Assemblies, components and methods for creating a flame or explosion resistant barrier
A polymer-based barrier member with a tapered edge and internal channel forms an interference fit, addressing uneven formation and stress issues to create reliable explosion and flame barriers compliant with Ex d and Ex e standards.
Patent Information
- Application Number
- JP2022549502
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-02-18
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2040-02-18
AI Technical Summary
Existing methods for creating explosion and flame barriers fail to consistently meet Ex d and Ex e standards due to uneven formation, material incompatibilities, and stress-induced asymmetrical expansion, leading to potential failure under pressure.
A barrier member composed of a polymer material with a tapered peripheral edge and internal channel, engaged with a conformal aperture, is pressed to form an interference fit, distributing pressure evenly and storing elastic potential energy to maintain compliance with flame and explosion protection standards.
The solution ensures consistent, reliable barriers that meet Ex d and Ex e standards by evenly distributing pressure and accommodating material expansion, preventing failure under varying conditions.
Smart Images

Figure 0007579869000001 
Figure 0007579869000002 
Figure 0007579869000003
Abstract
Description
[Technical field]
[0001] The embodiments described below relate to barriers, and more particularly, to blast protection barriers. [Background technology]
[0002] Creating explosion and / or flame barriers certified to meet Ex d and / or Ex e International Electrotechnical Commission (hereinafter "IEC") standards (hereinafter these barriers are referred to as "standard barriers") presents several challenges, especially when using materials and geometric configurations with different coefficients of thermal expansion (hereinafter "CTE"), malleability or stiffness. To comply with the standards, the gaps between the barriers that allow the passage of gases and the flame path length may be limited to several specific parameters that vary depending on the size and nature of the barrier and the environment to which the barrier will be exposed, in order to be certified.
[0003] Currently, the current state of the art for producing standard barriers, especially when using components made from materials such as stainless steel, aluminum, and C22, has barriers formed by composites, such as epoxies, that change from a liquid to a solid state. The problem with these methods is that the barriers formed are often non-uniform and inconsistent, resulting in failure of the barrier in an explosion scenario. Furthermore, to comply with Ex d and Ex e qualification standards for barriers produced with liquid polymers, the barrier must comply with certain standards before and after aging of the polymer. A standard barrier with a cylindrical joint made with a solid polymer would only require the barrier to meet the standards after aging has occurred, simplifying and speeding up the manufacturing and compliance procedures. Thus, there is a need for methods, components, and / or assemblies that use solid polymers to form standard barriers.
[0004] Existing methods do not allow for the creation of interference fit standard barriers using interference fit members. The interference fit may be, for example, one or more of a press fit and a friction fit. Existing potential barrier members that can be used to create a press fit standard barrier are often manufactured to have a substantially consistent edge around the circumference of the member that can be joined by interference fit inside an aperture that also has a substantially consistent linear edge (e.g., the barrier member). Correspondingly, the receiving aperture is also manufactured to have a relatively consistent linear edge. The way this interference fit can be achieved is by forcing the member into the restricted volume of the aperture, where the member expands to fill any gap between the member and the restrictive aperture. Pressure may be applied from both the top and bottom, or from the top with a flat, fully pressure resistant element to force the volume of the member into the aperture. This method creates significant loads on the top pressing plate and / or the opposing element, which may result in unnecessary pressure being placed on the element with the aperture, for example, the element that is the housing of the vibration sensor, with the aperture. Also, the members accumulate potential energy associated with the compression that can ultimately lead to failure. With respect to the context of creating flame and explosion resistant devices, the resulting barrier cannot effectively contain the combustion gases and therefore cannot qualify as a standard barrier. Part of this may be due to the material of the barrier member moving asymmetrically due to accumulated stresses. Also, these methods require a significant amount of energy to facilitate proper application of pressure, resulting in an unreliable barrier. The barrier member should use less energy in production, making manufacture simpler and more streamlined. Thus, there is a need for a barrier member and / or receiving aperture having a geometry that can improve the elements of the production method and the quality of the resulting standard barrier.
[0005] Creating an interference-fit rated barrier by interference-fitting the outer edge of the barrier member onto the inner edge of the aperture is cumbersome when using existing elements. If the barrier member is made of a material with a relatively high coefficient of friction (e.g., stainless steel or C22) when interacting with a common element of common or similar composition, significant stresses can be generated and can harm the penetrating element penetrating the barrier member. Friction can also cause failure of the barrier that can void the explosion or fire rating of the interference-fit rated barrier and / or the assembly containing the barrier. This can be particularly problematic in the context of flow sensors where ambient conditions such as temperature can change dramatically during operation. Also, barrier members constructed from rigid materials with limited malleability limit the range of operating conditions in which the barrier can operate. Also, when using polymers for interference-fit rated barriers, polymers can have sufficient resistance to extreme temperatures and reactive chemicals. Existing components are not specially constructed for this purpose and may not be easily adapted for the purpose of forming an interference-fit rated barrier. For example, existing polymeric bushings are typically layered with discrete levels and rounded internal channels that are not well suited to receiving penetrating members such as printed circuit boards (hereinafter "PCBs"), etc. Thus, there is a need for members constructed from materials that can facilitate an interference fit standard barrier for a wide range of conditions.
[0006] Standard barriers often have elements that penetrate them, so that the penetrating elements may be avoided or taken into account when creating an interference fit between components. These penetrating elements often have some elements suitable for one side of the standard barrier and other elements suitable for the other side of the standard barrier. In some situations, for example in the housing of flowmeter electronics, a special press block is used as a flat substrate (the end that receives pressure from the press) to form an interference fit seal under pressure from the press. The end of the press block that receives pressure from the press is flat, but the other end often has a recess to receive the component of the penetrating element that protrudes from the standard barrier after pressing, the recess being provided such that pressure is not significantly received by the protruding, often relatively weak penetrating element. This allows the protruding element to remain relatively intact when pressure is applied through the other end of the block to form the interference fit barrier from compression. The side of the press block with the recess exerts a higher pressure on the bushing being pressed by the press block due to the recess (due to the lower contact surface area). Additionally, because recesses are often asymmetric in relevant dimensions, pressure may be applied unevenly at the location of the recess. This asymmetric distribution of pressure can cause an uneven barrier and lead to failure of the barrier in the electronics housing due to fire and / or explosion. Thus, there is a need for pre-press assemblies, components, and / or methods for evenly distributing this pressure.
[0007] An effective solution has not been discovered for creating an interference fit rated barrier with a piercing element in a device (e.g., a vibration sensor transmitter, a housing for a vibration sensor transmitter, a vibration sensor, or a housing for a vibration sensor) that is primarily constructed from a rigid material such as stainless steel. Thus, there is a need for an assembly, component, and / or method that uses a rigid or hard material such as stainless steel as part of an interference fit rated barrier with a piercing element. Summary of the Invention
[0008] One embodiment of a barrier member (102) for use in forming an assembly (100, 200) having an interference fit standard barrier (199) is disclosed. The barrier member (102) comprises a first side (120), a second side (122), and a periphery (124) between the first side (120) and the second side (122), the periphery (124) being at least partially inclined at an angle (128) relative to a barrier reference line (130) that is perpendicular to both at least a portion of the first side (120) and at least a portion of the second side (122), the angle (128) decreasing from the first side (120) to the second side (122). The barrier member (102) may further have an internal channel (126) extending through a member depth (123) of the barrier member (102), the member depth (123) being between the first side (120) and the second side (122), the internal channel (126) having a length greater than its width at the surface of the first side (120) and at the surface of the second side (122), and the barrier member (102) being at least partially composed of a polymer.
[0009] One embodiment of an assembly (100, 200) is disclosed. The assembly (100, 200) comprises a barrier member (102) comprising a first side (120), a second side (122), a periphery (124) between the first side (120) and the second side (122), and an interior channel (126) extending through a member depth (123) of the barrier member (102), the member depth (123) being between the first side (120) and the second side (122). The assembly (100, 200) comprises an element having an aperture (104), the aperture (104) comprising a first opening (160), a second opening (162), and a conformal inner periphery (150) between the first opening (160) and the second opening (162), a barrier member (102) at least partially engaged with the aperture (104), the barrier member (102) having a periphery (124) at least partially interfacing with the conformal inner periphery (150). a first surface (122) of the barrier member (102) that is at least partially constructed from a material that is more malleable than a material from which the element having the aperture (104) is constructed, a second surface (122) of the barrier member (102) that is located within the aperture (104), and the assembly (100, 200) is a pre-press assembly (200) that can be pressed to form an interference fit standard barrier (199).
[0010] One embodiment of an assembly (100, 200) is disclosed. The assembly (100, 200) comprises an interference fit standard barrier (199) comprising a barrier member (102) having a first surface (120), a second surface (122), and a perimeter (124). The interference fit rated barrier (199) comprises an element having an aperture (104), the element being constructed from a material that is less malleable than a material from which the barrier member (102) is constructed, the aperture (104) having a conformal inner periphery (150) where at least a portion of the conformal inner periphery (150) fits over at least a portion of the periphery (124), the barrier member (102) exerting pressure against the aperture (104) and storing elastic potential energy that maintains the interference fit rated barrier (199), the interference fit rated barrier (199) complying with one or more of a flame barrier standard and an explosion barrier standard.
[0011] One embodiment of a method for making an assembly (100, 200) having an interference fit standard barrier (199) is disclosed. The method includes the steps of engaging a barrier member (102) having a periphery (124) with an aperture (104) having a conformal inner periphery (150), such that when the barrier member (102) engages the aperture (104), at least a portion of the periphery (124) conforms to at least a portion of the conformal inner periphery (150) and the barrier member (102) is at least partially, but not entirely, within the aperture (104); and applying pressure to the barrier member (102). and applying a pressure to form an interference fit compliant barrier (199) with the aperture (104), wherein elastic potential energy from the applied pressure is stored in the barrier member (102), the elastic potential energy causing application of a force by at least a portion of the perimeter (124) to at least a portion of the conformal inner perimeter (150), said interference fit compliant barrier (199) complying with one or more of a flame barrier standard and an explosion barrier standard.
[0012] [Aspects] According to one aspect, a barrier member (102) is disclosed for use in forming an assembly (100, 200) having an interference fit standard barrier (199). The barrier member (102) comprises a first side (120), a second side (122), and a periphery (124) between the first side (120) and the second side (122), the periphery (124) being at least partially inclined at an angle (128) relative to a barrier reference line (130) that is perpendicular to both at least a portion of the first side (120) and at least a portion of the second side (122), the angle (128) decreasing from the first side (120) to the second side (122). The barrier member (102) may further have an internal channel (126) extending through a member depth (123) of the barrier member (102), the member depth (123) being between the first side (120) and the second side (122), the internal channel (126) having a length greater than its width at the surface of the first side (120) and at the surface of the second side (122), and the barrier member (102) being at least partially composed of a polymer.
[0013] According to one aspect, an assembly (100, 200) is disclosed. The assembly (100, 200) comprises a barrier member (102) comprising a first side (120), a second side (122), a periphery (124) between the first side (120) and the second side (122), and an interior channel (126) extending through a member depth (123) of the barrier member (102), the member depth (123) being between the first side (120) and the second side (122). The assembly (100, 200) comprises an element having an aperture (104), the aperture (104) comprising a first opening (160), a second opening (162), and a conformal inner periphery (150) between the first opening (160) and the second opening (162), a barrier member (102) at least partially engaged with the aperture (104), the barrier member (102) having a periphery (124) at least partially interfacing with the conformal inner periphery (150). a first surface (122) of the barrier member (102) that is at least partially constructed from a material that is more malleable than a material from which the element having the aperture (104) is constructed, a second surface (122) of the barrier member (102) that is located within the aperture (104), and the assembly (100, 200) is a pre-press assembly (200) that can be pressed to form an interference fit standard barrier (199).
[0014] Preferably, the member depth (123) is less than the aperture depth (164) between the first opening (160) and the second opening (162).
[0015] Preferably, the surface area of the first surface (120) is greater than the total surface area of the second surface (122), the first opening (160) and the second opening (162), and the surface area of the second surface (122) is less than the surface area of the first opening (160) but the surface area of the second surface (122) is greater than the surface area of the second opening (162).
[0016] Preferably, the assembly (100, 200) further comprises a piercing element (106) that penetrates the internal channel (126) and thereby engages the internal channel (126), the piercing element (106) having a portion on each side of the barrier member (102) when the piercing element (106) engages the barrier member (102).
[0017] Preferably, the assembly (100, 200) further comprises a pressure distribution element (108), a surface of the pressure distribution element (108) that engages with the first surface (120) of the barrier member (102), the pressure distribution element (108) having a slot (182) extending from a surface of the pressure distribution element (108) to an opposite surface of the pressure distribution element (108), the slot (182) coinciding with the internal channel (126) when the pressure distribution element (108) engages with the barrier member (102), such that a passage exists through both the barrier member (102) and the pressure distribution element (108).
[0018] Preferably, the assembly (100, 200) further comprises a press block (220), the press block (220) having at least one surface that engages with one or more of at least a portion of the piercing element (106), at least a portion of the pressure distribution element (108), and at least a portion of the barrier member (102).
[0019] Preferably, the press block (220) has at least one recess, and the press block (220) at least partially engages the piercing element (106) within the at least one recess.
[0020] Preferably, the barrier member (102) engages the aperture (104) such that the barrier member (102) cannot be forced further into the aperture (104) without deforming the barrier member (102).
[0021] Preferably, the element having the aperture (104) has a first surface (152) about the first opening (160) of the aperture (104), the first surface (152) having alignment elements (222) for aligning one or more engaged elements.
[0022] Preferably, the alignment element (222) comprises a hole in the first surface (152) and a separably connectable alignment pin (224) separably connectable to the hole in the first surface (152), and one or more of the press block (220) and the pressure distribution element (108) have a hole for receiving the alignment pin (224), and the hole for receiving the alignment pin (224) is for aligning one or more engaged elements.
[0023] According to one aspect, an assembly (100, 200) is disclosed. The assembly (100, 200) comprises an interference fit standard barrier (199) comprising a barrier member (102) having a first surface (120), a second surface (122), and a perimeter (124). The interference fit rated barrier (199) comprises an element having an aperture (104), the element being constructed from a material that is less malleable than a material from which the barrier member (102) is constructed, the aperture (104) having a conformal inner periphery (150) where at least a portion of the conformal inner periphery (150) fits over at least a portion of the periphery (124), the barrier member (102) exerting pressure against the aperture (104) and storing elastic potential energy that maintains the interference fit rated barrier (199), the interference fit rated barrier (199) complying with one or more of a flame barrier standard and an explosion barrier standard.
[0024] Preferably, the stored elastic potential energy is sufficient to maintain compliance of the interference fit standard barrier (199) with one or more of a flame barrier standard and an explosion barrier standard over at least one predetermined range of at least one operating condition.
[0025] Preferably, any gap between the barrier member (102) and the aperture (104) in an interference fit standard barrier (199) is less than 5 thousandths of an inch.
[0026] Preferably, the assembly (100, 200) further comprises a piercing element (106) that pierces the interference fit standard barrier (199) by penetrating at least the interior channel (126) of the barrier member (102), and any gap between the piercing element (106) and the interior channel (126) is less than 5 thousandths of an inch.
[0027] Preferably, the assembly (100, 200) further comprises a pressure distribution element (108) that is coupled by a coupling element (180) that is coupled to the first surface (152) surrounding the first side (197) of the aperture (104).
[0028] Preferably, the barrier member (102) has a portion that flows cold over one or more of the first opening (160) and the second opening (162) of the aperture (104).
[0029] Preferably, the periphery (124) is at an angle (128) relative to the barrier reference line (130) and the conformal inner periphery (150) is at a complementary angle (158) relative to the aperture reference line (156), the aperture reference line (156) and the barrier reference line (130) being coincident, and both the angle (128) and the complementary angle (158) being less than 5 degrees in magnitude.
[0030] According to one aspect, a method for making an assembly (100, 200) having an interference fit standard barrier (199) is disclosed. The method includes the steps of engaging a barrier member (102) having a periphery (124) with an aperture (104) having a conformal inner periphery (150), such that when the barrier member (102) engages the aperture (104), at least a portion of the periphery (124) conforms to at least a portion of the conformal inner periphery (150) and the barrier member (102) is at least partially, but not entirely, within the aperture (104); and applying pressure to the barrier member (102). and applying a pressure to form an interference fit compliant barrier (199) with the aperture (104), wherein elastic potential energy from the applied pressure is stored in the barrier member (102), the elastic potential energy causing application of a force by at least a portion of the perimeter (124) to at least a portion of the conformal inner perimeter (150), said interference fit compliant barrier (199) complying with one or more of a flame barrier standard and an explosion barrier standard.
[0031] Preferably, the applied pressure stores a sufficient amount of elastic potential energy in the barrier member (102) such that the interference fit compliant barrier (199) maintains compliance with one or more of the flame barrier standard and the explosion barrier standard over at least one predetermined range of at least one operating condition.
[0032] Preferably, the applied pressure is no more than 3000 pounds that is distributed primarily through the pressure distribution element (108).
[0033] Preferably, the pressure applied is sufficient so that any gaps present in the interference fit rated barrier (199) have a gap depth of less than two thousandths of an inch.
[0034] Preferably, the step of applying pressure to the barrier member (102) includes applying pressure via a pressure distribution element (108), the surface of the pressure distribution element (108) pressing against the barrier member (102) being substantially flat to enable application of a substantially uniform pressure to the barrier member (102). Preferably, the method further comprises the step of engaging the piercing element (106) with an internal channel (126) of the barrier member (102), the internal channel (126) extending through the first surface (120), the member depth (123), and the second surface (122), wherein engaging the piercing element (106) with the internal channel (126) comprises passing the piercing element (106) through the internal channel (126) such that a portion of the piercing element (106) is located on one side of the barrier member (102) and another portion of the piercing element (106) is located on another side of the barrier member (102), and wherein applying pressure to the barrier member (102) causes compression of the internal channel (126) against the piercing element (106), thereby forming a piercing element interference fit, the piercing element interference fit complying with one or more of a flame barrier standard and an explosion barrier standard.
[0035] Preferably, the pressure is applied via a press block (220).
[0036] Preferably, the method further comprises aligning the parts of the assembly (100, 200) using one or more alignment elements (222).
[0037] Preferably, the step of engaging the barrier member (102) with the aperture (104) is a step of engaging the barrier member (102) with the aperture (104) such that the barrier member (102) cannot be forced further into the aperture (104) without deforming the barrier member (102).
[0038] Preferably, the applied pressure is sufficient to cause at least a portion of the barrier member (102) to flow at low temperature over one or more of the first opening (160) of the aperture (104) and the second opening (162) of the aperture (104).
[0039] Preferably, the method further comprises forming the barrier member (102) by cutting material from a block of material having sufficient material to form more than one barrier member (102).
[0040] Preferably, the method does not include the step of heating the barrier member (102) above the melting temperature of the material that comprises the barrier member (102), the melting temperature being determined at standard temperature and pressure.
[0041] Preferably, the method further comprises the step of aging the interference fit rated barrier (199), the interference fit rated barrier (199) being at least partially comprised of a polymer.
[0042] Preferably, the static coefficient of friction between the material from which the periphery (124) is constructed and the material from which the conformal inner periphery (150) is constructed, in a dry and clean condition, at standard temperature and pressure, is less than 0.2.
[0043] Preferably, the barrier member (102) has a volume that is greater than the volume of the aperture (104).
[0044] Preferably, the element having the aperture (104) is a housing for an electrical component (1002), the housing having a terminal side (1097) having at least one terminal (1012) for coupling to a network (1008) and an electronics side (1098) having electronics (1010) for communicating with the device (1004), with a first surface (120) facing the terminal side (1097) and a second surface (122) facing the electronics side (1098).
[0045] Preferably, the barrier member (102) is constructed at least in part from a fluorocarbon.
[0046] Preferably, the fluorocarbon is polytetrafluoroethylene (PTFE).
[0047] Preferably, the second surface (122) has a surface area that is less than the surface area of the first surface (120).
[0048] Preferably, the barrier member (102) is not cylindrical.
[0049] Preferably, the barrier member (102) is shaped as a narrow curved triangle. [Brief description of the drawings]
[0050] Like reference numbers represent like element embodiments in all drawings. It should be understood that the drawings are not necessarily to scale. [Figure 1] A bisecting view of one embodiment of a post press assembly 100 having an interference fit standard barrier 199 is shown. [Figure 2A] 2 shows a perspective view of one embodiment of a pre-press assembly 200 prepared for pressing. [Figure 2B] 2B shows an exploded view of the embodiment of the pre-press assembly 200 presented in FIG. 2A. [Figure 2C] 2 shows a bisected side view of one embodiment of a pre-press assembly 200. [Diagram 3] A perspective view of one embodiment of a barrier member 102 for forming an interference fit standard barrier 199 is shown. [Figure 4] 1 shows a perspective view of one embodiment of a pre-engagement assembly 400 before the barrier member 102 engages with the aperture 104. [Diagram 5] 5 shows a perspective view of one embodiment of a fastening assembly 500 after the pressure distribution element 108 has been bonded to the first surface 152. [Figure 6]6 shows a flow chart of one embodiment of a method 600 for forming a component having an interference fit standard barrier 199. [Figure 7] 7 shows a flow chart of one embodiment of a method 700 for forming a barrier member 102. [Figure 8] 8 shows a flow chart of one embodiment of a method 800 of engaging elements to form a pre-press assembly 200. [Figure 9] 9 illustrates a flow chart of one embodiment of a method 900 for pressing a pre-press assembly 200 to form a post-press assembly 100. [Figure 10] A block diagram of one embodiment of a system 1000 having an interference fit standard barrier 1099 is shown. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0051] 1-10 and the following description depict specific examples to teach those skilled in the art how to make and use the best mode of embodiments of the present invention. For the purpose of teaching the principles of the present invention, some conventional aspects have been simplified or omitted. Those skilled in the art will appreciate variations of these examples that fall within the scope of the present invention. Those skilled in the art will appreciate that the features described below can be combined in various ways to form multiple variations of the present invention. As a result, the embodiments described below are not limited to the specific examples described below, but only by the claims and their equivalents.
[0052] To make a barrier member usable for an interference fit rated barrier, the barrier member can be constructed from a material that has sufficient heat and flame resistance to be qualified. Furthermore, in embodiments where the interference fit rated barrier allows a piercing element to penetrate the barrier, the material of the barrier member must be such that it accommodates the piercing element and protects its integrity. When the barrier member has a piercing element disposed in an internal passage of the barrier member and the barrier member is compressed to form an interference fit barrier within the aperture, the material should have a sufficiently low coefficient of friction over a wide range of conditions to prevent damage to the piercing element during compression. For example, the coefficient of friction of the interaction between the material of which the barrier member is constructed and the material of which the apertured element is constructed when interacting can be below a predetermined threshold value. In one embodiment, the static coefficient of friction for interaction between the material from which the barrier member is constructed and the material from which the apertured element is constructed in a dry and clean condition is less than 0.2 or in the range of between 0.04 and 0.2 (at standard temperature of 273.15 degrees Kelvin and standard pressure of 101.6 kilopascals, hereinafter "STP").
[0053] Additionally, the malleability of the barrier member material must be such that the barrier member can be compressed relatively easily. Also, the ability of the barrier member material to store elastic potential energy must be such that the interference fit rated barrier can be maintained (while complying with the relevant standards) in a variety of conditions. Because polymers have a relatively high coefficient of thermal expansion, barrier members constructed from polymeric materials tend to expand and contract significantly with temperature changes. In applications such as flow meter transmitters, the barrier may be exposed to significantly changing conditions that cause these expansions and contractions. To counteract the expansions and contractions that the polymeric barrier member undergoes due to its environment and / or flow material conditions, the barrier member can store enough elastic potential energy from the original compression that formed the interference fit rated barrier to correspondingly expand (in response to the contraction) and release some of the elastic potential energy, or compress (in response to the expansion) and store additional elastic potential energy. Additionally, in the context of fire and explosion protection, the materials used must be sufficiently resistant to combustion and other reactions, so highly inert polymers are preferred. Some polymers are sufficiently malleable, sufficiently inert, have a sufficiently low coefficient of friction when interacting with conventional materials (such as those used in electronics compartments and / or vibration sensors or transmitters), and have sufficient capacity to store elastic potential energy that is used in the barrier member to form an interference fit compliant barrier by interference fit of the barrier member. One polymer material that has these properties is polytetrafluoroethylene (hereinafter "PTFE").
[0054] A special set of components, manufacturing assemblies, and methods may be useful to create this interference fit rated barrier. For example, to reduce the amount of pressure required to form the interference fit barrier and to create a more uniform and reliable interference fit rated barrier, the outer edge of the barrier member that will engage the aperture by interference fit may be tapered to provide resistance to compression without completely preventing the member from deforming through the aperture (as would be the case if a fully sealed opposing plate were used). The aperture may also have a correspondingly narrower internal taper, with a portion that substantially matches the outer edge taper of the barrier member, to provide an opposing force to the pressure applied to create the interference fit. In this embodiment, the applied pressure may force an elastic deformation of the barrier member, such that a portion of the barrier element fits into a portion of the aperture that would otherwise be too narrow to receive the undeformed barrier member. Deforming the barrier member in this manner relieves some of the elastic forces built up in the barrier member material that may be translated in a direction that causes the interference fit rated barrier to break. Also, by not having a flat opposing member on the side of the barrier opposite to that on which pressure is applied to counteract the force applied to the barrier member, less pressure needs to be applied to cause the desired deformation with the desired level of elastic potential energy (to compensate for the expansion and contraction of the barrier member material), with some of the pressure being converted into deformation of the barrier member to better conform to the narrower inner edge of the aperture in which the interference fit is being formed.
[0055] The barrier can be manufactured using some specialized equipment. For example, a specialized press block can be used to apply pressure resulting in an interference fit rated barrier. The press block can be specifically machined to accommodate the penetrating elements that penetrate the barrier member (and thus the resulting interference fit rated barrier). When pressed to form the interference fit rated barrier, the bond between the penetrating elements is also interference fit to the penetrating elements. If the block simply applied pressure to the penetrating elements, the applied pressure could damage the penetrating elements. By having a press block that accommodates the penetrating elements and applies the majority of the pressing force directly or indirectly to the barrier member, the penetrating elements can be spared harm. Naturally, such press blocks may have recesses to accommodate the penetrating elements. These recesses may cause uneven distribution of compression forces so that the barrier elements are not compressed evenly, causing an unbalanced barrier that is prone to failure. A distribution plate may be placed between the press block and the barrier member to facilitate a more uniform application of pressure to the barrier member, ensuring a more uniform interference fit barrier. This pressure distribution element may also be incorporated as a permanent element of the barrier after compression has taken place, thereby further reinforcing the barrier. This may add an extra layer of security to ensure that the barrier stays in place in the event of a pressure spike (e.g. from a significant explosion).
[0056] To ensure that the elements pressed by the press are correctly aligned, the guide pins can be positioned such that one or more special channels in the press block and pressure distribution element receive the guide pins, resulting in a set alignment that ensures that all elements are in place. If there is a piercing element, there may be a counter assembly on the opposite side to the side where compression is applied, such that the piercing element is positioned by a conformal recess in the counter assembly and press block. The counter assembly may be a removable element such that it is an element of the invention only during application of pressure where the counter assembly forms an interference fit standard barrier.
[0057] FIG. 1 illustrates a bisecting view of an embodiment of a post-press assembly 100 having an interference fit standard barrier 199. In the illustrated embodiment, the post-press assembly 100 may be considered a post-press assembly 100 since it has already been pressed to form the interference fit standard barrier 199. The post-press assembly 100 may include a barrier member 102, an aperture 104, a piercing element 106, a pressure distribution element 108, and a housing 110. The assembly prior to pressing may be referred to as a pre-press assembly 200. FIG. 2A illustrates a perspective view of an embodiment of a pre-press assembly 200 prepared for pressing. FIG. 2B illustrates an exploded view of the embodiment of the pre-press assembly 200 presented in FIG. 2A. FIG. 2C illustrates a bisecting side view of an embodiment of the pre-press assembly 200. In various embodiments, the pre-press assembly 200 can include a barrier member 102, an aperture 104, a piercing element 106, a pressure distribution element 108, and a press block 220. Elements described in connection with Figures 2A, 2B, and 2C having the same reference numbers as in Figure 1 are embodiments of the elements described in connection with Figure 1 prior to pressing. The pre-press assembly 200 and the post-press assembly 100 may be collectively referred to as assemblies 100 and / or 200. In one embodiment, the post-press assembly 100 may be a component of a housing 110 for a transmitter adapted and / or configured to communicate with a flow sensor.
[0058] Various embodiments of the interference fit barrier 199 are contemplated, such as those contained in a transmitter housing or other enclosure having electronic components. The postpress assembly 100 may have an interference fit barrier 199 that conforms to one or more of the standards of a recognized standards setting organization trusted by those skilled in the art, such as the IEC "Ex d" and "Ex e" standards. The Ex d standard is a "flame protection standard." The Ex e standard is an "explosion protection standard" with "improved safety." The IEC has separate sets of requirements for both the Ex d and Ex e standards. These standards are merely exemplary. Other standards in the industry for the interference fit barrier 199 are contemplated. The interference fit barrier 199 may be formed by an interference fit between the barrier member 102 and one or more of the aperture 104 and the piercing element 106. This embodiment of the interference fit barrier 199 may be referred to as the interference fit barrier 199. The interference fit rated barrier 199 may be such that it meets the IEC requirements of Ex e and Ex d standards for gaps between elements and flame path length. For example, the gap may have a gap depth less than a predetermined gap depth. In one embodiment, the gap may have a gap depth less than one of 5 thousandths of an inch and 2 thousandths of an inch. In one embodiment, the interference fit rated barrier 199 may have a flame path less than a predetermined threshold.
[0059] In one embodiment, the interference fit standard barrier 199 may have a first side 197 and a second side 198. In one embodiment, the first side 197 is a terminal side (e.g., terminal side 1097 of FIG. 10) having electronic communication elements that communicate with a first system, possibly a network (e.g., network 1008 of FIG. 10). In one embodiment, the second side 198 is an electronics side (e.g., electronics side 1098 of FIG. 10) having electronic components that can one or more of: store data, receive data, transmit data, process data, interpret data, display data, etc. In one embodiment, the electronics side (e.g., electronics side 1098 of FIG. 10) may have electronics that communicate with a vibration sensor. In one embodiment, the shape of one or more of the barrier member 102 and the aperture 104 may be defined by components installed on the electronics side (e.g., electronics side 1098 of FIG. 10). One embodiment of a system 1000 having a terminal side 1097 and an electronics side 1098 of an interference fit standard barrier 199 is shown in FIG.
[0060] The embodiments presented herein illustrate various arrangements of the elements of the interference fit standard barrier 199 in the context of the post-press assembly 100 and the pre-press assembly 200. In this application, the post-press assembly 100 and the pre-press assembly 200 are described within one embodiment of a flow sensor transmitter in communication with an external network, but this embodiment is not intended to be limiting. Those skilled in the art will readily appreciate that the post-press assembly 100 and the pre-press assembly 200 may also be used in other applications.
[0061] The barrier member 102 is an element that deforms under pressure to create an interference fit and form the interference fit rated barrier 199. The barrier member 102 may be pressed, for example using a press, to deform the barrier member 102 to conform to one or more of the apertures 104 and piercing elements 106 to form the interference fit rated barrier 199. The pressure may be applied in a pressure direction 196, possibly from a first side 197 to a second side 198. The barrier member 102 may have a first face 120, a second face 122, and a perimeter 124. In one embodiment, the first face 120 and the second face 122 are on opposite sides of the barrier member 102, and the perimeter 124 is between the first face 120 and the second face 122. In one embodiment, the first surface 120 and / or the second surface 122 may be substantially flat and may have substantially parallel surfaces, and the thickness of the barrier member 102 therebetween is relatively constant (at least prior to pressing).
[0062] In one embodiment, the periphery 124 may be tapered (before and / or after pressing) such that the barrier member 102 has a larger volume near the first surface 120 than near the second surface 122. In one embodiment, this may mean that the first surface 120 has a larger surface area than the second surface 122. In one embodiment, the taper along the periphery 124 is a substantially flat edge at an angle 128. In one embodiment, the angle 128 is less than 5 degrees in magnitude when measured from a barrier reference line 130 drawn from the first surface 120 to the second surface 122, the barrier reference line 128 being perpendicular to both the first surface 120 and the second surface 122. In another embodiment, the angle 128 is less than 2 degrees in magnitude relative to the same barrier reference line 130. It should be understood that positive and negative angles are only relative to a reference and are therefore given in magnitude here. The periphery 124 may be such that it is configured to partially match an internal conformal portion of the aperture 104. In one embodiment, the perimeter 124 is shaped to at least partially fit within a conformal portion of the interior of the aperture 104. It should be appreciated that the perimeter 124 may be flat, sloped, curved, have one or more of flat portions, sloped portions, curved portions, etc. In a different embodiment, the perimeter 124 may be flat and perpendicular to both the first surface 120 and the second surface 122.
[0063] In one embodiment, the overall shape of the barrier member 102 may be defined by the space occupied by other components in the assembly. In one embodiment, the shape of the barrier member 102 may not be cylindrical. In one embodiment, the shapes of the first face 120 and the second face 122 may not be circular and may be the same or different. For example, the shapes of the first face 120 and the second face 122 may be triangular, possibly with rounded corners. This may be described as a curved triangle for purposes of this specification. The volume and cross-section of the barrier member 102 may narrow from the first face 120 to the second face 122, such that the resulting three-dimensional shape of the barrier member 102 may be characterized as a narrow curved triangle. In one embodiment, the barrier member 102 may have a bulge. This bulge may be used to close the aperture 104 with extra space to accommodate a connector for the piercing element 106. In one embodiment, the periphery 124 may be uniform between the first side 120 and the second side 122, such that the overall shape of the barrier member 102 is a consistent shape that narrows at the edge from the first side 120 to the second side 122, for example a narrow curved triangular shape (possibly narrowing from the first side 120 to the second side 122).
[0064] In one embodiment, the barrier member 102 may need to accommodate the piercing element 106. The piercing element 106 may extend through the barrier member 102 and thus the interference fit rated barrier 199. The barrier member 102 may have an internal channel 126 to accommodate the piercing element 106. Prior to pressing to form the interference fit rated barrier 199, the internal channel 126 may have sufficient space to receive the piercing element 106. During compression, this internal channel 126 may be compressed around the piercing element 106 and possibly form an interference fit bond with the piercing element 106. In an alternative embodiment, the penetration is bonded to the interior of the barrier member 102 prior to pressing, such that the internal channel 126 is not needed or is already filled and possibly properly sealed by the piercing element 106.
[0065] In one embodiment, the barrier member 102 may be constructed from a material having desirable properties for making the interference fit standard barrier 199. For example, the material may be one or more of being sufficiently malleable, sufficiently inert, having a sufficiently low coefficient of friction when interacting with conventional materials, resistant to large temperature fluctuations (not too brittle at extremely low temperatures or melting at high temperatures), and having sufficient capacity to store elastic potential energy for use in the interference fit standard barrier 199. For example, the barrier member 102 may be constructed from a material having a predetermined one or more of maximum elasticity, minimum coefficient of friction when interacting with conventional materials, maximum melting point at standard temperature and pressure, minimum fire point, minimum autoignition temperature, minimum inertness, minimum tendency to absorb fluids such as water at a particular operating temperature. These specifications may be in terms of predetermined thresholds. In one embodiment, the barrier member 102 may be constructed from a material having properties selected to maintain a difference relative to the properties of the material of which the aperture 104 is constructed. Alternatively, the barrier member 120 may be constructed from a material selected to have a particular set of properties at a particular set of conditions (e.g., temperature and pressure). For example, the barrier member 102 (and / or periphery 124) may be constructed from one or more of a material that is more malleable, has a lower Young's modulus, and has a high Poisson's ratio than the material from which the aperture 104 (and / or conformal inner periphery 150) is constructed. In one embodiment, the barrier member 102 may be constructed from a polymer, such as a fluorocarbon or fluoropolymer.Examples of fluorocarbons that may be used include PTFE, polyvinyl fluoride (hereinafter, "PVF"), polyvinylidene fluoride (hereinafter, "PVDF"), polychlorotrifluoroethylene (hereinafter, "PCTFE"), polyethylene chlorotrifluoroethylene (hereinafter, "ECTFE"), ethylene tetrafluoroethane (hereinafter, "ETFE"), perfluoromethylalkoxy (hereinafter, "MFA"), perfluoroalkoxyalkane (hereinafter, "PFA"), fluorinated ethylene propylene (hereinafter, "FEP"), perfluorinated elastomer (hereinafter, "FFPM"), chlorotrifluoroethylene vinylidene fluoride (hereinafter, "FPM"), tetrafluoroethylene propylene (hereinafter, "FEPM"), perfluoropolyether (hereinafter, "PFPE"), perfluorosonic acid (hereinafter, "PFSA"), perfluoropolyoxetane, and the like.
[0066] The aperture 104 is an aperture of an element of the assembly 100 or 200 that receives the barrier member 102 to form an interference fit rated barrier 199. The aperture 104 is a hole or channel through a portion of the assembly 100 or 200. In one embodiment, the aperture 104 may be an element of the housing 110. The aperture 104 is configured to be blocked by receiving the barrier member 102 to form the interference fit rated barrier 199. The aperture 104 may be further configured to be large enough to receive a connector for an electronic device that may be provided on the piercing element 106. The aperture 104 may be surrounded by a first surface 152 and a second surface 154. The aperture 104 may have a first opening 160 and a second opening 162. In one embodiment, the first opening 160 has a larger surface area than the second opening 162. In another embodiment, the first opening 160 has the same surface area as the second opening 162.
[0067] In one embodiment, the aperture 104 has a conformal inner perimeter 150. For example, at least a portion of the conformal inner perimeter 150 may be adapted to conform with at least a portion of the perimeter 124 of the barrier member 102, such that when the perimeter 124 of the barrier member 102 engages the conformal inner perimeter 150 of the aperture 104, at least a portion of the barrier member 102 may be placed within the aperture 104 without applying any greater pressure than is necessary for the placement itself.
[0068] In one embodiment, the conformal inner periphery 150 may be flat and perpendicular to the first and second surfaces 152 and 154 around the aperture 104, representing a flat edge. In this embodiment, the periphery 124 of the barrier member 102 may also be flat and perpendicular to its first face 120 and second face 122. In another embodiment, the conformal inner periphery 150 may be inclined relative to the first and second surfaces 152 and 154. For example, the conformal inner periphery 150 may be inclined relative to an aperture reference line 156 drawn from the first surface 152 to the second surface 154, perpendicular to both the first surface 152 and the second surface 154, which line is at a point on the edge of the first surface 152. The conformal inner periphery 150 may have a portion having a complementary angle 158 that matches the angle 128 of the periphery 124 of the barrier member 102. For example, if the perimeter 124 has a portion that has an angle 128 with respect to a line drawn from the first surface 120 to the second surface 122 that is perpendicular to both the first surface 120 and the second surface 122 of the barrier member 102, then the conformal inner perimeter 150 may have a complementary angle 158 (which may be the same as or substantially the same as angle 128) with respect to the barrier reference line 130. In this embodiment, the barrier reference line 130 may be parallel and / or coincident with the aperture reference line 156.
[0069] In the embodiment shown in FIG. 2C, the barrier reference line 130 and the aperture reference line 156 are coincident. The angle 128 and the complementary angle 158 as well as the barrier reference line 130 and the aperture reference line 156 are shown in FIG. 2C in a close-up view 202 of the engagement between the barrier member 102 and the aperture 104 before compression. The close-up view 202 shows a close-up portion of one embodiment of the barrier member 102 engaged with the aperture 104 before compression. In this embodiment, the angle 128 and the complementary angle 158 are the same angle. Also, in this embodiment, the barrier reference line 130 and the aperture reference line 156 are the same and / or coincident. It can also be seen that the first surface 120 has a larger surface area than the second surface 122, the first opening 160 and the second opening 162. The second surface 122 has a smaller surface area than the first opening 160 but a larger surface area than the second opening 162. The second opening 162 may have a smaller surface area than any of the first surface 120, the second surface 122, and the first opening 160. These surface areas may reflect the relative volumes of the elements at the locations where the first surface 120 and the second surface 122 are relative to the first opening 160 and the second opening 162. When the barrier member 102 engages the aperture 104 prior to pressing, a portion of the barrier member 102 may fit into a portion of the aperture 104 without the application of significant pressure. This may be facilitated by portions of the perimeter 124 and conformal inner perimeter 150 having conformal or corresponding portions, possibly with edges at the appropriate or substantially same angle 128 and complementary angle 158. Other conformal arrangements are contemplated, for example, any combination of polygonal or curvilinear surfaces that conform or correspond to one another.
[0070] In one embodiment, prior to pressing, the aperture 104 may have an aperture depth 164 between the first surface 152 and the second surface 154 along the aperture reference line 156 that is greater than a member depth 123 that the barrier member 102 has between the first surface 120 and the second surface 122 along the barrier reference line 130. In various embodiments, prior to pressing to form the interference fit standard barrier 199, one or more relative dimensions of the elements may include a surface area of the first opening 160 may be greater than a surface area of the second surface 122, a surface area of the first opening 160 may be less than a surface area of the first surface 120, a surface area of the second opening 162 may be less than a surface area of the second surface 122, and a surface area of the second opening 162 may be less than a surface area of the first surface 120. The relative dimensions or dimensions may allow the perimeter 124 of the barrier member 102 to at least partially conformally engage with the conformal inner perimeter 150 of the aperture 104 prior to pressing. Upon pressing, the barrier member 102 may be compressed at its perimeter 124, such that the barrier member 102 stretches between its first surface 120 and its second surface 122 during pressing, distorting a greater amount of material to become part of the perimeter 124. This stretching may further allow a greater surface area of the perimeter 124 of the barrier member 102 to engage with a greater surface area of the conformal inner perimeter 150. In some embodiments, during and / or after pressing, the barrier member 102 can overhang one or more of the first opening 160 and second opening 162 of the aperture 104, such that one or more of the first faces 120 can cold flow and overhang around the first surface 152 and the second face 122 can cold flow and overhang around the second surface 154. In this embodiment, after pressing, the aperture 104 may have an aperture depth 164 between the first surface 152 and the second surface 154 along the aperture reference line 156 that is equal to the member depth 123 that the barrier member 102 has between the first surface 120 and the second surface 122 along the barrier reference line 130, or that is either smaller than or larger than the member depth 123.In one embodiment, the aperture 104 may have openings on the second side 198 and / or the first side 197 that allow a portion of the barrier member 102 to flow at a lower temperature under pressure to a location outside the aperture 104. In this embodiment, the barrier member 102 may be of a larger volume than the aperture 104. Embodiments in which the aperture 104 has a larger volume than the barrier member 102 are also contemplated.
[0071] In one embodiment, the first surface 152 may have alignment elements 222 for aligning elements of the pre-press assembly 200 during pressing. For example, the first surface 152 may have holes to receive alignment pins 224, which are configured to provide guidance to certain elements when engaging and pressing the pre-press assembly 200. In one embodiment, the alignment pins 224 may be releasably coupleable. In various embodiments, one or more elements of the assemblies 100 and / or 200 or the press block 220 may have holes to receive these alignment pins 224 to hold the elements of the assemblies 100 and / or 200 and the press block 220 in place. In another embodiment, the alignment elements 222 may also be holes and have threads. In this embodiment, the threads may allow for easy coupling and decoupling of the alignment pins 224. Additionally, in embodiments having a pressure distribution element 108, the pressure distribution element 108 may have a coupling element 180 such that the pressure distribution element 108 may be coupled to the first surface 152 after the pressing to form the interference fit rated barrier 199 has occurred. For example, the pressure distribution element 108 may have holes that allow a screw to be threaded or screwed into the alignment element 222 (here, a hole or threaded hole) of the first surface 152 to couple the pressure distribution element 108 to the first surface 152 after pressing. It should be appreciated that in this embodiment, the pressure distribution element 108 may be used to reinforce the interference fit rated barrier 199 to withstand higher explosion pressures.
[0072] The piercing element 106 is an element that penetrates the interference fit standard barrier 199 from the first side 197 to the second side 198. In one embodiment, the piercing element 106 penetrates the barrier member 102 and possibly the interior channel 126. It should be understood that the piercing element 106 may be pre-coupled, e.g., coupled to the interior channel 126 of the barrier member 102, with elements of the pre-press assembly 200 prior to pressing. In another embodiment, the piercing element 106 may be coupled to the interference fit standard barrier 199 by pressing, possibly causing the piercing to penetrate the interior channel 126 of the barrier member 102, and then pressing the barrier member 102 to cause a pressure fit coupling between the piercing element 106 and one or more of the barrier member 102 and the interior channel 126 of the barrier member 102.
[0073] In one embodiment, the penetrating element 106 may include a PCB. The PCB may be any type of PCB known in the art. In one embodiment, the PCB is formed from wafer layers. In one embodiment, the PCB is formed from wafer layers with a flexible electronics layer sandwiched between rigid layers. The use of flexible layers can reduce stress on the PCB when compression occurs with the penetrating element 106 engaged through the interior channel 126 of the barrier member 102. In one embodiment, the penetrating element 106 may have an electronic coupler on a first side 197 (e.g., terminal side 1097 of FIG. 10) of the interference fit standard barrier 199 for coupling to a first network (e.g., network 1008 of FIG. 10) and electronics on a second side 198 (e.g., electronics side 1098) for performing transmitter operations.
[0074] Also, in one embodiment, when pressing occurs, the applied pressure presses at least a portion of the piercing element 106 from the first side 197 to the second side 198 of the interference fit compliant barrier 199. For example, a portion of a portion of the piercing element 106 (e.g., electronics portion) that would be located on the second side 198 (e.g., electronics side 1098 of FIG. 10 ) prior to pressing may be located on the first side 197 (e.g., terminal side 1097 of FIG. 10 ). This portion of the portion of the piercing element 106 may be suitably pressed to the second side 198 by the pressing action that forms the interference fit compliant barrier 199.
[0075] During assembly, the press block 220 can be used to apply the pressure necessary to create the interference fit standard barrier 199. Pressure may be applied to the press block 220 at its pressure side 226. To reduce potential damage to the piercing element 106, the press block 220 may have recesses that at least partially conform to the shape of the piercing element 106. These recesses may cause uneven pressure to be applied to the barrier member 102 when pressing through the press block 220. This uneven application of pressure may result in a weak interference fit. For example, uneven pressing may cause uneven conversion of stored elastic potential energy, leading to failure of the interference fit standard barrier 199.
[0076] The pressure distribution element 108 is an element that applies a uniform pressure to another element when pressed. For example, in an embodiment in which a press block 220 having a conformal recess is used, the pressure distribution element 108 may be located at an end of the press block 220 opposite the pressure side 226 of the press block 220. In one embodiment, the pressure distribution element 108 is engaged between the press block 220 and the barrier member 102 prior to pressing such that when pressure is applied to the press block 220 to form an interference fit standard barrier 199, pressure may be applied through the pressure distribution element 108, and the pressure distribution element 108 applies a substantially uniform pressure to the barrier member 102 around a surface of the pressure distribution element 108 that opposes the pressure direction 196 of the press. In one embodiment, the pressure distribution element 108 may be a flat member having substantially parallel flat faces and a relatively narrow width between the faces. In one embodiment, the piercing element 106 may have a coupling element 180, for example, comprising a hole and / or a thread. These coupling elements 180 can be used to couple the pressure distribution element 108 to the post press assembly 100, for example to the first surface 152 surrounding the first side 197 of the aperture 104. In embodiments where the coupling element 180 comprises holes, the holes can be used to receive alignment pins 224 to help align the pressure distribution element 108 during pressing. The pressure distribution element 108 can also have a slot 182, allowing the piercing element 106 to pass through the slot 182. The slot 182 can be at a location on the pressure distribution element 108 where the pressure distribution element 108 aligns with the interior channel 126 of the barrier member 102 when the pressure distribution element 108 is engaged and / or coupled with the barrier member 102, allowing the piercing element 106 to pass straight through both the pressure distribution element 108 and the barrier member 102. The slot 182 may be shaped like a typical slot 182 in that in each cross-section of the piercing element 106 taken along a line perpendicular to the plane of the maximum surface area of the piercing element 106, one dimension is substantially wider than the other dimension.
[0077] The housing 110 is any container that holds electronic components. The housing 110 may be one that requires Ex d and / or Ex e certification. In an embodiment, the housing 110 may be a housing 110 or case for one of a flow sensor, a transmitter configured and / or adapted to communicate with a flow sensor, any other electronics containing device, etc. The housing 110 may be one that, when in use, resides in an environment with flammable and / or explosive gases. The housing 110 has an interference fit rated barrier 199 to ensure that any explosion / fire caused by a spark in the electronic circuitry within the housing 110 escapes the housing 110, and cools the flame or explosion within the housing 110 that may possibly spread to an already flammable or explosive environment. In the embodiment shown in FIG. 1, the housing 110 is a housing for a transmitter configured to receive signals from the meter assembly and transmit those signals to an associated network (e.g., network 1008 in FIG. 10). The second side 198 has the electronics used as part of the transmitter. These electronics may include circuitry configured to receive, store, and / or transmit data from the meter assembly to / from terminals on the other side of the interference fit rated barrier 199. In one embodiment, the first side 197 is a terminal side (e.g., terminal side 1097 of FIG. 10) having terminals for transmitting signals between the electronics side (e.g., electronics side 1098 of FIG. 10) and an external network (e.g., network 1008 of FIG. 10). The terminal side is separated from the electronics side by the interference fit rated barrier 199 to prevent transmission of flames / explosions caused by sparks in electronic circuitry on the electronics side that may otherwise escape to the terminal side and possibly then to an environment having sufficient concentrations of flammable or explosive gases to cause a dangerous fire and / or explosion. The penetrating element 106 may be a PCB in this embodiment, with the PCB having one side with the terminal elements and another side with the electronics. The electronics may be disposed on the electronics side of the interference fit compliant barrier 199 and the terminal elements may be disposed on the terminal side of the interference fit compliant barrier 199 .
[0078] Embodiments are contemplated in which one or more of the piercing element 106 and pressure distribution element 108 are not part of one or more of the assemblies 100 and 200. In these embodiments, the steps and portions of the arrangements involving these elements may not be incorporated into the present invention. For example, embodiments are contemplated in which the assemblies 100 and / or 200 do not have the piercing element 106 passing through the interference fit standard barrier 199. Additionally, embodiments are contemplated in which the assemblies 100 and / or 200 do not have the pressure distribution element 108. Embodiments in which neither are elements of the assemblies 100 and / or 200 are also contemplated.
[0079] After compression, the spacing between the elements forming the interference-fit barrier 199 may be limited to prevent a fire or explosion on one side of the interference-fit barrier 199 from reaching the other side of the interference-fit barrier 199. It should be understood that the interference-fit barrier 199 does not need to be an airtight seal. Some gas exchange may be permitted through the interference-fit barrier 199. To ensure that gas flow is restricted, the space between one or more elements forming the interference-fit barrier 199 may be limited to a predetermined threshold, for example, less than 2 / 1000 of an inch, less than 3 / 1000 of an inch, or less than 5 / 1000 of an inch. In one embodiment, any space between the barrier member 102 and the aperture 104 may be less than a predetermined threshold. In one embodiment, any space between the perimeter 124 and the conformal inner perimeter 150 is less than a predetermined threshold. In one embodiment, any space between the piercing element 106 and the barrier member 102 is less than a predetermined threshold. In one embodiment, any space between the piercing element 106 and the interior channel 126 of the barrier member 102 is less than a predetermined threshold.
[0080] As can be seen in FIGS. 2A and 2B, which show an embodiment of the pre-press assembly 200 before pressing, the side of the press block 220 opposite its pressure side 226 can engage one or more of the pressure distribution element 108 and the piercing element 106. When the press block 220 at least partially engages the piercing element 106, the press block 220 may have a recess (not shown) that receives at least a portion of the piercing element 106. In some embodiments, when the press block 220 is pressed with the piercing element 106 partially engaged in the recess of the press block 220, a portion of the piercing element 106 may be intentionally bent to conform to the resulting desired shape. This bending can better accommodate certain connectors for electronic components. In one embodiment, the press block 220 may have an internal channel for receiving an alignment element 222, e.g., an alignment pin 224 coupled to a corresponding hole in the first surface 152.
[0081] The pressure distribution element 108 may receive a non-uniformly distributed pressure from the press block 220 on the pressure-applied side of the pressure distribution element 108. The pressure distribution element 108 may have a substantially uniform and / or flat opposite side (opposite the side on which pressure is applied by the press block 220) that applies a uniform pressure to an opposite side element, e.g., the barrier member 102. In one embodiment, the pressure distribution element 108 may have holes for receiving alignment elements 222, e.g., alignment pins 224 coupled to corresponding holes in the first surface 152. In this embodiment, the holes (and possibly additional holes) in the pressure distribution element 108 may be used to couple the pressure distribution element 108 to the first side 197 of the interference fit standard barrier 199 and possibly reinforce the interference fit standard barrier 199. In this embodiment, the pressure distribution element 108 may abut against the first surface 120 of the barrier member 102. In an alternative embodiment where a pressure distribution element 108 is not used, the press block 220 may directly engage and press against the barrier member 102 .
[0082] The barrier member 102 may engage one or more of the press block 220 and the pressure distribution element 108 on the first surface 120. The barrier member 102 may engage the aperture 104, possibly at a periphery 124 of the barrier member 102. The pre-press assembly 200 may engage the periphery 124 of the barrier member 102 with an interior portion of the aperture 104, such as a conformal interior periphery 150.
[0083] Prior to pressing, the barrier member 102 may only partially engage with the aperture 104. For example, in one embodiment, prior to pressing, only a portion of the perimeter 124 engages and / or fits with the conformal inner perimeter 150. Prior to pressing, the perimeter 124 and the conformal inner perimeter 150 may be at least partially conformal, they are angled and / or complementary to one another, and / or conformal, in some cases, the perimeter 124 has an angle 128 and the conformal inner perimeter 150 has a complementary angle 158. For example, in one embodiment, the angle 128 and the complementary angle 158 may be negative of one another with respect to a particular reference, e.g., one or more of the barrier reference line 130 and the aperture reference line 156. It should be understood that the angle 128 and the complementary angle 158 may be exaggerated in the drawings for illustrative purposes. In embodiments where only a portion of the periphery 124 conforms to the conformal inner periphery 150 prior to pressing, the pressing deforms the inner periphery 124 together with the remainder of the barrier member 102, and the resulting deformed periphery 124 may share a greater complementary and / or conformal surface area between the periphery 124 and the conformal inner periphery 150 than prior to pressing, which may contribute to the formation of a tight fit standard barrier 199.
[0084] The aperture 104 may be an element of a rigid structure, such as the housing 110, which provides a substrate for providing a counter pressure that can be translated through the aperture 104, and possibly through the conformal inner periphery 150, to counter pressure applied to the first surface 120 of the barrier member 102.
[0085] In one embodiment, the arrangement of elements of the pre-press assembly 200 may be, in order from the first side 197 to the second side 198 (pressure direction 196), the press block 220, the pressure distribution element 108, the barrier member 102, and the aperture 104. It should be understood that the barrier member 102 may be partially conformal and engaged with a portion of the interior of the aperture 104 such that a portion of the barrier member 102 and the aperture 104 overlap in the direction from the first side 197 to the second side 198 (and / or pressure direction 196). Also, the piercing element 106 may be disposed within some elements, for example, one or more of the recess of the press block 220, the slot 182 of the pressure distribution element 108, the interior channel 126 of the barrier member 102, and the piercing portion of the aperture 104. The piercing element 106 may have an end at an axis defined by a pressure direction 196 defined from a first side 197 to a second side 198, e.g., an end that is partially located in a recess in the press block 220, and another end that is located on the second side 198 prior to pressing. In embodiments that do not use a pressure distribution element 108, the order may be the same, except that the pressure distribution element 108 is not included.
[0086] FIG. 3 shows a perspective view of an embodiment of a barrier member 102 for forming an interference fit standard barrier 199. The barrier member 102 presented in FIG. 3 may be an embodiment of the barrier member 102 presented in FIG. 2A and FIG. 2B (before pressing). Special components may be required to generate the interference fit standard barrier 199. Existing components may not be specially configured for this purpose and may not be easily adapted for the purpose of forming the interference fit standard barrier 199. For example, existing polymer bushings are typically layered with significant discontinuities between the discontinuous levels and circular shaped internal channels 126, making them less suitable for receiving and forming an interference fit standard barrier 199 around a penetrating element 106 such as a PCB. Applicant's barrier member 102, prior to pressing, may have one or more attributes that make it better suited for use in creating an interference fit standard barrier 199 and / or an interference fit standard barrier 199 with a penetrating element 106.
[0087] The barrier member 102 may be adapted for such applications by incorporating features already described with respect to the barrier member 102, for example, by having a perimeter 124 that interacts with a conformal inner perimeter 150 of the aperture 104, by a perimeter 124 and a conformal inner perimeter 150 having conformal and / or complementary portions prior to pressing, by having a perimeter 124 having an angle 128, by a first surface 120 having a larger surface area than the second surface 122, by constructing the barrier member 102 from a material having suitable properties (as described herein) for creating an interference fit standard barrier 199, by constructing the barrier member 102 from a material having properties relative to the elements defining the aperture 104 (such as the conformal inner perimeter 150 against which pressure is applied during pressing), by a portion of the first surface 120 having a larger surface area than any cross-section of the aperture 104, etc. This list of features is exemplary, and all of the features described with respect to the embodiments of the barrier member 102 herein are contemplated to improve the barrier member 102 and the manner in which the barrier member 102 is used in an interference fit standard barrier 199.
[0088] Figures 4 and 5 show diagrams of further embodiments of the present invention. The elements indicated by reference numbers in Figures 4 and 5 are embodiments of the elements having similar reference numbers in Figures 1 to 3.
[0089] FIG. 4 illustrates a perspective view of one embodiment of a pre-engagement assembly 400 before the barrier member 102 engages with the aperture 104.
[0090] 5 shows a perspective view of one embodiment of a fastening assembly 500 after the pressure distribution element 108 has been coupled to the first surface 152. In this embodiment, the pressure distribution element 108 is coupled to the fastening assembly 500 using a coupling element 180. A portion of the coupling element 180 may be received by a hole in the first surface 152, with a portion of the hole possibly functioning as a complementary and / or aligned element with the alignment element 222 prior to and during compression.
[0091] [flowchart] 6-9 show a flow chart of an embodiment of a method for engaging elements of the pre-press assembly 200, compressing elements of the pre-press assembly 200, forming the post-press assembly 100, and securing the post-press assembly 100 to form the securing assembly 500. The methods disclosed in the flow charts are not exhaustive, but merely represent potential embodiments of steps and sequences. The methods should be read in the context of the entire specification, including the description of the interference fit standard barrier 199, the description of the press assembly 100, the elements disclosed in the description of the pre-press assembly 200, and / or any of the elements disclosed in FIGS. 1-5. The methods represented by the flow charts and corresponding descriptions should be read in the context of the entire specification, including the elements disclosed in the description of FIGS. 1-5.The following terms are used explicitly or implicitly in the description of the flowcharts and corresponding methods: barrier member 102, aperture 104, piercing element 106, pressure distribution element 108, housing 110, interference fit standard barrier 199, post press assembly 100, pre press assembly 200, first side 197, second side 198, first face 120, second face 122, perimeter 124, interior channel 126, angle 128, barrier reference line 130, member depth 123, conformal interior perimeter 150, first surface 152, second surface 154, aperture reference line 156, complementary angle 158, and the like. 8, first opening 160, second opening 162, aperture depth 164, coupling element 180, slot 182, press block 220, alignment element 222, alignment pin 224, and pressure side 226 are similar to the barrier member 102, aperture 104, piercing element 106, pressure distribution element 108, housing 110, pressure direction 196, interference fit standard barrier 199, post press assembly 100, pre press assembly 200, first side 197, second side 198, first surface 120, second surface 122, periphery 124, internal channel 126, angle 128, burr 129, and the like disclosed in FIGS. datum 130, member depth 123, conformal inner periphery 150, first surface 152, second surface 154, aperture datum 156, complementary angle 158, first opening 160, second opening 162, aperture depth 164, coupling element 180, slot 182, pressure direction 196, press block 220, alignment element 222, alignment pin 224, and pressure side 226 may be embodied in an embodiment, although in alternative embodiments, any suitable barrier member 102, aperture 104, piercing element 106, pressure distribution element 108, housing 110, interference fit standard barrier 199, post 222, or the like may be embodied in an embodiment, such as ... The press assembly 100, pre-press assembly 200, first side 197, second side 198, first surface 120, second surface 122, perimeter 124, interior channel 126, angle 128, barrier reference line 130, member depth 123, conformal interior perimeter 150, first surface 152, second surface 154, aperture reference line 156, complementary angle 158, first opening 160, second opening 162, aperture depth 164, coupling element 180, slot 182, pressure direction 196, press block 220, alignment element 222, alignment pin 224, and pressure side 226 may be utilized.
[0092] FIG. 6 illustrates a flow chart of one embodiment of a method 600 for forming a component having an interference fit standard barrier 199 .
[0093] Step 602 is optionally a step of forming the components of the pre-press assembly 200. This forming step 602 may include forming one or more of the barrier member 102, the aperture 104 (and / or the physical elements that define the aperture 104), and the piercing element 106. Step 602 is optional as long as the parts can be formed before the method 600 begins. If an embodiment of the method 600 incorporates a pressure distribution element 108, the pressure distribution element 108 may also be optionally formed. The components may be formed by any known method, such as extrusion, molding, 3d printing, casting, bonding of sub-elements, any other known method for forming elements, etc. Any of the elements of the pre-press assembly 200 may be formed to have any number of characteristics described herein. With respect to the barrier member 102, the physical properties of the material may be such that traditional forming methods may be cumbersome. In these embodiments, the barrier member 102 may be formed by cutting material from a larger block, and then forming a plurality of barrier members 102 that can be cut or otherwise removed from the larger block. This may be advantageous for the barrier member 102 to be constructed from a material that has a low coefficient of friction when interacting with conventional materials in the relevant context (e.g., stainless steel, aluminum, or C22 in vibration sensors and / or transmitters), which may be too smooth to be handled individually using hands or tools, due to a sufficiently low coefficient of friction (e.g., between the tool or hand used and the material of the barrier member 102).
[0094] Step 604 is a step of engaging the elements to form the pre-press assembly 200. The elements of the pre-press assembly 200 can be engaged by engaging a conformal portion of the element. The step of engaging the piercing element 106 with the barrier member 102 may be performed before the method begins, such that the piercing element 106 is already coupled to the barrier member 102. In another embodiment, the piercing element 106 engages with the barrier member 102 by having the piercing element 106 penetrate the internal channel 126 of the barrier member 102. The step of engaging the press block 220 may include one or more of engaging a recess of the press block 220 with the piercing element 106, engaging the press block 220 with the optional pressure distribution element 108, and engaging the press block 220 with the first surface 120 of the barrier member 102. In embodiments where a pressure distribution element 108 is used to apply pressure evenly from the press block 220 to the barrier member 102 (to compensate for the recess), the press block 220 may not directly engage the barrier member 102. In other embodiments, possibly where a pressure distribution element 108 is not used to apply pressure from the press block 220 to the barrier member 102, the press block 220 may directly engage the barrier member 102. The barrier member 102 may engage the aperture 104, possibly where the periphery 124 of the barrier member 102 at least partially engages at least a portion of the conformal inner periphery 150 of the aperture 104. When engaged, the barrier member 102 may engage the aperture 104 such that the barrier member 102 is at least partially within the aperture 104. In one embodiment, engaging the barrier member 102 with the aperture 104 may include engaging the barrier member 102 with the aperture 104 such that the barrier member 102 cannot be forced further into the aperture 104 without deforming the barrier member 102. Some of the elements may be guided by alignment elements 222, e.g., alignment pins 224.In one embodiment, one or more of the barrier member 102, pressure distribution element 108, and press block 220 may have holes or channels for use as alignment elements 222 to align the elements for pressing, for example, using alignment pins 224. In one embodiment, the first surface 152 may have alignment elements 222 including holes for receiving guide elements such as alignment pins 224. In one embodiment, the holes and alignment pins 224 may be at least partially threaded to allow for a fixed, aligned, removable coupling.
[0095] Step 606 is a step of pressing the pre-press assembly 200 to form the post-press assembly 100. In this step, pressure is applied to the press block 220 in a pressure direction 196, for example, from the first side 197 to the second side 198. The pressure applied via the press block 220 may be applied to the first surface 120 of the barrier member 102 directly or via a pressure distribution element 108. Embodiments in which an intermediate press block 220 is not used are also contemplated. Step 606 may also apply pressure to the piercing element 106 via a recess in the press block 220. When pressure is applied by step 606, the rigid conformal inner periphery 150 of the aperture 104 can provide a counter pressure to the periphery 124 of the barrier member 102, such that the pressure applied to the first face 120 can deform the barrier member 102 to conform to the narrower portion of the conformal inner periphery 150 closer to the second side 198, and in some cases, even cause a portion of the barrier member 102 to flow cold across one or more of the first opening 160 and the second opening 162. The directional pressure applied in the pressure direction 196 is translated by the portion of the periphery 124 that is wider than the portion of the conformal inner periphery 150, forcing the wider portion of the periphery 124 into the conformal inner periphery 150 creating a lateral pressure gradient between the barrier member 102 and the aperture 104. A portion of the energy of the pressure is translated to deform the barrier member 102 to fit inside the aperture 104. A portion of the energy of the compression is converted into stored elastic potential energy in the barrier member 102, which may force the barrier member 102 to responsively expand and / or contract to maintain the interference fit rated barrier 199, possibly over a range of operating conditions. It should be appreciated that the element having the aperture 104 (possibly the housing 110) may expand and contract at a rate different than the rate of expansion of the barrier member 102, and this stored elastic potential energy maintains the interference fit rated barrier 199 by responding to the expansion and / or contraction of the aperture 104.In one embodiment, a portion of the energy from the pressing force is also converted to deform the barrier member 102, causing a portion of the barrier member 102 to flow at a lower temperature, and in some cases, flow at a lower temperature through one or more of the first opening 160 and the second opening 162 of the aperture 104. In an embodiment having a piercing element 106, the applied pressure may be sufficient to form an interference fit between the interior channel 126 of the barrier member 102, and in some cases, the piercing element interference fit, such that the interface between the interior channel 126 and the piercing element 106 can meet the same fire and / or explosion standards as the interference fit compliant barrier 199.
[0096] Step 608 is optionally a step of removing the press element. Removing the press element may include removing one or more of the press block 220, the pressure distribution element 108, the alignment element 222, and the alignment pin 224. In one embodiment, the pressure distribution element 108 is used during pressing and then removed. In another embodiment, the pressure distribution element 108 may be incorporated into the post-press assembly 100, as shown in step 612.
[0097] Step 610 is optionally a step of aging the interference fit standardized barrier 199. In embodiments where the interference fit standardized barrier 199 has a polymer component, for example, if the barrier member 102 is composed of a polymeric material, the interference fit standardized barrier 199 may be aged to ensure quality. When initially formed, the polymeric elements may still undergo significant structural changes. These changes may include physical structural changes and chemical changes related to interacting polymer chains. This aging allows the polymeric material to settle into a relatively consistent resting configuration and allows any chemical or physical interactions between the polymeric structural elements to occur. Typically, aging causes the polymer to shrink. In the context of the interference fit standardized barrier 199, this may be problematic since the space between the elements is considered to be limited. As the elements of the barrier member 102 shrink, more space is created between the polymeric and non-polymeric materials. The pressing can store significant elastic potential energy in the pressed polymer elements that form the interference fit (e.g., the polymer barrier member 102), so that even though aging causes shrinkage of the polymer elements, the stored elastic potential energy can counter some of the shrinkage. This stored elastic potential energy and the resulting expansion can mitigate the effects of shrinkage due to aging. This stored elastic potential energy causes a responsive expansion to effectively fill some of the created space. It should be appreciated that if, after aging, the gap between the elements of the interference fit standard barrier 199 is too large (possibly exceeding a predetermined threshold), the defective interference fit standard barrier 199 may have to be re-formed or the component having the defective interference fit standard barrier 199 may be discarded.Aging may be performed passively by exposing the polymeric element to ambient conditions, or aging may be active, for example, by exposing the polymeric element to radiation (e.g., sunlight), a particular humidity level, a particular chemical environment (e.g., an oxygen-rich environment), a particular temperature or temperature range, physical stress (e.g., vibration), combinations thereof, or other conditions commonly used in the art. Aging may be performed for a suitable period of time, such as at least one day, at least one week, at least two weeks, at least one month, or any period known in the art of aging polymers. Aging of polymers is well established in the art, and further description of aging is omitted for the sake of brevity.
[0098] Step 612 is optionally a step of fastening the pressure distribution element 108 to the post press assembly 100 to create the fastening assembly 500. The pressure distribution element 108 may be incorporated into the post press assembly 100 by bonding the pressure distribution element 108 to one or more of the first surface 152 and the barrier member 102. In embodiments with removable alignment elements 222, possibly alignment elements 222 having holes to receive alignment pins 224, the holes can also serve as a bonding substrate for bonding the elements 180 of the pressure distribution element 108 to the first surface 152. For example, the bonding elements 180 may be holes through the pressure distribution element 108 and screws that penetrate the holes and bond with holes in the first surface 152. In embodiments where the holes in the first surface 152 are threaded to receive the threaded alignment pins 224, the screws used to fasten the pressure distribution element 108 may be threaded such that the threads correspond to the threads of the holes in the first surface 152. In one embodiment, the first surface 152 may have additional holes, possibly threaded holes, that are not used to align the components of the pre-press assembly 200, but are used to couple the pressure distribution element 108 to the first surface 152. In this embodiment, the pressure distribution element 108 may have the same number of holes and / or threads as the first surface 152. In various embodiments, steps 608-612 may be performed in any order after step 606.
[0099] Embodiments are contemplated in which one or more of the piercing element 106 and pressure distribution element 108 are not part of the assembly 100 and / or 200. In these embodiments, portions of the steps involving those elements may not be performed.
[0100] In one embodiment, each step of the method shown in FIG. 6 is a separate step. In another embodiment, although depicted as separate steps in FIG. 6, steps 602-612 may not be separate steps. In other embodiments, the method shown in FIG. 6 may not have all of the steps listed above and / or may have other steps in addition to or instead of those listed above. The steps of the method 600 shown in FIG. 6 may be performed in a different order. Subsets of the steps listed above as part of the method 600 shown in FIG. 6 may be used to form their own method. The steps of the method 600 may be repeated any number of times in any combination and order, such as, for example, looping continuously to form multiple interference fit standard barriers 199.
[0101] 7 shows a flow chart of one embodiment of a method 700 for forming the barrier member 102. The method 700 may be one embodiment of step 602.
[0102] Step 702 is a step of forming the barrier member 102. The barrier member 102 can be formed by any known method, such as extrusion, molding, 3d printing, casting, bonding of sub-elements, any other known method for forming elements, etc. With respect to the barrier member 102, the physical properties of the material may be such that traditional forming methods may be cumbersome. In these embodiments, the barrier member 102 may be formed by cutting the material from a larger block and then forming substantially multiple barrier members 102 that can be cut or otherwise removed from the larger block. This may be advantageous for the barrier member 102 to be composed of a material that has a low coefficient of friction when interacting with traditional materials in the relevant context (e.g., stainless steel, aluminum, or C22 in vibration sensors and / or transmitters). These may be too smooth to be handled individually using hands or tools due to a sufficiently low coefficient of friction (e.g., between the tool or hand used and the material of the barrier member 102). Step 702 itself may be an embodiment of step 602.
[0103] In other embodiments, the method shown in Figure 7 may have other steps in addition to or in place of the steps listed above. Subsets of the steps listed above as part of the method 700 shown in Figure 7 may be used to form methods of their own. The steps of method 700 may be repeated any number of times, for example, looping continuously to form multiple barrier members 102.
[0104] 8 shows a flow chart of one embodiment of a method 800 of engaging elements to form the pre-press assembly 200. Method 800 may be one embodiment of step 604. The elements of the pre-press assembly 200 may be engaged by engaging conformal portions of the elements. The presented engaging steps may be performed in any order.
[0105] Step 802 is optionally a step of engaging alignment elements 222. Some of the engaged elements may be guided by alignment elements 222, e.g., alignment pins 224. In one embodiment, one or more of the barrier member 102, the pressure distribution element 108, and the press block 220 may have holes or channels for use as alignment elements 222 to align the elements for pressing, e.g., using alignment pins 224. In one embodiment, the first surface 152 may have alignment elements 222 including holes for receiving guide elements such as alignment pins 224. In one embodiment, the holes and alignment pins 224 may be at least partially screwed together to allow for a fixed, aligned, removable coupling. In one embodiment, step 802 may include engaging alignment pins 224 and possibly fixing them to other alignment elements 222 in the first surface 152.
[0106] Step 804 is optionally a step of engaging the piercing element 106 with the barrier member 102. In one embodiment, the piercing element 106 is not coupled to the barrier member 102 prior to the method. In this embodiment, the piercing element 106 may be engaged with the barrier member 102 by penetrating the barrier member 102 and possibly the internal channel 126. In this embodiment, the pressing that may be performed according to the method 800 may cause coupling between the piercing element 106 and the barrier member 102, for example, at least a portion of the piercing element 106 is coupled to the internal channel 126 of the barrier member 102 by an interference fit. In an embodiment in which the piercing element 106 is already coupled to the barrier member 102 prior to the start of the method, step 804 may not be necessary. Also, step 804 may itself be an embodiment of step 604.
[0107] Step 806 is engaging the barrier member 102 with the aperture 104. The barrier member 102 may engage with the aperture 104, in some cases with the periphery 124 of the barrier member 102 at least partially engaging with the conformal inner periphery 150 of the aperture 104. Upon engagement, the barrier member 102 may engage with the aperture 104 such that the barrier member 102 is at least partially within the aperture 104. In one embodiment, the barrier member 102 engages with the aperture 104 such that the barrier member 102 cannot be forced further into the aperture 104 without deforming the barrier member 102.
[0108] Step 808 is optionally a step of engaging the pressure distribution element 108 with the barrier member 102. In embodiments in which a pressure distribution element 108 is used in the assemblies 100 and / or 200, the pressure distribution element 108 may engage the barrier member 102. If the barrier member 102 has an engaging piercing element 106, engaging the pressure distribution element 108 with the barrier member 102 may include engaging the piercing element 106 with a slot 182 of the pressure distribution element 108. In embodiments in which the pressure distribution element 108 engages the barrier member 102 before the barrier member 102 engages the piercing element 106, the piercing element 106 may engage the pre-press assembly 200 by piercing both the pressure distribution element 108 and the barrier member 102 simultaneously, potentially eliminating the need for a separate step 802.
[0109] Step 810 is optionally a step of engaging the press block 220. Engaging the press block 220 may include one or more of engaging a recess of the press block 220 with the piercing element 106, engaging the press block 220 with an optional pressure distribution element 108, and engaging the press block 220 with the first surface 120 of the barrier member 102. In embodiments in which the pressure distribution element 108 is used to evenly apply pressure from the press block 220 to the barrier member 102 (to compensate for the recess), the press block 220 may not directly engage the barrier member 102. In other embodiments, possibly embodiments in which the pressure distribution element 108 is not used to apply pressure from the press block 220 to the barrier member 102, the press block 220 may directly engage the barrier member 102. For example, a combination of both is contemplated, such that the pressure distribution element 108 is present in the assembly 100 or 200 but there is still at least some direct contact between the press block 220 and the barrier member 102 .
[0110] Additionally, in embodiments using alignment element 222, press block 220 may have a hole or recess for receiving a portion of alignment element 222, such as alignment pin 224. In such embodiments, engaging step 808 may include engaging press block 220 with alignment element 222, such as engaging alignment pin 224. This step is optional, as embodiments are contemplated in which pressure is applied by something other than press block 220.
[0111] Embodiments are contemplated in which one or more of the piercing element 106 and pressure distribution element 108 are not part of the assembly 100 and / or 200. In these embodiments, portions of the steps involving those elements may not be performed.
[0112] In one embodiment, each step of the method shown in FIG. 8 is a separate step. In another embodiment, although depicted as separate steps in FIG. 8, steps 802-810 may not be separate steps. In other embodiments, the method shown in FIG. 8 may not have all of the steps listed above and / or may have other steps in addition to or instead of those listed above. The steps of the method 800 shown in FIG. 8 may be performed in a different order. Subsets of the steps listed above as part of the method 800 shown in FIG. 8 may be used to form their own method. The steps of the method 800 may be repeated any number of times in any combination and order, such as, for example, looping continuously to form multiple interference fit standard barriers 199.
[0113] 9 illustrates a flow chart of one embodiment of a method 900 for pressing the pre-press assembly 200 to form the post-press assembly 100. Method 900 may be one embodiment of step 606.
[0114] Step 902 is the step of applying pressure to form an interference fit standard barrier 199. In one embodiment, the pressure is applied to a first side of the press block 220. In an embodiment where the press block 220 is not used, the pressure may be applied directly to one of the barrier member 102 and the housing having the aperture 104. The pressure may be applied by any machine configured to press elements, such as a press machine. The pressure may be applied in a pressure direction 196 from the first side 197 to the second side 198. The pressure may be exerted on the press block 220 of the pre-press assembly 200, possibly on the pressure side 226 of the press block 220. The pressure is applied via the press block 220 to the element with which the press block 220 is engaged on the opposite side of the press block 220. The pressure applied via the press block 220 may be applied to the first surface 120 of the barrier member 102 directly or via the pressure distribution element 108. The pressing may also apply pressure to the piercing element 106 through the recess in the press block 220. When pressure is applied during step 606, the rigid conformal inner periphery 150 of the aperture 104 may provide a counter pressure to the periphery 124 of the barrier member 102, such that the pressure applied to the first face 120 may deform the barrier member 102 to conform to a narrower portion of the conformal inner periphery 150 closer to the second side 198, and in some cases, a portion of the barrier member 102 may even cold flow across one or more of the first opening 160 and the second opening 162. Step 902 itself may be an embodiment of step 606. In an embodiment, the pressing step 902 may be followed by any of steps 608-612 in any order. In the same or a different embodiment, the pressing step 902 may be followed by any of steps 602-604 in any order.
[0115] The pressure required in step 902 can be reduced by the arrangement of the elements of the pre-press assembly 200. For example, the pressure applied may be as much as 3000 pounds or less. Significantly higher pressures are required to compress a non-malleable barrier member 102. Furthermore, by allowing the barrier member 102 to deform and / or flow cold into the aperture 104 without providing an opposing surface, less pressure needs to be applied to create an interference fit standard barrier 199 than would be required if the aperture 104 did not accommodate the expansion and potential overflow of the barrier member 102 under pressure. Expansion and potential overflow can be facilitated by an aperture 104 having a depth between its perimeter first surface 152 and second surface 154 that is greater or less than the width between its first surface 120 and its second surface 122 of the barrier member 102. The expansion and potential overflow is facilitated by the aperture 104 having the second opening 162, potentially allowing a portion of the deformed barrier member 102 (during pressing) to partially protrude through the second opening 162. The result of step 902 may be a post-press assembly 100.
[0116] In one embodiment, the barrier member 102 is not heated before and / or after pressing to ensure that sufficient elastic potential energy is stored in the barrier member 102 after pressing. Heating may cause the barrier member 102 to expand or contract, and subsequent cooling may cause excessive contraction or expansion of the barrier member 102, compromising the interference fit standard barrier 199 as it cools. This may be facilitated by ensuring that the barrier member 102 is able to remain at a temperature below the melting point, determined at standard temperature and pressure, of the material of which it is constructed, before, during, and after one or more of the pressing and engagement of the elements.
[0117] Embodiments are contemplated in which one or more of the piercing element 106 and pressure distribution element 108 are not part of the assembly 100 and / or 200. In these embodiments, portions of the steps involving those elements may not be performed.
[0118] In other embodiments, the method shown in Figure 9 may have other steps in addition to or in place of the steps listed above. Subsets of the steps listed above as part of the method 900 shown in Figure 9 may be used to form methods of their own. The steps of method 900 may be repeated any number of times, such as looping continuously, to form multiple post press assemblies 100 and / or fixture assemblies 500.
[0119] [system] 10 illustrates a block diagram of an embodiment of a system 1000 having an interference fit compliant barrier 1099. The system 1000 includes an electrical component 1002, a device 1004, a network 1008, a first communication channel 1020, and a second communication channel 1022. The electrical component 1002 includes a feed-through PCB 1006, an electronics 1010, a terminal 1012, a terminal side 1097, an electronics side 1098, and an interference fit compliant barrier 1099.
[0120] The electrical component 1002 is a component that processes data from and / or transmits data to or between elements. In one embodiment, the electrical component 1002 is a transmitter configured to communicate with devices 1004 (e.g., sensors) and a network 1008. In this embodiment, the transmitter may include electronics 1010 that may do one or more of: act as a transceiver between the devices 1004, store data from the devices 1004, process data from the devices 1004, transmit and receive data to and from the devices 1004, etc. The electrical component 1002 may include an assembly (e.g., the postpress assembly 100 or the stationary assembly 500) that has an interference fit standard barrier 1099. The interference fit standard barrier 1099 may be an embodiment of the interference fit standard barrier 199. The interference fit standard barrier 1099 can provide a flame and / or explosion resistant barrier (possibly meeting one or more of the IEC standards "Ex d" and "Ex e") between the terminal side 1097 and the electronics side 1098. The terminal side 1097 and the electronics side 1098 can be embodiments of the first side 197 and the second side 198, respectively. The terminal side 1097 can have terminals 1012, which are elements configured to electronically communicate with external network elements via the network 1008. The electronics side 1098 can have electronics 1010, which are electronics for processing, storing, and / or communicating data. In one embodiment, the data processed, stored, or communicated by the electronics 1010 can be data representing one or more of flow rate, density, viscosity, speed of sound, time delay, phase shift, frequency, temperature, fluid composition, air permeability or porosity, response signal, drive signal, other signal associated with the vibration sensor, and the like. The electrical component 1002 may have a feed-through PCB 1006 that penetrates an interference-fit compliant barrier 1099 to allow communication between a terminal side 1097 and an electronics side 1098 of the interference-fit compliant barrier 1099. The feed-through PCB 1006 may be one embodiment of the feed-through element 106.Although not shown, in one embodiment, the interference fit standard barrier 1099 may have a fastening assembly 500 having a pressure distribution element 108 coupled thereto.
[0121] The device 1004 is an electronic element configured to communicate data with the electrical component 1002. The device 1004 may communicate with the electronics 1010 of the electrical component 1002 via a second communication channel 1022. In one embodiment, the device 1004 is a sensor, such as a Coriolis flow sensor, a density meter, a viscosity meter, a pressure sensor, any other device 1004 that measures a property of a fluid, a vibration sensor, etc. In this embodiment, the electrical component 1002 may be a transmitter configured to communicate data, such as sensor data, to and from the device 1004. In various embodiments, the sensor data may include one or more of a flow measurement, a density measurement, a viscosity measurement, a pressure measurement, a pickoff signal, a time delay or phase shift associated with the Coriolis force, a frequency, a phase difference, a phase error, a command frequency, other commands, etc.
[0122] The network 1008 is an electronic communication medium that can be used to communicate with any number of devices 1004 and / or electrical components 1002 and can store or transmit data, as needed. The network 1008 can one or more of store data on the electrical components 1002, transmit data to the electrical components 1002, or receive data from the electrical components 1002. The network elements can be used to provide commands to and / or receive data from one or more of the electrical components 1002 and devices 1004. These network 1008 elements can also process data from one or more of the electrical components 1002 and devices 1004. The data transmitted or processed can include one or more of sensor data, flow measurements, command signals, data retrieval, data writing, setting adjustments, and the like.
[0123] Although the system 1000 is described in the context of a transmitter for a sensor, it should be understood that embodiments of the interference fit standard barrier 199 may be used in any implementation having internal electronics, including implementations that are not configured to communicate with any other external electronics (e.g., not configured to communicate with the device 1004 and / or the network 1008).
[0124] The detailed description of the above embodiments is not an exhaustive description of all embodiments that the inventors contemplate within the scope of the present specification. Indeed, those skilled in the art will recognize that certain elements of the above-described embodiments can be combined or removed in various ways to create further embodiments, and such further embodiments are within the scope and teachings of the present specification. It will also be apparent to those skilled in the art that the above-described embodiments can be combined in whole or in part to create additional embodiments within the scope and teachings of the present specification. When specific numbers are specified to represent parameter values, all ranges between those numbers, as well as upper and lower ranges of those numbers, are contemplated and disclosed.
[0125] Thus, while specific embodiments have been described herein for illustrative purposes, various equivalent modifications are possible within the scope of the present disclosure, as those skilled in the art will recognize. The teachings provided herein may be applied to other methods and apparatus for making interference fit standard barriers, as well as the embodiments described above and illustrated in the accompanying drawings. Thus, the scope of the above embodiments should be determined from the following claims.
Claims
1. A barrier member (102) forming an assembly (100, 200) having an interference fit standard barrier (199), A first surface (120); A second surface (122); and a peripheral edge (124) between the first surface (120) and the second surface (122), the peripheral edge (124) being at least partially inclined at an angle (128) relative to a barrier reference line (130) that is perpendicular to both at least a portion of the first surface (120) and at least a portion of the second surface (122), the angle (128) decreasing from the first surface (120) to the second surface (122); an interior channel (126) extending through a member depth (123) of the barrier member (102), the member depth (123) being between the first face (120) and the second face (122), the interior channel (126) having a length that is greater than its width at a surface of the first face (120) and a surface of the second face (122); Equipped with Consisting at least in part of a polymer, The assembly (100, 200) includes a barrier member (102) having an inner periphery (150) further having a complementary angle (158) relative to the periphery (124).
2. An assembly (100) formed from a pre-press assembly (200), A barrier member (102), A first surface (120), The second face (122), a peripheral portion (124) between the first surface (120) and the second surface (122); and an interior channel (126) extending through a member depth (123) of said barrier member (102), said member depth (123) being between said first surface (120) and said second surface (122); a barrier member (102) comprising: An element having an aperture (104), said aperture (104) comprising: A first opening (160), A second opening (162), and a conformal inner periphery (150) between said first opening (160) and said second opening (162); An element comprising: Equipped with the barrier member (102) is pressed against the aperture (104) to at least partially engage the aperture (104), the barrier member (102) engaging the aperture (104) by at least partially conformal engagement of the periphery (124) with the conformal inner periphery (150); the barrier member (102) is at least partially constructed from a material that is more malleable than a material from which the element having the aperture (104) is constructed; An assembly (100), wherein the second surface (122) of the barrier member (102) is located within the aperture (104).
3. 3. The assembly (100) of claim 2, wherein the member depth (123) is less than an aperture depth (164) between the first opening (160) and the second opening (162).
4. 4. The assembly (100) of claim 2 or 3, wherein a surface area of the first surface (120) is greater than all of the surface areas of the second surface (122), the first opening (160) and the second opening (162), and the surface area of the second surface (122) is less than the surface area of the first opening (160) but the surface area of the second surface (122) is greater than the surface area of the second opening (162).
5. 5. The assembly (100) of any one of claims 2 to 4, further comprising a piercing element (106) that penetrates the internal channel (126) and thereby engages the internal channel (126), the piercing element (106) having a portion on each side of the barrier member (102) when the piercing element (106) engages the barrier member (102).
6. 6. The assembly (100) of any one of claims 2 to 5, further comprising a pressure distribution element (108), a surface of the pressure distribution element (108) engaging the first surface (120) of the barrier member (102), the pressure distribution element (108) having a slot (182) extending from a surface of the pressure distribution element (108) to an opposite surface of the pressure distribution element (108), the slot (182) coinciding with the internal channel (126) when the pressure distribution element (108) engages with the barrier member (102), such that a passage exists through both the barrier member (102) and the pressure distribution element (108).
7. 7. The assembly (100) of any one of claims 2 to 6, further comprising a press block (220), the press block (220) having at least one surface that engages with one or more of at least a portion of the piercing element (106), at least a portion of the pressure distribution element (108), and at least a portion of the barrier member (102).
8. 8. The assembly (100) of claim 7, wherein the press block (220) has at least one recess, and wherein the press block (220) at least partially engages the piercing element (106) within the at least one recess.
9. 9. The assembly (100) of any one of claims 2 to 8, wherein the barrier member (102) engages with the aperture (104) such that the barrier member (102) cannot be pushed further into the aperture (104) without deforming the barrier member (102).
10. 8. The assembly (100) of claim 7, wherein the element having the aperture (104) has a first surface (152) about a first opening (160) of the aperture (104), the first surface (152) having an alignment element (222) for aligning one or more engaged elements.
11. 11. The assembly (100) of claim 10, wherein the alignment element (222) comprises a hole in the first surface (152) and an alignment pin (224) detachably connectable to the hole in the first surface (152), and one or more of the press block (220) and the pressure distribution element (108) have a hole for receiving the alignment pin (224), and the hole for receiving the alignment pin (224) is for aligning the one or more engaged elements.
12. A first surface (120), The second face (122), Periphery (124) A barrier member (102) comprising: an element having an aperture (104), said element being constructed from a material that is less malleable than a material from which said barrier member (102) is constructed, said aperture (104) having a conformal inner periphery (150), at least a portion of said conformal inner periphery (150) matching at least a portion of said periphery (124); a interference fit standard barrier (199) having the barrier member (102) stores elastic potential energy that exerts pressure against the aperture (104) to maintain the interference fit of the barrier (199); The assembly (100), wherein the interference fit standard barrier (199) complies with one or more of a flame barrier standard and an explosion barrier standard.
13. 13. The assembly (100) of claim 12, wherein the stored elastic potential energy is sufficient to maintain compliance of the interference-fit standard barrier (199) with the one or more of the flame barrier standard and the explosion barrier standard over at least one predetermined range of at least one operating condition.
14. 14. The assembly (100) of claim 12 or 13, wherein any gap between the barrier member (102) and the aperture (104) in the interference fit standard barrier (199) is less than 5 thousandths of an inch.
15. 15. The assembly (100) of any one of claims 12 to 14, further comprising a piercing element (106) that pierces the interference fit standard barrier (199) by penetrating at least an interior channel (126) of the barrier member (102), and any gap between the piercing element (106) and the interior channel (126) is less than 5 thousandths of an inch.
16. 16. The assembly (100) of any one of claims 12 to 15, further comprising a pressure distribution element (108) coupled by a coupling element (180) coupled to a first surface (152) surrounding a first side (197) of the aperture (104).
17. 17. The assembly (100) of any one of claims 12 to 16, wherein the barrier member (102) has a portion that flows at a low temperature over one or more of the first opening (160) and the second opening (162) of the aperture (104).
18. 18. The assembly (100) of any one of claims 12 to 17, wherein the periphery (124) is at an angle (128) relative to a barrier reference line (130) and the conformal inner periphery (150) is at a complementary angle (158) relative to an aperture reference line (156), the aperture reference line (156) and the barrier reference line (130) being coincident, and the angle (128) and the complementary angle (158) both having a magnitude of less than 5 degrees.
19. A method for making an assembly (100) having an interference fit gauge barrier (199), comprising: engaging a barrier member (102) having a periphery (124) with an aperture (104) having a conformal internal periphery (150), wherein when the barrier member (102) engages the aperture (104), at least a portion of the periphery (124) conforms in engagement with at least a portion of the conformal internal periphery (150) and the barrier member (102) is at least partially, but not entirely, within the aperture (104); applying pressure to the barrier member (102) to form the interference fit standard barrier (199) with the aperture (104); Including, elastic potential energy from the applied pressure is stored in the barrier member (102), the elastic potential energy resulting in the application of a force by at least a portion of the periphery (124) to at least a portion of the conformal inner periphery (150); The method of claim 1, wherein the interference fit standard barrier (199) complies with one or more of a flame barrier standard and an explosion barrier standard.
20. 20. The method of claim 19, wherein the applied pressure causes the elastic potential energy to be stored in the barrier member (102) in an amount sufficient for the interference fit rated barrier (199) to maintain the compliance with the one or more of the flame barrier rating and the explosion barrier rating over at least one predetermined range of at least one operating condition.
21. 21. The method of claim 19 or 20, wherein the applied pressure is less than 3000 pounds and is distributed primarily to a pressure distribution element (108).
22. 22. The method of any one of claims 19 to 21, wherein the applied pressure is sufficient such that any gaps present in the interference fit rated barrier (199) have a gap depth of less than two thousandths of an inch.
23. 23. The method of any one of claims 19 to 22, wherein the step of applying pressure to the barrier member (102) comprises applying pressure via a pressure distribution element (108), the surface of the pressure distribution element (108) pressing against the barrier member (102) being substantially flat to enable application of a substantially uniform pressure to the barrier member (102).
24. engaging a piercing element (106) with an internal channel (126) of the barrier member (102), the internal channel (126) extending through a first surface (120), a member depth (123), and a second surface (122), the step of engaging the piercing element (106) with the internal channel (126) comprising passing the piercing element (106) through the internal channel (126) such that a portion of the piercing element (106) is located on one side of the barrier member (102) and another portion of the piercing element (106) is located on another side of the barrier member (102).
24. The method of claim 19, further comprising: wherein the step of applying pressure to the barrier member (102) causes compression of the interior channel (126) against the piercing element (106), thereby forming a piercing element interference fit, the piercing element interference fit complying with the one or more of the flame barrier standard and the explosion barrier standard.
25. 25. The method according to any one of claims 19 to 24, wherein the pressure is applied via a press block (220).
26. 26. The method of any one of claims 19 to 25, further comprising aligning parts of the assembly (100) using one or more alignment elements (222).
27. 27. The method of claim 19, wherein the step of engaging the barrier member (102) with the aperture (104) is a step of engaging the barrier member (102) with the aperture (104) such that the barrier member (102) cannot be pushed further into the aperture (104) without deforming the barrier member (102).
28. 28. The method of any one of claims 19 to 27, wherein the applied pressure is sufficient to cause at least a portion of the barrier member (102) to flow at low temperature over one or more of the first opening (160) of the aperture (104) and the second opening (162) of the aperture (104).
29. 29. The method of any one of claims 19 to 28, further comprising forming the barrier member (102) by cutting material from a block of material having sufficient material to form more than one barrier member (102).
30. 30. The method of any one of claims 19 to 29, not including the step of heating the barrier member (102) above a melting temperature of a material comprising the barrier member (102), the melting temperature being determined at standard temperature and pressure.
31. 31. The method of any one of claims 19 to 30, further comprising aging the interference fit rated barrier (199), the interference fit rated barrier (199) being at least partially constructed from a polymer.
32. 31. The method of claim 30, wherein the static coefficient of friction between the material of which the periphery (124) is constructed and the material of which the conformal inner periphery (150) is constructed in a dry and clean condition is less than 0.2 at standard temperature and pressure.
33. 19. The assembly (100) of any one of claims 2 to 18, wherein the barrier member (102) has a volume greater than the volume of the aperture (104).
34. 19. An assembly (100) as claimed in any one of claims 2 to 18, wherein the element having the aperture (104) is a housing for an electrical component (1002), the housing having a terminal side (1097) having at least one terminal (1012) for coupling to a network (1008) and an electronics side (1098) having electronics (1010) for communicating with a device (1004), the first surface (120) facing the terminal side (1097) and the second surface (122) facing the electronics side (1098).
35. The barrier member (102) of claim 1, wherein the barrier member (102) is constructed at least in part from a fluorocarbon.
36. 36. The barrier member (102) of claim 35, wherein the fluorocarbon is polytetrafluoroethylene (PTFE).
37. The barrier member (102) of claim 1, wherein the second surface (122) has a surface area that is less than a surface area of the first surface (120).
38. The barrier member (102) of claim 1, which is non-cylindrical.
39. The barrier member (102) of claim 1 , which is shaped as a narrow curved triangle.
40. An assembly (100) as described in any one of claims 2 to 18, wherein the barrier member (102) is at least partially constructed from a fluorocarbon.
41. The assembly (100) of claim 40, wherein the fluorocarbon is polytetrafluoroethylene (PTFE).
42. An assembly (100) as described in any one of claims 2 to 18, wherein the second surface (122) has a surface area smaller than a surface area of the first surface (120).
43. An assembly (100) as described in any one of claims 2 to 18, which is not cylindrical.
44. An assembly (100) as described in any one of claims 2 to 18, formed as a narrow curved triangle.
Citation Information
Patent Citations
Drain pipe arrangement structure and drain pipe installation method
JP2007270440A
Flame-retardant electrical feedthrough