Plating apparatus and plating method

The plating apparatus and method address uneven film thickness on polygonal substrates by using an adjustable anode mask and regulation plate to control the electric field and current distribution, achieving improved uniformity on polygonal substrates.

JP7590492B2Active Publication Date: 2024-11-26EBARA CORP
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023083690
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-05-22
Publication Date
2024-11-26
Estimated Expiration
2042-06-27

AI Technical Summary

Technical Problem

In polygonal substrates, the plating film thickness distribution is uneven due to the low symmetry of the substrate shape, leading to significant differences near corners and the center, which conventional methods struggle to address effectively.

Method used

A plating apparatus and method that utilizes an anode mask with adjustable mask members and a regulation plate to control the electric field and plating solution stirring, ensuring uniformity by adjusting the distance between mask members and using auxiliary anodes to balance current distribution.

Benefits of technology

The apparatus and method improve the in-plane uniformity of the plating film on polygonal substrates by minimizing thickness variations near corners and enhancing overall film consistency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007590492000001
    Figure 0007590492000001
  • Figure 0007590492000002
    Figure 0007590492000002
  • Figure 0007590492000003
    Figure 0007590492000003
Patent Text Reader

Abstract

To improve the in-plane uniformity of a film plated on a polygonal substrate.SOLUTION: A plating apparatus comprises: a plating tank; a substrate holder configured so as to hold a polygonal substrate; an anode arranged in the plating tank so as to face the substrate held by the substrate holder; and an anode mask for demarcating an aperture corresponding to the outer shape of the polygonal substrate. The anode mask includes: a first mask member for demarcating a first protrusion part that protrudes toward the center of the aperture in the central part of a first aperture side corresponding to a first side of the polygonal substrate in the aperture; and a second mask member for demarcating a second protrusion part that protrudes toward the center of the aperture in the central part of a second aperture side corresponding to a second side of the polygonal substrate in the aperture. The distance between the first mask member and the second mask member can be adjusted.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to a plating apparatus and a plating method. [Background technology]

[0002] Conventionally, wiring has been formed in fine wiring grooves, holes, or resist openings provided on the surface of a substrate such as a semiconductor wafer, and bumps (projecting electrodes) that are electrically connected to electrodes of a package, etc., have been formed on the surface of the substrate. Methods for forming such wiring and bumps include, for example, electrolytic plating, vapor deposition, printing, and ball bump methods. As the number of I / Os on semiconductor chips increases and the pitch becomes finer, electrolytic plating, which allows finer processing and has relatively stable performance, has come to be used more frequently.

[0003] When forming wiring or bumps by electrolytic plating, a seed layer (power supply layer) with low electrical resistance is formed on the surface of a barrier metal provided in wiring grooves, holes, or resist openings on a substrate. A plating film grows on the surface of this seed layer.

[0004] Typically, the substrate to be plated has an electrical contact at its periphery. That is, the current flows from the center of the substrate to the periphery. As the distance from the center of the substrate increases, the potential gradually drops by the amount of the electrical resistance of the seed layer, resulting in a more negative potential at the substrate's periphery than at the substrate's center. This phenomenon, in which the reduction current of metal ions, i.e., the plating current, is concentrated at the substrate's periphery due to the potential difference between the substrate's center and periphery, is called the terminal effect.

[0005] Known shapes of substrates to be plated by electrolytic plating include circular substrates and rectangular substrates (see, for example, Patent Documents 1 and 2).

[0006] In a circular substrate, the distance from the center of the circular substrate to the periphery of the substrate and the distance between adjacent electrical contacts are the same all around the substrate. Therefore, the terminal effect when plating a circular substrate occurs almost the same all around the substrate. Therefore, when plating a circular substrate, the plating speed at the center of the substrate decreases, and the thickness of the plating film at the center of the substrate becomes thinner than that at the periphery of the substrate. In the past, in order to suppress the decrease in the in-plane uniformity of the film thickness due to the terminal effect, a regulation plate, for example as disclosed in Patent Document 3, was used to adjust the electric field applied to the circular substrate, i.e., the advection of electroactive ions, while supplying current to electrical contacts evenly arranged on the periphery of the circular substrate. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 09-125294 [Patent Document 2] Special Publication No. 03-029876 [Patent Document 3] JP 2005-029863 A Summary of the Invention [Problem to be solved by the invention]

[0008] However, when electrical contacts are arranged on the periphery of all sides of a polygonal substrate, if a regulation plate or anode mask with an opening of a similar shape to the substrate is used in the same manner as for a circular substrate, the substrate itself has low symmetry, and the plating thickness distribution tendency differs between the vicinity of the corners and the center of the sides (the center between the vertices). Singular points are easily generated in the distribution, and in the case of polygonal substrates, the final plating thickness tends to be smaller in areas close to the corners, which are relatively far from the center.

[0009] In addition, these effects change depending on the resist opening ratio of the polygonal substrate to be processed, the plating recipe, and the use state of the plating solution. For this reason, it is also possible to make the opening size of the anode mask changeable depending on the plating processing conditions. However, for example, when the above-mentioned terminal effect is small and when it is large, the film thickness tendency is significantly different between the corners and other areas, and simply adjusting the opening size may not be enough to sufficiently improve the in-plane uniformity of the plating film.

[0010] The present invention has been made in view of the above-mentioned problems, and one of its objects is to improve the in-plane uniformity of a film plated on a polygonal substrate. [Means for solving the problem]

[0011] According to one embodiment, a plating apparatus is proposed, the plating apparatus comprising: a plating tank; a substrate holder configured to hold a polygonal substrate; an anode arranged in the plating tank to face the substrate held in the substrate holder; and an anode mask defining an opening corresponding to the outline of the polygonal substrate, the anode mask having a first mask member defining a first convex portion protruding toward the center of the opening at a central portion of a first opening edge corresponding to a first side of the polygonal substrate in the opening; and a second mask member defining a second convex portion protruding toward the center of the opening at a central portion of a second opening edge corresponding to a second side of the polygonal substrate in the opening, the anode mask being configured so that the distance between the first mask member and the second mask member can be adjusted.

[0012] According to another embodiment, a method for plating a polygonal substrate by passing an electric current between an anode and the polygonal substrate in a plating apparatus is proposed, the plating method including an anode mask defining an opening corresponding to the outline of the polygonal substrate, the anode mask having a first mask member defining a first convex portion protruding toward the center of the opening at a central portion of a first opening edge in the opening corresponding to a first side of the polygonal substrate, and a second mask member defining a second convex portion protruding toward the center of the opening at a central portion of a second opening edge in the opening corresponding to a second side of the polygonal substrate, the plating method including the steps of adjusting the distance between the first mask member and the second mask member, and passing an electric current between the anode and the polygonal substrate. [Brief description of the drawings]

[0013] [Figure 1] 1 is an overall layout diagram of a plating apparatus according to an embodiment; [Diagram 2] 1 is a schematic cross-sectional side view (longitudinal cross-sectional view) of a plating unit provided in a plating apparatus. [Figure 3A] FIG. 2 is a diagram showing an anode mask from the substrate side in one embodiment. [Figure 3B] FIG. 2 is a diagram showing an anode mask from the substrate side in one embodiment. [Figure 3C] FIG. 2 is a diagram showing an anode mask from the substrate side in one embodiment. [Figure 4A] FIG. 2 is a diagram showing a regulation plate from the substrate side in one embodiment. [Figure 4B] FIG. 2 is a diagram showing a regulation plate and an anode mask from the substrate side in one embodiment. [Figure 5A] 1 is a schematic diagram showing a plating film thickness when plating a square substrate using the plating apparatus of the present embodiment under conditions in which the terminal effect is large. FIG. [Figure 5B] 1 is a schematic diagram showing a plating film thickness when plating a square substrate using the plating apparatus of the present embodiment under conditions of a moderate terminal effect. FIG. [Figure 5C]1 is a schematic diagram showing a plating film thickness when plating a square substrate using the plating apparatus of the present embodiment under conditions in which the terminal effect is small. FIG. [Figure 6A] FIG. 11 is a schematic diagram showing a plating film thickness when plating a square substrate using a plating apparatus of a comparative example under conditions in which the terminal effect is large. [Figure 6B] FIG. 1 is a schematic diagram showing a plating film thickness when plating is performed on a square substrate using a plating apparatus of a comparative example under conditions of a moderate terminal effect. [Figure 6C] FIG. 11 is a schematic diagram showing a plating film thickness when plating a square substrate using a plating apparatus of a comparative example under conditions in which the terminal effect is small. [Figure 7] FIG. 2 is a schematic front view of a substrate holder used in the plating unit. [Figure 8] FIG. 2 is a schematic side view of a substrate holder. [Figure 9] FIG. 4 is a rear view of the front plate body. [Figure 10] 13 is an enlarged rear view showing the vicinity of a corner of the face portion closer to the connector. FIG. [Figure 11A] FIG. 13 is a view showing an anode mask in a modified example, viewed from the substrate side. [Figure 11B] FIG. 13 is a view showing an anode mask in a modified example, viewed from the substrate side. [Figure 11C] FIG. 13 is a view showing an anode mask in a modified example, viewed from the substrate side. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings described below, the same or corresponding components are designated by the same reference numerals and redundant description will be omitted.

[0015] Fig. 1 shows an overall layout of a plating apparatus according to an embodiment. As shown in Fig. 1, the plating apparatus has two cassette tables 102 on which cassettes 100 containing substrates such as semiconductor wafers are mounted, an aligner 104 for aligning the position of the substrate in a predetermined direction, and a rinse dryer 106 for drying the substrate after plating. A substrate loading / unloading section 120 for loading the substrate holder 30 thereon and loading / unloading the substrate is provided near the rinse dryer 106. A substrate transport device 122 consisting of a transport robot for transporting substrates between these units is provided in the center of these units 100, 104, 106, and 120.

[0016] The substrate loading / unloading section 120, a stocker 124 for storing and temporarily placing the substrate holder 30, a pre-wet tank 126 for immersing the substrate in pure water, a pre-soak tank 128 for etching away an oxide film on the surface of a conductive layer such as a seed layer formed on the surface of the substrate, a first cleaning tank 130a for cleaning the substrate after pre-soaking together with the substrate holder 30 with a cleaning liquid (such as pure water), a blow tank 132 for draining the substrate after cleaning, a second cleaning tank 130b for cleaning the substrate after plating together with the substrate holder 30 with a cleaning liquid, and the plating unit 10 are arranged in the following order.

[0017] The plating unit 10 is configured by housing a plurality of plating tanks 14 inside an overflow tank 136. Each plating tank 14 houses one substrate therein, and is adapted to immerse the substrate in the plating solution held therein to perform plating such as copper plating on the substrate surface.

[0018] The plating apparatus includes a substrate holder transport device 140, which is positioned to the side of each of these devices and transports the substrate holder 30 together with the substrate between each of these devices, and which employs, for example, a linear motor system. The substrate holder transport device 140 includes a first transporter 142 that transports the substrate between the substrate loading / unloading section 120, the stocker 124, the pre-wet tank 126, the pre-soak tank 128, the first cleaning tank 130a, and the blow tank 132, and a second transporter 144 that transports the substrate between the first cleaning tank 130a, the second cleaning tank 130b, the blow tank 132, and the plating unit 10. The plating apparatus may include only the first transporter 142, without including the second transporter 144.

[0019] On the opposite side of the overflow tank 136 from this substrate holder transport device 140, a paddle drive device 146 is arranged which is located inside each plating tank 14 and drives a paddle 16 (see Figure 2) which acts as a stirring rod to stir the plating solution in the plating tank 14.

[0020] The substrate attachment / detachment section 120 is equipped with a flat loading plate 152 that can slide laterally along rails 150. The two substrate holders 30 are placed horizontally in parallel on this loading plate 152, and after a substrate is transferred between one substrate holder 30 and the substrate transport device 122, the loading plate 152 is slid laterally, and a substrate is transferred between the other substrate holder 30 and the substrate transport device 122.

[0021] The plating apparatus also includes a control device 17 for controlling the entire apparatus. The control device 17 can be configured, for example, from a general computer or a dedicated computer that is provided with an input / output interface with an operator.

[0022] Fig. 2 is a schematic side cross-sectional view (longitudinal cross-sectional view) of a plating unit 10 provided in the plating apparatus shown in Fig. 1. As shown in Fig. 2, the plating unit 10 has a plating tank 14 configured to accommodate a plating solution, a substrate holder 30, and an anode holder 13, and an overflow tank (not shown). The substrate holder 30 is configured to hold a polygonal substrate Wf, and the anode holder 13 is configured to hold an anode 12 having a metal surface. The polygonal substrate Wf and the anode 12 are electrically connected via a plating power source 15, and a plating film is formed on the surface of the substrate Wf by passing a current between the substrate Wf and the anode 12.

[0023] The anode holder 13 has an anode mask 18 for adjusting the electric field between the anode 12 and the substrate Wf. The anode mask 18 is, for example, a substantially plate-shaped member made of a dielectric material, and is provided on the front surface of the anode holder 13. Here, the front surface of the anode holder 13 refers to the surface facing the substrate holder 30. In other words, the anode mask 18 is disposed between the anode 12 and the substrate holder 30. The anode mask 18 has an opening 18a in the substantially central portion through which a current flows between the anode 12 and the substrate Wf.

[0024] 3A to 3C are views showing the anode mask 18 in one embodiment from the substrate Wf side. The anode mask 18 has a frame member 182 that defines a polygonal opening corresponding to the polygonal shape of the substrate Wf, and a plurality of mask members 184 to 187 that are arranged adjacent to the frame member 182 and are movable relative to the frame member 182. In the example shown in FIGS. 3A to 3C, the substrate Wf has a substantially square plate shape, and the frame member 182 defines a substantially square opening 182a. Four mask members 184 to 187 are provided corresponding to each side of the opening 182a. For ease of viewing, the frame member 182 and the four mask members 184 to 187 are each hatched. In this embodiment, the four mask members 184 to 187 have the same shape and are arranged rotated by 90 degrees. However, the four mask members 184 to 187 may have different shapes. Representatively, in FIGS. 3A to 3C, mask member 184 provided corresponding to the upper side of opening 182a is hatched differently from other mask members 185 to 187.

[0025] Each of the mask members 184-187 has side portions 184a-187a along the sides of the substrate Wf (along the opening sides of the frame member 182) and protruding portions 184b-187b provided at positions corresponding to the centers of the sides of the substrate Wf and protruding toward the center (inner circumference side) of the anode mask 18. As an example, the protruding portions 184b-187b have a trapezoidal shape that narrows toward the center of the opening 18a of the anode mask 18. The mask members 184-187 are configured to be movable relative to the frame member 182, and together with the frame member 182, define the opening 18a of the anode mask 18. In the example shown in FIG. 3A, the mask members 184-187 are located outside and do not overlap with the opening 182a of the frame member 182, and the opening 182a of the frame member 182 becomes the opening 18a of the anode mask 18. From this state, when each of the mask members 184 to 187 is moved toward the center with respect to the frame member 182, as shown in FIG. 3B, an opening defined by a part of the frame member 182 and a part of the protrusions 184b to 187b of the mask members 184 to 187 becomes an opening of the anode mask 18. Then, when each of the mask members 184 to 187 is further moved toward the center with respect to the frame member 182, the protrusions 184b to 187b and the side portions 184a to 187a of the mask members 184 to 187 protrude into the opening 182a of the frame member 182, as shown in FIG. 3C. In the example shown in FIG. 3C, an opening defined by the mask members 184 to 187 becomes the opening 18a of the anode mask 18. 3A, 3B, and 3C each show one example of the state of the openings 18a of the anode mask 18, and it is sufficient that the positions of the multiple mask members 184 to 187 can be smoothly changed.

[0026] The anode mask 18 is made of, for example, vinyl chloride, which is a dielectric material. The frame member 182 and the mask members 184 to 187 may be made of the same material. The mask members 184 to 187 are preferably arranged adjacent to the frame member 182. The mask members 184 to 187 may be arranged on the side of the frame member 182 opposite to the anode 12, or on the side of the anode 12. The mask members 184 to 187 are configured to be movable relative to the frame member 182. The mask members 184 to 187 may be configured so that the distances from the center of the opening 18a of the anode mask 18 are equal to each other. The mask members 184 to 187 may be moved manually. The plating unit 10 may also include a moving mechanism (not shown) for moving the mask members 184 to 187. A known mechanism may be adopted as the moving mechanism, and may be realized by using, for example, a motor and a ball screw. The control device 17 of the plating device may control the movement mechanism so that the shape of the openings in the anode mask 18 is changed during plating. It is preferable that the distance between the mask members 184-187 and between the mask members 184-187 and the frame member 182 in the direction perpendicular to the surface of the substrate Wf is sufficiently close to each other compared to the inter-electrode distance (the distance between the anode 12 and the substrate Wf), but they may be spaced apart to some extent due to restrictions on installing the movement mechanism or other reasons.

[0027] As described above, the anode mask 18 has a frame member 182 and a plurality of mask members 184 to 187, and the openings 18a of the anode mask 18 are defined by the frame member 182 and the mask members 184 to 187. The anode mask 18 has a first mask member (e.g., mask member 184) that is provided on a first opening side corresponding to a first side (e.g., upper side) of the substrate Wf and defines a convex portion protruding toward the center of the opening 18a, and a second mask member (e.g., mask member 186) that is provided on a second opening side corresponding to a second side (e.g., lower side) opposite to the first side of the substrate Wf and defines a convex portion protruding toward the center of the opening 18a. The first mask member 184 and the second mask member 186 are configured to be movable with respect to the frame member 182, and the distance between them can be adjusted. The anode mask 18 also includes a third mask member (e.g., mask member 185) that is provided on a third opening side corresponding to the third side (e.g., right side) of the substrate Wf and defines a convex portion protruding toward the center of the opening 18a, and a fourth mask member (e.g., mask member 187) that is provided on a fourth opening side corresponding to the fourth side (e.g., left side) facing the third side of the substrate Wf and defines a convex portion protruding toward the center of the opening 18a. The third mask member 185 and the fourth mask member 187 are configured to be movable relative to the frame member 182, and the distance between them can be adjusted. In this embodiment, the first to fourth mask members 184 to 187 are configured to be movable in a direction perpendicular to the opening sides on which they are respectively disposed.

[0028] By configuring the anode mask 18 in this manner, the shape of the openings 18a in the anode mask 18 can be adjusted by moving the mask members 184-187. It is known that in a polygonal substrate, when the terminal effect is large, the final plating thickness tends to be smaller near the vertices of the substrate than in the areas between the vertices. In the anode mask 18 of this embodiment, the projections 184b-187b of the mask members 184-187 form a central A convex portion protruding toward the substrate is formed in the opening 18a (see Figs. 3B and 3C), and even if the mask members 184-187 are moved inward to reduce the area of ​​the opening 18a, the apex of the opening 18a is not covered much. The anode mask 18 has the opening 18a shaped as described above, which can improve the in-plane uniformity of the film plated on the substrate. The dimensions and shapes of the convex portions 184b-187b of the mask members 184-187 may be appropriately determined by experiment or simulation so as to improve the in-plane uniformity of the plating film.

[0029] The description will be made with reference to FIG. 2 again. The plating unit 10 has a regulation plate (adjustment plate) 20 for adjusting the electric field between the substrate Wf and the anode 12, and a paddle 16 for stirring the plating solution. The regulation plate 20 is disposed between the substrate holder 30 and the anode 12. As a specific example, the lower end of the regulation plate 20 is inserted between a pair of protruding members 28 provided on the floor surface of the plating tank 14, and the regulation plate 20 is fixed to the plating tank 14. The regulation plate 20 also has an arm (not shown) protruding outward near the upper end, and may be supported in a suspended state by hooking the arm on the upper surface of the peripheral wall of the stocker 124 shown in FIG. 1. The paddle 16 is disposed between the substrate holder 30 and the regulation plate 20.

[0030] FIG. 4A is a view showing the regulation plate 20 in one embodiment from the substrate Wf side. FIG. 4B is a view showing the regulation plate 20 and the anode mask 18 in one embodiment from the substrate Wf side. The regulation plate 20 has a polygonal opening 21 corresponding to the polygonal shape of the substrate Wf. In the example shown in FIG. 4A, the polygonal opening 21 is substantially square-shaped, and a convex portion 20b protruding toward the center is formed from each of the four sides, although this is not limited thereto. By forming such a convex portion not only on the anode mask 18 but also on the regulation plate 20, it is possible to further improve the tendency of the plating film thickness to become smaller in the region near the corner, which is seen when the terminal effect is large. As shown in the example shown in FIG. 4A, the convex portion 20b has a trapezoidal shape, and it is preferable that the convex portion has a slope on both sides, and the opening size formed between the convex portion on the other opposing side of the polygonal opening 21 changes continuously. This suppresses the occurrence of undulations in the plating film thickness distribution due to a sudden change in the degree of electric field shielding near the boundary between the convex portion 20b formation portion and the other portion, and improves the in-plane uniformity of the plating formed on the substrate Wf. As shown in FIG. 4B, in this embodiment, the polygonal opening 21 of the regulation plate 20 has a larger dimension than the opening 18a of the anode mask 18. In this embodiment, the regulation plate 20 has auxiliary anodes 214-217 arranged on each opening side of the polygonal opening 21. In other words, the multiple auxiliary anodes 214-217 are arranged corresponding to the convex portions 184b-187b of the multiple mask members 184-187. The polygonal substrate Wf and the auxiliary anodes 214-217 are electrically connected via the plating power source 15 or an auxiliary power source not shown.

[0031] The control device 17 can adjust the voltage applied between the auxiliary anodes 214-217 and the substrate Wf to adjust the current flowing between the auxiliary anodes 214-217 and the substrate Wf. As a specific example, the control device 17 increases the current flowing between the auxiliary anodes 214-217 and the substrate Wf as the distance between the mask members 184-187 in the anode mask 18 increases. In other words, when it is assumed that the thickness of the plating film is small in the center of the substrate Wf and large in the peripheral portion of the substrate Wf due to a so-called terminal effect or the like, the control device 17 decreases the distance between the mask members 184-187 in the anode mask 18 and reduces or eliminates the current flowing between the auxiliary anodes 214-217 and the substrate Wf. In addition, when it is assumed that the thickness of the plating film is large in the center of the substrate Wf and small in the peripheral portion of the substrate Wf, the control device 17 decreases the distance between the mask members 184-187 in the anode mask 18 and reduces or eliminates the current flowing between the auxiliary anodes 214-217 and the substrate Wf. When the distance between the mask members 184-187 in the anode mask 18 is set, the distance between the mask members 184-187 is increased and the current flowing between the auxiliary anodes 214-217 and the substrate Wf is increased. The length of the auxiliary anodes 214-217 (the dimension in the direction parallel to the polygonal opening 21 of the regulation plate 20) can be adjusted in advance to adjust the range of plating thickness control by the auxiliary anodes 214-217. For example, when the terminal effect is small, the plating thickness tends to be small near the protrusions 20b formed on the regulation plate due to the electric field shielding effect. However, by adjusting the length of the auxiliary anodes 214-217 according to the shape and length of the protrusions 20b, it is possible to effectively prevent the plating thickness in the vicinity of the protrusions 20b from becoming small. Such control can improve the in-plane uniformity of the plating formed on the substrate Wf.

[0032] Each of Figs. 5A to 5C is a schematic diagram showing the plating thickness when plating a rectangular substrate using the plating apparatus of this embodiment under conditions of large, medium, and small terminal effects. Each of Figs. 6A to 6C is a schematic diagram showing the plating thickness when plating a rectangular substrate using the plating apparatus of the comparative example under conditions of large, medium, and small terminal effects, similar to Figs. 5A to 5C. Note that Figs. 5A to 5C and 6A to 6C show the plating thickness of the upper right region obtained by dividing the rectangular substrate into four parts, with the lower left part corresponding to the center Ctr of the rectangular substrate and the upper right part corresponding to the corner Cor of the rectangular substrate. In these figures, the lighter the color, the smaller the film thickness is relative to the average film thickness, and the darker the color, the larger the film thickness is relative to the average film thickness. As shown in Fig. 6A, in the conventional plating apparatus of the comparative example, when the influence of the terminal effect is large, the film thickness is small near the corners of the substrate Wf and large near the center of the side. 6C, in the conventional plating apparatus of the comparative example, when the influence of the terminal effect is small, the film thickness is small at the center of the substrate Wf and large at the periphery including the corners. In contrast, as shown in FIGS. 5A to 5C, in plating using the plating apparatus of this embodiment, suitable in-plane uniformity can be obtained under any of the conditions in which the terminal effect is large, medium, or small.

[0033] Next, the substrate holder 30 will be described. Fig. 7 is a schematic front view of the substrate holder 30 used in the plating unit 10 shown in Fig. 2, and Fig. 8 is a schematic side view of the substrate holder 30. The substrate holder 30 includes a front plate 300 and a back plate 400. The substrate Wf is held between the front plate 300 and the back plate 400. In this embodiment, the substrate holder 30 holds the substrate Wf with one side of the substrate Wf exposed.

[0034] The front plate 300 includes a front plate body 310 and an arm section 330. The arm section 330 has a pair of pedestals 331, and the pedestals 331 are installed on the upper surface of the peripheral wall of each treatment tank shown in FIG. 1, thereby supporting the substrate holder 30 in a vertically suspended state. The arm section 330 is also provided with a connector 332 configured to come into contact with an electrical contact provided in the plating tank 14 when the pedestal 331 is installed on the upper surface of the peripheral wall of the plating tank 14. As a result, the substrate holder 30 is electrically connected to an external power source, and a voltage and current are applied to the polygonal substrate Wf held by the substrate holder 30.

[0035] The front plate body 310 is generally rectangular, has a wiring buffer portion 311 and a face portion 312, and has a front surface 301 and a rear surface 302. The front plate body 310 is attached to an arm portion 330 at two points by attachment portions 320. An opening 303 is provided in the front plate body 310, and the surface of the substrate Wf to be plated is exposed from the opening 303. In this embodiment, the opening 303 is formed in a shape corresponding to the polygonal shape of the substrate Wf. A mask for adjusting the electric field may be placed on the inner periphery of the opening 303 so as to shield part of the outer periphery of the plated surface of the substrate Wf. This is because the substrate Wf This is effective when the terminal effect is very large because the seed layer formed on the substrate is extremely thin, etc. The mask can be made of a dielectric material such as resin, for example.

[0036] The backplate 400 is generally rectangular and covers the back surface of the substrate Wf. The backplate 400 is fixed by a clamp 340 in a state in which the substrate Wf is sandwiched between the backplate 400 and the back surface 302 of the frontplate main body 310 (more specifically, the face portion 312). The clamp 340 is configured to rotate about a rotation axis 341 parallel to the surfaces 301, 302 of the frontplate main body 310. However, the clamp 340 is not limited to this example, and may be configured to clamp the backplate 400 by reciprocating in a direction perpendicular to the surfaces 301, 302.

[0037] 9 is a rear view of the front plate body, and FIG. 10 is an enlarged rear view showing the vicinity of a corner of the face part close to the connector. The rear face 302 of the front plate body 310 has 18 contact areas C1-C18. The contact areas C1-C7, C17, and C18 are arranged in a half area of ​​the face part 312 on the connector 332 side (proximal area, right half area in FIG. 9), and the contact areas C8-C16 are arranged in a half area of ​​the face part 312 farther from the connector 332 (distal area, left half area in FIG. 9). In the following description, for convenience, the cables arranged in the distal area may be referred to as the first group of cables, and the cables arranged in the proximal area may be referred to as the second group of cables.

[0038] As shown in FIG. 10, each of the contact areas C1-C18 includes a contact (contact member) 370 for supplying power to the substrate Wf. The contact 370 is arranged along each side of the opening 303 of the front plate 300. That is, the contact 370 is arranged along each side of the polygonal substrate Wf. Power is supplied from the outside to the contact 370 of each of the contact areas C1-C18 via cables L1-L18, respectively. In the following description, when it is not necessary to distinguish between the cables, the cables L1-L18 may be collectively referred to as cable L. Also, any cable may be referred to as cable L.

[0039] First ends of the cables L1-L18 are connected to a connector 332 provided at one end of the arm portion 330, and more specifically, are electrically connected to individual contacts or to a common contact (not shown) in the connector 332. The cables L1-L18 can be electrically connected to an external power source (power circuit, power supply device, etc.) via each contact of the connector 332.

[0040] The cables L1-L7 are arranged side by side on the same plane, introduced into the cable passage 365, and disposed along the side of the opening 303 on the connector 332 side. The cables do not overlap each other in the thickness direction of the face portion 312. Therefore, the thickness of the face portion 312 and the front plate 300 can be reduced.

[0041] The electrical connection between the cable L and the contacts 370 in each contact area is established as follows. Taking the cable L1 as an example, the coating 602 is removed from the tip (second end) of the cable L1, exposing the core wire (conductive wire) 601. The tip of the cable L1 is introduced into the wiring groove of the seal holder 363 in the vicinity of the contact C1, and is pressed together with the contacts 370 by four screws (fastening members) 511 in the contact area C1. In other words, the screws (fastening members) 511 and the seal holder 363 clamp the core wire 601 of the cable L1 together with the contacts 370. As a result, the cable L1 is electrically connected to the contacts 370. When the substrate holder 30 holds the substrate Wf, the contacts 370 come into contact with the substrate Wf, and the cable L1 and the contacts 370 are connected to each other from an external power source. The other contact areas C2-C18 are similarly configured, and power is supplied to the substrate Wf from 18 contacts 370.

[0042] As described above, in the substrate holder 30 according to this embodiment, the contacts 370 are provided on each side of the polygonal substrate Wf, and power is supplied to the substrate Wf from the contacts 370 provided on each side. As a result, a plating film is formed on the surface of the substrate Wf.

[0043] Although the process of plating a rectangular substrate Wf has been described above, the present invention is not limited to this, and a similar process can also be used to plate a triangular or pentagonal or greater substrate Wf. Even in such cases, the anode mask may be configured to have a plurality of mask members that define a convex portion at the center of the opening side corresponding to the shape of the substrate, and the distance between the plurality of mask members may be adjusted.

[0044] (Modification) 11A to 11C are views showing an anode mask 18A in a modified example from the substrate Wf side. The anode mask 18A in the modified example includes a frame member 182 that defines a polygonal opening corresponding to the polygonal shape of the substrate Wf, similar to the anode mask 18 in the above-described embodiment. The anode mask 18A also includes a plurality of mask members 184A to 187A that are disposed adjacent to the frame member 182 and are movable relative to the frame member 182. In FIGS. 11A to 11C, the frame member 182 and the four mask members 184A to 187A are hatched for ease of viewing. The four mask members 184A to 187A have the same shape and are disposed in a state rotated by 90 degrees. As a representative example, in FIGS. 11A to 11C, the mask member 184A disposed at the upper left of the opening 182a is hatched differently from the other mask members 185A to 187A.

[0045] Each of the mask members 184A to 187A of the modified example is arranged at a corner of the opening 182a and is configured to define a convex portion that protrudes toward the center of the opening 182a at two consecutive opening sides of the opening 182a. In the example shown in Figs. 11A to 11C, the mask members 184A to 187A have convex portions 184Ab to 187Ab that define the convex portions along the sides of the opening 182a, and concave portions 184Aa to 187Aa that are provided at positions corresponding to the corners of the opening 182a and are recessed toward the outer periphery more than the convex portions 184Ab to 187Ab. The mask members 184A to 187A are configured to be movable relative to the frame member 182, and together with the frame member 182, define the opening 18Aa of the anode mask 18A. In the example shown in FIGS. 11A to 11C, the mask members 184A to 187A can move linearly relative to the frame member 182 in a direction inclined at 45 degrees with respect to the up, down, left, and right directions of the page. In the example shown in FIG. 11A, the mask members 184A to 187A are located on the outside and do not overlap with the opening 182a of the frame member 182, and the opening 182a of the frame member 182 becomes the opening 18Aa of the anode mask 18A. When each of the multiple mask members 184A to 187A moves toward the center with respect to the frame member 182 from this state, each of the convex portions 184Ab to 187Ab protrudes into the opening 182a of the frame member 182, as shown in FIG. 11B. In the example shown in FIG. 11B, the opening defined by a part of the frame member 182 and a part of the convex portions 184Ab to 187Ab of the mask members 184A to 187A becomes the opening of the anode mask 18. At this time, the convex portions 184Ab-187Ab of the adjacent mask members 184A-187A define convex portions protruding toward the center of the opening 18Aa at the center of the opening side. For example, the convex portion 184Ab of the mask member 184A provided at the upper left and the convex portion 185Ab of the mask member 185A provided at the upper right define convex portions protruding toward the center of the opening at the center of the upper side. Then, when each of the multiple mask members 184A-187A further moves toward the center with respect to the frame member 182, the convex portions 184Ab-187Ab and the concave portions 184Aa-187Aa of the mask members 184A-187A protrude into the opening 182a of the frame member 182, as shown in FIG. 11C. In the example shown in FIG. 11C, the opening defined by the multiple mask members 184A-187A is moved toward the center of the anode mask 182a. 11A, 11B, and 11C each show one example of the state of the openings 18a in the anode mask 18, and it is sufficient that the positions of the multiple mask members 184A to 187A can be smoothly changed.

[0046] In the anode mask 18A of this modified example, the opening shape can be changed to improve the in-plane uniformity of the plating formed on the substrate Wf, as in the anode mask 18 of the above-described embodiment. Note that the multiple mask members 184A-187A may be moved manually or by a moving mechanism (not shown).

[0047] In the above-described embodiment and modified examples, the anode masks 18, 18A have a frame member 182 corresponding to the shape of the substrate Wf. However, the anode masks 18, 18A do not have to have such a frame member, and may be configured such that the opening 18a is defined by the multiple mask members 184-187, 184A-187A, for example, by forming the sides 184a-184b of the multiple mask members 184-187 to be long.

[0048] The present invention can also be described in the following forms. [Mode 1] According to mode 1, a plating apparatus is proposed, which includes a plating tank, a substrate holder configured to hold a polygonal substrate, an anode disposed in the plating tank so as to face the substrate held by the substrate holder, and an anode mask defining an opening corresponding to the outer shape of the polygonal substrate, the anode mask including a first mask member defining a first convex portion protruding toward the center of the opening at a center of a first opening side corresponding to a first side of the polygonal substrate in the opening, and a second mask member defining a second convex portion protruding toward the center of the opening at a center of a second opening side corresponding to a second side of the polygonal substrate in the opening, the anode mask being configured so that the distance between the first mask member and the second mask member can be adjusted. According to mode 1, the opening shape of the anode mask can be adjusted by adjusting the distance between the first mask member and the second mask member, and the in-plane uniformity of the film plated on the polygonal substrate can be improved.

[0049] [Form 2] According to Form 2, in Form 1, the first mask member is arranged on the first opening edge and configured to be movable in a direction perpendicular to the first opening edge, and the second mask member is arranged on the second opening edge and configured to be movable in a direction perpendicular to the second opening edge.

[0050] [Mode 3] According to Mode 3, in Mode 2, the anode mask further includes a third mask member arranged on a third opening edge corresponding to a third side of the polygonal substrate in the opening and defining a third convex portion protruding toward the center of the opening at a center portion of the third opening edge, and a fourth mask member arranged on a fourth opening edge corresponding to a fourth side of the polygonal substrate in the opening and defining a fourth convex portion protruding toward the center of the opening at a center portion of the fourth opening edge, and configured so that the distance between the third mask member and the fourth mask member can be adjusted. According to Mode 3, the opening shape of the anode mask can be adjusted by adjusting the distance between the first to fourth mask members, and the in-plane uniformity of the film plated on the polygonal substrate can be improved.

[0051] [Form 4] According to Form 4, in Form 1, the first mask member is positioned at a first corner of the opening and defines a convex portion protruding toward the center of the opening on two consecutive opening sides of the opening, and the second mask member is positioned at a second corner of the opening and defines a convex portion protruding toward the center of the opening on two consecutive opening sides of the opening.

[0052] [Mode 5] According to mode 5, in modes 1 to 4, the first convex portion and the second convex portion have a trapezoidal shape tapering toward the center of the opening.

[0053] [Mode 6] According to Mode 6, in Modes 1 to 5, the anode mask has a frame member that defines a polygonal opening corresponding to the outer shape of the polygonal substrate, and the first mask member and the second mask member are arranged adjacent to the frame member and together with the frame member define the opening of the anode mask.

[0054] [Mode 7] According to Mode 7, in any of Modes 1 to 6, a regulation plate is provided between the anode holder and the substrate holder, and the regulation plate has a first auxiliary anode arranged corresponding to the first side of the first mask member and a second auxiliary anode arranged corresponding to the second side of the second mask member. According to Mode 7, the first auxiliary anode and the second auxiliary anode can be used to further improve the in-plane uniformity of the plating film.

[0055] [Form 8] According to Form 8, in Form 7, a control device is provided that causes a current to flow between the first auxiliary anode and the second auxiliary anode and the polygonal substrate such that the current flowing through the first auxiliary anode and the second auxiliary anode increases as the distance between the first mask member and the second mask member increases.

[0056] [Mode 9] According to mode 9, a plating method for plating a polygonal substrate by passing a current between an anode and the polygonal substrate in a plating apparatus is proposed, the plating method including a step of adjusting a distance between the first mask member and the second mask member in an anode mask that defines an opening corresponding to an outer shape of the polygonal substrate, the anode mask having a first mask member that defines a first convex portion protruding toward the center of the opening at a center portion of a first opening side corresponding to a first side of the polygonal substrate in the opening, and a second mask member that defines a second convex portion protruding toward the center of the opening at a center portion of a second opening side corresponding to a second side of the polygonal substrate in the opening, the plating method including a step of adjusting a distance between the first mask member and the second mask member, and a step of passing a current between the anode and the polygonal substrate. According to mode 9, the opening shape of the anode mask can be adjusted by adjusting the distance between the first mask member and the second mask member, and the in-plane uniformity of a film plated on the polygonal substrate can be improved.

[0057] [Mode 10] According to mode 10, in mode 9, the plating apparatus includes a regulation plate provided between the anode holder and the substrate holder, the regulation plate having a first auxiliary anode arranged corresponding to the first side of the first mask member and a second auxiliary anode arranged corresponding to the second side of the second mask member, and the plating method includes a step of passing a current between the first auxiliary anode and the second auxiliary anode and the polygonal substrate such that the current flowing through the first auxiliary anode and the second auxiliary anode increases as the distance between the first mask member and the second mask member increases. According to mode 10, the in-plane uniformity of the plating film can be further improved by using the first auxiliary anode and the second auxiliary anode.

[0058] Although the embodiment of the present invention has been described above, the above-mentioned embodiment of the invention is intended to facilitate understanding of the present invention and does not limit the present invention. The present invention may be modified or improved without departing from the spirit thereof, and the present invention naturally includes equivalents thereof. Furthermore, any combination or omission of each component described in the claims and specification is possible within the scope of solving at least a part of the above-mentioned problems or achieving at least a part of the effects. [Explanation of symbols]

[0059] 10 Plating Unit 12 Anode 13 Anode holder 17 Control device 18,18A Anode Mask 18a,18Aa opening 20 Regulation Plate 21 Polygonal aperture 30 Substrate holder 184~187,184A~187A Mask material 184a~187a Edge 184b~187b Convex 184Aa~187Aa Concave 184Ab~187Ab Convex 214~217 Auxiliary anode Wf Polygonal Substrate

Claims

1. A plating tank; a substrate holder configured to hold a polygonal substrate; an anode disposed in the plating tank so as to face the substrate held by the substrate holder; a regulation plate disposed between the anode and the substrate holder and defining an opening corresponding to an outer shape of the polygonal substrate, a pair of protrusions protruding from each of the pair of opening sides toward the center of the opening at the center of a pair of opposing opening sides of the opening corresponding to each side of the polygonal substrate, the pair of protrusions having both sides with an opening size formed therebetween that changes continuously; a regulation plate having a pair of auxiliary anodes disposed on a surface of the regulation plate facing the substrate and provided outside the pair of opening sides; A plating apparatus comprising:

2. 2. The plating apparatus according to claim 1, wherein the pair of auxiliary anodes are arranged parallel to the pair of opening sides, and a length of the pair of auxiliary anodes along the pair of opening sides is shorter than a length of the pair of opening sides.

3. The plating apparatus according to claim 1 , wherein the pair of protrusions are trapezoidal in shape and narrow toward the center of the opening.

4. The substrate is a rectangular substrate, the regulation plate has a protrusion protruding from each of the opening sides toward the center of the opening at a center portion of each of the opening sides corresponding to each side of the rectangular substrate; 2. The plating apparatus according to claim 1.

5. 5. The plating apparatus of claim 4, wherein the substrate holder has contacts provided along each side of the rectangular substrate, and is configured to supply power to the rectangular substrate through the contacts.

Citation Information

Patent Citations

  • Radio wave monitor apparatus

    JP1991029876A

  • Surface-treating device

    JP1997125294A

  • Plating apparatus

    JP2005029863A

  • Regulation plate, plating system therewith and plating method

    JP2017115171A

  • Plating apparatus

    JP2019002051A