Bread
Applying carboxymethylated cellulose nanofibers to bread surfaces addresses the issue of excessive crumbing by improving crust integrity, reducing crumbs when cutting or shredding.
Patent Information
- Application Number
- JP2021052982
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-26
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-03-26
AI Technical Summary
Breads with hard crusts, such as French breads, tend to crumble excessively when cut or shredded, leading to a large amount of crumbs.
Applying a composition containing carboxymethylated cellulose nanofibers to the surface of bread, with a concentration of 0.01% to 1% by mass based on the solid content, which includes carboxymethylated cellulose nanofibers with a degree of carboxymethyl substitution of 0.01 to 0.50 and crystallinity of type I cellulose of 40% or more.
The application of carboxymethylated cellulose nanofibers significantly reduces the amount of crumbs when cutting or shredding the bread, enhancing the crust's integrity and reducing crumb formation.
Smart Images

Figure 0007581106000002 
Figure 0007581106000003 
Figure 0007581106000004
Abstract
Description
[Technical field]
[0001] The present invention relates to bread having a surface coated with a composition containing carboxymethylated cellulose nanofibers. [Background technology]
[0002] So-called French breads, such as baguettes and batards, consist of an outer layer called a crust and a soft inner layer called a crumb, and are characterized by a harder crust than other types of bread.
[0003] It is known that when bread is stored in poor conditions, the moisture content of the crust becomes extremely low, resulting in a lack of plasticity and a tendency to crumble, which causes the crust to peel off from the flexible crumb. In order to prevent the crust from peeling off, it has been disclosed that a crust peel inhibitor obtained by heat-treating a solution containing gluten and an organic acid is added to the raw materials of the bread to produce the bread (Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2020-156319 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, for breads with hard crusts such as French bread, regardless of storage conditions, when the bread is cut with a knife or torn by hand to eat, the crust crumbles, producing a large amount of crumbs. Therefore, the object of the present invention is to provide breads that produce less crumbs when cut or torn. [Means for solving the problem]
[0006] The present invention provides the following: (1) Bread having a composition containing carboxymethylated cellulose nanofibers applied to the surface of the bread, wherein the amount of the carboxymethylated cellulose nanofibers applied is, in terms of solid content, 0.01% by mass or more and 1% by mass or less relative to the solid content of the bread. (2) The bread according to (1), wherein the carboxymethylated cellulose nanofiber has a degree of carboxymethyl substitution per anhydrous glucose unit of the cellulose nanofiber of 0.01 to 0.50 and a degree of crystallinity of cellulose type I of 40% or more. (3) Bread according to (1) or (2), further containing carboxymethylcellulose. Effect of the Invention
[0007] According to the present invention, bread can be provided that produces less crumbs when cut or shredded. [Brief description of the drawings]
[0008] [Figure 1] 1 shows the results of observing crumbs that appear when the French bread produced in Example 1 is torn by hand. [Diagram 2] This shows the results of observing the crumbs that are produced when the French bread produced in Comparative Example 1 is torn by hand. [Diagram 3] This is an observation result of bread crumbs that are produced when the French bread produced in Comparative Example 2 is torn by hand. [Figure 4] This is an observation result of the crumbs that are produced when the French bread produced in the reference example is torn by hand. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The breads of the present invention will be described below. In the present invention, "to" includes both ends. That is, "X to Y" includes both ends of the values X and Y.
[0010] The breads of the present invention have a composition containing carboxymethylated cellulose nanofibers applied to the surface of the bread, and the amount of the carboxymethylated cellulose nanofibers applied is, in solid content, 0.01% by mass or more and 1% by mass or less of the solid content of the bread.
[0011] (Carboxymethylated cellulose nanofiber) Carboxymethylated cellulose nanofibers are carboxymethylated cellulose converted into nanofibers having a nanoscale fiber diameter. Carboxymethylated cellulose has a structure in which some of the hydroxyl groups in the glucose residues constituting cellulose are ether-bonded to carboxymethyl groups. Carboxymethylated cellulose may take the form of a salt, for example, a metal salt such as sodium salt of carboxymethylated cellulose, and the carboxymethylated cellulose nanofibers may also take the form of a salt.
[0012] (Degree of carboxymethyl substitution) The carboxymethylated cellulose nanofiber used in the present invention preferably has a carboxymethyl substitution degree per anhydrous glucose unit of cellulose of 0.50 or less. If the carboxymethyl substitution degree exceeds 0.50, it is considered that the cellulose will dissolve in water and will not be able to maintain its fiber shape. In addition, the carboxymethyl substitution degree per anhydrous glucose unit of cellulose is preferably 0.01 or more. If the carboxymethyl substitution degree is less than 0.01, it is considered that a large amount of energy is required to defibrate the carboxymethylated cellulose nanofiber. From the viewpoint of operability, the substitution degree is more preferably 0.02 to 0.50, even more preferably 0.05 to 0.50, and even more preferably 0.10 to 0.40. By introducing a carboxymethyl group into cellulose, the cellulose particles electrically repel each other, so that the cellulose particles can be defibrated into nanofibers. The carboxymethyl substitution degree can be adjusted by controlling the amount of the carboxymethylating agent to be reacted, the amount of the mercerizing agent, the composition ratio of water and organic solvent, and the like.
[0013] In the present invention, the anhydroglucose unit means each anhydroglucose (glucose residue) constituting cellulose. The degree of carboxymethyl substitution (also called the degree of etherification) indicates the ratio of hydroxyl groups in the glucose residues constituting cellulose that are substituted with carboxymethyl ether groups (the number of carboxymethyl ether groups per glucose residue). The degree of carboxymethyl substitution may be abbreviated as DS.
[0014] The carboxymethylated cellulose nanofibers used in the present invention maintain at least a part of their fibrous shape even when dispersed in water. That is, when an aqueous dispersion of carboxymethylated cellulose nanofibers is observed under an electron microscope, a fibrous substance can be observed. Furthermore, when the carboxymethylated cellulose nanofibers are measured by X-ray diffraction, a peak of cellulose type I crystals can be observed.
[0015] (Crystallization degree of cellulose type I) The crystallinity of cellulose type I in the carboxymethylated cellulose nanofiber used in the present invention is preferably 40% or more, more preferably 50% or more. When the crystallinity of cellulose type I is as high as 40% or more, the proportion of cellulose that does not dissolve in a solvent such as water and maintains its crystalline structure is high, so that the thixotropy is high and it becomes suitable for viscosity adjustment applications such as thickeners. In addition, when added to bread ingredients, it has the advantage of being able to impart excellent shape retention. The crystallinity of cellulose can be controlled by the concentration of the mercerizing agent, the temperature during treatment, and the degree of carboxymethylation. Since a high concentration of alkali is used in mercerization and carboxymethylation, cellulose type I crystals are easily converted to type II, but the desired crystallinity can be maintained by adjusting the degree of denaturation by adjusting the amount of alkali (mercerizing agent) used. There is no particular limit to the upper limit of the crystallinity of cellulose type I. In reality, it is considered that the upper limit is about 90%.
[0016] The method for measuring the crystallinity of cellulose type I of carboxymethylated cellulose nanofiber is as follows: The sample is placed in a glass cell and measured using an X-ray diffraction measuring device (LabX XRD-6000, manufactured by Shimadzu Corporation). The degree of crystallinity is calculated using the method of Segal et al., and is calculated from the diffraction intensity of the 002 plane at 2θ = 22.6° and the diffraction intensity of the amorphous part at 2θ = 18.5° using the diffraction intensity of the X-ray diffraction pattern at 2θ = 10° to 30° as the baseline, according to the following formula.
[0017] Xc = (I002c - Ia) / I002c x 100 Xc = Crystallinity of cellulose type I (%) I002c: 2θ=22.6°, diffraction intensity of 002 plane Ia: 2θ=18.5°, diffraction intensity of the amorphous part.
[0018] The proportion of type I crystals in the carboxymethylated cellulose nanofibers is usually the same as that in the carboxymethyl cellulose before it is made into nanofibers.
[0019] (fiber diameter, aspect ratio) The carboxymethylated cellulose nanofibers used in the present invention have a nanoscale fiber diameter, with an average fiber diameter of 3 nm to 500 nm, preferably 3 nm to 150 nm, more preferably 3 nm to 20 nm, even more preferably 5 nm to 19 nm, and even more preferably 5 nm to 15 nm.
[0020] The aspect ratio of the carboxymethylated cellulose nanofiber is not particularly limited, but is preferably 350 or less, more preferably 300 or less, more preferably 200 or less, more preferably 120 or less, more preferably 100 or less, and more preferably 80 or less. The lower limit of the aspect ratio is not particularly limited, but is preferably 25 or more, more preferably 30 or more. When the aspect ratio is 25 or more, the fibrous shape can provide an effect such as improved thixotropy. The aspect ratio of the carboxymethylated cellulose nanofiber can be controlled by the mixing ratio of the solvent and water during carboxymethylation, the amount of chemicals added, and the degree of carboxymethylation. In addition, carboxymethylated cellulose nanofibers having an aspect ratio in the above range can be produced, for example, by the production method described below.
[0021] The average fiber diameter and average fiber length of carboxymethylated cellulose nanofibers can be measured by analyzing 200 randomly selected fibers using an atomic force microscope (AFM) if the diameter is 20 nm or less, or a field emission scanning electron microscope (FE-SEM) if the diameter is 20 nm or more, and calculating the average. The aspect ratio can be calculated using the following formula: Aspect ratio = average fiber length / average fiber diameter.
[0022] (Method of producing carboxymethylated cellulose nanofiber) The carboxymethylated cellulose nanofibers used in the present invention are not particularly limited, but can be produced by defibrating carboxymethylated cellulose produced by the following method.
[0023] Carboxymethylated cellulose can generally be produced by treating cellulose with an alkali (mercerization) and then reacting the resulting mercerized cellulose (also called alkali cellulose) with a carboxymethylating agent (also called etherifying agent). Carboxymethylated cellulose capable of forming nanofibers having the above-mentioned characteristics of the present invention can be produced by carrying out mercerization (alkali treatment of cellulose) in a solvent mainly composed of water, and then carrying out carboxymethylation (also called etherification) in a mixed solvent of water and an organic solvent.
[0024] (cellulose) In the present invention, cellulose refers to a polysaccharide having a structure in which D-glucopyranose (also simply referred to as "glucose residue" or "anhydroglucose") is linked by β-1,4 bonds. Cellulose is generally classified into natural cellulose, regenerated cellulose, fine cellulose, microcrystalline cellulose excluding non-crystalline regions, etc., based on the origin, manufacturing method, etc. In the present invention, any of these celluloses can be used as a raw material for mercerized cellulose, but in order to maintain a crystallinity of cellulose type I of preferably 40% or more in carboxymethylated cellulose nanofibers, it is preferable to use cellulose with a high crystallinity of cellulose type I as the raw material. The crystallinity of cellulose type I of the raw material cellulose is preferably 70% or more, more preferably 80% or more. The method for measuring the crystallinity of cellulose type I is as described above.
[0025] Examples of natural cellulose include bleached pulp or unbleached pulp (bleached wood pulp or unbleached wood pulp), linters, refined linters, and cellulose produced by microorganisms such as acetic acid bacteria. The raw material for bleached pulp or unbleached pulp is not particularly limited, and examples thereof include wood, cotton, straw, bamboo, hemp, jute, kenaf, etc. The method for producing bleached pulp or unbleached pulp is also not particularly limited, and may be a mechanical method, a chemical method, or a method that is an intermediate combination of the two. Examples of bleached or unbleached pulp classified according to the production method include mechanical pulp (thermomechanical pulp (TMP), groundwood pulp), chemical pulp (sulfite pulp such as softwood unbleached sulfite pulp (NUSP) and softwood bleached sulfite pulp (NBSP), and kraft pulp such as softwood unbleached kraft pulp (NUKP), softwood bleached kraft pulp (NBKP), hardwood unbleached kraft pulp (LUKP), and hardwood bleached kraft pulp (LBKP)). Furthermore, in addition to papermaking pulp, dissolving pulp may be used. Dissolving pulp is chemically refined pulp that is mainly used by dissolving it in chemicals, and is the main raw material for artificial fibers, cellophane, etc.
[0026] Examples of regenerated cellulose include cellulose dissolved in some solvent such as cuprammonium solution, cellulose xanthate solution, or morpholine derivative, and then spun again. Examples of fine cellulose include those obtained by subjecting cellulosic materials, including the above-mentioned natural cellulose and regenerated cellulose, to depolymerization treatment (e.g., acid hydrolysis, alkaline hydrolysis, enzymatic decomposition, explosive crushing treatment, vibrating ball mill treatment, etc.), and those obtained by mechanically treating the above-mentioned cellulosic materials.
[0027] (Mercerization) Mercerized cellulose (also called alkali cellulose) is obtained by using the above-mentioned cellulose as a raw material and adding a mercerizing agent (alkali).
[0028] A solvent that mainly uses water (a solvent mainly made of water) refers to a solvent that contains water at a ratio of more than 50% by mass. The water content in the solvent mainly made of water is preferably 55% by mass or more, more preferably 60% by mass or more, more preferably 70% by mass or more, more preferably 80% by mass or more, even more preferably 90% by mass or more, and even more preferably 95% by mass or more. A particularly preferred solvent mainly made of water is 100% by mass (i.e., water).
[0029] Examples of the solvent other than water (used in a mixture with water) in the solvent mainly made of water include organic solvents used as a solvent in the subsequent carboxymethylation step. Examples include alcohols such as methanol, ethanol, N-propyl alcohol, isopropyl alcohol, N-butanol, isobutanol, and tertiary butanol, ketones such as acetone, diethyl ketone, and methyl ethyl ketone, as well as dioxane, diethyl ether, benzene, and dichloromethane. These can be used alone or in a mixture of two or more kinds in an amount of less than 50% by mass in water as a solvent in the mercerization step. The organic solvent in the solvent mainly made of water is preferably 45% by mass or less, more preferably 40% by mass or less, more preferably 30% by mass or less, more preferably 20% by mass or less, more preferably 10% by mass or less, more preferably 5% by mass or less, and more preferably 0% by mass.
[0030] Examples of the mercerizing agent include alkali metal hydroxides such as lithium hydroxide, sodium hydroxide, and potassium hydroxide, and any one or more of these can be used in combination. The mercerizing agent is not limited to these, but these alkali metal hydroxides can be added to the reactor as an aqueous solution of, for example, 1 to 60 mass %, preferably 2 to 45 mass %, and more preferably 3 to 25 mass %.
[0031] The amount of the mercerizing agent used is not particularly limited, but in one embodiment, it is preferably 0.1 mol or more and 2.5 mol or less, more preferably 0.3 mol or more and 2.0 mol or less, and even more preferably 0.4 mol or more and 1.5 mol or less, per 100 g of cellulose (bone dry).
[0032] The amount of the solvent mainly composed of water during mercerization is preferably 1.5 to 20 times by mass, and more preferably 2 to 10 times by mass, relative to the cellulose raw material. By using such an amount, stirring and mixing of the raw material becomes easy, and the reaction can be caused to occur uniformly in the raw material.
[0033] The mercerization treatment is carried out by mixing the bottom raw material (cellulose) with a solvent mainly composed of water, adjusting the temperature of the reactor to 0 to 70°C, preferably 10 to 60°C, more preferably 10 to 40°C, adding an aqueous solution of a mercerizing agent, and stirring for 15 minutes to 8 hours, preferably 30 minutes to 7 hours, more preferably 30 minutes to 3 hours, thereby obtaining mercerized cellulose (alkali cellulose).
[0034] The pH during mercerization is preferably 9 or more, which allows the mercerization reaction to proceed. The pH is more preferably 11 or more, further preferably 12 or more, and may be 13 or more. There is no particular upper limit to the pH.
[0035] The mercerization can be carried out using a reactor capable of mixing and stirring the above-mentioned components while controlling the temperature, and various reactors conventionally used for mercerization reactions can be used. For example, a batch-type stirring device having two shafts for stirring and mixing the above-mentioned components is preferred from the viewpoints of both uniform mixing ability and productivity.
[0036] (Carboxymethylation) Carboxymethylated cellulose is obtained by adding a carboxymethylating agent (also called an etherifying agent) to mercerized cellulose.
[0037] Examples of the carboxymethylating agent include monochloroacetic acid, sodium monochloroacetate, methyl monochloroacetate, ethyl monochloroacetate, isopropyl monochloroacetate, etc. Among these, monochloroacetic acid or sodium monochloroacetate is preferred in terms of availability of the raw material.
[0038] The amount of the carboxymethylating agent used is not particularly limited, but in one embodiment, it is preferably added in the range of 0.5 to 1.5 mol per anhydrous glucose unit of cellulose. The lower limit of the above range is more preferably 0.6 mol or more, even more preferably 0.7 mol or more, and the upper limit is more preferably 1.3 mol or less, even more preferably 1.1 mol or less. The carboxymethylating agent can be added to the reactor as, for example, a 5 to 80 mass % aqueous solution, more preferably 30 to 60 mass %, but is not limited thereto, or can be added in a powder state without dissolving.
[0039] The molar ratio of the mercerizing agent to the carboxymethylating agent (mercerizing agent / carboxymethylating agent) is generally 0.9 to 2.45 when monochloroacetic acid or sodium monochloroacetate is used as the carboxymethylating agent. The reason is that if it is less than 0.9, the carboxymethylation reaction may be insufficient, and unreacted monochloroacetic acid or sodium monochloroacetate may remain and be wasted, and if it exceeds 2.45, a side reaction between the excess mercerizing agent and monochloroacetic acid or sodium monochloroacetate may proceed, resulting in the production of an alkali metal glycolate, which may be uneconomical.
[0040] The concentration of the cellulose raw material in the carboxymethylation reaction is not particularly limited, but is preferably 1 to 40% (w / v).
[0041] Simultaneously with the addition of the carboxymethylating agent, or before or immediately after the addition of the carboxymethylating agent, an organic solvent or an aqueous solution of an organic solvent is appropriately added to the reactor, or the organic solvent other than water used in the mercerization treatment is appropriately reduced by reducing pressure or the like to form a mixed solvent of water and an organic solvent, and the carboxymethylation reaction is allowed to proceed in this mixed solvent of water and an organic solvent. The timing of the addition or reduction of the organic solvent may be any time between the end of the mercerization reaction and immediately after the addition of the carboxymethylating agent, and is not particularly limited, but is preferably within 30 minutes before or after the addition of the carboxymethylating agent, for example.
[0042] Examples of the organic solvent include alcohols such as methanol, ethanol, N-propyl alcohol, isopropyl alcohol, N-butanol, isobutanol, and tertiary butanol, ketones such as acetone, diethyl ketone, and methyl ethyl ketone, as well as dioxane, diethyl ether, benzene, and dichloromethane, and these can be used alone or in a mixture of two or more kinds as a solvent for carboxymethylation by adding them to water. Among these, monohydric alcohols having 1 to 4 carbon atoms are preferred because of their excellent compatibility with water, and monohydric alcohols having 1 to 3 carbon atoms are more preferred.
[0043] The ratio of the organic solvent in the mixed solvent during carboxymethylation is preferably 20% by mass or more, more preferably 30% by mass or more, even more preferably 40% by mass or more, even more preferably 45% by mass or more, and particularly preferably 50% by mass or more, based on the total of water and organic solvent. The upper limit of the ratio of the organic solvent is not limited, and may be, for example, 99% by mass or less. Considering the cost of the organic solvent to be added, it is preferably 90% by mass or less, more preferably 85% by mass or less, even more preferably 80% by mass or less, and even more preferably 70% by mass or less.
[0044] The reaction medium for carboxymethylation (a mixed solvent of water and an organic solvent, etc., not containing cellulose) preferably has a lower proportion of water (in other words, a higher proportion of organic solvent) than the reaction medium for mercerization. By satisfying this range, it becomes easier to increase the degree of carboxymethyl substitution while maintaining the crystallinity of the resulting carboxymethylated cellulose. In addition, when the reaction medium for carboxymethylation has a lower proportion of water (a higher proportion of organic solvent) than the reaction medium for mercerization, there is also an advantage that when transferring from the mercerization reaction to the carboxymethylation reaction, a mixed solvent for the carboxymethylation reaction can be formed by the simple means of adding a desired amount of organic solvent to the reaction system after the mercerization reaction is completed.
[0045] A mixed solvent of water and an organic solvent is prepared, and a carboxymethylating agent is added to the mercerized cellulose, followed by stirring for 15 minutes to 4 hours, preferably 15 minutes to 1 hour, while maintaining a constant temperature, preferably in the range of 10 to 40°C. The liquid containing the mercerized cellulose and the carboxymethylating agent are preferably mixed in several batches or by dropwise addition, in order to prevent the reaction mixture from becoming too hot. After adding the carboxymethylating agent and stirring for a certain period of time, the temperature is raised if necessary to a reaction temperature of 30 to 90°C, preferably 40 to 90°C, more preferably 60 to 80°C, and an etherification (carboxymethylation) reaction is carried out for 30 minutes to 10 hours, preferably 1 hour to 4 hours, to obtain carboxymethylated cellulose.
[0046] In the carboxymethylation, the reactor used in the mercerization may be used as it is, or a separate reactor capable of mixing and stirring the above-mentioned components while controlling the temperature may be used.
[0047] After the reaction is completed, the remaining alkali metal salt may be neutralized with a mineral acid or an organic acid. If necessary, by-products such as inorganic salts and organic acid salts may be removed by washing with aqueous methanol, and then dried, pulverized, and classified to obtain carboxymethylated cellulose or a salt thereof. When washing to remove by-products, the cellulose may be converted to an acid form before washing, and then converted back to a salt form after washing. Examples of devices used in dry grinding include impact mills such as hammer mills and pin mills, media mills such as ball mills and tower mills, and jet mills. Examples of devices used in wet grinding include homogenizers, mass colloiders, pearl mills, and other devices.
[0048] (Defibrillation into nanofibers) The carboxymethylated cellulose obtained by the above method can be defibrated to convert it into cellulose nanofibers having nanoscale fiber diameters.
[0049] For defibration, a dispersion of the carboxymethylated cellulose obtained by the above method is prepared. The dispersion medium is preferably water for ease of handling. The concentration of carboxymethylated cellulose in the dispersion at the time of defibration is preferably 0.01 to 10% (w / v) in consideration of the efficiency of defibration and dispersion.
[0050] The device used for defibrating carboxymethylated cellulose is not particularly limited, but devices such as high-speed rotation, colloid mill, high-pressure, roll mill, and ultrasonic devices can be used. When defibrating, it is preferable to apply a strong shear force to the dispersion of carboxymethylated cellulose. In particular, for efficient defibration, it is preferable to apply a pressure of 50 MPa or more to the dispersion and to use a wet high-pressure or ultra-high-pressure homogenizer that can apply a strong shear force. The pressure is more preferably 100 MPa or more, and even more preferably 140 MPa or more. Furthermore, prior to defibration and dispersion treatment with the high-pressure homogenizer, the dispersion may be subjected to a pretreatment, if necessary, using a known mixing, stirring, emulsifying, and dispersing device such as a high-speed shear mixer.
[0051] A high-pressure homogenizer is a device that emulsifies, disperses, breaks down, pulverizes, and ultra-finely disperses a fluid by pressurizing it (high pressure) with a pump and ejecting it from extremely fine gaps in the flow path, using a total energy of collisions between particles and shear forces caused by pressure differences.
[0052] In the present invention, the carboxymethylated cellulose nanofibers may be used in the form of a dispersion, or may be used as a powder after drying (removal of the dispersion medium), pulverization, and classification.
[0053] When the carboxymethylated cellulose nanofibers used in the present invention are used as a powder, they may contain other components as necessary. For example, when producing a powder, it is preferable to make a water-soluble polymer coexist with the dispersion of carboxymethylated cellulose nanofibers before drying, since this improves redispersibility. The reason why the water-soluble polymer improves redispersibility is not clear, but it is speculated that the water-soluble polymer covers the low charge density parts of the surface of the carboxymethylated cellulose nanofibers, suppresses the formation of hydrogen bonds, and prevents the nanofibers from agglomerating together during drying.
[0054] (Water-soluble polymer) When carboxymethylated cellulose nanofibers are used as a powder, examples of water-soluble polymers that can be present during the production of the powder include cellulose derivatives (carboxymethylcellulose, methylcellulose, hydroxypropylcellulose, ethylcellulose), xanthan gum, xyloglucan, dextrin, dextran, carrageenan, locust bean gum, alginic acid, alginates, pullulan, starch, potato starch, kudzu starch, processed starch (cationized starch, phosphorylated starch, phosphate crosslinked starch, phosphate monoesterified phosphate crosslinked starch, hydroxypropyl starch, hydroxypropylated phosphate crosslinked starch, acetylated adipic acid crosslinked starch, acetylated phosphate crosslinked starch, acetylated oxidized starch, sodium octenyl succinate starch, starch acetate, oxidized starch), co starch, gum arabic, locust bean gum, gellan gum, polydextrose, pectin, chitin, water-soluble chitin, chitosan, casein, albumin, soy protein lysate, peptone, polyvinyl alcohol, polyacrylamide, sodium polyacrylate, polyvinylpyrrolidone, polyvinyl acetate, polyamino acid, polylactic acid, polymalic acid, polyglycerin, latex, rosin-based sizing agent, petroleum resin-based sizing agent, urea resin, melamine resin, epoxy resin, polyamide resin, polyamide-polyamine resin, polyethyleneimine, polyamine, vegetable gum, polyethylene oxide, hydrophilic crosslinked polymer, polyacrylate, starch polyacrylic acid copolymer, tamarind gum, guar gum, and colloidal silica, and mixtures of one or more thereof. Among these, cellulose derivatives are preferred in terms of affinity with carboxymethylated cellulose nanofibers, and carboxymethylcellulose and its salts are particularly preferred. It is believed that water-soluble polymers such as carboxymethyl cellulose and its salts penetrate between the carboxymethylated cellulose nanofibers and increase the distance between the nanofibers, thereby improving redispersibility.
[0055] When carboxymethylcellulose or a salt thereof is used as the water-soluble polymer, it is preferable to use carboxymethylcellulose with a degree of carboxymethyl group substitution per anhydrous glucose unit of 0.55 to 1.6, more preferably 0.55 to 1.1, and even more preferably 0.65 to 1.1. In addition, a molecule with a long length (high viscosity) is preferable because it has a high effect of widening the distance between nanofibers. In addition, the B-type viscosity of a 1% by mass aqueous solution of carboxymethylcellulose at 25°C and 60 rpm is preferably 3 mPa·s to 14000 mPa·s, more preferably 7 mPa·s to 14000 mPa·s, and even more preferably 1000 mPa·s to 8000 mPa·s. Note that the "carboxymethylcellulose or a salt thereof" as the water-soluble polymer referred to here is completely dissolved in water, and is therefore distinguished from the carboxymethylated cellulose nanofibers whose fiber shape can be confirmed in water.
[0056] The blending amount of the water-soluble polymer is preferably 5% by mass to 300% by mass, more preferably 20% by mass to 300% by mass, more preferably 25% by mass to 200% by mass, and even more preferably 25% by mass to 60% by mass, based on the carboxymethylated cellulose nanofiber (bone dry solid content). Blending 5% by mass or more of the water-soluble polymer can improve the redispersibility. On the other hand, if the blending amount of the water-soluble polymer exceeds 300% by mass, problems such as viscosity characteristics such as thixotropy, which is a characteristic of the carboxymethylated cellulose nanofiber, and a decrease in dispersion stability may occur. It is preferable that the blending amount of the water-soluble polymer is 25% by mass or more, since particularly excellent redispersibility can be obtained. In addition, in consideration of thixotropy, it is preferable that the blending amount is 200% by mass or less, and particularly preferably 60% by mass or less.
[0057] (Dry) A dispersion of carboxymethylated cellulose nanofibers, or a dispersion of carboxymethylated cellulose nanofibers mixed with a water-soluble polymer in some cases, is dried (to remove the dispersion medium) to obtain a dry solid material containing carboxymethylated cellulose nanofibers. In this case, it is preferable to adjust the pH of the dispersion to 9 to 11 before drying, since this improves redispersibility.
[0058] The drying method may be any known method, and is not particularly limited. For example, spray drying, squeezing, air drying, hot air drying, and vacuum drying may be used. The drying apparatus is not particularly limited, and may be a continuous tunnel drying apparatus, a band drying apparatus, a vertical drying apparatus, a vertical turbo drying apparatus, a multi-stage disk drying apparatus, an air drying apparatus, a rotary drying apparatus, an air flow drying apparatus, a spray dryer drying apparatus, a spray drying apparatus, a cylindrical drying apparatus, a drum drying apparatus, a belt drying apparatus, a screw conveyor drying apparatus, a rotary drying apparatus with a heating tube, a vibration transport drying apparatus, a batch type box drying apparatus, an air drying apparatus, a vacuum box drying apparatus, and an agitation drying apparatus, etc., which may be used alone or in combination of two or more.
[0059] Among these, the use of an apparatus for forming a thin film and drying is preferred from the viewpoint of energy efficiency, since it can uniformly supply heat energy directly to the material to be dried and can perform the drying process more efficiently and in a short time. In addition, an apparatus for forming a thin film and drying is also preferred because it can immediately recover the dried material by a simple means such as scraping off the thin film. Furthermore, it has been found that the redispersibility is further improved when the thin film is formed and then dried. Examples of an apparatus for forming a thin film and drying include a drum drying apparatus and a belt drying apparatus that form a thin film on a drum or belt using a blade or die, etc., and then dry the thin film. The thickness of the thin film when forming and drying the thin film is preferably 50 μm to 1000 μm, and more preferably 100 μm to 300 μm. If it is 50 μm or more, it is easy to scrape off after drying, and if it is 1000 μm or less, the effect of further improving the redispersibility is observed.
[0060] The residual moisture content after drying is preferably 2% by mass to 15% by mass based on the total dried product.
[0061] (Crushing) The pulverization method is not particularly limited, and a known method can be used, including a dry pulverization method in which the material is treated in a powder state and a wet pulverization method in which the material is treated in a dispersed or dissolved state in a liquid. When wet pulverization is performed, it may be performed before the above-mentioned drying.
[0062] Examples of the equipment used in the dry grinding method include, but are not limited to, a cutting mill, an impact mill, an airflow mill, and a media mill. These can be used alone or in combination, and can be used in several stages with the same model. Among these, an airflow mill is preferred. Examples of cutting mills include a mesh mill (manufactured by HORAI Co., Ltd.), Atoms (manufactured by Yamamoto Hyakuma Seisakusho Co., Ltd.), a knife mill (manufactured by Parman Co., Ltd.), a granulator (manufactured by Herbolt Co., Ltd.), and a rotary cutter mill (manufactured by Nara Machinery Co., Ltd.). Examples of impact mills include Pulperizer (manufactured by Hosokawa Micron Corporation), Fine Impact Mill (manufactured by Hosokawa Micron Corporation), Super Micron Mill (manufactured by Hosokawa Micron Corporation), Sample Mill (manufactured by Seishin Corporation), Bantam Mill (manufactured by Seishin Corporation), Atomizer (manufactured by Seishin Corporation), Tornado Mill (Nikkiso Co., Ltd.), Turbo Mill (Turbo Kogyo Co., Ltd.), Bevel Impactor (Aikawa Iron Works Co., Ltd.), etc. Examples of airflow mills include CGS type jet mill (manufactured by Mitsui Mining Co., Ltd.), jet mill (manufactured by Sansho Industry Co., Ltd.), Ebara Jet Micronizer (manufactured by Ebara Corporation), Selenium Mirror (manufactured by Masuko Sangyo Co., Ltd.), Supersonic Jet Mill (manufactured by Nippon Pneumatic Mfg. Co., Ltd.), etc. Examples of media mills include vibration ball mills, etc. Examples of the apparatus used in the wet grinding method include a mass colloider (manufactured by Masuko Sangyo Co., Ltd.), a high pressure homogenizer (manufactured by Sanmaru Kikai Kogyo Co., Ltd.), and a media mill. An example of the media mill is a bead mill (manufactured by Imex Co., Ltd.).
[0063] (classification) After pulverization of the carboxymethylated cellulose nanofibers, classification is performed to adjust the particle size to a specific size. The classification method is not particularly limited, but can be performed, for example, by passing the nanofibers through a mesh (sieve) having a predetermined mesh size. As the mesh, preferably 20 to 400 mesh, more preferably 40 to 300 mesh, and even more preferably 60 to 200 mesh can be used, and these may be used in a multi-stage manner. The median diameter of the powder finally obtained is 10.0 μm to 150.0 μm, preferably 30.0 μm to 130.0 μm, and even more preferably 50.0 μm to 120.0 μm.
[0064] In the present invention, the amount of carboxymethylated cellulose nanofibers applied to the surface of bread is, in terms of solid content, 0.01 mass% or more relative to the solid content of the bread from the viewpoint of film-forming properties and 1 mass% or less from the viewpoint of ease of handling, preferably 0.02 mass% or more and 0.8 mass% or less, and more preferably 0.05 mass% or more and 0.5 mass% or less.
[0065] (Bread manufacturing method) An example of a method for producing breads of the present invention is a method for applying an aqueous dispersion of a composition containing carboxymethylated cellulose nanofibers to the surface of fermented bread dough before baking using a brush or the like. From the viewpoint of ease of handling, the concentration of the aqueous dispersion of the composition containing carboxymethylated cellulose nanofibers is preferably 0.1 to 2.0 mass%, more preferably 0.5 to 1.0 mass%, in terms of the solid content concentration of carboxymethylated cellulose nanofibers. The amount of the composition containing carboxymethylated cellulose nanofibers to be applied is, in terms of the solid content of carboxymethylated cellulose nanofibers, 1 cm of the dough surface area (top surface only). 2 The range of 0.00005 to 0.02 g per unit is preferable, and the range of 0.0005 to 0.002 g per unit is more preferable.
[0066] In the present invention, bread refers to breads made from cereal flour such as wheat flour (including starch and gluten) as the main ingredient, with water, foaming agents (yeast, baking soda, etc.), salt, sugar, dairy products, egg products, edible oils and fats as secondary ingredients, which are kneaded together and fermented, shaped, and then heated by baking, steaming, frying, etc. Examples of breads include white breads such as Pullman, French breads such as baguettes and batards, rolls such as sweet rolls and table rolls, sweet breads such as croissants, Danish pastries, and yeast donuts, and hotcakes.
[0067] The bread of the present invention has a composition containing carboxymethylated cellulose nanofibers applied to its surface, and the amount of the carboxymethylated cellulose nanofibers applied is 0.01% by mass or more and 1% by mass or less of the solid content of the bread, so that the amount of crumbs produced when the bread is cut or torn is small. In the present invention, it is presumed that the surface of the bread is protected by a coating layer containing carboxymethylated cellulose nanofibers, and the collapse of the crust is suppressed. EXAMPLES
[0068] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0069] (Method for measuring degree of carboxymethyl substitution) 1) Approximately 2.0 g of carboxymethylated cellulose fiber (bone dry) was weighed out and placed in a 300 mL Erlenmeyer flask equipped with a stopper. 2) 100 mL of a solution of 1000 mL of nitric acid methanol and 100 mL of special-grade concentrated nitric acid was added, and the mixture was shaken for 3 hours to convert the carboxymethyl cellulose salt (carboxymethyl cellulose) into hydrogen-type carboxymethyl cellulose. 3) 1.5 to 2.0 g of hydrogenated carboxylated cellulose (bone dry) was weighed out and placed in a 300 mL Erlenmeyer flask equipped with a stopper. 4) The hydrogenated carboxylated cellulose was moistened with 15 mL of 80% methanol, 100 mL of 0.1 N NaOH was added, and the mixture was shaken at room temperature for 3 hours. 5) Excess NaOH was back-titrated with 0.1N H2SO4 using phenolphthalein as an indicator. 6) The degree of carboxymethyl substitution (DS) was calculated by the following formula: A = [(100 × F'-(0.1N H2SO4) (mL) × F) × 0.1] / (bone-dry mass of hydrogenated carboxylated cellulose (g)) DS = 0.162 x A / (1-0.058 x A) A: The amount of 1N NaOH required to neutralize 1 g of hydrogenated carboxymethyl cellulose (mL) F': Factor of 0.1N H2SO4 F: Factor of 0.1N NaOH
[0070] (Method of measuring average fiber diameter and aspect ratio) The average fiber diameter and average fiber length of cellulose nanofibers (CNF) were analyzed using an atomic force microscope (AFM) for 200 randomly selected fibers. The aspect ratio was calculated using the following formula. Aspect ratio = average fiber length / average fiber diameter
[0071] Example 1 (Production of carboxymethylated cellulose nanofibers) In a 5L twin-shaft kneader with the rotation speed adjusted to 100 rpm, 1089 parts of isopropanol (IPA) and 31 parts of sodium hydroxide dissolved in 121 parts of water were added, and 200 parts of hardwood pulp (LBKP, manufactured by Nippon Paper Industries Co., Ltd.) were added in terms of dry mass when dried at 100 ° C for 60 minutes. The mixture was stirred and mixed at 30 ° C for 60 minutes to prepare mercerized cellulose. 117 parts of sodium monochloroacetate were further added while stirring, and after stirring at 30 ° C for 30 minutes, the mixture was heated to 70 ° C over 30 minutes and carboxymethylation reaction was carried out at 70 ° C for 60 minutes. The proportion of water in the reaction medium during the mercerization reaction and the carboxymethylation reaction was 10 mass%. After the reaction was completed, the mixture was neutralized, washed with 65% water-containing methanol, deliquored, dried, and pulverized to obtain a sodium salt of carboxymethylated cellulose with a carboxymethyl substitution degree of 0.27 and a crystallinity of cellulose I type of 64%. The methods for measuring the degree of carboxymethyl substitution and the crystallinity of cellulose type I are as described above.
[0072] The obtained sodium salt of carboxymethyl cellulose was dispersed in water to obtain a 1% (w / v) aqueous dispersion. This was treated three times with a high-pressure homogenizer at 150 MPa to obtain a dispersion of carboxymethyl cellulose nanofibers. The obtained carboxymethyl cellulose nanofibers had an average fiber diameter of 3.2 nm and an aspect ratio of 40.
[0073] (Production of CNF powder 1) The obtained carboxymethylated cellulose nanofibers were dispersed in water to a solid content of 0.7% by mass, and carboxymethyl cellulose (manufactured by Nippon Paper Industries Co., Ltd., product name: F350HC-4, viscosity (1% by mass, 25°C, 60 rpm) approximately 3000 mPa·s, degree of carboxymethyl substitution approximately 0.90) (CMC) was added in an amount of 40% by mass relative to the carboxymethyl cellulose nanofibers (i.e., so that the solid content of carboxymethyl cellulose was 40 parts by mass when the solid content of the carboxymethylated cellulose nanofibers was 100 parts by mass), and the mixture was stirred for 60 minutes with a TK homomixer (12,000 rpm).
[0074] To this dispersion, 0.5% by mass of sodium hydroxide solution was added to adjust the pH to 9, and then the mixture was applied to the drum surface of a drum dryer D0405 (manufactured by Katsuragi Kogyo Co., Ltd.) and dried at 140°C for 1 minute. The resulting dried product was scraped off and then pulverized using an impact mill at a rate of 10 kg per hour to obtain a dried pulverized product with a moisture content of 5% by mass. The pulverized product was classified using a 30 mesh to obtain a powder (CNF powder 1) containing carboxymethylated cellulose nanofibers (CM-CNF) and carboxymethyl cellulose (CMC).
[0075] (French bread manufacturing) Frozen French bread dough was thawed, and 45 g of the dough (solid content: 28 g) was dispensed and shaped, and then fermented at 40°C for 1 hour.
[0076] Water was added to the fermented dough so that the CNF solid concentration was 1% by mass per 1 part CNF powder, and the dough was stirred for 30 minutes using a homodisper. 2 to 3 g of the resulting CNF dispersion was then applied using a brush, and the dough was placed in an oven and baked at 210°C for 1 hour to produce French bread.
[0077] Comparative Example 1 French bread was produced in the same manner as in Example 1, except that a dispersion containing carboxymethyl cellulose (manufactured by Nippon Paper Industries Co., Ltd., product name: F350HC-4) and a CMC solids concentration of 1 mass% was used instead of the CNF dispersion.
[0078] Comparative Example 2 French bread was produced in the same manner as in Example 1, except that water was applied to the fermented dough instead of the CNF dispersion.
[0079] (Reference example) French bread was produced in the same manner as in Example 1, except that nothing was applied to the dough after fermentation.
[0080] For the French bread produced in the Examples, Comparative Examples, and Reference Examples, the weight loss rate (%) before and after baking was measured, and the bread crumbs that were generated when the bread was torn into eight equal pieces by hand were observed. The smaller the weight loss rate, the higher the water retention effect. The measurement results of the weight loss rate are shown in Table 1. The observation results of the bread crumbs for Example 1, Comparative Example 1, Comparative Example 2, and Reference Example are shown in Figures 1 to 4, respectively.
[0081] [Table 1]
[0082] As can be seen from the results in Table 1 and Figures 1 to 4, breads in which the composition containing carboxymethylated CNF of Example 1 was applied to the surface of breads and the amount of the carboxymethylated CNF applied was 0.01% by mass or more and 1% by mass or less of the solid content of the breads, had reduced crumbs when torn by hand, compared to breads produced by baking dough coated with a dispersion containing only CMC of Comparative Example 1. Furthermore, the breads of Example 1 had excellent water retention during baking and significantly reduced crumbs when torn by hand, compared to breads produced by baking dough coated with only water of Comparative Example 2 and breads produced by baking dough without any coating of Reference Example.
Claims
1. Breads comprising a composition containing carboxymethylated cellulose nanofibers applied to the surface of the breads, the amount of the carboxymethylated cellulose nanofibers applied being, in terms of solid content, 0.01% by mass or more and 1% by mass or less relative to the solid content of the breads.
2. The carboxymethylated cellulose nanofiber has a degree of carboxymethyl substitution per anhydrous glucose unit of the cellulose nanofiber of 0.01 to 0.50, and a crystallinity of cellulose type I of 40% or more.
3. The bread according to claim 1 or 2, further comprising carboxymethylcellulose.
Citation Information
Patent Citations
Method for producing confectionery or bread attached with chocolate
JP2007006787A
Hydrous chocolates
JP2017209086A
Plastic oil / fat composition and food product
JP2018068128A
Additive containing carboxymethylated cellulose nanofiber
JP2019206521A
Bread crust separation inhibitor and method of preventing separation of bread crust
JP2020156319A