Low-moisture composition

A low moisture composition with a mesh microstructure of sodium fatty acid carboxylates and polyethylene glycol domains addresses stability and dissolution issues, enhancing fragrance delivery and stability, making it suitable for laundry applications.

JP2024543587AActive Publication Date: 2024-11-21PROCTER & GAMBLE CO
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024532891
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-08-12
Filing Date
2023-08-08
Publication Date
2024-11-21
Estimated Expiration
2043-08-08

AI Technical Summary

Technical Problem

Existing solid soluble compositions face challenges in achieving physical stability, moisture resistance, and efficient dissolution while maintaining the integrity of cooling benefit agents under varying temperature and humidity conditions, leading to limitations in fragrance delivery and stability during shipping and use.

Method used

A low moisture composition comprising a mesh microstructure formed from sodium fatty acid carboxylates and polyethylene glycol domains, with a crystalline framework that includes cooling benefit agents, ensuring stability and high dissolution rates, allowing for enhanced fragrance delivery and protection from oxidation.

Benefits of technology

The composition provides significant cooling to fabrics, offers improved fragrance delivery, and maintains stability under varying conditions, reducing the need for special shipping conditions and enhancing the sustainability of cooling beads.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543587000001_ABST
    Figure 2024543587000001_ABST
Patent Text Reader

Abstract

A low moisture composition comprising a solid soluble composition domain having a crystallization agent and a PEGC domain.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] A low moisture composition comprising a solid dissolving composition (SDC) comprising a mesh microstructure formed from a dry sodium fatty acid carboxylate formulation, polyethylene glycol domains (PEGC), and a cooling benefit agent(s), which dissolves during normal use to deliver noticeable freshness to fabrics. [Background technology]

[0002] Cooling beads are added directly to the washing machine drum to provide cooling to the wash cycle. In the most basic design, the beads are composed of a "primary" carrier (e.g., PEG, different molecular weights) and a cooling benefit agent (e.g., perfume capsules, neat perfume) to deliver the cooling effect. Suitable base compositions are disclosed, for example, in U.S. Pat. No. 8,476,219 (B2). In more advanced designs, the beads are also composed of one or more "secondary" carriers (often called fillers) that are dispersed in the primary carrier to fulfill one or more specific functions in the bead. For example, in one disclosure (U.S. Pat. No. 9,347,022 (B1)), starch granules are added to the PEG in the beads to reduce the cost of the beads. In another disclosure (WO 2021 / 170759 (A1)), polymers, inorganic salts, clays, sugars, polysaccharides, glycerol, and fatty alcohols are added to facilitate processing and increase stability. In yet another example, the beads are composed of a "primary" carrier comprising salts and sugars, sodium acetate trihydrate, and block copolymers, as disclosed in U.S. Pat. Nos. 11,008,535 (B2), 11,220,657 (B2), and 10,683,475 (B2), respectively.

[0003] Formulating an effective solid dissolving composition presents considerable challenges. The composition must be physically stable, preferably temperature and humidity resistant, and must be able to dissolve into solution and perform the desired function by leaving little or no material behind. Solid dissolving compositions are well known in the art and are used in several roles, such as detergents, oral and personal care products, disinfectants, and cleaning compositions.

[0004] It is surprising that it is possible to create a solid soluble composition (SDC) with a mesh microstructure formed from dry sodium fatty acid carboxylates that can contain high concentrations of actives, that is readily soluble in water during laundry wash conditions, yet is temperature and humidity resistant, allowing for supply chain stability. It has been discovered that low moisture compositions with both PEGC and SDC domains offer significant advantages over current cooling beads, including improved dissolution rate, sustainability, expanded fragrance breadth, moisture control, broader sourcing opportunities, cost savings, lighter weight for efficient e-commerce shipping, and protection from incompatible chemicals. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] U.S. Patent No. 8,476,219(B2) [Patent Document 2] U.S. Patent No. 9,347,022(B1) [Patent Document 3] International Publication No. 2021 / 170759(A1) [Patent Document 4] U.S. Patent No. 11,008,535(B2) [Patent Document 5] Same No. 11,220,657(B2) [Patent Document 6] Same No. 10,683,475(B2) Summary of the Invention [Means for solving the problem]

[0006] 1. A low moisture composition that will substantially dissolve during normal use to provide noticeable cooling to fabrics, the composition comprising: a solid dissolvable composition (SDC) domain made from a crystallizing agent, a polyethylene glycol (PEGC), and a population of capsules containing a freshness benefit agent, the crystallizing agent being a sodium salt of a saturated fatty acid having from 8 to about 12 carbon atoms, the capsules being present in at least one of the SDC or the PEGC; The capsule, an oily core comprising a benefit agent; A shell surrounding the core, a substantially inorganic first shell component, a condensation layer comprising a condensation product of the precursors; a substantially inorganic first shell component comprising a nanoparticle layer comprising inorganic nanoparticles, the nanoparticle layer having a condensation layer disposed between the core and the nanoparticle layer; a shell comprising an inorganic second shell component surrounding the first shell component, the inorganic second shell component surrounding the nanoparticle layer; The precursor comprises at least one compound of formula (I), (M v O z Y n ) w (Formula I) wherein M is one or more of silicon, titanium, and aluminum; v is the valence of M and is 3 or 4; z is 0.5 to 1.6; Each Y is independently -OH, -OR 2 , Halo,

[0007] [ka] -NH 2 , -NHR 2 , -N(R 2 ) 2 , and

[0008] [ka] wherein R 2 is C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; R 3 , H, C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; n is 0.7~(v-1), A low moisture composition, wherein w is 2 to 2000. [Brief description of the drawings]

[0009] While the specification concludes with claims particularly illustrating and distinctly claiming the subject matter regarded as the present disclosure, it is believed that the disclosure will be better understood from the following description in conjunction with the accompanying drawings, in which: Some figures may be simplified by omitting selected elements for the purpose of more clearly showing other elements. The omission of such elements in some figures does not necessarily indicate the presence or absence of the elements in any of the exemplary embodiments, unless expressly depicted in the corresponding written description. None of the drawings are necessarily to scale. [Figure 1A] 1 shows a scanning electron micrograph (SEM) of crystallizing agent crystals. [Figure 1B] 1 shows a scanning electron micrograph (SEM) of a mesh microstructure made from crystallized crystallizing agent in an SDC domain. [Figure 2A]Shown is a scanning electron micrograph (SEM) of viable perfume capsules (eg, Red Arrow, top) dispersed within a mesh microstructure of SDC domains. [Figure 2B] 1 shows a scanning electron micrograph (SEM) of perfume capsules dispersed in a mesh microstructure of SDC domains. [Diagram 3] 1 is a graph showing the amount of perfume in the headspace on dried and rubbed fabric treated with a viable amount of commercial product (about 1 gram perfume capsule, heaped cap) and the composition of the present invention (about 2.5 grams perfume capsule, 1 / 2 cap) (e.g., similar to sample EO). The composition of the present invention has much more perfume in the air and much less product added to the wash. [Figure 4A] 1 shows the dissolution behavior of SDC prepared with different combinations of crystallization agents relative to commercial PEG, as determined using the dissolution test method. [Figure 4B] 1 shows the dissolution behavior of SDC prepared with different combinations of crystallization agents relative to commercial PEG, as determined using the dissolution test method. [Figure 4C] 1 shows the dissolution behavior of SDC prepared with different combinations of crystallization agents relative to commercial PEG, as determined using the dissolution test method. [Diagram 5] 1 is a graph showing the stability temperature of the SDC domain for three inventive compositions using the Thermal Stability Test Method. [Figure 6] FIG. 1 is a graph showing the hydration stability of SDC domains of the present invention (%dm<5% at 80% RH) as measured by the Humidity Test Method as water uptake at 25° C. when exposed to different relative humidities. [Figure 7] FIG. 2 is a diagram of particles in a low moisture composition as described in Example 1. [Figure 8] FIG. 2 is a diagram of particles in a low moisture composition as described in Example 2. [Figure 9] FIG. 2 is a diagram of particles in a low moisture composition as described in Example 3. [Figure 10]FIG. 1 is a diagram of particles in a low moisture composition as described in Example 4. [Figure 11A] 1 shows a representative scanning electron micrograph (SEM) of a comparative composition prepared from potassium palmitate (KC16) and showing platelet crystals. [Figure 11B] 1 shows a representative scanning electron micrograph (SEM) of a comparative composition prepared from triethanolamine palmitate (TEA C16) and showing platelet crystals. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The present invention comprises a low moisture composition that substantially or completely dissolves in the laundry wash cycle to provide noticeable cooling to fabrics. The low moisture composition comprises at least one domain of a solid soluble composition (DSC) containing a crystalline mesh, at least one domain of a polyethylene glycol composition (PEGC), and, in embodiments, one or more cooling benefit agents, which may be in high concentration. The crystalline mesh ("mesh") comprises a relatively rigid three-dimensional interlocking crystalline skeletal framework of fibrous crystalline particles formed during treatment with a crystallizing agent. The solid soluble composition of the present invention has a crystallizing agent(s), low moisture content, cooling benefit agent(s), and is readily soluble in water at the target wash temperature.

[0011] The present invention may be more readily understood by reference to the following detailed description of exemplary compositions: It is to be understood that the claims are not limited to the particular products, methods, conditions, devices, or parameters described herein, and that the terms used herein are not intended to limit the invention as claimed.

[0012] As used herein, a "solid dissolvable composition" (SDC) comprises a crystallizing agent of sodium fatty acid carboxylate, an optional cooling benefit agent, and up to 10% by weight water, which when properly processed forms an interconnected crystalline mesh of fibers that is readily soluble at the target wash temperature, and is present during the initial mixing stage in the form of solid particles.

[0013] As used herein, a "PEG composition" (PEGC) comprises PEG and an optional cooling benefit agent.

[0014] As used herein, a "domain" refers to a contiguous mass containing substantially the same material. In one embodiment, the domain may comprise SDC. In another embodiment, the domain may comprise PEGC.

[0015] As used herein, "low moisture composition" refers to a cooling composition that includes both SDC domains and PEGC domains, and a cooling benefit agent, where the low moisture composition has a moisture content of less than about 10% by weight.

[0016] In this specification, "consumer product" refers to a low moisture composition purchased to provide fabrics with freshness during the wash cycle, and includes a low moisture composition having single or multiple particles that are added to the washing machine drum before or during the rinse or wash cycle to provide superior freshness to fabrics. Such compositions include, but are not limited to, laundry cleaning compositions and detergents, fabric softening compositions, fabric enhancing compositions, fabric deodorant compositions, laundry pre-cleaning agents, laundry pre-treatment agents, laundry additives, spray products, dry cleaning agents or compositions, laundry rinse additives, cleaning additives, post-rinse fabric treatment agents, ironing aids, unit dose formulations, delayed delivery formulations, detergents contained on or in porous substrates or nonwoven sheets, and other suitable forms that may be apparent to those skilled in the art in light of the teachings of this specification. Such products may be used as pre-laundry and post-laundry treatments.

[0017] "Particles" as used herein means discrete masses (or chunks) in a low moisture composition, typically greater than about 5 mg in mass and greater than 1 mm in size. Particles may have different shapes, including, but not limited to, hemispheres, spheres, plates, gummy bears, and cashews. Particles may have one or more layers.

[0018] As used herein, a "solid soluble composition mixture" (SDCM) includes the components of a solid soluble composition prior to water removal (e.g., during a mixing or crystallization step). To produce a solid soluble composition, an intermediate solid soluble composition mixture is first formed that includes an aqueous phase that includes an aqueous carrier. The aqueous carrier may be distilled water, deionized water, or tap water. The aqueous carrier may be present by weight in an amount of about 65% to 99.5% by weight of the SDCM, alternatively about 65% to about 90% by weight, alternatively about 70% to about 85% by weight, alternatively about 75% by weight.

[0019] As used herein, "rheological solid composition" (RSC) describes the solid form of SDCM after crystallization (crystallization stage) prior to removal of water to obtain SDC, where RSC contains greater than about 65% water by weight and the solid form is from an interlocking "structured" mesh of fibrous crystalline particles (mesh microstructure) from the crystallizing agent.

[0020] As used herein, "PEG" includes polyethylene glycols (PEGs) having a molecular weight of about 200 to about 50,000 daltons, most preferably about 6,000 to 10,000 daltons.

[0021] As used herein and further described below, "cooling benefit agent" includes materials that are added to the domain to impart a cooling effect to fabrics throughout the wash. In some embodiments, the cooling benefit agent may be a neat perfume. In embodiments, the cooling benefit agent may be an encapsulated perfume (perfume capsule). In embodiments, the cooling benefit agent may be a mixture of perfumes and / or perfume capsules.

[0022] As used herein, "crystallization temperature" is used to describe the temperature at which a crystallization agent (or combination of crystallization agents) is completely solubilized in SDCM, or alternatively, as used herein, the temperature at which a crystallization agent (or combination of crystallization agents) exhibits some crystallization in SDCM.

[0023] As used herein, "dissolution temperature" is used to describe the temperature at which a low moisture composition becomes completely solubilized in water under normal washing conditions.

[0024] As used herein, "stability temperature" is the temperature at which the SDC and / or PEGC domain material(s) are completely melted such that the composition no longer exhibits a stable solid structure and can be considered a liquid or paste, and the low moisture composition no longer functions as intended. The stability temperature is the lowest temperature thermal transition determined by the thermal stability test method. In an embodiment of the present invention, the stability temperature may be greater than about 40°C, more preferably greater than about 50°C, more preferably greater than about 60°C, and most preferably greater than about 70°C to ensure stability in the supply chain. Those skilled in the art will understand how to measure the lowest thermal transition using a differential scanning calorimetry (DSC) instrument.

[0025] As used herein, "humidity stability" is the relative humidity at which a low moisture composition spontaneously absorbs more than 5% by weight of its original mass in water from humidity from the ambient environment at 25°C. Water absorption can occur in either the SDC domain and / or the PEGC domain. Absorbing a small amount of water when exposed to a humid environment allows for more sustainable packaging. Absorbing too much water risks the composition softening or liquefying and no longer functioning as intended. In an embodiment of the present invention, humidity stability may be greater than 70% RH, more preferably greater than 80% RH, more preferably greater than 90% RH, and most preferably greater than 95% RH. Those skilled in the art will understand how to measure 5% weight gain using a dynamic vapor sorption (DVS) device, further described in the humidity test method.

[0026] As used herein, "cleaning composition", unless otherwise indicated, includes all-purpose or "heavy duty" cleaners in granular or powder form, especially cleaning detergents; all-purpose cleaners in liquid, gel, or paste form, especially the so-called heavy duty liquid types; liquid detergents for delicate fabrics; hand dishwashing detergents or light duty dishwashing detergents, especially the high foaming types; dishwashing machine cleaners, liquid cleaners and disinfectants, including various pouch, tablet, granular, liquid and foam-removing types for home and commercial use (including antibacterial hand wash types, wash bars, mouthwashes, denture cleaners, dentifrices, car or carpet shampoos, bathroom cleaners); hair shampoos and hair rinses; shower gels and foam baths, and metal cleaners; as well as cleaning aids such as bleach additives and "stain sticks" or pre-treatment types, products with substrates such as dryer additive sheets, dry and wet wipes and pads, nonwoven substrates, and sponges; as well as sprays and mists.

[0027] As used herein, "dissolves during normal use" means that the low moisture composition dissolves completely or substantially during the wash cycle. Those skilled in the art will recognize that wash cycles have a wide range of conditions (e.g., cycle time, machine type, wash solution composition, temperature). A suitable composition will dissolve completely or substantially during at least one of these conditions.

[0028] As used herein, the term "bio-based" materials refers to renewable materials.

[0029] As used herein, the term "renewable material" refers to a material produced from renewable materials. As used herein, the term "renewable resource" refers to a resource that is produced by natural processes at a rate comparable to its consumption rate (e.g., within a 100-year time frame). The resource can be replenished naturally or by agricultural techniques. Non-limiting examples of renewable resources include plants (e.g., sugar cane, beets, corn, potatoes, citrus fruits, woody plants, lignocellulose, hemicellulose, and cellulosic waste), animals, fish, bacteria, fungi, and forest products. These resources may be naturally occurring, hybridized, or genetically modified organisms. Natural resources such as crude oil, coal, natural gas, and peat that take more than 100 years to generate are not considered renewable resources. Because at least a portion of the material of the present invention is derived from a renewable resource that can be separated from carbon dioxide, the use of the material can reduce global warming potential and fossil fuel consumption.

[0030] As used herein, the term "bio-based content" refers to the amount of carbon in a material that is derived from renewable resources as a percentage of the weight (mass) of the total organic carbon in the material, as determined using ASTM D6866-10, Method B.

[0031] The term "solid" refers to the state of the composition under expected conditions of storage and use of the low moisture composition.

[0032] As used herein, articles such as "a" and "an," when used in a claim, are understood to mean one or more of what is claimed or described.

[0033] As used herein, the terms "include," "includes," and "including" are meant to be non-limiting.

[0034] Unless otherwise noted, all component or composition concentrations are in terms of the active portion of that component or composition and are exclusive of impurities, e.g., residual solvents or by-products, that may be present in commercial sources of such component or composition.

[0035] All percentages and ratios are calculated on a weight basis unless otherwise specified. All percentages and ratios are calculated based on the total composition unless otherwise specified.

[0036] It should be understood that every maximum numerical limitation given throughout this specification includes every lower numerical limitation, as if such lower numerical limitation were expressly written herein. Every minimum numerical limit given throughout this specification includes every higher numerical limitation, as if such higher numerical limitations were expressly written herein. Every numerical range given throughout this specification includes every narrower numerical range that falls within such broader numerical range, as if such narrower numerical ranges were all expressly written herein.

[0037] The solid dissolving composition (SDC) comprises fibrous interlocking crystals (FIGS. 1A and 1B) with sufficient crystal fiber length and concentration to form a mesh microstructure. The mesh allows the SDC to be solid with a relatively small amount of material. The mesh also allows for the entrapment and protection of particles such as cooling benefit agents, such as fragrance capsules (FIGS. 2A and 2B). In an embodiment, the active is a discrete particle having a diameter of less than 100 μm, preferably less than 50 μm, more preferably less than 25 μm. Furthermore, the significant voids in the mesh microstructure also allow for the inclusion of liquid cooling benefit agents, such as neat fragrance. In an embodiment, preferably up to about 15% by weight of neat fragrance can be added, preferably 13% to 0.5% by weight, preferably 13% to 2% by weight, most preferably 10% to 2% by weight. The voids also provide a path for water to be incorporated into the microstructure during washing to accelerate dissolution compared to a completely solid composition.

[0038] Surprisingly, it is possible to prepare SDCs with high dissolution rates, low water content, moisture resistance, and thermal stability. Sodium salts of long chain fatty acids (i.e., sodium myristate (NaC14) to sodium stearate (NaC18)) can form fibrous crystals. It is generally understood that the crystal growth pattern resulting in a fibrous crystal habit reflects the hydrophilic (head group) and hydrophobic (hydrocarbon chain) balance of the NaC14-NaC18 molecules. As disclosed in this application, the crystallizing agents used have the same hydrophilic contribution but very different hydrophobicity due to the shorter hydrocarbon chains of the sodium fatty acid carboxylates used. In fact, the carbon chains are about half the length of those previously disclosed (US Patent Application Publication No. 2021 / 0315783(A1)). Furthermore, one skilled in the art would recognize that many surfactants, such as alkyl sulfates with the same chain but different head groups, are subject to significant humidity uptake and significant temperature-induced changes. The selected group of crystallizing agents in the present invention enables all these useful properties.

[0039] Current water-soluble polymers (e.g., PEG alone) limit the use of perfume capsules as fragrance enhancer delivery systems. The encapsulated perfume is delivered in an aqueous slurry, which is limited to a maximum of 20-30% by weight of the encapsulated perfume, with the total amount of encapsulated perfume limited to approximately 1.2% by weight. Use of encapsulated perfume at concentrations above these concentrations prevents the water-soluble carrier from solidifying, thereby limiting encapsulated perfume delivery. As a result, consumers generally do not fully enjoy the desired amount of freshness due to limitations on what consumers can add to their wash liquors. The solid soluble compositions of the present invention can be constructed with up to more than 18% by weight of perfume capsules, resulting in approximately 15 times the fragrance delivery compared to current water-soluble polymers. Such high delivery is made possible at least in part by the low water content of the present compositions, allowing the user a significant cooling upgrade over current commercially available fabric freshening beads (Figure 3).

[0040] The improved performance of the present compositions compared to current cooling laundry beads is believed to be related to the dissolution rate of the composition's matrix. Without being limited by theory, it is believed that if the composition dissolves later in the wash cycle, the encapsulated perfume is more likely to deposit on the fabric through the wash (TTW) and enhance cooling performance. Current water-soluble polymers used in commercial fabric cooling beads have limited dissolution rates set by a limited molecular weight (MW) range of polyethylene glycols (PEGs) used as the dissolution matrix. As a result, a single bead of PEG must function under a range of machine and wash conditions, limiting performance. In contrast, the dissolution rate of the present compositions can be tailored for a range of machine and wash conditions by adjusting the ratios of the composition components (e.g., sodium laurate (NaL) to sodium decanoate (NaD) ratio) (Figures 4A-4C). This allows the opportunity to create a wide range of compositions useful in many different wash conditions, allowing the SDC domains to release cooling benefit agents at different times during the wash cycle.

[0041] The main commercial fabric cooling bead making process limits the selection of cooling benefit agents. Instead, domains of SDC can be processed and added to low moisture compositions. The PEG used to form most current commercial beads must be processed at temperatures between 70°C and 80°C, which is higher than the melting point of PEG. Preparing SDC domains at room temperature allows for a greater variety of cooling technologies. In the actual process, the temperature of the melting point of PEG must be maintained for many hours, and some perfume ingredients are very volatile and evaporate during processing. The inclusion of perfume oils for SDC is done at about 25°C, opening up a wide range of added neat perfumes. Furthermore, many perfume capsule wall structures fail at higher process temperatures, releasing the encapsulated perfume and rendering them ineffective in low moisture compositions. Processing in perfume capsules at lower temperatures allows for a wider range of capsules.

[0042] Controlling water migration in mixed bead compositions (e.g., low and high moisture content beads) is difficult with the current water-soluble polymers used because water migrates to the surface of the high moisture content beads. Because beads are often packaged in enclosed packages that minimize moisture transmission into and out of the package, moisture trapped on the surface of the high moisture content beads comes into contact with the surface of the low moisture content beads, leading to bead clumping and product distribution problems. In contrast, the structure of the solid soluble composition prevents water migration, thus allowing the use of materials that are sensitive to water uptake (e.g., cationic polymers, bleaching agents).

[0043] As previously mentioned, current bead formulations using PEG (and other structuring materials) are prone to degradation when exposed to heat and / or humidity during shipping. Therefore, special shipping conditions and / or packaging are often required to mitigate such degradation. The SDC of the present invention comprises a crystalline structure that is stable over a range of temperature and humidity conditions. The SDC domains preferably exhibit a %dm of less than 5% at 70% RH, more preferably less than 5% at 80% RH, and most preferably less than 5% at 90% RH as determined by the humidity test method (Figure 5), and essentially no melt transition below 50°C as determined by the thermal stability test method (Figure 6). As a result, additional resources for refrigeration and plastic packaging during shipping to prevent moisture migration are not required. The inclusion of SDC domains in a low moisture composition allows for robust protection of the cooling benefit agent.

[0044] Finally, without wishing to be limited by theory, it is believed that the high dissolution rate of the solid dissolving composition is at least partially provided by the mesh microstructure. This is believed to be important because it is this porous structure that provides the product with both "lightness" and the ability to dissolve quickly compared to compressed tablets, which allows for easy delivery of active substances during use. It is believed to be important that a single crystallizing agent (or in combination with other crystallizing agents) forms fibers in the solid dissolving composition making process. The formation of fibers allows for a solid dissolving composition that can retain active substances without the need for compression, which can destroy the microencapsulation.

[0045] In an embodiment, the fibrous crystals may have a minimum length of 10 μm and a thickness of 2 μm as determined by the Fiber Test Method.

[0046] In embodiments, the active agent may be in the form of particles, and the particles may be a) uniformly distributed within the mesh microstructure, b) coated on the surface of the mesh microstructure, or c) some of the particles may be distributed within the mesh microstructure and some of the particles may be coated on the surface of the mesh microstructure. In embodiments, the active agent may be in the form of a) a soluble film on the top surface of the mesh microstructure, b) a soluble film on the bottom surface of the mesh microstructure, or c) a soluble film on both the bottom and top surfaces of the mesh. The active agent may be present as a combination of soluble film and particles. Non-limiting examples of particles are shown in Figures 7, 8, 9, and 10.

[0047] Crystallization Agent The crystallizing agents are selected for their ability to impart different properties to the SDC domains. The crystallizing agents are selected from a small group of sodium fatty acid carboxylates with saturated chains and chain lengths ranging from C8 to C12. In this composition range, and using the described preparation method, such sodium fatty acid carboxylates provide ideal solubilization temperatures for the fibrous mesh microstructure, fabrication and dissolution during use, and by appropriate blending, the resulting solid soluble composition can be tailored for these properties for a variety of applications and conditions.

[0048] The crystallization agent may be present in the solid soluble composition mixture used to make the SDC domains in an amount of about 5% to about 35% by weight, about 10% to about 35% by weight, about 15% to about 35% by weight. The crystallization agent may be present in the solid soluble composition in an amount of about 50% to about 99% by weight, about 60% to about 95% by weight, and about 70% to about 90% by weight. The crystallization agent may be present in the low moisture composition in an amount of about 5% to about 60% by weight, about 10% to about 50% by weight, and about 15% to about 40% by weight.

[0049] Suitable crystallizing agents include sodium octanoate (NaC8), sodium decanoate (NaC10), sodium dodecanoate or sodium laurate (NaC12), and combinations thereof.

[0050] Encapsulant The capsule comprises a shell (wall) material (benefit agent delivery capsule or simply "capsule") that encapsulates a benefit agent in a core. The benefit agent may be referred to herein as a "benefit agent" or an "encapsulated benefit agent." An encapsulated benefit agent is encapsulated within the core.

[0051] The capsules may be present in the composition in an amount of about 0.05% to about 20%, or about 0.05% to about 10%, or about 0.1% to about 5%, or about 0.2% to about 2% by weight of the composition. As discussed herein, the amount or weight percent of capsules refers to the combined shell material and core material.

[0052] The capsules can have an average shell thickness of about 10 nm to about 10,000 nm, preferably about 170 nm to about 1,000 nm, and more preferably about 300 nm to about 500 nm.

[0053] In various embodiments described herein, the capsules can have a volume weighted average capsule diameter of about 0.1 μm to about 300 μm, about 0.1 μm to about 200 μm, about 1 μm to about 200 μm, about 10 μm to about 200 μm, or about 10 μm to about 50 μm. Advantageously, it has been found that embodiments herein can provide large capsules (e.g., average diameter of about 10 μm or more) without sacrificing the overall stability of the capsule and / or while maintaining good breaking strength.

[0054] In various embodiments described herein, the capsules can have a volume weighted average capsule diameter of about 0.1 μm to about 300 μm, about 0.1 μm to about 200 μm, about 1 μm to about 200 μm, about 10 μm to about 200 μm, or about 10 μm to about 50 μm. Advantageously, it has been found that embodiments herein can provide large capsules (e.g., average diameter of about 10 μm or more) without sacrificing the overall stability of the capsule and / or while maintaining good breaking strength.

[0055] Surprisingly, it has been found that in addition to the inorganic shell, the volume core-to-shell ratio can also play an important role in ensuring the physical integrity of the capsule. Shells that are too thin relative to the overall capsule size (core-to-shell ratio >98:2) tend to suffer from lack of self-integrity. On the other hand, shells that are too thick relative to the capsule diameter (core-to-shell ratio <80:20) tend to have higher shell permeability in surfactant-rich matrices. While it would be intuitive to think that a thick shell would result in a lower shell permeability (because this parameter affects the average diffusion path of the active substance across the shell), it has been surprisingly found that capsules of the present invention with shells having a thickness above a threshold value have higher shell permeability. This upper threshold value is believed to depend to some extent on the capsule diameter. The volume core-to-shell ratio is determined according to the method provided in the Test Method section below.

[0056] The permeability measured by the permeability test method described below correlates with the porosity of the capsule shell. In an embodiment, the capsule or population of capsules has a permeability measured by the permeability test method described above of about 0.01% to about 80%, about 0.01% to about 70%, about 0.01% to about 60%, about 0.01% to about 50%, about 0.01% to about 40%, about 0.01% to about 30%, or about 0.01% to about 20%. For example, the permeability can be about 0.01, 0.1, 0.5, 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 20, 25, 30, 35, 40, 45, 50, 55, 60, 65, 70, 75, or 80%.

[0057] The capsules may have a volume core to shell ratio of 50:50 to 99:1, preferably 60:40 to 99:1, preferably 70:30 to 98:2, more preferably 80:20 to 96:4.

[0058] It may be desirable to have a particular combination of these capsule properties. For example, the capsules can have a volumetric core-to-shell ratio of about 99:1 to about 50:50, an average volume-weighted capsule diameter of about 0.1 μm to about 200 μm, and an average shell thickness of about 10 nm to about 10,000 nm. The capsules can have a volumetric core-to-shell ratio of about 99:1 to about 50:50, an average volume-weighted capsule diameter of about 10 μm to about 200 μm, and an average shell thickness of about 170 nm to about 10,000 nm. The capsules can have a volumetric core-to-shell ratio of about 98:2 to about 70:30, an average volume-weighted capsule diameter of about 10 μm to about 100 μm, and an average shell thickness of about 300 nm to about 1,000 nm.

[0059] In a particular embodiment, the capsules have an average volume-weighted diameter of 1-200 micrometers, preferably 1-10 micrometers, and even more preferably 2-8 micrometers. In another embodiment, the shell thickness is 1-10,000 nm, 1-1,000 nm, 10-200 nm. In a further embodiment, the capsules have an average volume-weighted diameter of 1-10 micrometers and a shell thickness of 1-200 nm. It has been found that capsules having an average volume-weighted diameter of 1-10 micrometers and a shell thickness of 1-200 nm have a higher breaking strength.

[0060] Without wishing to be bound by theory, it is believed that a higher breaking strength results in better survivability during the washing process, which may cause premature rupture of mechanically weak capsules due to mechanical constraints in the washing machine.

[0061] Capsules with an average volume weighted diameter of 1-10 micrometers and a shell thickness of 10-200 nm provide resistance to mechanical constraints only if they are made with a careful selection of the silica precursor used. In some embodiments, the precursor has a molecular weight of 2-5 kDa, and even more preferably of 2.5-4 kDa. In addition, the concentration of the precursor must be carefully selected, being 20-60% by weight, preferably 40-60% by weight, of the oil phase used during encapsulation.

[0062] Without being bound by theory, it is believed that higher molecular weight precursors have a much slower migration time from the oil phase to the water phase. The slower migration time is believed to result from a combination of three phenomena: diffusion, partitioning, and reaction kinetics. This phenomenon is important in the context of small size capsules due to the fact that the total surface area between the oil and water in the system increases as the capsule diameter decreases. The larger the surface area, the greater the migration of precursors from the oil phase to the water phase, which then reduces the yield of polymerization at the interface. Therefore, higher molecular weight precursors may be necessary to mitigate the effects caused by the increased surface area and obtain capsules according to the present invention.

[0063] The method used to produce the capsules can produce capsules with a low coefficient of variation in capsule diameter. Controlling the distribution of capsule sizes can improve the breaking strength of the population and allow the population to have a more uniform breaking strength. The capsule population can have a coefficient of variation in capsule diameter of 40% or less, preferably 30% or less, and more preferably 20% or less.

[0064] For a capsule containing a core material to be functional and cost-effective in consumer goods applications, it should i) be resistant to diffusion of the core during the shelf life of the product (e.g., low leakage or permeability), ii) be capable of depositing on the targeted surface during application, and iii) be capable of releasing the core material by mechanically rupturing the shell at the correct time and place to provide the intended benefit to the end consumer.

[0065] The capsules described herein can have an average breaking strength of 0.1 MPa to 10 MPa, preferably 0.25 MPa to 5 MPa, and more preferably 0.25 MPa to 3 MPa. Fully inorganic capsules traditionally have poor breaking strength, but the capsules described herein can have a breaking strength of greater than 0.25 MPa, improving stability and allowing the release of beneficial agent to be triggered upon application of a specified amount of burst stress.

[0066] Preferably, the core is oily. In an embodiment, the core may be liquid at the temperature at which the core is used in the formulated product. The core may be liquid at or near room temperature and may include one or more benefit agents.

[0067] The cooling benefit agent may be at least one of a perfume blend, a malodor counteractant, or a combination thereof. In one aspect, the perfume delivery technology may include a benefit agent delivery capsule formed by at least partially surrounding a benefit agent with a shell material. Beneficial agents include 3-(4-t-butylphenyl)-2-methylpropanal, 3-(4-t-butylphenyl)-propanal, 3-(4-isopropylphenyl)-2-methylpropanal, 3-(3,4-methylenedioxyphenyl)-2-methylpropanal, and 2,6-dimethyl-5-heptenal, α-damascone, β-damascone, γ-damascone, β-damascenone, 6,7-dihydro-1,1,2,3,3-pentamethyl-4(5H)-indanone, methyl-7,3-dihydro-2H-1,5-benzodioxepin-3-one, 2-[2-(4-methyl-3-cyclohexenyl-1-yl)propyl]cyclopentamethyl-1,2-dihydro-2H-indanone, methyl-7,3-dihydro-2H-1,5-benzodioxepin-3-one, methyl-7,3-dihydro-2H-indan ... The materials may include materials selected from the group consisting of: perfume raw materials such as ion-2-one, 2-sec-butylcyclohexanone, and β-dihydroionone, linalool, ethyl linalool, tetrahydrolinalool, and dihydromyrcenol; waxes such as silicone oils and polyethylene wax; essential oils such as fish oil, jasmine, camphor, and lavender; skin coolants such as menthol, methyl lactate; vitamins such as vitamins A and E; sunscreens; glycerin; catalysts such as manganese catalyst or bleach catalyst; bleach particles such as perborate; silicon dioxide particles; antiperspirant actives; cationic polymers, and mixtures thereof.Suitable benefit agents can be obtained from Givaudan Corp. (Mount Olive, New Jersey, USA), International Flavors & Fragrances Corp. (South Brunswick, New Jersey, USA), Firmenich Company (Geneva, Switzerland), or Encapsys Company (Wisconsin, USA).As used herein, "perfume raw materials" refers to one or more of the following ingredients: fragrant essential oils; aroma compounds; materials supplied with fragrant essential oils, aroma compounds, stabilizers, diluents, processing agents, and contaminants; and any materials commonly associated with fragrant essential oils, aroma compounds.

[0068] The core preferably comprises a perfume raw material. The core may comprise about 1% to 100% perfume by weight based on the total weight of the core. Preferably, the core may comprise about 50% to 100% perfume by weight based on the total weight of the core, or about 80% to 100% perfume by weight based on the total weight of the core. Typically, higher levels of perfume are preferred for improved delivery efficiency.

[0069] A perfume raw material may comprise one or more perfume raw materials, preferably two or more perfume raw materials. The term "perfume raw material" (or perfume raw material, "PRM"), as used herein, means a compound having a molecular weight of at least about 100 g / mole and useful for imparting an odor, fragrance, essence, or scent, alone or together with other perfume raw materials. Typical PRMs include alcohols, ketones, aldehydes, esters, ethers, nitrites, and alkenes such as terpenes, among others.

[0070] PRMs may be characterized by their boiling point (BP) measured at normal pressure (760 mmHg) and octanol / water partition coefficient (P), which may be described in terms of logP determined according to the test methods described in the Test Methods section. Based on these characteristics, PRMs may be classified as Quadrant I, Quadrant II, Quadrant III, or Quadrant IV perfumes, as described in more detail below. Perfumes with various PRMs from different quadrants may be desirable, for example, to provide fragrance benefits at different touch points during normal use.

[0071] Perfume raw materials having a boiling point BP below about 250° C. and a log P below about 3 are known as Quadrant I perfume raw materials. Quadrant I perfume raw materials are preferably limited to less than 30% of the perfume composition. Perfume raw materials having a BP above about 250° C. and a log P above about 3 are known as Quadrant IV perfume raw materials, perfume raw materials having a BP above about 250° C. and a log P below about 3 are known as Quadrant II perfume raw materials, and perfume raw materials having a BP below about 250° C. and a log P above about 3 are known as Quadrant III perfume raw materials.

[0072] Preferably, the capsule comprises a perfume. Preferably, the perfume of the capsule comprises a mixture of at least 3, or even at least 5, or at least 7 perfume raw materials. The perfume of the capsule may comprise at least 10 or at least 15 perfume raw materials. A mixture of perfume raw materials may provide more complex and desirable aesthetics and / or better perfume performance or longevity, for example, at various touch points. However, it may be desirable to limit the number of perfume raw materials in a perfume to reduce or limit the complexity and / or cost of formulation.

[0073] The perfume may include at least one perfume raw material of natural origin. Such ingredients may be desirable for sustainability / environmental reasons. The perfume raw material of natural origin may include natural extracts or essences that may contain a mixture of PRMs. Such natural extracts or essences may include orange oil, lemon oil, rose extract, lavender, musk, patchouli, balsam essence, sandalwood oil, pine oil, cedar, etc.

[0074] In addition to the perfume raw material, the core may contain a pro-perfume, which may contribute to improving the longevity of the refreshing effect. The pro-perfume may, for example, comprise a non-volatile substance that releases or converts a perfume substance as a result of simple hydrolysis, or may be a pH-change-triggered pro-perfume (e.g., triggered by a pH drop), or an enzymatically releasable pro-perfume, or a light-triggered pro-perfume. The pro-perfume may exhibit different release rates depending on the pro-perfume selected.

[0075] The core of the encapsulation of the present disclosure may include a core modifier, such as a partitioning modifier and / or a density modifier. In addition to the flavoring, the core may include from greater than 0% to about 80%, preferably from greater than 0% to about 50%, more preferably from greater than 0% to about 30% of a partitioning modifier based on the total weight of the core. The partitioning modifier may be selected from the group consisting of vegetable oils, modified vegetable oils, C 4 ~C 24 The oil may comprise a material selected from the group consisting of mono-, di- and triesters of fatty acids, isopropyl myristate, dodecanophenone, lauryl laurate, methyl behenate, methyl laurate, methyl palmitate, methyl stearate, and mixtures thereof. The partitioning modifier may preferably comprise or consist of isopropyl myristate. The modified vegetable oil may be esterified and / or brominated. The modified vegetable oil may preferably comprise castor oil and / or soybean oil.

[0076] The shell may comprise 90% to 100% by weight of the shell, preferably 95% to 100% by weight, more preferably 99% to 100% by weight of the shell, of inorganic material. Preferably, the inorganic material in the shell comprises a material selected from a metal oxide, a semi-metal oxide, a metal, a mineral, or a mixture thereof. Preferably, the inorganic material in the shell comprises SiO 2 , TiO 2 , Al 2 O 3 , ZrO 2 , ZnO 2 , CaCO 3 , Ca 2 SiO 4 , Fe 2 O 3 , Fe 3 O 4 , clay, gold, silver, iron, nickel, copper, or mixtures thereof. More preferably, the inorganic material in the shell comprises SiO 2 , TiO 2 , Al 2 O 3 , CaCO 3or a mixture thereof, most preferably SiO 2 Includes.

[0077] The shell may include a first shell component. The shell may preferably include a second shell component surrounding the first shell component. The first shell component may include a condensation layer formed from a condensation product of a precursor. As described in detail below, the precursor may include one or more precursor compounds. The first shell component may include a nanoparticle layer. The second shell component may include an inorganic material.

[0078] The inorganic shell may include a first shell component including a condensed layer surrounding the core, and may further include a nanoparticle layer surrounding the condensed layer. The inorganic shell may further include a second shell component surrounding the first shell component. The first shell component includes an inorganic material, preferably a metal / metalloid oxide, more preferably SiO2, TiO2 and Al2O3, or mixtures thereof, even more preferably SiO2. The second shell component includes an inorganic material, preferably a material from the group of metal / metalloid oxides, metals, and minerals, more preferably SiO2. 2 , TiO 2 , Al 2 O 3 , ZrO 2 , ZnO 2 , CaCO 3 , Ca 2 SiO 4 , Fe 2 O 3 , Fe 3 O 4 , clay, gold, silver, iron, nickel, and copper, or mixtures thereof, and even more preferably SiO 2 and CaCO 3 or mixtures thereof. Preferably, the material of the second shell component is of the same chemical type as the first shell component to maximize chemical compatibility.

[0079] The first shell component can include a condensation layer surrounding the core. The condensation layer can include a condensation product of one or more precursors. The one or more precursors can include at least one compound from the group consisting of Formula (I), Formula (II), and mixtures thereof, where Formula (I) is (M v O z Y n ) w and formula (II) is (M v O z Y n R 1 p ) w The precursor may contain only compounds according to formula (I) and not compounds according to formula (II) (i.e., R 1 Formulae (I) and (II) are described in more detail below.

[0080] The one or more precursors above may be of formula (I): (M v O z Y n ) w (Formula I) In the formula, M is one or more of silicon, titanium, and aluminum, v is the valence of M and is 3 or 4, z is 0.5 to 1.6, preferably 0.5 to 1.5, and each Y is -OH, -OR 2 , -NH 2 , -NHR 2 , -N(R 2 ) 2 Selected from R 2 is C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; R 3 , H, C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6~C 22 aryl, or 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S, n is 0.7-(v-1), and w is 2-2000.

[0081] The one or more precursors may be of formula (I), where M is silicon. Y is -OR 2 n may be 1 to 3. Y may be -OR 2 and n is preferably 1 to 3. n is at least 2, and one or more of Y's is -OR 2 and one or more of Y's may be preferably -OH.

[0082] R 2 is C 1 ~C 20 R may be alkyl. 2 is C 6 ~C 22 R may be aryl. 2 is C 1 Alkyl, C 2 Alkyl, C 3 Alkyl, C 4 Alkyl, C 5 Alkyl, C 6 Alkyl, C 7 Alkyl, and C 8 R may be one or more of alkyl. 2 is C 1 R may be alkyl. 2 is C 2 R may be alkyl. 2 is C 3 R may be alkyl. 2 is C 4 It may be alkyl.

[0083] z may be from 0.5 to 1.3, from 0.5 to 1.1, from 0.5 to 0.9, from 0.7 to 1.5, from 0.9 to 1.3, or from 0.7 to 1.3.

[0084] M is silicon, v is 4, and each Y is -OR2 where n is 2 and / or 3, and each R 2 is C 2 The precursor may be a polyalkoxysilane (PAOS). The precursor may be a polyalkoxysilane (PAOS) ​​synthesized via a non-hydrolytic process.

[0085] The precursor may alternatively or additionally comprise one or more compounds of formula (II): (M v O z Y n R 1 p ) w (Formula II) In the formula, M is one or more of silicon, titanium, and aluminum, v is the valence of M and is 3 or 4, z is 0.5 to 1.6, preferably 0.5 to 1.5, and each Y is -OH, -OR 2 , -NH 2 , -NHR 2 , -N(R 2 ) 2 Selected from R 2 is C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; R 3 , H, C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S, n is 0-(v-1), and each R 1 is C 1 ~C 30 Alkyl;C 1 ~C 30 Alkylene; halogen, -OCF 3 , -NO 2, -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, -C(O)OH, -C(O)O-alkyl, -C(O)O-aryl, -C(O)O-heteroaryl, and mixtures thereof. 1 ~C 30 Alkyl; and halogen, -OCF 3 , -NO 2 , -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, -C(O)OH, -C(O)O-alkyl, -C(O)O-aryl, and -C(O)O-heteroaryl. 1 ~C 30 alkylene, p is a number from 0 to pmax, and pmax=60 / [9 * Mw(R 1 )+8], and Mw(R 1 ) is R 1 is the molecular weight of the group, and w is 2 to 2,000.

[0086] R 1 -Halogen, -OCF 3 , -NO 2 , -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, CO 2 H (i.e., C(O)OH), -C(O)O-alkyl, -C(O)O-aryl, and -C(O)O-heteroaryl; 1 ~C 30 R may be alkyl. 1 -Halogen, -OCF 3 , -NO 2 , -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, CO 2 C substituted with 1 to 4 groups independently selected from H, C(O)O-alkyl, C(O)O-aryl, and C(O)O-heteroaryl 1 ~C 30It may be an alkylene.

[0087] As noted above, it may be preferable to reduce or even eliminate the presence of compounds according to formula (II) having R groups in order to reduce or even eliminate the organic content in the first shell component. The precursor, the condensation layer, the first shell component, and / or the shell may be free of compounds according to formula (II).

[0088] The precursors of formula (I) and / or (II) may be characterized by one or more physical properties, namely molecular weight (Mw), degree of branching (DB) and polydispersity index (PDI) of molecular weight distribution. It is believed that selecting a particular Mw and / or DB may be useful to obtain capsules that retain their mechanical integrity when dried on a surface and have low shell permeability in a surfactant-based matrix. The precursors of formula (I) and (II) may be characterized by having a DB of 0 to 0.6, preferably 0.1 to 0.5, more preferably 0.19 to 0.4, and / or a Mw of 600 Da to 100,000 Da, preferably 700 Da to 60,000 Da, more preferably 1,000 Da to 30,000 Da. The characteristics provide useful properties of the precursors to obtain the capsules of the present invention. The precursors of formula (I) and / or (II) may have a PDI of 1 to 50.

[0089] The condensation layer comprising a metal / semi-metal oxide may be formed from a condensation product of a precursor comprising at least one compound of formula (I) and / or at least one compound of formula (II), optionally in combination with one or more monomeric precursors of a metal / semi-metal oxide, the metal / semi-metal oxide comprising TiO2, Al2O3 and SiO2, preferably SiO2. The monomeric precursors of the metal / semi-metal oxide include compounds of formula M(Y) V-n R n (wherein M, Y, and R are as defined in formula (II) and n can be an integer from 0 to 3). The monomer precursor of the metal / semi-metal oxide is preferably a compound of the general formula Si(Y) 4-n R n(wherein Y and R are defined as in formula (II), and n can be an integer from 0 to 3.) Examples of such monomers are TEOS (tetraethoxyorthosilicate), TMOS (tetramethoxyorthosilicate), TBOS (tetrabutoxyorthosilicate), triethoxymethylsilane (TEMS), diethoxy-dimethylsilane (DEDMS), trimethylethoxysilane (TMES), and tetraacetoxysilane (TAcS). These are not intended to limit the scope of monomers that can be used, and suitable monomers that can be used in combination herein will be apparent to one of ordinary skill in the art.

[0090] In embodiments, the first shell component can include an optional nanoparticle layer. The nanoparticle layer includes nanoparticles. The nanoparticles of the nanoparticle layer can be SiO 2 , TiO 2 , Al 2 O 3 , ZrO 2 , ZnO 2 , CaCO 3 , clay, silver, gold, and copper. Preferably, the nanoparticle layer is made of SiO 2 It may include nanoparticles.

[0091] The nanoparticles can have an average diameter of from 1 nm to 500 nm, preferably from 50 nm to 400 nm.

[0092] The size of the capsule pores can be adjusted by changing the shape of the nanoparticles and / or by using a combination of nanoparticles of different sizes. For example, non-spherical and irregular nanoparticles can be used as they may improve the packing when forming the nanoparticle layer, thereby resulting in a denser shell structure. This may be advantageous when permeability needs to be limited. The nanoparticles used can have a more regular shape, such as spherical. Any conceivable nanoparticle shape can be used herein.

[0093] The nanoparticles may be substantially free of hydrophobic modifications. The nanoparticles may be substantially free of organic compound modifications. The nanoparticles may include organic compound modifications. The nanoparticles may be hydrophilic.

[0094] The nanoparticles may include surface modifications, examples of which include linear or branched chain C 1 ~C 20 These surface modifications include, but are not limited to, alkyl groups, surface amino groups, surface methacryl groups, surface halogens, or surface thiols. These surface modifications allow the nanoparticle surface to have organic molecules covalently attached thereto. When inorganic nanoparticles are disclosed herein for use, this means that they may or may not include any of the above surface modifications, even if not explicitly listed.

[0095] The capsule of the present invention may be defined as comprising a substantially inorganic shell, comprising a first shell component and a second shell component. Substantially inorganic means that the first shell component may comprise up to 10% by weight, or up to 5% by weight, preferably up to 1% by weight, as defined below in the calculation of organic content. It may be preferred that the first shell component, the second shell component, or both, comprise an organic content of about 5% by weight or less, preferably about 2% by weight or less, more preferably about 0% by weight, based on the weight of the first or shell component.

[0096] The first shell component is useful for building a mechanically robust scaffold or skeleton, but can also provide low shell permeability in products containing surfactants, such as laundry detergents, shower gels, cleansers, etc. (see Surfactants in Consumer Products, J. Falbe, Springer-Verlag). The second shell component can significantly reduce shell permeability improving capsule impermeability in surfactant-based matrices. The second shell component can also significantly improve capsule mechanical properties, such as capsule burst force and crush strength. Without being bound by theory, it is believed that the second shell component contributes to the overall shell densification by depositing precursors in the remaining pores in the first shell component. The second shell component also adds an additional inorganic layer on the surface of the capsule. These improved shell permeability and mechanical properties provided by the second shell component only occur when used in combination with the first shell component defined in the present invention.

[0097] The capsules of the present disclosure may be formed by first mixing a hydrophobic material with any of the above-defined precursors of the condensed layer, thereby forming an oil phase, which may include oil-based and / or oil-soluble precursors. The mixture of precursors and hydrophobic material is then used with an aqueous phase as a dispersed phase, and an O / W (oil-in-water) emulsion is formed when the two phases are mixed and homogenized via methods known to those skilled in the art. The nanoparticles can be present in the aqueous phase and / or the oil phase, regardless of the type of emulsion desired. The oil phase may include oil-based core conditioning agents and / or oil-soluble benefit agents as well as precursors of the condensed layer. Suitable core materials used in the oil phase are described herein above.

[0098] Once an emulsion is formed, the following steps may occur: (a) The process in which nanoparticles migrate to the oil / water interface, thereby forming a nanoparticle layer. (b) the precursor of the condensation layer, which comprises a precursor of a metal / metalloid oxide, begins to undergo a hydrolysis / condensation reaction with water at the oil / water interface, thus forming a condensation layer surrounded by the nanoparticle layer, and the precursor of the condensation layer can further react with the nanoparticles of the nanoparticle layer.

[0099] The precursors forming the condensation layer may be present in an amount of from 1% to 50% by weight, preferably from 10% to 40% by weight, based on the total weight of the oil phase.

[0100] The oil phase composition may contain any of the compounds defined in the core section above. The oil phase may contain from 10% to about 99% by weight of the benefit agent prior to emulsification.

[0101] The second shell component can be formed by mixing the capsules having the first shell component with a solution of a second shell component precursor. The solution of the second shell component precursor can include a water-soluble or oil-soluble second shell component precursor. The second shell component precursor can be one or more of the compounds of formula (I) defined above, tetraethoxysilane (TEOS), tetramethoxysilane (TMOS), tetrabutoxysilane (TBOS), triethoxymethylsilane (TEMS), diethoxy-dimethylsilane (DEDMS), trimethylethoxysilane (TMES), and tetraacetoxysilane (TAcS). The second shell component precursor can be Si(Y) 4-n R nThe second shell component precursor may also include one or more of the following silane monomers: (where Y is a hydrolyzable group, R is a non-hydrolyzable group, and n may be an integer from 0 to 3). Examples of such monomers are described above in this paragraph, but they are not meant to limit the scope of monomers that may be used. The second shell component precursor may include silicates, titanates, aluminates, zirconates, and / or zincates. The second shell component precursor may include carbonates and calcium salts. The second shell component precursor may include salts of iron, silver, copper, nickel, and / or gold. The second shell component precursor may include alkoxides of zinc, zirconium, silicon, titanium, and / or aluminum. The second shell component precursor may include one or more of a silicate solution, such as sodium silicate, a silicon tetraalkoxide solution, an iron sulfate and nitrate salt, a titanium alkoxide solution, an aluminum trialkoxide solution, a zinc dialkoxide solution, a zirconium alkoxide solution, a calcium salt solution, and a carbonate solution. CaCO 3 The second shell component comprising can be derived from the use of a calcium salt and a carbonate salt in combination. 3 The second shell component, including the cation, can be obtained from calcium salts without the addition of carbonate, but it requires the addition of CO 2 Carbonate ions must be generated in situ from

[0102] The second shell component precursor can include any suitable combination of any of the aforementioned compounds.

[0103] The solution of the second shell component precursor can be added dropwise to the capsule containing the first shell component. The solution of the second shell component precursor and the capsule can be mixed together for 1 minute to 24 hours. The solutions of the second shell component precursor and the capsule can be mixed together at room temperature or at an elevated temperature, for example, from 20° C. to 100° C.

[0104] The second shell component precursor solution can include the second shell component precursor in an amount of 1% to 50% by weight, based on the total weight of the second shell component precursor solution.

[0105] The capsules having the first shell component can be mixed with a solution of the second shell component precursor at a pH of 1 to 11. The solution of the second shell precursor can contain an acid and / or a base. The acid can be a strong acid. Strong acids include HCl, HNO 3 , H 2 SO 4 , HBr, HI, HClO 4 , and HClO 3 In other embodiments, the acid may be a weak acid. In embodiments, the weak acid may be acetic acid or HF. The concentration of the acid in the second shell component precursor solution may be 10 -7 The base may be an inorganic base or an organic base, preferably an inorganic base. The inorganic base may be a hydroxide, such as sodium hydroxide, and ammonia. For example, the inorganic base may be about 10 -5 M ~ 0.01M NaOH, or about 10 -5 The above exemplary list of acids and bases is not meant to limit the scope of the invention, and other suitable acids and bases that allow for control of the pH of the second shell component precursor solution are contemplated herein.

[0106] The process of forming the second shell component may include changing the pH during the process. For example, the process of forming the second shell component may start at an acidic or neutral pH and a base may be added later during the process to increase the pH. Alternatively, the process of forming the second shell component may start at a basic or neutral pH and an acid may be added later during the process to decrease the pH. Still further, the process of forming the second shell component may start at an acidic or neutral pH and an acid may be added during the process to further decrease the pH. Still further, the process of forming the second shell component may start at a basic or neutral pH and a base may be added during the process to further increase the pH. Any suitable pH shift may be used. Additionally, any suitable combination of acid and base may be used in the solution of the second shell component precursor at any time to achieve the desired pH. The process of forming the second shell component may include maintaining a stable pH during the process with a deviation of up to ±0.5 pH units. For example, the process of forming the second shell component may be maintained at a basic, acidic, or neutral pH. Alternatively, the process of forming the second shell component may be maintained at a particular pH range by controlling the pH using an acid or a base. Any suitable pH range may be used. Furthermore, any suitable combination of acid and base may be used in the solution of the second shell component precursor at any time to keep the pH stable in the desired range.

[0107] The emulsion can be cured under conditions to solidify the precursor, thereby forming a shell surrounding the core.

[0108] The reaction temperature for curing can be increased to increase the rate at which solidified capsules are obtained. The curing process can induce condensation of the precursors. The curing process can be carried out at room temperature or at a temperature higher than room temperature. The curing process can be carried out at a temperature between 30°C and 150°C, preferably between 50°C and 120°C, more preferably between 80°C and 100°C. The curing process can be carried out for any suitable period of time to allow the shell of the capsule to be strengthened through condensation of the precursor materials. The curing process can be carried out for a period of 1 minute to 45 days, preferably between 1 hour and 7 days, more preferably between 1 hour and 24 hours. A capsule is considered to be cured when it no longer disintegrates. The determination of capsule disintegration is described in detail below. During the curing process, hydrolysis of the Y moiety (from formula (I) and / or (II)) is believed to occur, followed by subsequent condensation of either the -OH group with another -OH group, or the -OH group with another moiety of the Y type (where the two Ys are not necessarily the same). The hydrolyzed portions of the precursor first condense with surface moieties of the nanoparticles (if the nanoparticles contain such moieties). As the formation of the shell proceeds, the precursor moieties become reactive with the previously formed shell.

[0109] The emulsion may be cured such that the shell precursors react with the nanoparticles and condense. The following is an example of the hydrolysis and condensation steps described herein for a silica-based shell:

[0110] [ka]

[0111] For example, when a precursor of formula (I) or (II) is used, the following describes the hydrolysis and condensation steps:

[0112] [ka]

[0113] The capsules may be provided as a slurry composition (or simply "slurry" herein). The slurry can be formulated into a product, such as a consumer product.

[0114] Test Method The log of the octanol / water partition coefficient (logP) is calculated for each PRM in the fragrance mixture being tested. The logP values ​​of the individual PRMs are calculated using the Consensus logP Computational Model, version 14.02 (Linux), available from Advanced Chemistry Development Inc. (ACD / Lab), Toronto, Canada, which results in unitless logP values. The ACD / Labs Consensus logP Computational Model is part of the ACD / Labs model suite.

[0115] Viscosity method The viscosity of the undiluted product is determined using a Brookfield® DV-E rotational viscometer, spindle 2, at 60 rpm and approximately 20-21°C.

[0116] Average Shell Thickness Measurement The capsule shell, including the first shell component and, if present, the second shell component, is measured in nanometers for 20 delivery capsules containing beneficial agent using a focused ion beam scanning electron microscope (FIB-SEM, FEI Helios Nanolab 650) or equivalent instrument. Samples are prepared by diluting (1:10) a small amount of liquid capsule dispersion (20 μL) with distilled water. The suspension is then deposited on an ethanol-cleaned aluminum stub and transferred to a carbon coating apparatus (Leica EM ACE600 or equivalent instrument). The samples are dried under vacuum in the coating apparatus (vacuum level: 10 -5mbar). 25 nm to 50 nm of carbon is then flash deposited onto the sample to deposit a conductive carbon layer on its surface. The aluminum stub is then transferred to the FIB-SEM and a cross section of the capsule is prepared. Using a cross section cleaning pattern, cross sections are prepared by ion milling with an emission current of 2.5 nA at an accelerating voltage of 30 kV. Images are acquired at 5.0 kV and 100 pA using immersion mode (dwell time: approximately 10 microseconds) at a magnification of approximately 10,000x.

[0117] Images of the crushed shells are obtained in cross-section from 20 randomly selected benefit agent delivery capsules with no size bias to create a representative sample of the size distribution of capsules present. The shell thickness of each of the 20 inclusions is measured at three different randomly selected locations using calibrated microscope software by drawing a measurement line perpendicular to the tangent plane of the outer surface of the capsule shell. Sixty independent thickness measurements are recorded and used to calculate the average thickness.

[0118] Mean and coefficient of variation of volume-weighted capsule diameter The capsule size distribution is determined by single particle optical detection (SPOS), also called optical particle counting (OPC), using an AccuSizer 780 AD instrument or equivalent and accompanying software CW788 version 1.82 (Particle Sizing Systems, Santa Barbara, Calif., USA) or equivalent. The instrument is configured with the following conditions and options: flow rate = 1 mL / sec; small diameter threshold = 0.50 μm; sensor model number = LE400-05SE or equivalent; autodilution = on; collection time: 60 seconds; number of channels = 512; reservoir fluid volume = 50 ml; maximum coincidence count = 9200. The measurement is started by cold-conditioning the sensor by flushing with water until the background count is less than 100. A sample of delivery capsules in suspension is introduced and the capsule density is adjusted, if necessary, via autodilution with deionized water to obtain a maximum capsule count of 9200 per mL. The suspension is analyzed for 60 seconds. The size range used was 1 μm to 493.3 μm.

[0119] Volume distribution:

[0120]

number

[0121]

number

[0122] Evaluation of volumetric core-to-shell ratio The value of the volumetric core-to-shell ratio is determined as follows and is dependent on the average shell thickness as measured by the Shell Thickness Test Method. The volumetric core-to-shell ratio for a capsule having a measured average shell thickness is calculated by the following equation:

[0123]

number

[0124] This ratio can be converted to a core to shell fraction value by calculating the core weight percentage using the following formula:

[0125]

number

[0126] Method for determining branching degree The branching degree of the precursor was determined as follows: The branching degree is measured using (29Si) nuclear magnetic resonance spectroscopy (NMR).

[0127] Sample preparation Each sample is diluted to a 25% solution using deuterated benzene (Benzene-D6 "100%" (D, 99.96%, available from Cambridge Isotope Laboratories Inc., Tewksbury, Massachusetts) or equivalent. 0.015 M chromium(III) acetylacetonate (99.99% purity, available from Sigma-Aldrich, St. Louis, Missouri, or equivalent) is added as a paramagnetic relaxation reagent. If glass NMR tubes (Wilmed-LabGlass, Vineland, New Jersey, or equivalent) are used for the analysis, a blank sample should also be prepared by filling the NMR tube with the same type of deuterated solvent used to dissolve the sample. The same glass tube should be used to analyze the blank and the sample.

[0128] Analysis of samples The degree of branching is determined using a Bruker 400 MHz nuclear magnetic resonance spectroscopy (NMR) instrument, or equivalent. A standard silicon (29Si) method (e.g., from Bruker) is used with default parameter settings, with a minimum of 1,000 scans and a relaxation time of 30 seconds.

[0129] Sample processing The samples are stored and processed using system software appropriate for NMR spectroscopy, such as MestReNova version 12.0.4-22023 (available from Mestrelab Research) or equivalent. Phase adjustment and background correction are applied. There is a large, broad signal extending from -70 to -136 ppm, which is a result of using glass NMR tubes as well as the glass present in the probe housing. This signal is suppressed by subtracting the spectrum of the blank sample from that of the synthetic sample, provided that the same tube and the same method parameters are used to analyze the blank and sample. To further account for slight differences in data collection, tubes, etc., the area outside the peak of interest should be integrated and normalized to a consistent value. For example, integrate from -117 to -115 ppm and set the integration value to 4 for all blanks and samples.

[0130] The resulting spectrum produces up to five main peak regions. The first peak (Q0) corresponds to unreacted TAOS. The second set of peaks (Q1) correspond to the end groups. The next set of peaks (Q2) correspond to the linear groups. The next set of broad peaks (Q3) are the semi-dendritic units. The final set of broad peaks (Q4) are the dendritic units. When PAOS and PBOS are analyzed, each group falls within a defined ppm range. Representative ranges are listed in the table below.

[0131] [Table 1]

[0132] Polymethoxysilanes have different chemical shifts for Q0 and Q1, overlapping signals for Q2, and Q3 and Q4 are unchanged, as listed in the table below:

[0133] [Table 2]

[0134] The ppm ranges shown in the table above may not apply to all monomers, however other monomers may give rise to different chemical shifts, but the proper assignment of Q0-Q4 should not be affected.

[0135] Using MestReNova, each peak group can be integrated and the branching degree calculated by the following formula:

[0136]

number

[0137] Molecular weight and polydispersity index determination method The molecular weight (weight average molecular weight (Mw) in terms of polystyrene) and polydispersity index (Mw / Mn) of the condensation layer precursors described herein are determined using size exclusion chromatography with refractive index detection, where Mn is the number average molecular weight.

[0138] Sample preparation The sample is weighed and then diluted to a target concentration of 10 mg / mL with the solvent used in the instrument system. For example, 50 mg of polyalkoxysilane is weighed into a 5 mL volumetric flask, dissolved, and diluted to a given volume with toluene. After the sample is dissolved in the solvent, it is passed through a 0.45 μm nylon filter and loaded into the instrument's autosampler.

[0139] Analysis of samples An HPLC system using an autosampler (e.g., Waters 2695 HPLC Separation Module, Milford, Massachusetts, or equivalent) connected to a refractive index detector (e.g., Wyatt 2414 Refractive Index Detector, Santa Barbara, Calif., or equivalent) is used for polymer analysis. Separation is performed on three columns, each 7.8 mm ID x 300 mm long, packed with 5 μm polystyrene-divinylbenzene media, with molecular weight cutoffs of 1, 10, and 60 kDA, respectively. Suitable columns are TSKGel G1000HHR, G2000HHR, and G3000HHR columns (available from TOSOH Bioscience, King of Prussia, Pa.) or equivalent. A 5 μm polystyrene-divinylbenzene guard column (e.g., TSKgel Guardcolumn HHR-L (TOSOH Biosciences), or equivalent), 6 mm ID×40 mm length, is used to protect the analytical column. Toluene (HPLC grade or equivalent) is pumped uniformly at 1.0 mL / min with both the column and detector maintained at 25° C. 100 μL of the prepared sample is injected for analysis. Sample data is stored and processed using software with GPC calculation capabilities (e.g., ASTRA Version 6.1.7.17 software available from Wyatt Technologies, Santa Barbara, Calif., or equivalent).

[0140] The system is calibrated using 10 or more narrowly dispersed polystyrene standards with known molecular weights ranging from about 0.250-70 kDa (e.g., Standard ReadyCal Set (e.g., Sigma-Aldrich, PN76552, or equivalent)) using a third-order fit to the Mp vs. retention time curve.

[0141] The system software is used to calculate and report the weight average molecular weight (Mw) and polydispersity index (Mw / Mn).

[0142] Method for calculating organic content in first shell component As used herein, the definition of organic moieties in the inorganic shell of the capsule according to the present disclosure: Any moiety X that cannot be cleaved from the metal precursor bearing metal M under the specified reaction conditions via hydrolysis of the MX bond (M belongs to the metal and metalloid group and X belongs to the non-metal group, linking the moiety to the inorganic precursor of metal or metalloid M) is considered an organic moiety. The reaction conditions set forth above are that it has a minimum degree of hydrolysis of 1% when exposed to distilled water with neutral pH without stirring for 24 hours.

[0143] This method allows the calculation of the theoretical organic content, assuming complete conversion of all hydrolyzable groups. It therefore becomes possible to evaluate the theoretical proportion of organic components for any mixture of silanes, the result of which represents only the organic content of this precursor mixture itself, and not the actual organic content in the first shell component. Therefore, if a specific percentage for the organic content of the first shell component is disclosed anywhere in this document, that percentage should be understood as containing any mixture of unhydrolyzed or prepolymerized precursors that gives a theoretical organic content smaller than the disclosed number according to the following calculation.

[0144] Examples of silanes include (but are not limited to) the general formula at the end of this section: Each mole fraction Y i Consider a mixture of silanes having the formula: where i is the identification number of each silane. This mixture can be represented as:

[0145]

number

[0146] Such a mixture of silanes results in a shell having the general formula:

[0147]

number

[0148] The weight percentage of the organic portion, as defined above, can then be calculated as follows: 1) Find the mole fraction of each precursor (including nanoparticles) 2) Determine the general formula for each precursor (including nanoparticles) 3) Calculate the general formula for the mixture of precursor and nanoparticles based on the mole fractions 4) Convert to reacted silane (all hydrolyzable groups converted to oxygen groups) 5) Calculate the weight ratio of the organic portion to the total mass (assuming 1 mole of Si per framework)

[0149] Working Example:

[0150] [Table 3]

[0151] To calculate the general formula of a mixture, the indices of each atom in the individual formulas are multiplied by their respective mole fractions. Then, in the case of a mixture, when similar indices occur, the sum of the fractional indices is taken (typically for the ethoxy groups).

[0152] Note: The sum of all Si fractions will always sum to 1 in the mixture general formula due to the calculation method (total mole fractions of Si sum to 1).

[0153]

number

[0154] To convert the unreacted formula to the reacted formula, simply divide all the hydrolyzable group indices by 2 and then add them together (along with any existing oxygen groups, if applicable) to get the fully reacted silane. SiO 1.88 Me 0.20

[0155] In this case, the expected result is SiO since the sum of all the exponents must follow the formula: 1.9 Me 0.2 Is: A+B / 2=2, In the formula, A is the oxygen atom index and B is the sum of all non-hydrolyzable indexes. Small errors arise from taking round numbers in the calculation, which should be corrected. Then, readjust the oxygen atom index to satisfy this formula.

[0156] Therefore, the final formula is SiO 1.9 Me 0.2 and the weight ratio of the organic component is calculated as follows: Weight ratio=(0.20 * 15) / (28+1.9 * 16+0.20 * 15)=4.9%

[0157] General case: The above formula can be generalized by considering the valence of the metal or metalloid M, thus obtaining the following modified formula: M(XR) V-ni R i ni A similar method is used, but the valence V of each metal is taken into account.

[0158] Beneficial Agent Permeation Testing The permeability test method allows to determine the rate of diffusion of a specific molecule from the capsule core to the continuous phase for a population of capsules, which can represent the permeability of the shell of the capsule. The permeability test method is a reference frame that relates to the shell permeability of a specific molecular tracer, thus fixing its size and fixing its affinity towards the continuous phase outside the capsule shell. This is the reference frame used to compare the permeability of various capsules in the art. When both the molecular tracer and the continuous phase are fixed, the shell permeability is a single capsule property that is evaluated under a set of specific conditions.

[0159] The permeability of the capsule shell correlates with the porosity of the shell, such that low permeability indicates low shell porosity.

[0160] Capsule permeability is generally given as a function of parameters such as shell thickness, concentration of active substance in the core, solubility of the active substance in the core, shell, and continuous phase, etc.

[0161] In order to diffuse active substance throughout the shell, active substance must be transferred from core to shell, and active substance must be transferred from shell to continuous phase. This latter process is rapid when the solubility of active substance in continuous phase is very favorable, and in this case, hydrophobic material is transferred into the surfactant system matrix. For example, active substance present in a system at a concentration of 0.025% by weight is very likely to be completely solubilized in 15% by weight of surfactant.

[0162] Considering the above, the limiting step of minimizing the shell permeability of the active substance in the surfactant-based matrix is ​​to limit the diffusion throughout the shell. In the case of hydrophobic shell materials, hydrophobic active substances are easily soluble in the shell if they can be swollen by the active substance. This degree of swelling can be limited by high shell crosslink density.

[0163] In the case of hydrophilic shell materials such as silicon dioxide, hydrophobic materials have limited solubility in the shell itself. Nevertheless, active substances can diffuse rapidly, taking into account the following factors: surfactant molecules and micelles can diffuse into the shell and then into the core itself, allowing a pathway from the core into the shell and ultimately into the external matrix.

[0164] Therefore, for hydrophilic shell materials, high shell crosslink density is required, but the amount of pores in the shell must also be reduced. Such pores can provide rapid mass migration of active substances into the surfactant-based matrix. Therefore, there is a clear and obvious link between the overall permeability of a capsule's shell and its porosity. In fact, the permeability of a capsule gives insight into the overall shell structure of any given capsule.

[0165] As mentioned above, the diffusion of an active substance is defined by the nature of the active substance, its solubility in the continuous phase, and the shell structure (porosity, crosslink density, and any general defects it may contain). Thus, by fixing two of the three relevant parameters, the permeability of various shells can be effectively compared.

[0166] The purpose of this permeability study is to provide a framework that allows for direct comparison of different capsule shells, and further allows for the evaluation of the properties of a large population of capsules, and therefore does not suffer from distorted results obtained by outliers.

[0167] Thus, the permeability of a capsule can be defined via the fraction of a given molecular tracer diffused into a given continuous phase under specific conditions within a given time (e.g., 20% tracer diffusion within 7 days).

[0168] The capsules of the present invention have a relative transmittance of less than about 80%, less than about 70%, less than about 60%, less than about 50%, less than about 40%, less than about 30%, or less than about 20% as measured by the Permeability Test Method.

[0169] The Permeability Test Method determines the shell permeability of the tracer from a capsule containing the molecular tracer, vergyl acetate (CAS#5413-60-5) (Vigon) in the core, compared to a reference sample representing complete diffusion (e.g., 100% permeability) of the tracer.

[0170] First, prepare a capsule according to any given capsule preparation method. For the permeability test method, the capsule core must contain at least 10% by weight of vergyl acetate tracer by weight of the core, or be supplemented to contain it during preparation. In this test, "core weight" refers to the weight of the core after the shell is formed and the capsule is manufactured. The capsule core contains the intended components, such as core modifiers and benefit agents. The capsule can be prepared as a capsule slurry, as is commonly done in the art.

[0171] The capsules are then formulated into a permeability test sample. Formulation of the permeability test sample involves thoroughly mixing the capsule slurry with an aqueous solution of sodium dodecyl sulfate (CAS#151-21-3) to achieve a total core oil content of 0.25%±0.025% by weight and an SDS concentration of 15%±1% by weight, based on the total weight of the test sample. The amount of capsule slurry required can be calculated as follows:

[0172]

number

[0173] The SDS solution can be prepared by dissolving SDS pellets in deionized water. The capsules and SDS solution can be mixed under conditions designed to prevent capsule breakage during mixing. For example, the capsules and SDS solution can be mixed by hand or with an overhead mixer, but should not be mixed with a magnetic stir bar. It has been found that mixing with a magnetic stir bar often results in capsule breakage. Suitable mixing methods can include an IKA propeller type mixer, mixing at 400 rpm or less, and a total mass of the mixture including the SDS solution and capsule slurry of 10 g to 50 g. Other suitable mixing equipment and suitable conditions for mixing without the use of a magnetic stir bar and without breaking a given capsule composition will be readily apparent to one of skill in the art.

[0174] Once the transmittance test sample is prepared, it is placed in a glass vial with a total volume no greater than twice the volume of the transmittance test sample and sealed with an airtight lid. The sealed transmittance test sample is stored for 7 days at a temperature of 35° C. and a relative humidity of 40%. During storage, the sealed transmittance test sample is not exposed to light and is not opened at any time prior to measurement.

[0175] A reference sample representing 100% diffusion is also prepared. The reference sample is prepared so that it can be used on the day of measurement (i.e., 7 days after the preparation of the permeability test sample). The reference sample is prepared by combining an oil-free mixture, intended to replicate the composition of the capsule core (containing the same weight percent of vergyl acetate tracer based on the weight of the core) as determined by mass balance of the capsule made in the permeability test sample, with 15% by weight aqueous SDS. The oil-free mixture and the SDS solution are homogenized with a magnetic stirrer until the oil-free mixture is completely solubilized, and the container should be sealed during mixing to avoid evaporation of the tracer. If homogenization takes a significant amount of time, the above needs to be taken into consideration, and the preparation of the reference sample can be started earlier than 7 days if necessary. Immediately after solubilization, the reference sample is placed in a glass vial with a volume not exceeding twice the volume of the reference sample and sealed with an airtight lid. The SDS solution can be prepared by dissolving SDS pellets in deionized water, as in the case of the permeability test sample.

[0176] A predetermined amount of the oil-free mixture is added to achieve a total concentration of 0.25% by weight ±0.025% of the oil-free mixture in the reference sample, based on the total weight of the reference sample.

[0177]

number

[0178] The permeability, as represented by gas chromatography area counts of vergyl acetate, is analyzed for the permeability test samples (7 days after preparation) and the reference samples on the same day using the same GC / MS analyzer. Specifically, for each test and reference sample, a 100 μL aliquot of the sample is transferred to a 20 ml headspace vial (Gerstel SPME vial 20 ml, part number 093640-035-00) and immediately sealed (Gerstel SPME crimp cap, part number 093640-050-00). Three headspace vials are prepared for each sample. The sealed headspace vials are allowed to equilibrate. The samples reach equilibrium after 3 hours at room temperature, but can be left longer, up to 24 hours after sealing the headspace vials, without compromising or changing the results. After equilibration, the samples are analyzed by gas chromatography mass spectrometry (GC / MS).

[0179] GC / MS analysis was performed by sampling the headspace of each vial through SPME (50 / 30 μm DVB / Carboxen / PDMS, Sigma-Aldrich part number 57329-U) with 25 mm vial penetration and 1 min extraction time at room temperature. The SPME fiber was then thermally desorbed online into the GC injector (270 °C, splitless mode, 0.75 mm SPME inlet liner (Restek, part number 23434) or equivalent, 300 s desorption time, and 43 mm injector penetration). Vergyl acetate was analyzed in full scan mode by fast GC / MS. The ion extraction of the specific mass of vergyl acetate (m / z = 66) was used to calculate the headspace response (expressed as area counts) of vergyl acetate (and isomers). The headspace responses of the permeability test sample and the reference sample, respectively, are referred to herein as vergyl acetate area counts for the permeability test sample and vergyl acetate area counts for the reference sample.

[0180] Suitable equipment for use in this method includes an Agilent 7890B GC equipped with a 5977MSD or equivalent, a Gerstel MPS as the SPME (autosampler), and an Agilent DB-5 UI 30m x 0.25 x 0.25 column (part number 122-5532UI) as the GC column.

[0181] The analyses of the transmittance test samples and the reference samples should be performed under the same room temperature conditions, on the same equipment, and on the same day, with little time between analyses.

[0182] Based on the GC / MS data and the actual known vergyl acetate content in the permeability test sample, the percent permeability can be calculated. The actual content of vergyl acetate in the permeability test must be determined to correct for any losses during capsule manufacturing. The method to be used is specified below. This accounts for inefficiencies often encountered in encapsulating products within capsule cores, where the total amount of vergyl acetate expected to be present during capsule formation is less than that present in the slurry (e.g., evaporation). The following formula can be used to calculate the percent permeability:

[0183]

number

[0184] This calculation is the percent transmittance of the capsules tested after being stored for 7 days at 40% relative humidity and 35°C.

[0185] To assess the actual vergyl acetate content in the SDS capsule mixture, an aliquot must be collected after a specific storage time. For this, the resulting mixture is opened on the same day that the first sample is measured, thereby ensuring that the vial is sealed during storage. First, the mixture must be mixed until homogenous, so that a representative aliquot containing the correct proportion of ingredients is collected. Next, 1 g of the homogenous mixture is introduced into a glass flat-bottomed vial with a diameter of 1 cm, and a magnetic stir bar with a length of at least half the diameter of the vial is introduced into the vial. The homogenous mixture in the designated jar with the magnetic stir bar is sealed, then placed on a magnetic stir plate, and mixing at 500 rpm is used so that all capsules are crushed by the stirring action of the stir bar. This allows the core material enclosed in the capsules to be completely released into the surrounding SDS solution, thus allowing the measurement of the actual vergyl acetate content. This content measurement protocol must be performed on unbroken capsules. In addition, prior to the measurement step, the capsules should be observed under an optical microscope to assess whether all capsules have been broken. If all capsules have not been broken, the capsule grinding should be repeated with increased mixing speed and / or mixing time.

[0186] Neat Fragrance Ingredients The solid dissolving composition may include unencapsulated fragrances, including one or more fragrance ingredients that only provide a hedonic effect (i.e., do not neutralize malodors but provide a pleasant aroma). Suitable fragrances are disclosed in U.S. Patent No. 6,248,135. For example, the solid dissolving composition may include a mixture of volatile aldehydes for neutralizing malodors and hedonic fragrance aldehydes.

[0187] aqueous phase The aqueous phase present in the solid soluble composition mixture and the solid soluble composition is comprised of an aqueous carrier of water and optionally other minor ingredients including sodium chloride.

[0188] The aqueous phase may be present in the solid soluble composition mixture in an amount of about 65% to about 95%, about 65% to about 90%, or about 65% to about 85% by weight of the rheological solid formed as the intermediate composition after crystallization of the solid soluble composition mixture. The aqueous phase may be present in the solid soluble composition in an amount of 0% to about 10%, 0% to about 9%, 0% to about 8%, or about 5% by weight of the intermediate rheological solid.

[0189] Sodium chloride in the aqueous phase solid soluble composition mixture may be present at 0% to about 10% by weight, 0% to about 5% by weight, and 0% to about 1% by weight. Sodium chloride in the aqueous phase solid soluble composition mixture may be present at 0% to about 50% by weight, 0% to about 25% by weight, and 0% to about 5% by weight. In embodiments, the SDC may contain less than 2% by weight of sodium chloride to ensure humidity stability.

[0190] SDC Domain The solid dissolvable composition domain is composed primarily of the solid dissolvable compositions described herein.

[0191] In one embodiment, the SDC domain contains less than about 13% by weight neat perfume. In another embodiment, the SDC domain contains between about 10% and less than 1% by weight neat perfume. In another embodiment, the SDC domain contains between about 8% and 2% by weight neat perfume, as exemplified in the examples as "Benefit Agent % (dry)".

[0192] In one embodiment, the SDC domain contains less than about 16% by weight. In another embodiment, the SDC domain contains about 15% and less than 1% by weight of perfume capsules. In another embodiment, the SDC domain contains about 15% and less than 2% by weight of perfume. In another embodiment, the SDC domain contains about 15% to 5% by weight of perfume capsules, as exemplified in the Examples as "Freshness % (Dry)".

[0193] PEGC domain Polyethylene glycol (PEG) materials are preferred carrier materials for the non-porous dissolving solid structure domains of the present invention. PEG materials are generally relatively low cost, can be formed into many different shapes and sizes, dissolve well in water, and liquefy at high temperatures. PEG materials come in a variety of molecular weights. In the consumer product compositions of the present invention, the PEG carrier material has a molecular weight of about 200 to about 50,000 daltons, preferably about 500 to about 20,000 daltons, preferably about 1,000 to about 15,000 daltons, preferably about 1500 to about 12,000 daltons, or about 6,000 to about 10,000 daltons, and combinations thereof. Suitable PEG carrier materials include materials having a molecular weight of about 8,000 daltons, PEG materials having a molecular weight of about 400 daltons, PEG materials having a molecular weight of about 20,000 daltons, or mixtures thereof. Suitable PEG carrier materials are commercially available from BASF under the trade name PLURIOL, such as PLURIOL E 8000.

[0194] In one embodiment, the PEGC domain contains less than about 30% by weight. In another embodiment, the PEGC domain contains 15% to less than 1% by weight of neat perfume. In another embodiment, the PEGC domain contains 12% to less than 2% by weight of neat perfume. In another embodiment, the PEGC domain contains 12% to less than 5% by weight of neat perfume. In another embodiment, the PEGC domain contains 10% to 2% by weight of neat perfume, as exemplified in the examples as "Coolant %".

[0195] In one embodiment, the PEGC domain contains less than about 2% by weight. In another embodiment, the PEGC domain contains 1.5% to 0.1% by weight of flavor capsules. In another embodiment, the PEGC domain contains 1.25% to 0.2% by weight of flavor capsules. In another embodiment, the PEGC domain contains 1.25% to 0.5% by weight of flavor capsules, as exemplified in the examples as "Freshness %".

[0196] particle The particle composition can be varied depending on the need for a low moisture composition.

[0197] As a non-limiting example, the particle is substantially composed of one domain. In one embodiment, the cooling benefit agent (or "benefit agent") is a flavor capsule dispersed in a particle composed primarily of SDC. In another embodiment, the cooling benefit agent is a neat flavor dispersed in a particle composed primarily of SDC. In one embodiment, the cooling benefit agent is a flavor capsule dispersed in a particle composed primarily of PEGC. In another embodiment, the cooling benefit agent is a neat flavor dispersed in a particle composed primarily of PEGC. In one embodiment, the cooling benefit agent comprises a flavor capsule and a neat flavor dispersed in a particle composed primarily of SDC. In one embodiment, the cooling benefit agent is a flavor capsule and a neat flavor dispersed in a particle composed primarily of PEGC.

[0198] As a non-limiting example, the particles are composed of two or more domains. In these cases, the SDC is small and completely encapsulated in the PEGC domain. In one embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in a PEGC domain (Figure 7, Example 1). In another embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in a PEGC domain containing a neat perfume. In another embodiment, the cooling benefit agent is a neat perfume dispersed in a particle composed primarily of SDC domains dispersed in a PEGC domain containing a perfume capsule. A typical particle contains less than about 50% by weight SDC domains, in another embodiment, about 45% to 10% by weight SDC domains, in another embodiment, about 40% to 15% by weight SDC domains, in another embodiment, about 35% to 20% by weight SDC domains.

[0199] As a non-limiting example, the particles are composed of two or more domains. In these cases, the particles have a core of a single SDC domain coated and completely encapsulated with a coating of PEGC domains. In one embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains (Figure 8, Example 2). In another embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains containing neat perfume. In another embodiment, the cooling benefit agent is a neat perfume dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains containing perfume capsules. A typical particle contains less than about 90% by weight SDC domains, in another embodiment about 80% to 40% by weight SDC domains, in another embodiment about 80% to 50% by weight SDC domains, in another embodiment about 50% to 35% by weight SDC domains.

[0200] As a non-limiting example, the particles are composed of two or more domains. In these cases, the particles have a core of PEGC domains, interspersed with SDC domains. In one embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains, dispersed in PEGC domains (Figure 9, Example 3). In another embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains, dispersed in PEGC domains containing neat perfume. In another embodiment, the cooling benefit agent is a neat perfume dispersed in a particle composed primarily of SDC domains, dispersed in PEGC domains containing perfume capsules. A typical particle contains less than 25% by weight, in another embodiment about 20% to 2% by weight of SDC domains, in another embodiment about 15% to 5% by weight of SDC domains.

[0201] As a non-limiting example, the particles are composed of two or more domains. In these cases, the particles have one side containing PEGC domains and one side containing SDC domains. In one embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains (Figure 10, Example 4). In another embodiment, the cooling benefit agent is a perfume capsule dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains containing neat perfume. In another embodiment, the cooling benefit agent is a neat perfume dispersed in a particle composed primarily of SDC domains dispersed in PEGC domains containing perfume capsules. A typical particle contains about 75% to 25% by weight of SDC domains, in another embodiment 70% to 30% by weight of SDC domains, in another embodiment 60% to 40% by weight of SDC domains.

[0202] In embodiments, the particles of the low moisture composition have shapes that may include hemispheres, plates, cubes, cashews, gummy bears, tubes, and spheres. In another embodiment, the particles have a longest dimension of 3 cm. In another embodiment, the particles have an average weight of less than about 1,000 mg, between about 750 mg and 1 mg, and between about 500 mg and 5 mg.

[0203] low moisture composition The low moisture composition is composed of one or more particles and contains at least one SDC domain and at least one PEGC domain (Example 5).

[0204] The SDC domains, when combined across all particles, can represent from about 10% to about 90% by weight of the low moisture composition, or from about 10% to about 70% by weight, or from about 30% to about 90% by weight, or from about 40% to about 60% by weight.

[0205] The PEGC domains, when combined across all particles, can represent from about 10% to about 90% by weight of the low moisture composition, or from about 10% to about 70% by weight, or from about 30% to about 90% by weight, or from about 40% to about 60% by weight.

[0206] consumer product compositions In one embodiment, the consumer product is added directly to the wash drum at the start of the wash. In another embodiment, the consumer product is added to a fabric enhancer cup in the washing machine. In another embodiment, the consumer product is added at the start of the wash. In another embodiment, the consumer product is added during the wash.

[0207] In one embodiment, the consumer product is sold in a paper package for hydration and temperature stability of the composition. In one embodiment, the consumer product is sold in a unit dose package. In one embodiment, the consumer product is sold in particles of different colors. In one embodiment, the consumer product is sold in a sachet. In one embodiment, the consumer product is sold in particles of different colors. In one embodiment, the consumer product is sold in a recyclable container.

[0208] Dissolution Test Method All samples and procedures are maintained at room temperature (25±3° C.) prior to testing and placed in a desiccant chamber (0% RH) for 24 hours or until constant weight is reached.

[0209] All dissolution measurements are performed at controlled temperature and constant stirring speed. A 600 mL jacketed beaker (Cole-Palmer, part number UX-03773-30, or equivalent) is fitted and cooled to temperature by circulating water through the jacketed beaker using a water circulator (Fisherbrand Isotemp 4100, or equivalent) set at the desired temperature. The jacketed beaker is placed in the center of the stirring element of a VWR Multi-Position Stirrer (VWR North American, West Chester, PA, USA catalog number 12621-046). 100 mL of deionized water (MODEL 18 MΩ, or equivalent) and a stir bar (VWR, Spinbar, catalog number 58947-106, or equivalent) are added to a second 150 mL beaker (VWR North American, West Chester, PA, USA catalog number 58948-138, or equivalent). The second beaker is placed in the jacketed beaker. Enough Millipore water is added to the jacketed beaker so that the water in the jacketed beaker is above the water level in the second beaker, being careful not to mix the water in the second beaker with the water in the jacketed beaker. The stir bar speed is set to 200 RPM, sufficient to create a gentle vortex. The temperature is set to reach 25°C or 37°C in the second beaker using the flow from the water circulator, and the relevant temperatures are reported in the Examples. The temperature in the second beaker is measured with a thermometer before performing the dissolution experiment.

[0210] All samples were sealed in a desiccator prepared with fresh desiccant (VWR, Desiccant-Anhydrous Indicating Drierite, Stock No. 23001, or equivalent) until a constant weight was reached. All test samples had a mass of less than 15 mg.

[0211] A single dissolution experiment is performed by removing a single sample from the desiccator. The sample is weighed within 1 min of being removed from the desiccator and the initial mass (M I) is measured. The sample is dropped into a second beaker while stirring. The sample is allowed to dissolve for 1 minute. At the end of the minute, the sample is carefully removed from the deionized water. The sample is placed back into the desiccator until a constant final mass is reached. The percentage of mass loss of the sample in a single experiment is given by M L =100 * (M I -M F ) / M I It is calculated as:

[0212] Perform nine additional dissolution experiments by replacing the initial 100 ml of water with fresh deionized water, adding a new sample from the desiccator for each experiment, and repeating the dissolution experiment described in the previous paragraph.

[0213] The average percent mass loss for the test (M A ) was calculated as the average percent mass loss for 10 experiments, and the average standard deviation of mass loss (SD A ) is the standard deviation of the average percent mass loss for 10 experiments.

[0214] This method calculates three values: 1) the average mass of the sample (M S ), 2) the temperature at which the sample is dissolved (T), and 3) the average percent of mass loss (M A If the method was not run on the sample, the method returns "NM" for all values. The average percent mass loss (M A ) and the mean standard deviation (SD A ) was used to plot the melting curves shared in Figures 4A, 4B, and 4C.

[0215] Humidity Test Method The humidity test method is used to determine the amount of water vapor sorption that occurs in a composition between drying at 0% RH and drying at various RHs at 25 °C. In this method, 10-60 mg of sample is weighed and the mass change associated with conditioning in different environmental conditions is captured in a dynamic vapor sorption instrument. The resulting mass gain is expressed as % mass change per dry sample mass recorded at 0% RH.

[0216] The method utilizes an SPSx Vapor Sorption Analyzer (ProUmid GmbH & Co. KG, Ulm, Germany) with 1 μg resolution, or an equivalent dynamic vapor sorption (DVS) instrument capable of controlling relative humidity (%RH) to within ±3%, temperature to within ±2°C, and measuring mass with an accuracy of ±0.001 mg.

[0217] A 10-60 mg sample of the raw material or composition is uniformly dispersed in a tared 1-inch diameter aluminum pan. The aluminum pan with the dispersed raw material or composition sample is placed in the DVS instrument, which is set to 25°C and 0% RH, at which point the mass is recorded approximately every 15 minutes to an accuracy of 0.001 mg or better. After the sample has been in the DVS at this environmental setting for a minimum of 12 hours and constant weight has been achieved, the mass of the sample, m d Record to 0.01 mg or better. Once this step is complete, advance the instrument in 10% RH increments to 90% RH. Keep the sample in the DVS for a minimum of 12 hours at each step and record the mass of the sample m until a constant weight is reached. n Record each step with an accuracy of 0.001 mg or better.

[0218] For a particular sample, constant weight can be defined as the change in mass of successive weighments that do not differ by more than 0.004%. For a particular sample, the percent mass change per dry sample mass (% dm) is defined as follows:

[0219]

number

[0220] The % mass change per dry sample mass is reported to the nearest 0.01%.

[0221] Humidity stable at 80% RH means less than 5% change at 80% RH. No humidity stability at 80% RH means more than 5% change at 80%.

[0222] Thermal Stability Test Method All specimens and procedures are maintained at room temperature (25±3°C) and at a relative humidity of 40±10% for 24 hours prior to testing.

[0223] In the thermal stability test method, differential scanning calorimetry (DSC) is performed on a 20 mg ± 10 mg sample of the sample composition. A simple scan is performed between 25°C and 90°C, and the temperature at which the maximum peak is observed to occur is reported to the nearest °C as the stable temperature.

[0224] The sample is loaded into the DSC pan. All measurements are performed with a High Volume Stainless Steel Pan Set (TA part number 900825.902). The pan, lid, and gasket are weighed and tared on a Mettler Toledo MT5 analytical microbalance (or equivalent, Mettler Toledo, LLC., Columbus, OH). The sample is loaded into the pan according to the manufacturer's specifications with a target weight of 20 mg (+ / - 10 mg), taking care to ensure that the sample is in contact with the bottom of the pan. The pan is then sealed with a TA High Volume Die Set (TA part number 901608.905). The final assembly is weighed to obtain the sample weight. The sample is loaded into a TA Q series DSC (TA Instruments, New Castle, DE) according to the manufacture's instructions. The DSC procedure uses the following settings: 1) equilibrate at 25°C; 2) mark the end of cycle 1; 3) ramp to 90.00°C at 1.00°C / min; 4) mark the end of cycle 3; then 5) end method; press Run.

[0225] Moisture Test Method All specimens and procedures are maintained at room temperature (25±3°C) and at a relative humidity of 40±10% for 24 hours prior to testing.

[0226] The moisture test method is used to quantify the weight percent of water in a composition. In this method, a Karl Fischer (KF) titration is performed on each of three similar samples of the sample composition. The titration is performed using a volumetric KF titrator, using a one-component solvent system. Samples weigh 0.3±0.05 g and are allowed to dissolve in the titration vessel for 2.5 minutes prior to titration. The average (arithmetic mean) water content of the three specimen replicates is reported to the nearest 0.1% by weight of the sample composition.

[0227] To measure the moisture content of the samples, measurements are performed using a Mettler Toledo V30S Volumetric KF Titrator. The instrument uses Honeywell Fluka Hydraanal Solvent (Cat. No. 34800-1L-US) to dissolve the samples, Honeywell Fluka Hydraanal Titrant-5 (Cat. No. 34801-1L-US) to titrate the samples, and is equipped with three drying tubes (titration bottle, solvent bottle, and waste bottle) filled with Honeywell Fluka Hydraanal Molecular sieve 3nm (Cat. No. 34241-250g) to preserve the effectiveness of the anhydrous material.

[0228] The method used to measure the samples is of type "KF vol", ID "U8000", and title "KFVol 2-comp 5", each with eight lines where each method functions.

[0229] Line 1 Title has the following selected: Set Type to Karl Fischer Titration Vol. Set Compatibility to V10S / V20S / V30S / T5 / T7 / T9 Set ID to U8000 Set Title to KFVol 2-comp 5 Set Author to Administrator. Date and time along with Modified on and Modified by defined when the method was created. Set Protection to no and SOP to None.

[0230] Line 2 Sample has Sample and Concentration as the two choices. If the Sample option is selected, the following fields are defined as follows: Set Number of IDs to 1. Set ID1 to -- and select Entry Type as Weight. Set Lower Limit to 0.0g. Set Upper Limit to 5.0g. Set Density to 1.0g / mL. Set Correction Factor to 1.0. Set Temperature to 25.0°C. Select Auto Start and set Entry as After Addition. If the Concentration option is selected, the following fields are defined as follows: Select Titrant to KF 2-comp 5. Set Nominal Concentration to 5mg / mL. Select Standard to Water-Standard 10.0. Select Entry Type as Weight. Set Lower Limit to 0.0g. Set Upper Limit to 2.0g. Set Temperature to 25.0°C. Mix Time to 10 seconds. Auto Start is selected. Entry is selected as After Addition. The lower concentration limit is set at 4.5 mg / mL and the upper concentration limit is set at 5.6 mg / mL.

[0231] Line 3, Titration Stand (KF Stand), has fields defined as follows: Set Type to KF Stand. Select Titration Stand to KF Stand. Select Source of Drift to Online. Set Max Starting Drift to 25.0 μg / min.

[0232] Line 4 Mix Time has fields defined as follows: Set duration to 150 seconds.

[0233] Line 5 Titration (KF Volume) [1] has six options: Titrant, Sensor, Stir, Pre-dispense, Control, and End. If the Titrant option is selected, the following fields are defined as follows: Select Titrant to KF 2-comp 5. Set Nominal Concentration to 5mg / mL and set Reagent Type to 2-comp. If the Sensor option is selected, the following fields are defined as follows: Set Type to Polarization. Select Sensor to DM143-SC. Set Units to mV. Set Indication to Voltammetry and set Ipol to 24.0μA. If the Stir option is selected, the following fields are defined as follows: Set Speed ​​to 50%. If the Pre-dispense option is selected, the following fields are defined as follows: Select Mode to None. Set Wait to 0 seconds. If the Control option is selected, the following fields are defined as follows: Set Endpoint to 100.00mV. Set Control Band to 400.00mV. Set Dose Rate (max) to 3 mL / min. Set Dose Rate (min) to 100 μL / min and select Start Normal. Once the End option is selected, the following fields are defined as follows: Select Type to Drift Stop Relative. Set Drift to 15.0 μg / min. Vmax at 15 mL; Min Time is set to 0 seconds and Max Time is set to ∞ seconds.

[0234] The calculation on line 6 has fields defined as follows: Result Type is selected as Predefined. Set Result to Content. Set Result Units to %. Set the formula to R1=(VEQ * CONC-TIME * Set Constant C to 0.1. Set Decimals to 2. Do not select Result Limits. Select Record Statistics. Do not select Extra Statistical Functions.

[0235] The Line 7 record has fields defined as follows: Select Results to No. Select Raw Results to No. Select Measurements Table to No. Select Sample Data to No. Select Resource Data to No. Select EV to No. Select Et to No. Select Vt to No. Select H2O-t to No. Select Drift-t to No. Select H2O-t&Drift-t to no. Select Vt&Drift-t to No. Select Method to No and Series Data to No.

[0236] Line 8 Sample End has the fields defined as follows: Select Open Series.

[0237] Once a method has been selected and start is pressed the following fields are defined as follows: Set Type to Method. Set Method ID to U8000. Set Number of Samples to 1. Set ID1 to -- and Sample Size to 0g. The start option is pressed again. The instrument measures maximum drift and once steady state is reached allows the user to select Add Sample, at which point the user adds the 3-hole adapter, removes the stopper, places the sample in the titration beaker, replaces the 3-hole adapter and stopper, and enters the mass of the sample in grams into the touch screen. The value reported is the weight percent of water in the sample. This measurement is repeated three times for each sample and the average of the three measurements is reported.

[0238] Fiber Test Methods The fiber test method is used to determine whether a solid dissolving composition crystallizes under process conditions and contains fiber crystals. A simple definition of fiber is "a thread or thread-like structure or object." Fibers have a long length in only one direction (e.g., Figures 1A and 1B). This differs from other crystalline forms such as plates or platelets that have long lengths in two or more directions (Figures 11A and 11B). Only solid dissolving compositions with DCS as fibers are within the scope of the present invention. Those skilled in the art will recognize the SDC domains from the PEGC domains in a solid dissolving composition when they are present in the same particle.

[0239] A sample approximately 4 mm in diameter is mounted on a SEM sample shuttle and stub (Quorum Technologies, AL200077B and E7406) with a pre-coated slit containing a 1:1 mixture of Scigen Tissue Plus Optimal Cutting Temperature (OCT) compound (Scigen 4586) and colloidal graphite (agar scientific G303E). The mounted sample is plunge frozen in a liquid nitrogen slush bath. The frozen sample is then inserted into a Quorum PP 3010 T cryoprep chamber (Quorum Technologies PP3010T) or equivalent and allowed to equilibrate to -120°C before freeze fracturing. Freeze fracturing is performed by cutting off the top of the vitreous sample using a cryoprep chamber with a cryo-built-in knife. An additional sublimation is performed at -90°C for 5 minutes to remove any residual ice on the surface of the sample. The sample is further cooled to -150°C and sputter coated with a layer of Pt that resides in a cryo-prep chamber for 60 seconds to reduce charging.

[0240] High resolution imaging is performed on a Hitachi Ethos NX5000 FIB-SEM (Hitachi NX5000) or equivalent.

[0241] To determine the fiber morphology of the sample, images are taken at a magnification of 20,000 times. At this magnification, individual crystals of the crystallizing agent can be observed. The magnification may be adjusted slightly to lower or higher values ​​until individual crystals are observed. Those skilled in the art can evaluate the longest dimension of representative crystals in the image. If this longest dimension is about 10 times or more than the other orthogonal dimension of the crystal, these crystals are considered as fibers and are within the scope of the present invention. EXAMPLES

[0242] These examples provide non-limiting examples of low moisture compositions that include solid soluble composition (SDC) domains having a mesh microstructure formed from a dry sodium fatty acid carboxylate formulation, polyethylene glycol (PEGC) domains, and active agents, such as cooling benefit agents, dispersed within these domains that deliver exceptional cooling to fabrics.

[0243] The compositions of the present invention exhibit particles containing SDC domains with crystallizing agents that, when processed correctly, form a fibrous mesh that dissolves completely within the wash cycle.The compositions of the present invention also exhibit PEGC domains that, when used in combination with the SDC domains, create unique low moisture compositions that are easy to process and provide unique aesthetic properties and improved cooling performance.

[0244] The cooling benefit agent(s) take the form of perfume capsules and / or neat perfume distributed in different domains. Example 1 demonstrates a particle composed of two or more domains where the SDC domain is small and completely encapsulated within a single PEGC domain (Figure 7). Example 2 demonstrates a particle composed of two or more domains where a single SDC domain is coated and completely encapsulated in the coating of the PEGC domain (Figure 8). Example 3 shows a particle composed of two or more domains where the particle has a core of PEGC domains and is interspersed with SDC domains (Figure 9). Example 4 demonstrates a particle composed of two or more domains where the particle has one side containing a PEGC domain and one side containing an SDC domain (Figure 10). Example 5 proposes a low moisture composition composed of a physical mixture of two or more different types of particles and cooling benefit agents, where some of the particles are structured as described in Examples 1-4. Example 6 suggests a particular blend of fatty acid materials that is neutralized and blended with PEGC to produce a solid soluble composition, and compositions prepared from fragrance capsules with different wall structures.

[0245] The data in Tables 1 to 8 provide parameters related to the particles in the following manner. SDC Domain Preparation - All weights listed in this section of the table correspond to the amount added to make the Solid Dissolvable Composition Mixture (SDCM). "% Coolant (Dry)" is the weight percent of coolant remaining in the SDC after drying assuming no residual water as determined by the Moisture Test Method. "% Slow CA" is the weight percent of NaC12 (slow dissolving) in a mixture of NaC12 with NaC10 and NaC8 (fast dissolving).

[0246] All SDC domains are prepared in three fabrication steps to ensure the formation of a fiber mesh in the domain. 1. Mixing - Completely solubilize the crystallizing agent in water to form SDCM and optionally add an activator. 2. Forming - The composition from the mixing step is shaped by techniques including crystallization into the desired SDC size and dimensions. 3. Drying - The amount of water is reduced to ensure desired performance including dissolution, hydration, and thermal stability, and optionally an active agent is added.

[0247] Preparation of PEGC Domains - All weights listed in this section of the table correspond to the amount of PEG and coolant added to make the PEGC. Any water added to the domain by the inclusion of the perfume capsule slurry is not removed and remains part of the domain when combined to form the low moisture composition.

[0248] Low moisture composition - All weights listed in this section correspond to the amount of SDC and PEGC combined to make the low moisture composition particles. For clarity, the percentages of the components of the low moisture composition are provided as follows: "CA%" = crystallization agent from SDC in the final low moisture composition, "Fragrance capsule%" = fragrance capsule in the final low moisture composition, "Fragrance%" = neat fragrance in the low moisture composition, "PEG%" = PEG in the low moisture composition, "Water%" = water in the low moisture composition including water not removed from PEGC. Finally, "Average mass" = average mass of particles made as described in each example of the low moisture composition.

[0249] The data in Tables 9-10 provide predictive particles composed only of SDC and PEGC domains, the former with different blends of crystallization agents and cooling benefit agents, the latter with different molecular weights of PEG and cooling benefit agents.

[0250] The data in Tables 11-12 provide predictive low moisture compositions comprising a physical mixture of particles having SDC domains, PEGC domains, and cooling benefit agents. The amount of "perfume capsules in wash" is the dosage of perfume capsules in wash to deliver the desired dry fabric feel benefit to the consumer. The amount of "neat capsules in wash" is the dosage of neat perfume in wash to deliver the desired wet fabric feel benefit to the consumer. The @ symbol displayed with the particles identifies the mass of the particle in the low moisture composition. The "composition dosage" is the sum of all particles in the low moisture composition and is the amount that the consumer adds to the wash liquor.

[0251] The data in Table 13 provide predicted low moisture compositions containing SDC domains prepared from mixtures of C8, C10, and C12 chain length fatty acids that are neutralized to produce SDC domains, and then combined with PEGC domains and flavor capsules having different wall structures.

[0252] material (1) Water: Millipore, Burlington, MA (18m-ohm resistance) (2) Sodium caprate (sodium octanoate, NaC8): TCI Chemicals, catalog number 00034 (3) Sodium caprate (sodium decanoate, NaC10): TCI Chemicals, catalog number D0024 (4) Sodium laurate (sodium dodecanoate, NaC12): TCI Chemicals, catalog number L0016 (5) Fragrance Capsule Slurry: Encapsys, Encapsulated Fragrance #1, Melamine Formaldehyde Wall Chemistry, Fragrance Encapsulation #1 (31% active) (6) Fragrance Capsule Slurry: Encapssys, Encapsulated Fragrance #2, Urea Wall Chemistry, (21% active) (7) PEG-6000 gmol -1 , Alfa Aesar, product code A17541.30. (8) PEG-8000gmol -1 , Alpha Aesar, product code 43443. (9) PEG-9000gmol -1 , Dow Chemical, Product Code C4633240. (10) PEG-10,000 gmol -1 , Alfa Aesar, product code B21955.30. (11) Neat Fragrance: International Flavors and Fragrances, Neat Fragrance #1 (12) Fatty acid blend: C810L, Procter & Gamble Chemicals, sample code: SR26399 (13) Lauric acid: Peter Cremer, Catalog No. FA-1299, Lauric acid (14) Sodium hydroxide (50 wt% solution): Fisher Scientific, catalog number SS254-4 (15) Fragrance Capsule Slurry: Encapssys, Encapsulated Fragrance #3, Polyacrylate Wall Chemistry, 21% wt. active (16) Fragrance capsule slurry: Encapssys, Encapsulated Fragrance #4, high core to wall ratio, polyacrylate wall chemistry, Encapsulated Fragrance #5, polyurea wall chemistry, 32 wt% active (17) Fragrance Capsule Slurry: Encapsulated Fragrance #6, Silica-Based Wall Chemistry, 6.2 wt.% Active

[0253] Example 1 Example 1 demonstrates a particle composed of two or more domains in which the SDC domain is completely encapsulated within a single PEGC domain (Figure 7).

[0254] This example demonstrates a composition that allows the amount and distribution of different cooling benefit agents to be tailored using different domains in a single particle. In this non-limiting example, SDC domains are dispersed in a continuous domain of PEGC. This offers several advantages. First, the SDC domains offer the opportunity to increase the amount of perfume capsules in the particle (e.g., about 18% by weight) compared to a single PEGC domain (e.g., about 1.2% by weight). Second, these particles maintain the "smooth" appearance from the PEGC, improving the particle's aesthetics. Third, such compositions offer advantages in manufacturing, as the flow properties of the "molten" composition are similar to those of the full PEG composition, offering the possibility that these composite compositions can be prepared with existing commercial equipment. Samples AA-AI are non-limiting examples of the possible compositions and weight ratios of different domains in the resulting particles that can be used as low moisture compositions.

[0255] Preparation of SDC domain Mixing-A 250ml stainless steel beaker (Thermo Fisher Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7CER Hotplate, Catalog No. NO97042-690). Water (Milli-Q Academic) and crystallizing agent were added to the beaker. A temperature probe was placed in the composition. A mixing device was assembled that included an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design, with the impeller positioned in the preparation. The heater was set to 80°C, the impeller was set to rotate at 250 rpm, and the composition was heated to 80°C until all the crystallizing agent was solubilized and the composition was clear. The preparation was then poured into a Max100 Mid Cup (Speed ​​Mixer), covered, and allowed to cool to 25°C. Cooling benefit agents were added as specified in the table by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) for 3 minutes at 3000 rpm.

[0256] Formulation - The preparation was poured onto aluminum foil to a uniform thickness of approximately 1 mm. The preparation was then placed in a refrigerator (VWR Door Solid Lock F Refrigerator 115V, 76300-508, or equivalent) equilibrated to 4° C. for 8 hours to allow the crystallizing agent to crystallize.

[0257] Drying - They were placed in a convection oven (Yamato, DKN400, or equivalent) set at 25°C for an additional 8 hours with a steady flow of air passing through to dry the compositions. The final SDC was confirmed to be less than 10% moisture by the moisture test method. The domains were either in the shape of the mold or flat sheets were crushed into coarse pieces around 1mm x 1mm in size.

[0258] Preparation of PEGC domain Separately, a 250 ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7CER Hotplate, Catalog No. NO97042-690). PEG (materials 8-11) was added to the beaker. A mixing device was assembled containing an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a three-blade impeller design to place the impeller in the composition. A temperature probe was also placed in the formulation. The impeller was set to rotate at 250 rpm. The formulation was heated to 100°C until the PEG was completely melted. Cooling benefit agents were added by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. This formulation was used to create a low moisture composition within 5 minutes of reaching the final temperature.

[0259] Preparation of low moisture compositions A 60 ml Speed ​​Mixer cup and cap was weighed. The cap was removed and the SDC domain was added to the cup. The cup was resealed with the cap and reweighed, and the mass of the SDC domain in the formulation is the difference in weight.

[0260] A second 60ml speed mixer cup and cap was weighed. The cap was removed and the cooling benefit agent was added to the cup. The cup was resealed with the cap and reweighed, where the mass of cooling benefit agent in the formulation is the difference in weight. The cap was again removed from the cup.

[0261] In less than 30 seconds, the PEGC was added to the cup, the cap replaced, the entire formulation re-weighed, and the mass of PEGC in the formulation is the difference in weight. The cup was placed in a Speedmixer, started, and the formulation mixed at 3000 RPM for 1 minute. In less than 30 seconds after mixing (and before crystallization), the formulation was transferred to a polymer mold patterned with a 5 mm diameter hemisphere. The formulation was allowed to cool at 25° C. for at least 30 minutes. A diagram of the structure of the particles in this low moisture composition is shown in FIG. 7.

[0262] [Table 4]

[0263] [Table 5]

[0264] [Table 6]

[0265] Example 2 Example 2 demonstrates a particle composed of two or more domains in which a single SDC domain is coated and completely encapsulated in a coating of PEGC domains (Figure 8).

[0266] This example demonstrates that the composition has particles with an SDC domain core and a PEGC coating. In this non-limiting example, the SDC single domain is encapsulated within a continuous domain of PEGC. This has several advantages. These particles offer the opportunity to increase the amount of perfume capsules in the SDC domains (e.g., about 18% by weight) versus the amount of perfume capsules in the SDC domains (e.g., about 1.3% by weight). The particles have about a 10-fold increase in cooling benefit agent capacity. The SDC domains are also about 50-70% less dense, making the particles (and the resulting low moisture compositions) more favorable for different commercial approaches such as e-commerce, more sustainable with less carrier required per unit cooling, and more sustainable replacement of petroleum-based PEG with natural crystallizing agents. Additionally, the use of the PEGC coating allows the particles to maintain the "smooth" or glossy appearance of the PEGC domains, which is appreciated by many consumers. Samples BA-BI are non-limiting examples of the different domain compositions and weight ratios possible in the resulting particles.

[0267] Preparation of SDC domain Mixing-A 250ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). Water (Milli-Q Academic) and crystallizing agent were added to the beaker. A temperature probe was placed in the composition. A mixing device was assembled that included an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design, and the impeller was placed in the composition. The heater was set to 80°C, the impeller was set to rotate at 250 rpm, and the composition was heated to 80°C until all the crystallizing agent was solubilized and the composition was clear. The preparation was then poured into a Max100 Mid Cup (Speed ​​Mixer), covered, and allowed to cool to 25°C. Cooling benefit agents were added as specified in the table by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) for 3 minutes at 3000 rpm.

[0268] Formulation - The preparation was transferred to a polymer mold patterned with a hemisphere of 5 mm diameter. The mold was then placed in a refrigerator (VWR Door Solid Lock F Refrigerator 115V, 76300-508, or equivalent) equilibrated to 4°C for 8 hours to allow the crystallizing agent to crystallize.

[0269] Drying - They were placed in a convection oven (Yamato, DKN400, or equivalent) set at 25°C for an additional 8 hours with a steady flow of air passing through to dry the compositions. The final SDC was confirmed to be less than 10% moisture by the Moisture Test Method.

[0270] Preparation of PEGC domain Separately, a 250 ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). PEG (materials 8-11) was added to the beaker. A mixing device was assembled containing an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design to place the impeller in the composition. A temperature probe was also placed in the formulation. The impeller was set to rotate at 250 rpm. The formulation was heated to 100°C until the PEG was completely melted. Cooling benefit agents were added by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. This formulation was used to create a low moisture composition within 5 minutes of reaching the final temperature.

[0271] Preparation of low moisture compositions The weighing dish was weighed. SDC was placed in the weighing dish and the weight of SDC was determined by mass difference. SDC was immersed in the PEGC melt. Excess PEGC was wiped off the surface of the SDC. The formulation was placed in a weighing dish. The formulation was allowed to cool at 25° C. for at least 30 minutes. The weighing dish was weighed and the weight of perfume was determined by mass difference. A diagram of the structure of the particles in this low moisture composition is shown in FIG. 8.

[0272] [Table 7]

[0273] [Table 8]

[0274] [Table 9]

[0275] Example 3 Example 3 shows a particle composed of two or more domains, where the particle has a core of PEGC domains and is interspersed with SDC domains (Figure 9).

[0276] Such particles provide the opportunity for particles with, for example, significant amounts of PEGC and SDC domains, independent of the solubility characteristics of each domain. In non-limiting Samples CA and CB, perfume capsules are placed in the SDC domains and released into the wash cycle at a rate consistent with the composition of the blend of crystallizing agents, and neat perfume is placed in the PEGC domains and released into the wash cycle at a rate consistent with the molecular weight of PEG. The percent solubility determined by the dissolution test method is not dependent on the different domains, in contrast to the particles described herein, for example, in Example 1. Such a morphology also allows the fixed domains to exhibit different functions in the particle, making it aesthetically advantageous for consumers. Moreover, such a morphology is easy to prepare commercially, for example, by passing warm PEGC domains through a "dusting" of SDC domain particles, which may adhere to the surface of the domains.

[0277] Preparation of SDC domain Mixing-A 250ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). Water (Milli-Q Academic) and crystallizing agent were added to the beaker. A temperature probe was placed in the composition. A mixing device was assembled that included an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design, and the impeller was placed in the composition. The heater was set to 80°C, the impeller was set to rotate at 250 rpm, and the composition was heated to 80°C until all the crystallizing agent was solubilized and the composition was clear. The preparation was then poured into a Max100 Mid Cup (Speed ​​Mixer), covered, and allowed to cool to 25°C. Cooling benefit agents were added as specified in the table by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) for 3 minutes at 3000 rpm.

[0278] Formulation - The preparation was poured onto aluminum foil to a uniform thickness of approximately 1 mm. The preparation was then placed in a refrigerator (VWR Door Solid Lock F Refrigerator 115V, 76300-508, or equivalent) equilibrated to 4° C. for 8 hours to allow the crystallizing agent to crystallize.

[0279] Drying - They were placed in a convection oven (Yamato, DKN400, or equivalent) set at 25°C for an additional 8 hours with a steady flow of air passing through to dry the compositions. The final SDC was confirmed to be less than 10% moisture by the Moisture Test Method. The flat sheets were crushed into coarse pieces approximately 1mm x 1mm in size.

[0280] Preparation of PEGC domain Separately, a 250 ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). PEG (materials 8-11) was added to the beaker. A mixing device was assembled containing an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design to place the impeller in the composition. A temperature probe was also placed in the formulation. The impeller was set to rotate at 250 rpm. The formulation was heated to 100°C until the PEG was completely melted. Cooling benefit agents were added by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. This formulation was used to create a low moisture composition within 5 minutes of reaching the final temperature.

[0281] Preparation of low moisture compositions A small amount of PEGC was placed in a weighing dish and weighed. Prior to significant crystallization (within 30 seconds), a small amount of SDC was gently sprinkled onto the PEGC. Small sized SDC domains attached to the surface of the PEGC domains as the material crystallized. The preparation was allowed to cool at 25° C. for at least 30 minutes. The resulting particles were removed from the mold and reweighed to determine the amount of SDC associated. A diagram of the structure of the particles in this low moisture composition is shown in FIG. 9.

[0282] [Table 10]

[0283] Example 4 Example 4 demonstrates a particle composed of two or more domains, where the particle has one side containing a PEGC domain and one side containing an SDC domain (Figure 10).

[0284] Such particles also provide the opportunity to have the dissolution characteristics of each domain independently, for example, for particles with significant amounts of PEGC and SDC domains.In the non-limiting examples of Sample DA and Sample DB, perfume capsules are placed in the SDC domain and released in the wash cycle at a rate consistent with the composition of the blend of crystallizing agents, and neat perfume is placed in the PEGC domain and released in the wash cycle at a rate consistent with the molecular weight of PEG.The solubility percentage determined by the dissolution test method here is not dependent on different domains, in contrast to the particles described in, for example, Example 1.Furthermore, such a morphology does not impose any restrictions on the absolute amount of SDC and PEGC domains in the particles, as compared to Example 3.

[0285] Preparation of SDC domain Mixing-A 250ml stainless steel beaker (Thermo Fisher Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7CER Hotplate, Catalog No. NO97042-690). Water (Milli-Q Academic) and crystallizing agent were added to the beaker. A temperature probe was placed in the composition. A mixing device was assembled that included an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design, with the impeller positioned in the preparation. The heater was set to 80°C, the impeller was set to rotate at 250 rpm, and the composition was heated to 80°C until all the crystallizing agent was solubilized and the composition was clear. The preparation was then poured into a Max100 Mid Cup (Speed ​​Mixer), covered, and allowed to cool to 25°C. Cooling benefit agents were added as specified in the table by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) for 3 minutes at 3000 rpm.

[0286] Formulation - The preparation was transferred to a polymer mold patterned with a hemisphere of 5 mm diameter. The mold was then placed in a refrigerator (VWR Door Solid Lock F Refrigerator 115V, 76300-508, or equivalent) equilibrated to 4°C for 8 hours to allow the crystallizing agent to crystallize.

[0287] Drying - They were placed in a convection oven (Yamato, DKN400, or equivalent) set at 25°C for an additional 8 hours with a steady flow of air passing through to dry the compositions. Once completely dry, the preparations were removed from the molds. The final SDC was confirmed to be less than 10% moisture by the Moisture Test Method.

[0288] Preparation of PEGC domain Separately, a 250 ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). PEG (materials 8-11) was added to the beaker. A mixing device was assembled containing an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design to place the impeller in the composition. A temperature probe was also placed in the formulation. The impeller was set to rotate at 250 rpm. The formulation was heated to 100°C until the PEG was completely melted. Cooling benefit agents were added by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. This formulation was used to make low moisture compositions within 5 minutes of reaching the final temperature. The preparation was transferred to a polymer mold patterned with 5 mm diameter hemispheres.

[0289] Preparation of low moisture compositions Within 30 seconds of placing the formulation in the mold, a domain of SDC was placed on the liquid PEGC and the flat side of the SDC was placed on the flat side of the PEGC. The formulation was allowed to cool at 25° C. for at least 30 minutes. After complete cooling, the low moisture composition was removed from the mold. The two domains were fixed and the resulting particles were spherical, as shown in FIG. 10.

[0290] [Table 11]

[0291] Example 5 Example 5 demonstrates a low moisture composition that is composed of two or more different particles, and the particles may contain a combination of SDC and PEGC domains as described in the previous examples, or may contain only a single SDC and PEGC domain with a cooling benefit agent.These non-limiting examples describe the latter.However, it is understood that the physical blending of such particles to create a low moisture composition may also include the former.

[0292] Particle composition Samples EA-EH (Tables 9 and 10) represent viable particle compositions containing a single SDC or PEGC domain. Samples EI-EQ (Tables 11 and 12) represent low moisture compositions of the present invention comprised of particle compositions. The type and amount of particles in the low moisture compositions are expressed as a "composition dose", or a typical amount used in one wash by a consumer. Many considerations are important when determining the dose, including the amount of "perfume capsule at wash" and the amount of "neat perfume at wash" added by the dose. However, other factors such as the selection of the composition of the SDC or PEGC domain are also important in providing a level of cooling benefit. For example, a consumer may prefer a very long-lasting refreshing sensation on dry fabrics during the wash, which may require a dose of about 5-10 grams of perfume capsule, or the consumer may prefer only an initial burst of refreshing sensation upon rubbing, which may require a dose of about 0.5-2 grams of perfume capsule. For example, a consumer may prefer a very "instant" coolness upon removing a damp fabric from a wash solution that may require about 5-10 grams of neat perfume, or a consumer may prefer a subtle, pleasant lingering coolness upon removing a damp fabric from a wash solution that may require only about 1-2 grams of pure perfume in the wash solution. These coolness profiles are further influenced by the dissolution rate of the domains that contain the cool benefit agent. Finally, the selection of particles that make up the low moisture composition is also influenced by commercial considerations. In many cases, it is more commercially viable to create two types of particles and physically mix them in different ratios to allow the composition to reach all consumer preferences, rather than a special process for each consumer. This is often referred to as "delayed product differentiation." Some consumers may prefer a dose that contains a large amount of composition, on the order of about 50-100 grams, while some e-consumers or sustainability-conscious consumers may prefer a more concentrated, compact dose of about 10-20 grams. Finally, these examples provide a variety of coolness performance and commercial opportunities.

[0293] [Table 12] * Fragrance capsule slurry prepared from materials 5 and 6.

[0294] [Table 13] * Fragrance capsule slurry prepared from materials 5 and 6.

[0295] [Table 14]

[0296] [Table 15]

[0297] Example 6 Example 6 proposes that compositions prepared from a specific blend of fatty acid materials neutralized to SDC compositions and blended with PEGC compositions to produce solid dissolving compositions with SDC (e.g., Figures 4A, 4B, and 4C) and PEGC domains having different dissolution rate profiles allow different ordering of actives in each domain at specific times of the wash cycle. The dissolution rate of SDC is affected by the percentage of slow crystallizing agent (retardant CA%), with higher concentrations of SDC (e.g., sample EU) dissolving slower than lower concentrations of SDC (e.g., sample ER). The absolute dissolution rate at different temperatures is determined by the dissolution test method. The dissolution rate of PEGC is affected by the molecular weight of PEG, whereby sample ER (e.g., PEG 10,000) dissolves slower than sample ES (e.g., PEG 8,000), which dissolves slower than samples ET and EU (e.g., PEG PEG 6,000). The absolute dissolution rate at different temperatures is determined by the dissolution test method.

[0298] Preparation of SDC domain Mixing-A 250ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7CER Hotplate, Catalog No. NO97042-690). Water (Milli-Q Academic) and crystallizing agent were added to the beaker. A temperature probe was placed in the composition. A mixing device was assembled that included an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design, with the impeller positioned in the composition. The heater was set to 80°C, the impeller was set to rotate at 250 rpm, and the composition was heated to 80°C until all the crystallizing agent was solubilized and the composition was clear.

[0299] Formation - The composition was then poured into a Max100 Mid Cup, covered, and allowed to cool to 25°C. The cooling benefit agent was added by placing the formulation in a Speedmixer (Flack Tek.Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. In a non-limiting example, the formulation was transferred to a polymer mold patterned with hemispheres 5 mm in diameter. In another non-limiting example, the formulation was sprayed through an orifice to create small droplets. The size and shape of the DSC domains are formed to fill the final structure of the final low moisture composition (e.g., Figures 7, 8, 9, and 10). The mold was then placed in a refrigerator (VWR Door Solid Lock F Refrigerator 115V, 76300-508, or equivalent) equilibrated to 4°C for 8 hours to allow the crystallizing agent to crystallize.

[0300] Drying - The formulation was placed in a convection oven (Yamato, DKN400, or equivalent) set at 25°C for an additional 8 hours with a steady stream of air passing through to dry the composition. Once completely dry, the formulation was removed from the mold. The final SDC was confirmed to be less than 10% moisture by the Moisture Test Method.

[0301] Preparation of PEGC domain Separately, a 250 ml stainless steel beaker (Thermo Fischer Scientific, Waltham, MA) was placed on a hot plate (VWR, Radnor, PA, 7x7 CER Hotplate, Catalog No. NO97042-690). PEG (materials 8-11) was added to the beaker. A mixing device was assembled containing an overhead mixer (IKA Works Inc, Wilmington, NC, model RW20 DMZ) and a 3-blade impeller design to place the impeller in the composition. A temperature probe was also placed in the formulation. The impeller was set to rotate at 250 rpm. The formulation was heated to 100°C until the PEG was completely melted. Cooling benefit agents were added by placing the formulation in a Speedmixer (Flack Tek. Inc, Landrum, SC, model DAC 150.1 FVZ-K) at 3000 rpm for 3 minutes, as specified in the table. In a non-limiting example, the preparation was used to create a low moisture composition within 5 minutes of reaching the final temperature. In a non-limiting example, the preparation was transferred to a polymer mold patterned with 5 mm diameter hemispheres. The size and shape of the DSC domains are shaped to fill the final structure of the final low moisture composition (e.g., Figures 7, 8, 9, and 10).

[0302] Preparation of low moisture compositions Sample ER (5 mg) - SDC composition is sprayed as small droplets onto a flat sheet, crystallized, and dried. PEGC is sprayed onto a flat sheet and crystallized. The two flat ends are combined to create low moisture composition particles (e.g., FIG. 10). Sample ES (5 mg) - SDC composition is sprayed as small droplets onto a flat sheet, crystallized, and dried. PEGC is sprayed onto the surface of the SDC composition and crystallized. The low moisture composition is a coated particle (e.g., FIG. 8). Sample ET (500 mg) - PEGC composition is placed onto a flat sheet as large droplets, crystallized, and dried. SDC is sprayed to produce fine granules that adhere to the surface of the large droplets. The low moisture composition is a sugar gum droplet-like particle (e.g., FIG. 9). Sample EU (500 mg) - SDC composition is a spray-dried small particle. Small SDC particles are added to a PEGC melt and a larger droplet is placed on a flat surface and allowed to crystallize. The low moisture composition encapsulates the SDC (e.g., Figure 7).

[0303] In non-limiting cases, the final low moisture composition for the cleaning process may contain particles including one of the particle combinations described in Sample ER, Sample ES, Sample ET, and Sample EU.

[0304] [Table 16]

[0305] Dimensions and values ​​disclosed herein should not be understood as being strictly limited to the exact numerical values ​​recited. Instead, unless otherwise specified, each such dimension is intended to mean both the recited value and a functionally equivalent range surrounding that value. For example, a dimension disclosed as "40 mm" is intended to mean "about 40 mm."

[0306] All documents cited herein, including any cross-referenced or related patents or patent applications, and any patent applications or patents to which this application claims priority or benefit, are incorporated herein by reference in their entirety, unless expressly stated to the contrary. The citation of any document shall not be deemed to be prior art to any invention disclosed or claimed herein, or to teach, suggest, or disclose any such invention, either alone or in combination with any other reference or references. Furthermore, to the extent that any meaning or definition of a term in this document conflicts with any meaning or definition of the same term in a document incorporated by reference, the meaning or definition given to that term in this document shall govern.

[0307] While particular embodiments of the present invention have been illustrated and described, it would be obvious to those skilled in the art that various other changes and modifications can be made without departing from the spirit and scope of the invention. It is therefore intended to cover in the appended claims all such changes and modifications that are within the scope of this invention.

Claims

1. 1. A low moisture composition comprising: 1) at least one solid soluble composition (SDC) domain having a crystallization agent; 2) at least one polyethylene glycol (PEGC) domain; 3) a population of capsules containing a freshness benefit agent; the crystallization agent is a sodium salt of a saturated fatty acid having from 8 to about 12 carbon atoms; the capsule is present in at least one of the SDC or the PEGC; The capsule comprises: an oily core containing a cooling benefit agent; A shell surrounding the core, a substantially inorganic first shell component, a condensation layer comprising a condensation product of the precursors; a substantially inorganic first shell component comprising a nanoparticle layer comprising inorganic nanoparticles, the condensation layer being disposed between the core and the nanoparticle layer; a shell comprising an inorganic second shell component surrounding the first shell component, the inorganic second shell component surrounding the nanoparticle layer; The precursor comprises at least one compound of formula (I), (M v O z Y n ) w (Formula I) wherein M is one or more of silicon, titanium, and aluminum; v is the valence of M and is 3 or 4; z is 0.5 to 1.6; Each Y is independently -OH, -OR 2 , Halo, 【Chemistry 1】 -NH 2 , -NHR 2 , -N(R 2 ) 2 , and 【Chemistry 2】 wherein R 2 is C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; R 3 is H, C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; n is 0.7 to (v-1); A low moisture composition, wherein w is 2 to 2000.

2. 2. The low moisture composition of claim 1, wherein the sodium salts of saturated fatty acids of the crystallization agent comprise 50% to 70% by weight C12, 15% to 25% by weight C10, and 15% to 25% by weight C8.

3. 2. The low moisture composition of claim 1, wherein the sodium salt of a saturated fatty acid comprises 50% to 70% percent slow crystallization agent (Slow CA%).

4. 4. The low moisture composition of claim 1, wherein the crystallization agent is in the form of a fiber as determined by the Fiber Test Method.

5. 5. The low moisture composition of any one of claims 1 to 4, wherein the amount of water is less than 10% by weight of the final low moisture composition as determined by the Moisture Test Method.

6. The cooling benefit agent is at least one of a fragrance or a malodor counteractant, preferably the cooling benefit agent is a neat fragrance, more preferably the cooling benefit agent is 3-(4-t-butylphenyl)-2-methylpropanal, 3-(4-t-butylphenyl)-propanal, 3-(4-isopropylphenyl)-2-methylpropanal, 3-(3,4-methylenedioxyphenyl)-2-methylpropanal, and 2,6-dimethyl-5-heptenal, α-damascone, β-damascone, γ-damascone, β-damascenoic acid ... 6,7-dihydro-1,1,2,3,3-pentamethyl-4(5H)-indanone, methyl-7,3-dihydro-2H-1,5-benzodioxepin-3-one, 2-[2-(4-methyl-3-cyclohexenyl-1-yl)propyl]cyclopentan-2-one, 2-sec-butylcyclohexanone, and at least one of β-dihydroionone, linalool, ethyl linalool, tetrahydrolinalool, dihydromyrcenol, or mixtures thereof. The low moisture composition according to any one of claims 1 to 5.

7. 7. The low moisture composition of any one of claims 1 to 6, wherein the inorganic nanoparticles of the first shell component comprise at least one of metal nanoparticles, mineral nanoparticles, metal oxide nanoparticles, or semi-metal oxide nanoparticles.

8. The inorganic nanoparticles are SiO 2 , TiO 2 , Al 2 O 3 , Fe 2 O 3 , Fe 3 O 4 , CaCO 3 , clay, silver, gold, or copper, and preferably the inorganic nanoparticles are SiO2, CaCO 3 , Al 2 O 3 8. The low moisture composition of claim 1, comprising:

9. The inorganic second shell component is SiO 2 , TiO 2 , Al 2 O 3 , CaCO 3 , Ca 2 SiO 4 , Fe 2 O 3 , Fe 3 O 4 , iron, silver, nickel, gold, copper, or clay, and preferably the inorganic second shell component is SiO 2 or CaCO 3 The low moisture composition according to any one of claims 1 to 8, comprising at least one of:

10. 10. The low moisture composition of any one of claims 1 to 9, wherein the capsules have an average volume weighted capsule diameter of from about 0.1 μm to about 200 μm.

11. The low moisture composition of any one of claims 1 to 10, wherein the shell has a thickness of from about 10 nm to about 10,000 nm.

12. 12. The low moisture composition of any one of claims 1 to 11, wherein the compound of formula (I) has a polystyrene equivalent weight average molecular weight (Mw) of from about 700 Da to about 30,000 Da, and the compound of formula (I) has a degree of branching of from 0.2 to about 0.

6.

13. The low moisture composition of any one of claims 1 to 12, wherein the compound of formula (I) has a molecular weight polydispersity index of from about 1 to about 20.

14. The precursor comprises at least one compound of formula (II), (M v O z Y n R 1 p ) w (Formula II) wherein M is one or more of silicon, titanium, and aluminum; v is the valence of M and is 3 or 4; z is 0.5 to 1.6; Each Y is independently -OH, -OR 2 , Halo, 【Chemistry 3】 -NH 2 , -NHR 2 , -N(R 2 ) 2 , and 【Chemistry 4】 wherein R 2 is C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; R 3 is H, C 1 ~C 20 Alkyl, C 1 ~C 20 Alkylene, C 6 ~C 22 aryl, or a 5-12 membered heteroaryl containing 1-3 ring heteroatoms selected from O, N, and S; n is 0 to (v-1); Each R 1 is independently 1 ~C 30 Alkyl, C 1 ~C 30 Alkylene, C 1 ~C 30 Alkyl, halogen, -OCF 3 , -NO 2 , -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, CO 2 H, CO 2 C substituted with one or more of alkyl, aryl, and heteroaryl 1 ~C 30 Alkyl and halogen, -OCF 3 , -NO 2 , -CN, -NC, -OH, -OCN, -NCO, alkoxy, epoxy, amino, mercapto, acryloyl, CO 2 H, CO 2 C substituted with one or more of alkyl, aryl, and heteroaryl 1 ~C 30 is selected from p is present in an amount of at most pmax; w is 2 to 2000; pmax=60 / [9 * Mw(R 1 ) + 8], Mw (R 1 ) is R 1 The low moisture composition according to any one of claims 1 to 13, wherein the molecular weight of the group is the molecular weight of the group.

15. 15. The low moisture composition of claim 14, wherein the compound of formula (II) has a weight average molecular weight (Mw) in terms of polystyrene of about 700 Da to about 30,000 Da.

Citation Information

Patent Citations

  • Soap composition

    JP1988248899A

  • Mild cosmetic cleansing bar soap with improved processability

    JP1994506260A

  • Method for producing aromatic beads

    JP2001521058A

  • Molded soap article containing talc, one or more fatty acids in the form of their alkali soap, and one or more fat reforming materials, simultaneous, in the absence of alkyl (Oligo) glycoside

    JP2002097496A

  • capsule

    JP2022525996A