Universal Process Kit
The innovative edge ring design in the process kit addresses non-uniform etching by maintaining the substrate in the same plane as the edge ring, enhancing etching uniformity and reducing ion deflection, thus improving plasma processing consistency.
Patent Information
- Application Number
- JP2022104311
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-03-04
- Filing Date
- 2022-06-29
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2037-02-13
AI Technical Summary
Existing semiconductor processing kits cause non-uniform etching due to perturbations in the plasma sheath, leading to localized ion flux deviations and etching non-uniformity.
A process kit with a specially designed edge ring comprising an inner and outer ring, where the inner ring is made of a non-metallic conductor with a notch, and the outer ring is made of quartz, positioned to minimize perturbations in the plasma sheath by maintaining the substrate in the same plane as the edge ring, thereby reducing ion deflection and enhancing etching uniformity.
The process kit minimizes plasma sheath perturbations, ensuring uniform ion flux and improved etching consistency across the substrate, even under varying plasma conditions.
Smart Images

Figure 0007562604000001 
Figure 0007562604000002 
Figure 0007562604000003
Abstract
Description
background
[0001] (Field) FIELD OF THE DISCLOSURE Embodiments of the present disclosure relate generally to semiconductor processing, and more specifically to a process kit for use in a semiconductor processing chamber.
[0002] Description of Related Art Various semiconductor manufacturing processes (e.g., plasma-assisted etching or chemical vapor deposition) are performed in plasma processing chambers. A substrate support supports a substrate at a processing position within the semiconductor processing chamber. A plasma region containing one or more process gases is maintained within the semiconductor processing chamber to perform the semiconductor manufacturing processes on a substrate disposed on the substrate support.
[0003] A plasma sheath is a thin region of strong electric field formed by space charges that separates the plasma to material boundaries. During plasma etching, a plasma sheath forms between the plasma and all other parts of the semiconductor processing chamber that come into contact with the plasma region, including the substrate being etched, the walls of the semiconductor processing chamber, and the process kits.
[0004] The thickness (d) of the plasma sheath is expressed by the following equation 1. d=(2 / 3)(ε / i) 1 / 2 (2e / m) 1 / 4 (V P -V DC ) 3 / 4 (Formula 1)
[0005] In the formula, "i" is the ion current density, "ε" is the dielectric constant of vacuum, "e" is the elementary charge, "m" is the ion mass, and "V P " is the plasma potential. As shown, the thickness of the plasma sheath is a function of the plasma parameters, namely, ion current "i" and "V DC" can be increased or decreased by adjusting the source power and bias power, which respectively affect the plasma flux. Ions generated in the plasma region are accelerated through the plasma sheath on trajectories perpendicular to the plasma sheath. Because the plasma sheath is generally parallel to the planar surface of the substrate, ions passing through the plasma sheath generally impinge on the substrate in a perpendicular direction. Conversely, perturbations in the shape of the plasma sheath (e.g., caused by the presence of a process kit at the edge of the substrate) locally change the ion flux and cause ions passing through the plasma sheath to impinge on the substrate in a non-perpendicular direction, thereby causing etch non-uniformity.
[0006] Thus, there is a need in the art for an improved process kit.
[0007] A process kit suitable for use in a semiconductor processing chamber is disclosed. In one embodiment, the process kit includes an edge ring. The edge ring includes an inner ring and an outer ring. The inner ring includes a non-metallic conductor having a first surface opposite a second surface. The non-metallic conductor has a resistivity of less than about 50 ohm·cm. The inner ring further includes a notch disposed along an inner diameter of the inner ring. The notch has a vertical component that rises less than about 1200 μm and a horizontal component that extends between about 1300 μm and about 2500 μm. The outer ring is coupled to the inner ring and surrounds a periphery of the inner ring. The outer ring includes a quartz body having a third surface opposite a fourth surface.
[0008] In another embodiment, a plasma chamber for performing a semiconductor process on a substrate is disclosed. The plasma chamber includes a substrate support assembly and a process kit. The process kit is adapted for use adjacent to the substrate support assembly and is coupled to a flange of the substrate support assembly. The process kit includes an edge ring and a conductive member. The edge ring includes a notch disposed along an inner diameter of the edge ring. The notch has a vertical component that rises less than about 1200 μm and a horizontal component that extends between about 1300 μm and about 2500 μm. Additionally, the conductive member is coupled to the edge ring.
[0009] In yet another embodiment, a process kit suitable for use in a processing chamber includes an edge ring, at least one thermal contact pad, and a conductive member. The edge ring surrounds a periphery of a substrate support assembly disposed in the processing chamber. The edge ring includes an inner ring and an outer ring. The inner ring is disposed adjacent to the substrate support assembly and includes a non-metallic conductive material. The inner ring further includes a notch disposed along an inner diameter of the inner ring, the notch having a vertical component rising less than about 1200 μm and a horizontal component extending between about 1300 μm and about 2500 μm. The outer ring is coupled to the inner ring and surrounds a periphery of the inner ring. The outer ring includes a quartz material. At least one thermal contact pad is coupled to the inner ring and disposed within a slot formed in the inner ring. Additionally, a conductive member is coupled to the outer ring. [Brief description of the drawings]
[0010] In order to allow the above-mentioned features of the present disclosure to be understood in detail, a more particular description of the present disclosure briefly summarized above will be made with reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings only illustrate exemplary embodiments, and therefore should not be construed as limiting the scope thereof, which may include other equally effective embodiments. [Figure 1]1 shows a schematic cross-sectional view of a plasma processing chamber according to an embodiment described herein. [Figure 2A] ~ [Figure 2B] 2A and 2B are a schematic cross-sectional view and an enlarged schematic cross-sectional view, respectively, of the process kit of FIG. [Diagram 3] 2 shows a schematic top view of the process kit of FIG. 1. [Figure 4A] ~ [Figure 4B] 1 shows a schematic graph of nitride etch rate performed at high source power versus bias power and low source power versus bias power.
[0011] To facilitate understanding, the same reference numbers have been used whenever possible to designate identical elements common to the figures. It is understood that elements and features of one embodiment may be beneficially incorporated in other embodiments without further description.
[0012] The embodiments described herein generally relate to a process kit suitable for use in a semiconductor processing chamber that reduces edge effects with a single edge ring compared to conventional process kits. The process kit generally includes an edge ring disposed adjacent to and surrounding a periphery of a semiconductor substrate in a plasma chamber. A dimension of a gap between the substrate and the edge ring is less than about 1000 μm, and a height difference between the substrate and the edge ring is less than about ±300 μm. The resistivity of the ring is less than about 50 ohm·cm.
[0013] A "substrate" or "substrate surface" as described herein generally refers to any substrate surface on which processing is performed. For example, the substrate surface may include silicon, silicon oxide, doped silicon, silicon germanium, germanium, gallium arsenide, glass, sapphire, and any other material (e.g., metals, metal nitrides, metal alloys, and other conductive or semiconductive materials) depending on the application. The substrate or substrate surface may also include dielectric materials (e.g., silicon dioxide, silicon nitride, organosilicates, and carbon-doped silicon oxide or nitride materials). The term "substrate" may further include the term "wafer". The substrate itself is not limited to a particular size or shape. Although the embodiments described herein are generally made with reference to round substrates, other shapes (e.g., polygonal, square, rectangular, curved, or other non-circular workpieces) may be utilized in accordance with the embodiments described herein. (General Description of Processing Chamber)
[0014] 1 shows a schematic cross-sectional view of one embodiment of a semiconductor processing chamber 100 in which the present embodiments may be used. The semiconductor processing chamber 100 shown is a magnetically enhanced plasma chamber suitable for either etching or chemical vapor deposition (CVD).
[0015] The processing chamber 100 includes a cylindrical sidewall 102, a circular bottom wall 104, and a circular top wall 106. An anode electrode 108 may be attached to the bottom of the top wall 106 and electrically grounded. The anode electrode 108 may be perforated to serve as a gas inlet for process gases to enter the semiconductor processing chamber 100. Each of the walls 102, 104, 106 of the semiconductor processing chamber 100 are metal, although some or all of the walls 102, 104, 106 may comprise a semiconductor material or a dielectric material. Any walls 102, 104, 106 that are not dielectric may be electrically grounded and function as part of the anode electrode 108.
[0016] The substrate support assembly 120 is disposed within the processing chamber 100. The substrate support assembly 120 has a substantially flat front surface 140 that faces the anode electrode 108. The front surface 140 of the substrate support assembly 120 supports the substrate 110 during processing. The substrate support assembly 120 may be supported by the bottom wall 104 of the semiconductor processing chamber 100. The substrate support assembly 120 has a metallic substrate support 122 that functions as a cathode electrode as described below, although the substrate support 122 need not be metallic as long as another electrode disposed within the substrate support assembly 120 is configured to operate as the cathode electrode.
[0017] The substrate 110 may be held in place on the substrate support assembly 120 by mechanical clamps, vacuum, gravity, or electrostatic forces. In one embodiment, the substrate support assembly 120 includes an energizable electrostatic chuck 126 to firmly hold the substrate 110 against a front surface 140 of the substrate support assembly 120 during processing.
[0018] The electrostatic chuck 126 includes at least one chucking electrode 124 surrounded by a dielectric material 142. The dielectric material 142 of the electrostatic chuck 126 electrically insulates the chucking electrode 124 from the substrate 110 and the metallic substrate support 122, thus enabling an electrostatic attraction to the substrate 110 when the chuck electrode 124 is energized. Power for operating the electrostatic chuck 126 is provided by a power supply 128.
[0019] The diameter of the portion 144 of the electrostatic chuck 126 that supports the substrate 110 may be smaller than the diameter of the substrate 110 (ie, the substrate 110 overhangs slightly beyond the perimeter of the portion 144 of the electrostatic chuck 126 that supports the substrate 110).
[0020] The substrate support assembly 120 further includes a substrate support 122 disposed below the electrostatic chuck 126. The substrate support 122 may be cylindrical in shape and may be constructed of a metallic material (e.g., anodized aluminum). The substrate support 122 has a larger radius than the electrostatic chuck 126 and provides a flange 146 that facilitates securing the electrostatic chuck 126 to the substrate support 122.
[0021] A vacuum pump (not shown) evacuates gases from the processing chamber through an exhaust manifold 130 and maintains the total gas pressure in the chamber at a level low enough to promote plasma generation (e.g., in the range of about 10 mTorr to 20 Torr), with pressures at the lower and upper ends of this range being more suitable for etching and CVD processes, respectively.
[0022] During processing of the substrate 110, a plasma is maintained in a region 148 of the processing chamber 100 defined between the substrate 110 and the anode electrode 108. The plasma is generated by exciting the processing gas mixture into a plasma state. The plasma can be generated within the processing chamber (in situ plasma) or generated in another chamber (remote plasma source) and pumped into the processing chamber.
[0023] A radio frequency (RF) power source 132 is connected through one or more series coupling capacitors 134 to one or more of the following chamber components: the substrate support 122, the chuck electrode 124, or an additional electrode (e.g., a wire mesh) embedded within the electrostatic chuck 126. If any of these components are connected to an RF power source, they collectively constitute the cathode electrode of the processing chamber. In one embodiment, the substrate support 122 is connected to the RF power source 132 to function as the cathode electrode.
[0024] An RF power supply 132 supplies an RF voltage between the cathode electrode and the grounded anode electrode 108, which helps provide the excitation power necessary to sustain the plasma. The RF voltage applied to the cathode also creates a negative time-averaged DC bias voltage at the cathode electrode relative to both the anode electrode and the plasma, which accelerates ionized process gas components toward the cathode electrode to facilitate processing of the substrate 110.
[0025] In an exemplary embodiment, the substrate 110 supported by the substrate support assembly 120 may be a 200 mm, 300 mm, or 450 mm silicon wafer. A standard 200 mm substrate typically has a thickness of about 725 μm. A standard 300 mm substrate typically has a thickness of about 775 μm. A standard 450 mm substrate typically has a thickness of about 925 μm. (Universal Process Kit)
[0026] FIG 2A shows a schematic cross-sectional view of a process kit 200 suitable for use in the semiconductor processing chamber 100 of FIG 1. FIG 3 shows a schematic top view of the process kit 200 of FIG 1. Referring to both FIG 2A and FIG 3, the process kit 200 is disposed in the semiconductor processing chamber 100 to improve plasma processing and protect chamber components during processing. In some embodiments, the process kit 200 can be coupled to and / or supported by the substrate support assembly 120 and can be used adjacent to the substrate support assembly 120. The process kit 200 can extend further around the periphery of the substrate 110 and / or be disposed adjacent to the substrate 110.
[0027] The process kit 200 includes an edge ring 202. The edge ring 202 includes an inner ring 204 and an outer ring 206. However, it is understood that in some embodiments, the inner ring 204 and the outer ring 206 can form a single ring. The edge ring 202 surrounds the periphery 150 of the substrate support assembly 120. The edge ring 202 includes a notch 210 disposed along an inner diameter 212 of the edge ring 202 and / or the inner ring 204.
[0028] The inner ring 204 is disposed adjacent to the substrate support assembly 120. The inner ring 204 includes a first side 214 and a second side 216, with the second side 216 facing the first side 214. The inner ring 204 is fabricated from a non-metallic and / or conductive material having a resistivity of less than about 100 ohm-cm (e.g., less than about 50 ohm-cm). The inner ring 204 may be fabricated from a silicon carbide material, a silicon material, a non-metallic material, and / or mixtures and combinations thereof.
[0029] The inner ring 204 further includes a notch 210. In some embodiments, the notch 210 is formed in an inner diameter 212 of the inner ring 204. The notch 210 includes a vertical component as represented by reference arrow "V" in FIG. 2A. The vertical component V can have a rise of less than about 1500 μm (e.g., less than about 1200 μm). The notch 210 further includes a horizontal component as represented by reference arrow "H" in FIG. 2A. The horizontal component H can have a run extending between about 1000 μm and about 3000 μm (e.g., about 1300 μm and about 2500 μm (e.g., about 1800 μm)). The notch 210 can support the substrate 110 and / or prevent movement of the substrate 110 during processing.
[0030] FIG. 2B is an enlarged cross-sectional view of the notch 210 of the edge ring 202 shown in FIG. 2A. The dimensions of the process kit 200 are precisely formed within tight tolerances so as not to perturb the plasma sheath at the edge of the substrate 110. Thus, the dimension of the gap E between the substrate 110 and the inner ring 204 of the edge ring 202 is less than about 1000 μm (e.g., less than about 800 μm (e.g., less than about 800 μm)). Furthermore, the height F of the inner ring 204 of the edge ring 202 is selected such that the top surface 240 of the substrate 110 and the first surface 214 of the inner ring 204 are substantially in the same plane. In some embodiments, substantially in the same plane means that the vertical distance between the plane formed by the top surface 240 of the substrate 110 and the plane formed by the first surface 214 of the inner ring 204 is within about ±400 μm of each other (e.g., within about ±300 μm of each other (e.g., within ±200 μm of each other)).
[0031] 2A and 3, the outer ring 206 may be coupled to the inner ring 204 and may surround a periphery 218 of the inner ring 204. In some embodiments, the outer ring 206 may support the inner ring 204 via a support ledge 220 formed along an inner circumference 222 of the outer ring. Additionally, the outer ring 206 includes a third side 224 and a fourth side 226. The third side 224 may oppose the fourth side 226. The outer ring 206 may include a quartz material.
[0032] The process kit 200 may further include at least one thermal contact pad 208. In some embodiments, the thermal contact pad 208 may be optional. Although only a portion of one thermal contact pad 208 is shown in FIG. 2A, it is understood that multiple thermal contact pads 208 may be utilized, as shown in FIG. 2B. The thermal contact pad 208 may be fabricated from a silicone (polymer) material. Furthermore, the thermal contact pad 208 and the edge ring 202 may each share a similar thermal conductivity. Benefits of the thermal contact pad 208 include facilitating good thermal contact between the edge ring 202 and the electrostatic chuck 126.
[0033] The thermal contact pads 208 may be coupled to the inner ring 204. Each thermal contact pad 208 contacts the second surface 216 of the inner ring 204, and in some embodiments, each thermal contact pad 208 may have a non-continuous (i.e., segmented) ring shape, as shown in FIG. 3. In this manner, the thermal contact pads 208 may include a ring shape similar to the edge ring 202, but the thermal contact may not extend completely around the edge ring 202. However, it is understood that in some embodiments, one thermal contact pad 208 may be a continuous ring and have a continuous ring shape extending completely around the edge ring 202. However, in other embodiments, the thermal contact pads 208 may be any suitable shape.
[0034] Additionally, as shown in Figure 3, multiple thermal contact pads 208 may contact the inner ring 204. Although four thermal contact pads 208 are shown in Figure 3, it is understood that any number of thermal contact pads 208 may be utilized. Each thermal contact pad 208 may facilitate good thermal contact between the edge ring 202 and the electrostatic chuck 126.
[0035] The second surface 216 of the inner ring 204 may include at least one slot 228 formed at least partially therein. Each slot 228 may accommodate a respective one of the thermal contact pads 208. As such, the number of thermal contact pads 208 and the number of slots 228 formed in the second surface 216 of the inner ring 204 may be the same. Each thermal contact pad 208 may be fully accommodated within each slot 228, but in some embodiments, each thermal contact pad 208 may extend partially out of its respective slot 228 such that it protrudes beyond the second surface 216 of the inner ring 204. Each slot 228 protects each thermal contact pad 208 and minimizes interference of the thermal contact pads 208 with other components.
[0036] In some embodiments, the process kit 200 may further include a conductive member 230. The conductive member 230 may be coupled to the fourth side 226 of the outer ring 206. In some embodiments, the outer ring 206 may include a channel 232 formed in the fourth side 226. The conductive member 230 may be at least partially disposed within the channel 232 such that the outer ring 206 is coupled to the conductive member 230.
[0037] Tests were conducted and results showed that the use of the process kit disclosed herein minimizes ion focusing and defocusing effects, as shown in the schematic graphs of FIG. 4A and FIG. 4B. As further shown, the position of the surface of the substrate relative to the top surface of the ring is important to minimize the perturbation of the plasma sheath at the edge of the substrate. If the edge ring is machined such that the substrate is above the plane of the edge ring, the plasma sheath may bend outward. Ions move perpendicular to the plasma sheath, thus deflecting away from the edge of the substrate and decreasing the etch rate. On the other hand, if the edge ring is machined such that the substrate is below the plane of the ring, the sheath may bend inward, thus focusing ions at the edge of the wafer and increasing the etch rate. The use of the process kit disclosed herein positions the substrate in the same plane as the edge ring, thus minimizing bending of the plasma sheath. Furthermore, the ability of the plasma sheath to bend depends on the thickness of the plasma sheath, which in turn depends on the plasma conditions (mainly the source and bias powers (see Equation 1)). 4A and 4B show that when the process kit of the present disclosure is used with a high power source (e.g., greater than about 1000 Watts) relative to the bias power (e.g., between about 50 Watts and about 500 Watts) or a low source power (e.g., less than about 500 Watts) relative to the bias power (e.g., between about 50 Watts and about 500 Watts), the geometry of the process kit minimized edge effects regardless of the plasma conditions.
[0038] Advantages of the present disclosure include a process kit that reduces plasma sheath perturbations at the edge of a substrate. The edge ring can include a conductive ring and a non-conductive ring, both of which can be machined to be flush with the substrate. The process kit thus serves to reduce plasma etch variations due to non-uniform plasma sheaths, thus improving process uniformity.
[0039] In summary, the embodiments described herein generally relate to a process kit suitable for use in a semiconductor processing chamber that reduces edge effects and widens a processing window with a single edge ring compared to conventional process kits. The process kit generally includes an edge ring that is positioned adjacent to and surrounds the periphery of a semiconductor substrate in a plasma chamber. A dimension of a gap between the substrate and the edge ring is less than about 1000 μm, and a height difference between the substrate and the edge ring is less than about ±300 μm. The resistivity of the ring is less than about 50 ohm·cm.
[0040] While the forgoing is directed to embodiments of the present disclosure, other and further embodiments of the present disclosure may be made without departing from the basic scope thereof, which is defined by the following claims.
Claims
1. 1. An inner ring suitable for use in a semiconductor processing chamber for processing a substrate, the inner ring being positioned adjacent the substrate, the inner ring comprising: the gap between the substrate and the inner ring is less than 1000 μm; a non-metallic conductor having a first surface opposite a second surface, the second surface including at least one slot drilled at least partially therein, the non-metallic conductor having a resistivity of less than 50 ohm-cm; a notch disposed along an inner diameter of the inner ring; the notch has a vertical component rising less than 1200 μm and a horizontal component extending between 1300 μm and 2500 μm; the at least one slot is disposed between the notch and an outer diameter of the inner ring; An inner ring, the vertical distance between the plane formed by the top surface of the substrate and the plane formed by the first surface is within ±400 nm.
2. The inner ring of claim 1 including at least one thermal contact pad received within the at least one slot.
3. The inner ring of claim 2 , wherein at least one thermal contact pad has a non-continuous ring shape.
4. The inner ring of claim 2 , wherein the at least one thermal contact pad comprises a silicone material.
5. The inner ring of claim 1, wherein the inner ring comprises a silicone material.
6. The inner ring of claim 1, wherein the inner ring comprises a silicon carbide material.
7. 1. A process kit suitable for use in a processing chamber for processing a substrate, comprising: An edge ring including an inner ring and an outer ring; The inner ring is disposed adjacent the substrate; the gap between the substrate and the inner ring is less than 1000 μm; a non-metallic conductor having a first surface opposite a second surface, the second surface including at least one slot drilled at least partially therein, the non-metallic conductor having a resistivity of less than 50 ohm-cm; a notch disposed along an inner diameter of the inner ring; the notch has a vertical component rising less than 1200 μm and a horizontal component extending between 1300 μm and 2500 μm; the vertical distance between a plane formed by the top surface of the substrate and a plane formed by the first surface is within ±400 nm; the outer ring is coupled to the inner ring and surrounds an outer diameter of the inner ring; a support ledge formed along an inner diameter of the outer ring; The at least one slot is disposed between the notch and the support ledge.
8. The process kit of claim 7 , comprising at least one thermal contact pad received in the at least one slot.
9. The process kit of claim 8 , wherein the at least one thermal contact pad has a non-continuous ring shape.
10. The process kit of claim 8 , wherein the at least one thermal contact pad comprises a silicone material.
11. The process kit of claim 8 , comprising a second thermal contact pad, a third thermal contact pad, and a fourth thermal contact pad, each thermal contact pad disposed in a slot formed in the inner ring.
12. The process kit of claim 7, wherein the inner ring comprises a silicone material.
13. The process kit of claim 7, wherein the inner ring comprises a silicon carbide material.
14. 1. A plasma chamber for performing a semiconductor process on a substrate, comprising: a substrate support assembly; an inner ring disposed adjacent to the substrate support assembly, a non-metallic conductor having a first surface opposite a second surface, the second surface including at least one slot drilled at least partially therein, the non-metallic conductor having a resistivity of less than 50 ohm-cm; a notch disposed along an inner diameter of the inner ring; the notch has a vertical component rising less than 1200 μm and a horizontal component extending between 1300 μm and 2500 μm; the at least one slot comprises an inner ring disposed between the notch and an outer diameter of the inner ring; A plasma chamber, wherein the vertical distance between a plane formed by a top surface of the substrate and a plane formed by the first surface is within ±400 nm, and the gap between the substrate and the inner ring is less than 1000 μm.
15. The plasma chamber of claim 14 including at least one thermal contact pad received within the at least one slot.
16. The plasma chamber of claim 15 , wherein at least one thermal contact pad has a non-continuous ring shape.
17. The plasma chamber of claim 15 , wherein the at least one thermal contact pad comprises a silicone material.
18. The plasma chamber of claim 15 including a second thermal contact pad, a third thermal contact pad, and a fourth thermal contact pad, each thermal contact pad disposed in a slot formed in the inner ring.
19. The plasma chamber of claim 14, wherein the inner ring comprises a silicon material.
20. The plasma chamber of claim 14, wherein the inner ring comprises a silicon carbide material.
Citation Information
Patent Citations
Annular heater
JP2006127900A
Heat-conducting sheet and placement device of substrate to be treated using it
JP2008244096A
Method for controlling temperature of material in chamber of plasma treatment device, mounting stage for material in chamber and substrate, and plasma treatment device equipped with the same
JP2010016319A
Wafer support device and component used for the same
JP2010016363A
Apparatus and method for plasma processing
JP2010251723A