Secondary battery
The secondary battery configuration using copper and non-aqueous electrolyte with iron, nickel, or cobalt as negative electrode materials addresses the high cost and complexity of lithium-ion batteries, achieving lower costs and simpler manufacturing with enhanced energy densities.
Patent Information
- Application Number
- JP2024005234
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-12-19
- Filing Date
- 2024-01-17
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2044-01-17
AI Technical Summary
Lithium-ion batteries face high manufacturing costs due to the use of rare metals like lithium, cobalt, and nickel, and the manufacturing process is complex, particularly in the application of active materials to current collectors.
A secondary battery configuration using copper as the positive electrode active material, iron, nickel, or cobalt as the negative electrode active material, and a non-aqueous electrolyte, where copper ions move between electrodes, forming solid solutions with iron, nickel, or cobalt, simplifying the manufacturing process and reducing the need for coating.
The solution results in lower manufacturing costs, improved weight and volumetric energy densities, and a simpler manufacturing process compared to lithium-ion batteries, with copper serving as both the positive electrode active material and current collector, and iron, nickel, or cobalt serving as the negative electrode active material and current collector.
Smart Images

Figure 0007578253000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention is directed to a secondary battery which includes a non-aqueous electrolyte and a separator between a positive electrode and a negative electrode, is small and has a high capacity like a lithium ion battery, and is capable of repeated charging and discharging. [Background technology]
[0002] Small, high-capacity lithium-ion secondary batteries are used as power sources for portable electronic devices such as laptops and smartphones, but in recent years, from the perspective of global environmental issues and decarbonization, they have also been adopted as storage batteries for renewable energy and secondary batteries in electric vehicles.
[0003] In lithium-ion secondary batteries, lithium compounds such as lithium cobalt oxide (LiCoO2), ternary compounds (Li(Ni,Co,Mn)O2), lithium manganese oxide (LiMn2O4), and lithium iron phosphate (LiFePO4) are used as the positive electrode active material, while carbon materials such as hard carbon and graphite, silicon oxide (SiO), and silicon (Si) are used as the negative electrode active material. However, because lithium, cobalt, and nickel are rare metals, production costs are high, and compared with iron, aluminum, etc., they are extracted in small quantities, meaning there is a risk of a shortage of raw materials in the event of a significant increase in demand.
[0004] Furthermore, it is essential that the positive electrode active material and the negative electrode active material are applied to a positive electrode current collector and a negative electrode current collector, respectively, that is, terminals that transmit the current generated by the positive electrode active material and the negative electrode active material to the outside of the battery. However, the manufacturing process involving such application is by no means simple and is complicated. Incidentally, in a typical lithium-ion battery, lithium cobalt oxide powder, which is the positive electrode active material, is applied to an aluminum foil, which is a positive electrode current collector, and graphite powder, which is the negative electrode active material, is applied to a copper foil, which is a negative electrode current collector. However, these application procedures are quite cumbersome.
[0005] Taking into consideration the current situation of lithium-ion batteries, the applicants filed a patent application for a secondary battery that uses copper as the positive electrode active material, aluminum as the negative electrode active material, and a non-aqueous electrolyte solution as the electrolyte (Patent Application No. 2022-047894), and based on this application, a patent right was established under Patent Document 1 (hereinafter, the invention based on the configuration of Patent Document 1 will be referred to as the "prior invention"). The prior invention is based on the following configuration. Note Copper is used as the positive electrode active material, aluminum is used as the negative electrode active material, and a non-aqueous electrolyte is used as the electrolyte. In addition, copper ions (Cu 2+ ) moves from the positive electrode to the negative electrode, and during discharge, copper ions (Cu 2+ ) moves in the opposite direction to that during charging.
[0006] The prior invention based on the above-mentioned basic configuration can exhibit the technical advantage of lower manufacturing costs compared to lithium ion batteries.
[0007] However, copper ions (Cu 2+ ), however, for secondary batteries in which metals move during charging and discharging, the metal used as the negative electrode active material does not need to be limited to aluminum. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Patent No. 7343116 Summary of the Invention [Problem to be solved by the invention]
[0009] The present invention aims to provide a secondary battery configuration that is cheaper to manufacture than lithium ion batteries, employs copper as the positive electrode active material, and employs a metal other than aluminum as the negative electrode active material. [Means for solving the problem]
[0010] In order to solve the above problems, the inventors envisioned the following basic configuration: (1) Copper is used as the positive electrode active material, iron, nickel, or cobalt is used as the negative electrode active material, and a non-aqueous electrolyte is used as the electrolyte, and copper ions (Cu 2+ ) moves from the positive electrode to the negative electrode By this, a solid solution of iron, nickel, or cobalt and copper is formed. During discharge, copper ions (Cu 2+ ) moves in a direction opposite to that during charging. (2) The secondary battery according to (1), characterized in that copper serves as a positive electrode active material and a positive electrode current collector, and iron, nickel or cobalt serves as a negative electrode active material and a negative electrode current collector. It is.
[0011] The basic configuration (1) includes the basic configuration (2) in which copper and iron or nickel or cobalt act as a positive electrode current collector and a negative electrode current collector, respectively. In addition to the basic configuration (1), the basic configuration (1) also includes a configuration in which, for example, silver foil or aluminum foil is used as the positive electrode current collector and silver foil or copper foil is used as the negative electrode current collector. However, the above configuration is an exception, and most of the embodiments of basic configuration (1) are based on basic configuration (2). In addition, the "nonaqueous electrolyte" in the basic configuration refers to an electrolyte that does not contain water and can conduct cations (copper ions in the case of basic configurations (1) and (2)) during charging and discharging. Effect of the Invention
[0012] As is clear from the above basic configurations (1) and (2), the present invention is composed of three elements: copper, iron or nickel or cobalt, and a separator that is integral with a non-aqueous electrolyte. Since the present invention does not use rare metals as in lithium-ion batteries, the manufacturing cost is low, as in the case of the prior invention. In particular, when iron is selected as the negative electrode active material, the manufacturing cost can be reduced even further compared to the prior invention.
[0013] Moreover, in the case of the basic structure (2), all of the positive electrodes are made of copper and all of the negative electrodes are made of iron, nickel, or cobalt, so that there is no need for a coating process as in the case of lithium-ion batteries, and the manufacturing process is extremely simple.
[0014] The operation of the basic configuration having such effects is as follows.
[0015] In the basic configurations (1) and (2), charging can be realized by copper acting as a positive electrode active material and iron, nickel, or cobalt acting as a negative electrode active material. In the charging step, at the positive electrode, Cu → Cu 2+ +2e - This ionization reaction occurs, and copper ions (Cu 2+ ) moves to the negative electrode, and electrons (e - ) moves to the positive electrode.
[0016] In contrast, in the negative electrode, Cu 2+ +xFe+2e - → CuFe x or Cu 2+ +xNi+2e - → CuNi x or Cu 2+ +xCo+2e - → CuCo x As shown in the figure, copper and iron, nickel, or cobalt are dissolved in a solid solution to form a crystal structure, forming an alloy, and the electrons (e - ) is released.
[0017] In addition, one copper ion (Cu 2+The reason why copper is alloyed with any number of iron, nickel, or cobalt (X is usually an integer of 5 or less) as a solid solution with copper is that copper and iron, nickel, or cobalt can form a stable crystal structure in a certain ratio.
[0018] Conversely, in the case of discharge, at the positive electrode, Cu 2+ +2e - → Cu The reaction between copper ions and electrons occurs, and at the negative electrode, CuFe x → Cu 2+ +Fe x +2e - or CuNi x → Cu 2+ +Ni x +2e - or CuCo x → Cu 2+ +Co x +2e - This is the ionization reaction between copper and electrons.
[0019] Therefore, the overall reaction due to the charging and discharging is as follows: Cu+Fe x ⇔ CuFe x or Cu+Ni x ⇔ CuNi x or CU 2+ +Co x ⇔ CuCox This is due to the fact that the alloying of copper with iron, nickel or cobalt has been realized and the separation of the two has been realized.
[0020] In the basic configuration (1), copper acts as the positive electrode active material, and iron, nickel, or cobalt acts as the negative electrode active material. However, when copper is used as the positive electrode current collector and iron, nickel, or cobalt is used as the terminal of the negative electrode current collector, as in the basic configuration (2), the positive electrode and the negative electrode are composed of copper and iron, nickel, or cobalt, respectively, and an extremely simple manufacturing process can be realized.
[0021] The theoretical capacity of copper, the positive electrode active material, is approximately 850 mAh / g. However, as described below, when the operating voltage during discharge is 3.5 V, the gravimetric energy density is 850 x 3.5 = 2,975 Wh / kg, and when the density is 8.91, the volumetric energy density is approximately 56,500 Wh / L.
[0022] When comparing the above density values with those of Li(Ni,Co,Mn)O2, the positive electrode material for existing lithium-ion secondary batteries, the weight energy density is about four times higher and the volumetric energy density is about eight times higher. Therefore, the gravimetric energy density is about three times that of the prior invention, and the volumetric energy density is about six times that of the prior invention. [Brief description of the drawings]
[0023] [Figure 1] 1 is a schematic diagram showing a configuration of a secondary battery of the present invention. [Diagram 2] FIG. 1 is a schematic diagram showing the configuration of a typical lithium ion battery. [Diagram 3] 1 is a graph showing the relationship between time and voltage, indicating the charged and discharged states, where (a) shows the case where iron is used as the anode, (b) shows the case where nickel is used as the anode, (c) shows the case where cobalt is used as the anode, and (d) shows the case where aluminum is used as the anode. [Figure 4(a)] 1 is a graph showing cycle characteristics based on the relationship between the number of repeated charge and discharge cycles, i.e., the cycle number, and the discharge current capacity in units of current value (mA)×time. [Figure 4(b)]4 is a graph showing the relationship between the cycle number and the average discharge voltage. [Figure 4(c)] 1 is a graph showing the relationship between current capacity in units of mA×time, which is the current value at the 10 cycle stage, and voltage (V) at the charge stage and the discharge stage. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] As shown in FIG. 1, the basic configuration (1) is a secondary battery that employs copper as a material constituting the positive electrode 1, employs iron, nickel, or cobalt as a material constituting the negative electrode 2, and employs a non-aqueous electrolyte solution as an electrolyte. The basic configuration (2) is a secondary battery of the above (1), characterized in that copper acts as a positive electrode active material and a positive electrode current collector, and iron, nickel, or cobalt acts as a negative electrode active material and a negative electrode current collector.
[0025] The basic structure (1) is based on the basic structure (2) in most cases, but as an exception, a copper foil made of a metal other than copper may be used as the positive electrode current collector, and a metal foil made of a metal other than iron, nickel, or cobalt may be used as the negative electrode current collector, as already pointed out in the section on means for solving the problem.
[0026] In comparison with the configuration of a typical lithium-ion battery shown in FIG. 2, the basic configuration (1) differs in that copper is used as the positive electrode active material 4 in place of a lithium-containing oxide or the like in the positive electrode, and that iron, nickel, or cobalt is used as the negative electrode active material 5 in place of graphite or the like in the negative electrode. The basic configuration (2) differs in that, in the case of a lithium-ion battery, a positive electrode active material made of copper doubles as the positive electrode current collector in place of a current collector 6 made of aluminum foil to which the oxide 4 is applied, and that a negative electrode active material made of iron, nickel, or cobalt doubles as the negative electrode current collector in place of a current collector 7 made of copper foil to which lithium carbide or the carbon material 5 is applied.
[0027] Due to these differences in structure, in the case of basic structure (1), the manufacturing costs are lower than those of lithium ion secondary batteries, and especially when iron is used as the negative electrode active material, the manufacturing costs are even lower than those of the prior invention. As already pointed out, in the case of basic structure (2), the manufacturing process is simpler than that of lithium ion secondary batteries.
[0028] In the basic structures (1) and (2), similarly to the lithium ion secondary battery, a separator 3 formed integrally with a non-aqueous electrolyte is provided between the positive electrode 1 and the negative electrode 2.
[0029] However, the separator 3 in the basic configurations (1) and (2) does not contain copper ions (Cu 2+ It is essential that the material is in a porous state that allows the passage of oxygen.
[0030] Typical examples of non-aqueous electrolytes are ionic liquids and organic electrolytes. 2+ ) and electrons (e - ) can flow during charging and discharging.
[0031] An ionic liquid is generally defined as a liquid in which cations and anions exist at temperatures below 100°C.
[0032] Depending on the type of cation, imidazolium salts, pyrrolidinium salts, pyridinium salts, piperidinium salts, ammonium salts, and phosphonium salts can be mentioned in terms of the basic skeleton of the cation, and any of these cations can be used.
[0033] Examples of anions that coexist with cations include bromide ions, halogen ions such as triflate, boron ions such as tetraphenylborate, and phosphorus ions such as hexafluorophosphate.
[0034] Since ionic liquids are non-flammable and non-volatile, when they are used as non-aqueous electrolytes, it is possible to obtain safe secondary batteries.
[0035] An organic electrolyte is defined as an electrolyte in which an electrolyte salt, i.e., both cations and anions, are dissolved in an organic solvent.
[0036] Examples of the organic solvent include acetonitrile, dioxolane, 1,2-dimethoxyethane, tetrahydrofuran, γ-butyrolactone, propylene carbonate, and ethylene carbonate. Examples of the electrolyte salt include alkali metal ions such as lithium ions, quaternary alkyl ammonium ions, cations, and anions such as halogen ions, sulfate ions, and perchlorate ions.
[0037] However, organic electrolyte solutions tend to be inferior to ionic liquids in terms of non-flammability and non-volatility.
[0038] In the basic configurations (1) and (2), a separator 3 impregnated with a non-aqueous electrolyte is used between a positive electrode 1 and a negative electrode 2. Separators are also used in ordinary lithium-ion secondary batteries to prevent short circuits between the positive and negative electrodes.
[0039] The following is an explanation based on each graph.
[0040] A rectangular copper plate measuring 50 mm x 70 mm x 0.1 mm thick was used as the positive electrode 1, and a rectangular iron, nickel, cobalt, or aluminum plate measuring 50 mm x 70 mm x 0.1 mm thick was used as the negative electrode 2. A sulfolane-based electrolyte was used as the electrolyte, and glass filter paper was used as the separator.
[0041] A cell was assembled based on the design based on the above dimensions, and a 0.1 mm thick aluminum laminate film was attached as an exterior and vacuum sealed to prepare a secondary battery.
[0042] A charge-discharge cycle test was carried out at an environmental temperature of 25° C. by repeatedly charging at a current of 40 mA and a cut-off voltage of 4.5 V and discharging at a current of 10 mA and a cut-off voltage of 2.5 V.
[0043] The results of the charge-discharge cycle test are shown in the form of charge-discharge curves in FIG. 3(a), FIG. 3(b), FIG. 3(c), and FIG. 3(d) for the cases where iron, nickel, cobalt, and aluminum were used as the negative electrode active material.
[0044] In the discharge curve, a plateau voltage value was observed around 3.5 V, that is, a voltage value in a relatively stable state.
[0045] From these observation results, it can be confirmed that the secondary battery according to the present invention is not a simple discharge capacitor but a secondary battery, as in the case of the prior invention. In the case of a capacitor, the voltage value due to discharge decays exponentially, and the voltage value due to the plateau described above cannot be realized.
[0046] Furthermore, as is clear from a comparison of the charge / discharge curves shown in Figures 3(a), (b), and (c) with the charge / discharge curve shown in Figure 3(d), it can be confirmed that the secondary battery in the simplified cell state of the present invention can be charged and discharged for at least 15 cycles, as in the case of the prior invention, and that the same charge / discharge cycles are possible as in the prior invention.
[0047] The present invention will be described below in concrete comparison with the prior invention. As shown in FIG. 4(a), when focusing on the cycle characteristics when the negative electrode is made of iron or nickel, as compared with the prior invention in which the negative electrode is made of aluminum, the current capacity during discharge of the present invention is slightly inferior to that of the prior invention as the number of cycles increases in the case of an iron negative electrode, is significantly inferior in the case of a nickel negative electrode, and is in an intermediate state between that of iron and nickel in the case of a cobalt negative electrode. However, since the nickel negative electrode exhibited approximately 3 mAh at 15 cycles and the cobalt negative electrode exhibited approximately 11 mAh at 15 cycles, even if the above-mentioned differences from the prior invention are observed, this does not mean that there are any serious defects in the nickel negative electrode and the cobalt electrode. As is clear from the graph of FIG. 4(b), it is clear that the iron negative electrode and the nickel negative electrode can achieve a higher discharge voltage under the same conditions as those of the prior invention. As is clear from FIG. 4(c), while the charging voltages at the 10-cycle stage are approximately the same, the iron negative electrode, nickel negative electrode, and cobalt negative electrode enable the realization of significantly higher discharge voltages than the prior art. [Industrial Applicability]
[0048] The secondary battery of the present invention, like the prior invention, is inexpensive to manufacture and has a simple configuration, while being capable of producing a higher discharge voltage than the prior invention, and in the case of an iron negative electrode, the secondary battery can be realized at a lower cost than the prior invention.
[0049] In this way, the secondary battery according to the present invention can be used in a wide range of industrial fields, such as power sources for various portable devices, power sources for electric vehicles, and power storage facilities for power standardization of renewable energy, beyond the scope of the prior invention. [Explanation of symbols]
[0050] 1. Copper-based positive electrode 2. Iron or nickel-based negative electrodes 3. Separator impregnated with non-aqueous electrolyte 4. Positive electrode active material in lithium-ion batteries 5. Negative electrode active material in lithium-ion batteries 6. Iron or nickel positive current collectors in lithium-ion batteries 7 Copper negative electrode current collectors in lithium-ion batteries
Claims
1. Copper is used as the positive electrode active material, iron, nickel, or cobalt is used as the negative electrode active material, and a non-aqueous electrolyte is used as the electrolyte. In addition, copper ions (Cu 2+ ) moves from the positive electrode to the negative electrode, forming a solid solution of iron, nickel, or cobalt with copper, and during discharge, copper ions (Cu 2+ ) moves in the opposite direction to that during charging.
2. 2. The secondary battery according to claim 1, wherein copper serves as a positive electrode active material and a positive electrode current collector, and iron, nickel or cobalt serves as a negative electrode active material and a negative electrode current collector.
3. 3. The secondary battery according to claim 1, wherein the positive and negative electrodes have an area of 50 mm x 70 mm, and the secondary battery can achieve a stable voltage with a plateau at about 3.5 V during the discharge stage by repeating a charge-discharge cycle in which charging is performed with a current of 40 mA and an end voltage of 4.5 V, and discharging is performed with a current of 10 mA and an end voltage of 2.5 V.
4. Cu in the negative electrode 2+ +XFe+2e ⇔ CuFe x Or C.U. 2+ +xNi+2e ⇔ CuNi x CuCox or Cu 2+ 3. The secondary battery according to claim 1, wherein the alloying of copper with iron, nickel or cobalt is realized during charging, and the separation of copper from iron, nickel or cobalt is realized during discharging, based on the reaction formula: +Co+2e⇔CuCox.
Citation Information
Patent Citations
Secondary battery
JP2010232148A
Secondary battery
JP2023141529A
Secondary batteries
JP7343116B1
Secondary battery
WO2013108309A1