Two-part glass reactor, manufacturing method and analytical method
The laser-etching method for glass reactors addresses mechanical damage and coating requirements, enabling high optical contrast and efficient light interaction in biochemical and biological processes.
Patent Information
- Application Number
- JP2022527207
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-11-12
- Filing Date
- 2020-11-10
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2040-11-10
AI Technical Summary
Existing methods for producing glass reactors with large aspect ratios and arrays of reactors are prone to mechanical damage and require selective coating, limiting their application in biochemical and biological processes.
A method involving laser irradiation and etching of glass plates to form recesses without mechanical action, allowing for high optical contrast and connection of glass plates without coatings, using laser pulses to create recesses with aspect ratios of at least 2:1, and connecting glass plates with fritted glass or anodic bonding.
The method enables the production of glass reactors with large aspect ratios and arrays without mechanical damage, suitable for biochemical and biological processes, providing high optical contrast and efficient light interaction.
Smart Images

Figure 0007560552000001 
Figure 0007560552000002 
Figure 0007560552000003
Abstract
Description
[Technical field]
[0001] The invention relates to a method for producing reactors made of glass, which are formed in the form of recesses in the glass, in which the reactors are formed in an array, which consists of two or more mutually connected glass elements, which are optionally connected to each other directly or by means of a connecting layer arranged between the glass elements. The method results in the formation of an array of a large number of reactors, which are formed in the glass, for example an array of 25x25 grids of 8x12 reactors each. The reactors are formed in a large number in a glass plate, which may consist of a first glass plate and a second glass plate closely connected to the first glass plate, or further glass plates connected in the same way. [Background technology]
[0002] The method has the advantage that the recesses forming the reactors are formed without mechanical action on the bulk glass, so that the reactors have no mechanical damage, e.g. microcracks. The reactors have a large aspect ratio of depth to diameter. A further advantage is that the method for producing the reactors can proceed without selective coating of at least the glass surfaces on which the cross-sectional openings of the reactors are formed, and optionally without any coating of the glass surfaces on which the reactors are formed.
[0003] 1999, pp. 1111-1115, 2003 describes the production of reactors 20 μm in diameter and 8 μm deep in a glass plate by etching after applying a mask made of chromium and a photoresist thereon.
[0004] US Pat. No. 5,399,433 describes the manufacture of reactors in glass using an ultrasonically irradiated tool and an abrasive between the tool and the glass.
[0005] US Patent No. 5,393,633 describes a microtiter plate with 96 wells, consisting of a glass bottom, which is transparent to UV light and connected by a glass frit to a glass plate, in which continuous recesses form the side walls of the wells.
[0006] US Pat. No. 5,399,633 describes the formation of surface structures on the bottom of a microtiter plate using photolithographic methods. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] US Patent Application Publication No. 2003 / 0211014 [Patent Document 2] European Patent Application Publication No. 1867612 [Patent Document 3] European Patent Application Publication No. 2011857 [Non-patent literature]
[0008] [Non-Patent Document 1] Deutsch et al., Lab Chip, 2006, 69, 995-1000 Summary of the Invention [Problem to be solved by the invention]
[0009] The object of the present invention is to provide an alternative manufacturing method suitable for producing reactors in glass, in particular with a large aspect ratio, with a generally small volume, and for providing an array of a large number of such reactors in glass. Preferably, the method should be suitable for providing an array of such reactors, such that when the glass is illuminated with light, it forms a high optical contrast for the cells in the reactor. [Means for solving the problem]
[0010] The present invention achieves this object with the features of the claims, in particular with a method for producing a glass reactor and with a glass reactor obtainable by said method, said method comprising the steps of: 1. A step of irradiating a laser beam having a wavelength that is transmitted through a first glass plate onto the surface of the first glass plate at locations where recesses are to be formed as reactors, preferably in a point-like manner; 2. Etching the first glass sheet to form recesses extending through the entire thickness of the first glass sheet, preferably for a length of time sufficient to form recesses along locations, preferably at least 40 μm or at least 30 μm deep, and preferably having a depth to diameter aspect ratio of at least 2, at least 4, at least 5 or at least 6 measured in the plane of the first surface; 3. After etching the first glass plate, connecting a second plate with the surface of the first glass plate to form a recess; The method comprises or consists of the steps:
[0011] In this regard, each glass pane may be a body made of glass having a lateral extent greater than its thickness, i.e., the pane may have a rectangular, circular or other shaped periphery that defines its facing surfaces.
[0012] The reactor is formed by a recess in the first glass plate, the recess having exactly one opening located in the plane of the first surface of the first glass plate. The use of the reactor is not limited to chemical reactions, but also includes biochemical, biological and physical processes. It may be a process with individual cells, which may be animal or plant cells or yeast cells, bacteria, viruses, proteins, etc., or clusters of these.
[0013] The point-like irradiation is obtained by focusing the laser beam to a point having a size of a few micrometers, for example 1 to 10 μm or even 5 μm. It is advantageous if the focus of the laser beam extends over a length along the propagation direction of the laser beam that is much larger than the Rayleigh length of a corresponding laser beam with a Gaussian distribution. This is obtained by suitable optical devices, for example diffractive optical elements. The irradiation can be a through irradiation or an irradiation that is not performed very deep, up to the first thickness part in contact with the first surface of the first glass sheet, for example by the focus of the laser beam not extending over the entire thickness of the glass sheet in the propagation direction of the laser beam. Since the interaction of the laser beam with the material of the glass sheet occurs only at the focus, it is possible to end the interaction area inside the first glass sheet. Preferably, the laser beam is composed of laser pulses.
[0014] When connecting the second glass sheet to a surface of the first glass sheet, the surface of the first glass sheet may be the first surface of the first glass sheet that is irradiated with the laser beam or may be the second surface opposite to the first surface.
[0015] In the absence of a coating of etching resist, the first surface of the first glass sheet and the second surface opposite the first surface are corroded during etching at the places where the laser was applied to the first glass sheet and towards which the laser beam was emitted, significantly faster than the adjacent areas. The areas of the first surface and possibly the second surface of the first glass sheet are thus corroded relatively slowly and conformally at a distance from the places of the point-like laser irradiation, for example because of the absence of a coating of etching resist. The first surface is thus formed by the surface parts, excluding the recesses, which are arranged in a plane from which the recesses extend into the glass volume of the first glass sheet. The surface parts, excluding the recesses, which are arranged in a common plane and form the first surface, are formed by the end faces of the walls located between the recesses. In the absence of a coating of the second surface opposite the first surface, the recesses can also extend into the glass volume starting from the second surface along the places where the laser beam was applied or passed in a point-like manner. In this case, a recess having an hourglass-shaped longitudinal section of the thickness of the glass sheet can be formed.
[0016] In step 2, etching is carried out for a length of time sufficient to form a recess that extends through the entire thickness of the first glass sheet, so that the depth of the recess corresponds to the depth of the first glass sheet.
[0017] Optionally, the point-like laser beam applied in step 1, with which recesses to form the reactors in step 2 are etched, is arranged in the plane of the first surface of the first glass plate at a distance of at least or exactly the diameter of one of the reactors, including the thickness of the wall between the reactors. The diameter of the reactors can be set by the reaction conditions and the duration of the etching, since the etching is performed concentrically around the straight path of the applied laser beam through the first glass plate. The walls arranged between the reactors end in a common plane. The end faces of these walls lie in a common plane and form a first surface or form a first surface in a common plane, the first surface being interrupted by a recess. The first surface is preferably interrupted only by the cross section of the recess.
[0018] The laser beam is preferably pulsed, for example having a wavelength of 1064 nm, and preferably having a pulse length of at most 100 ps or at most 50 ps, preferably at most 10 ps, at any location on the first glass sheet where the laser beam is applied. The laser is generally adjusted so that the laser beam does not impinge on the first glass sheet between said locations. Preferably, the laser beam is applied pointwise and perpendicularly on the surface of the first glass sheet. Preferably, the surface where the first laser beam is applied forms the first surface of the first glass sheet.
[0019] Etching is carried out using, for example, 1% to 48% by weight hydrofluoric acid, and / or sulfuric acid, and / or hydrochloric acid, and / or phosphoric acid, and / or nitric acid, or potassium hydroxide at a temperature of, for example, up to 140°C.
[0020] The first glass sheet may for example have a thickness before etching of up to 1000 μm, preferably from 100 μm to 1000 μm, such as up to 800 μm, for example from 300 μm to 500 μm, and after etching a thickness of 50 μm to 700 μm less, for example a thickness of up to 200 μm less.
[0021] The recess preferably extends in the shape of a cone or a frustocone, for example at an angle of between 0° and 15°, starting from the surface of the first glass sheet and extending within its volume.
[0022] In an embodiment according to the invention, in which a recess penetrates the first glass sheet and a second glass sheet is connected to the first glass sheet, the second surface of the first glass sheet may optionally be coated with an etching resist, the second surface of the first glass sheet facing the first surface and the laser beam being directed at the first surface or the laser beam being passed through the first surface and acting on the first glass sheet. Optionally, the etching resist may be applied over the entire second surface of the first glass sheet before or after irradiation with the laser beam.
[0023] Optionally, the first glass sheet in general can be etched without coating, for example without a mask and / or an etching resist, so that the method has the advantage that it is carried out without applying an etching resist to the glass sheet and without removing the etching resist from the glass sheet. In general, at least the first surface of the first glass sheet remains free of etching resist and mask and is etched without an etching resist.
[0024] Generally, optionally, the laser beam can be irradiated in a point-like manner at a plurality of mutually spaced positions, for example at least 3 or at least 10 or at least 30 positions, at every location where the first glass sheet is to be formed, the laser beam being irradiated successively or simultaneously, preferably parallel to each other and perpendicular to the first glass sheet. These positions form the locations where etching will corrode the first glass sheet faster than in the surface areas distant from the positions. The positions irradiated with the laser will cause the glass to corrode at a certain rate during etching, and together form the recesses. The positions irradiated in the area of the locations and forming the locations are arranged at intervals of, for example, 1 μm to 10 μm. Preferably, the positions are arranged around each location within the area where the recesses are to be formed, respectively. Preferably, the locations around which the laser beam is applied or to form the locations have a spacing of 1 μm to 10 μm, for example 2 μm to 5 μm or up to 3 μm, said spacing being determined in particular in the plane of the first surface of the first glass sheet.
[0025] Generally, the recesses can be formed by individual laser pulses or by multiple laser pulses. In the case of individual laser pulses, the diameter of the recesses is determined in particular by the duration of etching. In the case of forming recesses using multiple laser pulses, the diameter of the recesses is determined by the number and spacing of the positions at which the laser beam is irradiated for one location and penetrates into the first glass sheet. The depth of the recesses in the volume of the first glass sheet can be determined by the duration of etching and by the laser beam only partially penetrating the first glass sheet or not passing through the first glass sheet completely.
[0026] Optionally, a laser beam is applied around each location where a recess is to be formed, preferably in the shape of a ring, a rectangle or a hexagon, in a circumferentially closed path, for example formed by successively applied laser beam pulses. In this case, the laser beam pulses can be applied to the first glass surface on the circumferentially closed path, for example with a laser beam pulse interval of 3 μm, determined on the first surface of the first glass sheet. Optionally, therefore, the first glass sheet can be irradiated at each location with a laser beam in a point-like manner at a number of mutually spaced positions, around which a laser beam formed by successively applied laser beam pulses can be applied along a circumferentially closed path. The application of the laser beam along a circumferentially closed path has the advantage that, during the subsequent etching, recesses are formed with walls extending from the first surface and having a cross section surrounding the circumferentially closed path.
[0027] In general, the laser pulses can be applied to the first glass sheet at various depths at locations that form the locations where the etching will form recesses. For example, laser pulses can be applied deeper and penetrate deeper into the thickness of the first glass sheet at locations, and other laser pulses can be applied less deeply into the thickness of the first glass sheet at locations. During subsequent etching, deeper or wider recesses are formed at locations where the laser pulses are applied deeper into the glass sheet, and smaller recess bottoms are formed at locations where the laser pulses are applied less deeply into the glass sheet. In general, depending on the spacing of the locations, a concave indentation can be formed at the bottom at each location. A recess having a bottom and a deeper recess in the bottom can be formed by irradiating the laser pulse to a smaller depth into the first glass sheet at the location where the bottom is to be formed and by irradiating the laser pulse deeper into the first glass sheet at the location where the further recess is to be formed starting from the bottom and extending deeper into the first glass sheet, and by subsequent etching. For a larger diameter of the further recess extending deeper into the first glass sheet starting from the bottom of the recess, the laser pulses irradiated deeper into the first glass sheet can be spaced apart at adjacent locations, for example by 1 μm to 10 μm, for example by 2 μm to 5 μm or even 3 μm, so that at these locations the etching penetrates deeper into the first glass sheet. If at some locations the laser pulse can be directed to a smaller depth into the first glass sheet and at some locations the laser pulse can be directed deeper into the first glass sheet, then during etching at the locations where the laser pulse was directed to a smaller depth a concave bottom will be formed at a smaller depth and at the locations where the laser pulse was directed to a deeper depth a further recess will be formed that extends deeper into the first glass sheet.
[0028] In a further embodiment of the method, for example, comprising steps 1 to 3, the reactor is formed by a recess extending over the entire thickness of the first glass sheet, and the second sheet is connected to a surface of the first glass sheet. The second sheet forms the bottom of the reactor. The second sheet may then be connected to the first surface, preferably the second surface, of the first glass sheet. By arranging the second sheet on the second surface of the first glass sheet, the reactor is formed, which forms a cone shape from the opening located in the plane of the first surface of the first glass sheet towards the second glass sheet, and therefore does not form any undercut. The second sheet is preferably a second glass sheet, and is therefore also referred to as a second glass sheet in general, at will, instead of a second sheet made of another material. The second sheet may be a glass sheet or may comprise or consist of silicon, sapphire, ceramic, metal or at least two layers made of these.
[0029] In this case, the entire second surface of the first glass sheet is preferably coated with an etching resist in order to allow the etching to act only through the first surface. The coating of the second surface results in the formation of a recess extending from the first surface in a cylindrical or conical manner in the direction of the second surface, preventing the second surface from peeling off due to etching. In this embodiment, the etching can be acted on only the first surface of the first glass sheet in general until the recess extends in the plane of the second surface of the first glass sheet. It has been found that when the second surface is coated with an etching resist, the etching forms a recess through the entire thickness of the first glass sheet, the walls of the recess standing perpendicularly or at a conical or frustoconical angle to the plane of the second surface, and preferably does not have a transition curvature and / or a bevel from the wall of the recess towards the second surface. In this embodiment, the etching results in the recess extending in a cylindrical manner or at the same angle in the plane of the second surface.
[0030] The reactors have a depth of, for example, at least 40 μm, at least 50 μm, or at least 100 μm, or at least 150 μm, for example up to 250 μm, or up to 200 μm. The reactors have a diameter of, for example, at least 10 μm, or at least 30 μm, for example up to 200 μm, or up to 1 mm, generally preferably with an aspect ratio of depth to diameter of at least 2, at least 4, at least 5, or at least 6. The recess in the first glass plate has a volume of, for example, 1 pL to 1 μL inside the first glass plate.
[0031] The connection of the second sheet, in particular the second glass sheet, with the first glass sheet, preferably the second surface of the first glass sheet, can be carried out by directly overlapping the first and second sheets and then heating, for example, in the case of quartz glass, from 400°C to 1200°C. In this case, the connection can be carried out at a lower temperature with a longer duration of the connection process or at a higher temperature with a shorter duration, the temperature depending on the maximum temperature at which the first and second glass sheets are still sufficiently dimensionally stable. Alternatively, a frit glass, i.e. a paste containing glass particles, having a lower melting point than the first and second glass sheets is placed between the first and second glass sheets, and the glass sheets are connected by heating to a temperature at which the frit glass softens or melts. In this case, frit glass is applied, preferably to the second surface of the first glass plate or to the first surface of the second glass plate, for example by silk screening or 3D printing, after which the second glass plate is placed in contact with the first glass plate and heated.
[0032] Optionally, the frit glass is colored with a component of glass particles that have a smaller transmittance than the second glass plate when used for irradiating light, for example in the wavelength region of light. For example, the frit glass, and in particular the glass particles contained in the frit glass, may include metal oxides such as iron oxide, magnetite, titanium dioxide, mixed oxides such as cobalt aluminate, spinels such as iron chromium spinel, or a mixture of at least two of these. A reactor formed by a second glass plate molded in a first glass plate and connected at its bottom directly to the first glass plate through the colored frit glass has the advantage that during irradiation and detection of light for analysis, the interaction of radiation passing through the area of the first glass plate and the second glass plate in addition to the reactor is reduced.
[0033] If the first glass sheet is etched after being coated on the second surface with an etching resist after the laser irradiation, a recess with a conical cross section is generally formed. For the embodiment in which the recess is formed through, typically when the recess through the first glass sheet is formed with the desired diameter, the etching process is interrupted. Depending on the choice of the material of the etching resist, peeling of the etching resist and so-called undercutting may occur. The area of the second surface around the recess is likewise corroded by the etching medium, whereby the etching process continues along the contact surface between the glass sheet and the etching resist, and the etching resist is further peeled off. That is, around the recess, the thickness of the first glass sheet is reduced and a circumferential bevel, also called a transition curve, undercut or back taper, is formed on the second surface adjacent to the recess. During the subsequent connection process, this may result in the formation of a gap between the first glass sheet and the second sheet. This gap may be closed by applying a paste containing frit glass and then melting the frit glass. In such cases, therefore, the connection of the glass sheets with frit glass is particularly advantageous. Such an oblique surface is arranged facing the second surface of the first glass sheet, and can be filled with frit glass if the frit glass is arranged over the entire surface of the second glass sheet to be connected with the first glass sheet. In the case of an oblique surface extending from the recess towards the second surface of the first glass sheet, the frit glass can also be applied evenly to this second surface, for example, in particular by means of a silk screen, and the second glass sheet can be arranged facing the second surface. In such an embodiment, the oblique surface is capable of receiving the frit glass, and the bottom of the reactor covering the inside cross section of the recess is formed only by the second sheet. The bottom of the recess is therefore free from the frit glass paste, the bottom being subsequently formed by the surface of the second sheet. Alternatively, the frit glass can cover the bottom as well. This can be advantageous. This is because, during the joining process, the frit glass melts and is placed on the second plate, and has a surface tension that can result in the formation of a glass lens that forms the bottom of each reactor, respectively.This effect can be advantageous in illuminating the reactor.
[0034] Alternatively, the second glass sheet can be connected to the second surface of the first glass sheet by anodic bonding, where the second surface of the first glass sheet and / or the surface of the second glass sheet facing the first glass sheet is coated with silicon, for example by means of cathodic sputtering, also called sputtering, and the first glass sheet is placed in contact with the second sheet, a voltage of for example 300V to 500V is applied, and optionally heated, for example, to 400°C. Both glass sheets are thereby connected to each other by means of the diffusion of ions (for example Na, K) and oxygen anions contained in the glass.
[0035] Alternatively, the glass sheets may be joined without an intermediate layer by fusion, preferably by contact, heat and pressure between one of the surfaces of a first glass sheet and one of the surfaces of a second glass sheet.
[0036] The same connecting method or combination of methods may be used to connect further glass sheets to the first and / or second glass sheets.
[0037] Typically, the heating may be carried out in a furnace.
[0038] More generally, the second glass plate may be made of a glass that is more reactive to chemical surface modification than the glass of the first glass plate. For example, the second glass plate may be made of calcium oxide-natron glass and the first glass plate may be made of borosilicate glass, so that aqueous or organic reagents filled in the reactor adhere to the glass of the second glass plate, which in particular forms the bottom of the reactor. Additionally or alternatively, the second glass plate may be made of a different glass composition than the first glass plate, for example, the second glass plate may be made of quartz glass or fused quartz and the first glass plate may be made of borosilicate glass.
[0039] Optionally, conductor paths may be applied to the surface of the second sheet to be connected to the first glass sheet, the conductor paths being, for example, arranged separately next to each other and connected by separate connection surfaces and thus separately accessible to each other.Preferably, for the connection of the glass sheets, a frit glass paste is applied to the surface of the first glass sheet by means of a silk screen, and the second glass sheet is placed on the surface to which the frit glass has been applied and subsequently heated.
[0040] In the embodiment in which the first glass sheet is connected to the second glass sheet by means of a layer of molten frit glass located between them, optionally a first conductor path may be applied on the first glass sheet and a second conductor path may be applied on the surface of the second glass sheet facing the first glass sheet. The first conductor path preferably covers at least a part of the recess formed in the first glass sheet, and optionally the first conductor path covers the entire surface of the first surface and at least a part of the recess. The second conductor path extends along the area forming the bottom of the reactor and is preferably connected to a contact surface of the second glass sheet arranged on the part of the second glass sheet that protrudes from the first glass sheet. The first and second conductor paths can be applied by sputtering or printing, the first conductor paths for example after etching and the second conductor paths before the connection of the second glass sheet with the first glass sheet. The insulation between the first and the second conductor paths is formed by a layer of molten frit glass, which is arranged between the first and the second glass sheets, in particular only in the area where the first and the second glass sheets meet each other or except in the area where the recess is formed in the first glass sheet. Optionally, the second glass sheet may be formed with a recess, in which the second conductor path is arranged. Such a recess may extend along the surface of the second glass sheet facing the first glass sheet. Such a recess may be formed in the second glass sheet, for example by etching, for example after irradiating the second glass sheet along the path of such a recess, for example by using a pulsed laser beam which is simultaneously irradiated before etching. Alternatively, the recess can be formed by photolithographic formation of an etching mask followed by etching and removal of the etching mask after etching. Such depressions can be formed, for example, as grooves with a V-shaped or U-shaped cross section. The material for the conductor tracks can be introduced, for example, into the depressions, for example by means of a printing method. Preferably, the conductor tracks consist of a metal, such as gold, silver, copper, or a mixture of at least two of these.
[0041] The recess formed in the first glass sheet can have a larger cross-section in the upper thickness than in the lower thickness divided into at least two partial recesses adjacent to the upper thickness, the lower thickness being adjacent to the second sheet and connected, for example, directly to the second sheet or by means of a layer of molten and solidified frit glass. In this embodiment, the end cross-sectional openings of the at least two partial recesses adjacent to the second sheet are covered by the second sheet. The recess extending over the upper thickness covers at least two partial recesses. Between the partial recesses extending over the lower thickness, partial walls are arranged which are integrally formed from the first glass sheet to the lower thickness. The partial walls are spaced apart from each other around the partial recesses. The partial walls are formed by irradiation of a laser pulse which penetrates only at most the upper thickness of the first glass sheet in the region of the partial wall, irradiation of a laser pulse in the region of the partial recess which passes completely through the first glass sheet, and subsequent etching of the first glass sheet. During etching, a recess is formed in the upper thickness region adjacent to the first surface of the first glass sheet, which recess extends over the region of at least two partial recesses. The longitudinal central axes of the partial recesses may be arranged, for example, at intervals of 10 μm to 100 μm. The partial walls extend over the lower thickness portion between the partial recesses, which may have a diameter of, for example, 1 to 50 in the plane of the second surface of the first glass sheet adjacent to the second sheet. The upper thickness portion is also called here the first thickness portion and the lower thickness portion is also called the second thickness portion. The upper thickness portion and the lower thickness portion extend, starting from the first surface of the first glass sheet, independently of each other, for example, at least 20% or at least 30% or at least 40% or at least 50%, for example up to 80% or up to 70% or up to 60%, of the thickness of the original first glass sheet. In this case, the lower thickness portion extends into the thickness of the first glass sheet to a greater extent than the upper thickness portion, but generally these thickness portions do not extend through the entire thickness of the first glass sheet.For example, the first thickness and in particular the second thickness may be predetermined such that after etching in the area of the recess, at least 5%, at least 10% or at least 15% or at least 20% of the thickness of the first glass sheet remains between the recess and the second surface.
[0042] A third plate may be arranged on the first surface of the first glass plate facing the second plate and connected to the first glass plate. The third plate has a third recess, which extends over the entire thickness of the third plate and is appropriately, particularly aligned, arranged over the recess of the first glass plate. In this case, the third recess may have a diameter equal to or larger than the diameter of the recess of the first glass plate. Optionally, the third recess may each extend over two or more recesses of the first glass plate. The third recess is suitable for use, for example, as a hopper for filling the recesses of the first glass plate. The third recess may have a volume, for example, in the third plate, of 0.01 μL to 10 μL, for example, 0.1 μL to 3 μL.
[0043] In general, the recesses of the first glass sheet may be spaced apart from each other by 20 μm to 200 μm from their longitudinal central axis, particularly when the third sheet is placed on the first glass sheet. In general, when forming, laser pulses penetrating the first glass sheet are irradiated at intervals from the longitudinal central axis of the recesses or partial recesses. The recesses of the first glass sheet may have a diameter of, for example, 5 μm to 200 μm in the plane of the second surface of the first glass sheet.
[0044] The third plate may be, for example, a glass plate having a thickness of at least 100 μm or at least 300 μm, for example up to 2000 μm or up to 1000 μm. The third recess may have an inner diameter of, for example, at least 0.2 mm or at least 0.5 mm, for example up to 3 mm or up to 2 mm or up to 1 mm. The third plate may be connected to the first glass plate by anodic bonding, by a layer of melted and solidified frit glass between the first and third plates, for example applied by silk screen, or by fusion bonding.
[0045] Optionally, the second sheet, especially in the embodiment of the second glass sheet, can have a second recess in the area where it covers the recess formed in the first glass sheet, the second recess having a smaller diameter than the recess of the first glass sheet. The second recess can be a blind hole opened to the first glass sheet or can extend over the entire thickness of the second sheet, thereby forming a holding device for larger particles. The second recess can be formed in the second sheet by the method described for the formation of recesses in the first glass sheet. The second recess can be configured as a cone, preferably with its smaller diameter lying in the plane of the surface of the second sheet facing the first glass sheet and connected with the first glass sheet. The second recess can have a diameter of, for example, 1 μm to 50 μm in the plane of the surface of the second sheet facing the first glass sheet. Preferably, the recesses of the second plate have a diameter 5 to 10 times smaller than the diameter of the cells contained in the reactor. For example, for a cell diameter of 7 to 15 μm, the recesses have a diameter of 1 to 3 μm, in particular 1 μm or 1.5 to 2 μm. For example, the longitudinal central axes of the second recesses may be spaced apart by 10 to 100 μm. The second plate, which is preferably a second glass plate, preferably has a thickness in the range of 50 to 500 μm, for example up to 150 μm or up to 100 μm.
[0046] In this embodiment, the bottom of the recess in the second glass plate can have a microstructure provided for near-field illumination of the volume of the recess. Such a microstructure can have the shape of, for example, a thin and tall glass tip and can act as an optical waveguide for illumination or can influence each cell or a group of cells at its location or position. Such a structure can be formed, for example, by forming the recess through etching of a number of locations where the laser pulses are closely irradiated. If each laser pulse is emitted in the center of the recess, after the etching process the glass tip remains in the recess. In general, in this method, the recess can be formed by irradiation of a laser pulse at adjacent locations and subsequent etching, the locations being spaced apart by the same distance from each other, for example 1 μm to 5 μm or even 3 μm, forming together a location, where at least two or at least three locations are spaced apart by a larger distance, for example 10 μm to 30 μm, for example 15 μm to 20 μm. At least two or three locations of laser pulses spaced relatively far apart have areas between them, e.g., where laser pulses are emitted at equal intervals, or surround an area where the glass tip remains upon etching.
[0047] In an embodiment for forming a reactor having a recess in the second glass plate, the etching of the second glass plate is carried out for a length of time sufficient to obtain the desired depth of the recess in the glass volume of the second glass plate spaced apart from the second surface, or only for a length of time in which the second glass plate can still have the second surface closed. Optionally, the bottom of the reactor can have a concave recess with a parabolic or conical cross section. Such a concave recess can be formed at each point where the laser beam is irradiated in a point-like manner. Preferably, such a concave recess has a cross-sectional opening and a depth of several micrometers, for example 1 μm to 5 μm.
[0048] The embodiment in which the second plate has a second recess is particularly suitable for using the recess of the first plate as a culture vessel for cells, in particular human or animal cells. In the method for culturing cells in the recess, liquids such as culture medium and / or reagents to be tested can be moved through the second recess and can be introduced into or removed from the recess of the first glass plate. For example, a cell suspension in a medium can be filled into the recess of the first glass plate from the opposite direction of the second plate or into the open cross-sectional opening of the recess, and the medium flows out through the second recess. The cell culture in the medium can be whole blood or cells cultured in a buffer or culture medium. The embodiment is suitable for use as a filter, for example for a cell suspension in a medium. In the method, a medium, for example a culture medium or a buffer, can come into contact with or flow along the free surface of the second plate, whereby an exchange of the medium occurs through the second recess and for example metabolic products moving through the second recess are removed.
[0049] The invention further relates to an analytical method in which a reactor within glass is irradiated with light and light emitted from the reactor is detected, and to the use of a glass reactor in said analytical method.
[0050] In this case, light for analysis can be irradiated, preferably approximately perpendicularly, onto the surface of the second glass plate opposite the first glass plate, or onto the surface of the second glass plate facing the first glass plate.
[0051] It has been found that recesses, in particular recesses extending conically from the first surface of the first glass sheet into the volume, form a clear contrast with the bottom of the recess at their walls when irradiated with, for example, visible light, and thus upon light detection the periphery of the recess is recorded and can be visualized as a particularly dark ring in contrast with the bottom of the recess.
[0052] The invention further relates to an analytical method comprising the steps of providing a reactor produced according to the production method according to the invention or which is a reactor according to the invention, before, simultaneously or after placing in the reactor a sample, such as a patient sample, which may for example be an acellular sample such as plasma or a cellular sample such as whole blood or cells separated from whole blood or a tissue material, adding at least one reagent to the reactor and analyzing.
[0053] Optionally, at least one reagent may be added to the multiple reactors in different amounts, either once or multiple times in succession. The reagent may be, for example, a pharmaceutical agent, and the analysis may include measuring the effect of the agent on the sample. Optionally, the method may include, for example, assaying the sample under cell culture conditions (37° C., 5% CO 2 The method may include one or more incubation steps in an ambient, static or dynamic environment.
[0054] The analysis may be, for example, an optical measurement of the reactor during or after sequencing of DNA and / or RNA and / or proteins in the reactor, optionally after lysis of the cells, after addition of a reagent for sequencing, or a determination of proteins, for example after reaction with a binding molecule, such as an antibody, preferably marked with a dye, added as a reagent. Preferably, the analysis, for example in the case of a cell-containing sample, comprises the determination of the transcribed RNA and / or translated proteins, in particular for a sample to which an agent has not been added, compared to a sample to which an agent has been added. Optionally, the analysis method may comprise the removal of a portion of the sample from the reactor, and may further optionally comprise the injection of the removed portion of the sample into a further reactor according to the invention or a reactor manufactured according to the invention. The addition of the sample and / or the reagents to the reactor may be performed, for example, by the movement of droplets of the sample and / or by the movement of droplets of the reagents, the droplets being formed and moving, for example, as part of a fluid jet. This is done, for example, by the action of electromagnetic radiation, by sonic or ultrasonic irradiation, by application of an electric field or by pressure. The formation of droplets is known as inkjet printing or pipetting. Alternatively, it is also possible to use laser-based printing methods, such as laser transfer printing. Preferably, the addition of sample and / or reagents is done without contact between the metering device and the reactor.
[0055] In an embodiment in which the conductive paths are disposed in the recess, a method for analyzing the volume of the recess may involve applying a voltage between the conductive paths and measuring an electrical parameter present in the volume. [Brief description of the drawings]
[0056] [Figure 1] FIG. 1 shows a schematic representation of an embodiment of a glass reactor consisting of two glass plates in a cross section perpendicular to the surface of the first glass plate. [Diagram 2] FIG. 2 shows a schematic representation of an optical analysis of a reactor manufactured according to the present invention in a top view of a first surface of a first glass plate. [Figure 3a] FIG. 2 shows a schematic representation of a further embodiment in a cross section perpendicular to the surface of the first glass sheet. [Figure 3b] FIG. 2 shows a schematic representation of a further embodiment in a cross section perpendicular to the surface of the first glass sheet. [Figure 4a] FIG. 2 shows a schematic representation of an embodiment in a cross section perpendicular to the surface of the second glass plate. [Figure 4b] FIG. 2 shows a schematic representation of an embodiment in a cross section perpendicular to the surface of the second glass plate. [Figure 4c] FIG. 2 shows a schematic representation of an embodiment in a cross section perpendicular to the surface of the second glass plate. [Figure 5a] FIG. 2 shows a schematic representation of an embodiment with conductor paths in a cross section perpendicular to the surface of the first glass sheet. [Figure 5b] FIG. 2 shows a schematic representation of an embodiment with conductor paths in a cross section perpendicular to the surface of the first glass sheet. [Figure 6a] FIG. 2 shows a schematic representation of a further multi-part embodiment in a cross section perpendicular to the surface of the first glass sheet. [Figure 6b] FIG. 2 shows a schematic representation of a further multi-part embodiment in a cross section perpendicular to the surface of the first glass sheet. [Figure 6c] FIG. 2 shows a schematic representation of a further multi-part embodiment in a cross section perpendicular to the surface of the first glass sheet. [Figure 7] FIG. 2 shows a schematic representation of a further embodiment in a cross section perpendicular to the surface of the first glass sheet. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0057] FIG. 1 shows a first glass sheet 1 in which a recess 2 extends throughout its thickness, the bottom 3 being formed by a second glass sheet 6 intimately connected to a second surface 5 of the first glass sheet 1.
[0058] 2 shows the recess 2 in a top view of the first glass plate 1, the walls of which form a strong optical contrast with the base 3, so that the walls are clearly illustrated as the circumferential boundary of the base 3. Particles, for example biological cells Z, can be seen with good contrast with the base 3 when illumination is directed through the base 3, especially if the cells Z are marked by a dye, for example a fluorescent dye.
[0059] FIG. 3a) shows a first glass plate 1, the whole of whose second surface 5 is coated with an etching resist 8, for example a plastic film, by irradiation with a laser pulse perpendicular to the glass plate 1 using a UV-degradable adhesive, followed by etching. The etching forms a recess 2 symmetrically around the optical path of the laser pulse, so that the central longitudinal axis 7 is located along the original optical path of the laser pulse. The etching forms a truncated cone-shaped recess 2 starting from the first surface 4 and extending to the etching resist 8. A chamfer or undercut 9 surrounding the recess 2 is then formed along the second surface or between the second surface 5 and the etching resist 8.
[0060] Figure 3b) shows a glass reservoir formed in the first glass sheet 1 as a recess 2 and extending over the entire thickness of the first glass sheet 1. The bottom 3 of the recess is formed by a frit glass 10 which is applied over the entire surface of the second sheet 6 and which also fills the area of the chamfer 9.
[0061] 4 shows an embodiment of recesses 2 each formed integrally with the second glass sheet 6. It shows the irradiation of a first surface 24 of the second glass sheet with laser pulses at a number of locations, for example with a spacing of 1 μm to 10 μm, thus forming the exact location where the recesses 2 are to be formed by etching. In this way, a respective concave depression 12 may be formed at each location 12 of the bottom 3 of the recess 2 by etching.
[0062] As shown in Fig. 4a), a glass tip 11 protruding from the base 3 into the recess 2 perpendicular to the first surface 24 is formed during etching if at least three locations 12 at which the laser pulse is applied are arranged at relatively large intervals, for example at intervals of 20 μm, such that each location 12 at which the laser pulse is applied produces a concave indentation in the base 3 during etching.
[0063] FIG. 4b) shows that the laser pulses applied at each location 13 penetrating deeper into the thickness of the second glass sheet 6 will form additional recesses 14 during etching, which will extend deeper into the second glass sheet 6 than the indentations at other locations 12 where the laser pulses were applied to a smaller depth into the second glass sheet 6. The depth to which the laser pulses penetrate into the second glass sheet 6 may be predetermined by the setting of the focus position and / or the intensity of the pulse energy of the laser pulses.
[0064] FIG. 4c) shows that irradiation at an adjacently arranged position 13 with a laser pulse that penetrates deeper into the second glass sheet 6 forms a further recess 14 during etching at said position, the bottom 3 of which extends deeper into the thickness of the second glass sheet 6 than the recess formed by the other position 12 where the laser pulse is irradiated to a smaller depth into the second glass sheet 6.
[0065] 5a) and 5b) show an embodiment in which a first glass sheet, here on its first surface 4, is coated with first conductor paths 15, and a second sheet 6 has second conductor paths 16 placed on its flat surface facing the first glass sheet 1. The first and second conductor paths 15, 16 can be applied, for example, by sputtering, pressing or by chemical or electrical isolation, or a combination of these. One of the first and second conductor paths 15, 16 can be applied over the entire surface, while the respective other conductor path 15, 16 can be configured in the form of spaced paths that cross the cross section of the recess 2. A layer of frit glass 10, which solidifies after softening, arranged between the first glass sheet 1 and the second sheet 6, connects both sheets 1, 6 and spaces the first conductor paths 15 from the second conductor paths 16, so that they are in spaced contact with the liquid contained in the recess 2. Optionally, the layer consisting entirely of frit glass 10 may be arranged exclusively between the first glass plate 1 and the second plate 6, leaving the area of the recess 2 free, or the layer consisting of frit glass 10 may extend over the layer thickness of the first conductor path 15, into the recess 2, at a distance from or up to the second conductor path 16.
[0066] FIG. 5 a) shows an embodiment in which the second conductor path 16 extends within a groove 17 which is formed as a depression in the second plate 6, preferably by irradiation with a laser pulse along the path of the groove followed by etching.
[0067] FIG. 5 b ) shows an embodiment in which the second conductor paths 16 are arranged on a flat surface of the second plate 6 .
[0068] Figure 6a) shows an arrangement of at least two, in this case 10, recesses 2 whose longitudinal central axes 7 are arranged at the same distance from one another. The recesses 2 are surrounded by a wall extending over the entire thickness of the first glass pane 1. In this case, the recesses 2 are conically shaped from the first surface 4 to the second surface 5 of the first glass pane 1. The cross-sectional opening of the recesses 2 is covered in the plane of the second surface 5 by the second pane 6.
[0069] Figure 6b) shows an embodiment in which a third plate 18 is connected to the first surface 4 of the first glass plate 1, the third plate 18 having a third recess 23 through its thickness and covering at least two, in figure 7b) ten, recesses 2 formed in the first glass plate 1. The spacing of the longitudinal centre axes of the recesses 2 in the first glass plate can be, for example, between 10 μm and 100 μm.
[0070] FIG. 6c) shows an embodiment in which recesses are etched into the first glass sheet 1 after it has been irradiated with a laser pulse penetrating its entire thickness at the locations where the partial recesses 2′ are to be formed, and during this with a laser pulse extending at most over the upper thickness 20. The upper thickness 20 extends from the first surface 4 of the first glass sheet 1 up to the partial recesses 2′, and between the partial recesses 2′ partial walls 22 are left behind at the locations where the laser pulse was irradiated at most to the depth of the upper thickness 20. The cross-sectional opening at the end of the partial recess 2′ facing the first thickness 20 is covered by a second sheet 6 connected to the first sheet 1.
[0071] 7 shows an embodiment in which the second plate 6 has a second recess 19 in the region of the recess 2 formed in the first glass plate 1. The second recess 19 can optionally extend part of the thickness of the second plate 6 or, as shown in this figure, over the entire thickness of the second plate 6. The second recess has a diameter, in the plane of the surface of the second plate 6 connected to the first glass plate 1, which is for example 5 to 10 times smaller than the diameter of the cell Z. The second plate 6, together with the second recess 19 which penetrates its entire thickness, forms a holding device for larger particles such as the cell Z.
[0072] Corresponding to a preferred embodiment, in FIG. 7 the second recess 19 is conical in shape and has a smaller diameter in the plane of the surface of the second plate 6 facing the first glass plate. [Explanation of symbols]
[0073] 1. First Glass Pane 2 Recess 2' Partial recess 3 bottom 4. First Surface 5. Second Surface 6. Second Board 7 Longitudinal central axis 8 Etching resist 9 Beveled surface, undercut 10. Fritted Glass 11 Glass Tip 12 Position of the irradiated laser pulse 13 Position of the laser pulse at deeper depths 14 Further recesses 15 First Conductor Path 16 Second Conductor Path 17 Groove 18 Third Board 19 Second recess 20 Upper, first thickness 21 Lower, second thickness 22 partial wall 23 Third Recess 24 First surface of second plate 25 Second surface of second plate Z cell
Claims
1. A method for manufacturing a plurality of glass reactors formed as recesses (2) in a first glass sheet (1), comprising the steps of:
1. A step of irradiating a first surface (4) of the first glass sheet (1) with a laser pulse of a wavelength that is transparent to the first glass sheet (1) at the places where the recesses (2) are to be formed as reactors, the laser beam being irradiated in a point-like manner in the plane of the first surface (4) at a distance exactly the diameter of one of the reactors, including the thickness of the wall between the reactors; 2. Etching the first glass sheet (1) for a length of time sufficient to form the recess (2) along a location, in the absence of a coating made of etching resist, until the recess (2) is formed, the depth of which extends over the entire thickness of the first glass sheet (1), and a second sheet (6) made of glass is connected to a second surface (5) of the first glass sheet (1) opposite to the first surface (4), A method in which the connection is made by anodic bonding or simply by placing the first glass sheet (1) facing the second sheet (6) and then heating it.
2. 2. The method according to claim 1, characterized in that the depth of the recess (2) is at least 30 μm.
3. 3. The method according to claim 1 or 2, characterized in that the recess (2) has a depth to diameter aspect ratio, measured in the plane of the first surface (4), of at least 2.
4. 4. The method according to claim 1, characterized in that during the connection by anodic bonding, the surface of the second glass sheet (6) facing the first glass sheet (1) and / or the second surface (5) of the first glass sheet (1) is coated with silicon.
5. 5. The method according to claim 1, characterized in that a laser beam is applied to the first glass sheet (1) at a plurality of spaced apart positions at the locations where the recesses (2) are to be formed.
6. 6. The method according to claim 5, characterized in that at the location (12) a laser pulse is applied to a smaller depth into a first thickness (20) in the first glass sheet (1) and at the location (13) a laser pulse is applied to a greater depth into an adjacent second thickness (21) in the first glass sheet (1), such that during etching a recess (2) extending over the first thickness is formed and partial recesses (2') extending over the second thickness (21) and spaced apart by partial walls (22) are formed.
7. 7. A method according to claim 5 or 6, characterized in that the locations are spaced at most 10 μm apart, with at least three of the locations being at least 20 μm apart from each other.
8. 8. The method according to claim 1, characterized in that a focus position of a laser beam and / or a laser pulse is set in such a way that the laser beam and / or the laser pulse enters the first glass sheet (1) only in a thickness portion that does not extend over the entire thickness of the first glass sheet (1).
9. 9. The method according to claim 1, characterized in that a laser beam is applied in a circumferentially closed path at the location of the first glass sheet (1) where the recess (2) is to be formed.
10. 10. The method according to claim 9, characterized in that the laser beam applied in a circumferentially closed path is formed by laser beam pulses applied side by side.
11. 11. The method according to any one of claims 1 to 10, characterized in that a second recess (19) is formed in the second sheet (6) and that the second sheet (6) is connected to the first glass sheet (1) at the second recess (19) of the second sheet adjacent to the recess (2) of the first glass sheet (1).
12. A reactor formed as a glass recess, said reactor having a depth of said recess in a first glass sheet (1) of at least 30 μm and an aspect ratio of depth to diameter, measured in the plane of a first surface (4) of said first glass sheet (1), of at least 2, said recess (2) being surrounded by a wall, the end faces of said wall being arranged in a common plane and forming said first surface (4) of said first glass sheet (1), from which said recess (2) is excluded, the recess (2) extends over the entire thickness of the first glass plate (1), a second plate (6) forming the bottom (3) of the reactor is connected to the surfaces (4, 5) of the first glass plate (1) without an intermediate layer, A reactor, characterized in that the conductor paths are arranged inside grooves made in the surface of the second plate (6) connected to the first glass plate (1).
13. 13. A method for analyzing a sample, comprising the steps of manufacturing a reactor according to the method of any one of claims 1 to 11 or providing a reactor as described in claim 12, placing an acellular or cell-containing sample in the reactor, adding at least one reagent to the reactor, and performing an optical measurement of the reactor.
Citation Information
Patent Citations
Ultraviolet transmitting glass composition and glass article making use of the same
EP1867612A1
Method of producing cell culture container
EP2011857A1
Method for manufacturing glass array plate with closures
JP2002506789A
Drilling method for material transparent to laser
JP2004351494A
Manufacturing method of microarray manufacturing head, the microarray manufacturing head and microarray manufacturing apparatus
JP2005351774A