Long cylindrical ceramic body

The elongated cylindrical ceramic body design with inclined inner wall surfaces addresses discontinuities in metallized layers, enhancing electron beam deflection stability and durability in electron beam exposure apparatuses.

JP7555751B2Active Publication Date: 2024-09-25KYOCERA CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020129018
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-07-30
Publication Date
2024-09-25
Estimated Expiration
2040-07-30

AI Technical Summary

Technical Problem

Conventional liner tubes in electron beam exposure apparatuses suffer from discontinuous metallized layers at connection surfaces and difficulty in controlling the thickness of the titanium metallized layer, leading to challenges in electron beam deflection control.

Method used

An elongated cylindrical ceramic body with a design featuring a first inner circumferential portion, a second inner circumferential portion with a smaller diameter, and a connecting portion with an inclined inner wall surface, where metallized layers are applied, reducing the likelihood of discontinuities and stress concentration.

Benefits of technology

The design minimizes discontinuous portions in the metallized layer, ensuring stable electron beam deflection and prolonged durability even in environments with heating and cooling cycles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555751000001
    Figure 0007555751000001
  • Figure 0007555751000002
    Figure 0007555751000002
Patent Text Reader

Abstract

To provide a long cylindrical ceramic body in which even if a metalized layer is formed on an inner peripheral surface, a discontinuous portion is not likely to be generated on the metalized layer.SOLUTION: A long cylindrical ceramic body according to the present disclosure includes a ceramic main body having a cylindrical shape. An inner peripheral surface in the vicinity of one end of the ceramic main body is a first inner peripheral surface; an inner peripheral surface in the vicinity of the other end of the ceramic main body is a second inner peripheral surface; a portion connecting the first inner peripheral surface and the second inner peripheral surface with each other is a connection part. The second inner peripheral surface has a smaller diameter than that of the first inner peripheral surface. The center of the diameter of the first inner peripheral surface and the center of the diameter of the second inner peripheral surface are present on the same axis. At least part of an inner wall surface of the connection part is inclined with respect to the axis.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an elongated tubular ceramic body. [Background technology]

[0002] Conventionally, in an electron beam exposure apparatus, a liner tube is provided in an optical barrel to maintain a vacuum around the optical axis. An electromagnetic lens, an electromagnetic deflector, etc. are arranged on the outer periphery of the liner tube. Patent Document 1 describes a liner tube in which a titanium metallized layer and a platinum plated layer are sequentially formed on the inner surface of a ceramic cylinder.

[0003] However, the liner tube described in Patent Document 1 is prone to discontinuity of the metallization layer at both ends of the connection surface connecting the large diameter inner surface and the small diameter inner surface. Furthermore, it is difficult to sufficiently control the thickness of the titanium metallization layer. Therefore, it is difficult to control the deflection of the electron beam in a charged particle beam device equipped with the liner tube described in Patent Document 1. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-6594 ​​A DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]

[0005] An object of the present disclosure is to provide a long cylindrical ceramic body in which, even when a metallized layer is formed on the inner circumferential surface, discontinuous portions are unlikely to occur in the metallized layer. [Means for solving the problem]

[0006] The long cylindrical ceramic body according to the present disclosure includes a cylindrical ceramic body, an inner circumferential surface near one end of the ceramic body being a first inner circumferential portion, an inner circumferential surface near the other end of the ceramic body being a second inner circumferential portion, a portion connecting the first inner circumferential portion and the second inner circumferential portion being a connecting portion, the second inner circumferential portion having a smaller diameter than the first inner circumferential portion, the center of diameter of the first inner circumferential portion and the center of diameter of the second inner circumferential portion being on the same axis, and at least a portion of the inner wall surface of the connecting portion being inclined with respect to the axis.

[0007] The liner tube of the present disclosure includes the above-mentioned long cylindrical ceramic body, and has a metallized layer laminated on at least the surface of the first inner circumferential portion facing the connection portion, at least the surface of the second inner circumferential portion facing the connection portion, and the inner wall surface of the connection portion.

[0008] A charged particle beam device according to the present disclosure includes the above-mentioned liner tube, and an electromagnetic lens or an electromagnetic deflector on the outer periphery of the liner tube. Effect of the Invention

[0009] According to the present disclosure, it is possible to provide a long cylindrical ceramic body in which, even when a metallized layer is formed on the inner circumferential surface, discontinuous portions are unlikely to occur in the metallized layer. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2A is an explanatory diagram showing a long cylindrical ceramic body according to one embodiment of the present disclosure, and FIG. 2B is an explanatory diagram showing a cross section taken along line XX shown in FIG. [Diagram 2] FIG. 4 is an explanatory diagram showing a cross section of a long cylindrical ceramic body according to another embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] As described above, the long cylindrical ceramic body according to the present disclosure includes a ceramic body having a cylindrical shape, an inner circumferential surface near one end of the ceramic body is a first inner circumferential portion, an inner circumferential surface near the other end of the ceramic body is a second inner circumferential portion, and a portion connecting the first inner circumferential portion and the second inner circumferential portion is a connecting portion. The long cylindrical ceramic body according to the present disclosure will be described with reference to Figures 1 and 2.

[0012] 1(A), a long cylindrical ceramic body 1 according to one embodiment includes a cylindrical ceramic main body 10. In this specification, "long" means a length of 100 mm or more.

[0013] The ceramic body 10 is not limited as long as it is made of ceramic. Examples of ceramic include ceramics whose main components are aluminum oxide, silicon carbide, silicon carbonitride, titanium carbide, and titanium carbonitride. In this specification, the term "main component" refers to a component that accounts for 80% by mass or more of the total 100% by mass of the components that make up the ceramic. Each component contained in the ceramic is identified by an X-ray diffraction device using CuKα rays, and the content of each component may be determined by, for example, an ICP (Inductively Coupled Plasma) emission spectroscopic analyzer or a fluorescent X-ray analyzer.

[0014] In the case of ceramics whose main component is aluminum oxide, for example, magnesium, calcium and silicon may further be contained as oxides.

[0015] The length of the ceramic body 10 is not limited as long as it is 100 mm or more, and is appropriately set depending on the application of the long cylindrical ceramic body to be obtained. The length of the ceramic body 10 is, for example, about 100 mm or more and 250 mm or less. The outer diameter of the ceramic body 10 is also not limited, and is appropriately set depending on the application of the long cylindrical ceramic body to be obtained. The outer diameter of the ceramic body 10 is, for example, about 18 mm or more and 40 mm or less. In the case where the ceramic body does not have a single thickness (outer diameter) like the ceramic body 10, it is sufficient that the outer diameter of the thinnest part and the outer diameter of the thickest part have lengths in the above-mentioned ranges.

[0016] The inner peripheral surface of the ceramic body 10 will be described with reference to Fig. 1(B). As shown in Fig. 1(B), a first inner peripheral portion 11 is located near one end of the ceramic body 10, and a second inner peripheral portion 12 is located near the other end of the ceramic body 10. The first inner peripheral portion 11 has a length from one end face of the ceramic body 10 to about 45% of the total length of the ceramic body 10. The second inner peripheral portion 12 has a length from the other end face of the ceramic body 10 to about 35% of the total length of the ceramic body 10.

[0017] The second inner circumferential portion 12 has a smaller diameter than the first inner circumferential portion 11. The diameter D2 of the second inner circumferential portion 12 is not limited as long as it is smaller than the diameter D1 of the first inner circumferential portion 11. For example, the diameter D2 of the second inner circumferential portion 12 may be approximately 50% to 65% of the diameter D1 of the first inner circumferential portion 11. The center of the diameter D1 of the first inner circumferential portion 11 and the center of the diameter D2 of the second inner circumferential portion 12 are on the same axis.

[0018] In the long cylindrical ceramic body 1 according to one embodiment, the first inner peripheral portion 11 and the second inner peripheral portion 12 are connected via the connecting portion 13. Since the diameter D1 of the first inner peripheral portion 11 and the diameter D2 of the second inner peripheral portion 12 are different in size, the diameter of one end of the connecting portion 13 is different in size from the diameter of the other end. Therefore, at least a part of the inner wall surface of the connecting portion 13 is inclined with respect to the axis passing through the center of the diameter D1 of the first inner peripheral portion 11 and the center of the diameter D2 of the second inner peripheral portion 12. As a result, even if a metallized layer is formed on the inner wall surfaces of the first inner peripheral portion 11, the second inner peripheral portion 12, and the connecting portion 13, discontinuous portions are unlikely to occur in the metallized layer. The inclination angle of the inner wall surface of the connecting portion 13 with respect to the axis is not particularly limited, and may be, for example, about 4° to 18°.

[0019] As in the case of a long cylindrical ceramic body 1' according to another embodiment shown in Fig. 2, the inner wall surface of the connecting portion 13' may have a curvature. When the inner wall surface of the connecting portion 13' has a curvature in this manner, both ends of the connecting portion 13' are gently connected to the first inner circumferential portion 11' and the second inner circumferential portion 12'. As a result, even if a metallized layer is formed on the inner wall surfaces of the first inner circumferential portion 11', the second inner circumferential portion 12', and the connecting portion 13', discontinuous portions in the metallized layer are less likely to occur.

[0020] It is preferable that at least one of the ends of the connection part 13' has a larger curvature on the inner wall surface of the connection part 13' than the intermediate part of the connection part 13' sandwiched between the ends. In the case of such a configuration, even if a metallized layer is formed on the inner wall surfaces of the first inner circumferential part 11', the second inner circumferential part 12', and the connection part 13', stress is unlikely to concentrate on the metallized layer formed on both ends of the connection part 13'. As a result, the connection part 13' can be used for a long period of time, even in an environment where heating and cooling are repeated, for example.

[0021] The radius of curvature of the inner wall surface of the intermediate portion of the connecting portion 13' is not limited. The inner wall surface of the intermediate portion of the connecting portion 13' may have a radius of curvature of, for example, 250 mm or more, and preferably has a radius of curvature of about 300 mm or more and 350 mm or less. The radius of curvature of the inner wall surface of the end portion of the connecting portion 13' is preferably about 5 mm or more and 15 mm or less.

[0022] The method for producing the long cylindrical ceramic body of the present disclosure is not limited, and may be, for example, produced by the following procedure. First, aluminum oxide, silicon carbide, silicon carbonitride, titanium carbide, or titanium carbonitride powder is prepared. The purity of these powders is not limited. These powders may have a purity of, for example, 99% by mass or more. If necessary, other powders used as raw materials for ceramics may be used.

[0023] Hereinafter, a method for obtaining a long cylindrical ceramic body mainly composed of aluminum oxide will be described. First, aluminum oxide powder (with a purity of 99% by mass or more), which is the main component, and powders of magnesium hydroxide, silicon oxide, and calcium carbonate are charged into a grinding mill together with a solvent (ion-exchanged water) to obtain an average particle size (D 50 After pulverizing the powder to a particle size of 1.5 μm or less, an organic binder and a dispersant for dispersing the aluminum oxide powder are added and mixed to obtain a slurry.

[0024] Here, the content of magnesium hydroxide powder is 0.3 to 0.42 mass%, the content of silicon oxide powder is 0.5 to 0.8 mass%, the content of calcium carbonate powder is 0.060 to 0.1 mass%, and the remainder is aluminum oxide powder and unavoidable impurities, based on 100 mass% of the total of the above powders.

[0025] Examples of the organic binder include acrylic emulsion, polyvinyl alcohol, polyethylene glycol, and polyethylene oxide.

[0026] Next, the slurry is sprayed and granulated to obtain granules, which are then compressed at a molding pressure of 78 MPa to 128 MPa using a cold isostatic press to obtain a cylindrical compact. The compact is machined to form through holes along the axial direction.

[0027] The molded body having the through holes is sintered in an air atmosphere at a sintering temperature of 1500° C. to 1700° C. for a holding time of 4 hours to 6 hours to obtain a cylindrical sintered body. The outer peripheral surface of the obtained cylindrical sintered body is subjected to cylindrical grinding, and the inner peripheral surface is subjected to internal grinding, to obtain a long cylindrical ceramic body 1, 1' having a shape as shown in FIGS. 1 and 2.

[0028] The long cylindrical ceramic body of the present disclosure is used, for example, as a component of a liner tube. Hereinafter, a liner tube will be described taking as an example a case in which the long cylindrical ceramic body 1 according to one embodiment is used.

[0029] The liner tube of one embodiment of the present disclosure has a structure in which a metallized layer is laminated on at least the surface of the first inner circumferential portion 11 facing the connection portion 13 of the long cylindrical ceramic body 1 of one embodiment, on at least the surface of the second inner circumferential portion 12 facing the connection portion 13, and on the inner wall surface of the connection portion 13.

[0030] The metal contained in the metallization layer is not limited, and examples thereof include metals mainly composed of molybdenum, tungsten, titanium, silver, etc. Among these metals, metals mainly composed of molybdenum, tungsten, or titanium are preferable. Molybdenum, tungsten, and titanium are non-magnetic metals, and even if an electron beam passes through the internal space, they are unlikely to adversely affect the electron beam. Furthermore, molybdenum, tungsten, and titanium have a relatively high volume resistivity, and therefore are less likely to generate eddy currents.

[0031] When the metallization layer is mainly composed of molybdenum or tungsten, the metallization layer may contain 15% to 25% by mass of manganese and the remainder may be a metal that is the main component, out of 100% by mass of the metal elements that constitute the metallization layer.When the metallization layer is mainly composed of silver, the metallization layer may contain 25% to 30% by mass of copper, 0.8% to 2% by mass of titanium, and the remainder may be silver, out of 100% by mass of the metal elements that constitute the metallization layer.

[0032] The thickness of the metallization layer is not limited, and may be, for example, about 15 μm or more and 45 μm or less. The coefficient of variation of the thickness of the metallization layer is preferably, for example, 0.2 or less. If the coefficient of variation of the thickness of the metallization layer is 0.2 or less, the thickness variation is small even if the thickness of the metallization layer is made thin. As a result, discontinuous portions of the metallization layer are unlikely to occur, and the possibility of poor conduction is reduced.

[0033] The liner tube according to one embodiment may further include a first plating layer laminated on the metallized layer. The first plating layer is formed of a metal containing gold, platinum, or silver as a main component. The gold, platinum, or silver contained in such a first plating layer has a high standard potential and is also resistant to rust. As a result, the reliability of the liner tube can be further improved.

[0034] The thickness of the first plating layer is not limited, and may be, for example, about 0.01 μm or more and 0.1 μm or less. The arithmetic mean roughness Ra of the first plating layer is not limited, and may be, for example, about 1.1 μm or more and 1.7 μm or less. The coefficient of variation of the arithmetic mean roughness Ra on the surface of the first plating layer is preferably 0.2 or less (excluding 0). When the surface of the first plating layer has such a coefficient of variation of the arithmetic mean roughness Ra, gas is less likely to be adsorbed on the surface of the first plating layer. As a result, the exhaust efficiency for evacuating the internal space of the liner tube is improved.

[0035] The two-row root mean square slope RΔq of the first plating layer is not limited, and may be, for example, 0.4 or more and 1.6 or less. Furthermore, the coefficient of variation of the two-row root mean square slope RΔq on the surface of the first plating layer is preferably 0.25 or less (excluding 0). When the surface of the first plating layer has such a coefficient of variation of the two-row root mean square slope RΔq, gas is less likely to be adsorbed on the surface of the first plating layer. As a result, the exhaust efficiency for evacuating the internal space of the liner tube is further improved.

[0036] The arithmetic mean roughness Ra and the root mean square slope RΔq can be measured in accordance with JIS B 0601:2001 using a shape analysis laser microscope (Keyence Corporation, ultra-deep color 3D shape measuring microscope (VK-X1100 or its successor model)).

[0037] The measurement conditions are as follows: illumination method is coaxial illumination, magnification is 120x, cutoff value λs is none, cutoff value λc is 0.08mm, cutoff value λf is none, end effect correction is present, and the measurement range per point from the surface of the first plating layer to be measured is set to, for example, 2792μm×2093μm, and for each measurement range, one line to be measured is drawn along the longitudinal direction of the measurement range, and line roughness measurement is performed. The length of each line to be measured is, for example, 2640μm. The measurement range is set at eight points approximately equally spaced along the axial direction, and the number of lines to be measured is eight in total. The respective coefficients of variation of the arithmetic mean roughness Ra and the root mean square slope RΔq may be calculated from the average value and standard deviation obtained from the eight lines to be measured.

[0038] In the liner tube according to one embodiment, a second plating layer mainly composed of nickel may be laminated between the metallized layer and the first plating layer. By laminating the second plating layer, it is possible to suppress the components forming the first plating layer from diffusing into the metallized layer. The thickness of the second plating layer is not limited, and may be, for example, about 1 μm or more and 3 μm or less.

[0039] The coefficient of variation of the total thickness of the metallized layer, the first plating layer, and the second plating layer is preferably, for example, 0.2 or less. If the coefficient of variation of the total thickness of the metallized layer, the first plating layer, and the second plating layer is 0.2 or less, the thickness variation is small even if the thicknesses of these layers are made thin. As a result, the possibility of poor conduction is reduced.

[0040] When measuring the thickness of each of the metallized layer, the first plating layer, and the second plating layer, the liner tube is first cut or ground into a semi-cylindrical shape, and the cross section is then polished. The polished surface on one side obtained by this polishing is used as the measurement target, and 10 measurement ranges are set along the axial direction.

[0041] The measurement range may be set according to the length of the first inner circumference, the second inner circumference, and the connection part. In the case of the long cylindrical ceramic body 1', for example, 10 measurement ranges may be set, including 3 locations from the first inner circumference 11', 5 locations from the second inner circumference 12', and 2 locations from the connection part 13', so that the measurement ranges are approximately equally spaced for each part. Then, using a scanning electron microscope, the thickness of the layer to be measured may be measured at a magnification of, for example, 500 times. The coefficient of variation of the thickness of the metallized layer and the coefficient of variation of the total thickness of the metallized layer, the first plating layer, and the second plating layer may be calculated from the average value and standard deviation of the thicknesses obtained for each measurement range. Hereinafter, a method for manufacturing a liner tube will be described.

[0042] First, a paste containing molybdenum as a main component and manganese is applied to the inner wall surfaces of the first inner circumferential portion, the second inner circumferential portion and the connection portion of the long cylindrical ceramic body. The viscosity of the paste at room temperature is preferably 250p or less, particularly 210p or less. Next, the paste is heat-treated at a temperature of 1300°C to 1400°C in a forming gas atmosphere with a hydrogen:nitrogen volume ratio of 70-80:30-20. In this manner, a liner tube with a metallized layer laminated thereon can be obtained. Furthermore, when a first plating layer or a second plating layer is laminated, both layers may be laminated by electroless plating.

[0043] The liner tube according to the present disclosure is employed as a component of a charged particle beam device, such as, for example, an electron microscope, an ion beam microscope, an electron beam exposure device, an electron beam microanalyzer, an ion beam device, a cyclotron, an electron beam welding machine, etc. Such a charged particle beam device includes, for example, a liner tube according to an embodiment of the present disclosure and an electromagnetic lens or an electromagnetic deflector on the outer periphery of the liner tube. [Explanation of symbols]

[0044] 1, 1' Long cylindrical ceramic body 10 Ceramic body 11, 11' 1st inner circumference 12, 12' 2nd inner circumference 13, 13' Connection

Claims

1. a ceramic body having a cylindrical shape; an inner circumferential surface of the ceramic body in the vicinity of one end thereof is defined as a first inner circumferential portion, an inner circumferential surface of the ceramic body in the vicinity of the other end thereof is defined as a second inner circumferential portion, and a portion connecting the first inner circumferential portion and the second inner circumferential portion is defined as a connecting portion; The second inner periphery has a smaller diameter than the first inner periphery, a center of a diameter of the first inner circumferential portion and a center of a diameter of the second inner circumferential portion are on the same axis, The inner wall surface of the connection portion has a curvature, an inner wall surface of at least one of both end portions of the connection portion has a larger curvature than an inner wall surface of a middle portion sandwiched between the both end portions; The inner wall surface of the intermediate portion has a radius of curvature of 250 mm or more. A long cylindrical ceramic body, Including, A liner tube, comprising a metallized layer laminated on at least a surface of the first inner circumferential portion facing the connection portion, at least a surface of the second inner circumferential portion facing the connection portion, and an inner wall surface of the connection portion.

2. 2. The liner tube of claim 1, wherein the metallization layer comprises a major component of molybdenum, tungsten, or titanium.

3. 3. The liner tube of claim 1 or 2, wherein the metallization layer has a thickness coefficient of variation of 0.2 or less.

4. The liner tube according to any one of claims 1 to 3, further comprising a first plating layer mainly composed of gold, platinum or silver laminated on the metallized layer.

5. The liner tube according to claim 4 , further comprising a second plating layer, the second plating layer being mainly composed of nickel, laminated between the metallized layer and the first plating layer.

6. 6. The liner tube of claim 4 or 5, wherein the surface of the first plating layer has a coefficient of variation of arithmetic mean roughness Ra of 0.2 or less (excluding 0).

7. The liner tube of any one of claims 4 to 6, wherein the surface of the first plating layer has a coefficient of variation of the root mean square slope RΔq of 0.25 or less (excluding 0).

8. The liner tube according to any one of claims 5 to 7, wherein a coefficient of variation of a total thickness of the metallized layer, the first plating layer, and the second plating layer is 0.2 or less.

9. A charged particle beam device comprising the liner tube according to any one of claims 1 to 8, and an electromagnetic lens or an electromagnetic deflector on the outer periphery of the liner tube.

Citation Information

Patent Citations

  • Liner tube and charged particle beam device having the same

    JP2001006594A

  • Multi-piece wiring board

    JP2014045012A

  • Radiation generating tube, radiation generating apparatus using the same, and radiation imaging system

    JP2014241230A

  • X-ray generating tube, x-ray generating device, and x-ray imaging system

    JP2019009141A

  • Substrate for RFID tag, RFID tag, and RFID system

    JP2019110460A