Plating Equipment
The diaphragm with a silicon ring in the jet plating apparatus separates solutions and discharges bubbles efficiently, addressing inefficiencies in insoluble anode use, improving productivity and solution purity.
Patent Information
- Application Number
- JP2020193072
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-11-20
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2040-11-20
AI Technical Summary
Jet plating apparatus using insoluble anodes face challenges with bubble generation and solution mixing, leading to inefficiencies and incomplete realization of the benefits of insoluble anodes, particularly in large-scale applications.
A diaphragm with a silicon ring is fixed to the plating tank and liquid supply pipe, forming an annular flow path to separate and efficiently discharge bubbles from the lower isolation chamber, while ensuring separate solution flows for each chamber, using a simultaneous casting method to secure the diaphragm.
The solution effectively separates solutions and efficiently discharges bubbles, reducing pressure drop and maintaining solution purity, thereby enhancing the benefits of insoluble anodes in jet plating processes.
Smart Images

Figure 0007587816000001 
Figure 0007587816000002 
Figure 0007587816000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a plating apparatus using an insoluble anode. [Background technology]
[0002] Conventionally, various plating processes have been performed on objects to be plated, such as semiconductor wafers, printed wiring boards, etc. When performing plating processes on such objects to be plated, a so-called jet-type plating apparatus is known.
[0003] This jet-type plating apparatus generally comprises an opening on which the object to be plated can be placed, a liquid supply pipe for supplying plating solution to the object to be plated, and an anode arranged to face the object to be plated, and performs plating while supplying plating solution from the liquid supply pipe to the object to be plated. Jet-type plating apparatuses can perform uniform plating on the surface of the object to be plated, and can sequentially replace the object to be plated placed in the opening for plating, so they are widely used as suitable for small-lot production and automation of plating.
[0004] Although this jet-type plating apparatus has the above-mentioned advantages, when a soluble anode is used, a film formed on the anode surface, such as a black film, may peel off and become an impurity in the solution, which may flow together with the plating solution supplied to the object to be plated and adversely affect the plating process. In addition, air mixed in the solution or bubbles generated from the anode may reach the surface to be plated and hinder good plating. For this reason, a method is known for this jet-type plating apparatus in which a diaphragm is placed in the plating tank to separate the object to be plated from the anode (see Patent Documents 1 and 2). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2000-273693 A (9860P) [Patent Document 2] JP 2007-139773 A (EJ0137-P) Summary of the Invention [Problem to be solved by the invention]
[0006] The use of insoluble anodes in jet-type plating equipment equipped with a diaphragm offers various advantages over the use of soluble anodes, such as reducing the consumption of additives in the plating solution and improving productivity by eliminating the need for maintenance such as anode replacement as in the case of soluble anodes.
[0007] Although jet-type plating equipment using insoluble anodes like this has many advantages over soluble anodes, its use has not progressed much within the plating industry except for precious metal plating and copper plating.
[0008] When a diaphragm is placed in a plating tank of a jet-type plating apparatus, an upper isolation chamber is formed above the diaphragm by the diaphragm and the object to be plated placed on the opening, and a lower isolation chamber is formed below the diaphragm by the plating tank and the diaphragm. Since the insoluble anode is placed on the lower isolation chamber side, a large amount of bubbles appear below the diaphragm during plating due to gas generation caused by electrolysis of water. Therefore, it is necessary to efficiently discharge the bubbles that appear below the diaphragm. In addition, in order to obtain the advantages of using an insoluble anode, different types of solutions are supplied separately to the upper isolation chamber and the lower isolation chamber, but it is required that the diaphragm placed in the plating tank prevents the different types of solutions supplied to the upper isolation chamber and the lower isolation chamber from mixing with each other.
[0009] In the prior art of Patent Document 1, when supplying a solution to the lower isolation chamber, the pressure loss during supply is large, so the supply flow rate to the lower isolation chamber cannot be increased very much, and the large amount of bubbles generated from the insoluble anode tends to be unable to be sufficiently discharged. Also, in Patent Document 2, although the bubbles can be efficiently discharged in the lower isolation chamber, the solutions supplied to the upper isolation chamber and the lower isolation chamber cannot be separated, so the benefits of the insoluble anode cannot be fully realized.
[0010] The present invention has been made under the above circumstances, and has an object to provide a jet-type plating apparatus that uses an insoluble anode and can fully enjoy the benefits of the insoluble anode. [Means for solving the problem]
[0011] In order to solve the above problems, the present invention provides a plating apparatus comprising a plating tank having an opening for placing an object to be plated, a liquid supply pipe for supplying a plating solution toward the object to be plated, an insoluble anode arranged to face the object to be plated, and a diaphragm for isolating the object to be plated and the insoluble anode, wherein the outer peripheral end of the diaphragm is fixed to the inner wall of the plating tank and the peripheral end of a through hole provided in the center of the diaphragm is fixed to the liquid supply pipe, so that the diaphragm is arranged so as to be inclined upward from the liquid supply pipe toward the outer periphery, the plating apparatus being characterized in that a silicon ring is fixed to the outer peripheral end of the diaphragm and to the edge of the through hole of the diaphragm, the liquid supply pipe supplies plating solution to an upper isolated chamber in the plating tank formed by the diaphragm and the placed object to be plated, a ring-shaped flow path having a liquid discharge hole at an upper part is provided on the outer periphery of the liquid supply pipe, and a lower isolated chamber solution is supplied from the liquid discharge hole to a lower isolated chamber in the plating tank formed below the diaphragm, thereby forming a flow in the lower isolated chamber solution from the periphery of the through hole of the diaphragm toward the outer periphery of the diaphragm.
[0012] According to the plating apparatus of the present invention, the separate solutions supplied to the lower isolation chamber and the upper isolation chamber do not directly mix with each other. To achieve this, silicon rings are fixed to the outer periphery of the diaphragm and the edge of the through hole of the diaphragm. An annular flow path having a liquid discharge hole at the top is provided on the outer periphery of the liquid supply pipe, and the lower isolation chamber solution is supplied from the liquid discharge hole to the lower isolation chamber in the plating tank formed below the diaphragm. By forming a flow of the lower isolation chamber solution from the periphery of the through hole of the diaphragm toward the outer periphery of the diaphragm, the gas (bubbles) generated from the insoluble anode can be efficiently discharged from the lower isolation chamber.
[0013] When the silicon ring is fixed to the diaphragm in the plating apparatus according to the present invention, it is preferable to use a method of simultaneous casting of the silicon ring. In the simultaneous casting of the silicon ring, the diaphragm is fixed to a formwork that can press the outer peripheral end of the diaphragm and the hole edge of the through hole from above and below, an adhesive (primer) is applied to the outer peripheral end part and the hole edge part to which the silicon ring is fixed, silicon is injected into the adhesive-applied part, and the formwork is pressed. When the formwork is removed after the silicon has hardened, the silicon ring is fixed to the outer peripheral end of the diaphragm and the hole edge of the through hole of the diaphragm. When the diaphragm has such a silicon ring fixed thereto, it is possible to reliably prevent leakage of the solution from the outer peripheral end part of the diaphragm that is fixed to the inner wall of the plating tank and the hole edge part of the through hole in the center of the diaphragm that is fixed to the liquid supply pipe. There is no particular restriction on the material of the diaphragm, and it may be selected in consideration of the liquid permeability and plating solution resistance, but it is preferable to use a diaphragm whose base material is polyethylene terephthalate resin and whose material is polyvinylidene fluoride resin. 2 It is preferable that:
[0014] In the plating apparatus according to the present invention, it is preferable that the solution for the lower isolation chamber is supplied in the circumferential direction of an annular flow path provided on the outer periphery of the solution supply pipe. By flowing the solution for the lower isolation chamber into the lower isolation chamber while rotating it, it is possible to reduce pressure loss during solution supply and increase the supply amount, and it is possible to highly efficiently exhaust gas (bubbles) generated from the insoluble anode from the lower isolation chamber.
[0015] The plating apparatus according to the present invention is preferably provided with a flow rate controller for controlling the supply flow rate of the lower isolation chamber solution supplied to the lower isolation chamber. When the plating process is completed and the workpiece is removed from the opening, the upper side of the diaphragm is opened, and the liquid pressure of the lower isolation chamber solution supplied to the lower isolation chamber is applied from the lower side of the diaphragm. If such pressure from one side is continuously applied to the diaphragm, it tends to cause deformation of the diaphragm. Therefore, when the workpiece is removed from the opening, it is preferable to control the supply flow rate of the lower isolation chamber solution with a flow rate controller so that excessive liquid pressure is not applied to the diaphragm. Effect of the Invention
[0016] According to the present invention, in a jet-type plating apparatus, plating processing that can fully utilize the advantages of an insoluble anode is possible. [Brief description of the drawings]
[0017] [Figure 1] FIG. 2 is a cross-sectional view of the plating apparatus according to the present embodiment. [Diagram 2] FIG. 2 is a plan view of the plating apparatus according to the embodiment. [Diagram 3] Cross-sectional view of the plating apparatus at AA. [Figure 4] Top view of the diaphragm. [Diagram 5] Explanation of the simultaneous casting process. [Figure 6] A line graph showing the change in concentration of each additive. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] An embodiment of the present invention will be described with reference to the drawings. Fig. 1 shows a cross-sectional view of a plating apparatus according to the present embodiment, and Fig. 2 shows a plan view of the plating apparatus.
[0019] In the plating apparatus of this embodiment, a doughnut-shaped diaphragm 2 having a through hole in the center is installed in a plating tank 1, and the outer peripheral end of the diaphragm 2 is fixed to the inner wall of the plating tank, and the side of the through hole is fixed to the tip side of a liquid supply pipe 3, so that the diaphragm 2 is inclined upward from the liquid supply pipe 3 toward the outer periphery (the diaphragm is not shown in the plan view of FIG. 2). An annular flow path 4 is provided on the outer periphery of the liquid supply pipe 3. In addition, a mesh-like insoluble anode 5 is arranged at the bottom of the plating tank 1 (the insoluble anode is not shown in the plan view of FIG. 2).
[0020] When a wafer W to be plated is placed in the opening of plating tank 1, an upper isolated chamber U and a lower isolated chamber D are formed in plating tank 1. A plating solution is supplied to the upper isolated chamber U through a liquid supply pipe 3. A solution for the lower isolated chamber is supplied to the lower isolated chamber D through a liquid discharge hole 6 provided in the upper part of annular flow path 4.
[0021] Fig. 3 shows a cross-sectional view of line A-A' in Fig. 2. The solution is supplied to the annular flow path 4 through a lower isolation chamber solution supply pipe 7 provided on the bottom side of the plating tank, and this lower isolation chamber solution supply pipe 7 is configured to supply the solution in the circumferential direction of the annular flow path 4. The solution for the lower isolation chamber supplied through the lower isolation chamber solution supply pipe 7 flows into the lower isolation chamber D through the liquid discharge hole 6 while rotating and flowing in the annular flow path 4. The solution for the lower isolation chamber that has flowed into the lower isolation chamber D forms a flow that spreads along the lower surface of the diaphragm 2 to the outer periphery of the diaphragm 2.
[0022] The plating solution supplied to the upper isolation chamber D is guided to a liquid discharge outlet 8 provided in the plating tank 1 and discharged, and the solution for the lower isolation chamber supplied to the lower isolation chamber D is guided to a solution discharge outlet 9 provided in the plating tank 1 and discharged.
[0023] FIG. 4 shows a plan view of the diaphragm 2. A silicon ring 10 is attached to the outer peripheral edge 2' of the diaphragm 2 and to the edge of the through-hole 2". This silicon ring 10 is attached by a silicon ring simultaneous casting method. FIG. 5 shows a cross-sectional view of the simultaneous casting method, taking as an example the case of fixing a silicon ring to the outer peripheral edge side of the diaphragm. An upper mold 21 and a lower mold 22 that are capable of clamping the edge along the outer peripheral edge are arranged on the outer peripheral edge side of the diaphragm 2, and the diaphragm 2 is fixed thereto. The upper mold 21 and the lower mold 22 are processed so that a ring-forming space 23 is formed at the outer peripheral edge when the diaphragm 2 is clamped. The upper mold 21 has an injection path 24 for injecting silicon resin into the ring-forming space 23. Using such a mold, a diaphragm with a silicon ring attached was produced as shown in FIG. 4.
[0024] Next, a description will be given of the results of a test carried out by the plating apparatus of this embodiment, in which a copper plating process was carried out using a copper sulfate plating solution, and changes in the concentration of additives in the plating solution were examined.
[0025] In this test, copper sulfate plating solution containing three types of additives (commercially available products) called accelerator, suppressor, and leveler was supplied to the upper isolated chamber on the cathode side, and copper sulfate plating solution without additives was supplied to the lower isolated chamber on the anode side. The solution composition is shown below.
[0026] *Upper isolation room supply fluid: Copper sulfate plating solution (commercially available Microfab Cu525 / manufactured by Electroplating Engineers of Japan, Ltd.) Copper concentration...60g / L Sulfuric acid concentration...30g / L Accelerator (accelerator) 3mL / L Suppressor: 10mL / L Leveler (smoothing agent) 10mL / L Liquid temperature: 22~23℃ Liquid volume: 40L ·Supply flow rate 25L / min *Lower isolation room supply fluid: Copper sulfate plating solution (commercially available Microfab Cu525 / manufactured by Electroplating Engineers of Japan, the same solution as in the upper isolation chamber) Liquid temperature: 22~25℃ Liquid volume: 20L ·Supply flow rate 5L / min
[0027] The plating equipment used a mesh-shaped insoluble anode made of Pt-Ti, and the diaphragm was a commercially available product (membrane material: fluororesin, thickness: 0.12 mm, water permeability: 0.08 mL / min / cm 2 25℃) was used. An 8-inch PCB wafer was used as the object to be plated. This PCB wafer was made by attaching copper foil to a glass epoxy base material and processing it into a circular wafer shape.
[0028] The test method was to perform copper plating on a PCB wafer at 3A for 7 hours, and then to analyze the concentrations of copper, sulfuric acid, additives, etc. by sampling the upper isolation chamber supply solution and the lower isolation chamber supply solution immediately after plating. The upper isolation chamber supply solution was sampled after replenishing the upper isolation chamber supply solution immediately after plating with the same amount of copper as that consumed in the copper plating process. After plating, the solution was left for a specified time (16 hours). This leaving for a specified time and copper plating process were repeated five times to investigate the changes in the concentrations of copper, sulfuric acid, additives, etc. In addition, in order to investigate the deterioration of the solution over time, the solution was left for 48 hours after the fifth plating process, and then the changes in the concentrations of copper, sulfuric acid, additives, etc. were investigated without plating (sixth time). The results are shown in Figure 6. During the leaving period, the supply rate of the upper isolation chamber supply solution was 8 to 10 L / min, and the supply rate of the upper isolation chamber supply solution was 1 to 2 L / min.
[0029] Figure 6 shows the change in the concentration of each additive in the upper isolation chamber supply liquid and the lower isolation chamber supply liquid, with the concentration change being shown in a line graph in the order of accelerator, suppressor, and leveler from top to bottom. In each line graph, the vertical axis indicates the additive concentration (mL / L), the horizontal axis indicates the time of concentration measurement, with ■ indicating the concentration of the upper isolation chamber supply liquid and ● indicating the concentration of the lower isolation chamber supply liquid.
[0030] As shown in Figure 6, in the solution supplied to the lower isolation chamber, which does not contain additives, no additive components were detected even after the solution was left for a long time. In the solution supplied to the upper isolation chamber, there was a tendency for each additive to gradually decrease as the number of plating processes increased. Among these, the decrease in the concentration of the leveler was large, but compared to the decrease rate when a soluble anode was used, the decrease rate was considerably smaller. Furthermore, there was almost no change in the copper concentration and sulfuric acid concentration in either the solution supplied to the upper isolation chamber or the solution supplied to the lower isolation chamber.
[0031] From the test results, it was found that in the plating apparatus of this embodiment, the upper isolation chamber supply liquid and the lower isolation chamber supply liquid are controlled in a state of being completely separated by the diaphragm. It was also found that additives can be easily controlled in the upper isolation chamber supply liquid, and it was also found that the consumption of additives such as levelers, which are consumed in large amounts when a soluble anode is used, can be reduced. Furthermore, since the amount of solution supplied during the standstill was controlled, no deformation of the diaphragm was confirmed. [Explanation of symbols]
[0032] 1 Plating tank 2 Diaphragm 3 Liquid supply pipe 4 Annular flow path 5 Insoluble anode 6 Liquid discharge hole 7 Solution supply pipe for lower isolation chamber 8 Liquid outlet 9 Solution outlet 10 Silicone Ring 21 Upper mold 22 Lower mold 23 Ring-forming space 24 Injection path U upper isolation room D Lower isolation room W Wafer
Claims
1. a plating tank having an opening for placing an object to be plated, a liquid supply pipe for supplying a plating solution toward the object to be plated, an insoluble anode disposed so as to face the object to be plated, and a diaphragm for isolating the object to be plated and the insoluble anode; In a plating apparatus, an outer peripheral end of a diaphragm is fixed to an inner wall of a plating tank, and a peripheral end of a through hole provided in the center of the diaphragm is fixed to a liquid supply pipe, so that the diaphragm is arranged so as to have an upward inclination from the liquid supply pipe toward the outer periphery, A silicon ring is fixed to the outer peripheral edge of the diaphragm and to the edge of the through hole of the diaphragm. The liquid supply pipe supplies the plating liquid to an upper isolated chamber in the plating tank formed by the diaphragm and the object to be plated placed therein, An annular flow passage having a liquid discharge hole at the top is provided on the outer periphery of the liquid supply pipe, and the lower isolation chamber solution is supplied in the circumferential direction of the annular flow passage to the lower isolation chamber formed in the plating tank below the diaphragm, and the lower isolation chamber solution is caused to rotate and flow, A plating apparatus characterized in that a lower isolation chamber solution flows in a rotational manner from the periphery of the through hole of the diaphragm toward the outer periphery of the diaphragm.
2. 2. The plating apparatus according to claim 1, further comprising a flow rate controller for controlling a supply flow rate of the lower isolation chamber solution supplied to the lower isolation chamber.
Citation Information
Patent Citations
EJ0137-P
Cup-type plating equipment
JP2000273693A
Substrate plating device
JP2002004099A
Metal plating method and metal plating device
JP2006028629A
Measuring apparatus and operating method for optical imaging system
JP2007139773A