Friction welding machine, friction welding method, and manufacturing method of components

The friction welding machine and method ensure high accuracy in rotation angle alignment by using a servo motor and vise to adjust the workpiece angles, facilitating precise tooth surface matching and simplifying the manufacturing process for components like double pinion rack bars.

JP7578532B2Active Publication Date: 2024-11-06NETUREN CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021064084
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-04-05
Publication Date
2024-11-06
Estimated Expiration
2041-04-05

AI Technical Summary

Technical Problem

Existing friction welding machines face challenges in achieving high accuracy for the rotation angle alignment between workpieces after welding, which is crucial for precise matching of tooth surfaces in components like double pinion rack bars used in automobile power steering systems.

Method used

A friction welding machine and method that utilize a servo motor to control the rotation angle of a workpiece, combined with a vise to hold the second workpiece at a constant angle, and a control unit to adjust the rotation angle based on detected variations, ensuring high precision by rotating the workpiece again to align with the set angle.

Benefits of technology

The method achieves highly accurate rotation angle alignment, allowing for precise matching of tooth surfaces and simplifying the manufacturing process by avoiding the need for additional tooth surface formation post-welding, thus enabling the production of lightweight, hollow components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578532000001
    Figure 0007578532000001
  • Figure 0007578532000002
    Figure 0007578532000002
  • Figure 0007578532000003
    Figure 0007578532000003
Patent Text Reader

Abstract

To provide a friction pressure-welding machine with high rotation angle accuracy after joining, a friction pressure-welding method and a component manufacturing method.SOLUTION: A friction pressure-welding method comprises: a process in which while rotating a work-piece W1, a work-piece W2 is held at a constant rotation angle and is pressed against the rotating work-piece W1, thereby heating a contact part between the work-piece W1 and the work-piece W2; a process in which rotation of the work-piece W1 is stopped, and a load for pressing the work-piece W2 against the work-piece W1 is increased; a process in which while the work-piece W2 is pushed into the work-piece W1, a rotation angle θ of the work-piece W1 is detected, and the work-piece W1 is rotated again so that the rotation angle θ of the work-piece W1 approaches a set rotation angle θ0; and a process in which the load is released.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The embodiments relate to a friction welding machine, a friction welding method, and a method for manufacturing a member. [Background technology]

[0002] Some friction welding machines have a built-in servo motor in the chuck that can control the rotation angle of the workpiece after friction welding. However, when it is necessary to match the rotation angle between two workpieces with high precision after friction welding, the precision of the rotation angle may not be sufficient. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 3355586 Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the embodiments of the present invention is to provide a friction welding machine, a friction welding method, and a method for manufacturing a member that provide high accuracy of the rotation angle after joining. [Means for solving the problem]

[0005] A friction welding machine according to an embodiment of the present invention includes a chuck having a servo motor and rotating a first workpiece by the servo motor, a vice holding a second workpiece at a constant rotation angle and pressing it against the first workpiece, and a control unit. After the servo motor stops rotating with the vice pressing the second workpiece against the first workpiece, the control unit detects the rotation angle of the first workpiece based on a signal from the servo motor while the second workpiece is being pressed into the first workpiece, and causes the servo motor to rotate the first workpiece again so that the rotation angle of the first workpiece approaches a set value.

[0006] A friction welding method according to an embodiment of the present invention includes the steps of: rotating a first workpiece while holding a second workpiece at a constant rotation angle and pressing it against the rotating first workpiece, thereby heating the contact portion between the first workpiece and the second workpiece; stopping the rotation of the first workpiece and increasing the load pressing the second workpiece against the first workpiece; detecting the rotation angle of the first workpiece while the second workpiece is being pressed into the first workpiece, and rotating the first workpiece again so that the rotation angle of the first workpiece approaches a set rotation angle; and releasing the load.

[0007] A manufacturing method of a component according to an embodiment of the present invention includes the steps of: rotating a first workpiece while holding a second workpiece at a constant rotation angle and pressing it against the rotating first workpiece, thereby heating the contact portion between the first workpiece and the second workpiece; stopping the rotation of the first workpiece and increasing the load pressing the second workpiece against the first workpiece; detecting the rotation angle of the first workpiece while the second workpiece is being pressed into the first workpiece, and rotating the first workpiece again so that the rotation angle of the first workpiece approaches a set rotation angle; and releasing the load. Effect of the Invention

[0008] According to the embodiments of the present invention, it is possible to realize a friction welding machine, a friction welding method, and a method for manufacturing a member that provide high accuracy of the rotation angle after joining. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a diagram showing a friction welding machine according to a first embodiment. [Diagram 2] FIG. 1(a) is a top view showing a member manufactured by the friction welding machine according to the first embodiment, and FIG. [Diagram 3]1 is a cycle diagram showing a friction welding method according to a first embodiment, with the horizontal axis representing time and the vertical axis representing the rotation speed of a workpiece W1, the load applied to a workpiece W2, and the amount of movement of the workpiece W2. [Figure 4] 1 is a cycle diagram showing a friction welding method according to a second embodiment, with the horizontal axis representing time and the vertical axis representing the rotation speed of the workpiece W1, the load applied to the workpiece W2, and the movement amount of the workpiece W2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] (First embodiment) Hereinafter, an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a diagram showing a friction welding machine according to this embodiment. As shown in FIG. 1, the friction welding machine 1 according to this embodiment is provided with a base 10, a support portion 11, a chuck 12, a vice 13, and a control portion .

[0011] The base 10 is installed, for example, on the floor surface of the inner building. The support portion 11 is disposed on the base 10. The support portion 11 supports a chuck 12. The chuck 12 is provided with a servo motor 15. The chuck 12 can position and hold the workpiece W1 at a predetermined rotation angle. Furthermore, the chuck 12 can rotate the workpiece W1 by the servo motor 15. The servo motor 15 can control the rotation angle of the workpiece W1. Furthermore, the servo motor 15 can detect the rotation angle of the workpiece W1 and output a detection signal S1 representing the detection result.

[0012] In this specification, the "rotation angle" refers to, for example, the angle of the workpiece W1, which is the angle between the direction from the rotation axis of the workpiece W1 to a point on the surface of the workpiece W1 and a reference line passing through the rotation axis, and is an angle expressed as a value of 0° or more and less than 360°. The same applies to the workpiece W2.

[0013] The control unit 14 is disposed, for example, within the support unit 11. A set value θ0 of the rotation angle of the workpiece W1 can be input to the control unit 14. A detection signal S1 indicating a detected value θ of the rotation angle of the workpiece W1 is also input to the control unit 14 from the servo motor 15. The control unit 14 outputs a control signal S2 to the servo motor 15 based on the set value θ0 and the detected value θ of the rotation angle of the workpiece W1, and can rotate the servo motor 15 by a predetermined amount of rotation.

[0014] The vice 13 is disposed at a position away from the support portion 11 on the base 10. The vice 13 is, for example, a two-piece vice. The vice 13 can hold the workpiece W2 at a position facing the workpiece W1. The vice 13 can position the workpiece W2 at a predetermined rotation angle, and firmly grips the workpiece W2 so that this rotation angle does not change. The vice 13 can also move the workpiece W2 while holding it, and press it against the workpiece W1.

[0015] FIG. 2(a) is a top view showing a member manufactured by the friction welding machine according to this embodiment, and (b) is a side view thereof. As shown in Figures 2(a) and (b), workpieces W1 and W2 are components that are friction-welded to form one member M. In the member M, the workpiece W1 is joined to the workpiece W2 via a joining surface P. The member M is, for example, a double pinion rack bar used in an automobile power steering system, such as a hollow rack bar. When the member M is a hollow rack bar, the workpieces W1 and W2 are also hollow.

[0016] A tooth surface B1 is formed on the workpiece W1. The tooth surface B1 is a portion that meshes with a first pinion (not shown) of a power steering system. A tooth surface B2 is formed on the workpiece W2. The tooth surface B2 is a portion that meshes with a second pinion (not shown) of the power steering system. The phase of the tooth surface B1 and the phase of the tooth surface B2 must correspond with high precision. For this reason, the rotation angle of the workpiece W1 and the rotation angle of the workpiece W2 must correspond with high precision.

[0017] Next, the operation of the friction welding machine according to this embodiment, that is, the friction welding method and member manufacturing method according to this embodiment will be described. FIG. 3 is a cycle diagram showing the friction welding method according to this embodiment, with the horizontal axis representing time and the vertical axis representing the rotation speed of the workpiece W1, the load applied to the workpiece W2, and the amount of movement of the workpiece W2.

[0018] 1, the workpiece W1 is attached to the chuck 12 and positioned at a predetermined rotation angle. The workpiece W2 is attached to the vice 13 and positioned at a predetermined rotation angle. The set value θ0 of the rotation angle of the workpiece W1 after joining is input to the control unit 14.

[0019] Next, as shown in Figs. 1 and 3, the servo motor 15 of the chuck 12 rotates the workpiece W1. The rotation speed at this time is, for example, 1500 rpm to 2500 rpm when the workpiece is a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm. On the other hand, the vice 13 does not rotate the workpiece W2. Then, the vice 13 moves the workpiece W2 toward the workpiece W1 and presses it against the workpiece W1 with a constant load. The load at this time is, for example, 5.0 kN to 10 kN. As a result, heat is generated by friction at the contact portion between the workpieces W1 and W2, and this contact portion is heated.

[0020] This state is maintained for a certain period of time. For example, it is maintained for a period of 10 seconds or more and 20 seconds or less. The temperature of the contact part becomes, for example, about 800 to 1000°C. The workpiece W2 is pushed little by little into the workpiece W1. The process up to this point is called the "friction process (first process)".

[0021] Next, the servo motor 15 is stopped to abruptly stop the rotation of the workpiece W1, and the load with which the vice 13 presses the workpiece W2 against the workpiece W1 is increased. For example, the load is set to 20 kN or more and 25 kN or less. As a result, the workpiece W2 is pressed against the workpiece W1 for an additional 3 to 8 seconds, and the contact portion expands in the radial direction, forming a burr. This process is called the "load increasing process (second process)."

[0022] When the rotation of the workpiece W1 is suddenly stopped, the servo motor 15 attempts to stop the workpiece W1 at the set rotation angle θ0, but in reality, variations occur due to inertial forces, etc. For example, variations of about ±1° occur. After the servo motor 15 stops the rotation, it detects the actual rotation angle θ of the workpiece W1 and outputs a detection signal S1 representing the detection result to the control unit 14. The control unit 14 outputs a control signal S2 to the servo motor 15, and causes the servo motor 15 to rotate the workpiece W1 again so that the rotation angle θ of the workpiece W1 approaches the set value θ0. The absolute value of the amount of rotation at this time is, for example, less than 1°. This process is called the "rotation angle detection process (third process)".

[0023] As a result, the rotation angle θ of the workpiece W1 becomes closer to the set value θ0, for example, less than ±0.15°. This adjustment of the rotation angle θ is performed while the movement amount of the workpiece W2 continues to increase, that is, while the contact area is hot and soft. This makes it possible to suppress internal stress from remaining in the contact area.

[0024] After that, the load applied to the workpiece W2 is released, and the contact portion is allowed to cool. As a result, the workpiece W1 is joined to the workpiece W2, and the member M is produced. This process is called the "load releasing process (fourth process)." Depending on the specifications of the member M, the expanded portion at the contact portion may be removed.

[0025] Next, the effects of this embodiment will be described. In this embodiment, after the servo motor 15 stops rotating while the vice 13 is pressing the workpiece W2 against the workpiece W1, the control unit 14 detects the rotation angle θ of the workpiece W1 based on the detection signal S1 from the servo motor 15, and causes the servo motor 15 to rotate the workpiece W1 again so that the rotation angle θ approaches the set value θ0. At this time, since the rotation of the workpiece W1 for friction welding has already stopped, the inertial force due to this rotation does not affect the rotation of the workpiece W1 again. This allows the rotation angle of the workpiece W1 to correspond to the rotation angle of the workpiece W2 with high accuracy.

[0026] As a result, when the tooth surface B1 is formed on the workpiece W1 and the tooth surface B2 is formed on the workpiece W2, the phase of the tooth surface B1 and the phase of the tooth surface B2 can be made to correspond with high precision. Therefore, according to this embodiment, workpieces on which tooth surfaces have been formed in advance can be joined together. As a result, the process for manufacturing the member M can be simplified.

[0027] In this embodiment, the workpiece W1 is rotated again while the movement amount of the workpiece W2 continues to increase. This makes it possible to adjust the rotation angle by rotating the workpiece W1 again while the contact portion is still soft. This makes it possible to suppress residual internal stress in the contact portion. In this case, there is no need to provide a separate heat source in or around the friction welding machine 1.

[0028] If the workpiece W1 is not rotated again, the error in the rotation angle of the workpiece W1 in the manufactured member M is large, and the phase of the tooth surface B1 and the phase of the tooth surface B2 cannot be made to correspond with sufficient accuracy. Therefore, at least one of the tooth surface B1 and the tooth surface B2 needs to be formed after the workpiece W1 and the workpiece W2 are friction-welded. This complicates the process for manufacturing the member M. In addition, if a tooth surface is to be formed on a hollow workpiece by cutting or the like after friction welding, there is a possibility that a hole will be made in the workpiece, so the workpiece on which the tooth surface is to be formed after friction welding needs to be a solid workpiece. Therefore, for example, if the member M is a rack bar, it is difficult to manufacture a rack bar that is hollow as a whole. As a result, the weight reduction of the rack bar is hindered.

[0029] Second Embodiment Next, a friction welding method and a method for manufacturing a member according to a second embodiment will be described. FIG. 4 is a cycle diagram showing the friction welding method according to this embodiment, with the horizontal axis representing time and the vertical axis representing the rotation speed of the workpiece W1, the load applied to the workpiece W2, and the movement amount of the workpiece W2.

[0030] 1, the workpiece W1 is attached to the chuck 12 and positioned at a predetermined rotation angle. The workpiece W2 is attached to the vice 13 and positioned at a predetermined rotation angle. The set value θ0 of the rotation angle of the workpiece W1 after joining is input to the control unit 14.

[0031] Next, as shown in FIG. 1 and FIG. 4, the servo motor 15 of the chuck 12 does not rotate (fixes) the workpiece W1. The vice 13 also does not rotate (fixes) the workpiece W2. Then, the vice 13 moves the workpiece W2 toward the workpiece W1, presses it against the workpiece W1 with a constant load, and then rotates the workpiece W1. The rotation speed at this time is 1500 rpm or more and 2500 rpm or less when the workpiece is a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm, for example. The load at this time is 5.0 kN or more and 10 kN or less. As a result, heat is generated by friction at the contact portion between the workpiece W1 and the workpiece W2, and this contact portion is heated.

[0032] This state is maintained for a certain period of time. For example, it is maintained for a period of 10 seconds or more and 20 seconds or less. The temperature of the contact part becomes, for example, about 800 to 1000°C. The workpiece W2 is pushed little by little into the workpiece W1. The process up to this point is called the "friction process (first process)". The second to fourth steps after this first step are the same as those in the first embodiment, and therefore their explanations will be omitted. Furthermore, the effects of this embodiment are also the same as those in the first embodiment, and therefore their explanations will be omitted.

[0033] (Third embodiment) Next, a friction welding method and a method for manufacturing a member according to a third embodiment will be described.

[0034] 1, the workpiece W1 is attached to the chuck 12 and positioned at a predetermined rotation angle. The workpiece W2 is attached to the vice 13 and positioned at a predetermined rotation angle. The set value θ0 of the rotation angle of the workpiece W1 after joining is input to the control unit 14.

[0035] Next, as shown in FIG. 1 and FIG. 4, the servo motor 15 of the chuck 12 does not rotate (fix) the workpiece W1. The vice 13 also does not rotate (fix) the workpiece W2. Then, the vice 13 moves the workpiece W2 toward the workpiece W1 and presses it against the workpiece W1 with a certain load, and then rotates the workpiece W1 and the workpiece W2. For example, when the workpiece is a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm, the rotation speed of the workpiece W1 is 1500 rpm or more and 2500 rpm or less, and the rotation speed of the workpiece W2 is 100 rpm or more and 300 rpm or less. The load at this time is, for example, 5.0 kN or more and 10 kN or less. As a result, heat is generated by friction at the contact portion between the workpiece W1 and the workpiece W2, and this contact portion is heated.

[0036] This state is maintained for a certain period of time. For example, it is maintained for a period of 10 seconds or more and 20 seconds or less. The temperature of the contact part becomes, for example, about 800 to 1000°C. The workpiece W2 is pushed little by little into the workpiece W1. The process up to this point is called the "friction process (first process)".

[0037] Next, the servo motor 15 is stopped to abruptly stop the rotation of the workpieces W1 and W2, and the load with which the vice 13 presses the workpiece W2 against the workpiece W1 is increased. For example, the load is set to 20 kN or more and 25 kN or less. As a result, the workpiece W2 is pressed against the workpiece W1 for an additional 3 to 8 seconds, and the contact portion expands in the radial direction, forming a burr. This process is called the "load increasing process (second process)." The third and fourth steps after the second step are the same as those in the first embodiment, and therefore their explanations will be omitted. Furthermore, the effects of this embodiment are also the same as those in the first embodiment, and therefore their explanations will be omitted.

[0038] (Fourth embodiment) Next, a friction welding method and a method for manufacturing a member according to a fourth embodiment will be described.

[0039] 1, the workpiece W1 is attached to the chuck 12 and positioned at a predetermined rotation angle. The workpiece W2 is attached to the vice 13 and positioned at a predetermined rotation angle. The set value θ0 of the rotation angle of the workpiece W1 after joining is input to the control unit 14.

[0040] Next, as shown in FIG. 1 and FIG. 3, the servo motor 15 of the chuck 12 rotates the workpiece W1. On the other hand, the vice 13 does not rotate (fixes) the workpiece W2. Then, the vice 13 moves the workpiece W2 toward the workpiece W1, presses it against the workpiece W1 with a certain load, and then rotates the workpiece W2. For example, when the workpiece is a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm, the rotation speed of the workpiece W1 is set to 1500 rpm or more and 2500 rpm or less, and the rotation speed of the workpiece W2 is set to 100 rpm or more and 300 rpm or less. The load at this time is, for example, 5.0 kN or more and 10 kN or less. As a result, heat is generated by friction at the contact portion between the workpiece W1 and the workpiece W2, and this contact portion is heated.

[0041] This state is maintained for a certain period of time. For example, it is maintained for a period of 10 seconds or more and 20 seconds or less. The temperature of the contact part becomes, for example, about 800 to 1000°C. The workpiece W2 is pushed little by little into the workpiece W1. The process up to this point is called the "friction process (first process)".

[0042] Next, the servo motor 15 is stopped to abruptly stop the rotation of the workpieces W1 and W2, and the load with which the vice 13 presses the workpiece W2 against the workpiece W1 is increased. For example, the load is set to 20 kN or more and 25 kN or less. As a result, the workpiece W2 is pressed against the workpiece W1 for an additional 3 to 8 seconds, and the contact portion expands in the radial direction, forming a burr. This process is called the "load increasing process (second process)." The third and fourth steps after the second step are the same as those in the first embodiment, and therefore their explanations will be omitted. Furthermore, the effects of this embodiment are also the same as those in the first embodiment, and therefore their explanations will be omitted.

[0043] Fifth embodiment Next, a friction welding method and a method for manufacturing a member according to a fifth embodiment will be described. In the fifth embodiment, the rotation angle detection step (third step) is different from the first embodiment. The other steps and effects of the present embodiment are similar to those of the first embodiment, so the description will be omitted.

[0044] In the rotation angle detection step (third step) according to this embodiment, when the rotation of the workpiece W1 is suddenly stopped, the servo motor 15 tries to stop the workpiece W1 at the set rotation angle θ0, but in reality, variations occur due to inertial forces and the like. For example, variations of about ±1° occur. Therefore, the servo motor 15 does not stop the rotation, but detects the actual rotation angle θ of the workpiece W1 while maintaining a constant rotation speed (for example, in the case of a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm) with a reduced speed, and outputs a detection signal S1 representing the detection result to the control unit 14. The control unit 14 outputs a control signal S2 to the servo motor 15, and causes the servo motor 15 to rotate the workpiece W1 again so that the rotation angle θ of the workpiece W1 approaches the set value θ0. The absolute value of the rotation amount at this time is, for example, less than 1°. The friction welding method and member manufacturing method according to the present embodiment can suppress such variations by being configured as described above.

[0045] The rotation angle detection process (third process) in this embodiment can also be applied to the rotation angle detection process (third process) in the second embodiment. Other configurations and effects are similar to those in the first embodiment, so description thereof will be omitted.

[0046] Sixth embodiment Next, a friction welding method and a method for manufacturing a member according to a sixth embodiment will be described. In the sixth embodiment, the rotation angle detection step (third step) is different from the third embodiment. The other steps and effects of the present embodiment are similar to those of the third embodiment, so the description will be omitted.

[0047] In the rotation angle detection process (third process) according to this embodiment, when the rotation of the workpiece W1 is suddenly stopped, the servo motor 15 attempts to stop the workpiece W1 at the set rotation angle θ0, but in reality, variations occur due to inertial force, etc. For example, variations of about ±1° occur. The same can be said for the workpiece W2.

[0048] Therefore, the servo motor 15 and the vice 13 do not stop rotating, but maintain a constant rotation speed at a reduced speed (for example, when the workpiece is a hollow rack bar with a diameter of 30 mm and a thickness of 4 mm, the workpiece W1 is 100 rpm or more and 300 rpm or less, and the workpiece W2 is 10 rpm or more and 50 rpm or less), while detecting the actual rotation angle θ of the workpiece W1, and outputting a detection signal S1 representing the detection result to the control unit 14. The control unit 14 outputs a control signal S2 to the servo motor 15, and causes the servo motor 15 to rotate the workpiece W1 again so that the rotation angle θ of the workpiece W1 approaches the set value θ0. The absolute value of the amount of rotation at this time is, for example, less than 1°. The friction welding method and member manufacturing method according to the present embodiment can suppress such variations by being configured as described above.

[0049] The rotation angle detection process (third process) in this embodiment can also be applied to the rotation angle detection process (third process) in the fourth embodiment. Other configurations and effects are similar to those in the fourth embodiment, so description thereof will be omitted.

[0050] The above-described embodiments are examples of the present invention, and the present invention is not limited to these embodiments. For example, the present invention also includes the addition, deletion, or modification of some components or steps in each of the above-described embodiments. [Explanation of symbols]

[0051] 1: Friction welding machine 10: Base 11: Support part 12: Zipper 13: Vice 14: Control unit 15: Servo motor B1, B2: Tooth surface M: Material P: Joint surface S1: Detection signal S2: Control signal W1, W2: Work

Claims

1. a first step of rotating a first workpiece and pressing a second workpiece against the rotating first workpiece while holding the second workpiece at a constant rotation angle, thereby heating a contact portion between the first workpiece and the second workpiece; a second step of stopping the rotation of the first workpiece and increasing a load pressing the second workpiece against the first workpiece; a third step of detecting a rotation angle of the first work while the second work is being pushed into the first work, and rotating the first work again so that the rotation angle of the first work approaches a set rotation angle; A fourth step of releasing the load; A friction welding method comprising:

2. a first step of pressing a second workpiece against the fixed first workpiece while holding the second workpiece at a certain rotation angle, and then rotating the first workpiece to heat a contact portion between the first workpiece and the second workpiece; a second step of stopping the rotation of the first workpiece and increasing a load pressing the second workpiece against the first workpiece; a third step of detecting a rotation angle of the first work while the second work is being pushed into the first work, and rotating the first work again so that the rotation angle of the first work approaches a set rotation angle; A fourth step of releasing the load; A friction welding method comprising:

3. a first step of pressing a second workpiece against the fixed first workpiece while holding the second workpiece at a certain fixed angle, and then rotating the first workpiece and the second workpiece to heat a contact portion between the first workpiece and the second workpiece; a second step of stopping the rotation of the first workpiece and increasing a load pressing the second workpiece against the first workpiece; a third step of detecting a rotation angle of the first work while the second work is being pushed into the first work, and rotating the first work again so that the rotation angle of the first work approaches a set rotation angle; A fourth step of releasing the load; A friction welding method comprising:

4. A first step of rotating a first workpiece, pressing a second workpiece against the rotating first workpiece while holding the second workpiece at a constant fixed angle, and then rotating the second workpiece to heat a contact portion between the first workpiece and the second workpiece; a second step of stopping the rotation of the first workpiece and increasing a load pressing the second workpiece against the first workpiece; a third step of detecting a rotation angle of the first work while the second work is being pushed into the first work, and rotating the first work again so that the rotation angle of the first work approaches a set rotation angle; A fourth step of releasing the load; A friction welding method comprising:

5. The second step includes stopping the rotation of the second workpiece and increasing a load pressing the first workpiece against the second workpiece, 5. The friction welding method according to claim 3 or 4, wherein the third step comprises detecting a rotation angle of the second work while the first work is being pushed into the second work, and rotating the second work again so that the rotation angle of the second work approaches a set rotation angle.

6. A method for manufacturing a member, comprising the friction welding method according to any one of claims 1 to 5.

7. The member is a rack bar, The first workpiece has a first tooth surface formed thereon; The method for manufacturing a member according to claim 6, wherein the second workpiece has a second tooth surface formed thereon.

8. The method for manufacturing a member according to claim 6 or 7, wherein the member is hollow.

9. a chuck having a servo motor and rotating a first workpiece by the servo motor; A vice that holds a second workpiece at a certain rotation angle and presses the second workpiece against the first workpiece; a control unit that detects a rotation angle of the first work based on a signal from the servo motor while the second work is being pressed into the first work after the servo motor stops rotating in a state in which the vice presses the second work against the first work, and causes the servo motor to rotate the first work again so that the rotation angle of the first work approaches a set value; A friction welding machine equipped with

Citation Information

Patent Citations

  • JP1969013814Y1

  • Friction welding method

    JP2008272834A

  • Structural part and method of making this structural part

    JP3355586B2

  • Machine tool

    WO2020017514A1