Superconducting resonant cavity with laser welded seams and method of forming same

By relocating weld seams and employing laser welding to minimize surface roughness and magnetic field variations, the SRF cavity's performance is enhanced, addressing issues of dielectric breakdown and quenching.

JP7573670B2Active Publication Date: 2024-10-25II VI DELAWARE INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023041136
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-06-26
Filing Date
2023-03-15
Publication Date
2024-10-25
Estimated Expiration
2039-05-20

AI Technical Summary

Technical Problem

Superconducting radio frequency (SRF) cavities face limitations due to dielectric breakdown, field emission, and premature quenching caused by surface roughness and magnetic field enhancements at the equatorial weld seam, leading to reduced quality factor and acceleration gradient.

Method used

Repositioning weld seams to areas less critical for performance and using laser welding to form seamless connections, minimizing surface roughness and contamination, thereby reducing magnetic field variations.

Benefits of technology

Enhances the performance of SRF cavities by maintaining a smooth, uninterrupted inner surface, reducing the risk of quenching, and improving the quality factor and acceleration gradient.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573670000001
    Figure 0007573670000001
  • Figure 0007573670000002
    Figure 0007573670000002
  • Figure 0007573670000003
    Figure 0007573670000003
Patent Text Reader

Abstract

To provide a superconducting radio frequency (SRF) cell, a method of manufacturing the SRF cell, a welded seam usable with the SRF cell or another object, and a method of manufacturing the welded seam.SOLUTION: The superconducting radio frequency cell includes a body defining a hollow cavity having first and second opposite ends, an axis that extends between first and second irises, and an equator around the axis between the first and second irises. The body includes at least a first welded seam around the axis at a location on the body spaced from the equator. Each welded seam extends through the body and has opposite sides terminating proximate an interior and an exterior of the body, and each weld seam includes a first, conduction weld formed on one side of the welded seam and a second weld formed on the opposite side of the welded seam. The second weld can be a conduction weld, a keyhole weld, or a transition weld.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a superconducting radio frequency (SRF) cell, a method for manufacturing an SRF cell, an SRF cell or other objects, and methods for forming the welded seam Regarding the law. [Background technology]

[0002] The RF cavity is used to accelerate a group of charged particles towards a target. In many applications, the advantage of using a cavity with a superconducting inner surface is that the cavity outweighs the increased costs associated with cryogenically cooling the cavity. and the acceleration gradient. The quality factor (Q0) is the loss of the system with each cycle. A high quality factor reduces operating costs by reducing the need for cryogenic cooling. The acceleration gradient of the cavity represents the ability to accelerate particles. F) The acceleration gradient across the cavity is typically several million volts per meter. Gradient The higher the accelerating field, the smaller the cavity required to operate the system. However, higher gradients require higher internal magnetic fields, which reduces initial and operating costs. This requires a high-temperature field, pushing the performance limits of superconducting inner surfaces.

[0003] The SRF cavity is limited by any factor that would cause electrical breakdown in the superconducting field. Generally, this transition from the superconducting state is called a "quench." A high voltage along the inside of the cavity ejects electrons from the surface, generating X-rays and creating a cavity This is commonly known as field emission. A high intensity magnetic field is used to form a cavity or a coating inside the cavity. The magnetic field exceeding the critical magnetic field of niobium, which is known to be a superconducting material, can be reached. In addition, surface variations can cause the exposed surface of the cavity to collapse and quench. This can increase the amount of magnetic field that is absorbed, which can lead to premature quenching. The increase in magnetic flux experienced by the cavity due to is known as the field enhancement.

[0004] To obtain the maximum quality factor and acceleration gradient within a given cavity, the cavity The interior surfaces should be smooth, clean and uninterrupted. Microscopic surface contaminants Even in the case of ZnO, the superconducting state can be destroyed by exposing the non-superconducting phase to a high RF electric field. may act as points of field emission by concentrating the electric field. Surface roughness in the high magnetic field region leads to an enhancement of the local magnetic field to a level above the critical value for niobium. This can cause a breakdown in the superconducting state. Surface roughness in the junctions of the junctions can cause field emission, heating of the surface and destruction of the superconducting state. This could result in:

[0005] Developments in the field of SRF cavity fabrication have focused on the prevention of cavity destruction by contamination and field emission. The Q0 and acceleration gradient limitations are mainly due to the This is due to exceeding the critical magnetic field, which is the magnetic field at which the cavity transitions from its superconducting state to This is the magnetic field beginning to transition.

[0006] Current cavity designs place the maximum magnetic field along the "equator" of the cavity, The first and second half cells that form the pit are sometimes called the "equatorial weld seam." The cavity shapes are also designed to optimize different performances. The signal may be adjusted to reduce the

[0007] Niobium welding for SRF cavities is currently performed along the equator, but outside the cell equator. It is a "blind" process carried out in a vacuum using an electron beam oscillating around the The process, although well studied and controlled, still produces inconsistent results. Post-treatment of the surface consists of "on-stick grinding" and "strip-cutting" prior to chemical etching of the weld. This is limited to "tick-on camera" inspection.

[0008] Referring to FIG. 15, in one preferred non-limiting embodiment or example, a single superconducting The line frequency (SRF) cavity 2 may include a number of superconducting cells 4 connected in series. The exemplary SRF cavity 2 shown in FIG. In one example, the input 6 is adapted to couple to an RF energy source. The RF energy source generates a standing wave in the SRF cavity 2, and the standing wave is a particle By accelerating the particles, they pass from the input end 6 through the cavity 2 and then into another SRF cavity. The output terminal 8 can be connected to an RF amplifier (not shown). The energy is input to the SRF cavity 2 at its input end 6 via an RF input port 7. Input to F cavity 2.

[0009] With continued reference to FIG. 16 and FIG. 15, one preferred, non-limiting embodiment In the example, more specifically, RF electrical energy received at RF input port 7 is Use for accelerating particles (e.g., a particle beam) along the axis 20 of the RF cell 4. The electric and magnetic fields that can be generated within each cell 4 are shown in FIG. The passage 10 and the apertures 12-1 and 12-2 are defined on either side of the cell 4. As will be appreciated, in use, the SRF cavity 2 is typically heated to a superconducting temperature within a suitable enclosure 13. It is cooled at each temperature (Figure 15).

[0010] With continued reference to FIG. 17, and with continued reference to FIGS. 15 and 16, one preferred, non-limiting embodiment In an embodiment or example, the prior art cell 4 includes a first half cell 14 and a second half cell 15. The first and second half-cells are formed from a first half-cell 16 (which may be identical to the first half-cell 14). The outer or outer shells of the cells 14 and 16 are joined by welding to form the cell 4. The weld seam (or weld circle) where the first half cell 14 and the second half cell 16 are welded together defines the equator 18 of the cell 4. Finally, the half cells 14 and 16 each have an aperture 1 2-1 and 12-2, and when half cells 14 and 16 are joined together, cell The equator 18 of the cell 4 is defined at half the distance between the apertures 12-1 and 12-2 of the cell 4. In the figure, apertures 12-1 and 12-2 are spaced apart by a distance X, and equator 18 is 12-1 and 12-2 are located at distances Y1 and Y2, respectively. may be the same distance.

[0011] In one preferred, non-limiting embodiment or example, the equator of a sphere or planet (such as the Earth) Similarly, the equator 18 is a line of latitude or a circle of latitude, and is located midway between apertures 12-1 and 12-2. The apertures are like those of a sphere or planet, corresponding to the north and south poles of the sphere or planet. Similar to the equator of a sphere or planet that divides a planet into a northern and southern hemisphere, the equator 18 of cell 4 is The dividing line between the first half-cell 14 and the second half-cell 16. 8 is at 0° latitude in cell 4. Finally, cell 4, in one example, is at apertures 12-1 and 12 -2 defines an axis of symmetry of the cell 4, for example an axis of rotational symmetry 20.

[0012] Improves existing SRF cavity designs, which, when in use, experience the highest magnetic field strength near the equator To provide an SRF cavity having improved performance and a method for manufacturing the SRF cavity. It is desirable to do so. Summary of the Invention [Means for solving the problem]

[0013] In general, weld seams are placed in areas that are less critical to the performance of the superconducting (internal) surface. A method is provided for forming a niobium superconducting radio frequency (SRF) cell, the method comprising: Such a repositioning allows for better treatment of the inner surface at the equator of the cell.

[0014] Improved weld seam, SRF cell with improved weld seam, and improved A method for forming a weld seam is also provided.

[0015] These and other features of the present invention will become more apparent from the following description taken in conjunction with the accompanying drawings. It will be. [Brief description of the drawings]

[0016] [Figure 1]FIG. 1 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0017] [Diagram 2] FIG. 2 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0018] [Diagram 3] FIG. 3 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0019] [Figure 4] FIG. 4 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0020] [Diagram 5] FIG. 5 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0021] [Figure 6] FIG. 6 is a cross-sectional view of one preferred non-limiting embodiment or exemplary SRF cell according to the principles of the present invention.

[0022] [Figure 7] FIG. 7 is a diagram of one preferred non-limiting embodiment or exemplary method of forming an SRF cell according to the principles of the present invention.

[0023] [Figure 8A] FIG. 8A is a front view of one non-limiting embodiment or example of a laser conduction weld applied to one side of a seam formed by a pair of objects butted together. [Figure 8B] FIG. 8B is a cross-sectional view of one non-limiting embodiment or example of a laser conduction weld applied to one side of a seam formed by a pair of objects butted together, taken along line 8B-8B of FIG. 8A.

[0024] [Figure 9A] FIG. 9A is a front view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam, overlapping the conduction weld of FIG. 8A. [Figure 9B] FIG. 9B is a cross-sectional view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam, overlapping the conduction weld of FIG. 8B, taken along line 9B-9B of FIG. 9A.

[0025] [Figure 10A] FIG. 10A is a front view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam that substantially overlaps the conduction weld of FIG. 8A. [Figure 10B] FIG. 10B is a cross-sectional view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam, substantially overlapping the conduction weld of FIG. 8B, taken along line 10B-10B of FIG. 10A.

[0026] [Figure 11A] FIG. 11A is a front view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam that does not overlap (is spaced apart) from the conduction weld of FIG. 8A. [Figure 11B] FIG. 11B is a cross-sectional view of one non-limiting embodiment or example of a laser keyhole weld on the opposite side of the seam that does not overlap (is spaced apart) from the conduction weld of FIG. 8B, taken along line 11B-11B of FIG. 11A.

[0027] [Figure 12A] FIG. 12A is a front view of one non-limiting embodiment or example of a laser conduction weld on the opposite side of the conduction weld seam of FIG. 8A. [Figure 12B] FIG. 12B is a cross-sectional view of one non-limiting embodiment or example of a laser conduction weld taken along line 12B-12B of FIG. 12A on the opposite side of the conduction weld seam of FIG. 8B.

[0028] [Figure 13A] FIG. 13A is a front view of one non-limiting embodiment or example of a laser transition weld on the opposite side of the conduction weld seam of FIG. 8A. [Figure 13B] FIG. 13B is a cross-sectional view of one non-limiting embodiment or example of a laser transition weld on the opposite side of the conduction weld seam of FIG. 8B taken along line 13B-13B of FIG. 13A.

[0029] [Figure 14] FIG. 14 is a diagram of one preferred non-limiting embodiment or exemplary method of laser welding first and second objects in accordance with the principles of the present invention.

[0030] [Figure 15] FIG. 15 is a partial diagram of a prior art superconducting radio frequency (SRF) cavity that includes a plurality of prior art SRF cells.

[0031] [Figure 16] FIG. 16 is a generalized schematic diagram of a cross-section of a prior art SRF cell that can be used in the SRF cavity shown in FIG.

[0032] [Figure 17] FIG. 17 is an exemplary cross-sectional view of a single prior art SRF cell shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0033] Various non-limiting embodiments will now be described with reference to the accompanying drawings, in which like reference numerals refer to like or equivalent parts, and in which: corresponds to a functionally equivalent element.

[0034] For purposes of the following description, the terms "end," "top," "bottom," "right," "left," "Vertical", "Horizontal", "Top", "Bottom", "Transverse", "Longitudinal" and their The derivatives of the above refer to the examples shown in the drawings, but the examples are not limited to those shown in the drawings unless expressly stated otherwise. It is understood that various alternative variations and step sequences may be envisioned unless otherwise stated. The specific examples illustrated in the accompanying drawings and described in the following specification are to be construed as merely illustrative examples. It should also be understood that the present invention is an exemplary embodiment or aspect of the present invention. The specific examples or embodiments disclosed herein should not be construed as limiting.

[0035] Thus, the background art includes the prior art cell 4 and the cell 4 in which one or more cells 4 are used. The SRF cavity 2 is described below, and in the following description, several Examples of cells according to some preferred, non-limiting embodiments or examples are described.

[0036] In one preferred, non-limiting embodiment or example, the cross-sections of the cells shown in the various figures is a TESLA configuration. However, the present invention may be used in conjunction with cells of other configurations. This should not be construed in a limiting sense, as it is anticipated that other Examples of cell geometries include low-loss geometries and re-entrant geometries.

[0037] Referring to FIG. 1, in one preferred non-limiting embodiment or example, instead of cell 4, The cell 22 that can be used in combination includes a first partial cell 24 and a second partial cell 26. These are joined together at weld seams 28 at latitudes other than the equator 30 of the cells 22. The cell 22 is divided into a first partial cell 24 and a second partial cell 26. The cell 22 may include an axis 34, This is an axis of symmetry, for example an axis of rotational symmetry, between the apertures 32-1 and 32-2, which are spaced apart by a distance X. In one example, axis 34 extends through the centers of apertures 32-1 and 32-2. It is alive.

[0038] In one preferred non-limiting embodiment or example, the first partial cell 24 and the second partial cell The partial cells 26 can have different shapes / sizes. For example, the second partial cell 2 The distance from the aperture 32-2 of the first partial cell 24 to the weld seam 28 is 2 to the weld seam 28. In one embodiment or example, each cell 24, 26 may be fabricated from niobium.

[0039] In one preferred, non-limiting embodiment or example, each aperture described herein is circular. However, this should not be construed in a limiting sense. Each reference in this document to the distance or location of a weld seam from other elements shall This should be understood as the distance from the element to the center of the weld seam. The seam may have a width (measured in the direction of axis 34) that is formed during the welding operation. , the width may vary depending on the weld seam, within a single weld seam or between different weld seams. Or, a part of it may change depending on the conditions when it is formed.

[0040] In one preferred, non-limiting embodiment or example, the welded joint of cell 22 shown in FIG. The eye 28 is disposed along an axis 34 in a direction at least 5 mm from the equator 30 toward the aperture 32-1. In this example, the equator 30 is not a weld seam. The weld seam 28 is located at the first part. 2. Connect the first cell weld edge 36 of the partial cell 24 to the second cell weld edge 38 of the second partial cell 26. In other words, the weld seam 28 is formed by welding the first cell weld edge 36 and second cell weld edge 38 together.

[0041] With reference to FIG. 2 and continuing reference to FIG. 1, one preferred, non-limiting embodiment In this example, another exemplary cell 22 includes a first partial cell 24 including a first cell weld edge 36. and a second partial cell 26 including a second cell weld edge 38. Disposed between the second partial cell 26 is a pipe section 40, The section 40 includes a first pipe weld edge 42 and a second pipe weld edge 44. They face a first cell weld edge 36 and a second cell weld edge 38, respectively.

[0042] In one preferred, non-limiting embodiment or example, to complete the formation of the cell 22 shown in FIG. To achieve this, the first cell weld edge 36 is welded to the first pipe weld edge 42 to form a first weld. The second cell weld edge 38 is welded to the second pipe weld edge 44 to form a seam 46. A second weld seam 48 is formed. The first weld seam 46 and the second weld seam 48 are formed. The order in which the components are formed should not be construed in a limiting sense.

[0043] In one preferred non-limiting embodiment or example, the second weld seam 48 is Between -1 and 32-2, on the equator 30 located at the latitude coordinate 0° of the body of cell 22 The first weld seam 46 may be formed at a latitude other than the equator 30. As an example, the first weld seam 46 may extend from the equator 30 along the axis 34 to the draw 32- 1.

[0044] Referring to FIG. 3, one preferred, non-limiting embodiment or example of another exemplary cell 22 is 3, the pipe section 50 is welded to the first cell weld edge 36 to form a first weld seam. 56, and a second pipe weld edge 52 welded to the second cell weld edge 38 to form a second and a second pipe weld edge 54 forming a weld seam 58 at the equator 3. 0 is disposed between the first weld seam 56 and the second weld seam 58. In a preferred non-limiting embodiment or example, the equator 30 is formed by a first aperture 32-1 and a second aperture 32-2. 32-2, at the latitude coordinate 0° of the cell 22 forming the main body. In one example, the equator 30 is midway or between the first weld seam 56 and the second weld seam 58. In one example, the equator 30 can be disposed between the apertures 32-1 and 32-2. It can be placed in the middle or midway.

[0045] As one preferred, non-limiting embodiment or example, the exemplary cell 22 ( and in all exemplary cells 22 described herein, the pipe section 50 The imaginary line extension of the inner surface 60 and the inner surfaces 62 and 63 of the first partial cell 24 and the second partial cell 26 are and inner surface 64 are respectively colinear. The inner surface 60 of the section 50 may be straight or curved, and the first weld seam 5 6 and the inner surface 62 adjacent the second weld seam 58 and the inner surface 64 adjacent the second weld seam 58. or curvature, and such first weld seam 56 and second weld seam The inner surfaces 60, 62 and 64 adjacent the first weld seam 56 and the second weld seam 58 are A continuous or substantially continuous smooth and uninterrupted interior of the cells 22 adjacent the seam 58 In one example, the inner surface of the cell 22 may include a first weld seam 56 and a second weld seam 57. and the welding operation used to form the second weld seam 58. The presence of roughness and contamination and / or examples used to reduce roughness and contamination The interior surface of the cell 22 is polished at all points around the periphery by a process such as buffered chemical polishing or electrolytic polishing. It may not necessarily be smooth. It may be continuous or substantially continuous, smooth, and uninterrupted. A similar description of the inner surface adjacent to the weld seam 28 shown in FIG. A first weld seam is applied to the inner surfaces of the cell 24 and the second partial cell 26 and is shown in FIG. The pipe 40 adjacent to the joint 46 and the second weld seam 48, the first partial cell 24 and the second partial cell 25 are welded to the pipe 40 adjacent to the joint 46 and the second weld seam 48. The inner surface of the second partial cell 26 is also applied.

[0046] Referring to FIG. 4, in one preferred, non-limiting embodiment or example, a pipe section 70 can be disposed between the first partial cell 24 and the second partial cell 26. In this example, In the example, the pipe section 70 is made up of a first pipe section 72 and a second pipe section 73. 74 are welded together to form a third weld seam shown by solid line 76. Thus, it is formed.

[0047] In this example, the first weld seam 56 and the second weld seam 58 are the first weld seam 56 and the second weld seam 58 shown in FIG. The weld seam 56 and the second weld seam 58 may be formed in the manner described above with respect to the weld seam 56 and the second weld seam 58. In the example shown in FIG. 4, a first weld seam 56, a second weld seam 58, and The third weld seam 76 can be formed in any order. For example, the first pipe section The first pipe section 72 and the second pipe section 74 are first arranged in any order in the first partial cell 2. 4 and the second partial cell 26, the first weld seam 56 and the second weld seam 58 may then be formed. A third weld seam 76 may then be formed on the first pipe section 72. and the second pipe section 74. First, the first pipe section 72 and the second pipe section 74 are joined together, and then the third pipe section 76 is joined together. A weld seam 76 may then be formed between the first pipe section 72 and the second pipe section 73. The pipe section 74 is welded together with the pipe section 7 0 to the first partial cell 24 and the second partial cell 26 in any order to form a weld seam. 56 and weld seam 58 may be formed. In one example, pipe sections 70 and And the pipe section 72 may be a half-pipe section.

[0048] In one preferred non-limiting embodiment or example, the third weld seam 76 is The third weld seam 76 may be offset from the equator 30. Alternatively, the third weld seam 76 may be on the equator 30. The width 78 of the first pipe section 72 and the width 74 of the second pipe section 80 indicates whether the third weld seam 76 is to be on the equator 30 of the cell 22. or along axis 34 in a direction away from equator 30 toward aperture 32-1 or aperture 32-2. Depending on the circumstances, a person may make choices that he or she deems appropriate and / or desirable. In the example, the first partial cell 24 and the second partial cell 25 adjacent to the weld seams 56, 58, and 76 are The inner surfaces of the pipe 26, the first pipe section 72, and the second pipe section 74 are Forming a continuous or substantially continuous, smooth, uninterrupted interior surface of the cells 22. can be done.

[0049] Referring to FIG. 5, in one preferred, non-limiting embodiment or example, the cell 22 is aligned along axis 3. 4, the distance X between the aperture 32-1 and the aperture 32-2 is greater than 50% of the distance X. In one example, the first partial cell 24 and the pipe section 84 may include a pipe section 84 having a width Z. The first cell weld edge 36 and the second cell weld edge 38 of the second partial cell 26 are welded. Therefore, the first pipe weld edge 88 and the second pipe weld edge 89 in the vicinity of the constriction 32-1 and the constriction 32-2 are The pipe weld edge 90 is joined to the first weld seam 92 and the second weld seam 9 In one example, a first weld seam 92 and a second weld seam 4 can be formed. The distance Z between the aperture 94 is 50% or more of the distance X between the aperture 32-1 and the aperture 32-2. It may be 60% or more, or 70% or more. In the example, the distance Z is about 73% of the distance X. In one example, the distance Z is about 73% of the distance X. The distance Y1 to 2-1 may be, for example, less than 5 mm, or about 2.5 mm. The minimum distance Y1 is often determined by the width of the weld seam 94. The distance Y2 from the outside of the seam 94 to the aperture 32-2 may be, for example, less than 5 mm. The minimum distance Y2 may be about 2.5 mm, and the minimum distance Y2 may be determined by the width of the weld seam 92. However, these percentages and dimensions should be interpreted in a limiting sense. isn't it.

[0050] In one preferred non-limiting embodiment or example, the equator 30 of the cell 22 is aligned with a first weld For example, the equator 30 of the cell 22 may be disposed between the seam 92 and the second weld seam 94. The weld seam 92 may be disposed intermediate the first weld seam 92 and the second weld seam 94. In the example, the equator 30 of the cell 22 may be located midway between the apertures 32-1 and 32-2. In one example, pipe section 8 adjacent weld seam 92 and weld seam 94 may be welded. 4. The inner surfaces of the first partial cell 22 and the second partial cell 24 are continuous or A substantially continuous, smooth, uninterrupted interior surface can be formed.

[0051] Referring to FIG. 6, in one preferred non-limiting embodiment or example, the cell 22 of FIG. 5 with the following exceptions. Section 84 is made up of a first partial pipe section 96 and a second partial pipe section 98. and welded together to form a third weld seam 100, The seam 100 is near or on the equator 30. 0 can be formed in any order. In one example, adjacent weld seams 92, 94 and At 100, the first partial pipe section 96 and the second partial pipe section The inner surfaces of the first partial cell 24 and the second partial cell 26 are continuous with the inner surfaces of the cells 22. Alternatively, a substantially continuous, smooth, uninterrupted interior surface may be formed.

[0052] In one preferred non-limiting embodiment or example, the pipe section 84 is a first portion A third weld seam 100 is formed prior to joining the cell 24 and the second partial cell 26. For example, it may be desirable to change the shape of the first and second weld seams 92 and 94. 100 is formed following the formation of the third weld seam 100 in the pipe section 84. a third weld seam 100 before joining the first partial cell 24 and the second partial cell 26 By forming the third weld seam 100, the roughness and contamination caused by the formation of the third weld seam 100 can be reduced. For the purpose of reducing the size of the weld seam, access to the third weld seam 100 is more easily achieved. The section 70 is connected to the first partial cell 24 and the second partial cell 26 at the weld seam 56 and The formation of the third weld seam 76 in FIG. 4 before joining with 58 is also Your explanation can be applied.

[0053] In one preferred, non-limiting embodiment or example, a pipe is connected between the first partial cell 24 and the second partial cell 25. In the previous example, the first partial cell 24 is connected to the second partial cell 26 via a weld seam. or 26, and then a welded joint is formed before the pipe is joined to another partial cell. It is desirable to reduce roughness and contamination by treating the grain. This allows for improved access to the originally formed weld seam.

[0054] Referring to FIG. 7, in one preferred, non-limiting embodiment or example, the SRF cell is The method of forming may include starting at step 200 and proceeding to step 202, A first partial cell is provided that includes a first cell weld edge and a first restriction. The method then includes: Proceeding to step 204, a second partial cell is provided that includes a second cell weld edge and a second draw. In step 206, the first and second partial cells are In step 208, the first and second welding edges are placed against each other. The SRF cell is made by joining partial cells by welding and has a weld seam at a position other than the equator of the cell. The method may then proceed to end step 210. In a typical embodiment or example, the SRF cell is welded by electron beam welding from inside or outside the cell. Forming a weld seam requires significant heat input to create the entire weld, and SR The inner surface of the SRF cell is free of undesirable rough surfaces that may adversely affect the performance of the F cell. It was observed that the surface was left with a residue. Therefore, one preferred non-limiting embodiment For example, instead of forming the weld seam by electron beam welding, the weld seam is formed by laser welding. In one preferred, non-limiting embodiment, the ferroelectric thin film may be formed by laser welding using a beam of light. In one embodiment or example, the weld seam is formed by abutting a first and a second object against each other. The joint is formed by laser welding from both sides of the defined seam, for example, a pair of welded edges The present invention is not limited to abutting the welded edges of a pair of cells against each other, and the welded edges of a pair of cells may be abutted against each other. abutting the weld edge and the pipe weld edge against each other; abutting a pair of pipe weld edges against each other; It can be said that it is possible to bring them into contact with each other.

[0055] 8A-8B, in one preferred non-limiting embodiment or example, a first The abutment of the object 300 and the second object 302 forms a common boundary or seam 30 4, which may be formed on the first and second sides 308, 310 of the seam 304. More specifically, the first side 308 and the second side 309 of the objects 300 and 302 extend between the first side 308 and the second side 309 of the objects 300 and 302. 310. By way of example and not limitation, a first The object 300 is a pipe section or a half or partial cell of an SRF cavity. By way of example and not limitation, the second object 302 may be a different pipe section. The first side 3 may be a half or partial cell of a different SRF cavity. 308 may be one side of the abutted objects 300, 302, and the second side 310 may be the It may be the other side of the adjacent objects 300, 302. In one example, the first side 308 is S The second side 310 may be at least a portion of the inner surface of the SRF cell. However, in one preferred, non-limiting embodiment, In an embodiment, the first and second objects 300, 302 may be any suitable and / or desired any suitable and / or desired object formed from a suitable material, This should not be construed in a limiting sense.

[0056] Further, in one preferred non-limiting embodiment or example, the first and second objects 30 The illustration of the first and second sides 308, 310 of the casing 302 being planar with respect to one another is indicative of a limitation. For example, the first surface 308 of the first object 300 and and the first surface 308 of the second object 302 may be misaligned (non-planar), e.g. They may have a step between them and / or they may be curved together or one curved and one flat. The shape of the slit may be any suitable and / or desired shape, such as a square or rectangular shape. Similarly, the second side 310 of the first object 300 and the second side 310 of the second object 302 may be offset (non-planar), e.g. with a step between them, and / or , either curved or one curved and one flat, or any other suitable combination; and and / or may have any desired shape.

[0057] In one preferred non-limiting embodiment or example, first and second objects 300, 30 2 together to abut the first and second sides 308 of the objects 300 and 302, 310, and once the seam 304 is formed, the first The conduction weld 312 is formed by laser welding the first surface 308 of the seam 304; and More specifically, a first portion of the first and second objects 300, 302 adjacent the seam 304 The first conduction weld 312 may be formed by laser conduction welding the surface 308. a relatively smooth exposed surface 314 extending over the sides 308 of the seam 304; 314 and a body 316 extending between the second side 310. The body 316 extends less than 25% of the distance from the first side 308 to the second side 310. The shape of the first conductive weld 312 shown in the figures is for illustrative purposes only. It should not be interpreted in a restrictive manner.

[0058] With reference to FIGS. 9A-9B and continuing to FIGS. 8A-8B, one preferred non-limiting example In a typical embodiment or example, once the first conductive weld 312 is formed, A second keyhole weld 318 is formed by laser welding a second side 310 of the eye 304. The first and second objects 300 are formed, and more specifically, adjacent the seam 304. , 302 is laser keyhole welded to a second side 310. 3 shows a relatively porous exposed surface 316 and a surface 314 of the conduction weld 312. and a relatively porous body 322 extending between the 2 may extend more than 75% of the distance from the second side 310 to the first side 308. The shape of the second keyhole weld 318 shown in the figures is for illustrative purposes only. and should not be construed in a limiting sense.

[0059] In one preferred non-limiting embodiment or example, the conduction weld 312 is first, followed by the key Once the hole welds 318 are formed on each opposing side, the seam 304 can be further or Alternatively, it may be referred to as a weld seam 304 .

[0060] In one preferred, non-limiting embodiment or example, as known in the art, In laser conduction mode welding, the power density is determined by the material of the first and second objects 300, 302, For example, the weld penetration is large enough to cause melting of niobium. This is accomplished by the heat of the laser being conducted into the material. In one example, laser conduction welding can be performed in milliseconds. This is achieved by pulsed laser welding with a pulse duration in the range of 10 ... Generally, this is controlled by the duration of the pulse. The longer the pulse, the greater the The time for heat to "conduct" through the material forming the two objects 300, 302 is also increased. In conduction welding, the conduction weld 312 is typically wider than it is deep, as shown, for example, in FIG. 8A. wide.

[0061] In one preferred, non-limiting embodiment or example, as known in the art, Laser keyhole welding achieves weld penetration by heating in a way that differs from conduction welding. Specifically, during laser keyhole welding, the power density is sufficient to heat the metal above its melting point. The metal vaporizes and produces expanding gases that By pushing outward, a keyhole or tunnel is created from the side 310 to the depth of the weld. As the beam of laser light moves along the side 310 of the seam 304, e.g. , the laser beam moves vertically to the page in FIG. 9A and horizontally from right to left in FIG. 9B. When the laser moves to the center of the weld, or vice versa, the keyhole follows and creates a deep, narrow weld. As long as the power is high enough and the speed of movement of the laser over the side 310 of the seam 304 is not excessive, The keyhole will remain open in close proximity to the laser beam. It forms deep welds at the expense of porosity, sputtering, and changes in depth. Non-limiting examples of depth variations are shown in FIGS. This is indicated by wavy line 324 in FIG. 1B.

[0062] In one preferred non-limiting embodiment or example, first and second objects 300, 30 Each of the 2 is part of an SRF cell, e.g. a pipe section, partial cell, half The sides 308 are laser welded to form a conductive weld 312, and in one example, The inner surface of the formed SRF cell (which inner surface is preferably continuous or substantially continuous) , smooth and uninterrupted), and the side 310 forms a keyhole weld 318. In one example, this could be the exterior surface of a completed SRF cell. However, this should not be construed in a limiting sense.

[0063] In one preferred non-limiting embodiment or example, the depth of the keyhole weld 318 is It can be adjusted or selected as needed. For example, as shown in Figs. 9A-9B Next, the keyhole weld 318 forms a conduction weld 318 between the first side 308 and the second side 310. 12 body portions 316. Another example is shown in FIG. 10A-FIG. 10B. By way of reference, some or all of the keyhole weld 318 is connected to the surface 314 of the conduction weld 312. The conductive weld 312 may intersect with the main body portion 316 between the first side 308. As shown by line 324 in FIG. 10B, one preferred, non-limiting embodiment or example In the embodiment, part or all of the keyhole weld 318 is welded to the surface 314 of the conduction weld 312. As yet another example, referring to FIGS. 11A-11B, a keyboard may be All of the welds 318 form at least one of the first and second objects 300, 302. A gap 326 of material may be provided to separate the conductive weld 312. In a new non-limiting embodiment or example, a single continuous keyhole weld 318 is shown in FIG. 10B, and some or all of the variations shown at 324 in FIG. 11B. The keyhole weld 318 may have a depth of 0.1 mm.

[0064] 12A-12B, in one preferred, non-limiting embodiment or example, The second side 310 of the seam 304 may be riveted before or after the first conductive weld 312 is formed. 3, a conductive weld 328 may be formed by welding the conductive weld 328 to the seam 304. A second side 310 of the adjacent first and second objects 300, 302 is laser conduction welded. The order in which the first conductive weld 312 and the second conductive weld 328 are formed is not intended to be limiting. should not be interpreted.

[0065] Similar to the first conductive weld 312, the second conductive weld 328 is formed on the surface 310 of the seam 304. an upwardly rising, relatively smooth exposed surface 330; and a gap between surface 330 and first surface 308. The first conductive weld 312 and the second conductive weld 332 may have a body extending therebetween. The weld 328 forms at least one of the first and second objects 300, 302. The gaps 334 may be formed of material. The shape of the induction weld 318 is for illustrative purposes only and should not be construed in a limiting sense. isn't it.

[0066] 13A-13B, in one preferred, non-limiting embodiment or example, A second transition weld 338 is formed at the first end of the seam 304 before or after the first conduction weld 312 is formed. More specifically, the laser welding of the two sides 310 adjacent the seam 304 By laser transition welding the second sides 310 of the first and second objects 300, 302 together. The order of forming the first conduction weld 312 and the second transition weld 338 can be: It should not be construed in a limiting sense.

[0067] As is known in the art, transition welds such as transition weld 338 are conductive. Power density of the laser beam forming the weld and power of the laser beam forming the keyhole weld A transition weld is formed at a power density of the laser beam between densities 100 and 150, for example, at an intermediate power density of the laser beam. The laser beam penetrates more and has shallower penetration than the laser beam that forms the conduction weld Forms a keyhole. In one example, a typical transition weld has an aspect ratio (depth / width) of about 1. However, this should not be construed in a limiting sense. Hole welds and transition welds are each known in the art.

[0068] The transition weld 338 is connected to an exposed surface 330 that rises above the surface 310 of the seam 304. , and a body 342 extending between the surface 330 and the first surface 308. The surface of 338 may be relatively smooth depending on the power density used to form the transition weld 338. The conduction weld 312 and the transition weld 338 are first and while being formed of a material forming at least one of the second objects 300, 302. The transition welds 338 may be spaced apart by a gap 344. The shape of the transition weld 338 shown in the figure may be, for example, For illustrative purposes only and should not be construed in a limiting sense.

[0069] Referring to FIG. 14, in one preferred non-limiting embodiment or example, first and second The method for laser welding objects 300, 302 together begins at step 330 with steps 332, the first and second objects 300, 302 defining a seam 304. The method then proceeds to step 334, where a first The sides 308 of the substrate 302 are laser conduction welded to form a conduction weld 312. The method then proceeds to step 3. 36 where the second side 310 of the seam 304 is laser welded to form a conduction weld 328. , keyhole weld 318, or transition weld 338 is formed. The method then continues with a stopping step. You can proceed to 338.

[0070] In one preferred non-limiting embodiment or example, the weld seam 304 is 308, and further includes a second weld 318 on the second side 310; 328 or 338, and any of the welding materials shown in Figures 1 to 7 and Figures 13 to 15. It can also be used as a joint.

[0071] Thus, what is disclosed herein is a first and second spaced apart body axis 34. a hollow body having a first aperture 32-1 and a second aperture 32-2, and The latitudinal coordinate of the body between the aperture 32-2 and the cell equator 30 is 0°, The method includes the steps of: A first partial cell 24 having a cell weld edge 36 and a first constriction 32-1 on the opposite side. and providing a second cell weld edge 38 and a second choke 32-2 on the opposite side thereof. providing a second partial cell 26 comprising the first and second partial cells 24, 26 are positioned so that the first and second cell weld edges 36, 38 face each other. The first and second partial cells 24, 26 are welded together, thereby providing a 30 degree field of view at latitudes other than the equator 30. The welding step forms the weld seam 28, 304. At least one of the first and opposing second sides 308, 310 each includes a first Forming the weld 312 and forming the second weld 318, 328, or 338 This may include:

[0072] The first weld 312 can be a conduction weld. The second weld 318, 328, or 338 may be a conduction weld, a keyhole weld, or a transition weld.

[0073] The weld seam 28, 304 extends from the equator 30 along the axis 34 to the first draw 32-1 or the second draw The aperture 32-2 may be located 5 mm or more away from the aperture 32-1.

[0074] The weld seam 28, 304 welds the first and second cell weld edges 36, 38 together. The insulating layer can be formed by:

[0075] The method further includes providing first and second cell gaps between the first and second partial cells 24, 26. 1 and 2, including first and second pipe weld edges 42, 44 facing pipe weld edges 36, 38, respectively. The method may include placing the pipe section 40 at the first and second pipe weld edges. 42, 44 can be welded to the respective first and second cell weld edges 36, 38. The weld seam 28, 46, 304 is formed by the first pipe weld edge 42 and the first cell weld. The second weld seam 48, 304 can be formed by welding the edge 36. , formed by welding the second pipe weld edge 44 and the second cell weld edge 38 At least the first side 308 of either of the pipe weld edges 42, 44 may be and on the second side 310, a first weld 312 and second welds 318, 328 , or 338, each weld seam 28, 46, 48 may be formed.

[0076] The second weld seam 48 , 304 may be located on the equator 30 .

[0077] The weld seam 56, 304 and the second weld seam 58, 304 are on either side of the equator 30. They can be arranged to face each other.

[0078] The method includes welding the first and second pipe sections 72, 74 together to form a third weld. forming a pipe section 70 including joints 76, 304; and This may include placing the pipe section 70 on or near the equator 30. do.

[0079] Each of the first weld seams 46, 56, 304 may be formed by conduction welding, and each of the second weld seams The joints 48, 58, 304 may be formed by conduction welding, keyhole welding, or transition welding.

[0080] The first side 308 may be an inner surface of at least one partial cell. 0 may be an outer surface of at least one partial cell. The welding step may include laser welding. It is possible to do so.

[0081] Also disclosed is a hollow cavity having first and second opposing ends. A superconducting radio frequency (SRF) cell 22 having a body defining a first aperture 32- A second aperture 32-1 is at a first end of the body and a second aperture 32-2 is at a second end of the body. A shaft 34 extending between the first aperture 32-1 and the second aperture 32-2, and a shaft 35 extending between the first aperture and the second aperture The aperture defines an equator 30 about an axis 34. The body is spaced apart from the equator 30. At the upper position, at least a first weld seam 28, 46, 56, 304 is formed around the axis 34. Each weld seam may extend entirely through the body, and may also extend adjacent the inside and outside of the body. Each weld seam may have opposing sides that terminate at a first weld and a second weld. The welds can be provided at the weld seam in opposing directions.

[0082] The first weld can be a conduction weld. The second weld can be a conduction weld, a keyhole weld, or It may be a transition weld.

[0083] The body may include a second weld seam 58 about the axis 34. The weld seams 56 and 58 may be positioned on opposite sides of the equator. .

[0084] The first weld can be on the inside of the body. The second weld can be on the outside of the body.

[0085] The body may include first and second partial cells 24, 26 having different shapes. .

[0086] The body includes a pipe section 40 between the first partial cell and the second partial cell. can be done.

[0087] The body includes second and third pipes that join the pipe sections to the first and second partial cells. Weld seams 56, 58 may be included.

[0088] The first and third weld seams 92, 94 are connected to the first and second drawers 32-1 and 32-2. The first weld seam 92 may be located 5 mm or closer to the first aperture 32-1. The third weld seam 94 may be located at a position 5 mm or more from the second aperture 32-2. The position may be set to 0.5.

[0089] Also disclosed is a method for forming a first object by abutting a first and a second object against each other. Defining a seam in an object having one side and an opposing second side; Laser welding is performed to the first and second objects from a first side of the seam along the seam. applying a conduction weld to both the first and second welds along the seam from the second side of the seam; and applying the laser welding by conduction welding, keyhole welding, or transition welding. This is the method.

[0090] Each object may be part of the body of a superconducting radio frequency cell. The second side of the seam may be formed on the outside of the body. can.

[0091] As can be seen, the present invention focuses on the area of ​​the cell (weld seam) that has the greatest sensitivity to fluctuations. At least in part, the problem of having an electric or magnetic field with the greatest fluctuations is Moving one or more weld seams to different areas of the cell increases costs and manufacturing costs. Although this increases the complexity of the construction, one or more weld seams have no detrimental effect on the performance of the cell. In one example, the effect of the weld seam on the performance of the cell was investigated by connecting the weld seam to the electric field and The total magnetic field can be minimized by placing the weld seam at the cell Take into account the impact on performance limits.

[0092] In addition to raising the upper limit of cell performance, moving one or more weld seams away from the cell equator This is a good way to take advantage of the accessibility of cell centers on or near the equator. , opening up several processing options. For example, each of the exemplary cells 2 shown in Figs. Before completing / forming any or all of the two weld seams, the first and second section One or more of the interior surfaces of the pipes 24, 26, any pipe, any pipe section, and / or or any combination thereof, electrolytic polishing, and / or post-weld processing, and / or Alternatively, for example and without limitation, physical vapor deposition of niobium can be used, and partial cell 24 , 26, any tube, any pipe section, and / or any combination thereof is formed of a material other than niobium.

[0093] Additionally, the first conduction weld on the inner surface (or first side) of the cell provides a smooth weld surface. The second surface of the cell has a second void space and is generally void-free. Welding such as conduction welding, keyhole welding, or transition welding produces strong, deep welds, and and a strong weld seam can be formed throughout, which allows the cell to be fitted to the SRF cavity. If the second weld is a keyhole weld, the first is on the inner surface. By forming a conduction weld, the weld seam is sealed against keyhole weld spatter. A keyhole weld can then be made on the outer surface, after which In one example, the depth of the keyhole weld is such that it intersects the inner surface (or first side) of the cell. The back or inner depth of the conduction weld can be accessed without the need for a keyhole weld. The weld may completely overlap the conduction weld, partially overlap the conduction weld, or be spaced apart from the conduction weld. It is possible.

[0094] If the second weld is a conduction weld or a transition weld, the first and second welds may be any desired It is possible to form the layers in a desired order.

[0095] In one preferred, non-limiting embodiment or example, by bringing two objects into contact: Conduction welding is applied to one side of the formed seam, conduction welding is applied to the other side, and keyhole welding is applied to the other side. The combination forming the joint or transition weld may be any of the partial cells, pipes, or may be used on any suitable and / or desired object other than a pipe section. It can be used.

[0096] The present invention will now be described in detail with reference to what are presently believed to be the most practical and preferred embodiments. Although detailed description has been given, it is for the purpose of illustration only, and the present invention is not limited to the present embodiment. On the contrary, modifications are intended to be within the spirit and scope of the claims. and equivalent arrangements. For example, the present invention is intended to cover, to the extent possible, One or more features of any embodiment may be combined with one or more features of any other embodiment. It should be understood that it is contemplated that the above-mentioned embodiments may be combined with the above-mentioned embodiments.

Claims

1. 1. A method of manufacturing a superconducting radio frequency (SRF) cell defined by a hollow body having first and second apertures spaced apart from one another along an axis of the body, and a cell equator in the body between the first and second apertures, the cell equator having a latitude coordinate of 0°, the method comprising: (a) providing a first partial cell including a first cell weld edge and the first choke opposite thereto; (b) providing a second partial cell including a second cell weld edge and, on an opposite side thereof, the second choke; (c) arranging the first and second partial cells such that the first and second cell weld edges face each other and are adjacent to each other without any intervening constriction between the first and second constrictions, and disposing a pipe section between the first and second partial cells, the pipe section including first and second pipe weld edges facing the first and second cell weld edges, respectively; (d) welding the first and second partial cells together, the step of: welding the first pipe weld edge to the first cell weld edge, thereby forming a first weld seam located on the cell equator; electropolishing and / or post-weld machining the first weld seam; and after the electropolishing and / or post-weld machining, welding the second pipe weld edge to the second cell weld edge, thereby forming a second weld seam located at a latitude other than the cell equator, the step of welding including forming a first weld and a second weld on a first side and an opposite second side of at least one of the cell weld edges, respectively. A method for manufacturing a superconducting radio frequency (SRF) cell.

2. the first welding is a conduction welding; the second weld being either a conduction weld, a keyhole weld, or a transition weld; The method of claim 1.

3. The method of claim 1 , wherein the first weld seam is formed by abutting and welding the first pipe weld edge and the first cell weld edge together.

4. 2. The method of claim 1, wherein the first and second weld seams are formed by forming a first weld and a second weld on a first side and an opposing second side, respectively, of at least one of the pipe weld edges.

5. The method of claim 4 , wherein each of the first welds is a conduction weld and each of the second welds is a conduction weld, a keyhole weld, or a transition weld.

6. the first side is an inner surface of at least one partial cell; and The second side is an outer surface of at least one partial cell. The method of claim 1.

7. The method of claim 1 , wherein the welding step comprises laser welding.

8. A body defining a hollow cavity having first and second opposed ends, a first aperture located at the first end of the body; a second aperture located at the second end of the body; and an axis extending between the first aperture and the second aperture; a cell equator between the first and second apertures about the axis; and the first aperture and the second aperture are adjacent to each other without an intervening aperture being disposed between the first aperture and the second aperture, The body includes: a first weld seam around the axis at a position on the body on the cell equator, where a first partial cell including the first restriction and a pipe section are welded, the first weld seam having an electropolished and / or post-weld machined surface; a second weld seam around the axis at a location on the body spaced from the cell equator, the second partial cell including the second restriction and the pipe section being welded together; 1. A superconducting radio frequency (SRF) cell, wherein each weld seam extends through the body and has opposite sides terminating near an inside and an outside of the body, and wherein the first weld seam includes a first weld and a second weld at each end.

9. the first welding is a conduction welding; the second weld being either a conduction weld, a keyhole weld, or a transition weld; 9. The SRF cell of claim 8.

10. the first weld is on an interior side of the body; and the second weld is on the exterior of the body; 9. The SRF cell of claim 8.

11. The SRF cell of claim 8, wherein the first partial cell and the second partial cell have different shapes from each other.

12. the second weld seam is perpendicular to the axis; and The method of claim 1 , wherein the second weld seam is located 5 mm or more away from the cell equator along the axis in the direction of the first or second aperture.

Citation Information

Patent Citations

  • Superconducting cavity, its manufacture, and superconducting accelerator

    JP2000260599A

  • Reinforced supraconductive material, supraconductive cavity, and methods for making same

    US6348757B1

  • Superconductive acceleration pipe

    WO1992013434A1