Light control device
The light control device with a polarizing plate configuration and flexible resin base material effectively addresses the limitations of SPD cells by achieving high light blocking and transmission on curved surfaces, ensuring low visible light transmittance and design flexibility for applications like vehicle windows.
Patent Information
- Application Number
- JP2024082011
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-05-20
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2036-11-21
AI Technical Summary
Existing light control cells using suspended particles (SPD) and polarizing plates face challenges in achieving high light blocking performance, design flexibility, and suitability for curved surfaces, particularly in vehicles, where visible light transmittance exceeds 1% when light is blocked, and they are prone to distortions and design issues when attached to curved surfaces.
A light control device comprising a light control cell with a polarizing plate configuration, utilizing a flexible resin base material, optically transparent adhesive film, and specific layer arrangements to attach to a curved surface, including a liquid crystal layer, polarizing plates, and electrode layers, with a sealing material to maintain alignment and prevent distortions.
The solution enables high light transmission and blocking performance on curved surfaces without distortions, improving design flexibility and maintaining optical characteristics, while reducing visible light transmittance to less than 1% when light is blocked, suitable for applications like vehicle windows.
Smart Images

Figure 0007587769000001 
Figure 0007587769000002 
Figure 0007587769000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a light control device capable of adjusting light transmittance, and more particularly to a light control device including a liquid crystal driving type light control cell that is attached to a curved surface. [Background technology]
[0002] Conventionally, light control devices capable of changing the light transmittance have been known, such as a suspended particle device (SPD) that uses suspended particles whose alignment state changes depending on the presence or absence of an applied electric field. Also known are electrochromic (EC) type light control devices, light control devices that use polymer dispersed liquid crystal (PDLC), gasochromic type light control devices, thermochromic type light control devices, and photochromic type light control devices.
[0003] For example, Patent Document 1 discloses a laminate film used in SPDs. The SPD described in Patent Document 1 uses a suspension in which suspended particles are mixed into a liquid medium, and when the power is off and no electric field is applied, the particles are randomly arranged to block the transmission of light. On the other hand, when the power is on and an electric field is applied, the particles are aligned, and most of the light incident on the SPD (cell) passes through the SPD. Therefore, the user can change the light transmittance of the SPD by controlling the electric field applied to the suspension. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2011-189751 A Summary of the Invention [Problem to be solved by the invention]
[0005] In addition to the SPD mentioned above, a method using liquid crystal and a polarizing plate can be considered as a method for adjusting the light transmittance using a light-controlling cell. A light-controlling cell using liquid crystal and a polarizing plate can be simply constructed and can ensure very high light-blocking performance.
[0006] For example, when a light-control cell is applied to a vehicle window, in order to properly block sunlight when shading, it is required to suppress the transmittance of light in the visible wavelength range (i.e., visible light) to less than 1%, and in some cases, to 0.5% or less. However, the light-control cell using the above-mentioned SPD has a visible light transmittance of about 1% to 5% when shading, so it is not necessarily suitable for use in vehicles and the like in terms of light-blocking performance. On the other hand, a light-control cell using a polarizing plate can suppress the visible light transmittance to 0.1% or less when shading, and has sufficient light-blocking performance for practical use in vehicles and the like.
[0007] In addition, when comparing light-control cells using SPDs with light-control cells using polarizing plates, the latter are superior in various aspects such as design, cost, driving voltage, and driving speed. For example, the color of a light-control cell using SPDs when blocking light is "blue," while the color of a light-control cell using polarizing plates when blocking light is "black." In general, black is easier to harmonize with other colors than blue, and from the standpoint of design, it is easier to select the color of other items to be placed around the light-control cell when using black. In addition, light-control cells using SPDs have higher manufacturing costs, higher driving voltages, and slower driving speeds than light-control cells using polarizing plates.
[0008] As such, light-control cells using polarizing plates have many advantages in terms of performance compared to light-control cells using SPDs, making "light-control cells using polarizing plates" extremely useful.
[0009] On the other hand, in order to enable the application of light-controlling cells to various uses, there is an increasing need for light-controlling cells that can be applied to curved surfaces as well as flat surfaces. Therefore, there is a demand for a technology to appropriately apply a "light-controlling cell using a polarizing plate" that can ensure the desired light-transmitting and light-blocking properties to a curved surface.
[0010] Generally, a glass substrate is widely used as a substrate for holding electrodes for controlling the orientation of a liquid crystal member, but the glass substrate is a very hard and inflexible material. Therefore, a dimming cell having a glass substrate has a fixed shape, and the shape of the dimming cell cannot be changed after the dimming cell is manufactured. Therefore, a dimming cell using a glass substrate can be effectively applied to a flat surface, but cannot necessarily be appropriately applied to a curved surface that may have various curvatures. On the other hand, by using a flexible resin substrate instead of a glass substrate, the shape of the dimming cell can be changed even after the dimming cell is manufactured, and the dimming cell can be bent according to the curved surface to which it is attached.
[0011] However, it is not necessarily easy to properly attach a light-control cell made of multiple components with various rigidities and elasticities to a curved surface, and wrinkles and other distortions may occur in sheet-shaped light-control cells during installation. Such wrinkles and other distortions not only affect the optical properties of the light-control cell and impair its original light-transmitting and light-blocking performance, but also undesirably impair the product design.
[0012] Although a dimming cell using an SPD as disclosed in the above-mentioned Patent Document 1 can be formed into a curved shape, it is not a type that is attached to the object to be attached, so it needs to be made in a predetermined shape, making it difficult to flexibly adapt to various surface shapes.
[0013] The present invention has been made in consideration of the above-mentioned circumstances, and aims to provide a light control device that can appropriately attach a light control cell to a curved surface and has high light transmission and blocking performance. [Means for solving the problem]
[0014] One aspect of the present invention is a light control device including a light-transmitting plate having a curved surface and containing an ultraviolet ray blocking component that blocks the transmission of ultraviolet rays, a light control cell, and an optically transparent adhesive film that is disposed between the curved surface of the light-transmitting plate and the light control cell and bonds one side of the light control cell to the curved surface of the light-transmitting plate, the light control cell including a first polarizing plate, a second polarizing plate disposed at a position farther away from the light-transmitting plate than the first polarizing plate, a hard coat layer disposed at a position farther away from the light-transmitting plate than the second polarizing plate, and a hard coat layer disposed between the first polarizing plate and the second polarizing plate, the first polarizing plate the first electrode layer is disposed on the first resin substrate side and the second resin substrate side, the first electrode layer is disposed on the first resin substrate side and the second electrode layer is disposed on the second resin substrate side, the first alignment film is disposed between the first electrode layer and the second electrode layer and the second alignment film is disposed on the first electrode layer side, a sealant is disposed between the first alignment film and the second alignment film and defines a liquid crystal space between the first alignment film and the second alignment film, and a liquid crystal layer is disposed in the liquid crystal space.
[0015] The curved surface of the light-transmitting plate may be a three-dimensional curved surface.
[0016] The optically transparent adhesive film has a thickness of 50 μm or more and 500 μm or less, preferably 200 μm or more and 300 μm or less, in the direction in which the optically transparent adhesive film and the light control cell are laminated, and has a storage modulus of 1×10 7 Pa or more 1×10 8 Pa or less is more preferable. The loss tangent (tan δ) of the optically transparent adhesive film is preferably 0.5 to 1.5, more preferably 0.7 to 1.2. The "loss tangent" here is represented by the ratio of the storage shear modulus (G') to the loss shear modulus (G'') (i.e., "G'' / G'").
[0017] At least one of the first resin substrate and the second resin substrate may contain polycarbonate or cycloolefin polymer.
[0018] The length of the sealing material in a direction perpendicular to the direction in which the first alignment film, the sealing material, and the second alignment film are stacked may be 1 mm or more and 5 mm or less.
[0019] The liquid crystal layer is preferably at the same pressure as atmospheric pressure, but it is more preferable that the pressure inside the liquid crystal layer is negative relative to atmospheric pressure.
[0020] The light control device may further include a retardation compensation film provided at least either between the first polarizer and the first electrode layer or between the second polarizer and the second electrode layer.
[0021] The liquid crystal layer may be a VA, TN, IPS, or FFS liquid crystal layer.
[0022] The optical axis of the first resin base material may be perpendicular to the optical axis of the second resin base material, the optical axis of the first resin base material may be parallel to the absorption axis of the first polarizer, and the optical axis of the second resin base material may be parallel to the absorption axis of the second polarizer.
[0023] The optical axis of the first resin base material and the optical axis of the second resin base material may be parallel, the optical axis of the first resin base material may be perpendicular to the absorption axis of the first polarizer, and the optical axis of the second resin base material may be parallel to the absorption axis of the second polarizer.
[0024] The light control device may further include a retardation compensation film provided between the first resin substrate and the first polarizing plate, the absorption axis of the first polarizing plate may be perpendicular to the absorption axis of the second polarizing plate, the retardation compensation film may function as an A plate, and the slow axis direction of the retardation compensation film may be parallel to the optical axis of the first resin substrate, the optical axis of the second resin substrate, and the absorption axis of the second polarizing plate. The light control device may further include a retardation compensation film provided between the second resin substrate and the second polarizing plate, the absorption axis of the first polarizing plate may be perpendicular to the absorption axis of the second polarizing plate, the retardation compensation film may function as an A plate, and the slow axis direction of the retardation compensation film may be parallel to the optical axis of the first resin substrate, the optical axis of the second resin substrate, and the absorption axis of the first polarizing plate.
[0025] The dimming device may further include a plurality of spacers arranged at least in the liquid crystal space and supporting the first alignment film and the second alignment film, and when the Vickers hardness value of each of the plurality of spacers is represented by Xs and the Vickers hardness value of the portion of the first alignment film where the tip of each of the plurality of spacers abuts is represented by Xf, 16.9≦Xs≦40.2 is satisfied and 11.8≦Xf≦35.9 is also satisfied.
[0026] Another aspect of the present invention relates to a dimming device comprising a light-transmitting plate having a curved surface, a dimming cell, and an optically transparent adhesive film disposed between the curved surface of the light-transmitting plate and the dimming cell and adhering one side of the dimming cell to the curved surface of the light-transmitting plate, wherein the dimming cell has a liquid crystal layer containing a dichroic dye.
[0027] Another aspect of the present invention relates to a dimming device comprising a light-transmitting plate having a curved surface, a dimming cell, and an optically transparent adhesive film arranged between the curved surface of the light-transmitting plate and the dimming cell, and adhering one side of the dimming cell to the curved surface of the light-transmitting plate, in which the dimming cell has a first laminate including a first substrate, a first transparent electrode and a first alignment film provided on the first substrate, a second laminate including a second substrate, and a second alignment film provided on the second substrate, and a liquid crystal layer provided between the first laminate and the second laminate, and each of the first laminate and the second laminate includes an E-type linear polarizer.
[0028] The linear polarizer of the first laminate may be provided on the liquid crystal layer side of the first substrate, and the linear polarizer of the second laminate may be provided on the liquid crystal layer side of the second substrate.
[0029] The first laminate may have a first transparent electrode, a linear polarizer, a negative C plate layer and a first alignment film provided in that order on a first substrate, and the second laminate may have a linear polarizer and a second alignment film provided in that order on a second substrate.
[0030] The first laminate may have a linear polarizer, a negative C plate layer, a first transparent electrode and a first alignment film provided in that order on a first substrate, and the second laminate may have a linear polarizer and a second alignment film provided in that order on a second substrate.
[0031] In the first laminate, a negative C plate layer may be laminated on the pressure-sensitive adhesive layer.
[0032] Another aspect of the present invention relates to a dimming device comprising a first light-transmitting plate having a curved surface, a second light-transmitting plate, a dimming cell disposed between the first light-transmitting plate and the second light-transmitting plate, and an optically transparent adhesive film disposed between the curved surface of the first light-transmitting plate and the dimming cell, and adhering one side of the dimming cell to the curved surface of the first light-transmitting plate.
[0033] The second light-transmitting plate may be spaced apart from the dimming cell.
[0034] The second light-transmitting plate may be attached to the dimming cell via an adhesive layer.
[0035] The space between the second light-transmitting plate and the light-controlling cell may be sealed with a sealant.
[0036] Silicone may be disposed between the second light-transmitting plate and the dimming cell sealed by the sealant.
[0037] A vacuum may be created between the second light-transmitting plate and the dimming cell sealed by the sealant.
[0038] The light-transmitting plate may have a higher bending stiffness than the dimming cell.
[0039] The first light-transmitting plate may have a bending stiffness higher than that of the dimming cell.
[0040] The light control device may further comprise an anti-reflection layer.
[0041] The light control device may further include an anti-reflection layer, which may be provided on at least one of the light control cell and the light-transmitting plate.
[0042] The light control device may further include an anti-reflection layer, which may be provided on at least one of the light control cell and the second light-transmitting plate.
[0043] The anti-reflective layer may include at least one of an anti-glare layer, an anti-reflection layer, and a low-reflection layer.
[0044] The curved surface may be a three-dimensional curved surface.
[0045] The optically transparent adhesive film has a thickness of 50 μm or more and 500 μm or less in the direction in which the optically transparent adhesive film and the light-controlling cell are laminated, and a storage modulus of 1×10 7 Pa or more 1×10 8 It may be less than Pa.
[0046] The optically transparent adhesive film may have a loss tangent of 0.5 or more and 1.5 or less. Effect of the Invention
[0047] According to the present invention, the light-controlling cell is properly attached to the curved surface of the light-transmitting plate via the optically transparent adhesive film, and the light-controlling cell exhibits high light-transmitting and light-blocking performance. [Brief description of the drawings]
[0048] [Figure 1] FIG. 1 is a schematic cross-sectional view showing an example of a light control device. [Diagram 2] FIG. 2 is a diagram for explaining a three-dimensional curved surface. [Diagram 3] FIG. 3 is a schematic cross-sectional view for explaining the layer structure of the optically transparent adhesive film and the light control cell. [Figure 4A] FIG. 4A is a schematic cross-sectional view for explaining the layer structure of the first electrode alignment layer. [Figure 4B] FIG. 4B is a schematic cross-sectional view for explaining the layer structure of the second electrode alignment layer. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a modified example of the second polarizing plate (protective layer) and the hard coat layer. [Figure 6] FIG. 6 is a diagram illustrating a first resin base material, a second resin base material, a polarizing layer of a first polarizing plate, and a polarizing layer of a second polarizing plate, for explaining the first arrangement mode. [Figure 7] FIG. 7 is a diagram showing a first resin base material, a second resin base material, a polarizing layer of a first polarizing plate, and a polarizing layer of a second polarizing plate, illustrating a comparative arrangement to the first arrangement. [Figure 8] FIG. 8 shows the viewing angle characteristics of the light control cell for the first arrangement shown in FIG. 6 (see symbol "L1" in FIG. 8) and the viewing angle characteristics of the light control cell for the comparative arrangement shown in FIG. 7 (see symbol "L2" in FIG. 8). [Figure 9] FIG. 9 is a diagram illustrating a first resin base material, a second resin base material, a polarizing layer of a first polarizing plate, a polarizing layer of a second polarizing plate, and a retardation compensation film for explaining the second arrangement mode. [Figure 10] FIG. 10 is a diagram showing a first resin substrate, a second resin substrate, a polarizing layer of a first polarizing plate, a polarizing layer of a second polarizing plate, and a retardation compensation film, illustrating a comparative arrangement for the second arrangement. [Figure 11] FIG. 11 shows the viewing angle characteristics of the light control cell for the second arrangement shown in FIG. 9 (see symbol "L3" in FIG. 11) and the viewing angle characteristics of the light control cell for the comparative arrangement shown in FIG. 10 (see symbol "L4" in FIG. 11). [Figure 12] FIG. 12 is a table showing the evaluation of the state of bonding of the light-controlling cell (Examples 1 to 3) to the curved surface of the light-transmitting plate. [Figure 13] FIG. 13 is a table showing the evaluation of the state of bonding of the light-controlling cell (Examples 4 to 9) to the curved surface of the light-transmitting plate. [Figure 14] FIG. 14 is a table showing the evaluation of the state of bonding of the light-controlling cell (Examples 10 to 12) to the curved surface of the light-transmitting plate. [Figure 15]FIG. 15 is a flow chart showing an outline of the manufacturing process of the light-control cell. [Figure 16] FIG. 16 is a chart showing the test results used to confirm the spacer configuration. [Figure 17] FIG. 17 is a chart showing the test results used to confirm the spacer configuration. [Figure 18] FIG. 18 is a table showing the manufacturing conditions of the spacer. [Figure 19] FIG. 19 is a table showing the manufacturing conditions of the alignment film. [Figure 20] Figure 20 is a conceptual diagram to explain an example of a light-control cell using a guest-host type liquid crystal (light-blocking state), where Figure 20(a) is a cross-sectional view of the light-control cell, and Figure 20(b) is a plan view of the first polarizing plate with the absorption axis direction indicated by arrow "A". [Figure 21] Figure 21 is a conceptual diagram for explaining the same dimming cell (light transmitting state) as Figure 20, where Figure 21(a) is a cross-sectional view of the dimming cell and Figure 21(b) is a plan view of the first polarizing plate with the absorption axis direction indicated by arrow "A". [Figure 22] FIG. 22 is a conceptual diagram for explaining another example (light blocking state) of a light control cell using a guest-host type liquid crystal, and shows a cross section of the light control cell. [Figure 23] FIG. 23 is a conceptual diagram for explaining the same light control cell (light transmitting state) as in FIG. 22, and shows a cross section of the light control cell. [Figure 24] FIG. 24 is a cross-sectional view illustrating the basic configuration of a light-control cell. [Diagram 25] FIG. 25 is a cross-sectional view showing a light-controlling cell according to the first mode. [Figure 26] FIG. 26 is a flowchart showing the manufacturing process of the light-control cell of FIG. [Figure 27] FIG. 27 is a flow chart showing the upper laminate fabrication process in the manufacturing process of FIG. [Figure 28] FIG. 28 is a flow chart showing the lower laminate fabricating process in the manufacturing process of FIG. [Figure 29]FIG. 29 is a cross-sectional view showing a light-controlling cell according to the second mode of the present invention. [Diagram 30] FIG. 30 is a cross-sectional view showing a light-controlling cell according to the third mode of the present invention. [Diagram 31] FIG. 31 is a cross-sectional view showing a light-controlling cell according to the fourth mode of the present invention. [Diagram 32] FIG. 32 is a cross-sectional view showing a light-controlling cell according to the fifth mode of the present invention. [Diagram 33] FIG. 33 is a schematic cross-sectional view showing another example of a light control device. [Diagram 34] FIG. 34 is a schematic cross-sectional view showing another example of a light control device. [Diagram 35] FIG. 35 is a schematic cross-sectional view showing another example of a light control device. [Diagram 36] FIG. 36 is a schematic cross-sectional view showing an example of a light control device including an anti-reflection layer. [Figure 37] FIG. 37 is a schematic cross-sectional view showing another example of a light control device provided with an antireflection layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0049] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0050] The light control device 10 described below can be applied to various technical fields that require adjustment of light transmittance, and the scope of application is not particularly limited. For example, the light control device 10 according to the present invention can be used as any device that requires switching between light transmission and light blocking, such as windows (including skylights) of vehicles and other vehicles and buildings, showcases, and partitions placed indoors. In addition, each element constituting the light control device 10 can be manufactured by a known method, and is manufactured using any lamination technology, photolithography technology, and / or bonding technology.
[0051] The dimming device 10 (dimming cell 22, etc.) described below merely illustrates one embodiment of the present invention. Therefore, for example, some of the elements listed below as components of the dimming device 10 may be replaced with other elements or may not be included. Elements not listed below may be included as components of the dimming device 10. In addition, the scale and dimensional ratios of some parts in the drawings have been appropriately changed or exaggerated from those of the actual objects for the convenience of illustration and ease of understanding.
[0052] FIG. 1 is a schematic cross-sectional view showing an example of a light control device 10. As shown in FIG.
[0053] The dimming device 10 of this embodiment comprises a light-transmitting plate 21 having a curved surface 20, a dimming cell 22 having a variable transmittance of light (particularly visible light), and an optically clear adhesive film (OCA) 24 arranged between the curved surface 20 of the light-transmitting plate 21 and one side of the dimming cell 22.
[0054] The light-transmitting plate 21 contains an ultraviolet-ray blocking component and blocks the transmission of ultraviolet rays while transmitting visible light. The light-transmitting plate 21 has a curved surface 20 and includes one or more glass plates. The light-transmitting plate 21 does not necessarily need to contain an ultraviolet-ray blocking component, and the light-controlling cell 22 and the optically transparent adhesive film 24 described below can be applied to a light-transmitting plate 21 that does not contain an ultraviolet-ray blocking component. The light-transmitting plate 21 may have glass plates (two glass plates in total) arranged on the front side and the back side, or may have one glass plate such as reinforced glass. The light-transmitting plate 21 may also include a member other than a glass plate, and any functional layer such as a high-rigidity film (e.g., a COP (Cyclo Olefin Polymer) resin layer) or a heat-reflecting film may be provided on the light-transmitting plate 21.
[0055] The curved surface 20 of the light-transmitting plate 21 is typically a two-dimensional or three-dimensional curved surface, but is not particularly limited thereto, and the curved surface 20 of the illustrated light-transmitting plate 21 is a three-dimensional curved surface. Generally, it is not easy to attach a thin-film dimming cell 22 to a three-dimensional curved surface without causing wrinkles, but according to the "attachment technique for the dimming cell 22 to the light-transmitting plate 21" described later, it is easy to attach the thin-film dimming cell 22 to a three-dimensional curved surface without causing wrinkles.
[0056] 2 is a diagram for explaining the three-dimensional curved surface 20a. The three-dimensional curved surface 20a here is to be distinguished from a two-dimensional curved surface that is curved two-dimensionally around a single axis, or a two-dimensional curved surface that is curved two-dimensionally with different curvatures around multiple axes that are parallel to each other. In other words, the three-dimensional curved surface 20a means a surface that is partially or entirely curved around each of multiple axes that are inclined relative to each other.
[0057] One surface of the illustrated light-transmitting plate 21 (i.e., the curved surface 20 to which the optically transparent adhesive film 24 is attached) is curved as a whole as shown in Fig. 2, bending in a first direction d1 around a first axis A1 and also bending in a second direction d2 around a second axis A2. In the illustrated example, both the first axis A1 and the second axis A2 are inclined with respect to the X and Y directions shown in Fig. 2, and the first axis A1 is perpendicular to the second axis A2.
[0058] One side of a dimming cell 22 is adhered to the curved surface 20 of the light-transmitting plate 21 via an optically transparent adhesive film 24 .
[0059] 3 is a schematic cross-sectional view for explaining the layer structure of the optically transparent adhesive film 24 and the light-controlling cell 22. As described above, the optically transparent adhesive film 24 is provided on one side of the light-controlling cell 22. In addition, a hard coat layer 26 is provided on the other side of the light-controlling cell 22.
[0060] The optically transparent adhesive film 24 of this embodiment is made of a transparent adhesive sheet called OCA, does not include a substrate, and can be made of only an adhesive with a nearly constant thickness, for example, an acrylic adhesive with excellent transparency. The optically transparent adhesive film 24 (OCA) is manufactured by sandwiching an adhesive between sheets (separators (release materials)) with excellent peelability, and the laminate of the adhesive and separator is cut into a desired shape, and the adhesive (optically transparent adhesive film 24) can be attached to a desired location by removing the separator. The optically transparent adhesive film 24 can be formed by coating a transparent adhesive resin called OCR (Optical Clear Resin), for example.
[0061] The dimming cell 22 has a multi-layer structure, and from the optically transparent adhesive film 24 side toward the outside (i.e., in the direction away from the light-transmitting plate 21), "protective layer 47, polarizing layer 48, protective layer 47, adhesive layer 46, first electrode alignment layer 43, liquid crystal layer 49, second electrode alignment layer 44, adhesive layer 46, retardation compensation film 45, adhesive layer 46, protective layer 47, polarizing layer 48, protective layer 47, adhesive layer 46, and hard coat layer 26" are sequentially arranged in layers as shown in Fig. 3. These layers form a laminated structure of "polarizing plate-electrode layer-alignment film-liquid crystal layer-alignment film-electrode layer-polarizing plate-hard coat layer".
[0062] That is, the first polarizing plate 41 is formed by "the protective layer 47, the polarizing layer 48, and the protective layer 47" arranged on the light-transmitting plate 21 side, and the second polarizing plate 42 is formed by another "protective layer 47, the polarizing layer 48, and the protective layer 47" arranged on the hard coat layer 26 side. The first polarizing plate 41 of this embodiment is attached to the curved surface 20 of the light-transmitting plate 21 via the optically transparent adhesive film 24, and the second polarizing plate 42 is provided at a position farther away from the light-transmitting plate 21 than the first polarizing plate 41 is.
[0063] The polarizing layer 48 of the first polarizing plate 41 and the second polarizing plate 42 is composed of a member that performs a desired polarizing function, and is typically made by stretching PVA (polyvinyl alcohol) doped with an iodine compound. Typical arrangements of the polarizing layer 48 include a mode called "parallel Nicol" in which the absorption axis of the polarizing layer 48 of the first polarizing plate 41 and the absorption axis of the polarizing layer 48 of the first polarizing plate 41 are parallel to each other, and a mode called "cross Nicol (see Figures 6 and 9 described later)" in which the absorption axis of the polarizing layer 48 of the first polarizing plate 41 and the absorption axis of the polarizing layer 48 of the first polarizing plate 41 are perpendicular to each other.
[0064] The protective layer 47 has a role of protecting adjacent layers, and can be made of any material that is transparent to visible light, and is typically made of TAC (triacetylcellulose) or acrylic. Note that the protective layers 47 formed at multiple locations on the first polarizing plate 41 and the second polarizing plate 42 may be made of different materials depending on the location, or may be made of the same material.
[0065] Between the first polarizer 41 and the second polarizer 42, a first electrode alignment layer 43 is arranged on the first polarizer 41 side, and a second electrode alignment layer 44 is arranged on the second polarizer 42 side, so that the first electrode alignment layer 43 and the second electrode alignment layer 44 each form an "electrode layer and alignment film supported by a substrate."
[0066] 4A is a schematic cross-sectional view for explaining the layer structure of the first electrode alignment layer 43. In the first electrode alignment layer 43 of this embodiment, a hard coat layer 53, a first resin base material 29, a hard coat layer 53, an index matching layer 55, a first electrode layer 31, and a first alignment film 33 are sequentially provided in a layered form from the first polarizer 41 side toward the liquid crystal layer 49 side.
[0067] 4B is a schematic cross-sectional view for explaining the layer structure of the second electrode alignment layer 44. In the second electrode alignment layer 44 of this embodiment, the second alignment film 34, the second electrode layer 32, the index matching layer 55, the hard coat layer 53, the second resin base material 30, and the hard coat layer 53 are sequentially provided in a layered form from the liquid crystal layer 49 side toward the second polarizer 42 side.
[0068] In this manner, between the first resin base material 29 and the second resin base material 30, a first electrode layer 31 is disposed on the first resin base material 29 side, and a second electrode layer 32 is disposed on the second resin base material 30 side. The first electrode layer 31 and the second electrode layer 32 can be formed as transparent electrodes using various materials such as ITO (Indium Tin Oxide), and a power supply means such as FPC (Flexible Printed Circuits) is connected to apply a voltage. Depending on the voltage applied to the first electrode layer 31 and the second electrode layer 32, an electric field acting on the liquid crystal layer 49 disposed between the first electrode layer 31 and the second electrode layer 32 changes, and the orientation of the liquid crystal material constituting the liquid crystal layer 49 is adjusted.
[0069] Between the first electrode layer 31 and the second electrode layer 32, a first alignment film 33 arranged on the first electrode layer 31 side and a second alignment film 34 arranged on the second electrode layer 32 side are provided. The manufacturing method of the first alignment film 33 and the second alignment film 34 is not particularly limited, and the first alignment film 33 and the second alignment film 34 having liquid crystal alignment ability can be made by any method. For example, the first alignment film 33 and the second alignment film 34 may be made by performing a rubbing treatment on a resin layer such as polyimide, or the first alignment film 33 and the second alignment film 34 may be made based on a photoalignment method in which a polymer film is irradiated with linearly polarized ultraviolet light to selectively react polymer chains in the polarization direction.
[0070] 3, a spacer 52 and a sealant 36 are provided between the first alignment film 33 and the second alignment film 34 in addition to the liquid crystal layer 49. That is, a sealant 36 is provided between the first alignment film 33 and the second alignment film 34 to define a liquid crystal space 35, and a liquid crystal member is filled in the liquid crystal space 35 to form the liquid crystal layer 49. A plurality of spacers 52 are disposed at least in the liquid crystal space 35, and are discretely disposed to support the first alignment film 33 and the second alignment film 34. Each spacer 52 may be formed of a single or multiple members, and may extend in the stacking direction only in the liquid crystal space 35, or may extend in the stacking direction so as to penetrate one alignment film (e.g., the second alignment film 34) and the liquid crystal space 35. The spacer 52 has a core portion and a covering portion, and the covering portion may be in direct contact with the other alignment film (e.g., the first alignment film 33). Therefore, for example, the core portion of each spacer 52 may extend in the liquid crystal space 35 from above the second electrode layer 32, penetrating the second alignment film 34, to just before reaching the first alignment film 33, and a covering portion made of the same component as the second alignment film 34 may be provided on the core portion, and the covering portion may be in direct contact with the first alignment film 33, so that the distance (cell gap) between the first alignment film 33 and the second alignment film 34 may be maintained by each spacer 52.
[0071] The sealant 36 prevents leakage of the liquid crystal material constituting the liquid crystal layer 49, and also adheres to the first electrode alignment layer 43 (first alignment film 33) and the second electrode alignment layer 44 (second alignment film 34) to fix them to each other. The sealant 36 is generally made of a thermosetting epoxy resin, and when the liquid crystal material is filled into the liquid crystal space 35 by vacuum injection, the sealant 36 made of epoxy resin can be used suitably. When the ODF (One Drop Fill) method is used as the filling method of the liquid crystal material, a hybrid type material having both thermosetting and UV curing properties (ultraviolet ray curing properties) can be used suitably as the sealant 36. This is because liquid crystal contacting the uncured sealant 36 induces defects in appearance. Therefore, it is preferable that the material constituting the sealant 36 (the compositional components of the sealant 36) contains, for example, an ultraviolet ray curing acrylic resin and an epoxy resin. From the viewpoint of fixing the first electrode alignment layer 43 (first alignment film 33) and the second electrode alignment layer 44 (second alignment film 34) to each other while preventing leakage of the liquid crystal member, the hardness (hardness) of the sealant 36 is preferably at a maximum point measured with a durometer (type A in accordance with JIS K6253; 10N load) of 20 or more and 90 or less, and more preferably at a maximum point of 20 or more and 50 or less. Moreover, the glass transition point (glass transition temperature (Tg)) of the sealant 36 is preferably at least 0°C and not more than 60°C, and more preferably at least 0°C and not more than 40°C.
[0072] Between the first electrode alignment layer 43 (first alignment film 33) and the second electrode alignment layer 44 (second alignment film 34), a plurality of spacers 52 are disposed to define the thickness of the liquid crystal layer 49 (i.e., the distance between the first electrode alignment layer 43 (first alignment film 33) and the second electrode alignment layer 44 (second alignment film 34)). Each spacer 52 can be made of various resin materials and may have a columnar shape such as a truncated cone, or a spherical bead shape. The columnar liquid crystal spaces 35 can be formed at desired locations based on photolithography technology, and the bead-shaped liquid crystal spaces 35 are made in advance and dispersed in the liquid crystal spaces 35.
[0073] The liquid crystal layer 49 of this embodiment has a negative pressure in the liquid crystal space 35 from the viewpoint of "improving the bonding property of the light control cell 22 to the light-transmitting plate 21 (i.e., preventing distortion of the light control cell 22)". For example, such a negative pressure can be realized by injecting a liquid crystal material into the liquid crystal space 35 so that the liquid crystal material constituting the liquid crystal layer 49 occupies "less than 100% (preferably about 99%) of the volume of the liquid crystal space 35". The light control cell 22 of this embodiment is attached to the curved surface 20 of the light-transmitting plate 21 in a bent state, but if the liquid crystal space 35 is filled with an excessive amount of liquid crystal material, the flexibility of the light control cell 22 is impaired, and the attachment property of the light control cell 22 to the light-transmitting plate 21 is deteriorated. Therefore, it is preferable to inject a liquid crystal material into the liquid crystal space 35 so that the liquid crystal material constituting the liquid crystal layer 49 occupies "about 99% of the volume of the liquid crystal space 35" to ensure the flexibility of the light control cell 22. Note that if the amount of liquid crystal material injected is too small compared to the volume of the liquid crystal space 35, air bubbles are induced in the liquid crystal space 35, which is not preferable.
[0074] The liquid crystal layer 49 of this embodiment is a VA (Vertical Alignment) type liquid crystal layer, and adopts a type called "normally black" in which a light-blocking state is achieved when no voltage is applied to the first electrode layer 31 and the second electrode layer 32. However, the liquid crystal layer 49 may adopt other driving methods, and the liquid crystal layer 49 may be driven by, for example, a TN (Twisted Nematic) type, an IPS (In Plane Switching) type, an FFS (Fringe Field Switching) type, or other types.
[0075] Between the second polarizer 42 and the second electrode layer 32 (second electrode alignment layer 44), a retardation compensation film 45 having compensation performance according to the driving method of the liquid crystal layer 49 is provided, and in this embodiment, a retardation compensation film 45 for eliminating the retardation of the liquid crystal layer 49 of the VA method is provided. Since the retardation change due to the angle is large in the VA method, the retardation compensation film 45 of this embodiment has compensation performance that can effectively compensate for such a retardation change. On the other hand, when the liquid crystal layer 49 adopts the TN method, the retardation compensation film 45 has compensation performance for compensating for the retardation of the liquid crystal layer 49 of the TN method (for example, the angle dependency of the liquid crystal molecules). In the case of the IPS method liquid crystal layer 49, the retardation is generally small and the retardation change due to the angle is also small, so basically a retardation compensation film is often not required, and the retardation compensation film 45 does not need to be provided.
[0076] The retardation compensation film 45 is not necessarily an essential element and may not be provided in the light control cell 22, and the installation position is not limited as long as the desired compensation performance can be exhibited. Typically, the retardation compensation film 45 is provided at least one of "between the first polarizing plate 41 and the first electrode layer 31 (first electrode alignment layer 43)" and "between the second polarizing plate 42 and the second electrode layer 32 (second electrode alignment layer 44)". Therefore, the retardation compensation film 45 may be provided between the first polarizing plate 41 (protective layer 47) and the first electrode alignment layer 43 (hard coat layer 53) instead of the position shown in FIG. 3 (i.e., between the second electrode alignment layer 44 (hard coat layer 53) and the second polarizing plate 42 (protective layer 47)). The retardation compensation film 45 may be provided in two or more layers (i.e., in two or more places), and it is sufficient that the retardation compensation film 45 as a whole can compensate for the retardation of the liquid crystal layer 49.
[0077] The hard coat layer 26 is provided at a position farther away from the light transmission plate 21 than the second polarizing plate 42, and forms the outermost layer of the light control cell 22 of this embodiment. The illustrated hard coat layer 26 is fixed to the second polarizing plate 42 via an adhesive layer 46, and may contain any component. For example, the hard coat layer 26 may be formed of the same component as the protective layer 47 (e.g., TAC, etc.). The hard coat layer 26 may be formed directly on the surface of the second polarizing plate 42 (the protective layer 47 in this embodiment) as shown in FIG. 5. For example, a cured film containing fine particles (e.g., titanium dioxide, etc.) may be formed on the surface of the second polarizing plate 42 (on the protective layer 47) using a silicone-based ultraviolet curing resin to function as the hard coat layer 26.
[0078] The above-mentioned functional layers (the first polarizer 41, the first electrode alignment layer 43, the second electrode alignment layer 44, the retardation compensation film 45, the second polarizer 42, and the hard coat layer 26 shown in FIG. 3) are bonded to each other by an adhesive layer 46, and have an integral laminated structure. The components constituting this adhesive layer 46 are not particularly limited, and the components constituting the adhesive layer 46 may be determined according to the characteristics of each layer to be bonded. In this embodiment, all the adhesive layers 46 are made of the same material as the optically transparent adhesive film (i.e., OCA) 24, but an adhesive layer 46 containing other components such as an ultraviolet curing resin may be used, or an adhesive layer 46 containing a component different from that of the adhesive layer 46 at other locations may be used depending on the arrangement position or the object to be bonded.
[0079] 3 and the like are merely examples, and other functional layers may be provided as part of the dimming cell 22, or other functional parts may be additionally provided to the dimming cell 22. For example, although not shown, a seal protective material that functions as a protective material can be provided from the side parts of the dimming cell 22 and the optically transparent adhesive film 24 to a part of the curved surface 20 of the light-transmitting plate 21. This seal protective material can not only reinforce the adhesive strength of the dimming cell 22 and the optically transparent adhesive film 24 to the light-transmitting plate 21, but also reinforce the adhesive strength between adjacent layers of the dimming cell 22 and the optically transparent adhesive film 24.
[0080] As a result of intensive research, the inventors of the present invention have come to the knowledge that in order to bond a thin-film dimming cell 22 to a curved surface 20 (especially a three-dimensional curved surface) without wrinkles or other distortions, it is preferable to adjust the dimming cell 22 and the optically transparent adhesive film 24 so as to satisfy the following conditions.
[0081] That is, the optically transparent adhesive film 24 has a thickness in the direction in which the optically transparent adhesive film 24 and the light-controlling cell 22 are laminated of 50 μm or more and 500 μm or less, and preferably 200 μm or more and 300 μm or less, and a storage modulus in a room temperature environment of 1×10 7 Pa or more 1×10 8 It is more preferable that the loss tangent (tan δ) of the optically transparent adhesive film 24 is 0.5 or more and 1.5 or less, and more preferably 0.7 or more and 1.2 or less.
[0082] The optically transparent adhesive film 24 not only serves to bond the curved surface 20 of the light-transmitting plate 21 to the first polarizing plate 41 (protective layer 47), but also serves as a cushion to fill the difference in curvature between the curved surface 20 of the light-transmitting plate 21 and the first polarizing plate 41 (protective layer 47). Therefore, if the thickness of the optically transparent adhesive film 24 in the stacking direction is too small, it becomes difficult for the film 24 to properly function as a cushion, while if the thickness in the stacking direction is too large, it becomes difficult to properly fix the first polarizing plate 41 (protective layer 47) to the curved surface of the light-transmitting plate 21. In addition, if the storage modulus of the optically transparent adhesive film 24 is too large, the rigidity of the entire light-controlling cell 22 increases, resulting in insufficient conformity to a curved surface whose shape changes three-dimensionally. On the other hand, if the storage modulus of the optically transparent adhesive film 24 is too small, the flowability of the optically transparent adhesive film 24 increases too much, making it difficult to properly fix the first polarizing plate 41 (protective layer 47) to the curved surface of the light-transmitting plate 21, and there is a concern that reliability such as heat resistance will be insufficient and foaming will occur even in normal use environments. Furthermore, if the storage modulus of the optically transparent adhesive film 24 is too small, the processability of the optically transparent adhesive film 24 will be poor, and for example, due to glue overflow when the optically transparent adhesive film 24 is cut, undesired separation of the optically transparent adhesive film 24 may occur. Therefore, the present inventors have newly found that in order to properly attach the light control cell 22 to the curved surface 20 without causing distortion such as wrinkles, the thickness and storage modulus of the optically transparent adhesive film 24 in the lamination direction are preferably within the above ranges.
[0083] The first resin base material 29 and the second resin base material 30 can be made of various transparent film materials, and are preferably made of a film material with small optical anisotropy, such as COP. In particular, from the viewpoint of appropriately attaching the dimming cell 22 to the curved surface 20, it is preferable that at least one of the first resin base material 29 and the second resin base material 30 contains polycarbonate. The constituent materials, shapes and / or sizes of the first resin base material 29 and the second resin base material 30 may be the same as or different from each other.
[0084] Furthermore, the length of the sealing material 36 in a direction perpendicular to the stacking direction (the direction in which the first alignment film 33, the sealing material 36 and the second alignment film 34 are stacked) (i.e., the width direction) is preferably 1 mm or more and 5 mm or less, and particularly preferably 1.5 mm.
[0085] The smaller the length of the sealant 36 in the width direction, the lower the rigidity of the entire dimming cell 22, making it easier to attach the dimming cell 22 to the curved surface 20 without causing distortion such as wrinkles. On the other hand, if the length of the sealant 36 in the width direction is too small, the original functions of the sealant 36, such as "sealing the liquid crystal layer 49 in the liquid crystal space 35" and "bonding the first electrode alignment layer 43 (first alignment film 33) and the second electrode alignment layer 44 (second alignment film 34)", are impaired. Taking all these factors into consideration, the present inventors have newly discovered that the length of the sealant 36 in the width direction is preferably 1 mm or more and 5 mm or less (more preferably 1.5 mm) as described above.
[0086] Thus, generally speaking, the smaller the rigidity of the laminate constituting the dimming cell 22, the easier it is to deform in accordance with the curved surface 20 of the light-transmitting plate 21, and the easier it is to attach the dimming cell 22 to the curved surface 20 without causing distortion such as wrinkles. However, the present inventors have newly discovered that the dimming cell 22 cannot be properly attached to the curved surface 20 of the light-transmitting plate 21 simply because the rigidity of the laminate is sufficiently small, and that there are suitable conditions for the optically transparent adhesive film 24 and the dimming cell 22.
[0087] The light transmittance (particularly the total light transmittance) of the dimming cell 22 is preferably 30% or more, more preferably 35% or more. The "total light transmittance" here indicates the ratio of the total transmitted light flux to the parallel incident light flux of the test piece, and in the case of a diffusive sample, the "total transmitted light flux" includes the diffused transmitted light flux (diffused component). Details of the total light transmittance can be determined based on "JIS (Japanese Industrial Standards) 7375:2008". The total light transmittance can be calculated from the "proportion of light transmitted through the dimming cell 22" obtained based on the light intensity of a wavelength of 555 nm of the light before transmitting through the dimming cell 22. The color of the dimming cell 22 is preferably "black" in consideration of harmony with other surrounding members, but it is also preferable for it to be "achromatic color other than black."
[0088] In addition, distortion such as wrinkles of the dimming cell 22 caused by bonding to the curved surface 20 of the light-transmitting plate 21 is particularly likely to occur at the beginning of the bonding process (i.e., the bonding start region). Based on this knowledge, the dimming cell 22 is bonded to the curved surface 20 of the light-transmitting plate 21 at a location in the light-adjusting device 10 (the light-transmitting plate 21, the optically transparent adhesive film 24, and the dimming cell 22) that is not originally intended for optical use or that is difficult for the user to see, as the bonding start region, thereby making it possible to reduce the substantial effect of distortion of the dimming cell 22. Therefore, for example, by setting the bonding start region to an area outside the seal material 36 where the liquid crystal layer 49 is not provided, the "effect of distortion occurring in the dimming cell 22" on the light passing through the liquid crystal layer 49 can be substantially reduced. Therefore, when the first electrode orientation layer 43 and the second electrode orientation layer 44 (particularly the first electrode layer 31 and the second electrode layer 32) are extended outside the seal material 36 and a "power supply means for the first electrode layer 31 and the second electrode layer 32" such as an FPC is connected to this extension, this "region where the power supply means is connected" can be used as a bonding start region, and the dimming cell 22 can be bonded to the curved surface 20 of the light-transmitting plate 21 from that region, thereby effectively hiding distortion occurring in the dimming cell 22. In particular, the position of the extended portion of the first electrode layer 31 and the second electrode layer 32 where the power supply means such as an FPC is connected is relatively far from the region (active area) where the liquid crystal layer 49 is provided, so that distortion of the dimming cell 22 occurring in the bonding start region can be easily contained within the range of the inactive area.
[0089] As described above, according to the light control device 10 of this embodiment, the light control cell 22 can be appropriately attached without distortion to the curved surface 20 of the light-transmitting plate 21 via the optically transparent adhesive film 24. In particular, according to the light control cell 22 of this embodiment, light control is performed by a combination of the polarizing plates (the first polarizing plate 41 and the second polarizing plate 42) and the orientation control of the liquid crystal layer 49, so that high-level light transmitting performance and light blocking performance can be achieved with a simple configuration.
[0090] Furthermore, the dimming cell 22 of this embodiment does not include rigid elements such as glass, and is composed of a combination of highly flexible materials. Therefore, the dimming cell 22 of this embodiment can perform with high accuracy "bonding of the dimming cell 22 to the curved surface 20," which was difficult when glass was used as a base material supporting the first electrode layer 31 and the second electrode layer 32.
[0091] In general, the rigidity of a dimming cell using a resin base material is low, and such a dimming cell with low rigidity is relatively easily deformed when an external force is directly applied to it, and the optical properties of the liquid crystal layer are disturbed. Therefore, when a dimming device is used in an environment where an external force such as vibration is suddenly or continuously applied to a dimming cell with low rigidity, the orientation of the liquid crystal material of the liquid crystal layer is disturbed and the original optical function cannot be fully exhibited, and phenomena such as flickering may occur in the light observed through the dimming device. However, the dimming cell 22 (liquid crystal layer 49) of this embodiment is firmly supported by being attached to the light-transmitting plate 21 with a relatively high rigidity (i.e., the light-transmitting plate 21 with a higher bending rigidity than the dimming cell 22), so that the disturbance of the liquid crystal orientation caused by the external force can be effectively reduced, and phenomena such as flickering can be avoided.
[0092] As a mode of attaching the dimming cell 22 to the light transmission plate 21 having two or more glass plates, there are a mode of disposing the dimming cell 22 between two glass plates and a mode of disposing the dimming cell 22 outside the two glass plates. When the dimming cell 22 is disposed between two glass plates, it is possible to protect the dimming cell 22 with the glass plates and adjust the transmittance of the light incident on the glass plates with the dimming cell 22. However, while a relatively large force (such as a compressive force or a shearing force) may be applied between the two glass plates, the dimming cell 22 equipped with polarizing plates (the first polarizing plate 41 and the second polarizing plate 42) is not necessarily highly resistant to the force applied from the outside. Also, depending on the use environment, the temperature between the glass plates becomes very high, but the polarizing plates are not necessarily excellent in high-temperature resistance. Therefore, when the dimming cell 22 equipped with polarizing plates is disposed between two glass plates, there is a concern that the dimming cell 22 may be crushed or deteriorated, and the dimming cell 22 may not be able to perform the desired dimming function.
[0093] On the other hand, in the mode of attaching the dimming cell 22 to the outer surface of the light transmission plate 21 as in the dimming device 10 of the present embodiment shown in FIGS. 1 and 3 and the like, the endurance performance and the temperature resistance performance required for the dimming cell 22 are not high. Therefore, the dimming device 10 of the present embodiment can continuously exhibit the desired dimming function even though the dimming cell 22 is equipped with polarizing plates (the first polarizing plate 41 and the second polarizing plate 42). Also, by using the dimming cell 22 that satisfies the above conditions that facilitates attaching the dimming cell 22 to the curved surface 20 without causing distortion such as wrinkles, the light-transmitting performance and the light-shielding performance of the dimming cell 22 are not excessively impaired, and according to the specific degree of curvature of the curved surface 20 that can have various shapes, the dimming cell 22 can be appropriately attached to the light transmission plate 21.
[0094] <Directionality between the absorption axis of the polarizing plate and the optical axis of the substrate regarding the VA method> When the driving method of the liquid crystal layer 49 is the VA method, the following relationship exists regarding "the direction of the absorption axis of the polarizing layer 48 of the first polarizer 41 and the second polarizer 42" and "the direction of the optical axis of the substrate (first resin substrate 29 and second resin substrate 30) of the first electrode alignment layer 43 and the second electrode alignment layer 44."
[0095] <First arrangement> FIG. 6 is a diagram showing a first resin base material 29, a second resin base material 30, a polarizing layer 48 of a first polarizing plate 41, and a polarizing layer 48 of a second polarizing plate 42, for illustrating the first arrangement mode.
[0096] In this embodiment, the optical axis of the first resin base material 29 is perpendicular to the optical axis of the second resin base material 30 (see optical axis directions "Db1" and "Db2" in Figure 6), the absorption axis of the polarizing layer 48 of the first polarizing plate 41 is perpendicular to the absorption axis of the polarizing layer 48 of the second polarizing plate 42 (see absorption axis directions "Da1" and "Da2" in Figure 6), the optical axis direction Db1 of the first resin base material 29 is parallel to the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41, and the optical axis direction Db2 of the second resin base material 30 is parallel to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42.
[0097] As described above, by arranging the first resin base material 29 and the second resin base material 30 so that "the optical axis direction Db1 of the first resin base material 29 is perpendicular to the optical axis direction Db2 of the second resin base material 30", the phase difference imparted to the transmitted light by the first resin base material 29 can be cancelled by the phase difference imparted to the transmitted light by the second resin base material 30. Therefore, the phase difference imparted to the transmitted light by the first resin base material 29 and the second resin base material 30 can be reduced overall.
[0098] In addition, by arranging the first resin base material 29, the second resin base material 30, the first polarizing plate 41, and the second polarizing plate 42 so that "the optical axis direction Db1 of the first resin base material 29 and the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41 are parallel" and "the optical axis direction Db2 of the second resin base material 30 and the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42 are parallel", it is possible to suppress "deterioration of the viewing angle characteristics and the light blocking rate during light blocking (i.e., during black display)" caused by the optical anisotropy of the first resin base material 29 and the second resin base material 30. That is, the resin base materials (the first resin base material 29 and the second resin base material 30) that inherently have optical anisotropy affect the transmitted light, and deteriorate the viewing angle and the light blocking rate during light blocking, particularly in the light control cell 22 (light control device 10) that includes the VA type liquid crystal layer 49. On the other hand, as in this embodiment, "the optical axis directions Db1, Db2 of the first resin base material 29 and the second resin base material 30 arranged in front of and behind the liquid crystal layer 49 in the stacking direction are perpendicular to each other" and "the optical axis directions of the base materials arranged on the same side via the liquid crystal layer 49 and the absorption axis directions of the polarizing plates (i.e., "the optical axis direction Db1 of the first resin base material 29 and the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41" and "the optical axis direction Db2 of the second resin base material 30 and the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42") are made parallel," thereby preventing deterioration of the viewing angle and light blocking rate when light is blocked.
[0099] 7 is a diagram showing the first resin base material 29, the second resin base material 30, the polarizing layer 48 of the first polarizing plate 41, and the polarizing layer 48 of the second polarizing plate 42, illustrating a comparative embodiment to the first arrangement embodiment. In the comparative embodiment shown in FIG. 7, the optical axis direction Db1 of the first resin base material 29 is perpendicular to the optical axis direction Db2 of the second resin base material 30, the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41 is perpendicular to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42, the optical axis direction Db1 of the first resin base material 29 is perpendicular to the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41, and the optical axis direction Db2 of the second resin base material 30 is perpendicular to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42.
[0100] FIG. 8 shows the viewing angle characteristic of the dimming cell 22 in the first arrangement shown in FIG. 6 (see reference symbol "L1" in FIG. 8) and the viewing angle characteristic of the dimming cell 22 in the comparative arrangement shown in FIG. 7 (see reference symbol "L2" in FIG. 8). The viewing angle characteristics L1 and L2 shown in FIG. 8 were obtained by measuring the transmittance while changing the azimuth angle with the polar angle set to 60 degrees in a light-shielded state (i.e., power-off state) using the dimming device 10 having the configuration shown in FIG. 1, FIG. 3, FIG. 4A, and FIG. 4B. The horizontal axis of FIG. 8 indicates the azimuth angle (°), and the vertical axis indicates the total light transmittance (%) including the diffuse component. The "azimuth angle = 0°" shown in FIG. 8 corresponds to one side of the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41.
[0101] The "total light transmittance" here indicates the ratio of the total transmitted light flux to the parallel incident light flux of the test piece, and in the case of a diffusive sample, the "total transmitted light flux" includes the diffused transmitted light flux (diffused component). The details of the total light transmittance can be determined based on "JIS (Japanese Industrial Standards) 7375:2008". A "halogen lamp with a dichroic mirror" was used as the light source for measuring the total light transmittance. The total light transmittance is calculated based on the "proportion of light transmitted through the dimming cell 22" obtained based on the light intensity of the wavelength of 555 nm of the light before passing through the dimming cell 22 to be measured. Therefore, the total light transmittance can be expressed by the value (%) of the light intensity of the visible light wavelength after passing through the dimming cell 22 when the light intensity of the wavelength of 555 nm before passing through the dimming cell 22 is expressed as "100 (%)". The thickness of the dimming cell 22 used in the measurement was about 0.55 mm, and a haze meter HM-150 from Murakami Color Research Institute was used as the measuring device.
[0102] As is clear from Figure 8, the first arrangement shown in Figure 6 (see symbol "L1" in Figure 8) can reduce the amount of variation in transmittance due to changes in azimuth angle compared to the comparative arrangement shown in Figure 7 (see symbol "L2" in Figure 8), and it can be seen that it is possible to provide a dimming cell 22 (dimming device 10) with excellent viewing angle characteristics.
[0103] Also, with regard to the magnitude of the transmittance (total light transmittance) itself, the transmittance L1 of the dimming cell 22 according to the first arrangement mode is generally smaller than the transmittance L2 of the dimming cell 22 according to the comparative embodiment, which indicates that the dimming cell 22 according to the first arrangement mode can exhibit excellent light-blocking performance.
[0104] <Second arrangement> FIG. 9 is a diagram showing the first resin base material 29, the second resin base material 30, the polarizing layer 48 of the first polarizing plate 41, the polarizing layer 48 of the second polarizing plate 42, and a phase difference compensation film 45a to explain the second arrangement mode.
[0105] In this embodiment, a retardation compensation film 45a is provided between the first polarizer 41 and the first electrode alignment layer 43. This retardation compensation film 45a is adhered to the first polarizer 41 (protective layer 47) via an adhesive layer (OCA) 46, and is adhered to the first electrode alignment layer 43 (hard coat layer 53 (see FIG. 4A)) via another adhesive layer (OCA) 46, and functions as an A plate. In the retardation compensation film 45a functioning as an A plate, the refractive index (nx) in the x direction in the film plane is greater than the refractive index (ny) in the y direction perpendicular to the x direction, and the refractive index (nz) in the z direction perpendicular to the x and y directions is equal to the refractive index (ny) in the y direction (i.e., the relationship "nx>ny=nz" is satisfied). The material constituting the retardation compensation film 45a is not particularly limited, but the retardation compensation film 45a of this embodiment is constituted by a biaxially stretched transparent film made of COP.
[0106] The optical axis of the first resin base material 29 is parallel to the optical axis of the second resin base material 30 (see optical axis directions "Db1" and "Db2" in Figure 9), the absorption axis of the polarizing layer 48 of the first polarizing plate 41 is perpendicular to the absorption axis of the polarizing layer 48 of the second polarizing plate 42 (see absorption axis directions "Da1" and "Da2" in Figure 9), the optical axis direction Db1 of the first resin base material 29 is perpendicular to the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41, and the optical axis direction Db2 of the second resin base material 30 is parallel to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42.
[0107] As described above, by arranging the first resin base material 29 and the second resin base material 30 so that "the optical axis direction Db1 of the first resin base material 29 and the optical axis direction Db2 of the second resin base material 30 are parallel (matched)", the first resin base material 29 and the second resin base material 30 can be continuously supplied while being unwound from the roll. Generally, the first resin base material 29 and the second resin base material 30 are formed in a roll state, unwound from the roll in sequence, and cut into shapes and sizes according to each dimming cell 22 for use. On the other hand, the resin base material is provided with optical anisotropy such that the stretching direction is the direction of the optical axis by the stretching process in the manufacturing process, and in the roll state, the longitudinal direction (i.e., the unwound direction) is generally the direction of the optical axis. Therefore, when "the optical axis direction Db1 of the first resin base material 29 and the optical axis direction Db2 of the second resin base material 30 are matched" as in this arrangement mode, the first resin base material 29 unwound from the roll and the second resin base material 30 unwound from the roll can be continuously superimposed while being unwound without adjusting the direction. Therefore, for example, by arranging a hard coat layer 53, an index matching layer 55, a first electrode layer 31, a second electrode layer 32, a first alignment film 33 and a second alignment film 34 as shown in Figures 4A and 4B on the first resin base material 29 and the second resin base material 30 unwound from a roll, it is possible to produce long first electrode alignment layers 43 and second electrode alignment layers 44, and to efficiently mass-produce large-area dimming cells 22.
[0108] In addition, when the first resin base material 29 and the second resin base material 30 are arranged so that "the optical axis direction Db1 of the first resin base material 29 and the optical axis direction Db2 of the second resin base material 30 are parallel (matched)", the optical anisotropy of the first resin base material 29 and the second resin base material 30 strongly affects the transmitted light of the light control cell 22, and may deteriorate the viewing angle characteristics and the light blocking rate, for example, during light blocking (i.e., during black display). In order to suppress such deterioration of the viewing angle characteristics and the light blocking rate, in this arrangement, the second resin base material 30 and the polarizing layer 48 of the second polarizing plate 42 are arranged so that the optical axis direction Db2 of the second resin base material 30 and the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42 are parallel. In addition, the retardation compensation film 45a and the second resin base material 30 are arranged so that the slow axis direction Dc of the retardation compensation film 45a and the optical axis direction Db2 of the second resin base material 30 are parallel. Furthermore, the polarizing layer 48 of the first polarizing plate 41 and the polarizing layer 48 of the second polarizing plate 42 are arranged so that the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41 is perpendicular to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42. This makes it possible to suppress "deterioration in viewing angle characteristics and light blocking rate during light blocking (i.e., during black display)" caused by the optical anisotropy of the first resin base material 29 and the second resin base material 30.
[0109] 9, a retardation compensation film 45a functioning as an A plate may be provided between the second resin base material 30 and the polarizing layer 48 of the second polarizing plate 42, rather than between the first resin base material 29 and the polarizing layer 48 of the first polarizing plate 41. In this case, The components are arranged so that the slow axis direction Dc of the retardation compensation film 45a is parallel to the optical axis direction Db1 of the first resin base material 29, the optical axis direction Db2 of the second resin base material 30, and the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41. This arrangement also makes it possible to suppress "deterioration in the viewing angle characteristics and the light blocking rate during light blocking (i.e., during black display)" caused by the optical anisotropy of the first resin base material 29 and the second resin base material 30.
[0110] 10 is a diagram showing a first resin base material 29, a second resin base material 30, a polarizing layer 48 of a first polarizing plate 41, a polarizing layer 48 of a second polarizing plate 42, and a retardation compensation film 45a showing a comparative embodiment to the second arrangement embodiment. In the comparative embodiment shown in FIG. 10, the optical axis direction Db1 of the first resin base material 29 is parallel to the optical axis direction Db2 of the second resin base material 30, and the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41 is perpendicular to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42, but the optical axis direction Db1 of the first resin base material 29 is parallel to the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41, and the optical axis direction Db2 of the second resin base material 30 is perpendicular to the absorption axis direction Da2 of the polarizing layer 48 of the second polarizing plate 42.
[0111] FIG. 11 shows the viewing angle characteristic of the light control cell 22 in the second arrangement shown in FIG. 9 (see reference symbol "L3" in FIG. 11) and the viewing angle characteristic of the light control cell 22 in the comparative arrangement shown in FIG. 10 (see reference symbol "L4" in FIG. 11). The viewing angle characteristics L3 and L4 shown in FIG. 11 were obtained by using a light control device 10 in which a retardation compensation film 45a (see FIG. 9 and FIG. 10) is arranged instead of the retardation compensation film 45 (see FIG. 3) in the configuration shown in FIG. 1, FIG. 3, FIG. 4A, and FIG. 4B, and measuring the transmittance while changing the azimuth angle with the polar angle set to 60 degrees in a light-shielding state (i.e., a power-off state). The horizontal axis of FIG. 11 indicates the azimuth angle (°), and the vertical axis indicates the total light transmittance (%) including the diffusion component. The "azimuth angle = 0°" shown in FIG. 11 corresponds to one side of the absorption axis direction Da1 of the polarizing layer 48 of the first polarizing plate 41. The total light transmittance was measured in the same manner as shown in FIG.
[0112] As is clear from Figure 11, the second arrangement shown in Figure 9 (see symbol "L3" in Figure 11) can reduce the amount of variation in transmittance due to changes in azimuth angle compared to the comparative arrangement shown in Figure 10 (see symbol "L4" in Figure 11), and it can be seen that it is possible to provide a dimming cell 22 (dimming device 10) with excellent viewing angle characteristics.
[0113] Also, with regard to the magnitude of the transmittance (total light transmittance) itself, the transmittance L3 of the dimming cell 22 according to the second arrangement mode is generally smaller than the transmittance L4 of the dimming cell 22 according to the comparative embodiment, which indicates that the dimming cell 22 according to the second arrangement mode can exhibit excellent light-blocking performance.
[0114] <Example> Next, various examples relating to the verification results of the bonding performance of the light-controlling cell 22 to the light-transmitting plate 21 will be described.
[0115] FIG. 12 is a table showing the evaluation of the state of bonding of the light-controlling cell 22 (Examples 1 to 3) to the curved surface 20 of the light-transmitting plate 21. In FIG.
[0116] The light control devices 10 of Examples 1 and 3 use the same light control cells 22, but are different in planar size (X-direction size and Y-direction size perpendicular to the stacking direction) and thickness (length in the stacking direction (Z-direction size)) of the light-transmitting plate 21 and in curvature of the curved surface 20 of the light-transmitting plate 21. Note that "1800R" in Fig. 12 indicates the curvature of the curve described by a circle with a radius of 1800 mm, and "1400R" indicates the curvature of the curve described by a circle with a radius of 1400 mm.
[0117] The dimming cell 22 used in the dimming device 10 of Example 1 and Example 3 has planar sizes (X-direction size and Y-direction size perpendicular to the lamination direction) of 280 mm (X-direction size) and 288 mm (Y-direction size), and a thickness (length in the lamination direction (Z-direction size)) of 0.63 mm, polycarbonate is used as the substrate (see the first resin substrate 29 and the second resin substrate 30 in FIG. 3), an ITO film using this polycarbonate substrate is used as the electrode substrate, a dye-based and iodine-based polarizing element that has a proven track record in liquid crystal displays (LCDs) and car navigation applications is used as the polarizing layer (see the polarizing layer 48 in FIG. 3), a large number of bead-like spacers having a diameter of 6 μm and randomly arranged are used as the spacers (see the spacer 52 in FIG. 3) provided in the liquid crystal layer 49, and a hybrid sealant 36 containing a UV-curable resin and a thermosetting resin and having a width length (length perpendicular to the lamination direction) of 1.5 mm is used.
[0118] On the other hand, in the dimming device 10 of Example 2, the same light-transmitting plate 21 as in Example 3 was used, and the planar size (X-direction size and Y-direction size perpendicular to the stacking direction) was 423 mm (X-direction size) and 337 mm (Y-direction size), and the thickness (length in the stacking direction (Z-direction size)) was 0.7 mm. The dimming cell 22 used in the dimming device 10 of Example 2 has a planar size (X-direction size and Y-direction size perpendicular to the lamination direction) of 280 mm (X-direction size) and 280 mm (Y-direction size), a thickness (length in the lamination direction (Z-direction size)) of 0.54 mm, a COP is used as the substrate (see the first resin substrate 29 and the second resin substrate 30 in FIG. 3), a COP biaxial plate for VA compensation is used as the optical compensation film of the polarizing plate (see the polarizing layer 48 in FIG. 3), a plurality of columnar spacers having a cross-sectional diameter of 15 μm and spaced apart at a pitch of 230 μm are used as the spacers (see the spacer 52 in FIG. 3) provided in the liquid crystal layer 49, and a sealant 36 having a width direction length (length perpendicular to the lamination direction) of 5 mm is used. The other configurations of the dimming cell 22 of Example 2 were the same as those of the dimming cell 22 of Examples 1 and 3 described above.
[0119] Other configurations of the light control device 10 according to Examples 1 to 3 were similar to the configuration shown in FIG.
[0120] In the dimming devices 10 of the above-mentioned Examples 1 to 3, the state of attachment of the dimming cell 22 to the light-transmitting plate 21 was visually inspected. As a result, no noticeable distortion (wrinkles, etc.) occurred in the dimming cells 22 of Examples 1 and 3, whereas wrinkles were noticeable in the dimming cell 22 of Example 2, and the dimming cell 22 could not be properly attached to the light-transmitting plate 21.
[0121] FIG. 13 is a table showing the evaluation of the state of bonding of the light-controlling cell 22 (Examples 4 to 9) to the curved surface 20 of the light-transmitting plate 21.
[0122] In Examples 4 to 9, a "light-controlling cell 22 having different characteristics" was attached to a "light-transmitting plate 21 having the same characteristics" via an "optically transparent adhesive film 24 having the same characteristics", and the state of the light-controlling cell 22 attached to the light-transmitting plate 21 was evaluated. Specifically, the light-transmitting plate 21 had a planar size of 423 mm (length in the X direction) and 337 mm (length in the Y direction), and a thickness (length in the Z direction) of 0.7 mm.
[0123] The dimming cell 22 mainly has the substrate (see the first resin substrate 29 in FIG. 4A and the second resin substrate 30 in FIG. 4B), the shape of the spacer 52, the width direction length of the sealant 36 (see "seal width" in FIG. 13), the first polarizing plate 41 (see particularly "polarizing layer 48" in FIG. 3), and the second polarizing plate 42 (see particularly "polarizing layer 48" in FIG. 3) appropriately changed as shown in FIG. 13.
[0124] The item "Substrate" in FIG. 13 indicates the components of the substrate that were actually used, and COP (Examples 4, 6, and 7) or polycarbonate (Examples 5, and 8 to 9) was used.
[0125] In the "Spacer" section of Figure 13, "columnar" indicates that multiple cylindrical spacers 52 having a cross-sectional diameter of 15 μm are arranged at a pitch of 230 μm, and "bead-like" indicates that multiple spherical spacers 52 having a diameter of 6 μm are arranged randomly.
[0126] 13, "5 mm (+ margin 5 mm)" indicates a state in which the length of the seal material 36 in the direction perpendicular to the stacking direction is 5 mm, and the first electrode alignment layer 43 and the second electrode alignment layer 44 protrude by 5 mm in the direction perpendicular to the stacking direction on the opposite side of the seal material 36 from the liquid crystal layer 49. Also, "1.5 mm (+ margin 0 mm)" indicates a state in which the length of the seal material 36 in the direction perpendicular to the stacking direction is 1.5 mm, and the first electrode alignment layer 43 and the second electrode alignment layer 44 protrude by 0 mm in the direction perpendicular to the stacking direction on the opposite side of the seal material 36 from the liquid crystal layer 49 (i.e., the first electrode alignment layer 43 and the second electrode alignment layer 44 do not protrude from the seal material 36).
[0127] 13 indicates the components of polarizing layer 48 of first polarizing plate 41, and "second polarizing plate" indicates the components of polarizing layer 48 of second polarizing plate 42. "Iodine-based (with COP biaxial compensation plate)" in Fig. 13 indicates that polarizing layer 48 is composed of an iodine-based polarizer to which a COP plate having biaxial optical compensation performance is attached, "iodine-based" indicates that polarizing layer 48 is composed of an iodine-based polarizer (without optical compensation plate), and "dye-based" indicates that polarizing layer 48 is composed of a dye-based polarizer (without optical compensation plate).
[0128] The "bonding state" in FIG. 13 indicates the state of the light control cell 22 bonded to the curved surface 20 of the light-transmitting plate 21 via the optically transparent adhesive film 24 (particularly the degree and presence of distortion such as wrinkles). "Very Bad" (Example 4) indicates that very noticeable wrinkles have occurred on the light control cell 22, a cylindrical wrinkled portion called tunneling has been formed on the light control cell 22, and the light control cell 22 is in a state where it cannot be used practically. "Bad" (Example 5) indicates that noticeable wrinkles have occurred on the light control cell 22, tunneling has been formed on the light control cell 22, and the light control cell 22 is in a state where it is not easy to use practically. "Average" (Example 6) indicates that the wrinkles formed on the light control cell 22 are not noticeable, but small tunneling has been formed on the light control cell 22. "Good" (Example 7) indicates that the light control cell 22 has slight, inconspicuous wrinkles but no tunneling has been formed, and the light control cell 22 is in a state where it can be used practically. "Excellent" (Examples 8 to 9) indicates that no wrinkles or other distortions were found in the dimming cell 22, the dimming cell 22 was attached to the light-transmitting plate 21 in very good condition, and the dimming cell 22 was in a state in which it exhibited good light-transmitting and light-blocking performance.
[0129] Other configurations of the light control devices 10 according to Examples 4 to 9 were similar to the configuration shown in FIG.
[0130] From the results shown in FIG. 13, it can be seen that the bonding state of the dimming cell 22 is improved in the dimming device 10 of Examples 5 to 7 compared to the dimming device 10 of Example 4. The dimming cell 22 of Example 5 has the same configuration as the dimming cell 22 of Example 4, except that polycarbonate is used as the base material (see the first resin base material 29 of FIG. 4A and the second resin base material 30 of FIG. 4B) instead of COP. Therefore, it can be seen that polycarbonate is preferable as the constituent material of the first resin base material 29 and the second resin base material 30. The dimming cell 22 of Example 6 has the same configuration as the dimming cell 22 of Example 4, except that a "dye-based polarizer" is used as the polarizing layer 48 of the first polarizing plate 41 and the second polarizing plate 42 instead of an "iodine-based polarizer attached to a COP plate having biaxial optical compensation performance" or an "iodine-based polarizer". Therefore, it can be seen that a dye-based polarizer is preferable as the constituent material of the polarizing layer 48 of the first polarizing plate 41 and the second polarizing plate 42. The dimming cell 22 of Example 7 has the same configuration as the dimming cell 22 of Example 4, except that the width of the sealant 36 is 1.5 mm and there is no extended portion of the first electrode alignment layer 43 and the second electrode alignment layer 44 (i.e., "margin = 0 mm"). Therefore, it is found that the width of the sealant 36 in the direction perpendicular to the stacking direction is preferably 1.5 mm. If the width of the sealant 36 is too narrow, the dimming cell 22 may break due to a decrease in the adhesion of the sealant 36. On the other hand, if the width of the sealant 36 is too wide, the sealant 36 may not be able to follow a curved surface that changes shape three-dimensionally.
[0131] 13, the dimming cells 22 of Examples 8 to 9 have the same configuration as the dimming cell 22 of Example 4, except that "polycarbonate is used as the constituent material of the first resin base material 29 and the second resin base material 30 (see Example 5)," "a dye-based polarizer is used as the constituent material of the polarizing layer 48 of the first polarizing plate 41 and the second polarizing plate 42 (see Example 6)," and "the width of the sealant 36 is 1.5 mm and there are no extended portions of the first electrode alignment layer 43 and the second electrode alignment layer 44 (see Example 7)." The fact that the bonding state of the dimming cells 22 of Examples 8 to 9 was better than that of the dimming cells 22 of Examples 4 to 7 also confirms that the above considerations of Examples 4 to 7 are appropriate.
[0132] The light control cell 22 of Example 8 and the light control cell 22 of Example 9 have the same configuration except for the different shapes of the spacer 52, but the bonding state of the light control cell 22 of Example 8 and the light control cell 22 of Example 9 was very good. Therefore, it is presumed that the shape of the spacer 52 has no or very little effect on the bonding state of the light control cell 22.
[0133] FIG. 14 is a table showing the evaluation of the state of bonding of the light-controlling cell 22 (Examples 10 to 12) to the curved surface 20 of the light-transmitting plate 21.
[0134] In Examples 10 to 12, a "light-controlling cell 22 having the same characteristics" was attached to a "light-transmitting plate 21 having the same characteristics" via an "optically transparent adhesive film 24 having different characteristics", and the state of the light-controlling cell 22 attached to the light-transmitting plate 21 was evaluated. Specifically, the light-transmitting plate 21 and the light-controlling cell 22 having the same characteristics as those in Example 8 (FIG. 13) were used, while the optically transparent adhesive film 24 having different thicknesses in the lamination direction, storage modulus at room temperature, and loss tangent was used. These physical properties of Examples 10 to 12 shown in FIG. 14 are values obtained by measuring the vibration frequency at 10 Hz (Hertz), the temperature rise condition at 5° C. / min (minutes), and using a UBM Corporation (UBM) property measuring instrument "Rheogel E4000". FIG. 14 shows the storage modulus and loss tangent at 25° C. and 50° C., respectively.
[0135] Regarding the item "Attachment state of light-controlling cell" in Fig. 14, "Average" (Example 10) indicates a state in which some distortion was observed in the light-controlling cell 22. "Good" (Example 11) indicates that a smaller distortion was observed in the light-controlling cell 22 than in the light-controlling cell 22 in Example 10, but that the light-controlling cell 22 was in a relatively good state. "Excellent" (Example 12) indicates that no distortion was observed in the light-controlling cell 22, and that the light-controlling cell 22 was in an extremely good state.
[0136] Comparing Examples 10 to 12, from the viewpoint of improving the bonding state of the light-controlling cell 22 to the light-transmitting plate 21, it is preferable that the storage modulus of the optically transparent adhesive film 24 is small (for example, Example 10 ("2.9 × 10 7 Pa / 25° C.”) and Example 11 (“1.1×10 7 It can be seen that the loss tangent of the optically transparent adhesive film 24 is preferably small (for example, see Example 10 ("0.95 / 25°C"), Example 11 ("0.90 / 25°C") and Example 12 ("0.41 / 25°C"). It is also considered that the thickness of the optically transparent adhesive film 24 in the lamination direction is preferably large, but when Examples 10 to 12 are compared, it is considered that the storage modulus and loss tangent of the optically transparent adhesive film 24 have a greater effect on the bonding state of the light-controlling cell 22 to the light-transmitting plate 21 than the thickness of the optically transparent adhesive film 24.
[0137] <Detailed structure of spacer> A preferred example of the relationship between the "hardness of the spacer 52" and the "hardness of the portion with which the tip of the spacer 52 abuts" will be described below.
[0138] In the embodiment described below, the spacer 52 is formed in a cylindrical or truncated cone shape using a photoresist in the manufacturing process of the dimming cell 22 shown in FIG. 15. That is, in the manufacturing process of the dimming cell 22, the manufacturing of the first laminate (see reference symbol "SP1" in FIG. 15), the manufacturing of the second laminate (see reference symbol "SP2" in FIG. 15), the manufacturing of the liquid crystal cell (see "liquid crystal layer 49" in FIG. 3) (see reference symbol "SP3" in FIG. 15), and the lamination of these members (see reference symbol "SP4" in FIG. 15) are performed in sequence. The manufacturing process SP1 of the first laminate includes a manufacturing process SP1-1 of the electrode (i.e., the "second electrode layer 32"), a manufacturing process SP1-2 of the spacer 52, and a manufacturing process SP1-3 of the alignment layer (i.e., the "second alignment film 34"). Although not shown, the manufacturing process SP2 of the second laminate includes a manufacturing process of the electrode (i.e., the first electrode layer 31) and a manufacturing process of the alignment layer (i.e., the "first alignment film 33"). The spacers 52 are manufactured in this manner, and in this embodiment, the Vickers hardness value Xs of each spacer 52 is set to be 16.9 or more and 40.2 or less (i.e., "16.9≦Xs≦40.2" is satisfied), and the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) with which the tip of the spacer 52 abuts is set to be 11.8 or more and 35.9 or less (i.e., "11.8≦Xf≦35.9" is satisfied), thereby further improving the reliability of the spacers compared to the conventional case. Note that the Vickers hardness values are measured under the conditions described in the following examples.
[0139] For example, when no covering portion is provided and each spacer 52 is mainly composed of only the core portion (i.e., when the spacer 52 includes a core portion but not a covering portion), the above Xs is represented by the Vickers hardness value of each of the plurality of spacers (core portions) 52, and the above Xf is represented by the Vickers hardness value of the portion of the first alignment film 33 with which the tip of each of the plurality of spacers 52 abuts. On the other hand, when a covering portion is provided on the core portion and each spacer 52 is mainly composed of a combination of the core portion and the covering portion (i.e., when the spacer 52 includes a core portion and a covering portion), the above Xs is represented by the Vickers hardness value of the core portion and the covering portion of each spacer 52, and the above Xf is represented by the Vickers hardness value of the portion of the first alignment film 33 with which the covering portion covering the tip of each of the plurality of spacers 52 abuts. The "Vickers hardness value of the core portion and coating portion of each spacer 52" referred to here means the Vickers hardness value measured in a state in which the core portion is coated with the coating portion.
[0140] If the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) where the tip of the spacer 52 abuts is less than 11.8, the tip of the spacer 52 will penetrate into the opposing surface due to the pressing force during use, resulting in non-uniform cell gaps and local alignment defects. In this case, the first resin base material 29 may be scratched due to contact during assembly of the spacer 52, or cracks may occur when the entire assembly is bent.
[0141] Furthermore, if the Vickers hardness value Xs of the spacer 52 is less than 16.9, the spacer 52 will be crushed by external pressure, reducing the cell gap and making it impossible to obtain a desired cell gap. Also, if the Vickers hardness value Xs of the spacer 52 exceeds 40.2, or if the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) with which the tip of the spacer 52 abuts exceeds 35.9, the cell gap may be reduced or scratches or cracks may occur.
[0142] However, if the Vickers hardness value Xs of the spacer 52 is set to be 16.9 or more and 40.2 or less, and the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) with which the tip of the spacer 52 abuts is set to be 11.8 or more and 35.9 or less, these problems can be solved at once, and the reliability of the spacer 52 can be further improved compared to the conventional case.
[0143] [Test Results] 16 and 17 are charts showing test results used to confirm the configuration of the spacer. The examples in FIG. 16 and FIG. 17 are configured identically, except that the configurations of the spacer 52 and the alignment layer with which the spacer 52 abuts are different. More specifically, the light control cells of these examples are provided with the spacer 52 only in the lower laminate (see the second electrode alignment layer 44), and the Vickers hardness value Xs of the spacer 52 is changed by adjusting the manufacturing conditions for the spacer 52. In addition, the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) with which the tip of the spacer 52 abuts is changed by adjusting the manufacturing conditions for the first alignment film 33.
[0144] That is, the spacers 52 are formed by applying a coating liquid for the spacers 52, drying the coating liquid, and then selectively exposing the areas where the spacers 52 are to be manufactured by mask exposure using an exposure device. Note that this is the case for negative photoresist, and conversely, in the case of positive photoresist, the areas other than the areas where the spacers 52 are to be disposed are selectively exposed to light. Thereafter, the unexposed areas or the exposed areas of the spacers 52 are selectively removed by development, and processing such as rinsing is performed, and processing such as drying is performed as necessary.
[0145] In this exposure process, the exposure process may be performed on a photoresist that has been heated in advance to be in a so-called half-cured state, or in a heated environment, and in the development process, a heating process may be performed after a process such as rinsing to promote the reaction. The hardness value Xs of the spacer 52 can be determined depending on the selection of the photoresist material for the spacer 52, the heating temperatures in the coating process, the exposure process, and the baking in an oven, the heating temperature and time settings in the development process, the amount of exposure light and the exposure time, and the settings of the mask cap.
[0146] In this embodiment, the lower laminate (see the second electrode alignment layer 44) was manufactured with the spacer 52 having a Vickers hardness value Xs of 14.8, 16.9, 22.2, 40.2, or 51.4 by adjusting the heating temperature and time in the exposure process and the development process (FIG. 18). Note that this hardness is a measurement value obtained by adjusting the manufacturing conditions of the spacer 52 to manufacture the lower laminate (see the second electrode alignment layer 44), manufacturing the dimming cell 22 using this lower laminate (see the second electrode alignment layer 44), and then disassembling and measuring the hardness. In addition, this measurement value is a measurement result obtained by measuring 12 points on each dimming cell, excluding the maximum and minimum values, and averaging the remaining 10 points.
[0147] The spacers 52 were manufactured in a cylindrical shape with a diameter of 9 μm and a height of 6 μm. The spacers 52 were regularly arranged at a pitch of 110 μm in two directions perpendicular to the in-plane direction of the second resin base material 30. Therefore, the proportion (occupancy rate) of the spacers 52 on the second resin base material 30 was 0.5% (=(9 / 2) 2 ×3) / (110) 2 ).
[0148] In addition, when the occupancy rate of the spacers 52 is increased, the stress applied to each spacer is reduced, and the phenomenon of the spacers 52 being crushed or the tip penetrating can be reduced, but the transmittance and the light blocking rate deteriorate. However, when the occupancy rate of the spacers 52 is small, the optical properties such as the transmittance and the light blocking rate can be ensured, but the phenomenon of the spacers 52 being crushed or the tip penetrating cannot be avoided. For this reason, it is desirable that the occupancy rate of the spacers 52 be 0.5% or more and 10% or less.
[0149] On the other hand, the first alignment film 33 of the first electrode alignment layer 43, which is the surface that the spacer 52 abuts against, is manufactured by applying a coating liquid, drying and heat curing, and the Vickers hardness value Xf is set to a desired value by adjusting the conditions of this heat curing (heating temperature and heating time), etc. As a result, in the embodiment, the first electrode alignment layer 43 with a Vickers hardness value Xf of 10.2, 11.8, 24.8, 35.9, or 38.5 was manufactured (FIG. 19). Note that this hardness value Xf is a measurement value obtained by manufacturing the first electrode alignment layer 43 with different hardness for the first alignment film 33 of the first electrode alignment layer 43, which is the surface that the spacer 52 abuts against, by adjusting the manufacturing conditions of the first alignment film 33, and then disassembling and measuring the dimming cell 22 once using this first electrode alignment layer 43. In addition, this measurement value is a measurement result obtained by measuring at 12 points, excluding the maximum and minimum values, and averaging the remaining 10 points.
[0150] The Vickers hardness values Xs and Xf were measured using a PICODENTOR HM500 manufactured by Helmut Fischer GmbH. The measurement conditions were a push-in speed of 300 mN / 20 sec, a release speed of 300 mN / 20 sec, a creep time of 5 sec, and a maximum load of 100 mN.
[0151] In each embodiment of FIG. 16 and FIG. 17, a dimming cell was manufactured using the first electrode alignment layer 43 and the second electrode alignment layer 44 manufactured in this manner, and then tested. In the tests of FIG. 16 and FIG. 17, a load equivalent to 0.8 MPa was applied while the dimming cell was placed on a smooth surface having a high hardness made by a surface plate, and the cell gap was measured to determine the reduction in the cell gap. The load was applied for 24 hours. After the load was applied in this manner, the upper laminate including the first alignment film 33 and the lower laminate including the second alignment film 34 were peeled off, and the spacer 52 was observed under a microscope to observe the crushing of the spacer 52 (hereinafter also referred to as "spacer crushing") to observe the reduction in the cell gap, and the portion where the spacer 52 abutted was observed under a microscope to observe the state of penetration (film penetration) of the tip of the spacer 52.
[0152] Here, in the observation using the microscope, a method such as SEM was used to observe the front view, oblique view, and cross section, visually confirm the presence or absence of deformation of the spacer 52, and if deformation of the spacer 52 was confirmed, the presence or absence of "cell gap reduction, spacer crush" was judged as ○ or △ depending on the situation. Therefore, in Figures 16 and 17, "○" indicates a case where no abnormality in the corresponding item was found, and "△" indicates a case where an abnormality in the corresponding item was found.
[0153] Similarly, the area where spacer 52 abuts was viewed obliquely using a method such as SEM, and if a depression (concave) was confirmed, the "film penetration" was rated as "△", and if no concave was observed, the "film penetration" was rated as "○".
[0154] In addition, the first electrode alignment layer 43 and the second electrode alignment layer 44 were laminated and a load equivalent to 0.1 MPa was applied, and the relative positions of the first electrode alignment layer 43 and the second electrode alignment layer 44 were displaced at 0.1 cm / sec, and the occurrence of scratches was confirmed visually. If the occurrence of scratches was confirmed in more than half of the multiple samples, the "Scratches" item in Figures 16 and 17 is indicated by "△", and conversely, if the occurrence of scratches was not confirmed in more than half of the multiple samples, the "Scratches" item is indicated by "○".
[0155] Furthermore, in the state of a dimming cell, the dimming cell was wrapped around a cylindrical mandrel with a diameter of 2 mm in accordance with the bending test provisions of JIS K5600-5-1 to check for the presence or absence of cracks in the substrate (occurrence of cracks in the first resin substrate 29 and the second resin substrate 3). In this test, if cracks were confirmed in the substrate for more than half of the multiple samples, the "Crack" item in Figures 16 and 17 is indicated with a "△", and conversely, if cracks were not confirmed in the substrate for more than half of the multiple samples, the "Crack" item is indicated with a "○".
[0156] 16 and 17, when the Vickers hardness value Xs of the spacer 52 was less than 16.9 (Examples 30 and 32), a decrease in the cell gap was observed, and the tip of the spacer penetrated the film, scratches, and cracks were observed in Example 30. When the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) with which the tip of the spacer 52 abutted was less than 11.8 (Examples 20 and 22), scratches and cracks were observed, and the tip of the spacer penetrated the film in Example 22.
[0157] Furthermore, when the Vickers hardness value Xs of the spacer 52 exceeded 40.2 (Examples 31 and 33), a decrease in the cell gap and penetration of the tip of the spacer into the film were observed in Example 31, and scratches were observed in Example 33. Furthermore, when the Vickers hardness value Xf of the portion of the first electrode alignment layer 43 (particularly the first alignment film 33) where the tip of the spacer 52 abutted exceeded 35.9 (Examples 21 and 23), a decrease in the cell gap and scratches were observed, and furthermore, cracks were observed in Example 23.
[0158] However, in Examples 13 to 19 and 24 to 29, these phenomena ("cell gap reduction," "film penetration," "scratches," and "cracks" shown in Figures 16 and 17) were not observed, confirming that the reliability of spacer 52 can be sufficiently ensured.
[0159] <Guest Host LCD> The present invention is also applicable to a light control cell 22 that uses a guest-host type liquid crystal. That is, the liquid crystal layer 49 may contain a dichroic dye (guest) and liquid crystal (host). The dichroic dye contained in the liquid crystal layer 49 is preferably a coloring material that has a light-shielding property and can block (absorb) desired visible light.
[0160] The specific configuration of the light control cell 22 using guest-host type liquid crystal to which the present invention can be applied is not particularly limited. For example, instead of providing a pair of polarizing plates (see the first polarizing plate 41 and the second polarizing plate 42 in FIG. 3), only one polarizing plate may be provided as shown in FIGS. 20 and 21 described later, or no polarizing plate may be provided as shown in FIGS. 22 and 23 described later. A typical example of the light control cell 22 using guest-host type liquid crystal will be described below.
[0161] FIG. 20 is a conceptual diagram for explaining an example of a light control cell 22 using a guest-host type liquid crystal (light blocking state), where FIG. 20(a) is a cross-sectional view of the light control cell 22, and FIG. 20(b) is a plan view of a first polarizing plate 41 with the absorption axis direction indicated by an arrow "A". FIG. 21 is a conceptual diagram for explaining the same light control cell 22 (light transmitting state) as FIG. 20, where FIG. 21(a) is a cross-sectional view of the light control cell 22, and FIG. 21(b) is a plan view of a first polarizing plate 41 with the absorption axis direction indicated by an arrow "A". The absorption axis and the polarization axis (light transmitting axis) of the first polarizing plate 41 extend in directions perpendicular to each other.
[0162] The light control cell 22 shown in FIG. 20 and FIG. 21 also includes, like the light control cell 22 shown in FIG. 3, a pair of film substrates (i.e., the first resin substrate 29 and the second resin substrate 30), a pair of transparent electrodes (i.e., the first electrode layer 31 and the second electrode layer 32) disposed between the pair of film substrates, a pair of alignment films (i.e., the first alignment film 33 and the second alignment film 34) disposed between the pair of transparent electrodes, and a liquid crystal layer 49 and a spacer 52 disposed between the pair of alignment films. However, in the light control cell 22 shown in FIG. 20 and FIG. 21, only one polarizing plate (the first polarizing plate 41 in this example) is provided on the opposite side of the pair of transparent electrodes via one of the pair of film substrates (the first resin substrate 29 in this example). The first polarizing plate 41 is attached to the first resin substrate 29 via an adhesive layer 46. The liquid crystal layer 49 is composed of a guest-host type liquid crystal containing a dichroic pigment (dye) 61 and a liquid crystal 62.
[0163] The dichroic dye 61 exists in a dispersed state in the liquid crystal 62 , has the same orientation as the liquid crystal 62 , and is basically aligned in the same direction as the liquid crystal 62 .
[0164] In this example, when the voltage between the pair of transparent electrodes (the first electrode layer 31 and the second electrode layer 32) is OFF, the dichroic dye 61 and the liquid crystal 62 are aligned in a horizontal direction perpendicular to the light traveling direction L (i.e., the stacking direction of the dimming cell 22) (particularly, a direction perpendicular to the absorption axis direction A of the first polarizer 41 (i.e., the same direction as the polarization axis of the first polarizer 41)) (see FIG. 20(a)). On the other hand, when the voltage between the pair of transparent electrodes (the first electrode layer 31 and the second electrode layer 32) is ON, the dichroic dye 61 and the liquid crystal 62 are aligned in a vertical direction (i.e., the light traveling direction L) (see FIG. 21(a)). Note that in FIG. 20(a) and FIG. 21(a), the dichroic dye 61 and the liquid crystal 62 are conceptually illustrated to show the orientation directions of the dichroic dye 61 and the liquid crystal 62.
[0165] For example, when no voltage is applied to the first electrode layer 31 and the second electrode layer 32 by a dimming controller (not shown), a desired electric field is not applied to the liquid crystal layer 49, and the dichroic dye 61 and the liquid crystal 62 are aligned horizontally (see FIG. 20(a)). In this case, light vibrating in a direction perpendicular to the absorption axis direction A of the first polarizer 41 is blocked by the dichroic dye 61, and light vibrating in other directions is blocked by the first polarizer 41. Therefore, light traveling in a direction from the second film substrate 24 toward the first polarizer 41 (see arrow "L") is blocked by the dichroic dye 61 and the first polarizer 41.
[0166] On the other hand, when a voltage is applied to the first electrode layer 31 and the second electrode layer 32 by a dimming controller (not shown), a desired electric field is applied to the liquid crystal layer 49, and the dichroic dye 61 and the liquid crystal 62 are aligned in the vertical direction (see FIG. 21(a)). In this case, the light blocking performance of the dichroic dye 61 against the light passing through the liquid crystal layer 49 is not exhibited very much regardless of the vibration direction of the light, and the light that enters the liquid crystal layer 49 passes through the liquid crystal layer 49 (the dichroic dye 61 and the liquid crystal 62) with a high probability. In addition, the light vibrating parallel to the polarization axis (light transmission axis) of the first polarizer 41 (light vibrating in a direction perpendicular to the absorption axis direction A of the first polarizer 41 in this example) passes through the first polarizer 41 and is emitted from the dimming cell 22.
[0167] As described above, even when using the guest-host type liquid crystal layer 49 shown in Figures 20 and 21, the translucency of the dimming cell 22 can be appropriately changed by controlling the voltage applied to the first electrode layer 31 and the second electrode layer 32.
[0168] 20 and 21, the above description has been given of the case where the alignment films 33, 34 and the liquid crystal layer 49 of the so-called normally black type are used, but the alignment films 33, 34 and the liquid crystal layer 49 of the so-called normally white type may be used. That is, in the case of the normally black type, as described above, when a voltage is applied between the electrodes 25, 26 to apply an electric field to the liquid crystal layer 49, it is necessary to align the dichroic dye 61 and the liquid crystal 62 in the vertical direction, so horizontal alignment films are used as the alignment films 33, 34, and a positive type liquid crystal is used for the liquid crystal layer 49. On the other hand, in the case of the normally white type, when a voltage is applied between the electrodes 25, 26 to apply an electric field to the liquid crystal layer 49, it is necessary to align the dichroic dye 61 and the liquid crystal 62 in the horizontal direction as shown in FIG. 20(a), so vertical alignment films are used as the alignment films 33, 34, and a negative type liquid crystal is used for the liquid crystal layer 49.
[0169] Fig. 22 is a conceptual diagram for explaining another example (light blocking state) of a light control cell 22 using a guest-host type liquid crystal, and shows a cross section of the light control cell 22. Fig. 23 is a conceptual diagram for explaining the same light control cell 22 (light transmitting state) as Fig. 22, and shows a cross section of the light control cell 22.
[0170] 20 and 21, the light control cell 22 of this example has a basically similar configuration to the light control cell 22 shown in Figures 20 and 21, but does not have polarizing plates (first polarizing plate 41 and second polarizing plate 42), and is a guest-host type in which the liquid crystal layer 49 contains a dichroic pigment (dye) 51 and liquid crystal 62. In other words, the dichroic pigment 61 exists in a dispersed state in the liquid crystal 62, has the same orientation as the liquid crystal 62, and is basically aligned in the same direction as the liquid crystal 62.
[0171] In this example, when the voltage between the pair of transparent electrodes (the first electrode layer 31 and the second electrode layer 32) is OFF, the dichroic dye 61 and the liquid crystal 62 are aligned in the horizontal direction (i.e., the direction perpendicular to the light traveling direction L) (see FIG. 22). In particular, the orientation of the dichroic dye 61 and the liquid crystal 62 in this example is preferably twisted by 180 degrees or more with respect to the horizontal direction when no electric field is applied, so that the dichroic dye 61 is oriented in any horizontal direction. On the other hand, when the voltage between the pair of transparent electrodes (the first electrode layer 31 and the second electrode layer 32) is ON, the dichroic dye 61 and the liquid crystal 62 are aligned in the vertical direction (i.e., the light traveling direction L) (see FIG. 23). In FIG. 22 and FIG. 23, the dichroic dye 61 and the liquid crystal 62 are conceptually illustrated to show the orientation direction of the dichroic dye 61 and the liquid crystal 62.
[0172] For example, when no voltage is applied to the first electrode layer 31 and the second electrode layer 32 by a dimming controller (not shown), a desired electric field is not applied to the liquid crystal layer 49, and the dichroic dye 61 and the liquid crystal 62 are aligned in the horizontal direction (see FIG. 22). As a result, the light that enters the liquid crystal layer 49 is blocked (absorbed) by the dichroic dye 61.
[0173] On the other hand, when a voltage is applied to the first electrode layer 31 and the second electrode layer 32 by a dimming controller (not shown), a desired electric field is applied to the liquid crystal layer 49, and the dichroic dye 61 and the liquid crystal 62 are aligned in the vertical direction (see FIG. 23). In this case, the light blocking performance of the dichroic dye 61 against the light passing through the liquid crystal layer 49 is not exhibited very well regardless of the vibration direction of the light, and the light that enters the liquid crystal layer 49 passes through the liquid crystal layer 49 (the dichroic dye 61 and the liquid crystal 62) with a high probability. In addition, since a polarizing plate is not provided in this example, all of the light that passes through the liquid crystal layer 49 and is emitted from the first film substrate 23 is emitted from the dimming cell 22.
[0174] As described above, even when using the guest-host type liquid crystal layer 49 shown in Figures 22 and 23, the translucency of the dimming cell 22 can be changed by controlling the voltage applied to the first electrode layer 31 and the second electrode layer 32.
[0175] Regarding the dimming cell 22 shown in FIGS. 22 and 23, in the above description, a normally black guest-host type dimming cell 22 using a horizontal alignment film as the alignment films 33 and 34 and a positive type liquid crystal in the liquid crystal layer 49 has been described. However, a normally white guest-host type dimming cell 22 may also be used. That is, a vertical alignment film may be used as the alignment films 33 and 34, and a negative type liquid crystal may be used in the liquid crystal layer 49. When a voltage is applied between the electrodes 25 and 26 to apply an electric field to the liquid crystal layer 49, the dichroic dye 61 and the liquid crystal 62 may be aligned in the horizontal direction as shown in FIG. 22.
[0176] In addition, in FIGS. 20 to 23 described above, the hard coat layer 26 shown in FIG. 3 is not shown. However, in each dimming cell 22 shown in FIGS. 20 to 23, the hard coat layer 26 may or may not be provided. When the hard coat layer 26 is provided, for example, the hard coat layer 26 may be attached to the second resin substrate 30 via the adhesive layer 46. Also, in FIGS. 20 to 23 described above, the retardation compensation film 45 shown in FIG. 3 is not shown. However, in each dimming cell 22 shown in FIGS. 20 to 23, the retardation compensation film 45 may or may not be provided. When the retardation compensation film 45 is provided, for example, the retardation compensation film 45 may be attached to the second resin substrate 30 via the adhesive layer 46.
[0177] Even when using the dimming cell 22 having the above-described guest-host type liquid crystal (that is, the liquid crystal layer 49 containing the dichroic dye 61), an optically transparent adhesive film 24 can be disposed between the curved surface 20 of the light transmission plate 21 and the dimming cell 22, and one side of the dimming cell 22 can be adhered to the curved surface 20 of the light transmission plate 21.
[0178] <E-type linear polarizing plate> The present invention is also applicable to a dimming cell 22 equipped with an E-type linear polarizer. A VA-type dimming cell will be described below as an example, but the driving method of the dimming cell is not particularly limited, and the technology described below can be applied to a TN-type, IPS-type, or FFS-type dimming cell, for example. That is, the liquid crystal layer may be a VA-type, TN-type, IPS-type, or FFS-type liquid crystal layer.
[0179] [First mode] [Basic configuration] FIG. 24 is a cross-sectional view for explaining the basic structure of the light control cell according to the present invention. The light control cell 22 is a light control film by the VA method, and is configured by sandwiching a liquid crystal layer 114 and a spacer 115 between a lower laminate 112 and an upper laminate 113, which are first and second laminates in the form of films. The lower laminate 112 is provided with a linear polarizer 112D on a substrate 112B made of a transparent film material including a hard coat layer 112A and a hard coat layer 112C. Furthermore, a negative C plate layer 112F for optical compensation, a transparent electrode 112G, and an alignment film 112E are sequentially provided on the linear polarizer 112D. The outer hard coat layer 112A is configured, for example, with a laminate structure of two hard coat layers.
[0180] The upper laminate 113 includes a transparent electrode 113D provided on a substrate 113B made of a transparent film material including a hard coat layer 113A and a hard coat layer 113C, and further includes a linear polarizer 113E. In the upper laminate 113, an alignment film 113F is provided on the liquid crystal layer 114 side of the linear polarizer 113E.
[0181] Here, the hard coat layers 112A and 112C are made to have a thickness of about 10 μm and 5 μm. The hard coat layers 113A and 113C are made to have a thickness of about 5 μm and 5 μm. The substrates 112B and 113B are made of a versatile film material with high optical anisotropy, for example, a PET film with a thickness of 100 μm. The transparent electrodes 112G and 113D are made of ITO with a thickness of 50 nm.
[0182] The linear polarizers 112D and 113E are optical functional layers that function as E-type linear polarizers. Here, the E-type linear polarizer is a linear polarizer having a polarizing layer formed by the orientation of dye molecules, as described in JP 2011-59266 A and JP 8-511109 A. The polarizing layer of the linear polarizers 112D and 113E has an absorption axis in a direction perpendicular to the alignment direction of the dye molecules, and is a polarizing layer in which the extraordinary refractive index is smaller than the ordinary refractive index and the transmittance of the extraordinary wave is larger than that of the ordinary wave.
[0183] The E-type polarizing layer can be produced by applying a coating liquid containing dye molecules related to the polarizing layer to produce a coating film, and then applying mechanical stress (shear force) to the coating layer to orient the dye molecules, and various production methods can be applied, such as applying stress while applying the coating liquid. As a result, in this mode, the overall thickness can be made thin, and further, it is configured so that various highly versatile film materials can be applied to the base materials 112B and 113B.
[0184] That is, in the conventional light control cell, it is necessary to use a transparent film material with small optical anisotropy so that the transmitted light of the liquid crystal layer incident on the linear polarizer does not lose the polarization plane controlled by the liquid crystal layer, and therefore it is difficult to use a film material with high versatility. However, in this mode, when the linear polarizers 112D and 113E are provided on the liquid crystal layer 114 side of the substrates 112B and 113B, even if the transmitted light is polarized in various ways by the substrates 112B and 113B, it is possible to prevent the polarization plane of the transmitted light of the liquid crystal layer 114 from being affected at all, and therefore it is possible to apply a film material with large optical anisotropy, such as a PET film, to the substrates 112B and 113B, and therefore it is possible to use a transparent film material with high versatility.
[0185] Furthermore, by using the linear polarizers 112D and 113E related to the E-type linear polarizer, it is possible to sufficiently block transmitted light in an oblique direction, and this makes it possible to reduce the overall thickness without providing a compensation film.
[0186] Moreover, linear polarizers 112D, 113E related to such E-type linear polarizers can be provided on the inside of the liquid crystal cell by a coating film, whereby they can be provided on the liquid crystal layer 114 side of substrates 112B, 113B, simplifying the configuration related to the linear polarizers and making them even thinner. In practice, when linear polarizers 112D, 113E are arranged as shown in Fig. 24, the thickness of linear polarizers 112D, 113E related to E-type linear polarizers is about 1 µm, so that the thickness of light control cell 22 as a whole can be about 300 µm, thereby making it significantly thinner than before.
[0187] [Specific configuration of the first mode] 25 is a cross-sectional view showing a specific configuration of a light control cell 22 according to the first mode of the present invention. This light control cell 22 is formed in a film shape. This light control cell 22 is a VA type light control film that uses liquid crystal to control transmitted light, and is formed by sandwiching a liquid crystal layer 124 between a lower laminate 122 and an upper laminate 123, which are first and second laminates each in a film shape. Here, the light control cell 22 is a liquid crystal cell that controls the orientation of liquid crystal molecules in the liquid crystal layer 124 by the VA type.
[0188] That is, in the dimming cell 22, the lower laminate 122 has a transparent electrode 122B, which is a first electrode, formed on the entire surface of a base material 122A made of a transparent film material with hard coat layers on both sides. Here, for example, a PET film is applied to the base material 122A. Also, for example, ITO is applied to the transparent electrode 122B. Furthermore, the lower laminate 122 has an E-type linear polarizer 122C, a negative C plate layer 122D, and an alignment film 122E sequentially provided.
[0189] The upper laminate 123 is formed by sequentially fabricating a transparent electrode 123B, a linear polarizing plate 123C, and an alignment film 123D on a base material 123A made of a transparent film material having hard coat layers on both sides. Here, the linear polarizing plates 122C and 123C are provided in a cross Nicol arrangement.
[0190] Here, ITO is applied to the transparent electrodes 122B and 123B. The linear polarizing plates 122C and 123C are E-type linear polarizing plates, and more specifically, for example, the configuration disclosed in Japanese Patent Publication No. 8-511109 can be applied, and it is formed by a coating film of a dichroic organic dye that exhibits optical anisotropy in the vertical direction. The negative C plate layer 122D is a negative uniaxial retardation optical layer that satisfies nz < nx = ny when the main refractive index in the plane is nx (slow axis direction), ny is the refractive index in the fast axis direction, and the refractive index in the thickness direction is nz. Although a TAC (triacetyl cellulose) film material can be applied to the negative C plate layer 122D, in this mode, it is fabricated by a cholesteric polymerizable liquid crystal layer made of an ultraviolet curable resin. Although an optical alignment film is applied to the alignment films 122E and 123D, various configurations can be applied, such as an alignment film by rubbing treatment and an alignment film fabricated by a shaping treatment with a fine linear concavo-convex shape.
[0191] Note that although a columnar spacer 125 that holds the thickness of the liquid crystal layer 124 is fabricated on the alignment film 122E of the lower laminate 122 in the light control cell 22, it may be provided on the negative C plate layer 122D, or further, it may be provided on the linear polarizing plate 122C or the transparent electrode 122B. It may also be provided on the side of the upper laminate 123, or provided on both the lower laminate 122 and the upper laminate 123.
[0192] In addition, in the dimming cell 22, a sealant is arranged in a frame shape surrounding the liquid crystal layer 124, and this sealant prevents leakage of liquid crystal related to the liquid crystal layer 124, and furthermore holds the upper laminate 123 and the lower laminate 122 together. Here, the sealant can be made of various materials that can prevent leakage of liquid crystal and hold the upper laminate 123 and the lower laminate 122 together, but in this mode, for example, a thermosetting resin such as epoxy resin, an ultraviolet-curing resin such as acrylic resin, or a curing resin that is cured by heat and ultraviolet light is used.
[0193] 25, by applying an E-type linear polarizer to the linear polarizers 122C and 123C and providing the linear polarizers 122C and 123C on the liquid crystal layer 124 side of the lower laminate 122 and the upper laminate 123, it is possible to apply a highly versatile material to the base materials 122A and 123A of the lower laminate 122 and the upper laminate 123. Furthermore, by applying an E-type linear polarizer to the linear polarizers 122C and 123C, the overall thickness can be reduced.
[0194] 26 is a flowchart illustrating the manufacturing process of the dimming cell 22. In the manufacturing process of the dimming cell, an upper laminate 123 and a lower laminate 122 are manufactured in an upper laminate manufacturing process SP102 and a lower laminate manufacturing process SP103, respectively. In a lamination process SP104, the upper laminate 123 and the lower laminate 122 are laminated with a liquid crystal layer 124 sandwiched therebetween, and then the upper laminate 123 and the lower laminate 122 are integrated with a sealant to manufacture the dimming cell 22.
[0195] 27 is a flow chart showing the upper laminate fabrication step SP102 in detail. In this upper laminate fabrication step SP102 (SP111), in the transparent electrode fabrication step SP112, the transparent electrode 123B is fabricated by sputtering or the like using ITO, and in the subsequent linear polarizer fabrication step SP113, the coating liquid for the linear polarizer 123C is applied to the base material 123A on which the transparent electrode 123B is fabricated, and then the coating liquid is dried, thereby fabricating the linear polarizer 123C. In addition, in the linear polarizer fabrication step, when the coating liquid is applied or after the coating film is fabricated, the coating film is stretched by a blade or the like to apply a shear force to the coating film, and the dye related to the linear polarizer 123C is oriented in the stretched direction, thereby fabricating the linear polarizer 123C so as to function as a linear polarizer. Next, in the alignment film preparation step SP114, a coating liquid for the alignment film 123D is applied and dried, and then cured by irradiation with linearly polarized ultraviolet light to prepare the alignment film 123D.
[0196] FIG. 28 is a flow chart showing the lower laminate fabrication step SP103 in detail. In this lower laminate fabrication step SP103 (SP121), in an electrode fabrication step SP122, a transparent electrode 122B made of ITO is fabricated by sputtering on the entire surface of the base material 122A. Next, in a linear polarizer fabrication step SP123, the linear polarizer 122C is coated with a coating liquid and then dried in the same manner as in the linear polarizer fabrication step SP112, thereby fabricating the linear polarizer 122C. Next, in a C plate layer fabrication step SP124, the alignment film for the negative C plate layer 122D is coated with a coating liquid and then dried, and an alignment regulating force is set by irradiation with ultraviolet light or the like to fabricate an alignment film. In addition, a coating liquid for cholesteric liquid crystal is coated on this alignment film, dried, and then cured by irradiation with ultraviolet light, thereby fabricating the negative C plate layer 122D.
[0197] In the subsequent alignment film preparation step SP125, a coating liquid for the alignment film 122E is applied, dried, and exposed to light to form the alignment film 122E. In the subsequent spacer preparation step SP126, a photoresist material is applied to the entire surface, dried, exposed, and developed to form the spacer 125. Note that a transparent film material such as TAC may be applied to the negative C plate layer 122D, and the alignment film 122E and the like may be prepared in advance on this transparent film material and laminated on the substrate 122A side.
[0198] [Second mode] 29 is a cross-sectional view showing a dimming cell according to the second mode of the present invention. This dimming cell 22 is configured in the same manner as the dimming cell 22 according to the first mode, except that the transparent electrode 122B is disposed between the alignment film 122E and the negative C plate layer 122D to form the lower laminate 132.
[0199] According to this mode, even if the transparent electrode 122B is disposed between the alignment film 122E and the negative C plate layer 122D to form the lower laminate, the same effect as that of the dimming cell 22 in the first mode can be obtained.
[0200] [Third mode] 30 is a cross-sectional view showing a dimming cell according to the third mode of the present invention. In this dimming cell 22, a laminate for the negative C plate layer 122D is produced by producing a transparent electrode 122B and an alignment film 122E on a transparent film material such as TAC for the negative C plate layer 122D, and the laminate for the negative C plate layer is laminated on a base material 122A formed by producing a linear polarizer 122C with an adhesive layer 142A to produce a lower laminate 142. Note that after laminating the transparent film material for the negative C plate layer 122D on the base material 122A formed by producing a linear polarizer 122C, the transparent electrode 122B and the alignment film 122E may be produced, or only the transparent electrode 122B may be produced on the transparent film material for the negative C plate layer 122D. In this mode, the dimming cell is configured in the same manner as the dimming cell according to the above-mentioned mode, except that the configuration for the lower laminate 142 is different.
[0201] According to this mode, even if the lower laminate is fabricated by laminating the laminate relating to the negative C plate layer 122D with an adhesive layer, the same effect as that of the dimming cell relating to the first or second mode can be obtained.
[0202] [Fourth mode] 31 is a cross-sectional view showing a light control cell according to the fourth mode of the present invention. In this light control cell 22, a transparent film material for a negative C plate layer 122D formed by preparing an alignment film 122E and a spacer 125 is laminated on a base material 122A formed by sequentially preparing a transparent electrode 122B and a linear polarizer 122C, with an adhesive layer 142A to prepare a lower laminate 152. The alignment film 122E and / or the spacer 125 may be prepared after lamination with the base material 122A. In this mode, the light control cell is configured in the same way as the light control cell according to the above-mentioned mode, except that the order of preparation of each of these parts is different.
[0203] According to this mode, the same effect as the above-mentioned mode can be obtained by laminating a laminate relating to a negative C plate layer 122D formed by preparing an alignment film 122E and a spacer 125 on a base material 122A formed by sequentially preparing a transparent electrode 122B and a linear polarizer 122C with an adhesive layer 142A to prepare a lower laminate 152. In this case, the laminate of the base material, the transparent electrode, and the linear polarizer can have the same configuration for the upper laminate and the lower laminate, which can simplify the manufacturing process.
[0204] [Fifth mode] 32 is a cross-sectional view showing a dimming cell according to the fifth mode of the present invention. This dimming cell 22 is configured in the same manner as the first mode, except that the negative C plate layer 122D is omitted from the lower laminate 162.
[0205] When sufficient optical characteristics for practical use can be ensured as in this mode, the negative C plate layer can be omitted to simplify the configuration, and the same effect as the above-mentioned mode can be obtained.
[0206] [Other modes] Although specific configurations suitable for implementing the present invention have been described in detail above, the present invention allows combinations of the above-mentioned modes and further allows various modifications of the above-mentioned modes without departing from the spirit of the present invention.
[0207] For example, in the above-mentioned second mode, the transparent electrode is disposed directly below the alignment film to form the lower laminate, but the present invention is not limited to this, and the upper laminate may also be similarly configured by disposing the transparent electrode directly below the alignment film.
[0208] In the above-mentioned mode, the case where the spacers are formed in a columnar shape using photoresist has been described, but the present invention is not limited to this, and so-called bead spacers may also be applied.
[0209] Even when using a dimming cell 22 that uses the above-mentioned E-type linear polarizer, an optically transparent adhesive film 24 can be placed between the curved surface 20 of the light-transmitting plate 21 and the dimming cell 22, and one side of the dimming cell 22 can be adhered to the curved surface 20 of the light-transmitting plate 21.
[0210] <Structure in which the light control cell is sandwiched between light-transmitting plates> The present invention is also applicable to the case where the dimming cell 22 is sandwiched between a pair of light-transmitting plates.
[0211] Fig. 33 is a schematic cross-sectional view showing another example of the light control device 10. The light control device 10 shown in Fig. 33 is basically configured in the same manner as the light control device 10 shown in Fig. 1. That is, an optically transparent adhesive film 24 is disposed between the curved surface 20 of the first light-transmitting plate 221 containing an ultraviolet ray inhibitor and the light control cell 22, and one side of the light control cell 22 is adhered to the curved surface 20 of the first light-transmitting plate 221 by the optically transparent adhesive film 24. In this manner, the first light-transmitting plate 221 is configured in the same manner as the light-transmitting plate 21 shown in Fig. 1.
[0212] However, the light control device 10 shown in FIG. 33 further includes a second light-transmitting plate 222, and the light control cell 22 is disposed between the first light-transmitting plate 221 and the second light-transmitting plate 222. The second light-transmitting plate 222 is disposed apart from the light control cell 22 in the stacking direction of the first light-transmitting plate 221, the optically transparent adhesive film 24, and the light control cell 22, and the space between the second light-transmitting plate 222 and the light control cell 22 is configured as an air gap (air layer). The second light-transmitting plate 222 can be configured in the same manner as the first light-transmitting plate 221, for example, and the surface of the second light-transmitting plate 222 facing the light control cell 22 can be a curved surface similar to the curved surface 20 of the first light-transmitting plate 221. However, the second light-transmitting plate 222 may have a shape different from that of the first light-transmitting plate 221. For example, the surface of the second light-transmitting plate 222 facing the dimming cell 22 may be a curved surface different from the curved surface 20 of the first light-transmitting plate 221, or may be a flat surface. In addition, the components of the second light-transmitting plate 222 may be the same as or different from the components of the first light-transmitting plate 221.
[0213] By providing an air gap between the second light-transmitting plate 222 and the dimming cell 22, the light-adjusting device 10 shown in FIG. 33 has excellent heat insulation performance, and overheating of the light-adjusting device 10 can be prevented.
[0214] 33, the dimming cell 22 is protected by the first light-transmitting plate 221 and the second light-transmitting plate 222. Therefore, the dimming cell 22 does not need to have the hard coat layer 26 shown in FIG.
[0215] Fig. 34 is a schematic cross-sectional view showing another example of the dimming device 10. The dimming device 10 shown in Fig. 34 is basically configured similarly to the dimming device 10 shown in Fig. 33, but the second light-transmitting plate 222 is attached to the other side of the dimming cell 22 via an adhesive layer 223.
[0216] There is no particular limitation on the specific components of the adhesive layer 223. For example, the adhesive layer 223 can be made of a thermoplastic resin with excellent adhesiveness, such as PVB (polyvinyl butyral), or other adhesive materials having optical transparency.
[0217] In the light control device 10 in FIG. 34 as well, since the light control cell 22 is protected by the first light-transmitting plate 221 and the second light-transmitting plate 222, the light control cell 22 does not need to have the hard coat layer .
[0218] Fig. 35 is a schematic cross-sectional view showing another example of the light control device 10. The light control device 10 shown in Fig. 35 is basically configured similarly to the light control device 10 shown in Fig. 33, but the space between the second light-transmitting plate 222 and the light control cell 22 is sealed and airtight by a sealant 225. In the light control cell 22 shown in Fig. 35, the space between the first light-transmitting plate 221 and the second light-transmitting plate 222 is sealed by a sealant 225, and the optically transparent adhesive film 24 and the light control cell 22 are arranged in the airtight space.
[0219] By disposing a functional member in the sealed space between the second light transmitting plate 222 and the dimming cell 22, it is possible to add any function to the light control device 10. For example, by disposing silicone between the second light transmitting plate 222 and the dimming cell 22 sealed by the sealant 225, it is possible to impart the functional properties of silicone to the light control device 10. In addition, it is possible to dispose other fluids (gas and liquid) or solids (including gel-like bodies) having optical transparency between the second light transmitting plate 222 and the dimming cell 22 sealed by the sealant 225. Note that a member containing one or more types of components may be filled in the sealed space between the second light transmitting plate 222 and the dimming cell 22. Furthermore, the sealed space between the second light transmitting plate 222 and the dimming cell 22 may be evacuated.
[0220] <Other functional layers> Any functional layer may be added to the light control device 10 according to the above-described embodiment and modified examples. For example, an anti-reflection layer may be added to the light control device 10 to improve the optical characteristics.
[0221] Fig. 36 is a schematic cross-sectional view showing an example of a light control device 10 including an antireflection layer 300. The light control device 10 shown in Fig. 36 includes a light-transmitting plate 21 having a curved surface 20, a light control cell 22, and an optically transparent adhesive film 24 provided between the light-transmitting plate 21 and the light control cell 22, similar to the light control device 10 shown in Fig. 1. However, in the light control device 10 shown in Fig. 36, an antireflection layer 300 is provided on the outermost layer of the light control cell 22.
[0222] The specific type and configuration of the anti-reflection layer 300 are not particularly limited, but an optical layer that can adjust the reflection of incident light to exhibit excellent anti-glare properties or suppress outward reflection can be used as the anti-reflection layer 300. Typically, the anti-reflection layer 300 includes at least one of an anti-glare (AG) layer that can reduce regular reflection by diffusing incident light, an anti-reflection (AR) layer that can suppress regular reflection by utilizing the interference of reflected light, and a low-reflection (LR) layer that is made of a low-reflection material with low reflectance. Therefore, for example, the anti-reflection layer 300 may be made of an AGLR (Anti-Glare Low Reflection) layer that is made of a combination of an anti-glare layer and a low-reflection layer. The structure, components, and manufacturing method of the functional layers that make up the anti-reflection layer 300 are not particularly limited, and the anti-reflection layer 300 can be made up of any functional layer.
[0223] The antireflection layer 300 shown in Fig. 36 is provided so as to cover the hard coat layer 26 (see Fig. 3) of the dimming cell 22. However, the hard coat layer 26 and the antireflection layer 300 may be realized as a single layer by, for example, mixing fine particles for adjusting reflection in the hard coat layer.
[0224] Although not shown, a functional layer such as the antireflection layer 300 may be provided at another location in the light-adjusting device 10. For example, a functional layer such as an antireflection layer may be provided on the surface of the light-transmitting plate 21 in addition to or instead of the antireflection layer 300 shown in Fig. 1. In this manner, the antireflection layer 300 may be provided on at least one of the light-adjusting cell 22 and the light-transmitting plate 21.
[0225] Fig. 37 is a schematic cross-sectional view showing another example of the dimming device 10 including the anti-reflection layers 300, 301, and 302. The dimming device 10 shown in Fig. 37 includes a first light-transmitting plate 221 having a curved surface 20, a second light-transmitting plate 222, a dimming cell 22 provided between the first light-transmitting plate 221 and the second light-transmitting plate 222, and an optically transparent adhesive film 24 provided between the first light-transmitting plate 221 and the dimming cell 22, similar to the dimming device 10 shown in Fig. 33.
[0226] However, in the light control device 10 shown in Fig. 37, an antireflection layer 300 is provided on the outermost layer of the light control cell 22, and antireflection layers 301 and 302 are provided on the front surface (upper surface in Fig. 37) and rear surface (lower surface in Fig. 37) of the second light transmission plate 222. Note that the antireflection layers 300, 301, and 302 may include at least one of an antiglare layer, an antireflection layer, and a low reflection layer, as described above. The antireflection layers 300, 301, and 302 may have the same function and configuration as each other, or may have different functions and configurations from each other.
[0227] According to the light control device 10 shown in FIG. 37, for example, the antireflection layers 300 and 301 can improve the light transmittance, while the antireflection layer 302 can prevent glare.
[0228] Although not shown, functional layers such as the antireflection layers 300, 301, and 302 may be provided at other locations of the light control device 10. For example, in addition to the antireflection layers 300, 301, and 302 shown in FIG. 37 or instead of the antireflection layers 300, 301, and 302, a functional layer such as an antireflection layer may be provided on the surface of the first light transmission plate 221. Also, any one or two of the antireflection layers 300, 301, and 302 shown in FIG. 37 may not be provided. In this way, it is possible to provide the antireflection layer 300 on at least one of the dimming cell 22 and the second light transmission plate 222. From the viewpoint of improving visibility, it is often preferable to arrange a functional layer such as an antireflection layer on the observer side. Therefore, in the example shown in FIG. 37, when the second light transmission plate 222 is arranged closer to the observer side than the first light transmission plate 221, it is often preferable to arrange a functional layer such as an antireflection layer on the second light transmission plate 222 rather than the first light transmission plate 221.
[0229] The present invention is not limited to the above-mentioned embodiments and modifications, but may include various aspects to which various modifications that a person skilled in the art can conceive, and the effects of the present invention are not limited to the above-mentioned matters. Therefore, various additions, modifications, and partial deletions are possible for each element described in the claims and specification, without departing from the technical idea and purpose of the present invention. For example, the above-mentioned embodiments and modifications may be appropriately combined with each other. [Explanation of symbols]
[0230] 10 Dimmer 20 curved surface 20a 3D curved surface 21 Light-transmitting plate 22 Dimming cell 24 Optically transparent adhesive film 26 Hard coat layer 29 First resin base material 30 Second resin base material 31 1st electrode layer 32 Second electrode layer 33 First alignment film 34 Second alignment film 35 LCD space 36 Sealing material 41 First polarizing plate 42 Second polarizing plate 43 First electrode alignment layer 44 Second electrode alignment layer 45 Phase difference compensation film 45a Phase difference compensation film 46 Adhesive layer 47 Protective layer 48 Polarizing Layer 49 Liquid crystal layer 52 Spacer 53 Hard coat layer 55 Index Matching Layer 61 Dichroic Dyes 62 Liquid crystal 112 Lower laminate 112A Hard coat layer 112B Base material 112C Hard coat layer 112D linear polarizer 112E Alignment film 112F Plate Layer 112G transparent electrode 113 Upper laminate 113A Hard coat layer 113B Base material 113C Hard coat layer 113D transparent electrode 113E Linear polarizer 113F Alignment film 114 Liquid crystal layer 115 Spacer 122 Lower laminate 122A Base material 122B Transparent electrode 122C linear polarizer 122D Plate Layer 122E Alignment film 123 Upper laminate 123A Base material 123B Transparent electrode 123C Linear polarizer 123D alignment film 124 Liquid crystal layer 125 Spacer 132 Lower laminate 142 Lower laminate 142A Adhesive layer 152 Lower laminate 162 Lower laminate 221 First light-transmitting plate 222 Second light-transmitting plate 223 Adhesive layer 225 Sealing material 226 Closed Space 300 Anti-reflection layer 301 Anti-reflection layer 302 Anti-reflection layer
Claims
[Claim 1] A light control device comprising a first light-transmitting plate having a curved surface, a second light-transmitting plate, and a light control cell, the light-controlling cell is disposed between the first light-transmitting plate and the second light-transmitting plate, and includes a first laminate including a first resin base material, a second laminate including a second resin base material, and a liquid crystal layer provided between the first laminate and the second laminate; an optically transparent adhesive film is disposed between the curved surface of the first light-transmitting plate and the light control cell; the second light-transmitting plate is attached to the other side of the dimming cell via an adhesive layer; The optically transparent adhesive film is directly adhered to the curved surface of the first light-transmitting plate and the dimming cell; the first light-transmitting plate and the second light-transmitting plate are glass plates; A sealant is located between the first laminate and the second laminate, The optically transparent adhesive film is made of OCA (Optical Clear Adhesive), A light control device, wherein the adhesive layer disposed over the entire surface between the second light-transmitting plate and the light control cell is made of an OCA (Optical Clear Adhesive).
Citation Information
Patent Citations
Liquid crystal light controlling element for third order surface
JP1994018856A
Dimming device and its manufacturing method
JP2006330100A
Method for laminating film for SPD light valve and SPD light valve incorporating such laminated film
JP2011189751A
Light control panel structure and method for manufacturing the same
JP2014182287A
Solar load reduction panel with controllable light transparency
US5111329A