Beam Profile Monitor
Highly oriented graphite probes with aligned graphene sheets address the instability of carbon nanotube probes by providing stable, accurate beam profile measurements under high thermal loads, ensuring precise analysis of charged particle beams.
Patent Information
- Application Number
- JP2021111947
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-31
- Filing Date
- 2021-07-06
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2041-07-06
AI Technical Summary
Existing beam profile monitors using conductive probes face instability and breakdown due to high thermal loads from charged particle beams, particularly when using carbon nanotubes as probes for longitudinal measurements, leading to inaccurate or impossible measurements.
Employing highly oriented graphite probes with a mosaic spread of 10° or less, aligned with the in-plane direction of graphene sheets, to measure beam profiles in both lateral and longitudinal directions, leveraging high thermal conductivity and mechanical strength to withstand high heat loads.
Stable and accurate measurement of beam profiles in all directions is achieved, even under high thermal loads, using highly oriented graphite probes that maintain structural integrity and reduce electron emission, enabling precise beam profile analysis.
Smart Images

Figure 0007564547000002 
Figure 0007564547000003 
Figure 0007564547000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a beam profile monitor that measures the beam profile (spatiotemporal distribution of beam intensity) of a charged particle beam emitted from an accelerator. [Background technology]
[0002] A linear accelerator (LINAC) generates and emits charged particles such as electrons, positrons, and various ions as high-energy, high-intensity beams. In these beams, the charged particles are accelerated vertically at a constant rate and converged horizontally, and are periodically emitted as a bunch. The output beam is used in various physics experiments and medical applications, and in these cases it is required to recognize the three-dimensional intensity distribution (three-dimensional beam profile) of the beam (bunch) and optimize it for the purpose. In this case, the measured intensity corresponds to the distribution of charged particles within the bunch.
[0003] In Fig. 8, a situation where bunch B is repeatedly emitted is shown. Here, the traveling direction of the charged particle beam (bunch B) is the z direction (longitudinal direction), and the directions perpendicular to this (horizontal direction) are the x and y directions. Here, it is required to measure, for example, the intensity distribution of bunch B in the x and y planes (horizontal intensity distribution) and the intensity distribution of bunch B in the z plane (longitudinal intensity distribution).
[0004] For example, Patent Document 1 and the like disclose the configuration of a beam profile monitor for measuring a beam profile in the transverse direction. Figure 9 shows this principle in a simplified manner. Here, a conductive probe (wire) 80 and a current measurement system 90 for measuring a current induced therein are used. Here, it is assumed that the shape of the beam (bunch B) in the transverse direction is a simple ellipse.
[0005] In this configuration, the beam profile along the x direction is measured by moving the probe 80 extending in the y direction along the x direction. When the probe 10 is irradiated with a beam of charged particles, secondary electrons are emitted, and a current proportional to the amount of these secondary electrons is induced, and this current is measured by a current measurement system 90. Since the amount of these secondary electrons is proportional to the amount of charged particles irradiated onto the probe 80, if the charged particle density within bunch B is uniform, then in FIG. 9, the amount of secondary electrons is proportional to the length of the range irradiated by the beam on the probe 80, that is, the width of the beam along the y direction at the position where the probe 80 is placed. For example, the current intensity when the probe 80 is at position a is expressed as I a , the current intensity at position b is I b Then, I b >I a It becomes.
[0006] 9, the probe 80 can be moved, for example, from the positive side to the negative side in the x direction, and the current (current intensity) flowing through the probe 80 can be measured accordingly, and the beam profile in the x direction is measured as a current intensity distribution, as shown in the lower part of the figure. Instead of moving the probe 80, multiple probes 80 may be provided along the x direction, and the current intensity in each may be measured to measure the current intensity distribution along the x direction. Similarly, the beam profile in the y direction can be measured by moving the probe 80 extending in the x direction along the y direction, or by providing multiple probes along the y direction. The probe 80 is preferably thin in order to increase the resolution of the measurement, and has a diameter of 1 mm or less.
[0007] The probe 80 is used in the above-mentioned manner and is irradiated with high-energy charged particles, so that it is prone to breakage during use due to mechanical and thermal loads. For this reason, the material constituting it is required to have high electrical conductivity, as well as high mechanical strength and high heat resistance. An example of a material that satisfies such requirements is tungsten (W). On the other hand, since W has a high density, the energy loss of the beam (energy absorbed by the probe) is large and its thermal conductivity is low, when the beam intensity is high or when the beam is slow and the thermal load due to the interaction with the probe is large, the W wire that is the probe may break. For this reason, in the above-mentioned cases, carbon nanotubes (CNTs), which are electrically conductive, have a lower density, and are equally mechanically strong and heat-resistant, are used as an alternative material to W. This allows measurements to be made when the thermal load from the beam is larger than when W is used.
[0008] On the other hand, a method for measuring a beam profile in the vertical direction is described in, for example, Non-Patent Document 1. Fig. 10 shows a simplified version of the principle. Here, the z direction in Fig. 8 is the up-down direction. A conductive probe (wire) 180 is also used in this case, but since this probe 180 extends in the direction perpendicular to the paper surface in Fig. 10, it is depicted as a dot in Fig. 10. As in the above, secondary electrons are emitted from this probe 180 by irradiation with charged particles, but in this measurement method, the secondary electrons emitted to the outside from the probe 180 are measured.
[0009] For this reason, a negative potential is applied to the probe 180 to emit secondary electrons. These secondary electrons are emitted in all directions, and a part of them, secondary electrons S, pass between a pair of RF (radio frequency) deflector electrodes 130 after passing through the collimator 120. A voltage is applied between the RF deflector electrodes 130 in which an AC voltage that changes at the acceleration frequency of the accelerator (the repetition frequency of bunch B) is superimposed on an electrostatic lens voltage that converges the secondary electrons S on the downstream collimator 140. For this reason, the secondary electrons S are scanned on the surface of the collimator 140 according to the phase during acceleration. As a result, only the secondary electrons S at a specific phase pass through the collimator 140, and can be detected by the electron detector 150. This phase corresponds to a position along the z direction (vertical direction) in bunch B in FIG. 8.
[0010] In reality, in addition to the secondary electrons generated by the charged particles as described above, background electrons that should not be measured are also emitted from the probe 180 at the same time. Since the energy of such electrons is significantly different from the energy of the secondary electrons S to be measured, in Fig. 10, a deflection electromagnet 160 is provided downstream of the collimator 140, which applies a DC magnetic field perpendicular to the paper surface. This magnetic field makes it possible to set an orbit in which electrons that should not be measured are not incident on the electron detector 150, and only the secondary electrons S to be measured are incident on the electron detector 150.
[0011] This allows the intensity of secondary electrons of a specific phase to be measured by the electron detector 150, and by identifying the intensity of secondary electrons for each phase, the longitudinal beam profile of the charged particle beam (bunch B) can be measured. [Prior art documents] [Patent documents]
[0012] [Patent Document 1] Utility model registration No. 3105335 [Non-patent literature]
[0013] [Non-Patent Document 1] Akihiko Miura, Alexander V. Feschenko, Alexander N. Mirzojan, Tomoaki Miyao, Nobuo Ouchi, Hidetomo Oguri, Kazuo Hasegawa, Masaki Ikegami, "Development of a Bunch Shape Monitor for the J-PARC Linac", Proceedings of the 10th Annual Meeting of Particle Accelerator Society of Japan, SAP088, August 2013. Summary of the Invention [Problem to be solved by the invention]
[0014] In this way, since conductive probes are used in both the horizontal and vertical directions, in principle, it is possible to use a common probe for the probe 80 in Fig. 9 and the probe 180 in Fig. 10, in which case a common probe (measuring device) can be used to measure the three-dimensional (horizontal and vertical) beam profile of the charged particle beam. For this reason, when the heat load due to the interaction from the beam is low, a W probe can be used as the probe 80 in Fig. 9 and the probe 180 in Fig. 10, as described above.
[0015] On the other hand, when the thermal load due to the interaction with the beam is large, as described above, CNTs are preferably used as the material constituting the probe 80 for measuring the lateral beam profile. However, CNTs are known as electron-emitting materials that serve as electron sources, and emit many electrons when a voltage is applied in a vacuum. For this reason, when CNTs are used as the material of the probe 180 in FIG. 10 and a negative voltage is applied to the probe 180, many electrons are emitted from the probe 180 in addition to the secondary electrons caused by the irradiation of the charged particle beam. Such electrons other than the secondary electrons that are the subject of measurement not only become background components of the measurement, but also cause discharge between the probe 180 and the surroundings, and this discharge may cause the probe 180 to overheat and break, making it difficult to measure the secondary electrons.
[0016] For this reason, even when the thermal load of the probe due to the interaction with the charged particle beam is large, it has been difficult to stably measure the beam profile of the charged particle beam.
[0017] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide an invention that solves the above problems. [Means for solving the problem]
[0018] In order to solve the above problems, the present invention has the following configuration. The beam profile monitor of the present invention is a beam profile monitor using a conductive probe that extends in a direction intersecting the traveling direction of a charged particle beam and is used to measure the beam profile of the charged particle beam based on the characteristics when irradiated with the charged particle beam, and the probe is made of highly oriented graphite with a mosaic spread value of 10° or less. The traveling direction is the in-plane direction of the graphene sheets constituting the highly oriented graphite. Characterized by 。 In the beam profile monitor of the present invention, the extension direction of the probe is set to an in-plane direction of a graphene sheet constituting the highly oriented graphite. The beam profile monitor of the present invention is a beam profile monitor that uses a conductive probe that extends in a direction intersecting the traveling direction of a charged particle beam and is used to measure the beam profile of the charged particle beam based on its characteristics when irradiated with the charged particle beam, and is characterized in that the probe is made of a graphite material that has anisotropy in thermal conductivity and has a thermal conductivity of 1000 W / (m·K) or more along a direction in which the thermal conductivity is high, and the traveling direction is the direction in which the thermal conductivity is high. The beam profile monitor of the present invention is characterized in that a current induced in the probe when the probe is irradiated with the charged particle beam is measured according to the position of the probe along a direction intersecting the propagation direction and the extension direction of the probe, thereby measuring a beam profile in a direction perpendicular to the propagation direction of the charged particle beam. The beam profile monitor of the present invention is characterized in that the intensity of secondary electrons emitted from the probe when the probe is irradiated with the charged particle beam is measured according to the position of the probe along a direction intersecting the propagation direction and the extension direction of the probe, thereby measuring a beam profile in a direction perpendicular to the propagation direction of the charged particle beam. The beam profile monitor of the present invention is characterized in that the intensity of secondary electrons emitted from the probe when the probe is irradiated with the charged particle beam is measured according to the phase within a period of the periodically emitted charged particle beam, thereby measuring a beam profile in a direction along the propagation direction of the charged particle beam. The beam profile monitor of the present invention is characterized in that a current value of the charged particle beam is calculated from an integral value of the beam profile in a direction perpendicular to the traveling direction of the measured charged particle beam. Effect of the Invention
[0019] Since the present invention is configured as described above, it is possible to stably measure the beam profile of a charged particle beam even when the thermal load of the probe due to the interaction with the charged particle beam is large. [Brief description of the drawings]
[0020] [Figure 1] FIG. 1 is a diagram showing a configuration of a beam profile monitor according to an embodiment of the present invention. [Diagram 2] 2A to 2C show two typical examples of the microstructure of a probe used in a beam profile monitor according to an embodiment of the present invention. [Diagram 3] This shows the results of measuring the applied voltage dependence of pressure (a) and leakage current (b) when a probe made of highly oriented graphite (Example) and a wire-shaped probe made of CNT (Comparative Example) were placed in a vacuum. [Figure 4] 1 shows the results of measuring the beam profile in the horizontal direction (a) and vertical direction (b) in the embodiment. [Diagram 5] This is an example of a comparison of the lateral beam profile of a charged particle beam measured using a probe induced current and the secondary electron measurement. [Figure 6] 11 shows a result of comparing a current value of a charged particle beam measured by a conventional method with a current value measured using a beam profile monitor according to an embodiment of the present invention. [Figure 7] 1 shows the results of measuring the spatial shape of a charged particle beam using a beam profile monitor according to an embodiment of the present invention. [Figure 8] FIG. 2 is a diagram illustrating a schematic view of a charged particle beam to be measured when it is emitted from an accelerator. [Figure 9] 1 is a diagram showing the principle of measuring a lateral beam profile of a charged particle beam using a probe. [Figure 10] FIG. 1 is a diagram showing a configuration for measuring a longitudinal beam profile of a charged particle beam using a probe. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] A beam profile monitor according to an embodiment of the present invention will be described below. FIG. 1 is a diagram showing a schematic configuration of this beam profile monitor 1. A bunch B of a charged particle beam passes through the inside of a duct 20, which extends in a direction perpendicular to the paper and has a high or ultra-high vacuum inside, in a direction perpendicular to the paper, either upward or downward. This bunch B is the measurement target for the beam profile (three-dimensional charged particle distribution in bunch B). Bunch B is generated at a constant oscillation frequency by a linear accelerator (LINAC). Note that, for convenience, the x, y, and z axes are shown in FIG. 1 at a distance from the duct 20 (bunch B), but in reality, the z axis coincides with the central axis of the duct 20 (bunch B) perpendicular to the paper.
[0022] Here, similarly to the configuration of FIG. 9, conductive probes 10A and 10B are used, and the current induced in each of them during beam irradiation can be measured by a current measurement system 90. Here, the probe 10A extending along the y-axis direction is scanned in the x-direction to irradiate bunch B, and the current at this time is monitored to obtain a beam profile in the x-direction. Similarly, the probe 10B extending along the x-axis direction is scanned in the y-direction to irradiate bunch B, and the current at this time is monitored to obtain a beam profile in the y-direction. This is the same as in FIG. 9. When the beam profile is not being measured, the probe 10A waits in a vacuum on the positive side of the x-direction as seen from the duct 20, and the probe 10B waits in a vacuum on the negative side of the y-direction as seen from the duct 20. Their positions are controlled, for example, in mm units. This allows the beam profile in the lateral directions (x and y directions) of the charged particle beam to be measured.
[0023] On the other hand, in Fig. 1, to the left of the duct 20, a collimator 30, an RF deflector electrode 40, a collimator 50, an electron detector 60, and a deflection electromagnet 70 are provided for measuring the beam profile in the vertical direction, similarly to the collimator 120, the RF deflector electrode 130, the collimator 140, the electron detector 150, and the deflection electromagnet 160 in Fig. 10. When measuring the beam profile in the vertical direction, the probe 10A or the probe 10B is installed at a position where it is irradiated with the charged particle beam while a negative potential is applied, and for example, the probe 10A measures the distribution of the beam intensity in the z direction corresponding to the integral value of the amount of charged particles in the bunch B along the x direction. Similarly, the collimator 30, the RF deflector electrode 40, the collimator 50, the electron detector 60, and the deflection electromagnet 70 are arranged to face the probe 10B, whereby the distribution of the beam intensity in the z direction corresponding to the integral value of the amount of charged particles in the bunch B along the y direction is measured. The position of the bunch B in the z direction, which is the measurement point at this time, is adjusted by the phase of the high frequency applied to the RF deflector electrode 130, similarly to the configuration of Fig. 10. That is, with this configuration, the intensity of the secondary electrons S is measured by the electron detector 60, thereby measuring the beam profile of the charged particle beam in the vertical direction (z direction). This operation is as described in Non-Patent Document 1.
[0024] At this time, the position dependence of the intensity of the secondary electrons S in the x direction of the probe 10A and the position dependence in the y direction of the probe 10B can also be measured. These correspond to the beam profile in the x direction and the beam profile in the y direction of the charged particle beam, respectively. At this time, by adjusting the high frequency applied to the RF deflector electrode 130, these lateral beam profiles can be made to be at a certain point (a certain phase) in the z direction, and can also be made to be integral values in a certain range (for example, one period) in the z direction.
[0025] That is, the beam profile monitor 1 in Fig. 1 measures the beam profiles in the horizontal and vertical directions using a common probe 10A or probe 10B. The probes 10A and 10B used here are configured to enable such measurements even when the thermal load caused by the interaction with the charged particle beam is particularly large. This point will be explained below.
[0026] The probes 10A and 10B are made of highly oriented graphite. Highly oriented graphite is graphite that has a strong orientation corresponding to the layered structure of the graphene sheet, and generally is graphite that has a high orientation in the c-axis direction. Specifically, as described in, for example, Japanese Patent No. 6364404, the degree of this orientation is expressed by an angle (mosaic spread) corresponding to the half-width of the c-axis peak of graphene in X-ray diffraction, and a mosaic spread of 10° or less is particularly preferable for the probes 10A and 10B. Such orientation can be adjusted by the manufacturing conditions.
[0027] The density, thermal conductivity, and melting point of the three materials used as the probe material in the beam profile monitor, highly oriented graphite, CNT, and tungsten (W), as mentioned above, are shown in Table 1. It is known that the thermal conductivity of CNT in the length direction of the nanotube is equal to or greater than that of highly oriented graphite in the in-plane direction, but the only form of wire (probe) used here that can be realized is sintered CNT powder, so the actual thermal conductivity is low.
[0028] [Table 1]
[0029] As shown here, in highly oriented graphite, various properties are highly anisotropic due to its high degree of orientation, and the thermal conductivity differs greatly between the in-plane direction of the laminated structure (the direction perpendicular to the c-axis direction, which is the lamination direction of the graphene sheets) and the lamination direction, with the thermal conductivity being particularly high in the in-plane direction. Therefore, when such highly oriented graphite is used for probes 10A and 10B, the crystal orientation of the graphene therein can be set according to the aspect of probes 10A and 10B so that breakage, etc., is unlikely to occur during use.
[0030] In FIG. 1, the probes 10A and 10B are the same except that their orientations are different by 90°, so only the probe 10A will be described below. When a high-intensity charged particle beam is irradiated, the probe 10A is heated and is likely to break due to the high temperature. In order to reduce the effects of such heat, it is preferable that the probe 10A has high thermal conductivity and high heat dissipation efficiency, and this heat is generated along the incident direction (z direction) of the charged particle beam. For this reason, it is preferable that the thermal conductivity in the z direction is particularly high.
[0031] As described above, in a stacked structure of graphene sheets, the thermal conductivity along the in-plane direction of the graphene sheets is higher than the thermal conductivity along the stacking direction (c-axis direction). Therefore, it is preferable to align the incident direction of the charged particle beam (z direction) with the in-plane direction of the graphene.
[0032] A typical microstructure of the probe 10A in this case is shown in Fig. 2(a)(b). Here, a structure in which single-layer graphene sheets G are stacked is shown. Here, it is assumed that the probe 10A has an ideal graphene stacked structure (the mosaic spread is zero). In both cases, a cross section perpendicular to the plane of the graphene sheet G is shown. The direction in which the graphene sheets G are stacked is the c-axis direction, and in Fig. 2(a), the c-axis direction is the x-direction (perpendicular to the extension direction of the probe 10A and the traveling direction of the charged particle beam), and in Fig. 2(b), the c-axis direction coincides with the y-direction (the extension direction of the probe 10A).
[0033] On the other hand, the graphene laminate structure also has a large anisotropy in mechanical strength. The graphene sheet G has a high mechanical strength in the in-plane direction because it is composed of carbon bonds, whereas the graphene sheet G has a low mechanical strength in the c-axis direction because it is bonded by intermolecular forces. For this reason, in the structure of FIG. 2(b), the mechanical strength of the probe 10A in the extension direction (y direction) is low, and the probe 10A is likely to break. In contrast, in the structure of FIG. 2(a), the extension direction is the in-plane direction of the graphene sheet G, so the mechanical strength along the extension direction is high. In addition, as shown in FIG. 1, the probe 10A is provided in a vacuum with both ends in the extension direction (y direction) fixed, so that in order to increase the heat dissipation efficiency, it is preferable that the thermal conductivity in the y direction is particularly high. In the structure of FIG. 2(a), the y direction is also the in-plane direction of the graphene sheet G, so that the thermal conductivity along the y direction can be increased.
[0034] For this reason, the structure of Fig. 2(a) is particularly preferable for the probe 10A. The specific shape of the probe 10A having such a structure does not need to be a cylindrical shape that is symmetrical about the stretching direction, but may be a long and narrow rectangular shape with at least one surface coinciding with the surface of the graphene sheet G, and the processing direction is appropriately set according to the shape. In the case of highly oriented graphite, such a setting is possible due to its high orientation. That is, a narrow thin film sheet can be used for the probes 10A and 10B.
[0035] In FIG. 2, the graphite constituting the above-mentioned probes 10A and 10B is described as a laminate of ideal graphene sheets G, which corresponds to the case where the mosaic spread is zero. On the other hand, while the thermal conductivity of general graphite, which has no anisotropy in thermal conductivity, is 100 W / (m·K), the thermal conductivity of the highly oriented graphite in Table 1 is significantly higher than this in the in-plane direction (the direction that should be the z direction) and significantly lower than this in the stacking direction. More generally, any graphite that has high thermal conductivity along a specific direction (the direction that should be the z direction) as described above can be used as the material constituting the probes 10A and 10B in the same way.
[0036] A general characteristic required for this purpose is that the thermal conductivity of this graphite is anisotropic, and that the thermal conductivity in the direction in which the thermal conductivity is high (corresponding to the in-plane direction mentioned above) is 1000 W / (m·K) or more. For example, the thermal conductivity of copper, a metal material with high thermal conductivity, is not anisotropic, and its value is 403 W / (m·K), which is significantly lower than 1000 W / (m·K). For this reason, if a graphite material with such characteristics is used as the material constituting the probes 10A and 10B and the direction in which the thermal conductivity is high is aligned with the traveling direction of the charged particle beam, it is clear that this will be effective regardless of the mosaic spread.
[0037] The characteristics of a probe using the above-mentioned highly oriented graphite when actually used in the configuration of FIG. 1 will be described below. The mosaic spread of the highly oriented graphite used here is about 5°, and the average grain size is about 500 μm. Here, the results of a comparison with CNT, which is particularly suitable as a probe material when measuring the lateral beam profile of a high-intensity charged particle beam as described above, will be described. Here, both ends of the probe were fixed to tungsten plates that were sufficiently wider than the probe, and the current induced in the probe was measured.
[0038] Figures 3(a) and (b) show the results of measuring the pressure change (a) and leakage current (b) when a negative voltage is applied to probes made of these materials while they are held in a vacuum. The leakage current is a current caused by discharge, separate from the current flowing between both ends of the probe. A probe made of highly oriented graphite (HOPG) with a length of 50 mm (Example) and a CNT probe with a length of 16 to 125 mm (Comparative Example) were used here. The c-axis of the HOPG was oriented in the direction of incidence of the charged particle beam.
[0039] As can be seen from Figures 3(a) and (b), when a high voltage is applied to CNTs, the pressure rise and leakage current increase are particularly noticeable. This is due to electron emission (field emission) from the CNTs when voltage is applied. For this reason, it is difficult to apply a negative voltage of, for example, 10 kV to a CNT probe. In contrast, with a HOPG probe, both the pressure rise and leakage current are kept small, making it possible to apply a voltage of about 10 kV without generating a discharge.
[0040] FIG. 4 shows the results of (a) measuring the beam profile in the horizontal direction (x direction) and (b) determining the beam profile in the vertical direction (z direction) by measuring the current flowing through the probe 10A using the highly oriented graphite as described above with the current measuring system 90 as described above. In FIG. 4(a), the width of the probe 10A is set to 1 mm, and the position resolution corresponding to this width is about 300 μm in the horizontal direction. In FIG. 4(b), the width of the probe 10A is set to 0.2 mm, and the applied voltage during the measurement of the beam profile in the vertical direction is set to −10 kV. The charged particle beam is a negative hydrogen ion beam with an energy of 3 MeV and a peak current of 55 mA, and the oscillation frequency of the linear accelerator is 324 MHz.
[0041] In Fig. 4(a), which shows the beam profile in the lateral direction, the measurement results (beam intensity distribution and standard deviation σ) using the highly oriented graphite probe and the measurement results using the CNT probe are shown together with the results obtained by simulation. From this result, the measurement results using the highly oriented graphite probe and the CNT probe match within the error range, and it is presumed that these results reflect the actual beam profile. Furthermore, no high voltage was applied to the probe during this measurement, and no abnormalities were found in either probe after the measurement, and this measurement could be repeated.
[0042] On the other hand, in Fig. 4(b) showing the beam profile in the vertical direction, only the measurement results using the highly oriented graphite probe and the results obtained by simulation are shown because the CNT probe was broken by applying a voltage of -10 kV and measurement was impossible. Here, a width of 1° in the phase corresponds to a time width of 8.6 ps, corresponding to the above-mentioned oscillation frequency. The vertical resolution is determined depending on the deflection angle of the secondary electrons by the RF deflector 40, the focusing diameter, etc., and is about 1°. The actual measurement value and the simulation result match with high accuracy, and it was confirmed that it is possible to measure the beam profile in the vertical direction as well as the horizontal direction using the highly oriented graphite probe. The absorbed energy of the probe (width 0.2 mm) during irradiation under these conditions is 0.3 J per unit macrobunch of 50 μs length, which is a collection of bunches (macrobunch) irradiated every 3 ns.
[0043] In this way, the beam profile monitor using a probe made of highly oriented graphite can measure the transverse and longitudinal beam profiles of a charged particle beam. The beams of electrons, positrons, mesons, muons, protons, various ions (light ions, heavy ions), etc., as well as electromagnetic waves that have similar interactions, can be measured, and the beam profile can be measured even when the beam intensity is high or when the beam is slow and the thermal load due to the beam interaction is large. The length, diameter (width), etc. of the probe can be set appropriately depending on the spread of the charged particle beam and the equipment configuration, etc.
[0044] In Fig. 4(a), the beam profile along the x direction was measured by measuring the current flowing through the probe 10A with the current measurement system 90. Meanwhile, as described above, the beam profile in the lateral direction (x direction) can also be measured by measuring the secondary electrons emitted from the probe 10A with the electron detector 60 instead of measuring the current flowing through the probe 10A. Fig. 5 shows an example comparing the result of measuring the lateral profile with the induced current of the probe as described above with the result of measuring the same lateral profile with secondary electrons. From this result, it is clear that there is no significant difference between the two, and a lateral profile can be obtained by either method.
[0045] Also, the current value of the charged particle beam is generally measured by measuring the magnetic field generated by the current of the charged particle beam, as described in, for example, Chihiro Omori and Mitsutaka Kanazawa, "New Beam Monitor for Synchrotrons," National Institute of Radiological Sciences NEWS, No. 135, February 2008 (https: / / www.nirs.qst.go.jp / publication / nirs_news / 200802 / hik08p.htm). However, if the beam profiles in the horizontal and vertical directions can be measured, for example, as described above, these three-dimensional integral amounts can be made to correspond to the beam current. Alternatively, if the beam profile in the horizontal direction is taken as the integral value in one period as described above, the integral value of this beam profile in the horizontal direction corresponds to the current value. In other words, the above beam profile monitor can also be used to measure the current value of the charged particle beam.
[0046] FIG. 6 shows the relationship between the current value of the charged particle beam measured by the conventional method and the current value calculated by using the above-mentioned beam profile monitor. Here, the current value measured by using the above-mentioned beam profile monitor is smaller at low currents. This is because, when using the above-mentioned beam profile monitor, the current value is calculated as the integral value of the Gaussian distribution, which is the beam shape of the original charged particle beam, as shown in FIG. 5, while in the conventional method, components other than the Gaussian distribution component (halo component) are also measured without distinction. When the accelerator is actually used, this halo component is removed later, or does not contribute to the experimental results in which this charged particle beam is used, and only the Gaussian distribution component is important. Therefore, the above-mentioned beam profile monitor measures the current value of only the substantially effective component, which is more practically preferable in this respect than the conventional method.
[0047] Furthermore, as mentioned above, if both the horizontal (x and y) and vertical (z) beam profiles are measured, the spatial shape of the charged particle beam is finally measured. In other words, this spatial shape can be measured by adjusting the phase of the radio frequency to obtain the beam profile in the z direction for each position in the x direction (or y direction). Figure 7 shows the measurement results, with the vertical axis corresponding to the position in the x direction and the horizontal axis corresponding to the time corresponding to the phase and the position on the z axis. This shape corresponds to the shape of a single bunch in the xz plane.
[0048] 1, the travel distance of the secondary electrons emitted by the probe 10A to the electron detector 60 has a position dependency in the x direction. Since the energy of these secondary electrons is lower than the energy of the charged particle beam, when the travel distance is long, they are detected by the electron detector 60 with a significant delay compared to when the travel distance is short. In FIG. 7, the effect of this time difference is corrected.
[0049] The measurement results shown in FIGS. 5 to 7 were obtained only when using a probe made of HOPG, which does not cause an increase in pressure or leakage current, as shown in FIG.
[0050] In the above example, the traveling direction of the charged particle beam, the extension direction of the probe, and the scanning direction of the probe when measuring the beam profile in the lateral direction are perpendicular to each other. However, these do not need to be strictly perpendicular to each other, and the measurement can be performed in the same way even if they intersect at an angle other than perpendicular. In other words, the relationship between these can be set appropriately as long as the beam profile can be measured in the same way.
[0051] In addition, the configuration for measuring the current induced in the probe to measure the horizontal beam profile and the configuration for measuring the secondary electrons emitted from the probe to measure the vertical beam profile may be different from those shown in Figures 1, 9, and 10, respectively. [Explanation of symbols]
[0052] 1 Beam profile monitor 10A, 10B Probe 20 Duct 30, 50, 120, 140 collimator 40, 130 RF deflector electrode 60, 150 Electronic detector 70, 160 bending magnet 80, 180 Probe (wire) 90 Current measurement system B Bunch G Single-layer graphene sheet S Secondary electron
Claims
1. A beam profile monitor using a conductive probe that extends in a direction intersecting a traveling direction of a charged particle beam and is used to measure a beam profile of the charged particle beam based on a characteristic when the conductive probe is irradiated to the charged particle beam, The probe is made of highly oriented graphite having a mosaic spread value of 10° or less; A beam profile monitor, characterized in that the traveling direction is an in-plane direction of a graphene sheet that constitutes the highly oriented graphite.
2. 2. The beam profile monitor according to claim 1, wherein the extension direction of the probe is an in-plane direction of a graphene sheet constituting the highly oriented graphite.
3. A beam profile monitor using a conductive probe that extends in a direction intersecting a traveling direction of a charged particle beam and is used to measure a beam profile of the charged particle beam based on a characteristic when the conductive probe is irradiated to the charged particle beam, The probe is made of a graphite material having anisotropy in thermal conductivity, and a thermal conductivity along a direction in which the thermal conductivity is high is 1000 W / (m·K) or more; A beam profile monitor, characterized in that the traveling direction is a direction in which the thermal conductivity is high.
4. 4. The beam profile monitor according to claim 1, wherein a current induced in the probe when the probe is irradiated with the charged particle beam is measured according to a position of the probe along a direction intersecting the propagation direction and an extension direction of the probe, thereby measuring a beam profile of the charged particle beam in a direction perpendicular to the propagation direction of the charged particle beam.
5. 4. The beam profile monitor according to claim 1, wherein an intensity of secondary electrons emitted from the probe when the probe is irradiated with the charged particle beam is measured according to a position of the probe along a direction intersecting the propagation direction and an extension direction of the probe, thereby measuring a beam profile of the charged particle beam in a direction perpendicular to the propagation direction.
6. 5. The beam profile monitor according to claim 1, wherein an intensity of secondary electrons emitted from the probe when the probe is irradiated with the charged particle beam is measured according to a phase within a period of the periodically emitted charged particle beam, thereby measuring a beam profile in a direction along the traveling direction of the charged particle beam.
7. 6. The beam profile monitor according to claim 4, wherein a current value of the charged particle beam is calculated from an integral value of a beam profile in a direction perpendicular to the traveling direction of the measured charged particle beam.
Citation Information
Patent Citations
Graphite laminar sheet material and method for manufacturing the same
JP2002308611A
Electrode for quantum beam monitor and quantum beam monitor system
JP2007101367A
Nanowire crosslinking device utilizable for shape measurement of electron beam
JP2008256526A
Pyrolytic graphite tube device for directional heat management
JP2019526016A
Highly conductive graphite film and manufacturing method
JP2019532889A