Polyurethane condom mold, manufacturing method and use method of the mold
The polyurethane condom mold with specific surface properties and manufacturing methods addresses adhesion and contamination issues, enabling efficient and safe production of polyurethane condoms with high strength and biocompatibility.
Patent Information
- Application Number
- JP2022559542
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-05-20
- Filing Date
- 2020-06-16
- Publication Date
- 2024-12-04
- Estimated Expiration
- 2040-06-16
AI Technical Summary
Current methods for molding polyurethane condoms face challenges such as strong adhesion to traditional molds, difficulty in demolding, and potential contamination from mold release agents, making continuous production unstable and unsafe.
A polyurethane condom mold made of a thermoplastic polymer with a surface roughness of 0.2 or less and a surface tension of 10 to 35 mN/m, allowing for uniform film formation and easy demolding without mold release agents, using injection molding techniques.
Ensures uniform film formation, simplifies the production process, improves efficiency, and enhances product safety by avoiding contamination, while maintaining high tensile strength and biocompatibility.
Smart Images

Figure 0007594603000001 
Figure 0007594603000002 
Figure 0007594603000003
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of condom materials, and in particular to a mold for molding polyurethane condoms, a method for making the mold, and a method for using the mold. [Background technology]
[0002] Condoms are simple devices that are widely used worldwide for contraception and protection from sexually transmitted diseases. Current condom products mainly include natural rubber latex condoms and polyurethane condoms.
[0003] In the dip molding process of natural rubber latex condoms, molds made of glass or metal materials such as stainless steel are mainly used. Since natural latex rubber has a surface tension similar to that of glass or stainless steel, the film made of natural latex rubber on the surface of these two materials shows relatively weak adhesion. Furthermore, natural latex rubber has the property of swelling in an alkaline environment. Therefore, after natural latex rubber condoms are molded on the surface of a glass mold or a mold, they are swelled with ammonia water and demolded.
[0004] However, polyurethane material condoms do not swell like natural latex rubber and have a surface tension of about 55 mN / m. The surface tension of the dried film is about 45 mN / m. Although polyurethane emulsions can be applied to glass, ceramic and stainless steel molds, the dried water-based polyurethane film adheres very strongly to these molds and is difficult to roll and demold, so these two materials cannot be directly used to dip-mold polyurethane condoms. To solve the problems in molding polyurethane, two methods are currently used around the world: (1) A method of alkylating the glass surface so as to make the surface tension of the glass closer to that of the polyurethane material. This can solve the problems of film formation and demolding of the polyurethane material on the glass, but the effective usable time after alkylation is short, about 30 hours, and continuous production is not possible. In addition, the effect of alkylation changes in real time, so the quality stability of polyurethane condoms cannot be effectively guaranteed during the production process. (2) Pre-coating a layer of release agent on the surface of glass or stainless steel, which can solve the problem of continuous production, but the release agent may be mixed into the condom material during the production process, posing potential risks to product performance and biosafety.
[0005] Therefore, there is a need for further improvement and optimization of polyurethane condom molding molds, which is both a research hotspot and a research difficulty in this field. Summary of the Invention [Problem to be solved by the invention]
[0006] The present invention has been made in response to the above-mentioned shortcomings of the prior art. One of the objectives of the present invention is to provide a mold for molding a polyurethane condom, which is thin, flexible and strong, and meets the market demand for the product.
[0007] Another object of the present invention is to provide a method for manufacturing polyurethane condom molds.
[0008] Another object of the present invention is to provide a method of using the polyurethane condom mold. [Means for solving the problem]
[0009] The present invention provides a polyurethane condom molding die made of a thermoplastic polymer having a surface roughness of 0.2 or less and a surface tension of 10 to 35 mN / m.
[0010] In one embodiment, the thermoplastic polymer is any one or any combination selected from polyurethane, polymethyl methacrylate, polystyrene, polyethylene, polyvinyl chloride, polypropylene, polystyrene, acrylonitrile butadiene-styrene, polyamide, polycarbonate, polyoxymethylene, modified polyphenylene oxide, thermoplastic polyester, polyimide, polyphenylene sulfide, polysulfone, aromatic polyamide, and materials obtained by organic modification of the above polymers or inorganic modification by filling the above polymers with inorganic materials.
[0011] In one embodiment, the organic modification is any one selected from the group consisting of organosilicon modification, organofluorine modification, silane modification, acrylate copolymerization modification, vinyl monomer modification, and aromatic monomer modification, or any combination thereof.
[0012] In one embodiment, the inorganic modification is selected from heavy calcium modification, talc modification, graphene modification, water glass modification, attapulgite modification, kaolin modification, light calcium modification, and glass microbead modification, or any combination thereof.
[0013] In one embodiment, the polyurethane condom is a male condom, and the mold comprises a head portion and a tail portion connected to the head portion, the head portion having a cylindrical shape with a gradually increasing diameter and a slope of greater than 0 degrees and less than or equal to 5 degrees.
[0014] In one embodiment, the head portion has a front end that includes a semen sac.
[0015] In one embodiment, the length of the head portion is 200 to 260 mm.
[0016] In one embodiment, the head portion is connected to the tail portion through a transition section.
[0017] In one embodiment, the tail portion has a cylindrical shape with a constant diameter.
[0018] In one embodiment, the tail has a cylindrical shape with a gradually increasing diameter and has a slope of greater than 0 degrees and up to 3 degrees.
[0019] In one embodiment, the polyurethane condom is a female condom.
[0020] In one embodiment, the polyurethane condom is a molded condom, the mold having a surface with floating points or threads.
[0021] In one embodiment, the mold has a thickness of 2 to 10 mm or is a solid mold.
[0022] In one embodiment, the mold has an angle of less than 5 degrees to the vertical when the mold is oriented vertically.
[0023] The present invention further provides a method for manufacturing a polyurethane condom mold, the method comprising the steps of: Providing a thermoplastic polymer having a surface tension of 10 to 30 mN / m -The process of manufacturing polyurethane condom molds by injection molding of thermoplastic polymers. The mold has a surface roughness of 0.2 or less.
[0024] In one embodiment, the injection molding is performed by three shot feeding and two stage injection molding.
[0025] The present invention further provides a method of using a polyurethane condom mold, the method comprising the steps of: ·Mold providing process A process for providing an emulsion containing a polyurethane resin A process in which a mold is hung vertically and dipped into a latex containing polyurethane resin to obtain a dipped mold. The dipped mold is removed and dried to form a polyurethane film on the surface of the mold. Demolding process The mold is made of a thermoplastic polymer having a surface roughness of 0.2 or less and a surface tension of 10 to 35 mN / m.
[0026] In one embodiment, the polyurethane condom has a 100% tensile modulus of 2.5 N / mm 2 The following is the result.
[0027] In one embodiment, the polyurethane condom has a burst pressure of 1 kPa or more, a burst volume of 5 L or more, and a 100% elastic modulus of 3.5 N / mm 2 The following is the result.
[0028] The polyurethane condom with adhesive layer provided according to the present invention is made by using a polyurethane condom mold, and the mold is made of a thermoplastic polymer having a surface tension of 10 to 35 mN / m, so that the polyurethane can directly form a uniform film on the surface of the mold by dip molding. The film formed after drying has a weak adhesive force and can be uniformly demolded without the use of a release agent, ensuring the uniformity of the polyurethane film and preventing the inclusion of other substances, thereby fully ensuring the performance and biosafety of polyurethane condom products. In addition, according to the mold provided by the present invention, the polyurethane material can be directly post-treated on the surface of the mold for raw material characteristics without adding other processes such as demolding, so that the work procedure is greatly simplified, production efficiency is improved, and the product qualification rate is improved. The raw material of the mold of the present invention has a low-cost and abundant supply source, and the molding process is simple, safe, and environmentally friendly. Other features, benefits, and advantages will be apparent from the invention detailed herein, including the specification and claims.
[0029] In order to more clearly describe the technical solutions of the embodiments of the present invention, the following briefly describes the drawings used in the embodiments. It should be understood that the following drawings only illustrate some embodiments of the present invention, and therefore should not be taken as limiting the scope of the invention. Those skilled in the art can also obtain other related drawings according to these drawings without any effort. [Brief description of the drawings]
[0030] [Figure 1] FIG. 1 is a schematic structural diagram of a polyurethane condom according to a particular embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic structural diagram of a polyurethane condom mold according to a specific embodiment of the present invention. [Diagram 3] FIG. 1 is a schematic flow diagram of a method for manufacturing a polyurethane condom mold in accordance with one particular embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] In order to make the objectives, technical solutions and advantages of the embodiments of the present invention more clearly understandable, the technical solutions of the embodiments in the present invention will be clearly and completely described with reference to the accompanying drawings. Needless to say, it should be understood that the described embodiments are only a part of the present invention, and are not all of the present invention. In general, the components of the embodiments of the present invention described in this specification and illustrated in the drawings can be configured and designed according to different needs.
[0032] As shown in Figures 1 to 3, the process of making a polyurethane condom 100 includes a step of molding on a mold 200. Specifically, the polyurethane condom 100 is made by molding the raw material of the polyurethane condom 100, such as a polyurethane resin-containing emulsion, on the mold 200 by dip molding, and the polyurethane condom 100 has high strength, high moldability and excellent biocompatibility, and a thickness of, for example, 0.001mm to 0.08mm, preferably 0.05mm to 0.04mm, such as 0.01mm, 0.015mm, 0.02mm, and 0.030mm, which can provide a more comfortable experience for the user, is free of allergy problems, and can provide a softer and more delicate skin feel.
[0033] A polyurethane condom 100 having a thickness within the above range has a burst pressure of, for example, 1 kPa or more, preferably 3 kPa or more, for example 3 kPa, 4 kPa or 5 kPa, and a burst volume of, for example, 5 L or more, for example 6 L, 8 L or 10 L.
[0034] The polyurethane condom 100 has a strength, for example, a tensile strength of 30 MPa or more, preferably 70 MPa or more, and a 100% elastic modulus of 2 N / mm 2 , 1.8N / mm 2 , 1.5N / mm 2 or 1N / mm 2 3.5N / mm etc. 2 It is better to have the following:
[0035] It is noted that the emulsion containing polyurethane resin has a surface tension in the range of 20-80 mN / m, preferably 30-60 mN / m, such as 32 mN / m, 40 mN / m, 50 mN / m, 55 mN / m and 58 mN / m. After being molded and dried on the surface of the mold 20 provided by the present invention, the polyurethane film has a surface tension in the range of 15-68 mN / m, such as 20 mN / m, 28 mN / m, 45 mN / m or 50 mN / m. Within the above range, the emulsion containing polyurethane resin can be uniformly spread on the mold 200, and the dried film has low adhesion, ensuring uniform film formation and demolding.
[0036] In some embodiments, the layer may be formed from an emulsion containing a polyurethane resin, for example, a polyurethane resin mixed with other adjuvants, such as, but not limited to, functional adjuvants such as lubricants, bactericides, thickeners, wetting agents, defoamers, water, etc. The polyurethane resin may be any suitable type of aliphatic or aromatic polyurethane, such as, for example, anionic, cationic, nonionic, amphoteric, solvent-based or solvent-free polyurethane. processIt is preferable to adjust the viscosity so as to prepare a desired polyurethane. Furthermore, in order to obtain excellent film-forming properties and mold releasability, the polyurethane resin may be selected from polyurethane resins synthesized from, for example, polyether / polyester polyols, and may have a 100% tensile modulus of elasticity of, for example, 3.5 N / mm 2 Hereinafter, the tensile strength may be 25 MPa or more. Needless to say, the present invention is not limited thereto.
[0037] As shown in Figures 1 and 2, the present invention provides a specific embodiment of a polyurethane condom 100 having a multi-layer structure formed by multiple dip molding of a mold 200, such as three layers (e.g., a first layer 10, a second layer 20, and a third layer 30), four layers, five layers, six layers, etc., but is not limited thereto and can be adjusted according to actual needs. It should be understood that the polyurethane condom 100 can be configured as a male condom according to the type of mold 200, but the polyurethane condom 100 can also be configured as a female condom or other types of condoms according to the type of mold 200. For example, the mold 200 may have, but is not limited thereto, a floating point or a screw thread.
[0038] The mold 200 is made of a thermoplastic polymer having a surface tension in the range of 10-35 mN / m, for example, 25-35 mN / m, such as 35 mN / m, 32 mN / m, 30 mN / m, or 28 mN / m. If the surface tension of the thermoplastic polymer is less than 10 mN / m, it is difficult to spread the polyurethane emulsion evenly on the mold 200 made of the thermoplastic polymer, and if the surface tension of the thermoplastic polymer exceeds 35 mN / m, the adhesion between the dried film formed from the polyurethane emulsion and the mold 200 made of the thermoplastic polymer is too strong and it is not possible to smoothly remove the mold. If it is within the above range, when the polyurethane emulsion is molded on the mold 200, for example, by dip molding, the polyurethane emulsion can directly form a uniform film on the mold surface, and the film formed after drying has low adhesion and can be uniformly removed without the aid of a mold release agent, ensuring the uniformity of the polyurethane film and avoiding the introduction of other substances, so that the performance and biological safety of the polyurethane condom product can be fully ensured.
[0039] In some embodiments, the thermoplastic polymeric material may be, for example, ethylene-based polymers, propylene-based polymers, diene-based polymers, aromatic polymers, and polyurethanes, polycarbonates, polymethylmethacrylates, polyamides, thermoplastic polyesters, halogenated thermoplastic polymers such as polyoxymethylene and thermoplastic polyesters.
[0040] In some embodiments, the ethylene-based polymer may specifically be polyethylene and its copolymers, ethylene-butene copolymers, ethylene-hexene copolymers, ethylene-octene copolymers, ethylene-propylene-butene copolymers, ethylene-vinyl acetate copolymers, ethylene-ethyl acrylate copolymers, ethylene-methyl methacrylate copolymers, chlorinated polyethylene, ethylene-vinyl alcohol copolymers, and the like.
[0041] The propylene-based polymer may be polypropylene, polyacrylonitrile, propylene-ethylene copolymer, propylene-butene copolymer, propylene-hexene copolymer, propylene-octene copolymer, and the like.
[0042] The diene-based polymer may be polybutadiene, polyisoprene, butadiene-styrene copolymer, butadiene-acrylonitrile copolymer, ethylene-propylene-5-ethylene-2-norbornene copolymer, ethylene-propylene-dicyclopentadiene copolymer or ethylene-propylene-5-vinyl-2-norbornene copolymer.
[0043] The aromatic polymer may be polystyrene, modified polyphenylene ether, or copolymers thereof such as styrene-acrylonitrile copolymer, styrene-acrylonitrile-butadiene copolymer, acrylic rubber-acrylonitrile-styrene copolymer, acrylonitrile-chlorinated polyethylene-styrene copolymer.
[0044] The above-mentioned materials may further be selected from, for example, water-based polyurethane, polymethyl methacrylate, polystyrene, polyethylene, polyvinyl chloride, polypropylene, polystyrene, butadiene-styrene, polyamide (such as, for example, polyamide 6, polyamide 11, polyamide 12, polyamide 6.6, polyamide 4.6, polyamide 6.10, polyamide 6.12), polycarbonate, polyoxymethylene, modified polyphenylene oxide, thermoplastic polyester, polyimide, polyphenylene sulfide, polysulfone, aromatic polyamide, polyarylate, polyphenyl ether, polyaryl ether ketone, liquid crystal polymer, and fluororesin.
[0045] In other embodiments, the thermoplastic polymers may also include materials obtained by organic modification of the above polymers or by inorganic modification by filling the above polymers with inorganic materials. Furthermore, the modification may be a chemical or physical modification or any other suitable form.
[0046] The organic modification may be, for example, an organosilicon modification, an organofluorine modification, a graphene modification, a silane modification, an acrylate copolymer modification, a vinyl monomer modification, an aromatic monomer modification, or the like, but is not limited thereto.
[0047] The inorganic modification may be, for example, heavy calcium modification, talc modification, graphene modification, water glass modification, attapulgite modification, kaolin modification, light calcium modification, glass microbead modification, or the like.
[0048] As shown in FIG. 2, the mold 200 is composed of a head portion 210 and a tail portion 220. The front end of the head portion 210 is optionally provided with a semen bag 211. The rear end of the head portion 210 is provided with a transition section 212 for connecting the tail portion 220. The head portion 210 has a length H1 of 200 to 260 mm, for example, 220 mm, 230 mm, or 245 mm, from the viewpoint of molding. The head portion 210 has a columnar shape with a gradually increasing diameter, and has an inclination of more than 0 degrees and less than 5 degrees, for example, 2°, 3°, or 4°. In particular, the section close to the front end of the head portion 210 has a diameter of 30 to 45 mm, and the section close to the rear end has a diameter larger than the section close to the front end, for example, 32 to 50 mm, and the desired inclination can be formed by the difference in diameter between both ends. When the mold 200 has an inclination within the above range, the mold 200 can be smoothly pulled out from the injection molding machine, as described later in detail, and the demolding resistance can be further reduced. The tail portion 220 is connected to the head portion 210 via the transition section 212 so as to form a flat surface. The tail portion 220 has a length H2 of 10 to 150 mm, for example, 25 mm, 30 mm, 35 mm, 40 mm, or 55 mm. The tail portion 220 has a columnar shape with a constant diameter that matches the diameter of the end of the head portion 210. Of course, the tail portion may also have a columnar shape with a gradually increasing diameter, for example, with an inclination of more than 0 degrees and less than or equal to 3 degrees, such as 1 degree, 2 degrees, or 3 degrees. When the mold 200 is arranged vertically, it forms an angle of less than 5 degrees with respect to the vertical line, which sufficiently guarantees excellent stability during use, for example, when used vertically, and that the polyurethane film is not easily damaged during the rolling process and demolding process.
[0049] 2, the mold 200 made of a thermoplastic polymer has a thickness of, for example, 2 to 25 mm, or is a solid mold, and preferably has a thickness of 2 to 8 mm, for example, 3 mm, 4 mm, 5 mm, 6 mm, 7 mm, etc. By having a thickness in the above range, the mold 200 can have a certain strength.
[0050] 2, the mold 200 has a surface roughness (Ra) of 0.2 or less, such as 0.09, 0.09, 0.05, or 0.01. When the surface roughness (Ra) of the mold 200 is 0.2 or less, the polyurethane film is easy to handle without adding a demolding release agent when demolded, and damage to the polyurethane film due to external forces is avoided.
[0051] As shown in FIG. 3, the present invention further provides a method for manufacturing a mold 200, which includes the following steps. Step S1 of the process of providing a thermoplastic polymer Step S2, which is the process of making a mold by injection molding a thermoplastic polymer
[0052] The mold 200 may be obtained, for example, using an injection molding machine. A multi-shot feed, such as a three-shot feed, may be employed to ensure that the thermoplastic polymer is uniformly fed into the injection molding machine. Furthermore, the mold 200 may be obtained by, but is not limited to, two-stage molding, in which the head portion 210 and the tail portion 220 are formed separately and then assembled to form the mold 200. The head portion 210 and the tail portion 220 may also be molded integrally.
[0053] When the mold 200 is utilized to mold a polyurethane condom, the mold 200 is hung vertically and dipped into an aqueous polyurethane emulsion, then removed so that the polyurethane forms a film on the surface of the mold, and then demolded. The polyurethane film can be demolded smoothly without a release agent and does not adhere to the mold 200.
[0054] In a particular embodiment of the invention, the mold 200 can be manufactured by a method including three shot feeding through the open end of the tail section 210 and two-stage injection molding, where polyethylene (ExxonMobil Chemical's Enable® performance polyethylene) is formed into a cylindrical tubular body for the mold by injection molding. The head section 210 has a length H1 of 220 mm and a taper of 0.2 degrees from the front end to the rear end such that the diameter of the front end of the head section 210 is smaller than the diameter of the rear end and the tail section. The tail section 220 has an unlimited length H2. The mold 200 has a wall thickness of 2 mm, a surface roughness (Ra) of 0.2 or less, and a verticality of less than 5 degrees between the vertically placed mold and a vertical line.
[0055] In another specific embodiment of the present invention, the mold 200 can be manufactured by a method including three shot feeding through the open end of the tail section 210 and two-stage injection molding, where polypropylene (TB54I from Hanwha-Total) is formed into a cylindrical tubular body for the mold by injection molding. The head section 210 has a length H1 of 230 mm and a 3 degree slope from the front end to the rear end such that the diameter of the front end of the head section 210 is smaller than the diameter of the rear end and the tail section. The tail section 220 has an unlimited length H2. The mold 200 has a wall thickness of 5 mm, a surface roughness (Ra) of 0.2 or less, and a verticality such that the angle between the vertically placed mold 200 and a vertical line is less than 5 degrees.
[0056] In another particular embodiment of the present invention, the mold 200 can be manufactured by a method including three shot feeding through the open end of the tail section 210 and two-stage injection molding, where polycarbonate (Bayer 2407) is formed into a cylindrical tubular body for the mold by injection molding. The head section 210 has a length H1 of 240 mm and a 5 degree taper from the front end to the rear end such that the diameter of the front end of the head section 210 is smaller than the diameter of the rear end and the tail section. The tail section 220 has an unlimited length H2. The mold 200 has a wall thickness of 10 mm, a surface roughness (Ra) of 0.2 or less, and a verticality such that the angle between the vertically placed mold 200 and a vertical line is less than 5 degrees.
[0057] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the features in the above-mentioned embodiments can be combined with each other unless there is a contradiction, and the present invention can have various modifications and changes. Any modifications, equivalents, improvements, etc. that fall within the spirit and principle of the present invention are intended to be included in the scope of the present invention. Furthermore, the examples are to be construed as illustrative and not limiting, while the scope of the present invention is defined by the appended claims, not by the above description. Therefore, all changes that are within the meaning and range of equivalents of the claims are intended to be included in this specification. Any reference numbers used in the claims should not be construed as limiting the scope of the claims.
Claims
1. The surface roughness is 0.2 μm or less, and the surface tension is 10 to 35 mN / m. A mold for molding polyurethane condoms.
2. The thermoplastic polymer is any one selected from polyurethane, polymethyl methacrylate, polystyrene, polyethylene, polyvinyl chloride, polypropylene, polystyrene, acrylonitrile butadiene-styrene, polyamide, polycarbonate, polyoxymethylene, modified polyphenylene oxide, thermoplastic polyester, polyimide, polyphenylene sulfide, polysulfone, aromatic polyamide, and materials obtained by organic modification of the above polymers or inorganic modification by filling the above polymers with inorganic materials, or any combination thereof; 2. The polyurethane condom mold according to claim 1.
3. The organic modification is any one selected from the group consisting of organosilicon modification, organofluorine modification, silane modification, acrylate copolymerization modification, vinyl monomer modification, and aromatic monomer modification, or any combination thereof; 3. The polyurethane condom mold according to claim 2.
4. The inorganic modification is any one selected from heavy calcium modification, talc modification, graphene modification, water glass modification, attapulgite modification, kaolin modification, light calcium modification, and glass microbead modification, or any combination thereof; 3. The polyurethane condom mold according to claim 2.
5. The polyurethane condom is a male condom, and the mold is A head portion and a tail portion connected to the head portion, The head portion has a columnar shape with a gradually increasing diameter and has an inclination of greater than 0 degrees and less than 5 degrees.
2. The polyurethane condom mold according to claim 1.
6. The head portion has a front end with a semen sac.
6. The mold for molding a polyurethane condom according to claim 5.
7. The head portion has a length of 200 to 260 mm.
6. The mold for molding a polyurethane condom according to claim 5.
8. The head portion is connected to the tail portion via a transition section.
6. The mold for molding a polyurethane condom according to claim 5.
9. The tail portion has a columnar shape having a constant diameter.
6. The mold for molding a polyurethane condom according to claim 5.
10. The tail portion has a cylindrical shape with a gradually increasing diameter and has a slope of greater than 0 degrees and less than or equal to 3 degrees.
6. The mold for molding a polyurethane condom according to claim 5.
11. The polyurethane condom is a female condom.
2. The polyurethane condom mold according to claim 1.
12. The polyurethane condom is a non-standard condom and the mold has a surface with floating points or threads.
2. The polyurethane condom mold according to claim 1.
13. The mold has a thickness of 2 to 25 mm or is a solid mold; 2. The polyurethane condom mold according to claim 1.
14. The mold has an angle of less than 5 degrees with respect to the vertical when positioned vertically.
2. The polyurethane condom mold according to claim 1.
15. providing a thermoplastic polymer having a surface tension of 10 to 35 mN / m; and injection molding the thermoplastic polymer to produce a polyurethane condom mold. The mold has a surface roughness of 0.2 μm or less. A method for manufacturing a mold for molding polyurethane condoms.
16. The injection molding is carried out by three-shot feeding and two-stage injection molding; A method for producing the polyurethane condom mold according to claim 15.
17. Providing a mold; Providing an emulsion comprising a polyurethane resin; suspending the mold vertically and dipping it into the latex containing the polyurethane resin to obtain a dipped mold; removing the dipped mold and drying it to form a polyurethane film on the surface of the mold; and a demolding step, The mold is made of a thermoplastic polymer having a surface roughness of 0.2 μm or less and a surface tension of 10 to 35 mN / m. A method for using a polyurethane condom molding mold.
18. The polyurethane condom has a strength of 3.5 N / mm 2 Having a 100% tensile modulus of elasticity of 18. A method for using the polyurethane condom mold according to claim 17.
19. The polyurethane condom has a burst pressure of 1 kPa or more, a burst volume of 5 L or more, and a 100% elastic modulus of 3.5 N / mm 2 Below is the 18. A method for using the polyurethane condom mold according to claim 17.
Citation Information
Patent Citations
Production method of polyurethane latex condom and special mold thereof
CN104339485A
JP1975014755A
Polymer casing having surface changed into texture and manufacture thereof
JP1990004502A