Multi-state RF pulsing to control mask shape and break the selectivity vs. process margin trade-off

A multi-state RF pulsing method with intermediate states addresses the selectivity versus process margin challenge in high aspect ratio etching, enhancing etching precision and reducing defects by controlling mask shape and necking in semiconductor manufacturing.

JP7562637B2Active Publication Date: 2024-10-07LAM RES CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022509590
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-10-03
Filing Date
2020-08-21
Publication Date
2024-10-07
Estimated Expiration
2040-08-21

AI Technical Summary

Technical Problem

Current RF pulsing methods struggle to balance selectivity and process margin in high aspect ratio etching, particularly in dielectric etching processes for advanced semiconductor manufacturing, leading to issues like necking, warpage, and clogging, which are exacerbated by shrinking device sizes and pitch sizes.

Method used

Implementing a multi-state RF pulsing method with intermediate states based on source power only, combining traditional two-state on-off pulsing to control mask shape and improve selectivity versus process margin, using three distinct states to etch, passivate, and open the neck of features.

Benefits of technology

This approach enhances etching capabilities by maintaining adequate process margins while improving selectivity, reducing necking and warpage, and expanding the process window for high aspect ratio etching, allowing for more precise and defect-free feature formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562637000001
    Figure 0007562637000001
  • Figure 0007562637000002
    Figure 0007562637000002
  • Figure 0007562637000003
    Figure 0007562637000003
Patent Text Reader

Abstract

1. A method for performing an etching process on a substrate in a plasma processing system, comprising: applying source RF power and bias RF power to an electrode, wherein the source RF power and bias RF power together are pulse signals defining a plurality of multi-state pulsed RF cycles, each cycle having a first state, a second state, and a third state, wherein the first state is defined by the source RF power having a first source RF power level and the bias RF power having a first bias RF power level, the second state is defined by the source RF power and the bias RF power having substantially zero power levels, and the third state is defined by the source RF power having a second source RF power level lower than the first source RF power level and the bias RF power having substantially zero power level.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Embodiments of the present disclosure relate to a multi-state RF pulsing method to control mask shape and break the selectivity vs. process margin tradeoff. [Background technology]

[0002] RF pulsing technology has progressed from continuous wave (CW) mode to pulsed mode (on-off, inter-level) method in the last decade. Advances in two-state RF pulsing have enabled high aspect ratio etching by improving the trade-off between process margin and etch selectivity, profile bow, critical dimension (CD), and etch rate uniformity. In the current two-state RF pulsing method, “State 1” (or “S1”) represents a high bias and high source power (e.g., greater than 1 kW) state operated at pressures less than 30 mTorr to obtain a narrow IADF, with ion energy greater than 3 keV. The other state in the pulse, called “State 0” (or “S0”), represents a low bias and low source power (e.g., 1 kW) deposition process with ion energy less than 100 eV. State 0 primarily provides passivation by different mechanisms such as direct ion deposition and ion-activated neutral deposition. Typical pulse repetition rates for operating this two-state RF pulsing method are around 100 Hz to 2 kHz.

[0003] As device sizes continue to shrink and pitch sizes are further reduced (e.g., from 100 nm to currently less than about 60 nm), the tradeoff between selectivity and process margin is difficult to break with current pulsed techniques. Current technology methods struggle to balance a healthy high aspect ratio etch while maintaining sufficient process margins (e.g., under-etching, non-opening, capping).

[0004] It is against this background that the embodiments described in this disclosure arise. Summary of the Invention

[0005] Embodiments of the present disclosure include methods and systems for multi-state RF pulsing to control mask shape and break the trade-off between selectivity and process margin.

[0006] One of the challenges of high aspect ratio (HAR) contact etching is to selectively etch the stack with respect to the mask (e.g., poly) while maintaining adequate process margins. Typically, process margins are related to the shape and magnitude of the necking, as they set the limiting aspect ratio during the HAR process. However, embodiments of the present disclosure provide a method to control the mask (neck) shape and improve the selectivity vs. process margin tradeoff.

[0007] According to the embodiments of the present disclosure, multi-state RF pulsing with intermediate states based on source power only method helps to control mask shape (trimming neck) without causing undesired mask shoulder drop. Combining this source power only pulsing method with traditional two-state on-off pulsing significantly improves the margin vs. selectivity tradeoff and leverages the benefits of the refinement knobs in the HAR process.

[0008] In some embodiments, a method is provided for performing an etching process on a substrate in a plasma processing system, the method including applying a source RF power to an electrode of the plasma processing system and applying a bias RF power to the electrode, the source RF power and the bias RF power together being pulse signals defining a plurality of multi-state pulsed RF cycles, each cycle having a first state, a second state, and a third state, the first state being defined by a source RF power having a first source RF power level and a bias RF power having a first bias RF power level, the second state being defined by a source RF power having a substantially zero power level and a bias RF power having a substantially zero power level, and the third state being defined by a source RF power having a second source RF power level lower than the first source RF power level and a bias RF power having a substantially zero power level.

[0009] In some embodiments, the first condition is configured to result in etching of features on the substrate surface.

[0010] In some embodiments, the second condition is configured to effect passivation of features on the substrate surface.

[0011] In some embodiments, the third condition is configured to result in removal of material that forms a neck of the feature.

[0012] In some embodiments, the bias RF power has a frequency of less than about 10 MHz.

[0013] In some embodiments, the source RF power has a frequency greater than about 20 MHz.

[0014] In some embodiments, the third state has a duration approximately 1-5 times the duration of the first state.

[0015] In some embodiments, the second state has a duration approximately equal to the duration of the first state.

[0016] In some embodiments, the first source RF power level is in the range of approximately 1-6 kW and the first bias RF power level is in the range of approximately 5-20 kW.

[0017] In some embodiments, the second source RF power level is in the range of approximately 100 W to 6 kW.

[0018] In some embodiments, within each cycle, the third state immediately follows the second state.

[0019] In some embodiments, within each cycle, the second state immediately follows the third state.

[0020] In some embodiments, a controller is provided that is configured to cause the plasma processing system to perform an etching process on a substrate in the plasma processing system. Etching Process includes applying a source RF power to an electrode of a plasma processing system and applying a bias RF power to the electrode, where the source RF power and the bias RF power are both pulse signals defining a plurality of multi-state pulse RF cycles, each cycle having a first state, a second state, and a third state, where the first state is defined by a source RF power having a first source RF power level and a bias RF power having a first bias RF power level, the second state is defined by a source RF power having a substantially zero power level and a bias RF power having a substantially zero power level, and the third state is defined by a source RF power having a second source RF power level lower than the first source RF power level and a bias RF power having a substantially zero power level.

[0021] It will be understood that the foregoing represents a summary of certain non-limiting embodiments of the present disclosure, and further embodiments will become apparent to those skilled in the art per se by the scope of the present disclosure. [Brief description of the drawings]

[0022] [Figure 1A] 1 is a conceptual cross-sectional perspective view of a generic DRAM device 100 according to an embodiment of the present disclosure.

[0023] [Figure 1B] 1 is a conceptual cross-sectional perspective view of a high aspect ratio etch feature according to an embodiment of the present disclosure.

[0024] [Figure 2A] 13 is a graph of RF power versus time for a single pulse RF cycle of an etch process in accordance with an embodiment of the present disclosure.

[0025] [Figure 2B] 13 is a conceptual cross-sectional view of an etched feature from the S1 state of the interlevel pulse process described above. [Figure 2C] 13 is a conceptual cross-sectional view of an etched feature from the S0 state of the interlevel pulse process described above.

[0026] [Diagram 3] A schematic diagram of the trade-offs in current RF pulse technology.

[0027] [Figure 4A] 1 is a conceptual diagram of RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure. [Figure 4B] 1 is a conceptual diagram of RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure. [Figure 4C] 1 is a conceptual diagram of RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure.

[0028] [Figure 4D]1A-1C are conceptual cross-sectional views of etched features illustrating the effect of each state of a multi-state pulsed RF cycle as described herein. [Figure 4E] 1A-1C are conceptual cross-sectional views of etched features illustrating the effect of each state of a multi-state pulsed RF cycle as described herein. [Figure 4F] 1A-1C are conceptual cross-sectional views of etched features illustrating the effect of each state of a multi-state pulsed RF cycle as described herein.

[0029] [Diagram 5] 1 is a conceptual diagram illustrating different length states S2 over time during etching of a feature in accordance with an embodiment of the present disclosure.

[0030] [Figure 6A] 13 is a graph showing RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure. [Figure 6B] 13 is a graph showing RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure. [Figure 6C] 13 is a graph showing RF power versus time for a multi-state pulsed RF cycle in accordance with an embodiment of the present disclosure.

[0031] [Figure 6D] 6B and 6C, showing the effects of states S1, S2, and S0. [Figure 6E] 6B and 6C, showing the effects of states S1, S2, and S0. [Figure 6F] 6B and 6C, showing the effects of states S1, S2, and S0.

[0032] [Figure 7] FIG. 2 is a conceptual diagram illustrating the widening of the process window by using the multi-state RF pulsing method described herein.

[0033] [Figure 8] 1 illustrates an exemplary ICP deposition system according to an embodiment of the present disclosure.

[0034] [Figure 9] A control module for controlling the above system, according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0035] In the following description, several specific details are set forth in order to provide a thorough understanding of the present embodiments. The embodiments of the present disclosure may be practiced without some or all of these specific details. In other instances, well-known process operations have not been described in detail so as not to unnecessarily obscure the embodiments of the present disclosure. While the embodiments of the present disclosure will be described in conjunction with specific embodiments, it will be understood that they are not intended to limit the embodiments of the present disclosure.

[0036] Currently, state-of-the-art dielectric etch processes rely on the implementation of one or two RF methods supported by on / off or inter-level RF pulses to combine the benefits of high vertical etch rate and proper sidewall passivation. However, additional methods are identified by embodiments of the present disclosure to independently regain margin or add more margin in the process. Based on such methods, embodiments are provided to embody suitable intermediate states by implementing a multi-state RF pulsing method that overcomes basic process development limitations and barriers in existing etch technologies. The intermediate states promote a more active high energy state (on state / high state) and a more polymerized passivation state (off state / low state) based on preferential trimming of mask neck polymer in the low ion energy state. The introduction of such low ion energy states by source power alone helps control the neck / mask shape. Combining this approach with on-off pulses rather than inter-level pulses allows more polymer to be deposited on the mask and passivated on the mask to control the etch rate of the mask. This approach can essentially destroy the trade-off between mask neck / process margin and selectivity.

[0037] FIG. 1A conceptually illustrates a cross-sectional perspective view of a typical DRAM device 100 according to an embodiment of the present disclosure. A typical DRAM device may be comprised of stacks 1-1.5 microns high, and fabrication of such a DRAM device includes fabrication of a capacitor 102, which necessarily involves a capacitor etch process. Capacitor etch is an example of a dielectric etch process that requires proper etching of features (illustrated conceptually with reference character 104) with very high aspect ratios (e.g., about 60-100 depending on the node). Additionally, pitch sizes are also shrinking smaller and smaller, and the higher the aspect ratio, the less tolerance for defects in the etch process. As a non-limiting example, for capacitor etch, the pitch size may be less than 50 nm. Although embodiments of the present disclosure are described with respect to capacitor etch, it will be appreciated that the principles of the present disclosure may also be applied to the etching of any high aspect ratio dielectric in any suitable device context (e.g., memory hole etch for 3D NAND).

[0038] 1B conceptually illustrates a cross-sectional perspective view of a high aspect ratio etch feature according to an embodiment of the present disclosure. Also conceptualized are several challenges that arise in high aspect ratio etches, such as in the DRAM capacitor fabrication environment as described above. The issues can include bowing of the feature, where a portion of the etch profile becomes concave, twisting of the feature, where the etch direction deviates laterally from a straight vertical direction, critical dimension changes from top to bottom, such as the top of the feature being wider than the bottom, incomplete etching, where the feature is not etched completely to reach its desired endpoint, and inadequate selectivity to the hardmask, where the hardmask is etched away, causing shoulder drop and exacerbating the bowing problem.

[0039] Thus, in high aspect ratio etches, it is desirable to achieve profile control to allow etching of straight features with minimal twist and no warping, and to minimize aspect ratio dependent etching (ARDE). Selectivity to the hard mask is desirable, as is avoidance of incomplete etching (under-etching). Also, wafer uniformity as well as preservation of bottom layer integrity are required.

[0040] FIG. 2A is a graph of RF power versus time for a single pulse RF cycle of an etching process according to an embodiment of the present disclosure. The bias RF power and source RF power over time in a single pulse RF cycle are shown. Current RF pulsing technology uses a two-state pulsing method with level-to-level or on-off pulsing. In such a two-state pulsing method, state 1 (S1) is a high ion energy producing state with the source RF and bias RF at high power, while state 0 (S0) is a low ion energy producing state with the source RF and bias RF at low power or completely off. Since S1 produces high energy ions for surface activation and film etching, the job of S1 is to etch dielectric materials. On the other hand, the main role of S0 is passivation, and S0 is driven mainly with neutrals, which promotes passivation in the etch feature, but there may still be some low energy to continue etching.

[0041] 2B and 2C conceptually represent cross-sectional views of etched features from the S1 and S0 states of the interlevel pulsed process described above, respectively. As shown, S1 is primarily capable of etching high aspect ratio features, but can also cause sputtering of the mask and the formation of a "neck" profile. S0 is primarily capable of passivation, protecting the mask by direct ion deposition and ion-assisted neutral deposition.

[0042] Thus, in inter-level (L2L) pulsed RF, S1 provides high aspect ratio etching but also sputters and forms necks, and S0 provides ion-assisted neutral deposition. Both still cause some necking, and opening the neck becomes more difficult as either moves to higher AR and tighter pitch. In L2L, the most critical dimension occurs at the neck, which tends to constrain the etch when moving to very small feature or pitch sizes. For example, the AR of the neck can be nearly double that of the feature. This acts as a limiter in high aspect ratio etching, as it limits the types of chemicals that can be applied and the amount of current that can be applied to the structure being etched.

[0043] FIG. 3 conceptually represents the tradeoffs in current RF pulsing technology. For example, there are some limitations and constraints when using current interlevel RF pulsing methods in dielectric high aspect ratio contact etching (e.g., DRAM and 3D NAND). In current interlevel pulsing, high power bias (e.g., 400 kHz frequency) is desirable for state 1, but is practically unusable due to hole plugging at high ratios of 400 kHz:60 MHz. Also, chemical adjustments for compensation lead to excessive bowing. For state 0, low power is used to maintain mask selectivity and bowing. High power can improve plugging, but it impairs mask selectivity. Considering these constraints, it is difficult to break the tradeoff in two-state pulsing.

[0044] Thus, current technology encounters limitations in terms of scaling. The taller the stack, the higher the aspect ratio, and the etch rate decreases in the deeper the feature as a function of aspect ratio dependent etch (ARDE). So, to maintain a deep aspect ratio profile, the usual tradeoff is stack etch rate vs. ARDE. For tighter pitches, high ion energy is used to protect against warping and shouldering out of the mask. That is, S1 is manipulated to create high ion energy conditions, causing mask shouldering. On the other hand, to reduce cost at low pitch sizes, manufacturers want to reduce the amount of mask material. Considering the mask and the stacking underneath, cost savings from having less mask material are sought as the industry moves to lower pitches. So selectivity to the mask is important. But the tradeoff for improving selectivity at high aspect ratios is clogging. Holes clog each other, causing device defects.

[0045] So in current RF pulsing methods, these tradeoffs are seen and it is difficult to break the tradeoffs to improve the profile in any one direction.

[0046] However, embodiments of the present disclosure introduce a multi-state RF pulsing method with intermediate states based on the source power only method, which significantly improves the margin vs. selectivity tradeoff, enabling improved etching of high aspect ratio features with good profile and mask selectivity.

[0047] 4A, 4B, and 4C conceptually represent RF power versus time for a multi-state pulsed RF cycle according to an embodiment of the present disclosure. FIG. 4A shows both bias RF power and source RF power. For further clarity, FIG. 4B represents only bias RF power over time, and FIG. 4C represents only source RF power over time. FIG. 4D, 4E, and 4F conceptually represent cross sections of an etch feature, showing the effect of each state of the multi-state pulsed RF cycle described herein. The pulsed RF cycle can be characterized as a three-level pulsed RF using three different states of RF. As shown in the illustrated embodiment, S1 is configured to provide high source power and high bias power. This results in a high aspect ratio (HAR) etch, as shown in FIG. 4D, but also sputters the mask and forms a neck. S0 is configured as an off state with no source or bias power applied. As shown in FIG. 4E, S0 promotes more neutral deposition on the top surface and protects the mask. In some embodiments, S0 is configured to provide direct ion deposition and ion assisted neutral deposition.

[0048] The intermediate state S2 (state 2) is configured as a source power only state (e.g., 60 MHz RF) using low source power and zero bias power. As shown in FIG. 4F, S2 serves to open the neck by inducing separation and etching any necks that are formed. Thus, state S2 is configured to open the neck.

[0049] So, according to the embodiments of the present disclosure, S1 uses high energy ions to create the neck, S2 opens the neck, while S0 provides more passivation. The resulting feature has an open neck, but also a thicker mask with more passivation. This addresses the neck vs. selectivity tradeoff issue.

[0050] In contrast, with an interlevel RF pulsing scheme with only S1 and S0, there will be a lot of passivation, but also some necking that will cause clogging. However, a three-level RF pulsing scheme using S1, S0, and S2 provides open necking and passivation, destroying the selectivity vs. cap margin tradeoff. In general, state S0 provides selectivity, while state S2 improves cap margin.

[0051] Generally, in some embodiments, the bias power is at a frequency of less than about 10 MHz, hi some embodiments, the bias power is at a frequency of about 400 kHz.

[0052] In some embodiments, the source power is at a frequency greater than about 10 MHz. In some embodiments, the source power is at a frequency of about 20 MHz or greater. In some embodiments, the source power is at a frequency of about 60 MHz.

[0053] In some embodiments, the bias frequency and the source frequency are applied to the chuck using different generators.

[0054] It will be appreciated that in various embodiments, the particular parameters of the bias power and the source power may be different for each state.

[0055] In some embodiments, the S1 bias power is in the range of about 5-20 kW. In some embodiments, the S1 source power is in the range of 1-6 kW. In some embodiments, either or both of the S1 bias power and the S1 source power may vary over time, for example depending on the elapsed etch time in the feature, the current depth of the feature, or the current aspect ratio of the feature. In some embodiments, the S1 bias power and / or the S1 source power are configured to increase as the elapsed etch time, depth, or aspect ratio increases.

[0056] In general, the S0 state is an off state where both the bias power and the source power are substantially at zero or near zero levels.

[0057] In some embodiments, the S2 bias power is substantially zero or near zero. In some embodiments, the S2 source power is in the range of about 100 W to 6 kW. In some embodiments, the S2 source power may vary over time, for example, depending on the elapsed etch time in the feature, the current depth of the feature, or the current aspect ratio of the feature. In some embodiments, the S2 source power is configured to increase as the elapsed etch time, depth, or aspect ratio increases.

[0058] It will be appreciated that the relative durations of S1, S0, and S2 may be configured to provide a suitable etch profile and etch rate according to embodiments of the present disclosure, in some embodiments, the duration ratio of S2:S1 ranges from about one to one (1:1) to five to one (5:1).

[0059] In some embodiments, the ratio of durations of S0:S1 is approximately one to one (1:1). In some embodiments, this ratio can vary.

[0060] The relative duration of the various states may depend on the pitch, etch depth, and the parameters being controlled. For example, it may be seen that for a relatively shallow AR etch, S2 does not require a very long time to open up the neck since AR does not play a significant role at the beginning of the etch. However, as the etch gets deeper and a higher AR etch is desired, S2 plays a significant role in opening up the neck to allow for a higher aspect ratio etch.

[0061] FIG. 5 conceptually illustrates the change in length of state S2 over time during a feature etch, according to an embodiment of the present disclosure. Graph 500 of the figure illustrates the duration of S2 versus etch depth / time / aspect ratio. As shown, the duration of S2 increases as the current etch depth in the feature, or the etch time of the feature, or the current aspect ratio of the feature increases. By way of non-limiting example, when the feature has a relatively shallow depth, and therefore a low aspect ratio, such as in the first half of the feature etch (illustrated conceptually by reference character 502), the source RF power profile will be as shown in graph 504, with S2 having a relatively short duration. In contrast, when the feature has a relatively deep depth, and therefore a high aspect ratio, such as in the second half of the feature etch (illustrated conceptually by reference character 506), the source RF power profile will be as shown in graph 505, with S2 having a relatively long duration. 508 It will be as shown in.

[0062] Thus, the higher the aspect ratio, the longer the S2 duration and the more important the neck opening step becomes to maintain the etch profile. S2 The durations of S1, S2, and S0 can all be extended, and S2 can depend on S1 and S0. The source RF current is configured to remove the neck, followed by passivation.

[0063] In the above embodiment, the various states proceeded (and were repeated) in the order S1-S0-S2. Generally, this provides etching (by S1), followed by passivation (by S0), followed by neck opening (by S2).

[0064] However, in other embodiments, S2 may occur between S1 and S0 such that the sequence of states becomes (and repeats) S1-S2-S0, whereby etching is provided (by S1), followed by neck opening (by S2), followed by passivation (by S0).

[0065] 6A, 6B, and 6C depict graphs showing RF power versus time for a multi-state RF pulse cycle according to an embodiment of the present disclosure. FIG. 6A depicts both bias RF power and source RF power over time. For added clarity, FIG. 6B depicts only bias RF power over time, and FIG. 6C depicts only source RF power over time. In the illustrated embodiment, the states proceed in the order S1-S2-S0. As in the previous embodiment, S1 is a high ion energy state with high bias power and high source power. S2 is a source power only state with substantially zero bias power and low source power. S0 is an off state with substantially zero bias power and substantially zero source power.

[0066] Figures 6D, 6E, and 6F conceptually depict cross sections of an etch feature showing the effects of states S1, S2, and S0 according to the embodiment of Figures 6A, 6B, and 6C. As shown in Figure 6D, state S1 produces high ion energy to enable etching of high aspect ratio features, but also causes sputtering of the mask, forming a neck in the feature. As shown in Figure 6E, state S2 produces medium to low ion energy that opens the neck. As shown in Figure 6F, state S0 protects the mask by enabling direct ion deposition and ion-assisted neutral deposition.

[0067] Embodiments of the present disclosure are applicable to dielectric etching, in some embodiments, using fluorine-based chemicals, such as fluorocarbons, hydrofluorocarbons, etc.

[0068] When RF pulsing began, it was operated as an on-off pulse (S1S0). However, this added a lot of passivation, so the industry moved to level-to-level pulsing where some power was added at S0. However, adding more power introduces ions that sputter away the passivation, so this eliminates a lot of the selectivity advantage. However, the three-level multi-state RF pulsing described herein uses a new source-only state that opens the neck while passivation is being used. This destroys the traditional selectivity vs. neck process tradeoff.

[0069] FIG. 7 conceptually illustrates the process window expansion using the multi-state RF pulsing method described herein. Specifically, there is a tradeoff between non-open margin and bridging. The non-open state is indicated by reference character 700 and is a state where HAR etching is not possible due to neck deposition at the feature opening. However, the tradeoff for the non-open state is feature bow, which can cause feature-to-feature bridging that creates open contacts that result in device failure. Thus, the process window between the non-open and bridging states exists, but narrows as CD / pitch sizes decrease with each new / advanced technology node. Therefore, the primary process goal is to achieve bow reduction without sacrificing non-open margin to expand high aspect ratio contact etch capabilities. Improved non-open margin with smaller neck / larger cap margin is required, and improved bridging margin for bow reduction is also required.

[0070] Graph 704 shows plots of failures versus post-etch inspection illustrating the process window for the continuous wave (reference symbol 706), inter-level (reference symbol 708), and tri-level (reference symbol 710) RF pulse methods described herein.

[0071] As pitch sizes have decreased, technology has moved from previous continuous wave (CW) techniques to inter-level pulsing, where the pulses alternate between etching and passivating states, improving the process window for high aspect ratio etching. However, technology has now advanced to the point where the pitch size governs how well high aspect ratio features can be etched. As shown, the three-level RF pulsing technique introduced herein further widens the window for process operation, allowing etching without device failure. As can be seen, the process window is now wide and it becomes possible to control defects within this window.

[0072] As mentioned above, clogging can occur when there is too much polymer in the neck, and clogging or bridging of the feature opening can occur due to too much bowing and holes bridging into one (resulting in an open contact). In continuous wave mode, a shape that mainly clogging the neck may be seen, as shown by reference symbol 712. In inter-level mode, a profile with a larger neck and less bowing is provided, as shown by reference symbol 714, so clogging is controlled, but the process window is quite narrow. However, with a tri-level pulse according to an embodiment of the present disclosure, the profile shown by reference symbol 716 provides a wider opening neck and also a better process window. Faster etch rates and better selectivity are possible because the neck ARDE is mitigated.

[0073] Another advantage is that the three-level RF pulsing method allows for a wider selection of chemistries. Normally, it becomes more difficult to introduce new chemistries as the pitch size gets denser, but by providing a wider process window, it is possible to broaden not only the RF method but also the chemical recipe, allowing the application of a wider variety of passivation chemistries to passivate the sidewalls.

[0074] Various embodiments described herein may be implemented in a plasma processing system. Referring to Figure 8, an exemplary plasma processing system or apparatus includes a chamber 801 having a gas injector / showerhead / nozzle 803 for distributing gases (805, 807, 809) (e.g., reactant and purge gases) or other chemicals, chamber walls 811, and a chuck 813 (which may include electrostatic electrodes for chucking and dechucking the wafer) for holding a substrate or wafer 815 to be processed. The chuck 813 is heated for thermal control, allowing heating of the substrate 815 to a desired temperature. In some embodiments, the chuck 813 may be charged using an RF power source 817 to provide a bias voltage according to embodiments of the present disclosure.

[0075] A source RF power supply 819 is configured to supply source RF power to an electrode of the chuck 813 to generate a plasma 825 in the process space above the substrate 815. In some embodiments, the chamber walls are heated to support temperature management and thermal effects. A vacuum source 827 provides a vacuum to evacuate gases from the chamber 801. The system or apparatus may include a system controller 829 for controlling some or all of the operation of the chamber or apparatus, such as adjusting the chamber pressure, inert gas flow, plasma source power, plasma source frequency, reactive gas flow, bias power, bias frequency, temperature, vacuum settings, and other process conditions.

[0076] In some embodiments, the system / apparatus may include one or more chambers for processing the substrate.

[0077] FIG. 9 illustrates a control module 900 for controlling the above system according to an embodiment of the present disclosure. For example, the control module 900 may include a processor, a memory, and one or more interfaces. The control module 900 may be used to control devices in the system based in part on the sensed values. For example, the control module 900 may control one or more of the values ​​902, the filter heater 904, the pump 906, and other devices 908 based on the sensed values ​​and other control parameters. The control module 900 receives sensed values ​​from, by way of example only, a pressure gauge 910, a flow meter 912, a temperature sensor 914, and / or other sensors 916. The control module 900 may be used to control reactant delivery and process conditions during plasma processing. The control module 900 will typically include one or more memory devices and one or more processors.

[0078] The control module 900 may control the operation of the reactant delivery system and the plasma processing apparatus. The control module 900 executes a computer program that includes a set of instructions for controlling process timing, temperature of the delivery system, pressure differential across the filter, pressure position, mixture of gases, chamber pressure, chamber temperature, wafer temperature, RF power levels, wafer ESC or pedestal position, and other parameters of a particular process. The control module 900 may monitor the pressure differential and automatically switch the delivery of vapor reactants from one or more paths to one or more other paths. In some embodiments, other computer programs stored in a memory device associated with the control module 900 may be used.

[0079] Typically, there will be a user interface associated with the control module 900. The user interface may include a display device 918 (e.g., a display screen and / or graphical software display of equipment and / or process conditions) and a user input device 920 (pointing device, keyboard, touch screen, microphone, etc.).

[0080] Computer programs for controlling reactant delivery, plasma treatment, and other processes in a process sequence can be written in any suitable computer readable programming language (e.g., assembly language, C, C++, Pascal, Fortran, or others). The compiled object code or script is executed by a processor to perform the tasks identified in the program.

[0081] The control module parameters relate to process conditions such as, for example, filter pressure differential, process gas composition and flow rate, temperature, pressure, plasma conditions (such as RF power level and RF frequency), cooling gas pressure, and chamber wall temperature.

[0082] The system software may be designed or configured in many different ways. For example, various chamber component subroutines or control objects may be created to control the operation of the chamber components necessary to carry out the deposition process of the present invention. Examples of programs or program sections for this purpose include substrate positioning code, process gas control code, pressure control code, heater control code, and plasma control code.

[0083] Although the above embodiments have been described in some detail for clarity of understanding, it will be apparent that certain changes and modifications may be made within the scope of the embodiments of the present disclosure. It should be noted that there are many alternative ways of implementing the processes, systems, and apparatus of the present embodiments. Thus, the present embodiments should be considered as illustrative rather than restrictive, and should not be limited to the details described herein. The present disclosure may be realized in the following forms. [Form 1] 1. A method for performing an etch process on a substrate in a plasma processing system, comprising: applying a source RF power to an electrode of the plasma processing system; applying a bias RF power to the electrode; the source RF power and the bias RF power are both pulse signals defining a plurality of multi-state pulse RF cycles, each cycle having a first state, a second state, and a third state; the first state is defined by the source RF power having a first source RF power level and the bias RF power having a first bias RF power level; the second state is defined by the source RF power having a substantially zero power level and the bias RF power having a substantially zero power level; The method of claim 1, wherein the third state is defined by the source RF power having a second source RF power level lower than the first source RF power level and the bias RF power having a substantially zero power level. [Form 2] 2. The method of claim 1, further comprising: The method, wherein the first condition is configured to result in etching of a feature on a surface of the substrate. [Form 3] 3. The method of claim 2, further comprising: The method, wherein the second condition is configured to effect passivation of the features of the surface of the substrate. [Form 4] 3. The method of claim 2, further comprising: The method, wherein the third condition is configured to result in removal of material forming a neck of the feature. [Form 5] 2. The method of claim 1, further comprising: The method, wherein the bias RF power has a frequency less than about 10 MHz. [Form 6] 2. The method of claim 1, further comprising: The method, wherein the source RF power has a frequency greater than about 20 MHz. [Form 7] 2. The method of claim 1, further comprising: The third state has a duration of approximately 1 to 5 times the duration of the first state. [Form 8] 2. The method of claim 1, further comprising: The method, wherein the second state has a duration approximately equal to a duration of the first state. [Form 9] 2. The method of claim 1, further comprising: the first source RF power level is in the range of approximately 1 to 6 kW; The method wherein the first bias RF power level is in the range of approximately 5 to 20 kW. [Form 10] 2. The method of claim 1, further comprising: The method wherein the second source RF power level is in the range of approximately 100 W to 6 kW. [Form 11] 2. The method of claim 1, further comprising: A method wherein within each cycle, the third state immediately follows the second state. [Form 12] 2. The method of claim 1, further comprising: The method, wherein within each cycle, the second state immediately follows the third state. [Form 13] 1. A controller configured to cause a plasma processing system to perform an etching process on a substrate in the plasma processing system, the method comprising: applying a source RF power to an electrode of the plasma processing system; applying a bias RF power to the electrode; the source RF power and the bias RF power are both pulse signals defining a plurality of multi-state pulse RF cycles, each cycle having a first state, a second state, and a third state; the first state is defined by the source RF power having a first source RF power level and the bias RF power having a first bias RF power level; the second state is defined by the source RF power having a substantially zero power level and the bias RF power having a substantially zero power level; The method of claim 1, wherein the third state is defined by the source RF power having a second source RF power level lower than the first source RF power level and the bias RF power having a substantially zero power level. [Form 14] 14. The method of claim 13, further comprising: The method, wherein the first condition is configured to result in etching of a feature on a surface of the substrate. [Form 15] 15. The method of claim 14, further comprising the steps of: The method, wherein the second condition is configured to effect passivation of the features of the surface of the substrate. [Form 16] 15. The method of claim 14, further comprising the steps of: The method, wherein the third condition is configured to result in removal of material forming a neck of the feature. [Form 17] 14. The method of claim 13, further comprising: The method, wherein the bias RF power has a frequency less than about 10 MHz. [Form 18] 14. The method of claim 13, further comprising: The method, wherein the source RF power has a frequency greater than about 20 MHz. [Form 19] 14. The method of claim 13, further comprising: The third state has a duration of approximately 1 to 5 times the duration of the first state. [Form 20] 14. The method of claim 13, further comprising: The method, wherein the second state has a duration approximately equal to a duration of the first state. [Form 21] 14. The method of claim 13, further comprising: the first source RF power level is in the range of approximately 1 to 6 kW; The method wherein the first bias RF power level is in the range of approximately 5 to 20 kW. [Form 22] 14. The method of claim 13, further comprising: The method wherein the second source RF power level is in the range of approximately 100 W to 6 kW. [Form 23] 14. The method of claim 13, further comprising: A method wherein within each cycle, the third state immediately follows the second state. [Form 24] 14. The method of claim 13, further comprising: The method, wherein within each cycle, the second state immediately follows the third state.

Claims

1. 1. A method for performing an etch process on a substrate in a plasma processing system, comprising: applying source RF power to an electrode of the plasma processing system; applying a bias RF power to the electrode; the source RF power and the bias RF power are both pulse signals defining a plurality of multi-state pulse RF cycles, each cycle having a first state, a second state, and a third state; the first state is defined by the source RF power having a first source RF power level and the bias RF power having a first bias RF power level; the second state is defined by the source RF power having a power level of zero and the bias RF power having a power level of zero; the third state is defined by the source RF power having a second source RF power level lower than the first source RF power level and the bias RF power having a zero power level; the first condition is configured to effect etching of a feature on a surface of the substrate; the second condition is configured to provide passivation of the features of the surface of the substrate; The method, wherein the third condition is configured to result in removal of material that forms a neck of the feature.

2. 2. The method of claim 1 , The method of claim 1, wherein the bias RF power has a frequency less than 10 MHz.

3. 2. The method of claim 1 , The method of claim 1, wherein the source RF power has a frequency greater than 20 MHz.

4. 2. The method of claim 1 , The third state has a duration that is 1 to 5 times the duration of the first state.

5. 2. The method of claim 1 , The method of claim 1, wherein the second state has a duration equal to a duration of the first state.

6. 2. The method of claim 1 , the first source RF power level is in the range of 1 to 6 kW; The method of claim 1, wherein the first bias RF power level is in the range of 5 to 20 kW.

7. 2. The method of claim 1 , The method of claim 1, wherein the second source RF power level is in the range of 100 W to 6 kW.

8. 2. The method of claim 1 , A method wherein within each cycle, the third state immediately follows the second state.

9. 2. The method of claim 1 , A method wherein within each cycle, the second state immediately follows the third state.

10. 1. A controller configured to cause a plasma processing system to perform an etching process on a substrate in the plasma processing system, the etching process comprising: applying a source RF power to an electrode of the plasma processing system; applying a bias RF power to the electrode; the source RF power and the bias RF power are both pulse signals defining a plurality of multi-state pulse RF cycles, each cycle having a first state, a second state, and a third state; the first state is defined by the source RF power having a first source RF power level and the bias RF power having a first bias RF power level; the second state is defined by the source RF power having a power level of zero and the bias RF power having a power level of zero; the third state is defined by the source RF power having a second source RF power level lower than the first source RF power level and the bias RF power having a zero power level; the first condition is configured to effect etching of a feature on a surface of the substrate; the second condition is configured to provide passivation of the features of the surface of the substrate; The third state is configured to cause removal of material forming a neck of the feature.

11. The control device according to claim 10, The bias RF power has a frequency less than 10 MHz.

12. The control device according to claim 10, The source RF power has a frequency greater than 20 MHz.

13. The control device according to claim 10, The third state has a duration between 1 and 5 times the duration of the first state.

14. The control device according to claim 10, The second state has a duration equal to the duration of the first state.

15. The control device according to claim 10, the first source RF power level is in the range of 1 to 6 kW; The first bias RF power level is in the range of 5 to 20 kW.

16. The control device according to claim 10, The second source RF power level ranges from 100 W to 6 kW.

17. The control device according to claim 10, The third state immediately follows the second state within each cycle.

18. The control device according to claim 10, Within each cycle, the second state immediately follows the third state.

Citation Information

Patent Citations

  • Apparatus and method for plasma treatment

    JP1999224796A

  • Manufacturing method, manufacturing device and manufacturing program of silicon structure

    JP2009239054A

  • Substrate processing apparatus and substrate processing method

    JP2010238960A

  • Plasma treatment technology for substrates

    JP2013535074A

  • Plasma processing apparatus and plasma processing method

    JP2017069542A