Substrate Processing Chamber

The substrate processing chamber with a resonant cavity and magnetic assembly addresses the etch selectivity and deposition rate challenges of hardmask materials, enhancing film deposition and reducing stress for improved semiconductor manufacturing.

JP7565947B2Active Publication Date: 2024-10-11APPLIED MATERIALS INC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2021569407
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-08-19
Filing Date
2020-05-18
Publication Date
2024-10-11
Estimated Expiration
2040-05-18

AI Technical Summary

Technical Problem

Current hardmask materials used in semiconductor manufacturing lack desired etch selectivity and deposition rates, especially as critical dimensions decrease, leading to insufficient protection of underlying layers during pattern transfer processes.

Method used

A substrate processing chamber with a resonant cavity, magnetic assembly, and movable substrate support, utilizing dual frequency RF power sources and adjustable substrate positioning, along with a flexible equipment cable and electrostatic chuck, to enhance film deposition and reduce neutral stress.

Benefits of technology

The solution achieves improved film deposition with reduced neutral stress, leading to better planarity and accuracy in substrate processing, addressing the challenges of etch selectivity and deposition rate issues in hardmask materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007565947000001
    Figure 0007565947000001
  • Figure 0007565947000002
    Figure 0007565947000002
  • Figure 0007565947000003
    Figure 0007565947000003
Patent Text Reader

Abstract

FIELD OF THE DISCLOSURE Embodiments of the present disclosure generally relate to apparatus and methods utilized in the manufacture of semiconductor devices. More particularly, embodiments of the present disclosure relate to substrate processing chambers for forming semiconductor devices, as well as components thereof.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE

[0002] Embodiments of the present disclosure relate generally to apparatus and methods utilized in the manufacture of semiconductor devices. More particularly, embodiments of the present disclosure relate to substrate processing chambers and components thereof for forming semiconductor devices. [Background technology]

[0002] Integrated circuits have evolved into complex devices capable of incorporating millions of transistors, capacitors, and resistors on a single chip. The evolution of chip designs continues to include faster circuits and higher circuit density. The demand for faster circuits with higher circuit density places similar demands on the materials used in the manufacture of such integrated circuits. In particular, as the dimensions of integrated circuit components shrink to the sub-micron scale, there is a trend to use conductive materials with low resistivity, as well as insulating materials with low dielectric constant, to obtain adequate electrical performance from such components.

[0003] The demand for higher integrated circuit density also places demands on the process sequences used to manufacture integrated circuit components. For example, in a process sequence using conventional photolithography techniques, a layer of energy sensitive resist is formed on a stack of material layers disposed on a substrate. The energy sensitive resist layer is exposed to an image of a pattern to form a photoresist mask. The mask pattern is then transferred to one or more material layers of the stack using an etching process. A chemical etchant used in the etching process is selected to have a higher etch selectivity for the material layers of the stack than the energy sensitive resist mask. That is, the chemical etchant etches the one or more layers of the material stack at a much faster rate than the energy sensitive resist. The etch selectivity for one or more material layers of the stack on the resist prevents the energy sensitive resist from being consumed before the pattern transfer is complete.

[0004] As the dimensions of the patterns are scaled down, the thickness of the energy sensitive resist is correspondingly reduced to control the resolution of the patterns. Such a thin resist layer may be insufficient to mask the underlying material layer during the pattern transfer process due to attack by chemical etchants. An intermediate layer called a hard mask (e.g., silicon oxynitride, silicon carbine, or carbon film) is often used between the energy sensitive resist layer and the underlying material layer to facilitate the pattern transfer due to its high resistance to chemical etchants. Hard mask materials that have both high etch selectivity and high deposition rate are often utilized. As critical dimensions (CDs) decrease, current hard mask materials often lack the desired etch selectivity compared to the underlying materials (e.g., oxides and nitrides) and are difficult to deposit. Thus, there is a need in the art for improved methods and apparatus for fabricating semiconductor devices. Summary of the Invention

[0005] FIELD OF THE DISCLOSURE Embodiments of the present disclosure relate generally to apparatus and methods utilized in the manufacture of semiconductor devices. More particularly, embodiments of the present disclosure relate to substrate processing chambers and components thereof for forming semiconductor devices.

[0006] In one embodiment, a processing chamber is disclosed that includes a lid assembly and a chamber body coupled to the lid assembly by a spacer. The spacer and the chamber body define a resonant cavity. The processing chamber also includes a rotatable magnetic assembly coupled to the spacer outside the resonant cavity, and a moveable substrate support disposed within the resonant cavity, the substrate support coupled to a facility cable that bends based on the operation of an actuator coupled to the substrate support.

[0007] In another embodiment, a processing chamber is disclosed that includes a lid assembly including a showerhead and a chamber body coupled to the lid assembly by a spacer. The spacer and the chamber body define a resonant cavity. The processing chamber also includes a magnetic assembly coupled to the spacer outside the resonant cavity, and a substrate support disposed within the resonant cavity, the substrate support including an electrostatic chuck coupled to an equipment cable and having a puck including a plurality of electrodes.

[0008] In another embodiment, a processing chamber is disclosed that includes a lid assembly including a showerhead and a chamber body coupled to the lid assembly by a spacer. The spacer and the chamber body define a resonant cavity. The processing chamber also includes a magnetic assembly coupled to the spacer outside the resonant cavity, and a substrate support movably disposed within the resonant cavity, the substrate support coupled to an equipment cable including a single piece conductor including a bend, the substrate support including an electrostatic chuck having a puck including a plurality of electrodes.

[0009] So that the above-mentioned features of the present disclosure can be understood in detail, a more particular description of the present disclosure, briefly summarized above, can be had by reference to embodiments, some of which are illustrated in the accompanying drawings, in which it is noted, however, that the present disclosure is open to other equally effective embodiments, and therefore, the accompanying drawings illustrate only typical embodiments of the present disclosure, and should not be considered as limiting its scope. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic cross-sectional side view of an exemplary processing chamber, according to one embodiment; [Figure 2A] 2 is a schematic side view of the processing chamber of FIG. 1 rotated approximately 90 degrees, in accordance with one embodiment; [Figure 2B] 2 is a schematic side view of the processing chamber of FIG. 1 rotated approximately 90 degrees, in accordance with one embodiment; [Figure 3A] 1 is a schematic cross-sectional view of a processing chamber according to one embodiment; [Figure 3B] 1 is a schematic cross-sectional view of a processing chamber according to one embodiment; [Figure 4A] 1 is a schematic cross-sectional view of a substrate support according to an embodiment; [Figure 4B] FIG. 4B is an enlarged cross-sectional view of a portion of the substrate support shown in FIG. 4A, according to one embodiment. [Figure 5A-5D] 1A-1D are various views of a support structure of a substrate support and a portion of a cathode assembly, according to one embodiment; [Figures 6A-6C] 1 shows various cross-sectional views of a facility cable according to one embodiment. [Figure 7] 1 is a schematic cross-sectional view of a lid assembly according to one embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] To facilitate understanding, wherever possible, like reference numerals are used to designate like elements common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.

[0012] Embodiments of the present disclosure relate to substrate processing chambers utilized for substrate processing in the manufacture of electronic devices. Substrate processing includes deposition processes, etching processes, and other low pressure, plasma, and thermal processes used to manufacture electronic devices on substrates. An example of a processing chamber and / or system that can be adapted to benefit from exemplary aspects of the present disclosure is the Producer® APF™ PECVD system available from Applied Materials Inc., Santa Clara, Calif., USA. It is contemplated that other processing chambers and / or processing platforms, including those from other manufacturers, can also be adapted to benefit from aspects of the present disclosure.

[0013] The embodiments of the deposition chamber disclosed herein can be utilized for the fabrication of memory devices, and in particular for the deposition of hard masks utilized during the fabrication of memory devices. Current memory devices can retain stored data for very long periods without the application of voltage, and the read speed of such memory devices is relatively high. It is relatively easy to erase stored data and rewrite data to memory devices. Thus, memory devices are widely used in microcomputers and automatic control systems, etc. 3D NAND (3-dimensional, not AND) memory devices are being developed to increase the bit density of memory devices and reduce the cost per bit. Other memory devices, such as DRAM (Dynamic Random Access Memory), EM (Enhanced Memory), and ReRAM (Resistive Memory), as well as advanced hard mask materials for forming them, are also being developed to further advance the semiconductor industry.

[0014] Vertical gate 3D memory cells are being considered in 3D NAND technology to reduce costs as the number of memory cell layers increases. Oxide / silicon and oxide / nitride layer stacks are useful because of their material integration advantages, but as the number of memory cell layers increases, the thickness of the layers becomes a limiting factor. Thus, there is interest in reducing the thickness of the memory cell layers, but issues with oxide quality (i.e., breakdown voltage), silicon resistance, and high aspect ratio etching persist even as the layer thickness is reduced.

[0015] 1 is a schematic cross-sectional side view of an exemplary processing chamber 100 suitable for performing a deposition process. In one embodiment, which may be combined with other embodiments described herein, the processing chamber 100 may be configured to deposit highly patterned films, such as, for example, amorphous carbon hard mask films, onto a substrate.

[0016] The processing chamber 100 includes a lid assembly 105, a spacer 110 disposed on a chamber body 192, a substrate support 115, and a variable pressure system 120. The lid assembly 105 includes a lid plate 125 and a heat exchanger 130. In the illustrated embodiment, which can be combined with other embodiments described herein, the lid assembly 105 also includes a showerhead 135. However, in other embodiments, which can be combined with other embodiments described herein, the lid assembly 105 includes a concave or dome-shaped gas introduction plate (shown in FIG. 7 ).

[0017] The lid assembly 105 is coupled to a first process gas source 140. The first process gas source 140 includes a precursor gas for forming a film on a substrate 145 supported on the substrate support 115. By way of example, the first process gas source 140 includes a precursor gas, such as a carbon-containing gas, a hydrogen-containing gas, helium, etc., among others. In a particular example, the carbon-containing gas is acetylene (C 2 H 2 1. The first process gas source 140 provides precursor gas to a plenum 190 disposed in the lid assembly 105. The lid assembly includes one or more channels for directing precursor gas from the first process gas source 140 into the plenum 190. From the plenum, the precursor gas flows through the showerhead 135 and into the process volume 160. In some embodiments, which can be combined with other embodiments described herein, the second process gas source 142 is fluidly coupled to the process volume 160 via an inlet 144 disposed through the spacer 110. By way of example, the second process gas source 142 provides precursor gas, such as a carbon-containing gas, a hydrogen-containing gas, helium, or the like, among others, e.g., C 2 H 2In one embodiment, which can be combined with other embodiments described herein, the total flow rate of the precursor gases into the process volume 160 is about 100 sccm to about 2 slm. The flow of the precursor gases in the process volume 160 through the second process gas source 142 regulates the flow of the precursor gases through the showerhead 135 such that the precursor gases are uniformly distributed in the process volume 160. In one example, the multiple inlets 144 can be radially distributed around the spacer 110. In such an example, the flow of gas to each of the inlets 144 can be separately controlled to further promote uniformity of the gases in the process volume 160.

[0018] The lid assembly 105 is also coupled to an optional remote plasma source 150. The remote plasma source 150 is coupled to a cleaning gas source 155 for providing a cleaning gas to a process volume 160 formed within the spacer 110 between the lid assembly 105 and the substrate 145. In one example, the cleaning gas is provided through a central conduit 191 formed axially through the lid assembly 105. In another example, the cleaning gas is provided through the same channels that conduct the precursor gases. Examples of cleaning gases include oxygen-containing gases, such as oxygen and / or ozone, as well as NF 3 fluorine-containing gases such as fluorine-containing fluorine, ...

[0019] In addition to or as an alternative to the remote plasma source 150, the lid assembly 105 is also coupled to a first or upper radio frequency (RF) power source 165. The first RF power source 165 facilitates the maintenance or generation of a plasma, such as a plasma generated from a cleaning gas. In one example, the remote plasma source 150 is omitted and the cleaning gas is ionized into a plasma in situ via the first RF power source 165. The substrate support 115 is coupled to a second or lower RF power source 170. The first RF power source 165 can be a high frequency RF power source (e.g., about 13.56 MHz to about 120 MHz) and the second RF power source 170 can be a low frequency RF power source (e.g., about 2 MHz to about 13.56 MHz). It should be noted that other frequencies are also contemplated. In some implementations, the second RF power source 170 is a mixed frequency RF power source, providing both high frequency and low frequency power. The use of a dual frequency RF power source improves film deposition, particularly with the second RF power source 170. In one example, the use of the second RF power source 170 provides dual frequency power: a first frequency of about 2 MHz to about 13.56 MHz improves the implantation of species into the deposited film, while a second frequency of about 13.56 MHz to about 120 MHz increases the ionization and deposition rate of the film.

[0020] One or both of the first RF power source 165 and the second RF power source 170 are utilized to generate or maintain a plasma in the process volume 160. For example, the second RF power source 170 can be utilized during a deposition process and the first RF power source 165 can be utilized during a cleaning process (alone or in combination with the remote plasma source 150). In some deposition processes, the first RF power source 165 is used in conjunction with the second RF power source 170. During a deposition or etching process, one or both of the first RF power source 165 and the second RF power source 170 provide a power of about 100 W to about 20,000 W in the process volume 160 to promote ionization of the precursor gas. In one embodiment, which can be combined with other embodiments described herein, at least one of the first RF power source 165 and the second RF power source 170 is pulsed. In another embodiment, which can be combined with other embodiments described herein, the precursor gas is selected from the group consisting of helium and C. 2 H 2 In one embodiment, which may be combined with other embodiments described herein, 2 H 2 is provided at a flow rate of about 10 sccm to about 1,000 sccm, and He is provided at a flow rate of about 50 sccm to about 10,000 sccm.

[0021] The substrate support 115 is coupled to an actuator 175 (i.e., a lift actuator) that effects its movement in the Z direction. The substrate support 115 is also coupled to a flexible facility cable 178 that allows vertical movement of the substrate support 115 while maintaining communication with the second RF power source 170 and other power and fluid connections. The spacer 110 is disposed on the chamber body 192. The height of the spacer 110 allows vertical movement of the substrate support 115 within the processing volume 160. The height of the spacer 110 is about 0.5 inches to about 20 inches. In one example, the substrate support 115 is movable from a first distance 180A to a second distance 180B relative to the lid assembly 105 (e.g., relative to the underside of the showerhead 135). In one embodiment, the second distance 180B is about 2 / 3 of the first distance 180A. For example, the difference between the first distance 180A and the second distance is about 5 inches to about 6 inches. Thus, from the position shown in FIG. 1, the substrate support 115 can move about 5 inches to about 6 inches relative to the underside of the showerhead 135. In another example, the substrate support 115 is fixed at one of the first distance 180A and the second distance 180B. In contrast to conventional plasma enhanced chemical vapor deposition (PECVD) processes, the spacer 110 significantly increases the distance (and therefore the volume therebetween) between the substrate support 115 and the lid assembly 105. The increased distance between the substrate support 115 and the lid assembly 105 reduces the bombardment of ionized species within the volumetric processing volume 160, resulting in the deposition of a film with less neutral stress, such as less than 2.5 gigapascals (GPa). The film deposited with less neutral stress promotes improved flatness (e.g., less warping) of the substrate on which the film is formed. The reduced warping of the substrate results in improved accuracy of downstream patterning operations.

[0022] The variable pressure system 120 includes a first pump 182 and a second pump 184. The first pump 182 is a roughing pump that can be utilized during the cleaning process and / or the substrate transfer process. A roughing pump is generally configured to move a higher volumetric flow rate and / or operate at a relatively high (but still subatmospheric) pressure. In one example, the first pump 182 maintains a pressure in the processing chamber below 50 mTorr during the cleaning process. In another example, the first pump 182 maintains a pressure in the processing chamber between about 0.5 mTorr and about 10 Torr. The utilization of a roughing pump during the cleaning operation facilitates a relatively high pressure and / or volumetric flow rate of the cleaning gas (compared to the deposition operation). The relatively high pressure and / or volumetric flow rate during the cleaning operation improves cleaning of the chamber surfaces.

[0023] The second pump 184 can be one of a turbo pump and a cryogenic pump. The second pump 184 is utilized during the deposition process. The second pump 184 is generally configured to operate at a relatively low volumetric flow rate and / or pressure. For example, the second pump 184 is configured to maintain the processing region 160 of the processing chamber at a pressure less than about 50 mtorr. In another example, the second pump 184 maintains the pressure in the processing chamber at about 0.5 mtorr to about 10 Torr. The reduced pressure in the processing region 160 maintained during deposition may provide reduced neutral stress and / or sp when depositing a carbon-based hardmask. 2 -sp 3 The conversion promotes increased film deposition. Thus, the processing chamber 100 is configured to utilize both relatively low pressures to improve deposition and relatively high pressures to improve cleaning.

[0024] In some embodiments, which may be combined with other embodiments described herein, both the first pump 182 and the second pump 184 are utilized during the deposition process to maintain the processing volume 160 of the processing chamber at a pressure less than about 50 mTorr. In other embodiments, the first pump 182 and the second pump 184 maintain the processing volume 160 at a pressure between about 0.5 mTorr and about 10 Torr. A valve 186 is utilized to control the conductance path to one or both of the first pump 182 and the second pump 184. The valve 186 also provides symmetric pumping from the processing volume 160.

[0025] The processing chamber 100 also includes a substrate transfer port 185. The substrate transfer port 185 is selectively sealed by an inner door 186A and an outer door 186B. Each of the doors 186A and 186B is coupled to an actuator 188 (i.e., a door actuator). The doors 186A and 186B facilitate vacuum sealing of the processing volume 160. The doors 186A and 186B also provide symmetrical RF application and / or plasma symmetry within the processing volume 160. In one example, at least the door 186A is formed of a material that facilitates conductance of RF power, such as stainless steel, aluminum, or alloys thereof. A seal 116, such as an O-ring, disposed at the interface of the spacer 110 and the chamber body 192 can further seal the processing volume 160. A controller 194 coupled to the processing chamber 100 is configured to control aspects of the processing chamber 100 during processing.

[0026] 2A and 2B are schematic side views of the processing chamber of FIG. 1 rotated approximately 90 degrees. In FIG. 2A and 2B, details of the spacer 110 are shown. The spacer 110 includes a liner 200 that surrounds the processing volume 160. In one embodiment, which may be combined with other embodiments described herein, the spacer 110 and the liner 200 are comprised of a single piece. The liner 200 may be bonded (e.g., diffusion bonded) to the spacer 110.

[0027] The spacer 110 also includes a number of heater elements 205 embedded in or thermally coupled to the body of the spacer 110. The heater elements 205 are utilized to maintain the temperature of the spacer 110 at or above about 80 degrees Celsius. Each of the heater elements 205 can be a cartridge heater.

[0028] The liner 200 includes an upper or first portion 210 and a lower or second portion 215. The thickness of the liner 200, for example, the thickness of the portion 210 and the thickness of the second portion 215, can be varied. The varying thickness of the liner 200 provides the ability to control the flow conductance at the lower portion of the processing volume 160. Controlling the flow conductance at the lower portion of the processing volume 160 provides the ability to expose the substrate 185 to a substantially uniformly distributed precursor gas, as well as to a uniform exposure to the cleaning gas in the processing volume 160, resulting in more uniform processing of the substrate. In one embodiment, which can be combined with other embodiments described herein, the first portion 210 has a thickness greater than the thickness of the second portion 215. One advantage of the reduced thickness of the second portion 215 is that the space between the substrate support 115 and the inner wall of the spacer 110 is increased, thus increasing the vacuum conductance. Another advantage of the reduced thickness of the second portion 215 is the change in the thermal mass of the liner 200. Thus, the portion of the liner 200 adjacent to or within the first portion 210 is maintained at a higher temperature than the portion of the liner 200 adjacent to or within the second portion 215.

[0029] The liner 200 includes an inner surface 202 exposed to the process volume 160. In one embodiment, which may be combined with other embodiments described herein, the inner surface 202 may include one or more materials including aluminum, titanium, or alloys thereof. The inner surface 202 of the liner 200 may be coated with one or more of aluminum, titanium, or alloys thereof. In another embodiment, which may be combined with other embodiments described herein, the inner surface 202 may include one or more ceramic-containing materials. In one example, the liner 200 extends from the lid assembly 105 through the substrate support 115 and adjacent to the bottom of the process chamber 100. In such an example, the liner 200 does not contact the bottom of the chamber 100, but instead is spaced therefrom. Additionally, although FIGS. 2A and 2B depict the liner 200 as being a single piece, it is contemplated that multiple liners may be utilized to line the inner surface of the process chamber. For example, a first (or upper) liner may be utilized to line the spacer 110, while a second (or lower) liner may be used to line the inner surface of the chamber body (shown in FIG. 1).

[0030] In the embodiments described herein, the electrical conductivity of the liner 200, controlled by at least one of the inner surfaces 202 exposed to the process volume 160, and the thickness of the liner 200, change the flow of electrical current (e.g., direct current (DC), RF current, and other suitable current) provided to the electrostatic chuck 330 (shown in FIG. 3 ) of the substrate support 115. Increasing the electrical conductivity of the liner 200 provides a short, symmetrical path for the RF energy of the plasma sheath generated within the process volume 160 to propagate from the sidewall to ground. The path for the RF energy to propagate from the sidewall to ground improves the current flow and reduces the amount of current required by the electrostatic chuck 330 through increased efficiency. Reducing the amount of current required by the electrostatic chuck 330 allows for increased voltage (e.g., V dc) to the electrostatic chuck 330. The increase in voltage results in greater ionization of the plasma sheath to increase ion or radical bombardment of the substrate 105. The increase in ion or radical bombardment of the substrate 105 reduces stress in the film being deposited or etched.

[0031] The spacer 110 also includes a magnetic assembly 220. In one embodiment, which can be combined with other embodiments described herein, as shown in FIG. 2A, the magnetic assembly 220 includes a plurality of magnets 225 surrounding the spacer 110. Each of the magnets 225 is coupled to an actuator 230 (i.e., a magnetic actuator). The actuator 230 rotates the magnets 225 around the spacer 110 outside the liner 200 about a longitudinal axis 235 of the processing chamber 100. The actuator 230 is also adapted to move the magnets 225 vertically (in the Z direction) along the longitudinal axis 235. Each of the magnets 225 can be a permanent magnet, or an electromagnet, or a combination thereof. Each of the magnets 225 is positioned within a cavity 240 formed in a sidewall 242 of the spacer 110. In one example, the magnets are positioned below the heater element 205. The material and thickness of the outer sidewall 242 controls the magnetic permeability of the outer sidewall 242, thereby providing confinement of the magnetic field to the processing volume 160. Confinement of the magnetic field to the processing volume 160 reduces the effect of the magnetic field on nearby processing volumes of adjacent processing chambers, thus improving process uniformity. A controller 194 coupled to the processing chamber 100 and the magnetic assembly 220 is configured to control aspects of the processing chamber 100 and the magnetic assembly 220 during processing.

[0032] In another embodiment, which can be combined with other embodiments described herein, as shown in FIG. 2B, the magnetic assembly 220 includes a conductive wire 204 that can be wrapped one or more times around (or embedded within) the spacer 110 to form a single electromagnet circumscribing the spacer 110. A power source 206 is coupled to the conductive wire 204 to pass a current in a circular path around the processing volume 160. The conductive wire 204 can be disposed on one of the spacer 100 and the liner 200. The material and thickness of the outer shield 208 provide confinement of the magnetic field to the processing volume 160 by controlling the magnetic permeability of the outer shield 208. Confinement of the magnetic field to the processing volume 160 reduces the effect of the magnetic field on nearby processing volumes of adjacent processing chambers, thus improving process uniformity.

[0033] In some embodiments, which can be combined with other embodiments described herein, about half of the magnets 225 are oriented with their north poles facing the substrate support 115 (substantially parallel to the longitudinal axis 235). The other part of the magnets 225 are oriented with their south poles facing the substrate support 115 (substantially parallel to the longitudinal axis 235). In one example, the magnets 225 are arranged in a circle around the spacer 110 (in a plan view). The magnets 225 are separated into a first part or first semicircle and a second part or second semicircle. Each of the magnets 225 in the first semicircle is oriented with its north pole facing the substrate support 115 (substantially parallel to the longitudinal axis 235). Each of the magnets 225 in the second semicircle is oriented with its south pole facing the substrate support 115 (substantially parallel to the longitudinal axis 235). In such an example, the multiple magnets 225 may be rotated during deposition, or the multiple magnets may remain stationary.

[0034] In some embodiments, which may be combined with other embodiments described herein, the conductive wire 204 includes at least one of voids in the core material of the conductive wire 204, a varying cross-sectional area of ​​the core material, and a varying distance between each turn of the conductive wire 204. The core material of the first half of the conductive wire 204 (e.g., encompassing about 180 degrees) may have more voids than the second half of the conductive wire 204 (e.g., encompassing about 180 degrees). The core material of the first half of the conductive wire 204 may have a larger cross-sectional area than the second half of the conductive wire 204. The distance between each turn of the conductive wire 204 in the first half may be less than the distance between each turn of the conductive wire 204 in the second half.

[0035] In other embodiments that can be combined with other embodiments described herein, the magnetic assembly 220 includes two or more conductive wires 204. Each of the conductive wires 204 is disposed on a respective portion of the spacer 110. An electrically operable power source 206 is connectable to the controller 194. The controller 194 is operable to sequentially turn on or off each of the power sources 206 and simultaneously turn on or off each of the power sources 206 to control the supply of power to each of the conductive wires 204. Turning off each of the power sources 206 simultaneously allows for shunting of the magnetic field generated by the electromagnet. In one example, a first conductive wire is wound one or more times in a semicircle and disposed in a first half of the spacer 110 corresponding to a first half of the processing volume 160 to form a first electromagnet. A second conductive wire is wound one or more times in a semicircle and disposed in a second half of the spacer 110 corresponding to a second half of the processing volume 160 to form a second electromagnet. The first and second electromagnets may have opposite polarities.

[0036] In another example, a first conductive wire is wound one or more times in a semicircle having an angular arc of 90 degrees or less and placed in a first quadrant of the spacer 110 corresponding to a first quadrant of the processing volume 160 to form a first electromagnet. A second conductive wire is wound one or more times in a semicircle having an angular arc of 90 degrees or less and placed in a second quadrant of the spacer 110 corresponding to a second quadrant of the processing volume 160 to form a second electromagnet. A third conductive wire is wound one or more times in a semicircle having an angular arc of 90 degrees or less and placed in a third quadrant of the spacer 110 corresponding to a third quadrant of the processing volume 160 to form a third electromagnet. A fourth conductive wire is wound one or more times in a semicircle having an angular arc of 90 degrees or less and placed in a fourth quadrant of the spacer 110 corresponding to a fourth quadrant of the processing volume 160 to form a fourth electromagnet. The first, second, third, and fourth electromagnets may have alternating polarities.

[0037] The magnetic assembly 220 assists in confining and / or regulating the plasma within the processing volume 160. In one embodiment, which can be combined with other embodiments described herein, the magnetic assembly 220 also forms a resonant cavity 245 within the processing volume 160 during the deposition process. The resonant cavity 245 provides a magnetic flux that extends the plasma sheath vertically downward (Z direction) toward the substrate (not shown in FIGS. 2A and 2B). The strength of one of the magnets 225 and the core material of the conductive wire 204 compresses the plasma within the processing volume 160 and extends the plasma sheath radially outward to the spacer 110. As previously described, extending the plasma sheath to the spacer 110 (e.g., the liner 200 of the spacer 110) provides a short, symmetrical path for RF energy to propagate from the sidewall to the ground.

[0038] The magnetic assembly 220 provides a B-field in the X / Y plane as well as in the Z direction. The magnetic assembly 220 also allows for adjustment of the plasma in the process volume 160 and / or the resonant cavity 245. Eddy currents in the plasma can be monitored to provide a metric for adjusting one or both of the position of the magnet 225 and the rotational speed of the magnet 225. Additionally or alternatively, measurements of a film previously deposited on the substrate can be performed and the results can be used to change the position and / or rotational speed of the magnet 225. Thus, the resonant cavity 245 and the magnetic assembly 220 provide better film uniformity on the substrate. In embodiments that include the magnet 225, the opposite polarity of the magnet 225 distorts the B-field generated through the magnet 225. In some embodiments that include an electromagnet, the B-field generated by the flowing current through the conductive wire 204 is distorted by adjusting at least one of the air gap, the cross-sectional area, and the distance between each turn of the conductive wire 204. In some embodiments including two or more electromagnets with opposite or alternating polarity, sequentially powering each of the conductive wires 204 distorts the B-field generated by the flowing current through the conductive wires 204. The distortion of the B-field shifts the peak of the plasma sheath. Rotating the magnets and flowing current through the conductive wires 204 in a circular path around the process volume 160 promotes more uniform exposure of the substrate 150 to the ions and radicals of the distorted plasma sheath. In one embodiment, which can be combined with other embodiments described herein, a metal band (not shown) is disposed within the liner 200. The metal band can further shift the B-field.

[0039] The spacer 110 includes a height 250 that provides a much larger processing volume 160 and / or volume of the resonant cavity 245 than conventional chambers. In some embodiments described herein above, the height 250 is from about 0.5 inches to about 20 inches, such as from about 0.5 inches to about 3 inches, such as from about 15 inches to about 20 inches. The height of the resonant cavity 245 provided by the height 250 provides many advantages. One advantage includes reduced film stress, which reduces stress-induced bowing of substrates being processed therein.

[0040] 3A and 3B are schematic cross-sectional views of the processing chamber 100. Shown in Figures 3A and 3B is a cathode assembly 300 that includes a substrate support 115. The cathode assembly 300 is coupled to an actuator 305 (similar to the actuator 175 shown in Figure 1) that moves the cathode assembly 300 vertically in the Z direction.

[0041] 3A shows the cathode assembly 300 in a lowest position (e.g., first distance 180A) relative to the lid assembly 105, and FIG. 3B shows the cathode assembly 300 in a highest position (e.g., second distance 180B) relative to the lid assembly 105. The ability to adjust the position of the cathode assembly 300 for the deposition process allows for optimal film quality to be achieved.

[0042] The cathode assembly 300 also includes an equipment interface 310. The equipment interface 310 provides connections for RF power and other electrical and fluid connections. The equipment interface 310 is coupled to the substrate support 115 via an equipment cable 178. Other connections include a power supply 315, a coolant source 320, and a gas supply 325.

[0043] The power supply 315 is utilized to power the electrostatic chuck 330 that is part of the substrate support 115. The power supply 315 can be a DC power supply. Dechucking is facilitated by a controller (not shown) that flushes the electrostatic chuck 330. Additionally, an equipment cable 178 is coupled to the power supply 170, optionally via a matching network, to facilitate operation within the processing chamber 100. In one example, the equipment cable 178 facilitates the transfer of RF power during a PECVD process. Due to the relatively large volume created by the spacer 110 and the pressure at which the processing chamber 100 operates during a PECVD process, higher power levels (compared to conventional PECVD processes) are used to establish and maintain the plasma. For example, the equipment cable can transmit about 4 kW to about 9 kW of power at 110 amps during a PECVD process. It is believed that the amperage can be reduced to a range of about 78 amps to about 80 amps without degrading film quality when utilizing the magnets 225 in a tuned configuration.

[0044] The coolant source 320 includes a coolant that cools the substrate support 115. For example, coolant from the coolant source 320 is flowed to the substrate support 115 to maintain the temperature of the electrostatic chuck 330 (and / or a substrate positioned thereon) at about 25 degrees Celsius or less. The electrostatic chuck 330 (and / or a substrate positioned thereon) may be maintained at a cryogenic temperature of about -40 degrees Celsius or less. The cryogenic temperature allows ions to impinge on the upwardly facing surface of the substrate 145 and / or materials disposed on the substrate 145, reducing spontaneous deposition or etching and resulting in improved uniformity and properties of the deposited or etched film. The coolant includes a fluid for maintaining a cryogenic temperature, such as a perfluoropolyether fluorinated fluid.

[0045] A gas supply 325 provides a fluid to the space below the electrostatic chuck 330 to prevent condensation. The fluid may be clean, dry air, nitrogen (N 2The fluid may be argon (Ar), helium (He), or other suitable gas. The fluid supplied to the space below the electrostatic chuck reduces condensation on the electrostatic chuck, including its underside.

[0046] One or more combinations of cooling the substrate support 115, the heated spacer 110 (using the heater element 205 shown in FIGS. 2A and 2B), and the resonant cavity 245 described herein provide many advantages. Lower substrate temperatures increase deposition rates and reduce substrate warping. Maintaining the temperature of the spacer 110 and / or the liner 200 below about 100 degrees Celsius promotes more efficient cleaning and / or minimizes particle adhesion to the liner 20. One or more cooling channels can be formed in the spacer 110 to facilitate cooling of the liner 200.

[0047] 3A and 3B also shows a support structure 335. Although only one is shown, the support structure 335 has three reduced pressure channels 340 formed therein. The reduced pressure channels 340 are coupled to the variable pressure system 120. The reduced pressure channels 340 facilitate symmetric pumping out of the processing volume 160.

[0048] The cathode assembly 300 is coupled to a base ring 340 and an optional mounting plate 345. Fasteners 355 extend from the base ring 340 to secure the substrate support 115 thereon.

[0049] Figure 4A is a schematic cross-sectional view of one embodiment of the substrate support 115. Figure 4B is an enlarged cross-sectional view of a portion of the substrate support 115 shown in Figure 4A.

[0050] As described above, the substrate support 115 includes an electrostatic chuck 330. The electrostatic chuck 330 includes a puck 400. The puck 400 includes one or more electrodes 405 embedded therein (a first electrode 405A and a second electrode 405B are shown in FIG. 4B). The first electrode 405A is utilized as a chucking electrode and the second electrode 405B is utilized as an RF bias electrode. The substrate support 115 can be biased by providing RF power to the second electrode 405B at a frequency of about 300 kHz to about 60 MHz. The frequency provided to the second electrode 405B may be pulsed. The puck 400 is formed from a dielectric material, such as a ceramic material, for example, aluminum nitride (AlN).

[0051] The puck is supported by a dielectric plate 410 and a base plate 415. The dielectric plate 410 may be formed from an electrically insulating material such as quartz, or a thermoplastic material such as a high performance plastic sold under the trade name REXOLITE®. The base plate 415 may be made from a metallic material such as aluminum. During operation, the base plate 415 is either tied to ground or is electrically floating while the puck 400 is RF hot. At least the puck 400 and the dielectric plate 410 are surrounded by an insulator ring 420. The insulator ring 420 may be made from a dielectric material such as quartz, silicon, or a ceramic material. The base plate 415 and a portion of the insulator ring 420 are surrounded by a ground ring 425 made of aluminum. The insulator ring 420 prevents or minimizes arcing between the puck 400 and the base plate 415 during operation. The ends of the facilities cable 178 are shown in openings formed in the puck 400, the dielectric plate 410, and the base plate 415. Power for the electrodes of the puck 400 and fluids from the gas supply 325 (shown in FIGS. 3A and 3B) to the substrate support 115 is provided by the facilities cable 178.

[0052] The edge ring 422 is disposed adjacent to the inner circumference of the insulator ring 420. The edge ring 422 may be made of any of a variety of materials, including quartz, silicon, cross-linked polystyrene, and divinylbenzene (e.g., REXOLITE®), PEEK, Al, among others. 2 O 3 , AlN, or other dielectric materials. Utilizing an edge ring 422 that includes such a dielectric material modulates the plasma coupling and voltage at the substrate support (V dc ) and thus improve the properties of the hardmask film deposited on the substrate. By modulating the RF coupling to the wafer or substrate by the edge ring 422 material, the elastic modulus of the film can be decoupled from the stress in the film.

[0053] Each of the puck 440, the dielectric plate 410, and the base plate 415 includes a respective axially aligned opening formed therein or therethrough for receiving the equipment cable 178. The puck 440 includes an opening 495 shaped to engage the equipment cable 178. For example, the opening 495 can be configured as a female receptacle for receiving the equipment cable 178. The dielectric plate 410 includes an opening 496 axially aligned with the opening 495. The opening 496 includes an upper portion 496a having a diameter approximately equal to the diameter of the opening 495, a middle portion 496b having a diameter greater than the diameter of the upper portion, and a lower portion 496c having a diameter greater than the diameter of the middle portion 496b. The base plate 415 includes an opening 497 having an upper portion 497a having a first diameter, and a lower portion 497b having a second diameter less than the first diameter. The multiple diameters of openings 496, 496, and 497 facilitate securement of facility cable 178 therein.

[0054] The pack 400 includes a plurality of fluid channels 430 formed therein. Each of the fluid channels 430 is in fluid communication with an inlet channel 432. The inlet channel 432 is fluidly coupled to an inlet conduit 434. The inlet conduit 434 is coupled to the coolant source 320. Each of the fluid channels 430 and the inlet channel 432 are sealed by a cap plate 436. The cap plate 436 may be made from the same material as the pack 400 or from aluminum, and may be welded or otherwise coupled to the pack 400 to seal the fluid channels 430 and the inlet conduit 434. Although not shown, an outlet conduit similar to the inlet conduit 434 is provided in the substrate support 115 so that the cooling fluid can be recirculated therein.

[0055] A portion of the inlet conduit 434 is formed by a tubular member 438. The tubular member 438 is formed from a dielectric material, such as a ceramic material. Seals 440 are provided at the ends of the tubular member 438 adjacent the cap plate 436 and the base plate 415. The tubular member 438 prevents arcing that may occur due to the cooling fluid flowing therethrough. The tubular member 438 may also thermally insulate the dielectric plate 410 from the relatively cool cooling fluid flowing therethrough to prevent cracking of the dielectric plate 410.

[0056] The substrate support 115 also includes a plurality of lift pins 442 (only one is shown in FIG. 4A). Each of the lift pins 442 is movably disposed within a dielectric bushing 444. Each of the lift pins 442 may be formed from a ceramic material, such as AlN, sapphire, quartz, or the like. A dielectric bushing 444 is provided in or through each of the puck 400, the dielectric plate 410, and the base plate 415. The dielectric bushing 444 is made of a polymeric material, such as a polytetrafluoroethylene (PTFE) material. The dielectric bushing 444 includes an opening 446 along its length through which the lift pin 442 is guided. The opening 446 is sized slightly larger than a dimension (diameter) of the lift pin 442 such that a conductance path is formed in the dielectric bushing 444. For example, the opening 446 is coupled to the variable pressure system 120 such that a reduced pressure conductance is provided between the process volume 160 and within the variable pressure system 120 through the dielectric bushing 444. The conductance path provided by the opening 446 prevents arcing of the lift pins. The dielectric bushing 444 includes a number of steps 448 that are sections of varying diameter. The steps 448 reduce arcing between the puck 400 and the base plate 415 by increasing the length of the path through which electricity can travel as well as by introducing turns along the path.

[0057] The substrate support 115 also includes a plurality of fastener devices 450 (only one is shown). The fastener devices 450 are utilized to attach the puck 400 to the dielectric plate 410. Each fastener device 450 includes a fastener 452, a metal washer 454, and a fastener cap 456 (the washer 454 and the fastener cap 456 are shown in FIG. 4B). When the fastener 452 is tightened, the washer 454 is biased against a surface 458 of an opening 460 formed in the dielectric plate 410. The washer 454 and the fastener 452 are made from a metallic material, such as stainless steel. The washer 454 includes a rounded top corner 462. The rounded top corner 462 prevents cracking of the material of the dielectric plate 410 when the fastener 452 is tightened.

[0058] A fastener cap 456 is utilized to fill the remainder of the opening 460 in the dielectric plate 410. The fastener cap 456 includes a pocket 464 sized to receive the head of the fastener 452. The fastener cap 456 is formed from a dielectric material such as, for example, polyetheretherketone (PEEK). The exterior surface of the fastener cap 456 includes a step 466. The step 466 reduces arcing between the puck 400 and the base plate 415 by increasing the length of the path through which electricity can travel.

[0059] The substrate support 115 also includes a number of gaps between their layers. A first gap 470 is provided between the puck 400 and the dielectric plate 410. A second gap 472 is provided between the dielectric plate 410 and the base plate 415. The first gap 470 and the second gap 472 are in fluid communication with the gas supply 325 shown and described in Figures 3A and 3B. Fluid from the gas supply 325 is channeled into the first gap 470 and the second gap 472 to prevent condensation between adjacent layers. The fluid in the first gap 470 and the second gap 472 is sealed at the edge of the substrate support 115 by an edge ring 420. The edge ring 420 can be sized to provide controlled leakage of fluid from the first gap 470 and the second gap 472.

[0060] 5A-5D are various views of the support structure 335 and a portion of the cathode assembly 300. FIG. 5A is a perspective view showing the base ring 340 on the support structure 335. FIG. 5B shows the lift pin spider 500 interfacing with the base ring 340 and the support structure 335. FIG. 5C is an enlarged partial cross-sectional view of the cathode assembly 300 with the lift pin spider 500 assembled therein. FIG. 5D is another enlarged partial cross-sectional view of the cathode assembly 300 with the lift pin spider 500 assembled therein.

[0061] As shown in Figures 5A and 5B, the lift pin spider 500 includes a ring body 505 (shown in Figure 5B) having a pin gripping device 510 coupled thereto. Each pin gripping device 510 supports a lift pin 442 (shown in Figure 5B). The lift pin spider 500 also includes a bellows 515 that houses a lift shaft 520 (both shown in Figures 5B-5D). The ring body 505 includes a circular or nearly circular outer edge 560, and an inner edge 561. The inner edge 561 is circular and includes one or more lobes (two minor lobes 562 and one major lobe 563 that is larger in size than the minor lobes 562 are shown). The lobes 562, 563 are spaced apart at approximately equal angular distances from each other (e.g., about 120 degrees) and include lift pins attached thereto. In addition, a lift shaft 520 is coupled to the major lobe 563 on the opposite side of each lift pin 442. In such an example, the lift shaft 520 and respective lift pins are axially aligned, although other configurations are contemplated.

[0062] The ring body 505 is adapted to fit within a vacuum channel 525 (shown in FIGS. 5A, 5C, and 5D) and move vertically (in the Z direction). Vertical movement of the ring body 505 is provided by an actuator 530 (shown in FIG. 5C) to raise and lower a lift pin 442 coupled to the pin gripping device 510. The vacuum channel 525 is in fluid communication with the variable pressure system 120 via one or more vacuum conduits 535 (shown in FIGS. 5A and 5D). In this manner, a conductance path is formed around the lift pin 442 through the opening 446 in the dielectric bushing 444.

[0063] Referring to FIG. 5C, the lift pins 442 extend from the pin gripping apparatus 510 through openings 540 formed in the base ring 340 to a dielectric bushing 444 .

[0064] Each pin gripping device 510 includes a gripper 546, a gripper stem 548, and a gripper housing 550. Gripper housing 550 is coupled to a first fastener 552A, which couples gripper housing 550 to standoff 554. A second fastener 552B couples standoff 554 to ring body 505. A fastener plate 556 secures second fastener 552B to ring body 505. Fastener plate 556 and second fastener 552B are positioned within a recess 558 formed in the underside of ring body 505.

[0065] The gripper housing 550, the first fastener 552A, the second fastener 552B, the fastener plate 556, and the bellows 515 are fabricated from a metallic material, such as stainless steel. The gripper 546, the gripper stem 548, the standoff 554, and the ring body 505 may be fabricated from a dielectric material, such as a polymer or ceramic material. In a particular example, the gripper 546 and the gripper stem 548 may be made from a plastic material, such as a polyimide plastic material. The standoff 554 may be made from a PEEK material. The ring body 505 may be made from an aluminum oxide (Al 2 O 3The metallic materials in or on the ring body 505 and the pin grip device 510 are either grounded or electrically floating during operation of the cathode assembly 300.

[0066] 6A-6C show various cross-sectional views of the equipment cable 178. The equipment cable 178 includes a first end 600 and a second end 605. The first end 600 interfaces with the substrate support 115 and the second end 605 interfaces with the equipment interface 310 (shown in FIGS. 3A and 3B).

[0067] The equipment cable 178 is a single piece conductor (i.e., a single unit or monolith). The equipment cable 178 according to this embodiment is an improvement over conventional cables. For example, the equipment cable 178 includes a bend 610 (e.g., a curved or arcuate section) where a conventional conductor would have an L-shaped or 90 degree connection of two conductors. The bend 610 eliminates arcing at a conventional 90 degree connection and improves current flow along the conductor. The single piece design also provides a more robust insulation while having a smaller outside diameter compared to conventional conductors. In some instances, the equipment cable 178 is manufactured in a bent shape that maximizes contact between the composite layers of the equipment cable 178, as opposed to forming a straight equipment cable 178 and then bending it. Manufacturing the equipment cable 178 in a pre-bent shape avoids wrinkling of the material that can occur around the bend when bending a straight formed cable. Such wrinkling can inadvertently increase resistance or induce arcing. As described above, the facility cables 178 bend upon actuation of the actuators 175 (shown in FIG. 1), which provides vertical movement of the substrate support 115 .

[0068] 6B is a cross-sectional view of a first end 600 of the equipment cable 178. The first end 600 includes a connector 620 extending from a dielectric sheath 625. FIG 6B is a cross-sectional view of a second end 605 of the equipment cable 178. The second end 605 also includes a connector 630 extending from the dielectric sheath 625.

[0069] Connectors 620 and 630 include a first conductor 635 centrally located within a dielectric sheath 625. The dielectric sheath 625 does not extend to the termination of the end 620 of the equipment cable 178 to allow for coupling to the substrate support 115. Connectors 620 and 630 also include a second conductor 640 that substantially surrounds the first conductor 635.

[0070] With reference to connector 620, first conductor 635 is connected to a socket 645 that is coupled to first conductor 635 by a conductive housing 650. Socket 645 and conductive housing 650 include a threaded connection 655. With reference to connector 630, first conductor 635 is coupled to a male insert 660.

[0071] The first conductor 635 and the second conductor 640 are electrically separated by one or both of a dielectric material 665 and a space or gap 670. The dielectric material 665 can be a polymeric material such as PEEK, PTFE, or other polymeric and / or electrically insulating material. Both the first conductor 635, the second conductor 640, the socket 645, the conductive housing 650, and the male insert 660 are made of a conductive metal such as copper. At the bend 610, thinning of the second conductor 640 and collapse of the dielectric material 665 (i.e., strain of the equipment cable 178) can cause separation of the dielectric material 665 from the second conductor 640. This separation can result in arcing at the bend 610. Pre-treatment, such as stress relief and / or annealing, of the pre-bent equipment cable 178 at the bend 610 eliminates possible distortion of the equipment cable 178 due to potential thinning of the second conductor 640 and collapse of the dielectric material 665.

[0072] The construction of the equipment cable 178 described herein provides an exposed interface surface 675 of the second conductor 640 that includes a length 680 that is longer than that of a conventional conductor. In addition, the construction of the equipment cable 178 described herein provides a shoulder area or stop 685 for the male insert 660.

[0073] 7 is a schematic cross-sectional view of another embodiment of the lid assembly 105. The lid assembly 105 according to this embodiment includes a dome structure 700 formed on a portion of the heat exchanger 130. The dome structure 700 is coupled to the remote plasma source 150 by a flange 705 having an opening 706 formed axially therethrough to facilitate flow of plasma through the flange 705. The dome structure 700 is also coupled to a gas distribution assembly 710.

[0074] The gas distribution assembly 710 includes a first process gas source 140 and a purge gas source 715. Both the first process gas source 140 and the purge gas source 715 are coupled to the gas distribution assembly 710 by valves (not shown). The gas distribution assembly 710 also includes a baffle plate 720. The baffle plate 720 is utilized to diffuse energized cleaning gas from the remote plasma source 150. The baffle plate 720 is coupled to an inner surface 707 of the gas distribution assembly 710 by one or more brackets 708. The brackets 708 are spaced equiangularly apart in a spoke-and-hub configuration (e.g., three brackets spaced 120 degrees apart). The baffle plate 720 also includes a central opening 725. The central opening 725 may be utilized to supply one or both of the process gas and the purge gas from the respective sources.

[0075] The heat exchanger 130 includes an inlet 730 and an outlet 735. Heat exchange fluid flows from the inlet 730 through channels 740 formed in the dome structure 700 and exits through the outlet 735.

[0076] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, the scope of which is determined by the claims that follow.

Claims

1. A processing chamber comprising: Lid assembly; a chamber body coupled to the lid assembly by a spacer, the spacer and the chamber body defining a resonating cavity; a rotatable magnetic assembly coupled to the spacer outside the resonant cavity; and a movable substrate support disposed within the resonant cavity, the substrate support coupled to a facilities cable that bends based on movement of an actuator coupled to the substrate support; a processing chamber comprising:

2. The processing chamber of claim 1 , wherein the lid assembly includes a heat exchanger.

3. The processing chamber of claim 1 , wherein the spacer also comprises a plurality of heater elements.

4. The processing chamber of claim 1 , wherein the spacer comprises a liner surrounding the resonating cavity.

5. The processing chamber of claim 4 , wherein the liner comprises a first portion and a second portion, the second portion comprising a thickness less than a thickness of the first portion.

6. The processing chamber of claim 1 , wherein the rotatable magnetic assembly comprises a plurality of magnets coupled to a magnetic actuator.

7. The processing chamber of claim 1 , further comprising a variable pressure system coupled to the chamber body.

8. The processing chamber of claim 7 , wherein the variable pressure system comprises a first pump and a second pump.

9. The processing chamber of claim 1 , wherein the facility cable comprises a single piece of conductor.

10. A processing chamber as described in claim 5, wherein a portion of the liner adjacent to or within the first portion is maintained at a higher temperature than a portion of the liner adjacent to or within the second portion.

11. The processing chamber of claim 4, wherein the liner includes an inner surface exposed within the resonant cavity.

12. The processing chamber of claim 11, wherein the inner surface comprises at least one of aluminum, titanium, or an alloy thereof.

13. The processing chamber of claim 11, wherein the inner surface is coated with aluminum, titanium, or an alloy thereof.

Citation Information

Patent Citations

  • Electrode assembly and apparatus for the same

    JP1988147322A

  • Apparatus and method for plasma reaction using electromagnetic RF coupling

    JP1994112166A

  • Plasma treatment apparatus

    JP1995288195A

  • Plasma treatment apparatus

    JP2004039844A

  • Magnetron with swiveling central magnet for curved sputtering targets