Battery
The battery design addresses the issue of reduced energy density by suppressing electrolyte rise and eliminating caulking, thereby improving energy density through effective sealing without welding defects.
Patent Information
- Application Number
- JP2020186691
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-11-09
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2040-11-09
AI Technical Summary
Conventional battery sealing methods increase the longitudinal dimension near the sealing member, reducing the energy density due to the formation of a protuberance and caulking portion, which leads to electrolyte mixing during welding, causing defects.
A battery design that suppresses electrolyte rise by providing grooves or surface treatments on the sealing member to prevent electrolyte from entering the molten zone during welding, eliminating the need for a caulking portion and reducing the distance between the electrode body and the sealing member.
This design improves energy density by preventing welding defects and reducing the battery can volume, enhancing the energy-to-volume ratio.
Smart Images

Figure 0007561371000001 
Figure 0007561371000002 
Figure 0007561371000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to batteries. [Background technology]
[0002] 2. Description of the Related Art Sealed batteries of various configurations have been conventionally known (see, for example, Patent Document 1).
[0003] Such a conventional battery has a battery can with an open end, and the open end of the battery can is sealed. The following method is known as a method for sealing the open end. After the electrode body is housed in the battery can, the battery can is narrowed inward near the open end of the battery can. This narrowing forms an annular protuberance on the inner peripheral surface of the battery can, and a gasket and a sealing member are placed on the protuberance. The open end of the battery can is crimped to the sealing member via the gasket, forming a crimped portion on the sealing member. Thus, the battery is sealed and a sealed battery can be manufactured. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 7-105933 Summary of the Invention [Problem to be solved by the invention]
[0005] In such conventional batteries, the longitudinal dimension of the battery in the vicinity of the sealing material increases because a protrusion is formed under the sealing material and a crimped portion is formed on the sealing material, which increases the volume of the battery can and reduces the energy density of the battery.
[0006] Therefore, an object of the present disclosure is to provide a battery capable of realizing an improvement in energy density by solving the above-mentioned problems of the conventional art. [Means for solving the problem]
[0007] A battery according to one aspect of the present disclosure includes a metal battery can, an electrode body, an electrolyte, and a sealing member. The battery can has a cylindrical portion having an opening edge at one end, and a bottom portion that closes the other end of the cylindrical portion. The electrode body is accommodated in the battery can. The battery can is filled with an electrolyte. The sealing member seals the opening edge portion of the cylindrical portion of the battery can. The sealing member is disposed so that the outer peripheral surface of the sealing member faces the inner peripheral surface of the opening edge portion. A part of the inner peripheral surface of the opening edge portion and a part of the outer peripheral surface of the sealing member are joined by a fusion portion. In addition, a suppression portion is provided on the outer peripheral surface of the sealing member closer to the bottom than the fusion portion, suppressing the electrolyte from rising between the inner peripheral surface of the opening edge portion and the outer peripheral surface of the sealing member toward a position where the fusion portion is formed. Effect of the Invention
[0008] According to the present disclosure, it is possible to achieve an improvement in the energy density of a battery. [Brief description of the drawings]
[0009] [Figure 1A] Schematic diagram of a battery according to embodiment 1 of the present disclosure. [Figure 1B] 1 is a cross-sectional view of a battery according to a first embodiment. [Figure 2A] 1 is a schematic cross-sectional view of a battery according to a first embodiment, in the vicinity of a groove portion; [Figure 2B] Schematic diagram of a sealing member in a battery according to embodiment 1. [Figure 2C] Schematic cross-sectional view of the vicinity of the two grooves in the battery according to embodiment 1. [Figure 2D] Schematic cross-sectional view of the vicinity of both side grooves in the battery according to embodiment 1. [Figure 2E] FIG. 1 is a schematic diagram of a sealing member having an angled groove in a battery according to embodiment 1. [Figure 2F] Cross-section of Figure 2E [Figure 3A] Schematic cross-sectional view of a battery according to a second embodiment of the present disclosure in the vicinity of a surface-treated portion. [Figure 3B] Schematic diagram of a sealing member in a battery according to embodiment 2. [Figure 3C]Schematic cross-sectional view of the vicinity of surface-treated portions on both sides of a battery according to embodiment 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] (Background to this disclosure) In the conventional battery sealing method of Patent Document 1, a crimped portion is formed, which results in an increase in the longitudinal dimension of the battery in the vicinity of the sealing material, and a decrease in the energy density of the battery. Therefore, in order to solve the conventional problems, the present inventors have investigated a sealed battery in which the battery can can be sealed without forming a crimped portion by joining the battery can and the sealing material by, for example, welding.
[0011] However, when the battery can is sealed by welding, when a sealing member is inserted into the edge of the opening of the battery can, the electrolyte rises between the battery can and the sealing member toward the opening side of the battery can due to capillary action, and the electrolyte gets mixed into the molten part formed by welding, which causes welding defects.
[0012] The rise of the electrolyte will be described in detail. In this specification, "up" refers to the direction from the bottom of the battery can toward the molten part in the battery after the battery can is filled with the electrolyte. Also, the "rise of the electrolyte" occurs upward. The rise of the electrolyte occurs due to capillary action in the space between the inner circumferential surface of the opening edge and the outer circumferential surface of the sealing member. In the capillary action, the electrolyte in the space between the inner circumferential surface of the opening edge and the outer circumferential surface of the sealing member is subjected to surface tension and gravity according to the volume of the electrolyte in the space. The electrolyte rises to a position where the surface tension and gravity are balanced.
[0013] Next, the mixing of the electrolyte into the molten part will be described in detail. After inserting a sealing member into the battery can, a part of the battery can and a part of the sealing member are melted to form a molten part. When the electrolyte that has risen by capillary action reaches the height at which the molten part is formed, it enters the molten part that has been melted during welding, and the electrolyte is mixed into the molten part. Such mixing of the electrolyte causes, for example, poor welding such as opening defects. Therefore, the present inventors have studied the following battery as a battery that can solve the above problem.
[0014] A battery according to one aspect of the present disclosure includes a metal battery can, an electrode body, an electrolyte, and a sealing member. The battery can has a cylindrical portion having an opening edge at one end, and a bottom portion that closes the other end of the cylindrical portion. The electrode body is accommodated in the battery can. The battery can is filled with an electrolyte. The sealing member seals the opening edge portion of the cylindrical portion of the battery can. The sealing member is disposed so that the outer peripheral surface of the sealing member faces the inner peripheral surface of the opening edge portion. A part of the inner peripheral surface of the opening edge portion and a part of the outer peripheral surface of the sealing member are joined by a fusion portion. In addition, a suppression portion is provided on the outer peripheral surface of the sealing member closer to the bottom than the fusion portion, suppressing the electrolyte from rising between the inner peripheral surface of the opening edge portion and the outer peripheral surface of the sealing member toward a position where the fusion portion is formed.
[0015] According to this configuration, the capillary phenomenon can be suppressed, and the rise of the electrolyte toward the molten part between the inner circumferential surface of the opening edge part and the outer circumferential surface of the sealing member can be suppressed. By suppressing the rise of the electrolyte, the intrusion of the electrolyte into the molten part can be suppressed. Therefore, the reduction of welding defects due to the intrusion of the electrolyte into the molten part can be realized. If the electrolyte is in the molten part, the electrolyte expands in volume suddenly due to heating of the molten part, and the shape of the molten part is distorted and the electrolyte solidifies, resulting in a welding defect. By reducing the welding defect, the battery can can be sealed by welding and the sealing member can be fixed to the battery can. Since it is not necessary to provide an annular protuberance (also called a reduced diameter part) on the inner circumferential surface of the battery can and a crimping part at the open end of the battery can as in the conventional battery, the distance between the electrode body and the sealing member can be reduced. This allows the volume of the battery can to be reduced, and the energy density of the battery, which is the ratio of the battery energy to the volume of the battery can, is improved.
[0016] Furthermore, as the suppression portion, a groove portion may be provided over the entire outer circumferential surface of the sealing member.
[0017] According to this configuration, the width of the space between the inner peripheral surface of the opening edge portion and the outer peripheral surface of the sealing member is increased in the groove portion. The larger the width of the space, the greater the gravity acting on the electrolyte per unit height, and therefore the rise of the electrolyte due to capillary action is suppressed. This makes it possible to suppress the electrolyte from mixing into the molten portion. Furthermore, since the groove portion is provided around the entire outer peripheral surface of the sealing member, the rise of the electrolyte can be suppressed over a wider range around the outer periphery of the sealing member than with groove portions that are discontinuously formed.
[0018] The direction in which the groove extends may form an angle greater than 0° and smaller than 90° with respect to the circumferential direction of the outer circumferential surface of the sealing member. By providing an angle, the effect of making it easier for the electrolyte to fall in the direction of gravity is obtained.
[0019] The groove may be formed so that the volume of the groove is larger than the expected amount of electrolyte attached to the inner circumferential surface of the opening edge portion.
[0020] According to this configuration, even if the electrolyte rises due to capillary action, the groove does not fill up, and the electrolyte does not rise higher than the groove. Since the groove is located closer to the bottom of the battery can than the molten part, it is possible to prevent the electrolyte from mixing with the molten part.
[0021] Furthermore, as the suppression portion, a surface-treated portion having a water-repellent effect or an oil-repellent effect against the electrolyte may be provided over the entire outer periphery of the sealing member.
[0022] According to this configuration, the wettability of the electrolyte to the sealing member at the surface-treated portion is reduced. The reduced wettability of the electrolyte to the sealing member reduces the surface tension of the electrolyte and the gravity required to balance the surface tension, making it possible to suppress the rise of the electrolyte due to capillary action. This makes it possible to suppress the electrolyte from mixing into the molten portion. Furthermore, since the surface-treated portion is provided around the entire outer periphery of the sealing member, the rise of the electrolyte can be suppressed over a wider area around the outer periphery of the sealing member than with a surface-treated portion that is discontinuously formed.
[0023] In addition, the sealing member may be provided with a surface treatment portion such that the wetting angle of the electrolyte is 90° or more.
[0024] According to this configuration, the electrolyte does not rise above the surface-treated portion. Since the surface-treated portion is located closer to the bottom of the battery can than the molten portion, it is possible to prevent the electrolyte from mixing with the molten portion.
[0025] Furthermore, two suppression parts, a first suppression part and a second suppression part, may be provided. The first suppression part may be provided on the outer circumferential surface of the plugging member closer to the bottom than the molten part, and the second suppression part may be provided on the inner circumferential surface of the opening edge part and closer to the bottom than the molten part.
[0026] With this configuration, the electrolyte can be further prevented from rising between the inner circumferential surface of the opening edge portion and the outer circumferential surface of the sealing member.
[0027] Hereinafter, embodiments of the present disclosure will be described with reference to the accompanying drawings. Note that the present disclosure is not limited to the embodiments described below.
[0028] (Embodiment 1) Hereinafter, the first embodiment will be described in detail with reference to the drawings. Fig. 1A shows a schematic diagram of a battery 10 according to the first embodiment. Fig. 1B shows a cross-sectional view of the battery 10 according to the first embodiment.
[0029] As shown in FIG. 1A, a battery 10 according to the first embodiment is composed of a battery can 11, a sealing member 12, an electrolyte 13, an electrode assembly 14, a positive electrode tab 19, and a negative electrode tab 20.
[0030] The battery can 11 has a tube portion 33 having an opening edge portion 17 at one end, and a bottom portion 34 that closes the other end of the tube portion 33. In the first embodiment, the tube portion 33 is, for example, a cylindrical portion, and the battery can 11 is a bottomed metal container having a cylindrical shape with an open upper end in the drawing. The negative electrode tab 20 is connected to the bottom portion 34. The electrode body 14 is accommodated in the battery can 11, and the electrolyte 13 is filled in the battery can 11. The battery can 11 is sealed with a sealing member 12. The space inside the battery can 11 that accommodates the electrode body 14 and the electrolyte 13 is a sealed space. Therefore, the battery 10 according to the first embodiment is a sealed battery.
[0031] The sealing member 12 has a central portion having a disk shape and an outer peripheral portion having a ring shape protruding above the central portion, and the outer peripheral edge of the central portion is fixed to the inner peripheral edge of the outer peripheral portion via a gasket 12a. A positive electrode tab 19 is connected to the central portion of the sealing member 12, and the central portion becomes the positive electrode part of the battery 10. The sealing member 12 has an outer peripheral surface arranged to face the inner peripheral surface of the battery can 11. The sealing member 12 is inserted into the battery can 11 so that the height of the upper end of the sealing member 12 on the drawing and the height of the upper end of the battery can 11 on the drawing are approximately the same. In this inserted state, the part of the battery can 11 facing the outer peripheral surface of the sealing member 12 corresponds to the opening edge portion 17. The inner peripheral surface of the opening edge portion 17 is called the first opposing surface 15, and the outer peripheral surface of the sealing member 12 is called the second opposing surface 16. 1A, a suppression portion is provided on the outer peripheral surface of sealing member 12 to suppress electrolyte 13 from rising between the inner peripheral surface of opening edge portion 17 and the outer peripheral surface of sealing member 12. This will be described later in the explanation of FIG. 2A.
[0032] In the description of this specification, the shape of the battery can 11 is a cylinder, but the shape of the battery can 11 is not limited to this. For example, it may be an elliptical cylinder or a polygonal cylinder. In the description of this specification, the shape of the sealing member 12 is a disk shape with the outer periphery protruding upward from the center, but the shape of the sealing member 12 is not limited to this and may be any shape that can be inserted inside the opening edge 17 of the battery can 11 so that the outer periphery faces the inner periphery of the opening edge 17 and can seal the opening edge 17.
[0033] The electrode body 14 releases or absorbs electrons or ions into the battery can 11 depending on the material. The electrode body 14 has two types of electrodes, a positive electrode and a negative electrode, and has a three-layer structure with a separator sandwiched between them to block the movement of electrons or ions. The electrolyte 13 is a medium through which the electrons or ions released from the electrode body 14 can move. In addition, a positive electrode tab 19 and a negative electrode tab 20 through which electrons or ions flow are connected to the positive electrode and negative electrode of the electrode body 14, respectively.
[0034] The battery 10 according to the first embodiment is manufactured through the following steps. An electrode body 14 is inserted into a battery can 11, and an electrolyte 13 is injected. The electrolyte 13 is once poured into the battery can 11 up to the height of the molten part 26 shown in FIG. 1B during injection. After injection, the liquid level is lowered to below the molten part 26 by an impregnation process. Through this series of steps, the electrolyte 13 adheres once to the entire opening edge part 17 of the battery can 11. When the sealing member 12 is inserted into the battery can 11, the electrolyte 13 already adhered to the opening edge part 17 is easily sucked up by capillary action. Next, as shown in FIG. 1B, the sealing member 12 is inserted into the battery can 11 so that the upper end of the inner peripheral surface of the opening edge part 17 in the drawing and the upper end of the outer peripheral surface of the sealing member 12 in the drawing roughly coincide with each other. As a result, the first opposing surface 15 and the second opposing surface 16 face each other. Next, for example, a welding laser 25 is used to irradiate a part of the sealing member 12 and a part of the opening edge 17. Specifically, the upper ends of the sealing member 12 and the opening edge 17, which are roughly aligned in the drawing, are irradiated from above the sealing member 12 and melted. The laser 25 is also scanned along the circumferential direction of the outer periphery of the sealing member 12. This irradiation forms a molten portion 26, and the outer periphery of the sealing member 12 is joined to the inner periphery of the opening edge 17. As a result, the battery can 11 is sealed, and the sealing member 12 is fixed to the battery can 11.
[0035] Fig. 2A shows a schematic cross-sectional view of the vicinity of groove portion 22 in battery 10 according to embodiment 1. Fig. 2B shows a schematic view of sealing member 12 in battery 10 according to embodiment 1.
[0036] 2A, since it is difficult to process the inner peripheral surface of the opening edge 17 and the outer peripheral surface of the sealing member 12 into the same shape, a space 18 is generated between the opening edge 17 and the sealing member 12. Furthermore, the width of the space 18 in the horizontal direction on the drawing (hereinafter, the width of the space 18), i.e., the distance between the first opposing surface 15 and the second opposing surface 16 in the horizontal direction on the drawing, is small compared to the outer diameter of the sealing member 12. In such a space 18, the electrolyte may rise due to the capillary phenomenon as described above.
[0037] As shown in FIG. 2B, in battery 10 of Embodiment 1, groove 22 is provided in the outer peripheral surface of sealing member 12 to suppress the rise of electrolyte 13 in space 18 due to capillary action.
[0038] The groove portion 22 is formed on the outer peripheral surface of the sealing member 12 so as to extend along the circumferential direction of the outer peripheral surface. Moreover, the groove portion 22 is formed as one continuous groove around the entire circumference of the sealing member 12. Since the groove portion 22 extends around the entire circumference of the outer peripheral surface of the sealing member 12, the groove portion 22 exists in a direction perpendicular to the circumferential direction on the outer peripheral surface of the sealing member 12. Moreover, the groove portion 22 is located closer to the bottom 34 of the battery can 11 than the molten portion 26.
[0039] In the first embodiment, groove portion 22 is formed as a suppression portion that suppresses electrolyte 13 from rising between the inner circumferential surface of opening edge portion 17 and the outer circumferential surface of sealing member 12 toward the position where molten portion 26 is formed. Groove portion 22 increases the width of space 18. Furthermore, electrolyte 13 accumulates in groove portion 22. The larger the width of space 18, the greater the gravity per unit height acting on electrolyte 13 accumulated therein, and the greater the suppression of electrolyte 13 rising in space 18.
[0040] In the outer peripheral surface of the sealing member 12, the groove portion 22 may be provided closer to the bottom 34 of the battery can 11 than the fusion portion 26. In addition, in the outer peripheral surface of the sealing member 12, the groove portion 22 may be formed at a position away from the fusion portion 26. For example, in a continuous output fiber laser with a wavelength of 1070 nm, a power of 700 W, a speed of 125 mm / s, and a spot diameter of 0.7 mm, the penetration depth of the fusion portion 26 is about 0.25 mm. By forming the groove portion 22 at a position 0.1 mm or more away from the position of the penetration depth, it is possible to suppress the vaporized electrolyte 13 from mixing with the fusion portion 26. Therefore, by providing a predetermined distance between the groove portion 22 and the fusion portion 26, it is possible to suppress the electrolyte 13 in the groove portion 22 from being vaporized by the heat of welding and being mixed with the fusion portion 26.
[0041] The groove portion 22 may be provided on the inner peripheral surface of the opening edge portion 17, or on both the outer peripheral surface of the opening sealing member 12 and the inner peripheral surface of the opening edge portion 17, in addition to the outer peripheral surface of the opening sealing member 12. The groove portion 22 is not limited to a single continuous groove. For example, multiple continuous grooves may be provided. Also, multiple discontinuous grooves may be provided so that at least one groove exists in a direction perpendicular to the circumferential direction.
[0042] 2C shows a modified example of groove portion 22 of the first embodiment, and is a schematic cross-sectional view of the vicinity of two groove portions 23 of the modified example. This modified example includes two groove portions 23 instead of groove portion 22. Furthermore, two groove portions 23 extend in the circumferential direction of the outer circumferential surface of sealing member 12, spanning the entire circumference. Two groove portions 23 are provided so as to be located closer to bottom portion 34 of battery can 11 than molten portion 26.
[0043] FIG. 2D also shows a modified example of the groove 22 of the first embodiment, and shows a schematic cross-sectional view of the vicinity of the both-side groove 24 of the modified example. This modified example includes both-side grooves 24 formed on both sides of the sealing member 12 side and the opening edge 17 side instead of the groove 22. The both-side grooves 24 extend in the circumferential direction of the outer peripheral surface of the sealing member 12 over the entire circumference, and extend in the circumferential direction of the inner peripheral surface of the opening edge 17 over the entire circumference. The both-side grooves 24 are provided so as to be located closer to the bottom 34 of the battery can 11 than the molten part 26. By providing the both-side grooves 24, the rise of the electrolyte 13 can be further suppressed.
[0044] 2E and 2F show another modified example of groove 22 of embodiment 1, showing a schematic diagram and a cross-sectional view of plugging member 12 having angled groove 27. As shown in Fig. 2E and 2F, the direction in which angled groove 27 extends may have an angle greater than 0° and less than 90° with respect to the circumferential direction of the outer circumferential surface of plugging member 12. For example, Fig. 2E shows angled groove 27 in which the direction in which angled groove 27 extends has an angle of 30° with respect to the circumferential direction of the outer circumferential surface of plugging member 12.
[0045] The electrolyte 13 can be stored in the grooves 22-24 and 27. The grooves 22-24 and 27 may be formed so that the volume that can be stored in the grooves 22-24 and 27 is larger than the amount of electrolyte attached. In this specification, the term "amount of electrolyte attached" refers to the volume of the electrolyte 13 attached to the inner circumferential surface of the opening edge portion 17 when the sealing member 12 is inserted. By forming the volume of the grooves 22-24 and 27 so that it is larger than the amount of electrolyte attached, the electrolyte 13 does not rise higher than the grooves 22-24 and 27. Therefore, the electrolyte 13 can be prevented from mixing with the molten portion 26.
[0046] For example, the dimension of the outer peripheral surface of the sealing member 12 in the direction perpendicular to the circumferential direction is 2.0 mm, and the inner diameter of the battery can 11 is 10 mm. In addition, within the range of the opening edge 17, the electrolyte 13 is uniformly attached to the entire surface with a thickness of 0.05 mm. In this case, the amount of attached electrolyte is about 3.2×10 -9 m 3 For example, when forming groove portion 22 as shown in Fig. 2A, if one groove is formed by cutting so that the cross section is a triangle with a width of 1 mm and a depth of 1 mm, the volume of groove portion 22 will be equal to or greater than the amount of attached electrolyte.
[0047] 2C under the same conditions as above, if two grooves with a width of 1 mm and a depth of 0.5 mm are formed as double groove portion 23, the volume of double groove portion 23 will be equal to or greater than the amount of attached electrolyte. Therefore, double groove portion 23 can be formed with a smaller groove depth than groove portion 22. Similarly, both side groove portions 24 can be formed with a smaller groove depth than groove portion 22 because multiple grooves are formed.
[0048] There are no particular limitations on the method for forming the grooves 22-24 and 27, and the method may be appropriately selected depending on the materials of the sealing member 12 and the battery can 11. Examples of the method for forming the grooves 22-24 and 27 include cutting, pressing, and laser processing.
[0049] (effect) The battery 10 according to the first embodiment has a suppressing portion that suppresses the electrolyte 13 in the space 18 between the inner circumferential surface of the opening edge portion 17 and the outer circumferential surface of the sealing member 12 from rising toward the position where the molten portion 26 is formed. The suppressing portion suppresses the rise of the electrolyte 13 due to the capillary phenomenon, and as a result, the electrolyte 13 can be suppressed from mixing into the molten portion 26 when the battery can 11 and the sealing member 12 are welded together. Therefore, it is possible to reduce welding defects caused by the electrolyte 13 mixing into the molten portion 26. Therefore, the battery can 11 and the sealing member 12 can be joined by welding to seal the battery can 11, and the sealing member 12 can be fixed to the battery can 11. Therefore, it is not necessary to form a crimping portion between the sealing member 12 and the battery can 11 as in the conventional battery, and the distance between the electrode body 14 and the sealing member 12 can be reduced. Therefore, it is possible to provide a battery 10 with improved energy density.
[0050] When the grooves 22-24, 27 are formed on the outer peripheral surface of the sealing member 12 as suppression sections for suppressing the rise of the electrolyte 13, the width of the space 18 between the first opposing surface 15 and the second opposing surface 16 in the grooves 22-24, 27 increases. Furthermore, the electrolyte 13 accumulates in the grooves 22-24, 27. The larger the width of the space 18, the greater the gravity per unit height acting on the electrolyte 13 accumulated therein. Therefore, the height of the electrolyte 13 at which gravity balances with the surface tension decreases, and the rise of the electrolyte 13 is suppressed. Therefore, the electrolyte 13 can be prevented from being mixed into the molten part 26 when the battery can 11 and the sealing member 12 are welded together.
[0051] Furthermore, since grooves 22-24 and 27 are provided along the entire outer periphery of sealing member 12, the rising of electrolyte 13 can be suppressed over a wider area of the outer periphery of sealing member 12 than with discontinuously formed grooves.
[0052] Furthermore, the direction in which grooves 22-24 and 27 extend may form an angle greater than 0° and smaller than 90° with respect to the circumferential direction of the outer circumferential surface of sealing member 12. Providing an angle has the effect of making it easier for electrolyte 13 to drop in the direction of gravity.
[0053] Also, the grooves 22-24, 27 may be formed so that the volume formed by them is larger than the amount of electrolyte attached. By forming the grooves 22-24, 27 in this manner, even if the electrolyte 13 rises, the grooves 22-24, 27 are not filled with the electrolyte 13, and the electrolyte 13 does not rise higher than the grooves 22-24, 27. Also, the grooves 22-24, 27 are provided closer to the bottom 34 of the battery can 11 than the fusion zone 26. Therefore, the electrolyte 13 does not reach the fusion zone 26, and the electrolyte 13 can be prevented from mixing with the fusion zone 26 when the battery can 11 and the sealing member 12 are welded together.
[0054] (Embodiment 2) In battery 40 of embodiment 2, a suppression portion that suppresses the electrolyte from rising between the inner circumferential surface of the opening edge portion and the outer circumferential surface of the sealing member toward the position where the molten portion is formed is different from groove portions 22-24, 27. In battery 40 of embodiment 2, the configuration other than the suppression portion is the same as battery 10 of embodiment 1. In embodiment 2, configurations that are the same as or similar to those in embodiment 1 are described with the same reference numerals. Also, in embodiment 2, differences from embodiment 1 are mainly described, and descriptions that overlap with embodiment 1 are omitted.
[0055] The second embodiment will be described in detail below with reference to the drawings. Fig. 3A shows a schematic cross-sectional view of the vicinity of surface-treated portion 31 in battery 40 according to the second embodiment. Fig. 3B shows a schematic view of sealing member 12 in battery 40 according to the second embodiment.
[0056] 3A, in battery 40 of embodiment 2, similarly to battery 10 of embodiment 1, space 18 is generated between opening edge portion 17 and sealing member 12. In such space 18, electrolyte 13 may rise due to capillary action as described above.
[0057] As shown in FIG. 3B, in battery 40 of embodiment 2, in order to suppress the rise of electrolyte 13 due to capillary action in space 18, a surface-treated portion 31 having an oil-repellent effect against electrolyte 13 is provided on the outer peripheral surface of sealing member 12.
[0058] The surface-treated portion 31 is formed on the outer peripheral surface of the sealing member 12 so as to extend along the circumferential direction of the outer peripheral surface. Moreover, the surface-treated portion 31 is formed as one continuous surface-treated portion around the entire circumference of the sealing member 12. Since the surface-treated portion 31 extends around the entire circumference of the outer peripheral surface of the sealing member 12, the surface-treated portion 31 exists on the outer peripheral surface of the sealing member 12 in a direction perpendicular to the circumferential direction. Moreover, the surface-treated portion 31 is located closer to the bottom 34 of the battery can 11 than the molten portion 26.
[0059] In the second embodiment, the surface-treated portion 31 is formed as a suppression portion. The surface-treated portion 31 has an oil-repellent effect on the electrolyte 13, and can reduce the wettability of the electrolyte 13. If the wettability of the electrolyte 13 is low, the surface tension of the electrolyte 13 and the gravity for balancing the surface tension are reduced, and the rise of the electrolyte 13 in the space 18 is suppressed. Note that instead of the surface-treated portion 31, a surface-treated portion having a water-repellent effect may be provided.
[0060] The decrease in wettability of the electrolyte 13 due to the surface-treated portion 31 will be described in detail. For example, consider capillary action mainly involving ethylene carbonate, which is the main component of the electrolyte of a secondary battery. It is known that the height of rise h due to capillary action can be expressed by formula (1) using density ρ, surface tension T, wetting angle θ, radius r of the space 18 (half the width of the space 18 is regarded as the radius), and gravitational acceleration g. h = 2Tcosθ / ρgr (1) When ethylene carbonate is used at 20°C, the density ρ is calculated as 1.320 g / cm 3 , surface tension T is 0.02N / m, radius r of space 18 is 0.01mm, and gravitational acceleration g is 9.8m / s 2 Here, when the surface is processed so that the wetting angle θ is 90°, the rising height h of the electrolyte 13 in the space 18 is theoretically 0 mm. Therefore, it is possible to suppress the electrolyte 13 from rising due to the capillary phenomenon and being mixed into the molten part 26. On the other hand, when the wetting angle θ is 89°, the rising height h is about 5.4 mm, so it is desirable that the wetting angle of the electrolyte 13 by the surface processed part 31 is 90° or more.
[0061] Also, as in the first embodiment, the surface processed portion 31 may be provided on the outer peripheral surface of the sealing member 12 closer to the bottom 34 of the battery can 11 than the fusion portion 26. Also, the surface processed portion 31 may be formed on the outer peripheral surface of the sealing member 12 at a position away from the fusion portion 26. For example, in a continuous output fiber laser with a wavelength of 1070 nm, a power of 700 W, a speed of 125 mm / s, and a spot diameter of 0.7 mm, the penetration depth of the fusion portion 26 is about 0.25 mm. By forming the surface processed portion 31 at a position 0.1 mm or more away from the position of the penetration depth, it is possible to suppress the vaporized electrolyte 13 from mixing into the fusion portion 26. Therefore, by providing a predetermined distance between the surface processed portion 31 and the fusion portion 26, it is possible to suppress the electrolyte 13 near the surface processed portion 31 from being vaporized by the heat of welding and being mixed into the fusion portion 26.
[0062] As in the first embodiment, the surface-treated portion 31 may be provided on the inner peripheral surface of the opening edge portion 17, or on both the outer peripheral surface of the sealing member 12 and the inner peripheral surface of the opening edge portion 17, in addition to the outer peripheral surface of the sealing member 12. The surface-treated portion 31 is not limited to one continuous surface-treated portion. For example, multiple continuous surface-treated portions 31 may be provided. Also, multiple discontinuous surface-treated portions 31 may be provided so that at least one surface-treated portion 31 exists in a direction perpendicular to the circumferential direction.
[0063] 3C shows a modified example of the surface-treated portion 31 of the second embodiment, and is a schematic cross-sectional view of the vicinity of the both-side surface-treated portion 32. In this modified example, instead of the surface-treated portion 31, both-side surface-treated portions 32 are formed on both sides of the sealing member 12 side and the opening edge portion 17 side. The both-side surface-treated portions 32 extend in the circumferential direction of the outer peripheral surface of the sealing member 12 over the entire circumference, and extend in the circumferential direction of the inner peripheral surface of the opening edge portion 17 over the entire circumference. The both-side surface-treated portions 32 are provided so as to be located closer to the bottom 34 of the battery can 11 than the molten portion 26.
[0064] The method for forming the surface processed portion 31 and the both-side surface processed portions 32 is limited to surface fine patterning. In coating processing, the coating material peels off from the sealing member 12 during welding and gets mixed into the molten portion 26, which causes welding defects. The surface fine patterning method is not particularly limited, and may be appropriately selected depending on the materials of the sealing member 12 and the battery can 11. Examples of the surface fine patterning method include cutting, nanoimprinting, and laser processing.
[0065] (effect) In battery 40 according to the second embodiment, sealing material 12 is formed with surface-treated portion 31 having a water-repellent or oil-repellent effect as a suppression portion.
[0066] The surface-treated portion 31 reduces the wettability of the electrolyte 13 to the sealing member 12 at the surface-treated portion 31. The reduction in the wettability of the electrolyte 13 to the sealing member 12 reduces the surface tension of the electrolyte 13 and the gravity required to balance the surface tension, making it possible to suppress the electrolyte 13 from rising due to the capillary phenomenon. This makes it possible to suppress the electrolyte 13 from mixing into the molten portion 26 when the battery can 11 and the sealing member 12 are welded together.
[0067] Furthermore, the surface-treated portion 31 may be provided over the entire outer periphery of the sealing member 12. Therefore, the intermittently formed surface-treated portion 31 can suppress the rise of the electrolyte 13 over a wide range on the outer periphery of the sealing member 12.
[0068] For example, it is preferable to form a surface-treated portion 31 on the sealing member 12 that has a water-repellent effect or an oil-repellent effect such that the wetting angle of the electrolyte 13 with respect to the sealing member 12 is 90° or more. When the wetting angle is 90° or more, the electrolyte 13 does not rise higher than the surface-treated portion 31. In addition, the surface-treated portion 31 is provided closer to the bottom 34 of the battery can 11 than the fusion portion 26. Therefore, the electrolyte 13 does not reach the fusion portion 26, and it is possible to suppress the electrolyte 13 from mixing with the fusion portion 26 when the battery can 11 and the sealing member 12 are welded together.
[0069] Incidentally, by appropriately combining any of the various embodiments described above, it is possible to obtain the effects that each embodiment has. [Industrial Applicability]
[0070] Batteries according to the present disclosure can be used in various can-type batteries, and are useful in applications such as power sources for portable devices, hybrid vehicles, electric vehicles, etc. [Explanation of symbols]
[0071] 10 batteries 11 Battery can 12 Sealing member 13 Electrolyte 14 Electrode body 15 First opposing surface 16 Second opposing surface 17 Opening edge 18 Space 19 Positive tab 20 Negative tab 22 Groove 23 2 grooves 24 Both side grooves 25 Laser 26 Welding section 27 Angled Groove 31 Surface processing section 32 Surface treatment on both sides 33 Cylinder part 34 Bottom 40 batteries
Claims
1. a metal battery can having a cylindrical portion with an open edge at one end and a bottom portion closing the other end of the cylindrical portion; An electrode assembly housed in the battery can; An electrolyte filled in the battery can; a sealing member having an outer circumferential surface arranged to face an inner circumferential surface of the opening edge portion of the cylindrical portion and sealing the opening edge portion, a part of an inner circumferential surface of the opening edge portion and a part of an outer circumferential surface of the plugging material are joined by a fusion zone, a suppression portion that suppresses the electrolytic solution from rising between an inner peripheral surface of the opening edge portion and an outer peripheral surface of the sealing member toward a position where the molten portion is to be formed is provided on the outer peripheral surface of the sealing member closer to the bottom than the molten portion, The battery, wherein the suppression portion is a groove portion provided around the entire outer periphery of the sealing member.
2. The battery according to claim 1 , wherein the extending direction of the groove portion forms an angle greater than 0° and smaller than 90° with respect to the circumferential direction of the outer circumferential surface of the sealing member.
3. The battery according to claim 1 , wherein a volume formed by the groove is larger than an expected amount of electrolyte attached to the inner circumferential surface of the opening edge portion.
4. The suppression unit is a first suppression unit, The battery according to any one of claims 1 to 3, wherein a second suppression portion that suppresses the electrolyte from rising between the inner surface of the opening edge portion and the outer surface of the sealing member toward a position where the molten portion is formed is provided on the inner surface of the opening edge portion and on the bottom side of the molten portion.
5. A battery as described in claim 4, wherein the second restraining portion is another groove portion provided on the inner surface of the opening edge portion.
6. A battery as described in claim 4 or 5, wherein the second suppression portion is provided around the entire inner surface of the opening edge portion.
7. A metal battery can having a cylindrical portion with an open edge at one end and a bottom portion closing the other end of the cylindrical portion; An electrode assembly housed in the battery can; An electrolyte filled in the battery can; a sealing member having an outer circumferential surface arranged to face an inner circumferential surface of the opening edge portion of the cylindrical portion and sealing the opening edge portion, a part of an inner circumferential surface of the opening edge portion and a part of an outer circumferential surface of the plugging material are joined by a fusion zone, a suppression portion that suppresses the electrolytic solution from rising between an inner peripheral surface of the opening edge portion and an outer peripheral surface of the sealing member toward a position where the molten portion is to be formed is provided on the outer peripheral surface of the sealing member closer to the bottom than the molten portion, The battery, wherein the suppression portion is a surface-treated portion provided around the entire outer periphery of the sealing member and having a water-repellent effect or an oil-repellent effect against the electrolyte.
8. A battery as described in claim 7, wherein the surface-treated portion has a water-repellent effect or an oil-repellent effect such that the wetting angle of the electrolyte to the sealing material is 90° or more.
9. The suppression section is a first suppression section, 9. The battery according to claim 7, wherein a second suppression portion that suppresses the electrolyte from rising between an inner surface of the opening edge portion and an outer surface of the sealing member toward a position where the molten portion is formed is provided on the inner surface of the opening edge portion and on the bottom side of the molten portion.
10. A battery as described in Claim 9, wherein the second suppression portion is provided around the entire inner surface of the opening edge portion.
Citation Information
Patent Citations
sealed battery
JP1995008950U
Anti-explosive enclosed battery
JP1995105933A
Sealing structure for angular sealed battery
JP1997007561A
Method for manufacturing sealed battery, and sealed battery
JP2007157519A
Cell and cell manufacturing method, and vehicle mounted with cell
JP2008159536A