte that alters the absorption spectrum of a TSPP, comprising: A transmissive optical component; a light source at the input side of the transmissive optical component; a detector at the output of the transmissive optical component for detecting light of at least one frequency; It is equipped with 7. An optical sensor, wherein the transmissive optical component comprises a coating according to any one of claims 1 to 6.
8. 8. The optical sensor of claim 7, including at least one gas-permeable waterproof membrane protecting the coating of the transmissive optic.
9. The optical sensor of claim 8 , wherein the at least one gas-permeable waterproof membrane is made of expanded polytetrafluoroethylene.
10. 10. The optical sensor according to claim 8 or 9, wherein the at least one gas-permeable waterproof membrane is two in number, and between these two planes is an active part of the transmissive optical component.
11. 11. The optical sensor of claim 7, wherein the transmissive optic comprises an optical fiber.
12. The optical sensor of claim 11 , wherein the optical fiber is U-shaped.
13. 13. The optical sensor of claim 11 or 12, wherein the optical fiber is housed in a holder for manual use, and the working portion of the optical fiber extends from the holder.
14. The optical sensor of claim 13 , wherein the holder has an opening through which the working portion of the optical fiber extends.
15. 15. The optical sensor of claim 8, 9 or 10, wherein the at least one gas-permeable waterproof membrane is fastened around the opening.
16. 16. The optical sensor of claim 7, further comprising a temperature sensor configured to compensate for temperature dependent variations in the analyte measurement.
17. 1. A method of manufacturing an optical sensor, comprising the steps of: Immersing at least a portion of a transmissive optical component in a TSPP and a DAR; crosslinking the TSPP and the diazo resin to form a coating; A method comprising:
18. 20. The method of claim 17, comprising separate immersions in an aqueous solution of a diazo resin and an aqueous solution of TSPP.
19. 20. The method of claim 18, comprising alternating immersion in an aqueous solution of a diazo resin and an aqueous solution of TSP.
20. 20. The method of claim 18 or 19, wherein the solution of TSPP further comprises PSS.
21. 21. The method of any of claims 17 to 20, wherein crosslinking is performed using ultraviolet light.
22. 22. The method according to any of claims 17 to 21, comprising the subsequent step of protecting the part of the transmissive optical component carrying said coating with at least one waterproof, gas-permeable membrane.
23. 23. The method of any of claims 17 to 22, wherein the transmissive optical component comprises an optical fiber.
24. 24. The method of claim 23, wherein the immersed portion is a U-shaped bend in the optical fiber.
25. 25. The method of claim 24, including the preliminary step of forming the U-shaped bend in the optical fiber.
Citation Information
Patent Citations
Atmospheric sensor
JP2009236857A
Gas sensor
JP2012122814A
Laminate, organic-semiconductor manufacturing kit, and resist composition for manufacturing organic semiconductor
JP2015087611A
Laminate film and method for manufacturing the same
JP2021024195A
Composite thin film, atmosphere sensor comprising the composite thin film, and optical waveguide sensor
WO2009119796A1