Welding quality inspection method for electrode tab-electrode lead welds

A non-destructive vision-based method for inspecting welding quality between electrode tabs and leads in lithium secondary batteries addresses the limitations of destructive testing, enabling accurate and comprehensive quality assessment.

JP7566400B2Active Publication Date: 2024-10-15LG ENERGY SOLUTION LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2022549185
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-09-10
Filing Date
2021-06-22
Publication Date
2024-10-15
Estimated Expiration
2041-06-22

AI Technical Summary

Technical Problem

Existing methods for inspecting the welding quality between an electrode tab and electrode lead in lithium secondary batteries are destructive and unreliable, limiting the ability to perform 100% inspection.

Method used

A non-destructive inspection method using vision inspection to measure the size of welding marks, such as the diagonal length or area, and compare it with reference values to determine weak, excessive, or normal welding.

Benefits of technology

Enables accurate and non-destructive 100% inspection of welding quality, allowing for the detection of weak or excessive welding, and complements destructive tensile strength testing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566400000002
    Figure 0007566400000002
  • Figure 0007566400000003
    Figure 0007566400000003
  • Figure 0007566400000004
    Figure 0007566400000004
Patent Text Reader

Abstract

The present invention is a method for inspecting the welding quality of the electrode tab-electrode lead welds of a pouch-type lithium secondary battery, and includes a vision inspection step of recognizing welding marks in the welds using a vision inspection device, a measurement step of measuring the size of the recognized welding marks, and a judgment step of comparing the measured size with a reference value and judging the welds as one of weak welding, overwelding, and normal welding.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims the benefit of priority based on Korean Patent Application No. 10-2020-0116258, filed on September 10, 2020, and all contents disclosed in the documents of said Korean patent application are incorporated herein by reference.

[0002] The present invention relates to a method for inspecting welding quality, which determines whether a weld between an electrode tab and an electrode lead is weakly welded, over-welded, or normally welded. [Background technology]

[0003] As technological development and demand for mobile devices increases, the demand for secondary batteries as an energy source is rapidly increasing. Among such secondary batteries, lithium secondary batteries, which exhibit high energy density and working potential, long cycle life, and low self-discharge rate, have been commercialized and are widely used.

[0004] A lithium secondary battery has a structure in which an electrode assembly having a porous separator interposed between a positive electrode and a negative electrode, each of which has an active material applied to a current collector, is impregnated with a non-aqueous electrolyte containing a lithium salt.

[0005] Such lithium secondary batteries are classified into can-type secondary batteries, in which the cell assembly is housed in a metal can, and pouch-type secondary batteries, in which the cell assembly is housed in a pouch case made of an aluminum laminate sheet, depending on the shape of the exterior case.

[0006] Pouch-type lithium secondary batteries have the advantages of low manufacturing costs, high energy density, and ease of configuring a large-capacity battery pack through series or parallel connection. For this reason, they have been attracting attention as a power source for recent electric vehicles and hybrid vehicles. Such pouch-type lithium secondary batteries have a structure in which a cell assembly, to which plate-shaped electrode leads are connected, is sealed in a pouch case together with an electrolyte. A portion of the electrode lead is exposed to the outside of the pouch case, and the exposed electrode lead is used to electrically connect to a device in which the secondary battery is installed or to electrically connect secondary batteries to each other.

[0007] A pouch-type lithium secondary battery includes an electrode assembly, a plurality of electrode tabs extending from the electrode assembly, electrode leads welded to the electrode tabs, and a pouch exterior material that receives the electrode assembly.

[0008] Such electrode tabs extend from each electrode plate of the electrode assembly, and the electrode leads are electrically connected to the electrode tabs extending from each electrode plate by welding, and are joined in a form in which a portion of the electrode leads is exposed to the outside of the pouch exterior material.

[0009] When welding the electrode tab and the electrode lead, laser welding, resistance welding, and ultrasonic welding can be used. Here, ultrasonic welding is a technique that generates ultrasonic vibrations of 10 kHz to 75 kHz and welds metals through ultrasonic vibration friction heat between metals. That is, when ultrasonic vibrations are applied by an ultrasonic welding device while the electrode tab and the electrode lead are in contact with each other, friction heat is generated at the contact surface between the electrode tab and the electrode lead, and the electrode tab and the electrode lead are welded to each other due to the friction heat generated in this way.

[0010] The welding quality of the electrode tab-electrode lead welded joint was judged by measuring the tensile strength by pulling the electrode tab and electrode lead with a gripper, respectively. However, this is a destructive inspection method and does not allow for 100% inspection, so the welding quality could only be confirmed by intermittent sample inspection.

[0011] Korean Patent No. 10-1678662 discloses a technology for determining the quality of welding by measuring the welding points in an inspection area with a vision and then comparing the total welding points with the welding strength. However, the above technology has a problem in that the inspection area is limited to some pressure points, which reduces reliability. Therefore, there is a need for the development of a non-destructive inspection method that can improve the reliability of the inspection of the welding quality of electrode tab and electrode lead welds. Summary of the Invention [Problem to be solved by the invention]

[0012] The present invention has been devised to solve the above problems, and aims to provide a method for non-destructively inspecting the welding quality of the electrode tab and electrode lead welds of a pouch-type lithium secondary battery.

[0013] Another object of the present invention is to provide an inspection method by which welding quality can be judged in a simple manner. [Means for solving the problem]

[0014] A welding quality inspection method according to one embodiment of the present invention includes a vision inspection step of recognizing a welding mark in a weld using a vision inspection device, a measurement step of measuring the size of the recognized welding mark, and a judgment step of comparing the measured size with a reference value to judge the weld mark as one of weak welding, over-welding, and normal welding.

[0015] In one embodiment of the present invention, the measuring step includes measuring a diagonal length of the weld mark.

[0016] In one embodiment of the invention, the welding can be ultrasonic welding or laser welding.

[0017] In one embodiment of the present invention, the vision inspection step may be vision inspecting an electrode lead surface of the weld.

[0018] In one embodiment of the present invention, the measuring step may further include measuring an area of ​​the weld mark.

[0019] In one embodiment of the present invention, the reference value may be obtained from correlation data of weld quality with the pitch of a welding horn.

[0020] In one embodiment of the present invention, the judgment step may be to judge the welding to be weak when the average value of the size of the weld mark is smaller than a reference value, and to judge the welding to be over-welded when the average value of the size of the weld mark is larger than the reference value.

[0021] In one embodiment of the present invention, the measuring step may be measuring the sizes of the remaining pressure points excluding the pressure points present in the first rows above / below / left / right of the weld.

[0022] In one embodiment of the present invention, the weld quality inspection method of the present invention further includes performing a tensile strength test on the individual determined to be a normal weld in the above determination step. Effect of the Invention

[0023] The present invention has the advantage that the weld quality can be judged in a simple manner since the measured value of the diagonal length of the weld mark of the weld is compared with a reference value to judge the weld quality.

[0024] The present invention performs vision inspection of the weld lead surface, which allows the boundary of the weld mark to be clearly recognized, enabling more accurate quality inspection. [Brief description of the drawings]

[0025] [Figure 1] 1 is a flowchart showing a procedure of a welding quality inspection method according to an embodiment of the present invention. [Diagram 2] 1 is a schematic diagram illustrating a vision inspection process according to an embodiment of the present invention; [Diagram 3] FIG. 1 is a conceptual diagram showing the size of a welding mark. [Figure 4] 10 is a flowchart showing the procedure of a welding quality inspection method according to another embodiment of the present invention. [Diagram 5] 1 is a diagram showing a result of vision measurement of a size of a welding mark according to an embodiment of the present invention. [Figure 6] 1 is a diagram showing a result of vision measurement of a size of a welding mark according to an embodiment of the present invention. [Figure 7] 1 is a diagram showing a result of vision measurement of a size of a welding mark according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0026] The present invention will be described in detail below. Before that, the terms or words used in the specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted as meanings and concepts that correspond to the technical idea of ​​the present invention, based on the principle that the inventor can appropriately define the concept of the term in order to best describe his own invention.

[0027] In this application, the terms "comprise" or "have" are intended to specify the presence of a feature, number, step, operation, component, part, or combination thereof described herein, and should be understood as not precluding the presence or addition of one or more other features, numbers, steps, operations, components, parts, or combinations thereof. In addition, when a layer, film, region, plate, or other part is described as being "on" another part, this includes not only the case where it is "directly on" the other part, but also the case where there is another part in between. Conversely, when a layer, film, region, plate, or other part is described as being "under" another part, this includes not only the case where it is "directly under" the other part, but also the case where there is another part in between. In addition, in this application, "on" may include not only the case where it is located on the top, but also the case where it is located on the bottom.

[0028] The present invention will be described in detail below.

[0029] Fig. 1 is a flow chart showing the procedure of a welding quality inspection method according to an embodiment of the present invention. Referring to Fig. 1, the welding quality inspection method of the present invention is a method for inspecting the welding quality of an electrode tab-electrode lead weld of a pouch-type lithium secondary battery, and includes a vision inspection step (S10) of recognizing a welding mark of the weld with a vision inspection device, a measurement step (S20) of measuring the size of the recognized welding mark, and a judgment step (S30) of comparing the measured size with a reference value and judging the welding mark as one of weak welding, over-welding, and normal welding.

[0030] The inventors of the present invention focused on the fact that the greater the weld strength of a welded part, the larger the size of the weld mark in the welded part, and came up with the present invention, which measures the size of the weld mark in a welded part to determine the weld quality.

[0031] In the present invention, the weld mark is a concept including a welding pressure point in the case of ultrasonic welding, and a weld bead in the case of laser welding.

[0032] The only conventional method for inspecting welding quality was to measure the tensile strength by pulling the electrode tab and electrode lead with a gripper, but this method destroys the battery. Therefore, it was limited to intermittent inspection such as sample testing. However, the welding quality inspection method of the present invention inspects the welding marks of the welded parts with a vision and measures the size of the welding marks recognized by the vision inspection to determine the welding quality. Since the battery is not destroyed during the welding quality inspection, it has the advantage of being possible to inspect all the batteries.

[0033] The vision inspection step (S10) includes recognizing a weld mark at a welded portion where the electrode tab and the electrode lead are welded by a vision inspection device. The vision inspection device can be a microscope or an image camera.

[0034] 2 is a schematic diagram showing a vision inspection process of an ultrasonic welded portion according to an embodiment of the present invention. Referring to FIG. 2, the vision inspection unit 210 may photograph or scan the welded portion and transmit image data or an image file to the data input unit 220. The data input unit 220 transmits data such as the image image transmitted from the vision inspection unit 210 to the measurement unit 230, and the measurement unit 230 may measure the diagonal length of the pressure point and / or the area of ​​the pressure point from the image image received from the data input unit 220 and transmit the measured values ​​to a data storage unit (not shown), a display unit 250, or a judgment unit 240. The judgment unit 240 compares the measured values ​​of the diagonal length of the pressure point and / or the area of ​​the pressure point, which represent the size of the pressure point, transmitted from the measurement unit 230 with a reference value serving as a reference for a welding defect, to judge whether the welding quality of the welded portion is weak welding, over-welding, or normal welding.

[0035] Referring to FIG. 2, in the case of ultrasonic welding, welding is performed with the electrode tab 120 positioned on the top of the electrode lead 110, and the vision inspection unit 210 vision inspects the bottom surface (back), which is the electrode lead surface, of the top and bottom surfaces (top and back) of the welded portion between the electrode tab 120 and the electrode lead 110. This is because the top surface of the welded portion is the electrode tab surface, but since the electrode tab is made of electrode current collector foil material, there is light reflection, and the boundary of the weld mark is not clearly recognized during vision inspection. On the other hand, the lead surface, which is the bottom surface of the welded portion, is different from the electrode current collector foil, and there is no problem of unclear boundary caused by light reflection. Therefore, the inspection method of the present invention is characterized in that a vision inspection is performed on the lead surface of the welded portion in the vision inspection step.

[0036] On the other hand, in the case of laser welding, unlike ultrasonic welding, welding is performed with the electrode tab positioned at the bottom of the electrode lead, so in this case the vision inspection unit vision inspects the upper surface, which is the electrode lead surface of the electrode lead welded part.

[0037] The measuring step S20 is a step of measuring the size of the weld mark from the image of the welded portion obtained by the vision inspection. In one embodiment, the size of the pressure point can be the length of the diagonal line of the weld mark. Fig. 3 is a conceptual diagram of the size of the weld mark. Referring to Fig. 3, the welded portion includes a number of weld marks, and one weld mark has a diamond shape. The size of the diamond-shaped weld mark can be measured by the length of the diagonal line (a, b), which is the distance between two opposite vertices.

[0038] In one embodiment, the size of the weld mark can be measured by measuring the area of ​​the weld mark. There are various methods for measuring the area of ​​the weld mark, but one preferred example is measuring it in units of pixels of a video image. This is preferred because it is possible to apply a uniform measurement standard that can be automated by identifying the number of pixels that correspond to the area occupied by the weld mark in the video image.

[0039] In one embodiment, the measuring step may measure the size of the remaining pressure points from the image of the weld obtained in the vision inspection step, excluding the pressure points present in the first row above / below / left / right of the weld.

[0040] 6 to 7 are diagrams showing image images of welds obtained by a vision inspection unit according to an embodiment of the present invention. FIG. 6 is an image image of the lead surface at the welded portion between the positive electrode tab and the lead, and FIG. 7 is an image image of the lead surface at the welded portion between the negative electrode tab and the lead. The measurement unit measures the area and diagonal length (width, height) of a number of weld marks from the image images of FIG. 6 and FIG. 7, and can display these measured values ​​through the display unit. The size of all weld marks in the inspection area can be measured, but the pressure points present in the first row of each of the top / bottom / left / right are excluded from the measurement object. Referring to FIG. 6, it can be seen that the pressure points present in the first row at the top are significantly smaller in size than the other pressure points. Referring to FIG. 7, the pressure points present in the first row at the bottom of the inspection area are significantly smaller in size than the other pressure points. Therefore, such weld marks are excluded during the weld quality inspection because they become noise.

[0041] The judgment step S30 is a step of judging whether or not there is a welding defect in the welded portion by comparing the diagonal length and / or area of ​​the weld mark measured in the measurement step S20 with a reference value. The reference value includes a process of setting a numerical range of the size of the weld mark that satisfies normal welding as a reference value in advance from data of the welding quality result according to the size of the weld mark, and judging that the weld mark is weakly welded if it is below the set reference value, over-welded if it is above the reference value, and normal welding if it meets the reference value.

[0042] In one embodiment, the reference value may be obtained from correlation data of welding quality depending on the pitch of a welding horn. Here, the welding horn is a component included in an ultrasonic welding device. In ultrasonic welding, the workpiece is sandwiched between a horn and an anvil and joined by ultrasonic vibration, and the welding conditions can be determined by adjusting the pitch of the horn. In one preferred embodiment, the reference value may be set based on the horn pitch.

[0043] The length of the horn pitch is the length of one side of a diamond-shaped weld mark. Assuming that all four sides are the same length, the length of the diagonal when the horn pitch is 0.9 mm is as follows:

[0044]

number

[0045] That is, based on 1.27 mm, which is the length of the diagonal of a welding horn having a pitch of 0.9 mm, a numerical range of 70 to 80% of the above length (=0.889 mm to 1.016 mm) can be set as the reference value.

[0046] 5 shows the results of determining the welding quality according to a reference value set according to the horn pitch in accordance with one embodiment of the present invention. When the horn pitch is 0.9 mm, the reference value for normal welding is 0.0889 to 1.016 mm, so if the size of the weld mark measured in the measurement step is below the above numerical range, it is determined to be weak welding, and if it is above the above numerical range, it is determined to be overwelding. When the horn pitch is 1.2 mm, it is also possible to determine weak welding, overwelding, and normal welding by setting a reference value as described above.

[0047] Judging the weld quality by comparing the diagonal lengths of the weld marks has the advantage that the measurement method is simpler than judging the weld quality by comparing the weld area.

[0048] FIG. 5 shows an embodiment in which the length of the diagonal line of the weld mark is measured to determine whether or not there is a weld defect. However, it is also possible to determine whether or not there is a weld defect by measuring the area occupied by the weld mark.

[0049] Since there are multiple weld marks and the length or area of ​​each diagonal of the weld marks is different, the length or area of ​​the diagonals of the multiple weld marks can be measured, the average of the measured values ​​can be calculated, and the calculated average value can be compared with a standard value to determine the weld quality.

[0050] FIG. 4 is a flow chart showing the procedure of a welding quality inspection method according to another embodiment of the present invention. Referring to FIG. 4, after performing the above-mentioned non-destructive welding quality inspection method, a process of additionally performing a tensile strength inspection on the individual determined to be a normal weld can be included. The method of measuring the size of the weld mark by vision and determining the welding quality of the present invention estimates the weld strength from the size of the weld mark, so even if the welding is actually weak, it can be determined to be a normal weld. Therefore, a tensile strength inspection is additionally performed. Since the tensile strength inspection is a destructive inspection in which the weld breaks in the inspection method, it is not possible to inspect all the individual determined to be normal, and inspection is performed intermittently on some of the individual. The inspection method of the present invention includes the above-mentioned non-destructive inspection on all the battery cells, and therefore has the advantage of being able to complement the intermittent tensile strength inspection.

[0051] Meanwhile, the battery cell to be judged as good or bad by the inspection method of the present invention may have a structure in which an electrode assembly having a structure in which a positive electrode, a separator, and a negative electrode are alternately stacked is housed inside a battery case. The positive electrode and the negative electrode each have a structure in which an active material layer is formed by applying an electrode slurry containing an electrode active material to a current collector, followed by a drying and rolling process. When the electrode assembly is housed in the battery case, an electrolyte solution can be injected therein and sealed to manufacture a battery cell.

[0052] Here, the current collector may be a positive electrode current collector or a negative electrode current collector, the electrode active material may be a positive electrode active material or a negative electrode active material, and the electrode slurry may further include a conductive material and a binder in addition to the electrode active material.

[0053] In the present invention, the positive electrode current collector is generally made to a thickness of 3 to 500 μm. Such a positive electrode current collector is not particularly limited as long as it has high conductivity without inducing chemical changes in the battery. For example, stainless steel, aluminum, nickel, titanium, baked carbon, or aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. may be used. The current collector may have fine irregularities on its surface to increase the adhesive force of the positive electrode active material, and may be in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.

[0054] In the case of a negative electrode current collector sheet, it is generally made to a thickness of 3 to 500 μm. Such a negative electrode current collector is not particularly limited as long as it is conductive and does not induce chemical changes in the battery. For example, copper, stainless steel, aluminum, nickel, titanium, baked carbon, copper or stainless steel surface treated with ecarbon, nickel, titanium, silver, etc., aluminum-cadmium alloy, etc. can be used. In addition, like the positive electrode current collector, the binding force of the negative electrode active material can be strengthened by forming fine irregularities on the surface, and it can be used in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.

[0055] In the present invention, the positive electrode active material is a material capable of undergoing an electrochemical reaction, and contains two or more transition metals as a lithium transition metal oxide. For example, lithium cobalt oxide (LiCoO2) substituted with one or more transition metals, layered compounds such as lithium nickel oxide (LiNiO2), lithium manganese oxide substituted with one or more transition metals, and lithium manganese oxide having the chemical formula LiNi 1-y M y Lithium nickel oxide represented by the formula LiO2 (where M=Co, Mn, Al, Cu, Fe, Mg, B, Cr, Zn or Ga, containing at least one of the above elements, and 0.01≦y≦0.7), 1+z Ni 1 / 3 Co 1 / 3 Mn 1 / 3 O2, Li 1+z Ni0.4 Mn 0.4 Co 0.2 Like O2 and the like, Li 1+z Ni b Mn c Co 1-(b+c+d) M d O (2-e) A e (Here, -0.5 ≦ z ≦ 0.5, 0.1 ≦ b ≦ 0.8, 0.1 ≦ c ≦ 0.8, 0 ≦ d ≦ 0.2, 0 ≦ e ≦ 0.2, b + c + d < 1, M = Al, Mg, Cr, Ti, Si or Y, and A = F, P or Cl) Lithium nickel cobalt manganese composite oxide represented by the chemical formula Li 1+x M 1-y M' y PO 4-z X z (Here, M = transition metal, preferably Fe, Mn, Co or Ni, M' = Al, Mg or Ti, X = F, S or N, and 0.5 ≦ x ≦ +0.5, 0 ≦ y ≦ 0.5, 0 ≦ z ≦ 0.1) Examples include olivine-type lithium metal phosphate represented by the formula, but are not limited thereto.

[0056] The negative electrode active material is, for example, carbon such as graphitizable carbon and graphite-based carbon; Li x Fe2O3 (0 ≦ x ≦ 1), Li x WO2 (0 ≦ x ≦ 1), Sn x Me 1-x Me’ y O z (Me: Mn, Fe, Pb, Ge; Me’: Al, B, P, Si, Group 1, Group 2, Group 3 elements of the periodic table, halogen; 0 < x ≦ 1; 1 ≦ y ≦ 3; 1 ≦ z ≦ 8) and other metal composite oxides; lithium metal; lithium alloy; silicon-based alloy; tin-based alloy; metal oxides such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO, GeO2, Bi2O3, Bi2O4, Bi2O5; conductive polymers such as polyacetylene; Li-Co-Ni-based materials and the like can be used.

[0057] The conductive material is usually added in an amount of 1 to 30% by weight based on the weight of the entire mixture containing the positive electrode active material. Such a conductive material is not particularly limited as long as it has conductivity without inducing a chemical change in the battery. For example, graphite such as natural graphite or artificial graphite, carbon black such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, and thermal black, conductive fibers such as carbon fiber and metal fiber, metal powders such as carbon fluoride, aluminum, and nickel powder, conductive whiskers such as zinc oxide and potassium titanate, conductive metal oxides such as titanium oxide, and conductive materials such as polyphenylene derivatives can be used.

[0058] The binder is a component that aids in binding the active material and conductive material, etc., and binding to the current collector, and is usually added in an amount of 1 to 30% by weight based on the weight of the entire mixture including the positive electrode active material. Examples of such binders include polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene terpolymer (EPDM), sulfonated EPDM, styrene-butylene rubber, fluororubber, and various copolymers.

[0059] Meanwhile, the separator is an insulating thin film that is interposed between the positive and negative electrodes and has high ion permeability and mechanical strength. The pore diameter of the separator is generally 0.01 to 10 μm, and the thickness is generally 5 to 300 μm. As such a separator, for example, a sheet or nonwoven fabric made of an olefin polymer such as polypropylene, which is chemically resistant and hydrophobic, glass fiber, or polyethylene, etc. is used.

[0060] In the electrode assembly, an electrode tab is formed on one side of the electrode, and the electrode tab may be a positive electrode tab or a negative electrode tab. A positive electrode lead and a negative electrode lead are connected to the positive electrode tab and the negative electrode tab, respectively. The positive electrode lead and the negative electrode lead are drawn out to the outside of the battery case and serve as terminals electrically connected to the outside. In this case, the positive electrode lead and the negative electrode lead may be joined to the positive electrode tab and the negative electrode tab, respectively, by welding.

[0061] Meanwhile, the battery case is not particularly limited as long as it is used as an exterior material for packaging a battery, and may be cylindrical, rectangular, or pouch-shaped, and more specifically, a pouch-shaped battery case may be used. The pouch-shaped battery case is generally made of an aluminum laminate sheet, and may be composed of an inner sealant layer for sealing, a metal layer for preventing the penetration of substances, and an outer resin layer forming the outermost part of the case. Hereinafter, detailed description of the battery case will be omitted since it is well known to ordinary skilled artisans.

[0062] The electrodes constituting the electrode assembly have electrode tabs drawn out on one side for electrical connection to an external device or another battery cell. The electrode tabs may be positive or negative tabs. The positive and negative tabs are connected to electrode leads by welding, respectively. The electrode leads are drawn out to the outside of the battery case.

[0063] Meanwhile, in this specification, terms indicating directions such as up, down, left, right, front, and back are used, but it is obvious that such terms are used for convenience of explanation and may change depending on the position of the object in question, the position of the observer, etc. [Explanation of symbols]

[0064] 110: Electrode lead 120: Electrode tab a, b: Diagonal length of weld mark

Claims

1. A method for inspecting the welding quality of an electrode tab-electrode lead weld of a pouch-type lithium secondary battery, comprising: a vision inspection step of recognizing welding marks on the welded parts using a vision inspection device; A measuring step of measuring the size of the recognized welding mark; and determining whether the welding is weak, over, or normal by comparing the measured size with a reference value; The measuring step includes measuring a length of a diagonal line of the weld mark, The judgment step includes comparing the measured length of the diagonal line with a reference value, and judging the welding as weak if the measured length is below the reference value, as overwelding if the measured length is above the reference value, and as normal welding if the measured length meets the reference value.

2. The weld quality inspection method according to claim 1 , wherein the welding is an ultrasonic welding or laser welding method.

3. The welding quality inspection method according to claim 1 or 2, wherein the vision inspection step vision inspects an electrode lead surface of the welded portion.

4. The weld quality inspection method according to claim 1 , wherein the measuring step further comprises measuring an area of ​​the weld mark.

5. The method of claim 2 , wherein the reference value is obtained from correlation data of weld quality as a function of welding horn pitch.

6. 6. The method for inspecting weld quality according to claim 1, wherein the determining step determines that the weld is weakly welded when the average value of the size of the weld mark is smaller than a reference value, and determines that the weld is over-welded when the average value of the size of the weld mark is larger than the reference value.

7. The weld quality inspection method according to claim 1 , wherein the measuring step measures the size of the remaining pressure points excluding the pressure points present in the first rows above / below / left / right of the weld.

8. The weld quality inspection method according to claim 1 , further comprising carrying out a tensile strength inspection on an individual determined to be a normal weld in the determining step.

Citation Information

Patent Citations

  • Welding inspection method

    JP2000221016A

  • Apparatus and method for inspecting ultrasonic welding, and apparatus and method for ultrasonic welding

    JP2008145252A

  • Ultrasonic joining monitor and its method

    JP2009103691A

  • Battery

    JP2013165054A