Decorative films and airbags
A styrenic resin-based decorative film with controlled elongation and stress differences ensures easy one-direction breakage, addressing deployment and opening needs while maintaining aesthetic and functional integrity.
Patent Information
- Application Number
- JP2021039942
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-12
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2041-03-12
AI Technical Summary
Decorative films that hinder airbag deployment and door opening are not easily breakable in one direction, and there is a need for a film that can be easily torn in one direction to enhance the sense of luxury and functionality in vehicles.
A decorative film with a styrenic resin layer having specific elongation and orientation relaxation stress differences in the machine and transverse directions, combined with optional PMMA and printing layers, ensuring easy breakage in one direction.
The film can be easily broken in one direction, allowing airbag deployment and door opening without interference, while maintaining decorative appeal and impact resistance.
Smart Images

Figure 0007583652000003 
Figure 0007583652000001 
Figure 0007583652000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a decorative film and an airbag. [Background technology]
[0002] Airbags installed in automobiles and the like deploy quickly in an emergency to absorb impact. Because airbags need to deploy quickly in an emergency, no decorative film that may impede deployment has been attached to the deployment portion of the airbag in the past. However, in recent years, in order to increase the sense of luxury inside the vehicle, it has been desired to attach a decorative film to the deployment portion of the airbag as well. The decorative film is required to break easily in one direction when the airbag deploys, and not to impede the deployment of the airbag.
[0003] In addition, in some cases, a decorative film is attached to a gap in a door that is normally kept closed in order to prevent sand, insects, etc. from entering through the gap. Even when such a door needs to be opened, the decorative film is required to be easily torn in one direction when the door is opened so that the door can be opened easily.
[0004] Patent Document 1 discloses a composite film for in-mold decoration, in which at least the upper and lower outermost layers are made of a styrene-based resin layer and a decorated polybutylene terephthalate-based resin layer, respectively, as a decorative film. Meanwhile, Patent Documents 2 to 6 disclose films or sheets containing a styrene-based resin. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 10-272652 [Patent Document 2] JP 2007-269913 A [Patent Document 3] Patent No. 6389574 [Patent Document 4] Patent No. 6190542 [Patent Document 5] Patent No. 6190541 [Patent Document 6] Patent No. 6148411 Summary of the Invention [Problem to be solved by the invention]
[0006] However, the decorative film disclosed in Patent Document 1 does not easily break in one direction when a force is applied, and further improvement is desired. An object of the present invention is to provide a decorative film that can be easily broken in one direction, and an airbag including the decorative film. [Means for solving the problem]
[0007] The present invention includes the following embodiments.
[0008] [1] A decorative film having a styrene-based resin layer containing a styrene-based resin, The styrene-based resin layer has a breaking elongation of 15% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%, A decorative film, in which the difference (AB) between the orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and the orientation relaxation stress (B) in the TD direction of the styrene-based resin layer at a temperature of 23°C and a relative humidity of 50% is 0.15 MPa or more.
[0009] [2] The decorative film according to [1], wherein the tensile elongation at break in the MD and TD directions of the styrene-based resin layer is 7% or less at a temperature of 23°C and a relative humidity of 50%.
[0010] [3] The decorative film according to [1] or [2], wherein the difference (AB) between the orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and the orientation relaxation stress (B) in the TD direction of the styrene-based resin layer exceeds 0.3 MPa at a temperature of 23°C and a relative humidity of 50%.
[0011] [4] The decorative film according to any one of [1] to [3], wherein the styrene-based resin comprises a homopolymer of a styrene-based monomer, or a copolymer of a styrene-based monomer and at least one monomer selected from the group consisting of (meth)acrylic acid, (meth)acrylic acid esters, maleic anhydride, unsaturated dicarboxylic acids, N-phenylmaleimide, and acrylonitrile.
[0012] [5] The decorative film according to any one of [1] to [4], wherein the styrene-based resin contains at least one resin selected from the group consisting of high impact polystyrene (HIPS) and styrene-butadiene block copolymers.
[0013] [6] The decorative film according to any one of [1] to [5], further comprising a PMMA layer containing polymethyl methacrylate resin (PMMA).
[0014] [7] The decorative film according to any one of [1] to [6], which has an impact resistance of 5 J / mm or less as measured using a film impact tester at a temperature of 23°C and a relative humidity of 50%.
[0015] [8] An airbag equipped with a decorative film according to any one of [1] to [7]. Effect of the Invention
[0016] According to the present invention, it is possible to provide a decorative film that can be easily torn in one direction, and an airbag including the decorative film. [Brief description of the drawings]
[0017] [Figure 1] FIG. 2 is a schematic diagram showing a method for evaluating the fracture direction in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] [Decorative film] The decorative film according to the present embodiment includes a styrene-based resin layer containing a styrene-based resin. Here, the MD and TD breaking elongations of the styrene-based resin layer at a temperature of 23° C. and a relative humidity of 50% are 15% or less. That is, at a temperature of 23° C. and a relative humidity of 50%, the MD breaking elongation of the styrene-based resin layer (hereinafter also referred to as MD breaking elongation) is 15% or less, and the TD breaking elongation of the styrene-based resin layer (hereinafter also referred to as TD breaking elongation) is 15% or less. In addition, the difference (AB) between the MD orientation relaxation stress (A) of the styrene-based resin layer (hereinafter also referred to as MD orientation relaxation stress (A)) and the TD orientation relaxation stress (B) of the styrene-based resin layer (hereinafter also referred to as TD orientation relaxation stress (B)) at a temperature of 23° C. and a relative humidity of 50% is 0.15 MPa or more.
[0019] The present inventors have found that the decorative film is easily broken in one direction when a force is applied by providing a styrene-based resin layer. This is presumed to be due to the low tear strength of the styrene-based resin layer. In particular, the present inventors have found that the decorative film is more easily broken in one direction when broken when the styrene-based resin layer has an MD-direction orientation relaxation stress (A) and a TD-direction orientation relaxation stress (B) that satisfy the relationship AB≧0.15MPa. This is presumed to be because the molecules are more oriented in the MD direction than in the TD direction, so the film strength in the MD direction is stronger and less likely to break, and breaks in the TD direction where the film strength is weaker. The present inventors have also found that the decorative film can be easily broken with a small force when the airbag is deployed or the door is opened when both the MD-direction breaking elongation and the TD-direction breaking elongation of the styrene-based resin layer are 15% or less.
[0020] In addition, "MD direction" means the machine direction, and "MD direction" means the direction that coincides with the flow direction of the resin. In addition, in "TD direction", TD means the transverse direction, and "TD direction" means the direction perpendicular to the MD direction.
[0021] The decorative film according to this embodiment can include other layers such as a PMMA layer containing polymethyl methacrylate resin (PMMA) and a printing layer for decoration, in addition to the styrene-based resin layer. The thickness of the decorative film according to this embodiment is not particularly limited, but can be, for example, 50 to 100 μm. The decorative film according to this embodiment is particularly useful as a decorative film for an airbag, which is provided on the deployment portion of the airbag.
[0022] The decorative film according to this embodiment preferably has an impact resistance of 5 J / mm or less, more preferably 4 J / mm or less, and even more preferably 3.5 J / mm or less, as measured using a film impact tester at a temperature of 23°C and a relative humidity of 50%. When the impact resistance is 5 J / mm or less, the decorative film can be easily broken with a small force. The impact resistance is measured by the following method using a film impact tester (manufactured by Toyo Seiki Seisakusho Co., Ltd.) at a temperature of 23°C and a relative humidity of 50%. The decorative film is cut into a predetermined size, set in the film impact tester, and a hemispherical impact ball is passed through the decorative film from a lifting height of 90 degrees, and the amount of work at that time is measured.
[0023] (Styrene-based resin layer) <Breaking elongation in MD direction and TD direction> In the styrene resin layer included in the decorative film according to this embodiment, the elongation at break in the MD direction is 15% or less, and the elongation at break in the TD direction is 15% or less. By having both the elongation at break in the MD direction and the elongation at break in the TD direction be 15% or less, the decorative film can be easily broken with a small force. It is preferable that both the elongation at break in the MD direction and the elongation at break in the TD direction be 10% or less, more preferably both be 7% or less, and even more preferably both be 5% or less. The lower limit of the range of the elongation at break in the MD direction and the elongation at break in the TD direction is not particularly limited, but for example, both can be 1% or more. For example, by increasing the content of polystyrene in the styrene resin layer, both the elongation at break in the MD direction and the elongation at break in the TD direction of the styrene resin layer can be adjusted to 15% or less. Note that the elongation at break in the MD direction and the elongation at break in the TD direction may be the same or different. The elongation at break in the MD direction and the elongation at break in the TD direction are values measured at a temperature of 23°C and a relative humidity of 50% in accordance with JIS-C-2151 and ASTM-D-882.
[0024] <MD direction, TD direction orientation relaxation stress> In the styrene resin layer included in the decorative film according to this embodiment, the difference (A - B) between the orientation relaxation stress (A) in the MD direction and the orientation relaxation stress (B) in the TD direction is 0.15 MPa or more. By having the difference be 0.15 MPa or more, the decorative film is likely to break in one direction at the time of breakage. The difference is preferably more than 0.3 MPa, more preferably 0.35 MPa or more, and even more preferably 0.5 MPa or more. When the difference exceeds 0.3 MPa, the decorative film is particularly likely to break in one direction at the time of breakage. The upper limit of the range of the difference is not particularly limited, but for example, it can be 10 MPa or less. For example, by increasing the difference in the draw ratio between the MD direction and the TD direction, the difference (A - B) between the orientation relaxation stress (A) in the MD direction and the orientation relaxation stress (B) in the TD direction of the styrene resin layer can be adjusted to 0.15 MPa or more.
[0025] The MD orientation relaxation stress (A) is not particularly limited as long as the difference (AB) between the MD orientation relaxation stress (A) and the TD orientation relaxation stress (B) is 0.15 MPa or more, but may be, for example, 0.3 to 2.0 MPa, and preferably 0.5 to 1.5 MPa. The TD orientation relaxation stress (B) is not particularly limited as long as the difference (AB) between the MD orientation relaxation stress (A) and the TD orientation relaxation stress (B) is 0.15 MPa or more, but may be, for example, 0.1 to 0.5 MPa, and preferably 0.15 to 0.4 MPa. The MD orientation relaxation stress (A) and the TD orientation relaxation stress (B) are measured according to ASTM D1504 by adopting the peak stress value in silicone oil set at 30°C higher than the Vicat softening temperature of the resin composition constituting the sheet.
[0026] <Styrene-based resin> The styrene-based resin layer of the decorative film according to the present embodiment includes a styrene-based resin. The styrene-based resin may include a homopolymer or copolymer of a styrene-based monomer. Examples of the styrene-based monomer include styrene and α-methylstyrene. Examples of the copolymer of a styrene-based monomer include copolymers of a styrene-based monomer with (meth)acrylic acid, (meth)acrylic acid ester, maleic anhydride, unsaturated dicarboxylic acid, N-phenylmaleimide, acrylonitrile, and the like.
[0027] The styrene resin may contain a styrene graft polymer obtained by graft polymerization of a styrene monomer with a rubber component, a block copolymer obtained by anion polymerization of a diene monomer with a styrene monomer, and the like. Examples of the styrene graft polymer include high impact polystyrene (HIPS), acrylonitrile-butadiene-styrene graft copolymer (ABS resin), and acrylonitrile-(meth)acrylic acid ester-styrene graft copolymer. Examples of the block copolymer include styrene-butadiene block copolymer. Among these, high impact polystyrene and styrene-butadiene block copolymers are preferred because they have high compatibility with homopolymers or copolymers of styrene monomers when used in combination with homopolymers or copolymers of styrene monomers. As the styrene resin, these resins may be used alone or in combination of two or more.
[0028] Among these, polystyrene (styrene resin) is preferable as the styrene-based resin, from the viewpoint that the decorative film is more likely to break in one direction when a force is applied thereto.
[0029] The styrene resin preferably contains 70 to 97% by mass, and more preferably 75 to 97% by mass, of structural units based on styrene monomers relative to the total structural units. The molecular weight of the styrene resin is not particularly limited as long as it provides sufficient melt viscosity when formed into a film.
[0030] <Other ingredients> From the viewpoint of thermal stability and weather resistance, the styrene-based resin layer preferably further contains an antioxidant. Examples of the antioxidant include triethylene glycol-bis[3-(3-t-butyl-5-methyl-4-hydroxyphenyl)propionate], 2,4-bis(n-octylthio)-6-(4-hydroxy-3,5-di-t-butylanilino)-1,3,5-triazine, pentaerythrityl tetrakis[3-(3,5-di-t-butyl-4-hydroxyphenyl)propionate], octadecyl-3-(3,5-di-t-butyl-4-hydroxyphenyl)propionate, and the like. phenolic antioxidants such as 2,2-thiobis(4-methyl-6-t-butylphenol)propionate, 2,2-thiobis(4-methyl-6-t-butylphenol) and 1,3,5-trimethyl-2,4,6-tris(3,5-di-t-butyl-4-hydroxybenzyl)benzene, ditridecyl-3,3'-thiodipropionate, dilauryl-3,3'-thiodipropionate, ditetradecyl-3,3'-thiodipropionate, distearyl-3,3'-thiodipropionate, propionate, dioctyl-3,3'-thiodipropionate and other sulfur-based antioxidants, trisnonylphenyl phosphite, 4,4'-butylidene-bis(3-methyl-6-t-butylphenyl-di-tridecyl) phosphite, (tridecyl)pentaerythritol diphosphite, bis(octadecyl)pentaerythritol diphosphite, bis(di-t-butylphenyl)pentaerythritol diphosphite, bis(di- Examples of phosphorus-based antioxidants include t-butyl-4-methylphenyl)pentaerythritol diphosphite, dinonylphenyl octyl phosphonite, tetrakis(2,4-di-t-butylphenyl)1,4-phenylene-diphosphonite, tetrakis(2,4-di-t-butylphenyl)4,4'-biphenylene-diphosphonite, and 10-decyloxy-9,10-dihydro-9-oxa-10-phosphaphenanthrene. The styrene-based resin layer may also contain a phenol-based, amine-based, phosphorus-based, hindered amine-based, or other stabilizer.
[0031] <Other physical properties, etc.> The styrene resin layer preferably has an impact resistance of 5 J / mm or less, more preferably 4 J / mm or less, and even more preferably 3.5 J / mm or less, measured using a film impact tester at a temperature of 23° C. and a relative humidity of 50%. When the impact resistance is 5 J / mm or less, the decorative film can be easily broken with a small force. The impact resistance is measured by the method described above. The thickness of the styrene resin layer is not particularly limited, but can be, for example, 30 to 100 μm.
[0032] The styrene-based resin layer may be, for example, a stretched film in which a composition containing a styrene-based resin is stretched in the MD direction and then in the TD direction. The stretching ratios in the MD direction and the TD direction are not particularly limited, but for example, the stretching ratio in the MD direction may be 3 to 6 times, and the stretching ratio in the TD direction is preferably 2 to 5 times.
[0033] (PMMA layer) The decorative film according to the present embodiment preferably further comprises a PMMA layer containing polymethyl methacrylate resin (PMMA) in addition to the styrene-based resin layer. When the decorative film comprises a PMMA layer, weather resistance is improved. The PMMA layer may contain, in addition to PMMA, for example, acrylic rubber. The PMMA layer preferably contains 80% by mass or more of PMMA, more preferably 90% by mass or more, and even more preferably 95% by mass or more. The PMMA layer may be made of PMMA. The thickness of the PMMA layer is not particularly limited, but may be, for example, 30 to 70 μm.
[0034] (Printing layer) The decorative film according to the present embodiment may include a printing layer for decoration. Printing may be performed on any part other than the outermost surface. For example, printing may be performed on the surface opposite to the outermost surface of the styrene resin layer.
[0035] (Method of manufacturing decorative film) The method for producing the decorative film according to the present embodiment is not particularly limited, but for example, the film can be produced by the following method. The composition containing the styrene-based resin is successively stretched in the MD direction and the TD direction in this order to produce a stretched film that becomes a styrene-based resin layer. The stretching ratios in the MD direction and the TD direction are not particularly limited, but for example, the stretching ratio in the MD direction can be 3 to 6 times and the stretching ratio in the TD direction can be 2 to 5 times, and it is preferable that the stretching ratio in the MD direction is 4 to 6 times and the stretching ratio in the TD direction is 2 to 4 times. The temperature during stretching can be 120 to 130°C. A printing layer is formed on one surface of the stretched film. One surface of the stretched film on which the printing layer is formed and one surface of the PMMA layer are dry laminated using an adhesive to produce a decorative film having a PMMA layer / printing layer / styrene-based resin layer configuration.
[0036] [Airbag] The airbag according to the present embodiment includes the decorative film according to the present embodiment at the opening. Since the airbag includes the decorative film according to the present embodiment, the airbag has a good appearance, and when the airbag is deployed, the decorative film is easily torn in one direction, so that the deployment of the airbag is not hindered. The decorative film according to the present embodiment can be provided on the deployment portion of the airbag. EXAMPLES
[0037] Hereinafter, the embodiment of the present invention will be described in more detail with reference to examples, but the present invention is not limited to these examples. The physical properties of the stretched film (styrene-based resin layer) and the decorative film were measured and evaluated by the following methods.
[0038] [MD and TD elongation at break] The MD and TD breaking elongation of the stretched film (styrene-based resin layer) were measured under conditions of 23° C. and 50% relative humidity in accordance with JIS-C-2151 or ASTM-D-882.
[0039] [MD and TD orientation relaxation stress] The MD orientation relaxation stress (A) and TD orientation relaxation stress (B) of the stretched film (styrene-based resin layer) were measured as peak stress values in silicone oil set at 30°C higher than the Vicat softening temperature of the resin composition constituting the sheet in accordance with ASTM D1504.
[0040] [Impact resistance] The impact resistance of the stretched film (styrene-based resin layer) and the decorative film was measured by the above-mentioned method using a film impact tester (manufactured by Toyo Seiki Seisakusho Co., Ltd.) at a temperature of 23° C. and a relative humidity of 50%.
[0041] [Fracture direction] As shown in FIG. 1, a film 1 (a stretched film (styrene resin layer) or a decorative film) measuring 20 cm in length and 20 cm in width was attached to the top of a double-leaf door 2. At this time, the film 1 was attached so that the MD direction 3 of the film 1 was parallel to the opening line 4 of the door 2 and the center of the film 1 was on the opening line 4. After that, a 5 kg spherical weight was dropped from a height of 0.5 m from the back side of the door 2 to which the film 1 was not attached, opening the door 2 and breaking the film 1. The breaking of the broken film 1 was visually observed and evaluated according to the following criteria. If the film was rated as "A" or "B", it was effective for use in the deployment part of an airbag, etc., because it broke in a straight line when force was applied. In addition, this evaluation was performed at a temperature of 23°C and a relative humidity of 50%. A: It cut straight without any forks. B: The cut is straight and directional, but branches are formed at the cut part. C: Cut in a curved line. D: It had no direction and cut in various directions.
[0042] [Example 1] (Preparation of Stretched Film 1 (Styrene-Based Resin Layer)) A styrene resin (product name: HRM61, manufactured by Toyo Styrene Co., Ltd.) was stretched at 130°C in the MD direction and then in the TD direction to produce a stretched film 1 that would become a styrene-based resin layer. The stretching ratio in the MD direction was 3 times, and the stretching ratio in the TD direction was 2 times. The thickness of the stretched film 1 was 50 μm. The physical properties of the stretched film 1 were measured and evaluated by the methods described above. The results are shown in Table 1.
[0043] (Creating decorative film) A printed layer was formed on one side of the stretched film 1 by gravure printing. This produced a decorative film. The decorative film was subjected to impact resistance measurement and evaluation of the breaking direction by the above-mentioned method. The results are shown in Table 2.
[0044] [Examples 2 to 5] In producing the stretched films, stretched films 2 to 5 were produced in the same manner as in Example 1, except that the stretch ratios in the MD and TD directions were changed as shown in Table 1, and the physical properties were measured and evaluated. The results are shown in Table 1. In addition, decorative films were produced in the same manner as in Example 1 using stretched films 2 to 5, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0045] [Example 6] Stretched film 6 was produced in the same manner as stretched film 2, except that the styrene-based resin was changed to a styrene-butadiene block copolymer (product name: Asaflex 805, manufactured by Asahi Kasei Corporation), and each physical property was measured and evaluated. The results are shown in Table 1. In addition, a decorative film was produced using stretched film 6 in the same manner as in Example 1, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0046] [Example 7] Stretched film 1 was prepared in the same manner as in Example 1, and a printed layer was formed on one surface of stretched film 1. A PMMA film (trade name: Technoloy S000 (thickness: 30 μm), manufactured by Sumitomo Chemical Co., Ltd.) was dry laminated to one surface of stretched film 1 on which the printed layer was formed, using an adhesive (trade name: AD-393 / CAT-EP1, manufactured by Toyo-Morton Co., Ltd.), to prepare a decorative film. The impact resistance and breaking direction of the decorative film were measured by the above-mentioned method. The results are shown in Table 2.
[0047] [Example 8] A decorative film was produced in the same manner as in Example 7, except that Stretched Film 2 was used instead of Stretched Film 1, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0048] [Comparative Example 1] Stretched film 7 was produced in the same manner as in Example 1, except that in the production of the stretched film, simultaneous biaxial stretching was performed instead of sequential stretching at the stretch ratio shown in Table 1, and each physical property was measured and evaluated. The results are shown in Table 1. In addition, a decorative film was produced using stretched film 7 in the same manner as in Example 1, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0049] [Comparative Example 2] In the preparation of the stretched film, a stretched film 8 was prepared in the same manner as in Comparative Example 1, except that the stretch ratios in the MD and TD directions were changed as shown in Table 1, and the physical properties were measured and evaluated. The results are shown in Table 1. In addition, a decorative film was prepared using the stretched film 8 in the same manner as in Comparative Example 1, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0050] [Comparative Example 3] In producing the stretched film, a stretched film 9 was produced in the same manner as in Comparative Example 1, except that a mixture of styrene resin (product name: HRM61, manufactured by Toyo Styrene Co., Ltd.) and high impact polystyrene (product name: E640N, manufactured by Toyo Styrene Co., Ltd.) (HRM61:E640N = 8:2 (mass ratio)) was used as the styrene-based resin, and the physical properties were measured and evaluated. The results are shown in Table 1. In addition, a decorative film was produced using stretched film 9 in the same manner as in Comparative Example 1, and the impact resistance was measured and the breaking direction was evaluated. The results are shown in Table 2.
[0051] [Table 1]
[0052] [Table 2]
[0053] As shown in Table 2, the decorative films of Examples 1 to 8 according to this embodiment had low impact resistance and good evaluations of the breaking direction. Therefore, it was found that the decorative films according to this embodiment can be easily broken in one direction. In particular, the decorative films of Examples 1, 3 to 5, and 7, which use stretched films 1 and 3 to 5 in which the styrene-based resin layer is made of styrene resin and the difference (AB) between the MD orientation relaxation stress (A) and the TD orientation relaxation stress (B) exceeds 0.3 MPa, were all evaluated as "A" in the breaking direction, and it was found that they are more likely to break in one direction. [Explanation of symbols]
[0054] 1. Film (stretched film (styrene resin layer) or decorative film) 2 Doors 3 MD direction 4 Opening Line
Claims
1. A decorative film having a styrene-based resin layer containing a styrene-based resin, The styrene-based resin layer has a breaking elongation of 15% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%, A decorative film, in which the difference (A-B) between the orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and the orientation relaxation stress (B) in the TD direction of the styrene-based resin layer at a temperature of 23°C and a relative humidity of 50% exceeds 0.3 MPa.
2. A decorative film having a styrene-based resin layer containing a styrene-based resin, The styrene-based resin layer has a breaking elongation of 15% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%, the difference (A-B) between the orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and the orientation relaxation stress (B) in the TD direction of the styrene-based resin layer at a temperature of 23°C and a relative humidity of 50% is 0.15 MPa or more; The decorative film, wherein the styrene-based resin contains at least one resin selected from the group consisting of high impact polystyrene (HIPS) and a styrene-butadiene block copolymer.
3. A decorative film having a styrene-based resin layer containing a styrene-based resin, The styrene-based resin layer has a breaking elongation of 15% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%, the difference (A-B) between the orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and the orientation relaxation stress (B) in the TD direction of the styrene-based resin layer at a temperature of 23°C and a relative humidity of 50% is 0.15 MPa or more; The decorative film further comprises a PMMA layer comprising polymethyl methacrylate resin (PMMA).
4. The decorative film according to claim 1 , wherein the styrene-based resin layer has a breaking elongation of 7% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%.
5. The decorative film according to any one of claims 1 to 4, wherein the styrene-based resin comprises a homopolymer of a styrene-based monomer, or a copolymer of a styrene-based monomer and at least one monomer selected from the group consisting of (meth)acrylic acid, (meth)acrylic acid ester, maleic anhydride, unsaturated dicarboxylic acid, N-phenylmaleimide, and acrylonitrile.
6. 6. The decorative film according to claim 1, which has an impact resistance of 5 J / mm or less at a temperature of 23° C. and a relative humidity of 50% as measured using a film impact tester.
7. An airbag having a decorative film, The decorative film includes a styrene-based resin layer containing a styrene-based resin, The styrene-based resin layer has a breaking elongation of 15% or less in the MD and TD directions at a temperature of 23° C. and a relative humidity of 50%, The airbag has an orientation relaxation stress (A) in the MD direction of the styrene-based resin layer and an orientation relaxation stress (B) in the TD direction of the styrene-based resin layer, the difference (A-B) being 0.15 MPa or more at a temperature of 23°C and a relative humidity of 50%.
Citation Information
Patent Citations
Preparation of isotropic carbon material
JP1986048411A
Optical reception circuit
JP1986090541A
Frame aligner
JP1986090542A
Extensible paint composition
JP1988089574A
In-mold decorative film and molded article thereof
JP1998272652A