Melt forming mold
The melt molding mold with a cylindrical hole and grooves minimizes heat conduction to maintain uniform temperature in the quartz plate, enhancing precision and reducing costs in manufacturing vibrators.
Patent Information
- Application Number
- JP2021107971
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-06-29
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2041-06-29
AI Technical Summary
The heat conduction from the heated quartz plate to the mold generates a temperature gradient in the quartz plate, affecting the processed shape of the vibrator.
The melt molding mold features a back surface with a hollowed-out cylindrical hole, a support extending from the hole's bottom, and parallel and vertical grooves that minimize heat conduction paths, along with a lower mold made of a material with lower thermal conductivity.
This design suppresses temperature gradients in the quartz plate, allowing for precise shaping and improved manufacturing accuracy, reducing manufacturing costs and extending the life cycle of the mold.
Smart Images

Figure 0007579215000001 
Figure 0007579215000002 
Figure 0007579215000003
Abstract
Description
[Technical field]
[0001] The present specification relates to a melt-molding mold for a transducer. [Background technology]
[0002] Patent Document 1 discloses a Bird-bath Resonator Gyroscope (BRG) that uses fused silica as an oscillator as a gyro capable of achieving high accuracy. Specifically, a quartz plate is placed in a mold having a hole formed in its surface so as to cover the hole. While reducing the pressure inside the hole, the top surface of the quartz plate is heated with a burner. The quartz plate is melted and deformed so as to enter the inside of the hole, thereby producing a hemispherical oscillator. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] US Patent Application Publication No. 2018 / 079129 Summary of the Invention [Problem to be solved by the invention]
[0004] The heat from the heated quartz plate is released to the mold via the contact surface between the quartz plate and the surface of the mold. This creates a temperature gradient in the quartz plate, where the temperature drops from the center of the hole to the periphery. This temperature gradient can affect the processed shape of the transducer. [Means for solving the problem]
[0005] One embodiment of the melt-molding mold disclosed in the present specification has a back surface. The melt-molding mold has a surface parallel to the back surface. The melt-molding mold has a hole formed on the surface, the hole having a shape in which a cylinder is hollowed out with an axis perpendicular to the surface as its center and having a hole bottom surface. The melt-molding mold has a support extending upward from the hole bottom surface with the axis as its center. The melt-molding mold has a first groove formed so as to surround the periphery of the hole. The first groove communicates with at least one of the outer peripheral surface or the hole of the melt-molding mold, and does not communicate with the back surface or the front surface. The width of the first groove in a direction perpendicular to the surface is smaller than the width in a direction parallel to the surface.
[0006] The first groove can reduce the heat conduction path from the top to the bottom of the melt forming mold. It can suppress the heat discharge to the melt forming mold. This can suppress the temperature gradient that occurs in the processed material, where the temperature decreases from the center of the hole to the periphery.
[0007] The melt forming mold may further include a temperature sensor disposed inside the first groove. The effects will be described in detail in the Examples.
[0008] The melt molding die may include a lower mold and an upper mold that are integrated by fitting together. A first groove may be formed in a region where the upper surface of the lower mold and the lower surface of the upper mold face each other with a distance therebetween. Details of the effect will be described in the examples.
[0009] The lower mold may be made of a material having a lower thermal conductivity than the upper mold, the effect of which will be described in detail in the examples.
[0010] The first groove may be connected to the hole, but may not be connected to the outer peripheral surface of the melt-molding mold. The melt-molding mold may further include one or more exhaust holes penetrating from the bottom surface of the hole to the back surface. Details of the effects will be described in the examples.
[0011] The melt forming mold may further include a second groove formed so as to surround the periphery of the hole. The second groove may be connected to the back surface, and may not be connected to the outer peripheral surface, the hole, or the front surface of the melt forming mold. The width of the second groove in a direction parallel to the front surface may be smaller than the width in a direction perpendicular to the front surface. Details of the effects will be described in the examples.
[0012] The melt molding die may further include a cylindrical member disposed inside the hole and having a cylindrical shape centered on the axis. A certain gap may be formed between the outer peripheral surface of the cylindrical member and the inner peripheral surface of the hole. Details of the effects will be described in the examples. [Brief description of the drawings]
[0013] [Figure 1] FIG. 2 is a top view of the molding apparatus 1 of the first embodiment. [Diagram 2] FIG. 1 is a cross-sectional view of a molding apparatus 1 of a first embodiment. [Diagram 3] FIG. 3 is a cross-sectional view after melt deformation. [Figure 4] 1A and 1B are top and cross-sectional views of BRG 60. [Diagram 5] 13 is a cross-sectional view showing a case where a vibrator 31 is produced using a conventional molding die 1020. FIG. [Figure 6] 1 is a cross-sectional view showing a case where a vibrator 31 is produced using the molding die 20 of this embodiment. [Figure 7] FIG. 11 is a top view of a molding apparatus 201 according to a second embodiment. [Figure 8] FIG. 11 is a cross-sectional view of a molding apparatus 201 according to a second embodiment. [Figure 9] FIG. 11 is a cross-sectional view of a molding apparatus 301 according to a third embodiment. [Figure 10] FIG. 11 is a top view of a molding apparatus 401 according to a fourth embodiment. [Figure 11] FIG. 11 is a cross-sectional view of a molding apparatus 401 according to a fourth embodiment. [Figure 12] 13A to 13C are diagrams illustrating a method for forming a cylindrical liner 421. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS EXAMPLES
[0014] Figures 1 and 2 show a molding apparatus 1 of Example 1. Figure 1 is a top view. Figure 2 is a cross-sectional view taken along line II-II in Figure 1. The molding apparatus 1 includes a plate 10, a molding die 20, a quartz plate 30, a thermocouple 40, and a burner 50. Note that the burner 50 is not shown in Figure 1.
[0015] The plate 10 is a stainless steel base for mounting the molding die 20. The plate 10 has an opening 10a. The opening 10a can be evacuated by a vacuum pump (not shown).
[0016] The mold 20 is a mold for molding a hemispherical vibrator 31 using fused silica. The vibrator 31 will be described later. The mold 20 includes a lower mold 20L and an upper mold 20U. The lower mold 20L and the upper mold 20U can be integrated by fitting them together. In this embodiment, the cylindrical protrusion 20Up of the upper mold 20U is fitted into the circular groove 20Lt of the lower mold 20L, and the two are integrated together. The lower mold 20L is made of a material with a lower thermal conductivity than the upper mold 20U. In this embodiment, the material of the lower mold 20L is boron nitride (BN), and the material of the upper mold 20U is graphite.
[0017] In this embodiment, the mold 20 has a disk shape with a central axis CA. The mold 20 has a back surface 20r, a front surface 20s, a hole 20h, a support 20p, an exhaust port 20e, and a parallel groove 20t1. The back surface 20r and the front surface 20s are flat surfaces perpendicular to the central axis CA. The front surface 20s is parallel to the back surface 20r. A hole 20h is formed in a part of the front surface 20s. The hole 20h is a deformation space for the quartz plate 30 to melt and deform. In this embodiment, the hole 20h has a shape in which a cylinder centered on the central axis CA is hollowed out. The hole 20h has a bottom surface 20b. A support 20p extending vertically upward from the bottom surface 20b is arranged in the center of the hole 20h. The support 20p is a cylinder with the central axis CA as its central axis. The bottom surface 20b has a plurality of exhaust ports 20e penetrating the back surface 20r. The exhaust port 20e communicates with the opening 10a.
[0018] The parallel groove 20t1 is a groove extending approximately parallel to the surface 20s. The parallel groove 20t1 is formed so as to surround the periphery of the hole 20h. In this embodiment, the parallel groove 20t1 is formed in an area where the upper surface 20Lu of the lower molding die 20L and the lower surface 20Ur of the upper molding die 20U face each other with a distance. In other words, the parallel groove 20t1 is formed by the gap between the divided lower molding die 20L and upper molding die 20U. This makes it possible to form the parallel groove 20t1 with high accuracy and at low cost, compared to the case where a parallel groove is formed in an integral molding die.
[0019] The parallel groove 20t1 communicates with the outer peripheral surface 20c of the forming die 20 (see region R1). The parallel groove 20t1 does not communicate with the back surface 20r or the front surface 20s. The parallel groove 20t1 has a width W1 in a direction perpendicular to the front surface 20s and a width W2 in a direction parallel to the front surface 20s. The width W1 is smaller than the width W2.
[0020] A thermocouple 40 is disposed inside the parallel groove 20t1, thereby making it possible to measure the temperature of the region TR located in the vicinity of the hole 20h of the upper molding die 20U.
[0021] Three spacers 20Us are arranged on the outer periphery of the lower surface 20Ur of the upper mold 20U. The spacers 20Us may be formed integrally with the upper mold 20U or may be formed as separate parts. The height H1 of the spacers 20Us is equal to the width W1 of the parallel groove 20t1. The lower surface of the spacers 20Us is in contact with the upper surface 20Lu of the lower mold 20L. This allows the outer periphery of the upper mold 20U to be supported, thereby increasing the rigidity. It is possible to prevent damage to the mold 20 due to thermal shock or the like. The number of spacers 20Us can be freely set as long as it is three or more. This allows the outer periphery of the upper mold 20U to be supported by a surface.
[0022] A quartz plate 30 is disposed on the surface 20s so as to cover the hole 20h. The quartz plate 30 is a material to be processed for forming an oscillator. The thickness of the quartz plate 30 is, for example, 100 μm or less. In this embodiment, the quartz plate 30 is square, but may be rectangular or circular. The burner 50 is a means for heating the quartz plate 30 by flame. The burner 50 is movable up and down along a central axis CA.
[0023] (manufacturing process) The manufacturing process of the vibrator will be described with reference to Figures 2 and 3. In step S1, the mold 20 is placed on the plate 10. In step S2, the quartz plate 30 is placed on the surface 20s. In step S3, the opening 10a is evacuated to a desired vacuum level. The hole 20h is also evacuated via the exhaust port 20e. The quartz plate 30 is adsorbed and fixed to the surface 20s. This results in the state shown in Figure 2.
[0024] In step S4, a heating step is performed. Specifically, the burner 50 is ignited and lowered at a desired speed. In step S5, a measurement step is performed. The temperature of the region TR of the upper mold 20U is measured using a thermocouple 40. In step S6, processing parameters are controlled based on the measured temperature values. Specifically, various processing parameters such as the gas flow rate of the burner 50, the distance between the burner 50 and the quartz plate 30, the reduced pressure, and the heating time are feedback-controlled based on the measured temperature values. This allows the quartz plate 30 to be melted and deformed into a desired shape, as shown in FIG. 3.
[0025] In step S7, in response to detection of the end point of processing, the burner 50 is raised and extinguished. After the quartz plate 30 is cooled to a desired temperature, the hole 20h is opened to the atmosphere. The fused quartz plate 30 is removed from the mold 20.
[0026] It should be noted that step S6 may be omitted. In this case, the end point of processing may be detected based on the temperature measured by the thermocouple 40 in step S7.
[0027] In step S8, the unformed region UR of the quartz plate 30 is removed by a CMP method or the like to complete the transducer 31. In step S9, a Bird-bath Resonator Gyroscope (BRG) is assembled. FIG. 4(A) shows a top view of the BRG 60. FIG. 4(B) shows a cross-sectional view along line BB in FIG. 4(A). The BRG 60 includes a transducer 31, a glass substrate 61, and a silicon electrode 62. The transducer 31 includes an anchor 31a and a rim 31r. The anchor 31a is fixed to a fixing portion 61f of the glass substrate 61. The silicon electrode 62 is disposed so as to surround the periphery of the rim 31r.
[0028] The operation of the BRG 60 will now be described. A voltage of a desired frequency is applied between the vibrator 31 and the silicon electrode 62, causing the vibrator 31 to resonate. When the BRG 60 is rotated around the z-axis in this state, the vibration mode changes. By measuring the electrostatic capacitance between the vibrator 31 and the silicon electrode 62 that accompanies this change, the rotation angle can be detected with high precision.
[0029] (effect) The problem will be explained. In order to increase the sensitivity of the BRG 60, the inclination angle θ (see FIG. 4(B)) of the rim 31r of the vibrator 31 needs to be close to 90°. This is because the change in capacitance due to the action of the rotation angle is increased by making the rim 31r and the side of the silicon electrode 62 parallel and reducing the distance between them. Here, as a comparative example, a case where the vibrator 31 is manufactured using a conventional molding die 1020 shown in FIG. 5 will be explained. The conventional molding die 1020 is a die that does not have parallel grooves 20t1. The white arrow indicates the heat conduction in the molding die 1020, and the larger the area of the arrow, the larger the amount of heat transfer. In the conventional molding die 1020, the entire molding die 1020 becomes a heat conduction path to the plate 10, so the width HW1 of the heat conduction path is very wide. Therefore, as shown by the white arrow, a large part of the heat of the quartz plate 30 is discharged to the plate 10 through the molding die 1020. As a result, the quartz plate 30 has a temperature gradient in which the temperature decreases toward the outer periphery of the hole 20h, and an undeformed region NR (a region that is not heated above the softening temperature of quartz and does not deform the quartz plate 30) is formed. Therefore, the inclination angle θ becomes smaller than 90°. Next, a case where the vibrator 31 is produced using the mold 20 of this embodiment shown in FIG. 6 will be described. The mold 20 of this embodiment has parallel grooves 20t1. The black arrows indicate the thermal conduction of the air in the parallel grooves 20t1, and the larger the area of the arrow, the larger the amount of heat transfer. The thermal conductivity of the air in the parallel grooves 20t1 is extremely low compared to the thermal conductivity of graphite. Therefore, as shown by the black arrows, the amount of heat transfer can be reduced in the region where the parallel grooves 20t1 are arranged compared to the region where the parallel grooves 20t1 are not arranged. In other words, the parallel grooves 20t1 can insulate the plate 10. As a result, the region where the parallel grooves 20t1 are not formed becomes a heat transfer path to the plate 10, so the width HW2 (FIG. 6) of the heat transfer path can be made narrower than the width HW1 (FIG. 5). Since the amount of heat exhausted to the plate 10 via the forming die 20 can be reduced, it is possible to suppress the temperature gradient occurring in the quartz plate 30. Since the formation of the undeformed region NR is suppressed, it is possible to make the inclination angle θ closer to 90°.
[0030] The lower molding die 20L (boron nitride) is made of a material having a lower thermal conductivity than the upper molding die 20U (graphite). This makes it possible to suppress the conduction of heat from the upper molding die 20U to the plate 10.
[0031] The parallel groove 20t1 can be used as a passage for inserting the thermocouple 40. This allows the process to be controlled based on the temperature information of the region TR of the upper molding die 20U, improving the accuracy of the process control. The variation in the processed shape of the resonator can be suppressed, improving the yield and reducing the manufacturing cost. EXAMPLES
[0032] 7 and 8 show a top view and a cross-sectional view of a molding apparatus 201 of Example 2. Example 2 differs from Example 1 in that a fitting portion between a lower molding die 220L and an upper molding die 220U is disposed on the outer periphery of a molding die 220. Parts common to the molding apparatus 1 of Example 1 are given the same reference numerals and description thereof will be omitted.
[0033] The molding die 220 includes a lower molding die 220L and an upper molding die 220U. The lower molding die 220L includes a circular groove 220Lt that surrounds the outer periphery. The upper molding die 220U includes a cylindrical protrusion 220Up that surrounds the outer periphery. The protrusion 220Up fits into the groove 220Lt, thereby forming the lower molding die 220L and the upper molding die 220U into one body.
[0034] The parallel groove 220t1 communicates with the hole 20h (see region R21 in FIG. 8). The parallel groove 220t1 does not communicate with the outer peripheral surface 20c, the back surface 20r, or the front surface 20s of the forming die 220. A thermocouple 40 is disposed inside the parallel groove 220t1, penetrating the protrusion 220Up. The penetration portion of the thermocouple 40 is kept airtight by a seal or the like. The other configurations of the parallel groove 220t1 of the second embodiment are the same as those of the parallel groove 20t1 of the first embodiment, and therefore will not be described.
[0035] Three spacers 220Us are arranged on the inner periphery of the lower surface 20Ur of the upper molding die 220U. The configuration of the 220Us in the second embodiment is similar to that of the spacer 20Us in the first embodiment, and therefore a detailed description thereof will be omitted. The three spacers 220Us can support the inner periphery of the upper molding die 220U with a surface, thereby increasing the rigidity.
[0036] (effect) The airtightness of the outer periphery of the parallel groove 220t1 is maintained by the engagement between the groove 220Lt and the protrusion 220Up. The parallel groove 220t1 is also connected to the hole 20h. Therefore, the inside of the parallel groove 220t1 can be made into a vacuum state by evacuating the hole 20h. Compared to the case where air exists in the parallel groove 220t1, it is possible to further reduce the amount of heat transfer in the area where the parallel groove 220t1 is arranged. It is possible to make the inclination angle θ of the vibrator 31 close to 90°. EXAMPLES
[0037] 9 shows a cross-sectional view of a molding apparatus 301 of Example 3. Example 3 differs from Example 2 in that a lower molding die 220L is provided with a vertical groove 220t2. The same reference numerals are used to designate parts common to the molding apparatus 201 of Example 2, and description thereof will be omitted.
[0038] The lower molding die 220L has a vertical groove 220t2. The vertical groove 220t2 is a groove that extends substantially perpendicular to the surface 20s. The vertical groove 220t2 is formed so as to surround the periphery of the hole 20h. The vertical groove 220t2 communicates with the opening 10a via the back surface 20r. The vertical groove 220t2 does not communicate with the outer peripheral surface 20c, the hole 20h, or the surface 20s of the molding die 220. The vertical groove 220t2 has a width W31 in a direction parallel to the surface 20s and a width W32 in a direction perpendicular to the surface 20s. The width W31 is smaller than the width W32.
[0039] (effect) The vertical grooves 220t2 can insulate the periphery of the hole 20h. As a result, the area where the vertical grooves 220t2 are not formed becomes a heat conduction path to the plate 10, so that the heat conduction path can be further narrowed. Since the amount of heat exhausted to the plate 10 via the molding die 20 can be further reduced, the inclination angle θ of the vibrator 31 can be made closer to 90°.
[0040] By drawing a vacuum through the opening 10a, the inside of the vertical groove 220t2 can be made into a vacuum state, which can further improve the heat insulating effect of the vertical groove 220t2 compared to a case where air exists inside the vertical groove 220t2. EXAMPLES
[0041] Figures 10 and 11 show a top view and a cross-sectional view of a forming apparatus 401 of Example 4. Figure 11 is a cross-sectional view taken along line XI-XI in Figure 10. Note that the quartz plate 30 and the burner 50 are omitted in Figure 10. Also, Figure 11 shows the quartz plate 30 after deformation.
[0042] The molding apparatus 401 includes a plate 410, a mold base 420, a support 420p, a cylindrical liner 421, and a quartz plate 30. The plate 410 is made of stainless steel. The plate 410 includes a lower plate 410L and an upper plate 410U. The lower plate 410L includes an opening 410a. The opening 410a is connected to a vacuum pump (not shown) via an exhaust pipe 410p.
[0043] Upper plate 410U has engagement grooves 410t1-410t3 on front surface 410s. The lower surface of mold base 420 engages with engagement groove 410t1. The lower surface of cylindrical liner 421 engages with engagement groove 410t2. The lower surface of support 420p engages with engagement groove 410t3. Upper plate 410U also has intake holes 410v1-410v3 penetrating through rear surface 410r of upper plate 410U. The upper end of intake hole 410v1 contacts the rear surface of mold base 420. The upper end of intake hole 410v2 contacts the rear surface of cylindrical liner 421. The upper end of intake hole 410v3 contacts the rear surface of support 420p. As a result, by drawing a vacuum in opening 410a, casting mold base 420, cylindrical liner 421, and support 420p can be adsorbed and fixed to upper plate 410U. Upper plate 410U also has exhaust port 410e penetrating rear surface 410r. Exhaust port 410e communicates between hole 421h and opening 410a.
[0044] The molding die base 420 includes a lower molding die base 420L and an upper molding die base 420U. A parallel groove 420t1 is formed between the lower molding die base 420L and the upper molding die base 420U. The structures of the lower molding die base 420L and the upper molding die base 420U are similar to those of the lower molding die 220L and the upper molding die 220U of the second embodiment, and therefore a description thereof will be omitted.
[0045] The mold base 420 has a hole 420a having a shape of a hollow cylinder centered on a central axis CA. A cylindrical liner 421 is disposed inside the hole 420a. The cylindrical liner 421 is a cylindrical member having a cylindrical shape centered on the central axis CA. A hole 421h is formed inside the cylindrical liner 421, which is a deformation space for the quartz plate 30 to melt and deform. A processing reference surface 421m is formed on the upper side of the inner wall of the cylindrical liner 421. A certain gap G1 is formed between the outer peripheral surface of the cylindrical liner 421 and the inner peripheral surface of the hole 420a.
[0046] In the molding device 401, materials can be appropriately selected according to the functions required for each part. For example, the cylindrical liner 421 and the support 420p that contact the quartz plate 30 may be made of a material that is excellent in thermal shock resistance and has a thermal conductivity of 30 W / (m·K) or more. In addition, the parts that do not contact the quartz plate 30 may be made of an oxide that has a thermal conductivity of less than 10 W / (m·K) and is not subject to oxidation wear. Since the thermal conductivity of the parts that do not contact the quartz plate 30 can be reduced, it is possible to suppress the heat conduction to the plate 410. In this embodiment, the cylindrical liner 421 and the support 420p are graphite or BN. In addition, the mold base 420 is cordierite.
[0047] (Method of Formation and Function of Cylindrical Liner 421) A method for forming the cylindrical liner 421 will be described with reference to Figs. 12(A) to (C). Figs. 12(A) to (C) are cross-sectional views passing through the central axis CA. The first reference mold 71 and the second reference mold 72 have a concentric shape centered on the central axis CA. As shown in Fig. 12(A), raw material powder 73 (e.g. boron nitride) is placed in the first reference mold 71 and compressed by the second reference mold 72. By sintering in this state, a sintered body 73s is obtained as shown in Fig. 12(B). As shown in Fig. 12(C), the opening 73a is processed to complete the cylindrical liner 421.
[0048] The cylindrical liner 421 has a machining reference surface 421m. The machining reference surface 421m is a curved surface that follows the ideal shape of the rim 31r of the transducer 31. As shown in Fig. 11, the quartz plate 30 after melt molding comes into contact with the machining reference surface 421m. This allows the transducer 31 to be molded along the machining reference surface 421m, thereby improving the reproducibility of the shape of the rim 31r.
[0049] In this embodiment, the machining reference surface 421m is powder-pressed by the second reference mold 72. This makes it possible to suppress variation in the machining accuracy of the machining reference surface 421m compared to the case where the machining reference surface 421m is formed by cutting or the like. As a result, it is possible to improve the reproducibility of the shape of the rim 31r of the vibrator 31.
[0050] (effect) By forming gap G1 between the outer circumferential surface of cylindrical liner 421 and the inner circumferential surface of hole 420a, the difference in the amount of thermal expansion between cylindrical liner 421 and mold base 420 can be absorbed. It becomes possible to prevent damage to cylindrical liner 421 and mold base 420. In addition, gap G1 can suppress the thermal conduction from cylindrical liner 421 to mold base 420, so that it becomes possible to suppress the exhaust of heat to mold base 420.
[0051] By forming the mold base 420, the support columns 420p, and the cylindrical liner 421 as separate parts, it is possible to replace only the deteriorated parts, thereby making it possible to extend the life cycle of the molding apparatus 401.
[0052] (Modification of the fourth embodiment) The cross-sectional shape of the cylindrical liner 421 may be a shape that does not include the machining reference surface 421m. The gap G1 may be in a vacuum state.
[0053] Although specific examples of the present invention have been described in detail above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and changes of the specific examples exemplified above.
[0054] (Modification)
[0055] The mold is not limited to a form divided into the upper molding die 20U (or 220U) and the lower molding die 20L (or 220L), and may be integrally molded.
[0056] The parallel grooves 20t1 and 220t1 are not limited to being parallel to the surface 20s, but may be inclined or meandering with respect to the surface 20s.
[0057] The material of the molds 20, 220 is not limited to boron nitride or graphite, but may be any material having a desired thermal shock resistance and thermal conductivity.
[0058] A configuration not including the spacers 20Us and 220Us is also possible.
[0059] The material of the vibrator is not limited to the quartz plate 30. Any dielectric material that melts and deforms may be used.
[0060] In addition, the technical elements described in this specification or drawings exert technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technologies exemplified in this specification or drawings can achieve multiple objectives simultaneously, and achieving one of those objectives is itself technically useful.
[0061] The parallel grooves 20t1 and 220t1 are an example of a first groove. The thermocouple 40 is an example of a temperature sensor. The vertical groove 220t2 is an example of a second groove. [Explanation of symbols]
[0062] 1, 201, 301, 401: Molding equipment 20, 220: Molding mold 20L, 220L: Lower mold 20U, 220U: Upper mold 20r: Back side 20s: Surface 20h, 421h: Hole 20t1, 220t1, 420t1: Parallel groove 20e, 410e: Exhaust port
Claims
1. The back and A surface parallel to the back surface; a hole formed in the surface, the hole having a cylindrical shape with an axis perpendicular to the surface as a center and a hole bottom surface; A support pillar extending upward from the bottom surface of the hole about the axis; A first groove formed to surround the hole; A melt molding mold comprising: The first groove is the hole portion is in communication with at least one of the outer peripheral surface of the melt-molding mold and the hole portion, and is not in communication with the back surface and the front surface; A melt-forming mold having a width perpendicular to said surface that is smaller than a width parallel to said surface.
2. The molten mold of claim 1 further comprising a temperature sensor disposed within the first groove.
3. The melt molding die includes a lower molding die and an upper molding die which are integrated by fitting together, 3. The melt-molding mold according to claim 1, wherein the first groove is formed in a region where an upper surface of the lower mold and a lower surface of the upper mold face each other with a distance therebetween.
4. The melt-molding mold according to claim 3 , wherein the lower mold is made of a material having a lower thermal conductivity than the upper mold.
5. the first groove communicates with the hole portion but does not communicate with the outer circumferential surface of the melt-molding mold; The melt-forming mold according to any one of claims 1 to 3, further comprising one or more exhaust holes penetrating from the bottom surface of the hole to the back surface.
6. A second groove is further provided so as to surround the hole, The second groove is the hole portion is connected to the rear surface of the melt-molding mold, and is not connected to the outer peripheral surface of the melt-molding mold, the hole portion, or the front surface; a width in a direction parallel to the surface is smaller than a width in a direction perpendicular to the surface; The melt-molding mold according to any one of claims 1 to 5.
7. The cylindrical member is disposed inside the hole and has a cylindrical shape centered on the axis.
7. The melt molding die according to claim 1, wherein a constant gap is formed between an outer peripheral surface of the cylindrical member and an inner peripheral surface of the hole.
Citation Information
Patent Citations
Production of glass container
JP1986281032A
Half-donut-shaped resonator gyroscope
JP2012042452A
MEMS mirror mechanism and method for manufacturing the same
JP2020528582A
Thermal Control Mold For Making Three-Dimensional Microstructures
US20180079129A1