Display panel and manufacturing method thereof
Beveled weld pads with truncated pyramidal shapes in mini-LED display panels ensure complete curing of the reflective ink, enhancing reflectance and display performance while reducing energy consumption.
Patent Information
- Application Number
- JP2021577100
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-12-10
- Filing Date
- 2021-12-17
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2041-12-17
AI Technical Summary
The reflective ink in mini-LED display panels is not fully cured due to insufficient light irradiation, leading to undercut defects that reduce reflectance by 15% to 20%, thereby affecting display performance.
The display panel features beveled weld pads with truncated pyramidal shapes that reflect curing light to the bottom layer, ensuring complete curing of the reflective ink, using materials like copper, aluminum, and silver.
The solution enhances reflectance to over 92.5%, improving display brightness and reducing energy consumption by ensuring complete curing of the reflective layer.
Smart Images

Figure 0007583750000001 
Figure 0007583750000002 
Figure 0007583750000003
Abstract
Description
[Technical field]
[0001] The present invention relates to the technical field of displays, and in particular to display panels having highly reflective bevel weld pads. [Background technology]
[0002] With the development of display technology, various types of display panels have been developed. Compared with liquid crystal (LC) display technology and organic light-emitting diode (OLED) display technology, mini-light-emitting diode (mini-LED) display technology has advantages such as better response speed, display color gamut, contrast, resolution and power consumption performance, and the mini-LED display technology can also realize precise dimming of ultra-high number of sections, so it is expected to develop in the future and is a focus of development plans of each display panel manufacturer.
[0003] In order to improve the brightness and emission efficiency of the display panel using the mini light emitting diode display technology and reduce the energy consumption, the prior art applies a reflective ink to the surface of the driving substrate of the display panel so as to reflect the light emitted from the mini light emitting diode in the display panel as much as possible. The reflectance of the display panel can be adjusted by adjusting the coating thickness of the reflective ink and the accuracy of the window. At present, the most commonly used method for manufacturing the reflective ink is to apply the reflective ink to the driving substrate of the display panel by inkjet printing or screen printing, harden the reflective ink by exposure and development, and expose a number of welds for bonding the mini light emitting diodes by windowing. Summary of the Invention [Problem to be solved by the invention]
[0004] 1 is a schematic diagram of a part of the display panel of the prior art. The display panel includes a driving substrate 100, a number of welding pads 200, a reflective ink 300, and a number of mini light-emitting diodes 400. A pair of the welding pads 200 is electrically connected to one of the mini light-emitting diodes 400 and a number of wirings 110 on the driving substrate 100. The reflective ink 300 is located between two adjacent pairs of the welding pads 200 and is used to reflect the light emitted from the mini light-emitting diodes 400.
[0005] In the prior art, in order to improve the reflectance of the display panel as much as possible, the coating thickness of the reflective ink is designed to be about 60 microns. However, since the reflective ink 300 is a photo-curable material, the reflective ink 300 near the surface layer is completely cured by sufficient light irradiation, but the reflective ink 300 near the bottom layer is not completely cured by insufficient light irradiation. The reflective ink 300 that is not completely cured is washed away by a developer in the subsequent manufacturing process and disappears, and further forms an undercut shape UC shown in FIG. 1. According to the simulation test and calculation by the inventors, the reflectance of the display panel is reduced by 15% to 20% due to the defects of the undercut shape UC of the reflective ink 300, which greatly reduces the display effect of the display panel.
[0006] The display panel of the prior art has a technical problem in that the reflective ink cannot be cured sufficiently, so there is a demand for a display panel having a high reflectivity bevel welding pad to solve the technical problem. [Means for solving the problem]
[0007] The present invention provides a display panel with a highly reflective beveled weld pad. The display panel includes a drive substrate, a plurality of weld pads, a reflective layer, and a plurality of light-emitting units. The drive substrate includes a plurality of wirings of a drive circuit of the display panel. The plurality of weld pads are provided on the drive substrate and electrically connected to the plurality of wirings of the drive circuit of the drive substrate. The weld pads are provided in pairs of two. Each of the weld pads includes a truncated cone. The reflective layer is provided between two adjacent pairs of the weld pads. The material of the reflective layer includes a light-cured reflective ink. Each of the light-emitting units is electrically connected to one pair of the weld pads.
[0008] In one embodiment, the included angle between at least one side surface and a base surface of the truncated cone of each of the weld pads is between 40 degrees and 50 degrees.
[0009] In this embodiment, the included angle between at least one side and a base of the truncated cone of each of the weld pads is 45 degrees.
[0010] In one embodiment, each of the weld pads is a truncated pyramid or cone.
[0011] In one embodiment, the material of the plurality of weld pads includes copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
[0012] In one embodiment, the height of each of the weld pads is between 8 microns and 10 microns.
[0013] In this embodiment, the thickness of the reflective layer is between 55 microns and 60 microns.
[0014] The present invention further provides a method for manufacturing a display panel, the method comprising the steps of: forming a driving substrate, the driving substrate including a plurality of wirings of a driving circuit of the display panel; forming a plurality of weld pads on the drive board, the weld pads being electrically connected to the plurality of traces of the drive circuit of the drive board, the weld pads being provided in pairs, and each being formed as a truncated cone; forming a reflective layer on the driving substrate, the reflective layer being formed between two adjacent pairs of the welding pads, and a material of the reflective layer including a photocurable reflective ink; and electrically connecting a light emitting unit to each pair of the welding pads.
[0015] In one embodiment, the included angle between at least one side surface and a base surface of the truncated cone of each of the weld pads is between 40 degrees and 50 degrees.
[0016] In one embodiment, the included angle between at least one side and a base of the truncated cone of each of the weld pads is 45 degrees.
[0017] In one embodiment, each of the weld pads is a truncated pyramid or cone.
[0018] In one embodiment, the material of the plurality of weld pads includes copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
[0019] In one embodiment, the height of each of the weld pads is between 8 microns and 10 microns.
[0020] In this embodiment, the thickness of the reflective layer is between 55 microns and 60 microns.
[0021] In one embodiment, the step of forming a plurality of weld pads on the drive substrate further comprises: forming an electroplating seed layer on a surface of the driving substrate; forming a photoresist on the electroplating seed layer; patterning the photoresist to form a truncated cone cavity in an area where each of the weld pads is to be formed; electroplating the photoresist and the electroplating seed layer to form the weld pad filling the cavity in the photoresist; removing the photoresist; and etching the plurality of weld pads and the electroplating seed layer to remove the electroplating seed layer except for the areas where the plurality of weld pads are formed.
[0022] In one embodiment, the electroplating seed layer has a thickness between 0.5 microns and 1 micron.
[0023] In one embodiment, the electroplating seed layer material includes copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
[0024] In one embodiment, the photoresist material includes a negative photoresist.
[0025] In one embodiment, a depth of the cavity is greater than or equal to a height of each of the weld pads, and a difference between the depth of the cavity and the height of each of the weld pads is between 0 microns and 5 microns.
[0026] In one embodiment, the photoresist has a thickness between 10 microns and 12 microns. Effect of the Invention
[0027] The present invention provides the display panel and the manufacturing method thereof. The display panel includes the driving substrate, the plurality of welding pads, the reflective layer, and the plurality of light-emitting units. The driving substrate includes a plurality of wirings of the driving circuit of the display panel. The plurality of welding pads are provided on the driving substrate and electrically connected to the plurality of wirings of the driving circuit of the driving substrate. The welding pads are provided in pairs. Each of the welding pads includes the truncated cone. The reflective layer is provided between two adjacent pairs of the welding pads. The material of the reflective layer includes the photocurable reflective ink. Each of the light-emitting units is electrically connected to a pair of the welding pads. Since each of the welding pads includes the truncated cone, the present invention can use the plurality of welding pads with a slope with high reflectivity to solve the technical problem that the photocurable reflective ink of the reflective layer in the prior art cannot be sufficiently cured. [Brief description of the drawings]
[0028] [Figure 1] FIG. 1 is a schematic diagram illustrating a portion of a display panel according to a related art. [Diagram 2] FIG. 2 is a schematic diagram illustrating a part of a display panel according to the present invention. [Diagram 3] FIG. 2 is a schematic perspective view of a welding pad of the display panel of the present invention. [Figure 4] FIG. 2 is another schematic perspective view of the welding pad of the display panel of the present invention. [Diagram 5] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 6] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 7] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 8] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 9] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 10]3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 11] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. [Figure 12] 3A to 3C are schematic diagrams illustrating a manufacturing process for the display panel of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0029] In order to make the above and other objects, features and advantages of the present invention more apparent, preferred embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings.
[0030] Referring to FIG. 2, it is a schematic configuration diagram of a part of a display panel of the present invention. The display panel includes a driving substrate 100, a plurality of welding pads 200, and a plurality of light emitting units 400. The driving substrate 100 includes a plurality of wirings 110 of a driving circuit of the display panel. The plurality of welding pads 200 are provided on the driving substrate 100 and are electrically connected to the plurality of wirings 110 of the driving circuit of the driving substrate 100. The plurality of welding pads 200 serve as bonding pads for bonding the light emitting units 400, and the welding pads 200 are provided as a pair every two. The light emitting units 400 are electrically connected to a pair of the welding pads 200. That is, each pair of the welding pads 200 includes an anode and a cathode to be electrically connected to the plurality of wirings 110 of the driving substrate 100.
[0031] In order to improve the brightness and emission efficiency of the display panel and reduce the energy consumption of the display panel, the present invention provides a reflective layer 300 on the driving substrate 100 of the display panel, so that the light emitted from the light emitting unit 400 is reflected from the display panel as much as possible. In one embodiment, the reflective layer 300 is provided between two adjacent pairs of the welding pads 200, that is, surrounding the area to be bonded of the light emitting element. The material of the reflective layer 300 includes a reflective ink whose main color is white, and preferably includes a photocurable reflective ink. According to the simulation test by the inventors, when the thickness is between 55 microns and 60 microns, the reflectivity can reach 92.5% or more.
[0032] In order to allow the light to sufficiently irradiate the light-cured reflective ink of the reflective layer 300 during the exposure process, the present invention configures the shape of each of the welding pads 200 to include a truncated cone. The truncated cone is formed by cutting off the head of a general cone, and the cross section is parallel to the base 220 of the cone. The truncated cone is also called a parallel truncated cone, a frustum, and a trapezoid.
[0033] Since at least one of the side surfaces 230 of each of the welding pads 200 of the present invention is configured as a slope, in the process of exposing the light-curable reflective ink of the reflective layer 300, the curing light can be reflected to the area close to the bottom layer of the reflective layer 300. In this way, not only the reflective layer 300 close to the surface layer is fully cured by sufficient light irradiation, but also the reflective layer 300 close to the bottom layer is fully irradiated by the reflected light of the multiple welding pads 200 and fully cured.
[0034] Referring to FIG. 3, it is a schematic perspective view of one of the welding pads 200 of the display panel of the present invention. In this embodiment, each of the welding pads 200 is a truncated square pyramid, preferably a truncated regular square pyramid. Each of the welding pads 200 includes a top surface 210, a bottom surface 220 and four side surfaces 230. In each of the welding pads 200, the top surface 210 is parallel to the bottom surface 220, and the four side surfaces 230 are connected to the top surface 210 and the bottom surface 220. As shown in the figure, the present invention configures one of the side surfaces 230 of each of the welding pads 200 to have an included angle with the bottom surface 220 between 40 degrees and 50 degrees, preferably 45 degrees.
[0035] Referring to FIG. 4, it is another schematic perspective view of one of the welding pads 200 of the display panel of the present invention. In this embodiment, each of the welding pads 200 may further be a truncated cone, preferably a truncated regular cone. Each of the welding pads 200 includes a top surface 210, a bottom surface 220 and a side surface 230. In each of the welding pads 200, the top surface 210 is parallel to the bottom surface 220, and the side surface 230 is connected to the top surface 210 and the bottom surface 220. As shown in the figure, the present invention configures the side surface 230 of each of the welding pads 200 to have an included angle with the bottom surface 220 between 40 degrees and 50 degrees, preferably 45 degrees.
[0036] Compared with the truncated square pyramid weld pad 200 shown in FIG. 3, the truncated regular cone weld pad 200 can more evenly reflect the curing light toward the reflective layer 300 closer to the bottom layer of the reflective layer 300, thereby more completely curing the light-curable reflective ink on the reflective layer 300.
[0037] In one embodiment, the present invention configures the material of the welding pads 200 to be a metal material with high reflectivity, so as to reflect the curing light to the reflective layer 300 close to the bottom layer as much as possible, thereby completely curing the light curing reflective ink on the reflective layer 300. Preferably, the material of the welding pads 200 includes copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof. And, the material of the welding pads 200 has high conductivity, so that it can stably supply current to the light emitting units 400 as the bonding pads of the light emitting units 400.
[0038] According to a simulation test by the inventor, when the thickness of the reflective layer 300 is between 55 microns and 60 microns, there is a possibility that the undercut defect having a height of about 10 microns exists after the conventional patterning process is performed on the reflective layer 300. Therefore, the present invention configures at least one of the side surfaces 230 of each of the welding pads 200 to have an included angle with the bottom surface 220 between 40 degrees and 50 degrees, and accordingly configures the height of each of the welding pads 200 to be between 8 microns and 10 microns.
[0039] Due to the structural design of the plurality of welding pads 200 of the present invention, the photo-cured reflective ink of the reflective layer 300 can be cured entirely after the patterning process, thus avoiding the undercut defect caused by incomplete curing in the reflective layer of the display panel in the prior art. As a result, the reflective layer 300 of the display panel of the present invention can achieve a reflectance higher than the theoretical value, i.e., the reflectance of the reflective layer 300 can reach 92.5% or more, thereby improving the display effect of the display panel and reducing the energy consumption of the display panel.
[0040] The present invention further provides a method for manufacturing a display panel, which includes the following steps S1 to S4. As shown in Fig. 5 to Fig. 12, they are schematic diagrams of the manufacturing process of the display panel of the present invention.
[0041] In S1, the driving substrate 100 is formed. The driving substrate 100 includes the plurality of wirings 110 of the driving circuit of the display panel.
[0042] In S2, the plurality of welding pads 200 are formed on the driving substrate 100. The plurality of welding pads 200 are electrically connected to the plurality of wirings 110 of the driving substrate. In order to form the plurality of welding pads 200, this step further includes the following steps S21 to S26.
[0043] In S21, an electroplating seed layer 500 is formed on the surface of the driving substrate 100. As shown in Fig. 5, in order to form the metal welding pads 200 on the non-metallic surface of the driving substrate 100, a metal thin film of the electroplating seed layer 500 must be formed first. The thickness of the electroplating seed layer is between 0.5 microns and 1 micron, and preferably, the thickness of the formed electroplating seed layer 500 may be 0.6 microns.
[0044] In this step, in order to homogenize the subsequently formed multiple weld pads 200 with the electroplating seed layer 500, the electroplating seed layer 500 can be selected from the materials of the multiple weld pads 200, such as copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
[0045] In S22, a photoresist 600 is formed on the electroplating seed layer 500. As shown in Fig. 6, the present invention then forms the photoresist 600 having a thickness between 10 microns and 12 microns on the electroplating seed layer 500. Since the planned height of the plurality of welding pads 200 is between 8 microns and 10 microns, the planned thickness of the photoresist 600 of the present invention is configured to be equal to or greater than the planned height range of the plurality of welding pads 200.
[0046] In S23, the photoresist 600 is patterned to form a truncated cone cavity 610 in the region where each of the weld pads 200 is to be formed. As shown in Fig. 7, a patterning process such as exposure, development and washing of a photomask opens a plurality of truncated cone cavities 610 in the photoresist 600 to provide a molding space for the subsequent weld pads 200. In one embodiment, the depth of the cavity 610 is equal to or greater than the height of each of the weld pads 200, and the difference between the depth of the cavity 610 and the height of each of the weld pads is between 0 microns and 5 microns.
[0047] It should be noted that the material of the photoresist 600 of the present invention includes a negative photoresist 600. Preferably, the negative photoresist 600 can be selected from commercially available models, such as Merck CPT-100. Due to the characteristics of the negative photoresist 600, the photoresist 600 forms an undercut structure as shown in FIG. 7 after patterning. The shape of the undercut structure, such as the slope angle, can be adjusted by the exposure degree, development time, or baking time of the photoresist 600. In this way, the cavities 610 of predetermined truncated pyramids can be formed according to the needs of practical implementation.
[0048] In S24, the photoresist 600 and the electroplating seed layer 500 are electroplated to fill the cavities 610 of the photoresist 600 to form the weld pads 200. As shown in Fig. 8, after the cavities 610 are opened in the photoresist 600, the material of the weld pads 200, such as copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel and combinations thereof, can be filled into the cavities 610 of the truncated cones under the guidance of the electroplating seed layer 500 by an electroplating process such as wet electroplating to form the weld pads 200 of the truncated cones.
[0049] In S25, the photoresist 600 is removed. After the weld pads 200 are formed in the cavities 610 of the photoresist 600, the photoresist 600 can be peeled off from the electroplating seed layer 500 and the weld pads 200, as shown in FIG.
[0050] In S24, the plurality of welding pads 200 and the electroplating seed layer 500 are etched to remove the electroplating seed layer 500 other than the region where the plurality of welding pads 200 are formed. As shown in Fig. 10, in step S21, the entire electroplating seed layer 500 is first formed, and here, the plurality of wirings 110 of the driving substrate 100 are all electrically connected to the electroplating seed layer 500. In order to insulate the respective welding pads 200 from each other and electrically connect them to the plurality of wirings 110 of the driving circuit of the driving substrate 100, the electroplating seed layer 500 other than the region where the plurality of welding pads 200 are formed must be removed.
[0051] In this step, the weld pads 200 and the electroplating seed layer 500 can be etched over the entire surface, thereby removing the electroplating seed layer 500 except the area where the weld pads 200 are formed. Since the thickness of the electroplating seed layer 500 is about 0.6 microns, it is possible to achieve the insulation of each of the weld pads 200 from each other by only sacrificing a thin surface of the weld pads 200.
[0052] In S3, a reflective layer 300 is formed on the driving substrate 100. As shown in FIG. 11, after step S2 is completed, the reflective layer 300 is formed between two pairs of adjacent welding pads 200. The photo-curable reflective ink of the reflective layer 300 is applied to the driving substrate 100 by inkjet printing or screen printing, and the photo-curable reflective ink of the reflective layer 300 is completely cured by processes such as a pre-bake process, an exposure process, a development process and a post-bake process. In this step, preferably, the exposure process can be a laser direct imaging (LDI) process.
[0053] 11, when the light curable reflective ink of the reflective layer 300 is subjected to the exposure process, at least one of the side surfaces 230 of each of the welding pads 200 of the present invention is configured as a slope, so that in the process of exposing the light curable reflective ink of the reflective layer 300, the curing light can be reflected to the area close to the bottom layer of the reflective layer 300. In this way, not only the reflective layer 300 close to the surface layer is fully cured by sufficient light irradiation, but also the reflective layer 300 close to the bottom layer is fully irradiated by the reflected light of the multiple welding pads 200 and fully cured.
[0054] In S4, one of the light emitting units 400 is electrically connected to each pair of the welding pads 200. As shown in Fig. 12, after step S3 is completed, the light emitting units 400 can be electrically connected to the welding pads 200. In this step, the light emitting units 400 are bonded to the pair of the welding pads 200 by a reflow soldering (mass reflow bonding) process.
[0055] The present invention provides the display panel and its manufacturing method. The display panel includes the driving substrate 100, the plurality of welding pads 200, the reflective layer 300 and the plurality of light emitting units 400. The driving substrate 100 includes a plurality of wirings 110 of the driving circuit of the display panel. The plurality of welding pads 200 are provided on the driving substrate 100 and electrically connected to the plurality of wirings 110 of the driving circuit of the driving substrate 100. The welding pads 200 are provided in pairs. Each of the welding pads 200 includes the truncated cone. The reflective layer 300 is provided between two adjacent pairs of the welding pads 200. The material of the reflective layer 300 includes the photocurable reflective ink. Each of the light emitting units 400 is electrically connected to one pair of the welding pads 200. Because each of the welding pads 200 includes the truncated cone, the present invention can use the multiple welding pads 200 with high reflectivity slopes to solve the technical problem in the prior art that the photocurable reflective ink of the reflective layer cannot be sufficiently cured.
[0056] The above description is merely a preferred embodiment of the present invention, and those skilled in the art can make further improvements and modifications without departing from the principles of the present invention, and these improvements and modifications should also be considered to be within the scope of protection of the present invention. [Explanation of symbols]
[0057] 100 Drive board 110 Wiring 200 Welding Pad 210 Top surface 220 Bottom 230 Side 300 reflective layer 400 Light Units 400 Mini Light Emitting Diode 500 seed layer 600 Photoresist 610 Cavity
Claims
1. A display panel, a driving substrate including a plurality of wirings of a driving circuit of the display panel; a plurality of weld pads provided on the drive board and electrically connected to the plurality of wirings of the drive circuit of the drive board, the plurality of weld pads being provided as a pair for every two of the weld pads, each weld pad including a truncated cone; a reflective layer disposed between two adjacent pairs of the welding pads, the reflective layer material including a photocurable reflective ink; a plurality of light emitting units each electrically connected to a pair of said welding pads; an included angle between at least one side surface and a base surface of the truncated cone of each of the weld pads is between 40 degrees and 50 degrees; the height of each of said weld pads is between 8 microns and 10 microns; A display panel, wherein the thickness of the reflective layer is between 55 microns and 60 microns.
2. 2. The display panel of claim 1, wherein an included angle between at least one side surface and a base surface of the truncated cone of each of the weld pads is 45 degrees.
3. The display panel of claim 1 , wherein each of the weld pads is a truncated pyramid or a truncated cone.
4. 10. The display panel of claim 1, wherein the material of the plurality of weld pads comprises copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
5. A method for manufacturing a display panel, comprising the steps of: forming a driving substrate, the driving substrate including a plurality of wirings of a driving circuit of the display panel; forming a plurality of weld pads on the drive board, the weld pads being electrically connected to the plurality of wires of the drive circuit of the drive board, the weld pads being provided in pairs of two, each formed as a truncated cone; forming a reflective layer on the driving substrate, the reflective layer being formed between two adjacent pairs of the welding pads, and a material of the reflective layer including a photocurable reflective ink; and electrically connecting a light emitting unit to each pair of the welding pads; an included angle between at least one side surface and a base surface of the truncated cone of each of the weld pads is between 40 degrees and 50 degrees; the height of each of said weld pads is between 8 microns and 10 microns; The method for manufacturing a display panel, wherein the thickness of the reflective layer is between 55 microns and 60 microns.
6. The method for manufacturing a display panel according to claim 5 , wherein an included angle between at least one side surface and a bottom surface of the truncated cone of each of the welding pads is 45 degrees.
7. The method for manufacturing a display panel according to claim 5 , wherein each of the welding pads is a truncated square pyramid or a truncated cone.
8. The method for manufacturing a display panel according to claim 5, wherein the material of the plurality of welding pads includes copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
9. The step of forming a plurality of weld pads on the drive substrate further comprises: forming an electroplating seed layer on a surface of the driving substrate; forming a photoresist on the electroplating seed layer; patterning the photoresist to form a truncated cone cavity in an area where each of the weld pads is to be formed; electroplating the photoresist and the electroplating seed layer to form the weld pad filling the cavity in the photoresist; removing the photoresist; The method for manufacturing a display panel according to claim 5, further comprising the step of: etching the plurality of welding pads and the electroplating seed layer to remove the electroplating seed layer except for the area where the plurality of welding pads are formed.
10. 10. The method for manufacturing a display panel according to claim 9, wherein the thickness of the electroplating seed layer is between 0.5 microns and 1 micron.
11. 10. The method for manufacturing a display panel according to claim 9, wherein the material of the electroplating seed layer comprises copper, aluminum, silver, cobalt, palladium, iron, cadmium, nickel, and combinations thereof.
12. The method for manufacturing a display panel according to claim 9 , wherein the photoresist material includes a negative photoresist.
13. 10. The method for manufacturing a display panel according to claim 9, wherein a depth of the cavity is equal to or greater than a height of each of the welding pads, and a difference between the depth of the cavity and the height of each of the welding pads is between 0 microns and 5 microns.
14. 10. The method for manufacturing a display panel according to claim 9, wherein the thickness of the photoresist is between 10 microns and 12 microns.
Citation Information
Patent Citations
Wireless power transfer pad with ferrite chimney
CN111434003A
Backlight module and display device
CN112309243A
Micro light-emitting diode display and manufacturing method thereof
CN113380847A
Backlight module and display equipment
CN210405499U
Device circuit board, light-emitting device, array circuit board, device array and display screen
CN212209546U