Joining device and joining method for friction stir welding and resistance welding
A combined friction stir welding and resistance welding device and method addresses the challenges of joining dissimilar metal plates by using a single apparatus with integrated electrodes, achieving efficient, stable bonding and reduced environmental impact.
Patent Information
- Application Number
- JP2021118229
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-07-16
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2041-07-16
AI Technical Summary
Conventional methods for joining three or more metal plates with dissimilar materials face challenges such as increased production time, capital investment, and environmental impact due to the need for multiple joining techniques and equipment, leading to unstable bonding strength and difficulty in expanding the stirring range during friction stir welding.
A combined joining device and method that utilizes an anvil and probe for both friction stir welding and resistance welding, where the anvil and probe serve as electrodes for resistance welding, allowing simultaneous performance of both techniques to reduce equipment size and processing time, and includes insulating components to prevent melting and improve bonding quality.
The solution reduces the size of the equipment, minimizes capital investment, and decreases processing time while enhancing bonding strength and energy efficiency, reducing environmental impact by minimizing gas generation and power consumption.
Smart Images

Figure 0007579763000001 
Figure 0007579763000002 
Figure 0007579763000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a joining apparatus and a joining method for friction stir welding and resistance welding. [Background technology]
[0002] Resistance welding and friction stir welding are examples of methods for joining multiple metal plates together that generate less gas than conventional welding methods, thereby reducing the negative environmental impact on air quality (SDGs 11.6). Furthermore, friction stir welding consumes less electricity than conventional welding methods, contributing to improved energy efficiency during manufacturing (SDGs 7.3).
[0003] When three or more metal plates including dissimilar materials are joined together by resistance welding, an adhesive is used to prevent electrolytic corrosion. This causes defects due to the adhesive, making it impossible to obtain a stable joint strength, and rivets must be used in combination to obtain the required strength. When three or more metal plates including dissimilar materials are joined together by friction stir welding, for example, one aluminum alloy plate and two steel (iron alloy) plates, the first and second layers (Al-Fe) can be joined, but it is difficult to join the second and third layers (Fe-Fe) because the stirring range cannot be expanded. Thus, it is difficult to join three or more metal plates including dissimilar materials using one joining method.
[0004] As a method for joining three or more metal members including dissimilar materials to each other by combining different joining methods, Patent Document 1 describes a method for joining an aluminum material, a steel material, and a clad material (a composite material in which dissimilar materials are rolled into one plate) including an aluminum material layer and a steel material layer. Patent Document 1 describes an embodiment in which an aluminum material and an aluminum material layer of a clad material are joined to each other by friction stir welding, and a steel material and a steel material layer of a clad material are joined to each other by a thermosetting adhesive using frictional heat generated by the friction stir welding, and an embodiment in which a steel material and a steel material layer of a clad material are joined to each other by resistance welding, and an aluminum material and an aluminum material layer of a clad material are joined to each other by a thermosetting adhesive using heat generated by the resistance welding. However, this method is lacking in versatility because it uses a clad material. Patent Document 2 describes that two members that are butted against each other are joined to each other by friction stir line welding, and then another member is fusion-welded or resistance-welded to the joint. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2005-111489 A [Patent Document 2] JP 2007-237253 A Summary of the Invention [Problem to be solved by the invention]
[0006] In order to join three or more metal components, including dissimilar materials, it is necessary to combine two or more joining methods. However, with conventional methods, the number of joining steps increases, more than two types of joining equipment must be prepared, and the production line must be lengthened, necessitating increased capital investment.
[0007] In view of the above background, the present invention has an objective of providing a joining device and a joining method that combines friction stir welding and resistance welding, which contributes to reducing adverse environmental impacts on air quality (SDGs 11.6) and / or contributing to improving energy efficiency in manufacturing (SDG 7.3), and which reduces the increase in size of the device and the increase in processing time. [Means for solving the problem]
[0008] In order to solve the above-mentioned problems, one aspect of the present invention provides a joining device (1, 51) for joining each of a first member (3), an intermediate member (4), and a second member (5) which are electrically conductive and extend along a predetermined main surface of a laminate (2) including the first member (3), the intermediate member (4), and the second member (5) stacked in this order, the joining device (1, 51) comprising an anvil (11) which is at least partially electrically conductive for supporting a first surface (6) which constitutes the surface of the laminate (2) facing the first member (3), and a joining device (1, 51) which is at least partially electrically conductive and supports a second surface (7) which constitutes the surface of the laminate (2) facing the second member (5), at a position corresponding to the anvil (11), in a direction intersecting the main surfaces. the anvil (11) and the probe (12, 41, 52) being at least partially conductive and rotatable about an axis extending in the direction of the stack (2) and movable along the axis relative to the second member (5); a drive mechanism (14, 54) for rotating the probe (12, 41, 52) about the axis and moving the probe (12, 41, 52) along the axis; a power source (15) electrically connected to the anvil (11) and the probe (12, 41, 52) so as to pass a current between the anvil (11) and the probe (12, 52) through the stack (2); and a control device (16) for controlling the operation of the drive mechanism (14) and the power source (15). The probes (12, 41, 52) are rotated and advanced toward the stack (2) from the second surface (7) side until the tips of the probes (12, 41, 52) enter the intermediate member (4), and after the tips of the probes (12, 41, 52) reach the intermediate member (4), a current is passed between the probes (12, 41, 52) and the anvil (11) through the pressurized stack (2), The joining device (1, 51) is for resistance welding the first member (3) and the intermediate member (4) together, and for friction stir joining the second member (5) and the intermediate member (4) together.
[0009] According to this embodiment, the anvil and probe used for friction stir welding also serve as electrodes for resistance welding, so that it is possible to suppress the enlargement and increase in size of the equipment and the lengthening of the manufacturing line, and therefore the capital investment can be suppressed. In addition, since friction stir welding and resistance welding can be performed simultaneously, it is possible to suppress the increase in processing time. Furthermore, this embodiment joins the laminated bodies by resistance welding, which generates less gas than general welding methods, and friction stir welding, which generates less gas than general welding methods and consumes less power than general welding methods, thereby reducing the adverse environmental impact on air quality (SDGs 11.6) and contributing to improving energy efficiency during manufacturing (SDG 7.3).
[0010] In the above aspect, the probe (12, 41) may further include a shoulder member (13, 13a, 44) including a through hole (20, 20a) through which the probe (12, 41) is inserted, a shoulder abutment surface (24, 24a) to be pressed against the second surface (7), and a recess (25, 25a) recessed relative to the shoulder abutment surface (24, 24a) to define a bottom surface (26, 26a) to face the second surface (7) and receiving a portion of the probe (12, 41).
[0011] According to this embodiment, a hook that penetrates into the second member is formed in the intermediate member by friction stir welding, resulting in a strong joint.
[0012] In the above aspect, the shoulder member (13) may be at least partially conductive, and the probe (41) may include a probe conductive portion (42) extending from a portion to which the power source (15) is electrically connected to a tip that should face the second surface (7), and a probe insulating portion (43) provided along an outer peripheral surface of the probe conductive portion (42) to insulate between an inner peripheral surface of the through hole (20) and the probe conductive portion (42).
[0013] According to this aspect, the probe insulating portion suppresses or prevents current flow from the probe to the shoulder member, thereby preventing melting of the second member, stabilizing and improving the joining quality, and also increasing the electrical safety of the equipment.
[0014] In the above aspect, the shoulder member (44) may be partially conductive and include a shoulder member insulating portion (46) provided on the shoulder abutment surface (24) and the inner surface of the through hole (20).
[0015] According to this aspect, the shoulder member insulating portion suppresses or prevents current flow to the shoulder member, thereby preventing melting of the second member, stabilizing and improving the joining quality, and also increasing the electrical safety of the equipment.
[0016] In the above aspect, the friction stir welding may be friction stir spot welding, and the shoulder abutment surface (24) may be annular with the probe (12, 41) as its center.
[0017] According to this aspect, the appearance of the joint is improved by the annular shoulder abutment surface.
[0018] In the above aspect, the friction stir welding may be friction stir line welding, and the recess (25a) may be open rearward in a traveling direction along the main surface of the probe (12, 41).
[0019] According to this embodiment, the shoulder member can be advanced so that the deformed portion of the second member that rises due to the insertion of the probe does not collide with the shoulder member, thereby making it possible to perform friction stir line welding.
[0020] One aspect of the present invention is a joining method for joining each member (3, 4, 5) of the stack (2) to one another using the joining device (1, 51) of the above aspect, the method including the steps of: supporting the first surface (6) of the stack (2) on the anvil (11); operating the drive mechanism (14, 54) to insert the probe (12, 41, 52) into the stack (2) from the second surface (7) while rotating the probe (12, 41, 52 about the axis; and turning on the power source (15) after the tip of the probe (12, 41, 52) reaches the intermediate member (4). Therefore, the joining method includes a step of resistance welding the first member (3) and the intermediate member (4) together by passing a current between the probe (12, 41, 52) and the anvil (11), and a step of pulling out the probe (12, 41, 52) from the stack (2), in which the first member (3) and the intermediate member (4) are made of the same material and are made of a different material from the second member (5), and the materials of the first member (3) and the intermediate member (4) have higher strength and higher electrical resistance than the material of the second member (5). Here, the same material means alloy materials having a common main component, and the different materials means alloy materials having different main components.
[0021] According to this embodiment, the anvil and the probe used for friction stir welding also serve as electrodes for resistance welding, so that the size and number of devices and the length of the manufacturing line can be suppressed, and capital investment can be suppressed. In addition, since friction stir welding and resistance welding can be performed simultaneously, an increase in processing time can be suppressed. In addition, it is possible to suppress the occurrence of a brittle intermetallic compound between the second member and the intermediate member, which causes a decrease in the joining strength.
[0022] In the above aspect, the resistance welding step and the withdrawing step may be performed while rotating the probe (12, 41, 52) about the axis.
[0023] According to this aspect, frictional heat generated by the rotation of the probe contributes to resistance welding, thereby reducing energy consumption and suppressing rapid cooling of the portion melted by heat, thereby suppressing a decrease in the toughness of the nugget. Effect of the Invention
[0024] According to the above aspects, it is possible to provide a joining apparatus and a joining method that combine friction stir welding and resistance welding, and that reduces increases in the size of the apparatus and the processing time. [Brief description of the drawings]
[0025] [Figure 1] FIG. 1 is a vertical cross-sectional view showing a joining device according to a first embodiment; [Diagram 2] FIG. 11 is a vertical cross-sectional view showing a modification of the joining device according to the first embodiment with respect to insulation. [Diagram 3] 4A and 4B are diagrams showing a shoulder member of the joining device according to the first embodiment (A: first embodiment, B: modified example, upper figure: cross-sectional view taken along line IV-IV in the lower figure, lower figure: bottom view). [Figure 4] FIG. 1 is an explanatory diagram of a bonding method using a bonding device according to a first embodiment; [Diagram 5] FIG. 11 is a vertical cross-sectional view showing a joining device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a cross-sectional view of a plane including an axis, showing a bonding device 1 according to a first embodiment and a state in the middle of bonding a laminate 2 bonded by the bonding device 1. Below, a case where the axis extends in the vertical direction will be described as an example, but the axis may be inclined with respect to the vertical direction, may extend in the horizontal direction, or may be upside down.
[0027] The laminate 2 includes a first member 3, an intermediate member 4, and a second member 5, each of which is electrically conductive and extends along a main surface perpendicular to the axis, stacked in this order. The axis may intersect with the main surface at an angle other than 90 degrees, instead of being perpendicular. The laminate 2 has a first surface 6 that forms the surface (lower surface) on the first member 3 side, and a second surface 7 that forms the surface (upper surface) on the second member side. The first member 3, the intermediate member 4, and the second member 5 are each formed into a plate shape. One or more other plate materials made of the same material as the first member 3 may be stacked below the first member 3.
[0028] The first member 3 and the intermediate member 4 are made of the same material, and the second member 5 is made of a different material from the first member 3 and the intermediate member 4. The material of the first member 3 and the intermediate member 4 has higher strength and higher electrical resistance than the material of the second member 5. For example, the first member 3 and the intermediate member 4 may be made of an iron alloy (steel) and the second member 5 may be made of an aluminum alloy, the first member 3 and the intermediate member 4 may be made of an iron alloy and the second member 5 may be made of a magnesium alloy, the first member 3 and the intermediate member 4 may be made of a titanium alloy and the second member 5 may be made of an aluminum alloy, the first member 3 and the intermediate member 4 may be made of a titanium alloy and the second member 5 may be made of a magnesium alloy, the first member 3 and the intermediate member 4 may be made of an iron alloy and the second member 5 may be made of a copper alloy, the first member 3 and the intermediate member 4 may be made of a titanium alloy and the second member 5 may be made of a copper alloy, or the first member 3 and the intermediate member 4 may be made of an aluminum alloy and the second member 5 may be made of a copper alloy.
[0029] The joining apparatus 1 comprises an anvil 11 for supporting the first surface 6 of the laminate 2, a probe 12 arranged above the anvil 11, a shoulder member 13 arranged above the anvil 11 and surrounding the probe 12, a drive mechanism 14 for driving the anvil 11, the probe 12 and the shoulder member 13, a power supply 15 for passing current between the probe 12 and the anvil 11 which sandwich the laminate 2, and a control device 16 for controlling the operation of the drive mechanism 14 and the power supply 15.
[0030] The anvil 11 is electrically conductive and has an anvil contact surface 17 that contacts the first surface 6 of the laminate 2 .
[0031] The probe 12 is a part of the rotor 18, and the entire rotor 18 is rotationally symmetrical about the axis and can rotate integrally about the axis. The probe 12 extends along the axis and preferably has a cylindrical shape that is thinner than the upper part 19 of the rotor 18. The tip (lower end) of the probe 12 is a free end so that it can enter the laminate 2. The probe 12 is made of a material such as a copper alloy (chromium copper, alumina-dispersed copper, tungsten copper alloy, etc.), conductive ceramic, or cemented carbide.
[0032] As shown in Fig. 1 and Fig. 3(A), the shoulder member 13 preferably has a rotational symmetric shape around the axis. The shoulder member 13 includes a probe support portion 21 having a through hole 20, a flange 22 extending radially outward from the probe support portion 21, and a side wall portion 23 extending downward from the lower surface of the probe support portion 21 and having a circular ring shape when viewed from below. The central axis of the through hole 20 coincides with the axis. The probe 12 is inserted into the through hole 20. The upper portion of the through hole 20 is expanded in diameter toward the upper portion so as to guide the probe 12 when the probe 12 is inserted. The inner diameter of the lower portion of the through hole 20 is slightly larger than the outer diameter of the probe 12, and when the probe 12 rotates around the axis, the inner peripheral surface of the through hole 20 slides against the outer peripheral surface of the probe 12 to support the probe 12. The inner diameter of the side wall portion 23 is larger than the outer diameter of the probe 12, and the inner peripheral surface of the side wall portion 23 is spaced from the outer peripheral surface of the probe 12. The inner peripheral surface of the side wall portion 23 is preferably inclined so as to be radially outward as it goes downward, but may be parallel to the axial direction. The lower surface of the side wall portion 23 forms a shoulder abutment surface 24 that abuts against the second surface 7 of the laminate 2. A recess 25 is provided on the lower surface of the shoulder member 13. The recess 25 is defined by a bottom surface 26 that is recessed with respect to the shoulder abutment surface 24 and faces the second surface 7 of the laminate 2, and the inner peripheral surface of the side wall portion 23, and receives the lower part of the probe 12. The bottom surface 26 forms the lower surface of the probe support portion 21. The shoulder member 13 is made of a material such as steel, ceramic, or cemented carbide.
[0033] As shown in FIG. 1, the drive mechanism 14 includes an anvil drive mechanism 27 that moves the anvil 11, a rotational drive mechanism 28 that rotates the rotor 18 including the probe 12 about an axis, an advance / retract drive mechanism 29 that moves the probe 12 forward and backward along the axis, and a shoulder drive mechanism 30 that moves the shoulder member 13.
[0034] The power source 15 is electrically connected to the first terminal 31 and the second terminal 32. The first terminal 31 is electrically connected to the anvil 11, and the second terminal 32 is electrically connected to the rotor 18. Even if the anvil 11 and the rotor 18 have partially non-conductive regions, the anvil 11 has electrical conductivity from the point where the first terminal 31 is electrically connected to the anvil abutment surface 17, and the rotor 18 has electrical conductivity from the point where the second terminal 32 is electrically connected to the tip of the probe 12.
[0035] FIG. 2(C) shows the flow of current when the tip of the probe 12 is inserted into the laminate 2 from the second surface 7, and a current is applied from the probe 12 to the anvil 11 through the laminate 2 by the power source 15 (see FIG. 1). The arrows shown in dot patterns indicate the direction of insertion of the probe 12, the thin black arrows indicate the direction of rotation of the probe 12, and the thick black arrows indicate the direction of the current. By applying a current, a nugget 33 (a portion in which the members to be joined are melted and solidified by resistance welding) is formed between the first member 3 and the intermediate member 4, and the first member 3 and the intermediate member 4 are joined to each other. However, the current not only flows straight from the probe 12 to the anvil 11, but also flows from the probe 12 to the shoulder member 13, which reduces the energy efficiency in performing resistance welding. Therefore, as shown in FIG. 2(A) or FIG. 2(B), it is preferable to partially insulate the probe 12 or the shoulder member 13.
[0036] In the description of the modified example of FIG. 2(A) and FIG. 2(B), the same reference numerals are used for the same configurations as those of the first embodiment, and the description thereof will be omitted. In the modified example shown in FIG. 2(A), the probe 41 includes a probe conductive portion 42 that extends along an axis, has a cylindrical shape, and is conductive, and an insulating probe insulating portion 43 that is provided along the outer circumferential surface of the probe conductive portion 42. The lower surface of the probe conductive portion 42 is not covered by the probe insulating portion 43. In the probe 41, it is the probe insulating portion 43 that slides against the inner circumferential surface of the through hole 20 of the shoulder member 13. Instead of the probe insulating portion 43 sliding against the inner circumferential surface of the through hole 20, a layer (not shown) that is highly wear-resistant and insulated from the probe conductive portion 42 by the probe insulating portion 43 may be provided along the outer circumferential surface of the probe insulating portion 43, and this layer may slide against the inner circumferential surface of the through hole 20. The probe insulating portion 43 can prevent a current from flowing from the probe 41 toward the shoulder member 13.
[0037] 2(B), the shoulder member 44 includes the probe support portion 21, the flange 22 (see FIG. 1), and the side wall portion 23, and also includes a conductive shoulder member main body 45, and a shoulder member insulating portion 46 having insulating properties provided along the shoulder abutment surface 24 and the region of the inner circumferential surface of the through hole 20 that comes into sliding contact with the probe 12. The shoulder member insulating portion 46 is preferably further provided along the inner circumferential surface of the side wall portion 23. The shoulder member insulating portion 46 can prevent or suppress a current from flowing from the probe 12 and the laminate 2 to the shoulder member 44.
[0038] In the above two modified examples, the probe conductive part 42 and the shoulder member main body 45 are made of, for example, a copper alloy (chromium copper, alumina-dispersed copper, tungsten copper alloy, etc.), conductive ceramic, cemented carbide, etc. The probe insulating part 43 and the shoulder member insulating part 46 are made of, for example, insulating ceramic, bakelite (phenolic resin), mica, etc.
[0039] The friction stir welding in the above-mentioned joining apparatus 1 is friction stir spot welding, and the appearance of the joint is improved by forming the shoulder abutment surface 24 in an annular shape. On the other hand, by changing the shape of the shoulder member 13 to that shown in Fig. 3(B), friction stir line welding can be achieved. In the shoulder member 13a shown in Fig. 3(B), configurations similar to those of the shoulder member 13 shown in Fig. 3(A) are designated by the same reference numerals with the suffix "a", and explanations of the common parts will be omitted, with only the differences being explained.
[0040] The shoulder member 13a shown in FIG. 3B includes a probe support portion 21a having a through hole 20a, a flange 22a, and a side wall portion 23a having a shoulder abutment portion 24a formed on the lower surface. When the shoulder member 13a is advanced along the second surface 7 while being pressed against the second surface 7, the side wall portion 23a is not provided on the rear side in the advancing direction of the shoulder member 13a, and the rear side in the advancing direction of the recess 25a is open so that the second member 5, which rises upward due to the insertion of the probe 12, is not caught. Therefore, the side wall portion 23a is U-shaped when viewed from below. Instead of the U-shaped shape, the side wall portion 23a may be formed by a pair of walls parallel to the advancing direction (not shown).
[0041] A method for bonding the laminate 2 using the bonding apparatus 1 will be described with reference to FIG.
[0042] As shown in Fig. 4(A), an operator places the laminate 2, in which the layers have not yet been joined, between the anvil 11 and the probe 12 and shoulder member 13. The operator sets and operates the joining apparatus 1 so that the control device 16 (see Fig. 1) moves the anvil 11, shoulder member 13, and probe 12 via the drive mechanism 14 (see Fig. 1) to perform friction stir spot joining and resistance spot joining.
[0043] 4(B), the anvil 11 presses the first surface 6 of the laminate 2 upward, and the shoulder member 13 presses the second surface 7 of the laminate 2 downward. With the laminate 2 pressed by the anvil 11 and the shoulder member 13, the probe 12 advances from the second surface 7 side toward the laminate 2 while rotating about its axis.
[0044] As shown in FIG. 4(C), the tip of the probe 12 penetrates into the second member 5. The second member 5 is deformed, and an amount equivalent to the portion pushed aside by the probe 12 is received in the recess 25 of the shoulder member 13. In the vicinity of the probe 12, the second member 5 undergoes plastic flow due to frictional heat caused by the rotation of the probe 12, and a flow region having an annular or circular shape as viewed from above is formed. After the tip of the probe 12 reaches the intermediate member 4, the control device 16 (see FIG. 1) applies a current between the probe 12 and the anvil 11. The position of the tip of the probe 12 is managed by the insertion depth of the probe 12, the plunge pressure (plunging load) of the probe 12 into the laminate 2, the rotation load of the probe 12, or the like.
[0045] As shown in FIG. 4(D), while a current flows between the probe 12 and the anvil 11, the probe 12 moves further downward while rotating, and the tip of the probe 12 penetrates the intermediate member 4. When a current flows between the probe 12 and the anvil 11, a molten part 34 is formed in the first member 3 and the intermediate member 4 by resistance heating of the first member 3 and the intermediate member 4 and frictional heat due to the rotation of the probe 12. In addition, in the vicinity of the probe 12, not only the second member 5 but also the intermediate member 4 undergoes plastic flow. Therefore, the part of the intermediate member 4 pushed aside by the probe 12 penetrates toward the second member 5 along the side of the probe 12. At this time, the temperature decreases and the fluidity decreases as the intermediate member 4 moves away from the probe 12, so that the part of the intermediate member 4 that penetrates into the second member 5 is pushed outward in the radial direction. Therefore, in the vicinity of the probe 12 of the intermediate member 4, a hook 35 is formed that extends outward in the radial direction toward the upper end.
[0046] As shown in Fig. 4(E), the control device 16 (see Fig. 1) stops the current flow between the probe 12 and the anvil 11, and the probe 12 retracts along the axis while rotating. Furthermore, the anvil 11 and the shoulder member 13 stop applying pressure to the laminate 2 and move away from the laminate 2. When the current is stopped and the probe 12 moves away, the molten part 34 (see Fig. 4(D)) solidifies to form a nugget 33, and the first member 3 and the intermediate member 4 are joined together. Furthermore, a hook 35 is formed by the second member 5 and the intermediate member 4 that have been plastically flowed by the rotation of the probe 12, and therefore the second member 5 and the intermediate member 4 are joined together.
[0047] The effects of the first embodiment will be described.
[0048] Since the anvil 11 and the probe 12 used for friction stir welding also serve as electrodes for resistance spot welding, the size and number of devices and the length of the production line can be suppressed, and capital investment can be suppressed, compared to the case where separate friction stir welding devices and resistance spot welding devices are prepared. Also, since friction stir welding and resistance spot welding can be performed simultaneously, an increase in processing time can be suppressed.
[0049] If dissimilar materials were resistance welded, brittle intermetallic compounds would be generated, which could reduce the joint strength. In this embodiment, the second member 5 and the intermediate member 4, which are dissimilar materials, are joined by friction stir welding, which can prevent the joint strength from being reduced by intermetallic compounds.
[0050] Not only the resistance heat generated by the current flow but also the frictional heat caused by the rotation of the probe 12 contributes to the melting of the first member 3 and the intermediate member 4, so that it is possible to reduce the amount of energy consumed for resistance welding. Furthermore, while the toughness of the nugget 33 decreases when the molten portion 34 is rapidly cooled, in this embodiment, after the current flow is stopped, the probe 12 is pulled out from the laminate 2 while being rotated, so that the frictional heat caused by the rotation of the probe 12 is transmitted to the molten portion 34, the molten portion 34 is prevented from being rapidly cooled, and the toughness of the nugget 33 is prevented from being reduced.
[0051] 2(A) or 2(B), in the modified example including the probe insulating portion 43 or the shoulder member insulating portion 46, the passage of electricity to the shoulder member 13 is suppressed or prevented, and the current path is limited. As a result, almost no current flows inside the second member 5, melting of the second member 5 is prevented, and the joining quality can be stabilized and improved. In addition, the electrical safety of the equipment can be improved.
[0052] 5 shows a joining device 51 according to the second embodiment. The same components as those in the first embodiment are denoted by the same reference numerals, and the description thereof will be omitted. The joining device 51 according to the second embodiment includes an anvil 11, a rotor 53 including a probe 52, a drive mechanism 54 including an anvil drive mechanism 27, a rotation drive mechanism 28, and an advance / retract drive mechanism 29, and a control device 16 that controls the operation of the advance / retract drive mechanism 29 and the power source 15.
[0053] The rotor 53 rotates around the axis as a whole. The rotor 53 includes a body 55 having a generally cylindrical shape centered on the axis, and a probe 52 extending downward along the axis from the lower surface of the body 55. The rotor 53 is conductive. The probe 52 preferably has a thread groove on its outer circumferential surface. The lower surface of the body 55 forms a shoulder 56 that is recessed upward from the radial outer edge toward the central portion from which the probe 52 extends. The probe 52 is made of, for example, a copper alloy (chromium copper, alumina-dispersed copper, tungsten copper alloy, etc.), conductive ceramic, or cemented carbide.
[0054] The method of joining the layers of the laminate 2 together using the joining device 51 according to the second embodiment is similar to that of the first embodiment, except that the shoulder member 13 (see FIG. 1) is not used. The concave shoulder 56 of the rotor 53 receives a part of the second member 5 pushed out by the insertion of the probe 52, similar to the concave portion 25 (see FIG. 1) of the shoulder member 13 in the first embodiment.
[0055] Although the description of the specific embodiment is finished above, the present invention is not limited to the above embodiment and modified examples, and can be modified in a wide range of ways. The second member and the intermediate member may be joined by resistance welding other than spot welding. The insulating portion shown in Fig. 3(A) and / or (B) may be applied to the modified example in which the shoulder member shown in Fig. 4(B) is applied. The current may flow from the anvil to the probe. [Explanation of symbols]
[0056] 1,51:Joining equipment 2: Laminate 3: First member 4: Intermediate parts 5: Second member 6: 1st page 7:Second side 11: Anvil 12,41,52: Probe 13, 13a, 44: Shoulder member 14,54: Drive mechanism 15: Power supply 16: Control device 20:Through hole 24: Shoulder contact surface 25: Recess 42: Probe conductive part 43: Probe insulation part 46: Shoulder member insulation part
Claims
1. A joining device for joining each member to each other in a laminate including a first member, an intermediate member, and a second member stacked in this order, each of which is electrically conductive and extends along a predetermined main surface, comprising: an anvil having at least a portion thereof being conductive, for supporting a first surface of the laminate that is a surface on the first member side; a probe that is at least partially conductive, the probe being rotatable about an axis extending in a direction intersecting the main surface and movable toward and away from the second member along the axis so as to face a second surface that forms a surface of the laminate on the second member side at a position corresponding to the anvil; a drive mechanism for rotating the probe about the axis and moving the probe forward and backward along the axis; a power source electrically connected to the anvil and the probe to pass an electrical current between the anvil and the probe through the stack; A control device that controls the operation of the drive mechanism and the power source; Equipped with A joining device for resistance welding the first member and the intermediate member to each other and friction stir welding the second member and the intermediate member to each other by rotating the probe and advancing the probe into the stack from the side of the second surface until the tip of the probe penetrates the intermediate member, and after the tip of the probe reaches the intermediate member, passing an electric current between the probe and the anvil through the pressurized stack.
2. 2. The joining apparatus according to claim 1, further comprising a shoulder member including a through hole through which the probe is inserted, a shoulder abutment surface to be pressed against the second surface, and a recess that is recessed relative to the shoulder abutment surface to define a bottom surface to face the second surface and that receives a portion of the probe.
3. the shoulder member is at least partially conductive; 3. The joining device according to claim 2, wherein the probe includes a probe conductive portion extending from a portion to which the power source is electrically connected to a tip that should face the second surface, and a probe insulating portion provided along an outer peripheral surface of the probe conductive portion to insulate between an inner peripheral surface of the through hole and the probe conductive portion.
4. 4. The joining device according to claim 2, wherein the shoulder member is partially conductive and includes a shoulder member insulating portion provided on the shoulder contact surface and an inner circumferential surface of the through hole.
5. The friction stir welding is friction stir spot welding, The joining device according to any one of claims 2 to 4, wherein the shoulder contact surface forms an annular shape with the probe as a center.
6. The friction stir welding is friction stir line welding, The bonding device according to any one of claims 2 to 4, wherein the recessed portion opens rearward in a direction of travel along the main surface of the probe.
7. A joining method for a laminate including a first member, an intermediate member, and a second member, each of which is electrically conductive and extends along a predetermined main surface, stacked in that order, the method comprising: using a joining device to resistance weld the first member and the intermediate member to each other, and friction stir weld the second member and the intermediate member to each other, The joining device includes: an anvil having at least a portion thereof being conductive, for supporting a first surface of the laminate that is a surface on the first member side; a probe that is at least partially conductive, the probe being rotatable about an axis extending in a direction intersecting the main surface and movable toward and away from the second member along the axis so as to face a second surface that forms a surface of the laminate on the second member side at a position corresponding to the anvil; a drive mechanism for rotating the probe about the axis and moving the probe forward and backward along the axis; a power source electrically connected to the anvil and the probe to pass an electrical current between the anvil and the probe through the stack; A control device that controls the operation of the drive mechanism and the power source; Equipped with The bonding method includes: supporting the first surface of the laminate on the anvil; activating the drive mechanism to cause the probe to enter the laminate from the second surface while rotating the probe about the axis; after the tip of the probe reaches the intermediate member, a current is caused to flow between the probe and the anvil by the power source to resistance weld the first member and the intermediate member together; withdrawing the probe from the stack; Equipped with the first member and the intermediate member are made of the same material and are made of a different material from the second member; A joining method, wherein materials of the first member and the intermediate member have higher strength and higher electrical resistance than a material of the second member.
8. The joining method according to claim 7 , wherein the resistance welding step and the withdrawing step are performed while rotating the probe about the axis.
Citation Information
Patent Citations
Structure and method for joining different kinds of materials
JP2005081375A
Structure and method for joining dissimilar material
JP2005111489A
Joining method
JP2007237253A
Friction stir welding apparatus, and friction stir welding method
JP2011083805A
Design of sandwich structures including a polymeric / electrically non-conducting core for weldability
US20160200074A1