Electroless Anti-Pathogenic Coating
The electroless nickel-copper-phosphorus plating bath addresses the limitations of existing methods by providing a uniform, durable, and antimicrobial coating on diverse substrates, effectively inhibiting pathogens like Staphylococcus aureus and MRSA.
Patent Information
- Application Number
- JP2024524995
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-30
- Filing Date
- 2022-10-25
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing plating methods like electroplating and immersion deposition fail to provide uniform, durable, and effective antipathogenic coatings on both metallic and non-metallic substrates, particularly due to issues such as self-shielding, current density distribution, line-of-sight limitations, and adhesion problems, while electroless nickel plating lacks the efficacy of copper and silver in antimicrobial properties.
Development of an electroless nickel-copper-phosphorus plating bath that forms a uniform nickel-copper-phosphorous alloy coating, which can encapsulate various substrates, including metals and non-metals, offering improved durability and antimicrobial properties.
The electroless nickel-copper-phosphorus coating effectively inhibits the growth of bacteria, fungi, and viruses, including Staphylococcus aureus and MRSA, with enhanced durability and biofilm resistance, achieving nearly complete disinfection within 2 hours.
Smart Images

Figure 2024541237000001 
Figure 2024541237000002 
Figure 2024541237000003
Abstract
Description
[Technical field]
[0001] This application relates to an electroless nickel-copper-phosphorus plating bath, a method for forming an electroless antipathogenic coating on a workpiece, and the electroless antipathogenic coating so formed. [Background technology]
[0002] SARS-CoV-2 is the pathogen that is the cause of coronavirus disease 2019 (COVID-19). The spread of COVID-19 has led to increased awareness of the spread of disease based on the ability of the pathogen to survive on surfaces and infect people who come into contact with the surfaces while the pathogen remains viable. There is an entire industry premised on producing disinfectants that can be sprayed or wiped on surfaces to eliminate the viability of the pathogen and make the surface safe for contact. There are also substances that can be applied to surfaces that maintain their disinfecting properties for some length of time, but must be repeatedly applied to the material to maintain efficacy.
[0003] Rather than applying a disinfectant to a surface, it is also possible to modify the surface so that the surface itself is the disinfecting medium. This can be achieved, for example, by coating the surface with a layer of a metal that has anti-pathogenic properties. The use of a metal anti-pathogenic coating is desirable because the metal coating can provide anti-pathogenic properties without forging heavy parts (e.g., plating on plastic) or use a cheaper metal (iron) in the primary production and then coat the contact surface with a layer of a metal that has anti-pathogenic properties.
[0004] The ability of metals to exhibit biocidal effects is known as the oligodynamic effect. Antipathogenic effectiveness varies from metal to metal, but effectiveness is sometimes evident even at low concentrations, and the two metals with the greatest effectiveness are copper and silver. Both of them have good antipathogenic tendencies, but because they are soft metals, they tend to have poor wear properties when compared to nickel, chromium, or iron, which have poor antipathogenic properties.
[0005] It is desirable to encapsulate the entire substrate or workpiece with a metallic antipathogenic coating so that the entire surface of the substrate can provide antiseptic properties where the substrate is contacted. One way to achieve such encapsulation is by plating the substrate or workpiece. However, not all types of plating provide good results. Electroplating has problems with self-shielding, current density distribution, and line of sight that can potentially result in uncovered areas. Immersion deposition, often referred to as substitution or displacement plating, can provide total coverage, but the deposits are very thin and often involve adhesion problems. Furthermore, deposition can only be performed if the metal to be deposited is more noble than the substrate. Electroplating requires a conductive substrate, while immersion deposition requires a metallic substrate.
[0006] Autocatalytic electroless plating does not encounter any of these problems. Autocatalytic electroless plating allows for the coating of a variety of substrates, both metals (iron and copper bearing) and plastics (plating on plastics), and the electroless deposits can be robust enough to tolerate significant wear from repeated contact. One metal that offers a robust combination of durability and versatility is electroless nickel, typically deposited as a nickel phosphorus alloy. Nickel has some anti-pathogenic properties, but is not as effective as other metals. Summary of the Invention
[0007] The embodiments described herein relate to electroless nickel-copper-phosphorous plating baths that deposit alloys of nickel-copper-phosphorous (NiCuP) having anti-pathogenic properties and improved durability. Advantageously, the electroless nickel-copper-phosphorous baths can provide uniform electroless nickel-copper-phosphorous deposits that can fully encapsulate both metallic and non-metallic substrates.
[0008] In some embodiments, the aqueous electroless nickel-copper-phosphorus plating baths can include about 2.0 g / L to about 8.0 g / L Ni, about 150 ppm to about 1500 ppm Cu, and about 10 g / L to about 50 g / L hypophosphite reducing agent. The electroless nickel-copper-phosphorus baths can provide uniform electroless nickel-copper-phosphorus alloy deposits on substrates that are antipathogenic and / or oligoactive.
[0009] In some embodiments, the concentration of Ni in the bath relative to the concentration of Cu is such that the electroless nickel-copper-phosphorus alloy deposit contains from about 30% to about 85% Cu.
[0010] In some embodiments, the Ni concentration in the bath is about 3 g / L to about 6 g / L. Ni can be provided in the bath by dissolving a water-soluble nickel salt in the bath. The water-soluble nickel salt can be selected from nickel sulfate, nickel chloride, nickel methanesulfonate, nickel sulfamate, nickel fluoroborate, or combinations thereof.
[0011] In some embodiments, the Cu concentration in the bath is about 400 ppm to about 1000 ppm. Cu can be provided in the bath by dissolving a water-soluble copper salt in the aqueous solution. The copper salt can be selected from copper sulfate, copper chloride, copper methanesulfonate, copper sulfamate, copper fluoroborate, or combinations thereof.
[0012] In some embodiments, the bath may have a neutral to alkaline pH, for example, the bath may have a pH of about 8 to about 9.
[0013] In some embodiments, the bath can include about 10 g / L to about 50 g / L of at least one organic acid complexing agent, in some embodiments, the organic acid complexing agent can be a carboxylic acid, such as at least one of malic acid, lactic acid, or succinic acid.
[0014] In other embodiments, the bath may include at least one of a chelating agent, a stabilizing agent, or a pH buffering agent.
[0015] In some embodiments, the bath may consist essentially of water, about 3 g / L to about 6 g / L Ni, about 10 g / L to about 50 g / L hypophosphite reducing agent, about 400 ppm to about 1000 ppm Cu, less than about 25 g / L of an organic acid complexing agent selected from the group consisting of malic acid, lactic acid, and succinic acid, optional stabilizers, and optional pH adjusters. The bath may have a pH of about 8 to about 9.
[0016] Other embodiments described herein relate to a method of forming an electroless anti-pathogenic coating on a surface of a substrate. The method may include providing a substrate and contacting the surface of the substrate with an aqueous electroless nickel-copper-phosphorus plating bath described herein.
[0017] In some embodiments, the surface of the substrate is contacted with the aqueous electroless nickel-copper-phosphorus plating bath by submerging at least a portion of the substrate in the bath. The bath can have a temperature of from about 160° F. to about 195° F. during electroless plating of the surface of the substrate.
[0018] In some embodiments, the surface of the substrate may be in contact with the bath for at least 1 hour. The coating formed using the bath may have a thickness of at least about 50 microinches.
[0019] Still other embodiments described herein relate to electroless nickel-copper-phosphorus alloy coatings comprising at least about 30 wt. % Cu, about 5 wt. % to about 15 wt. % P, the balance being Ni, along with unavoidable impurities.
[0020] In some embodiments, the coating comprises at least about 40% by weight, at least about 50% by weight, or at least about 60% by weight Cu and has a thickness of at least about 50 microinches. The coating may be formed using the baths and / or methods described herein.
[0021] In some embodiments, the coating may be bactericidal, antimicrobial, and / or capable of destroying or inhibiting the growth of microorganisms such as bacteria, fungi, and viruses.
[0022] In other embodiments, the coating may be anti-pathogenic and capable of destroying or inhibiting the growth of bacteria, such as Staphylococcus aureus or Methicillin-resistant Staphylococcus aureus.
[0023] In yet other embodiments, the coating is capable of inhibiting biofilm formation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] In the following specification and claims, reference will be made to a number of terms that shall be defined to have the following meanings.
[0025] The singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise.
[0026] "Optional" or "optionally" means that the subsequently described event or circumstance may or may not occur, and that the description includes cases where the event occurs and cases where it does not occur.
[0027] As used herein throughout the specification and claims, approximating language may be applied to modify any quantitative expression that may be acceptably varied without causing a change in the basic function to which it pertains. In some instances, the approximating language may correspond to the precision of an instrument for measuring a value.
[0028] As used herein, the term "about" refers to a measurable value of a parameter, amount, duration, etc., and is meant to include no more than + / -15% variation, preferably no more than + / -10% variation, more preferably no more than + / -5% variation, even more preferably no more than + / -1% variation, and even more preferably no more than + / -0.1% variation of and from the specifically recited value, so long as such variations are appropriate to practice the invention described herein. It is further to be understood that the values to which the modifier "about" refers are themselves specifically disclosed herein.
[0029] As used herein, the terms "comprises" and / or "comprising" specify the presence of stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof.
[0030] As used herein, the terms "substantially free" or "essentially free" with respect to a particular element or compound, unless otherwise defined herein, mean that the given element or compound is not detectable by conventional analytical means well known to those skilled in the art of metal plating for bath analysis. Such methods typically include atomic absorption spectroscopy, titration, UV-Vis analysis, secondary ion mass spectrometry, and other commonly available analytical techniques.
[0031] The terms "plating" and "depositing" or "deposition" are used interchangeably throughout this specification.
[0032] The terms "composition" and "bath" and "electrolyte" and "solution" are used interchangeably throughout this specification.
[0033] The embodiments described herein relate to electroless nickel-copper-phosphorus plating baths that deposit alloys of nickel-copper-phosphorus (NiCuP) having anti-pathogenic or oligodynamic properties, such as anti-bacterial, anti-fungal, and anti-biofilm properties, as well as improved durability. Advantageously, the electroless nickel-copper-phosphorus baths can provide uniform electroless nickel-copper-phosphorus deposits that can fully encapsulate both metallic and non-metallic substrates.
[0034] In some embodiments, the electroless nickel-copper-phosphorus plating bath used to form the electroless nickel-copper-phosphorus coating comprises Ni ions, Cu ions, a hypophosphite reducing agent, and optionally at least one of a complexing agent, a chelating agent, a stabilizer, and / or a pH buffer. For example, an aqueous electroless nickel-copper-phosphorus plating bath may comprise about 2.0 g / L to about 8.0 g / L of Ni, about 150 ppm to about 1500 ppm of Cu, and about 10 g / L to about 50 g / L of a hypophosphite reducing agent. The electroless nickel-copper-phosphorus bath provides a uniform electroless nickel-copper-phosphorus alloy deposit on a substrate that is antibacterial, antipathogenic, and / or oligoactive.
[0035] In some embodiments, the concentration of Ni in the bath relative to the concentration of Cu is such that the electroless nickel-copper-phosphorus alloy deposit comprises about 20% to about 90% Cu, or about 30% to about 85% Cu, or about 50% to 70% Cu.
[0036] In some embodiments, the Ni concentration in the bath can be about 2 g / L to about 8 g / L or about 3 g / L to about 6 g / L. Ni can be provided in the bath by dissolving a water-soluble nickel salt in the bath. Water-soluble nickel salts can include those that are soluble in the plating bath and can provide an aqueous solution of a predetermined concentration. In one embodiment, the nickel salt can be selected from the group consisting of nickel sulfate, nickel chloride, nickel bromide, nickel iodide, nickel acetate, nickel malate, nickel hypophosphite, nickel methanesulfonate, nickel sulfamate, nickel fluoroborate, and combinations thereof.
[0037] In some embodiments, the Cu concentration in the bath is from 150 ppm to about 1500 ppm or from about 400 ppm to about 1000 ppm. Cu can be provided in the bath by dissolving a water-soluble copper salt in the aqueous solution. The copper salt can be selected from the group consisting of copper sulfate, copper chloride, copper methanesulfonate, copper sulfamate, copper fluoroborate, and combinations thereof.
[0038] The hypophosphite reducing agent used in the bath can include any of a variety of hypophosphite reducing agents used in known types of electroless nickel plating baths, hi some embodiments, the hypophosphite reducing agent is selected from the group consisting of sodium hypophosphite, potassium hypophosphite, ammonium hypophosphite, and combinations thereof.
[0039] The concentration of the hypophosphite reducing agent in the electroless nickel plating bath may vary depending on the type of hypophosphite reducing agent and may be adjusted to vary the concentration of phosphorus in the electroless nickel-copper-phosphorus coating formed using the bath. In some embodiments, the concentration of the hypophosphite reducing agent in the electroless nickel-phosphorus plating bath may be about 10 g / L to about 50 g / L, or about 15 g / L to about 35 g / L, or about 20 g / L to about 30 g / L. In other embodiments, the concentration of the hypophosphite reducing agent in the electroless nickel-copper-phosphorus plating bath may be about 25 g / L.
[0040] In some embodiments, a complexing agent or mixture of complexing agents may be included in the electroless nickel-copper-phosphorus plating bath. The complexing agent used herein may also include a chelating agent. The complexing agent and / or chelating agent generally retards the precipitation of nickel or copper ions as insoluble salts, such as phosphites, from the plating solution by forming more stable nickel complexes with nickel ions or more stable copper complexes with copper ions, providing an adequate reaction rate for nickel or copper precipitation.
[0041] Complexing and / or chelating agents may be included in the plating baths in an amount sufficient to complex the nickel or copper ions present in the bath and to further solubilize hypophosphite decomposition products formed during the plating process. In some embodiments, complexing and / or chelating agents are provided in the electroless nickel-phosphorus plating baths in an amount of less than about 30 g / L, or less than about 25 g / L, or from about 20 g / L to about 30 g / L.
[0042] A variety of complexing agents can be used in known electroless nickel plating solutions. Specific examples of complexing agents include monocarboxylic acids such as glycolic acid, lactic acid, gluconic acid, or propionic acid, dicarboxylic acids such as malic acid, malonic acid, succinic acid, tartaric acid, oxalic acid, or adipic acid, aminocarboxylic acids such as glycine or alanine, ethylenediamine derivatives such as ethylenediaminetetraacetate, versenol (N-hydroxyethylethylenediamine-N,N',N'-triacetic acid) or quadrol (N,N,N',N'-tetrahydroxyethylethylenediamine), phosphinic acids such as 1-hydroxyethane-1,1-diphosphonic acid, ethylenediaminetetramethylenephosphonic acid, and water-soluble salts thereof. Complexing agents can be used either alone or in combination.
[0043] For example, some complexing agents, such as acetic acid or succinic acid, can also act as pH buffers, and the appropriate concentrations of such additive components can be optimized for any plating bath after taking into account their dual functionality.
[0044] In some embodiments, the at least one pH buffering agent, complexing agent, or chelating agent may be selected from the group consisting of acetic acid, formic acid, succinic acid, malonic acid, ammonium salts, lactic acid, malic acid, citric acid, glycine, alanine, glycolic acid, lysine, aspartic acid, ethylene diamine tetraacetic acid (EDTA), and combinations thereof. In some embodiments, mixtures of two or more of the above pH buffering agents, complexing agents, and / or chelating agents may be used in the electroless nickel-copper-phosphorus plating baths described herein.
[0045] In some embodiments, the electroless nickel-copper-phosphorus plating baths can include from about 20 g / L to about 30 g / L of a combination of organic acid complexing agents selected from the group consisting of malic acid, lactic acid, and succinic acid. In other embodiments, the electroless nickel-copper-phosphorus plating baths can include less than about 25 g / L of a combination of organic acid complexing agents selected from the group consisting of malic acid, lactic acid, and succinic acid.
[0046] In addition to the above components, the plating bath may also contain additives having various kinds of purposes, so long as the properties of the plating bath are not impaired. For example, the bath may contain a stabilizer such as lead acetate at a concentration of about 0.0004 g / L to about 0.0007 g / L. Other stabilizers, including metal cations that act as catalyst poisons, such as Pb, Bi, Sn, In, salts or compounds thereof, and combinations thereof, may also be used in addition to or in addition to lead acetate.
[0047] In other embodiments, the electroless nickel-copper-phosphorus plating baths may be free or substantially free of additives such as surfactants that may have adverse effects on the antipathogenic properties, oligodynamic properties, durability, and / or surface morphology of the electroless nickel-copper-phosphorus deposit. Surfactants, including organic compounds from the class of fatty acids and their water-soluble salts, amino compounds, and sulfates and sulfonates of fatty acids and fatty alcohols, are typically used in electroless nickel plating baths to modify the inherent properties of the plating bath itself or the quality of the nickel deposit. However, these additives may potentially form colloids with other components of the bath, such as free Ni or Cu ions, that may produce plating defects. Advantageously, the plating baths described herein may be free or substantially free of such additives to minimize defects such as micropitting and particle deposition in the electroless nickel-copper-phosphorus deposit.
[0048] The aqueous electroless nickel-copper-phosphorus plating baths can be operated or maintained at a neutral to alkaline pH. For example, the baths can have a pH of from about 7 to about 10, more preferably from about 8 to about 9, during the electroless nickel-copper-phosphorus plating of the substrate.
[0049] At least one pH adjuster can be used to adjust the pH to the above ranges. If the pH of the bath is too high, it can be adjusted, for example, by adding an acid. If the pH of the bath is too low, it can be adjusted, for example, by adding ammonium hydroxide.
[0050] The stability of the operating pH of the plating bath can be controlled by adding various buffer compounds, such as acetic acid, propionic acid, boric acid, etc., in amounts up to about 30 g / L, with amounts of about 2 g / L to about 30 g / L being typical. As noted above, some of the buffer compounds, such as acetic acid and succinic acid, can also function as complexing agents.
[0051] In other embodiments, the bath may consist essentially of a combination of water, about 3 g / L to about 6 g / L Ni, about 10 g / L to about 50 g / L hypophosphite reducing agent, about 400 ppm to about 1000 ppm Cu, less than about 25 g / L of an organic acid complexing agent selected from the group consisting of malic acid, lactic acid, and succinic acid, optional stabilizers, and optional pH adjusters.
[0052] According to the methods described herein, substrates or workpieces can be plated with electroless nickel-copper-phosphorus plating baths to provide electroless nickel-copper-phosphorus alloy deposits or coatings on the substrates having antipathogenic or oligodynamic properties and improved durability.
[0053] The substrate can include any substance or material. In some embodiments, the substrate can be a substance onto which the electroless nickel-copper-phosphorus alloy can be deposited. The substrate can also include a substance or material having at least one surface onto which the electroless nickel-copper-phosphorus alloy can be deposited. The substrate can include, for example, metal, plastic, paper, glass, ceramic, textile, rubber, polymer, composite, or any combination of substrates. The substrate can also include at least a portion of an electronic product, a food or agricultural product, a medical device, or the like.
[0054] By way of example, the substrate may be a medical device such as a catheter, an endotracheal tube, a tracheostomy tube, a wound drainage device, a wound dressing, a stent, an implant, an intravenous catheter, a suture, a shunt, a gastrostomy tube, a medical tubing, a cardiovascular product, a heart valve, a pacemaker lead, a guidewire, or a urine collection device.
[0055] The electroless nickel-copper-phosphorus plating bath can be used to plate a substrate by contacting the substrate with or immersing the substrate in the plating bath for a duration effective to form an electroless nickel-copper-phosphorus coating or deposit on at least a portion of a surface of the substrate with a desired thickness.
[0056] In some embodiments, a suitable precleaner may be used to clean or pretreat the substrate prior to plating. During plating, the bath may be maintained at a bath temperature of about 150°F to about 200°F, for example, or from about 160°F to about 195°F. The duration of contact of the electroless nickel-copper-phosphorus plating bath with the substrate to be plated will determine the thickness of the electroless nickel-copper-phosphorus coating. Typically, the contact time may range from as little as about one minute to several hours, or even several days, for example, from about 60 to about 120 minutes. Coatings formed using the bath may have a thickness of at least about 50 microinches, or at least about 100 microinches up to about 500 microinches, or 1,000 microinches, or 2000 microinches.
[0057] Light to heavy agitation may be used during deposition of the electroless nickel-copper-phosphorus deposit or coating. Light agitation may be, for example, light air agitation, mechanical agitation, bath circulation by pump, barrel rotation for barrel plating, mandrel rotation for disk plating, etc. The electroless nickel-copper-phosphorus plating bath may also be subjected to periodic or continuous filtration to reduce the level of contaminants in the bath. Also, in some embodiments, replenishment of the bath components may be performed on a periodic or continuous basis to maintain the concentrations of components, particularly nickel ions, copper ions, and hypophosphite ions, and pH levels within desired limits.
[0058] The electroless nickel-copper-phosphorus alloy coated substrate so formed may be removed from the electroless nickel-copper-phosphorus plating bath and rinsed, for example, with deionized water.
[0059] In some embodiments, the electroless nickel-copper-phosphorus alloy coating so formed comprises at least about 30% by weight Cu, about 5% to about 15% by weight P, the balance being Ni, along with unavoidable impurities.
[0060] In some embodiments, the coating may comprise at least about 40% by weight, at least about 50% by weight, or at least about 60% by weight Cu and have a thickness of at least about 50 microinches. The coating may be formed using the baths and / or methods described herein.
[0061] In some embodiments, the coating may be bactericidal, antimicrobial, and / or capable of destroying or inhibiting the growth of microorganisms such as bacteria, fungi, and viruses.
[0062] In other embodiments, the coating may be anti-pathogenic and capable of destroying or inhibiting the growth of bacteria, such as Staphylococcus aureus or Methicillin-resistant Staphylococcus aureus.
[0063] In yet other embodiments, the coating is capable of inhibiting biofilm formation.
[0064] The following examples are illustrative of the electroless nickel-copper-phosphorus plating solutions of the present invention, in which, unless otherwise indicated herein and in the claims, all parts and percentages are by weight, temperatures are in degrees Fahrenheit, and pressures are at or near atmospheric. EXAMPLES
[0065] An autocatalytic electroless plating system has been developed that can provide a uniform coating on a substrate consisting of a nickel-copper-phosphorus alloy that exhibits enhanced anti-pathogenic properties. In another embodiment, the electroless plating system provides a uniform coating on a substrate consisting essentially of a nickel-copper-phosphorus alloy. By "consisting essentially of" it is meant that the alloy does not include any components that would have an adverse effect on the durability of the alloy deposit and / or would have an adverse effect on the anti-pathogenic properties of the alloy deposit. In another embodiment, the alloy consists of or includes a nickel-copper-phosphorus alloy. The autocatalytic electroless plating system allows for complete encapsulation of the substrate, high durability such that it can withstand many contacts, and copper for enhanced anti-pathogenic properties.
[0066] The following examples demonstrate the improved anti-pathogenic properties of the alloys. 3g / L nickel (provided by nickel sulfate hexahydrate) 15-35 g / L hypophosphite reducing agent (provided by sodium hypophosphite monohydrate) An electroless nickel-copper-phosphorus bath was prepared containing 400-1,000 ppm copper (provided by copper sulfate pentahydrate). The temperature of the bath was maintained at 160-195 F and the pH of the bath was adjusted and maintained within the range of 8 to 9. The plating time for the substrate was 1 hour and the plating rate was about 0.4 mils / hour.
[0067] The copper concentration was varied to achieve both 40% and 60% copper concentration in the resulting alloy while keeping the Ni concentration constant. 60% copper is the lowest concentration recognized to produce optimal antipathogenic properties. However, the present inventors surprisingly discovered that even the lower copper percentages have significant biocidal activity.
[0068] Two controls were used during the testing. The first was a control done on the plastic alone which should have had no effect on the bacteria. The second was a standard electroless nickel-phosphorus deposit. Two separate standard test bacteria were used: Staphylococcus aureus ATCC6538P Methicillin-resistant Staphylococcus aureus (MRSA) ATTC33592.
[0069] Test procedure overview Prepare and dilute the test organisms to 2.5–10 × 10 5 A starting inoculum concentration of CFU / mL was obtained. Controls were tested in triplicate at time=0 and time=2 hours. Test samples were tested in triplicate at time=2 hours. Each sample piece was placed in a sterile Petri dish, inoculated, and then the inoculum was spread evenly over the sample surface, then covered with sterile plastic to hold it in place. The samples were incubated at 35°C and at least 90% relative humidity. At the appropriate time, neutralizing broth was added to each sample, placed on a shaker, and mixed thoroughly to promote release of the inoculum from the sample surface. Serial dilutions of neutralizing broth containing the inoculum were plated. All plates were incubated at 35°C for 24-48 hours. After incubation, bacterial colonies were counted and recorded. Results are found in the "Test Results" section below. These results pertain only to the samples tested.
[0070] [Table 1]
[0071] [Table 2]
[0072] The results show that the anti-pathogenic response of the copper-containing coatings was indeed improved compared to the nickel-phosphorus only control. For Staphylococcus aureus ATCC 6538P, 40% copper in the alloy improved efficacy by 32%, and 60% improved efficacy by 95%. In fact, the 60% alloy had a nearly 100% disinfection rate after only 2 hours of exposure.
[0073] The alloys were even more effective against Methicillin-resistant Staphylococcus aureus (MRSA) ATTC 33592. The 40% copper alloy had a 95% improvement over the control, and the 60% alloy achieved a 96% improvement. Both provided 99.98% elimination of pathogens after 2 hours of exposure. The surfaces were essentially self-disinfecting.
[0074] In both cases, the plastic-only controls contained more bacteria after two hours of incubation, proof that the test was valid (the bacteria had not just died off naturally).
[0075] Those skilled in the art will perceive improvements, changes, and modifications of the present invention from the above description. Such improvements, changes, and modifications are within the scope of the skill of those skilled in the art and are intended to be covered by the appended claims. All patent publications and references cited in this application are incorporated herein by reference in their entirety.
Claims
1. 1. An aqueous electroless nickel-copper-phosphorus plating bath for forming an anti-pathogenic coating on a substrate, said plating bath comprising: About 2.0 g / L to about 8.0 g / L of Ni; About 150 ppm to about 1500 ppm Cu; about 10 g / L to about 50 g / L of a hypophosphite reducing agent; The electroless nickel-copper-phosphorus bath provides a uniform electroless nickel-copper-phosphorus deposit on the substrate which is anti-pathogenic and / or oligoactive.
2. The bath of claim 1, wherein the concentration of Ni in the bath relative to the concentration of Cu is such that the electroless nickel-copper-phosphorus deposit contains from about 30% to about 85% Cu by weight.
3. The bath of claim 1 or claim 2, wherein the Ni concentration in the plating bath is from about 3 g / L to about 6 g / L.
4. A bath according to any one of claims 1 to 3, wherein Ni is provided in the bath by dissolving a water soluble nickel salt in the bath.
5. 5. The bath of claim 4, wherein the water-soluble nickel salt is selected from nickel sulfate, nickel chloride, nickel methanesulfonate, nickel sulfamate, nickel fluoroborate, or combinations thereof.
6. The bath according to any one of claims 1 to 5, wherein the Cu concentration is from about 400 ppm to about 1000 ppm.
7. The bath according to any one of claims 1 to 6, wherein Cu is provided in the bath by dissolving a water-soluble copper salt in an aqueous solution.
8. 8. The bath of claim 7, wherein the copper salt is selected from copper sulfate, copper chloride, copper methanesulfonate, copper sulfamate, copper fluoroborate, or combinations thereof.
9. A bath according to any one of the preceding claims, having a neutral to alkaline pH.
10. The bath according to any one of claims 1 to 9, having a pH of from about 8 to about 9.
11. The bath of any one of claims 1 to 10 comprising from about 10 g / L to about 50 g / L of at least one organic acid complexing agent.
12. 12. The bath of claim 11, wherein the organic acid complexing agent comprises a carboxylic acid selected from the group consisting of malic acid, lactic acid, succinic acid, and combinations of the foregoing.
13. The bath according to any one of claims 1 to 2, further comprising at least one of a chelating agent, a stabilizing agent, or a pH buffering agent.
14. 10. The bath of claim 1 consisting essentially of a combination of water, about 3 g / L to about 6 g / L Ni, about 10 g / L to about 50 g / L hypophosphite reducing agent, about 400 ppm to about 1000 ppm Cu, less than about 25 g / L of an organic acid complexing agent selected from the group consisting of malic acid, lactic acid, and succinic acid, optional stabilizers, and optional pH adjusters, said bath having a pH of about 8 to about 9.
15. 1. A method for forming an electroless anti-pathogenic coating on a surface of a substrate, the method comprising: Providing a substrate; contacting a surface of the substrate with the aqueous electroless nickel-copper-phosphorus plating bath of any one of claims 1 to 14.
16. 16. The method of claim 15, wherein a surface of the substrate is contacted with the aqueous electroless nickel-copper-phosphorus plating bath by immersing at least a portion of the substrate in the bath.
17. The method of claim 15, wherein the bath has a temperature of about 160° F. to about 195° F. during electroless plating of the surface of the substrate.
18. 16. The method of claim 15, wherein the surface is in contact with the bath for at least 1 hour.
19. 16. The method of claim 15, wherein the anti-pathogenic coating has a thickness of at least about 50 microinches.
20. Electroless nickel-copper-phosphorus coating, at least about 30 wt. % Cu; and about 5 wt. % to about 15 wt. % P; Electroless nickel-copper-phosphorus coating with the balance being Ni, along with unavoidable impurities.
21. 21. The coating of claim 20, comprising at least about 40 wt%, at least about 50 wt%, or at least about 60 wt% Cu.
22. 21. The coating of claim 20 having a thickness of at least about 50 microinches thick.
23. 21. The coating of claim 20, wherein the coating is anti-pathogenic, anti-bacterial, and / or inhibits biofilm formation.
24. 24. The coating of claim 23, wherein the coating is anti-pathogenic to bacteria including at least one of Staphylococcus aureus or Methicillin-resistant Staphylococcus aureus.
25. 21. The coating of claim 20 formed by the method of claim 15.