Manufacturing method of artificial lung
A simplified method using dopamine-based coatings on polypropylene hollow fiber membranes in artificial lungs addresses the issues of plasma leaks and gas exchange performance, resulting in improved durability and functionality for circulatory support.
Patent Information
- Application Number
- JP2022505898
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-03-12
- Filing Date
- 2021-02-24
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2041-02-24
AI Technical Summary
Existing methods for manufacturing artificial lungs with porous hollow fiber membranes suffer from reduced gas exchange performance due to wet lungs and plasma leaks, with silicone coating processes being complex and time-consuming.
A method involving the use of a coating solution containing dopamine or its salts and oligomers to form a polymer layer on the surface of polypropylene hollow fiber membranes, enhanced by oxygen gas exposure, simplifying the manufacturing process and improving plasma leak resistance and gas exchange performance.
The method results in an artificial lung with improved gas exchange ability, enhanced plasma leak resistance, and antithrombotic properties, suitable for long-term use in circulatory support devices.
Smart Images

Figure 0007595644000005 
Figure 0007595644000006 
Figure 0007595644000007
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing an artificial lung. [Background technology]
[0002] The gas exchange performance of an artificial lung having a porous hollow fiber membrane may decrease with long-term use. Wet lung and plasma leakage are considered to be the main causes. Wet lung can restore gas exchange performance by blowing air at high pressure to remove condensation water from the hollow fiber membrane. On the other hand, plasma leakage is considered to cause an irreversible performance decrease of the artificial lung. In the long-term use of an artificial lung, it is essential to solve the problem of plasma leakage, and many studies have been conducted so far. Among them, methods such as blocking the micropores in the hollow fiber membrane or making the micropores of the hollow fiber membrane extremely fine have been adopted as a means of improving plasma leakage resistance.
[0003] For example, Japanese Patent Application Laid-Open No. 2002-035116 describes that applying a silicone coating to the outer surface of a porous hollow fiber membrane made of polypropylene makes plasma leakage less likely to occur, enabling long-term use. Summary of the Invention
[0004] However, according to the method described in JP 2002-035116 A, a continuous line of hollow fiber membrane is moved at 0.5-50 m / min in a silicone monomer atmosphere undergoing plasma discharge under high vacuum, and silicone monomer is polymerized on the outer surface of the hollow fiber membrane to perform silicone coating. Therefore, there is a problem that the coating process requires complicated equipment and a long time.
[0005] Therefore, an object of the present invention is to provide a technique for producing an artificial lung by a simpler method.
[0006] The present inventors have conducted extensive research to solve the above problems, and as a result have found that the above object can be achieved by contacting a coating liquid containing dopamine (or a salt or oligomer thereof) with a porous hollow fiber membrane made of polypropylene under oxygen gas blowing, thereby completing the present invention.
[0007] That is, the above-mentioned object can be achieved by a method for producing an artificial lung having a plurality of porous hollow fiber membranes for gas exchange, at least a portion of which is made of polypropylene, the hollow fiber membranes having an inner surface forming an inner lumen and an outer surface, the method comprising: preparing a coating liquid containing at least one compound selected from the group consisting of dopamine and its salts and oligomers; contacting the inner or outer surface of the hollow fiber membranes with the coating liquid for less than 10 hours while blowing oxygen gas through the coating liquid, thereby forming a polymer layer containing a polymer of the compound on the inner or outer surface. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a cross-sectional view of a hollow fiber membrane external hemoperfusion type oxygenator according to one embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged cross-sectional view of a porous hollow fiber membrane for gas exchange used in a hollow fiber membrane external hemoperfusion type oxygenator according to one embodiment of the present invention. [Diagram 3] FIG. 3 is a cross-sectional view of a hollow fiber membrane external hemoperfusion type oxygenator according to another embodiment of the present invention. [Figure 4] FIG. 4 is a cross-sectional view taken along line AA in FIG. [Diagram 5] FIG. 5 is a front view showing an example of an inner tubular member used in the hollow fiber membrane external hemoperfusion type oxygenator according to the present invention. [Figure 6] FIG. 6 is a central vertical cross-sectional view of the inner tubular member shown in FIG. [Figure 7] FIG. 7 is a cross-sectional view taken along line BB in FIG. [Figure 8] FIG. 8 is a graph showing the formation of dopamine polymers in Examples 1 to 4 and Comparative Example 1. [Figure 9] FIG. 9 is a graph showing the formation of dopamine polymer in Comparative Example 2. [Figure 10] FIG. 10 is a graph showing gas permeability in the examples and comparative examples. [Figure 11] FIG. 11 is a graph showing resistance to plasma leakage in the examples and comparative examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The present invention relates to a method for producing an artificial lung having a plurality of porous hollow fiber membranes for gas exchange, at least a part of which is made of polypropylene, the hollow fiber membranes having an inner surface forming a lumen and an outer surface, the method comprising: preparing a coating solution containing at least one compound selected from the group consisting of dopamine and its salts and oligomers; contacting the inner or outer surface of the hollow fiber membrane with the coating solution for less than 10 hours while blowing oxygen gas into the coating solution, thereby forming a polymer layer containing a polymer of the compound on the inner or outer surface. According to the present invention, it is possible to provide an artificial lung by a simpler method. In this specification, at least one compound selected from the group consisting of dopamine and its salts and oligomers is also simply referred to as a "polymer layer-forming compound".
[0010] The method for producing an artificial lung according to the present invention makes it possible to provide an artificial lung in a simpler manner than the method described in JP 2002-035116 A. The mechanism by which the configuration of the present invention exerts the above-mentioned effects is presumed to be as follows. Note that the following mechanism is based on presumption, and the present invention is not limited to the following mechanism in any way.
[0011] In the method of the present invention, while blowing oxygen gas into the coating solution of the polymer layer-forming compound, the coating solution is brought into contact with the hollow fiber membrane surface for a predetermined time, and the polymer layer-forming compound is polymerized on the hollow fiber membrane surface to form a polymer layer on the hollow fiber membrane surface. For example, dopamine is usually oxidized to produce 5,6-dihydroxyindole, which is polymerized to form and deposit a dopamine polymer (polydopamine) on the substrate to form a dopamine polymer layer. Therefore, according to the method of the present invention, an artificial lung can be manufactured by a simple operation of bringing a coating solution containing a polymer layer-forming compound such as dopamine (or its salt, oligomer) into contact with the hollow fiber membrane surface. In addition, as in the present invention, by bringing a coating solution containing a polymer layer-forming compound such as dopamine (or its salt, oligomer) into contact with the hollow fiber membrane surface while blowing oxygen gas, the reaction of the polymer layer-forming compound (for example, oxidation and polymerization of dopamine) proceeds more quickly and more efficiently. Oxygen gas easily passes through the hollow fiber membrane in the thickness direction through the small-diameter hollow fiber membrane lumen and the pores of the hollow fiber membrane. Therefore, according to the method of the present invention, the reaction of the polymer layer-forming compound (e.g., oxidation and polymerization of dopamine, etc.) proceeds rapidly on the surface of the hollow fiber membrane, so that a polymer layer of a predetermined thickness can be formed by simple operations and in a short time. Here, if the coating liquid is contacted with the hollow fiber membrane for 10 hours or more, the reaction of the polymer layer-forming compound proceeds too much, the layer becomes thick, and the gas exchange capacity (gas permeation rate) is excessively reduced. Therefore, the artificial lung produced by the method of the present invention has excellent gas exchange capacity (gas permeability).
[0012] Furthermore, according to the method of the present invention, after assembling an artificial lung (or a hollow fiber membrane bundle), it is possible to contact the surface of the hollow fiber membrane with a coating liquid containing a compound such as dopamine (or a salt thereof) while blowing oxygen gas into the hollow fiber membrane. Therefore, the method of the present invention is also preferable from the viewpoint of productivity / mass production.
[0013] In addition, the reactant (particularly dopamine polymer (polydopamine)) of the polymer layer-forming compound according to the present invention has high reactivity with organic substances, and the polymer layer (dopamine polymer layer; the same applies below) according to the present invention is highly reactive. Therefore, the polymer layer has high adhesion to the hollow fiber membrane made of polypropylene. Furthermore, when an antithrombotic agent layer is formed on the polymer layer, the reactant (particularly polydopamine) of the polymer layer-forming compound in the polymer layer also exhibits high reactivity with the antithrombotic agent (e.g., polymethoxyethyl (meth)acrylate) of the antithrombotic agent layer. Therefore, the polymer layer exhibits high reactivity with the antithrombotic agent and has high adhesion to the antithrombotic agent layer. In other words, the antithrombotic agent layer can be firmly integrated with the hollow fiber membrane via the polymer layer. Therefore, the artificial lung produced by the method of the present invention has excellent effects due to the antithrombotic agent (e.g., antithrombotic properties) and resistance to plasma leakage, and can maintain its antithrombotic properties and resistance to plasma leakage even when used for a long period of time, for example, more than one month (i.e., has excellent antithrombotic properties, resistance to plasma leakage, antithrombosis maintenance properties, and resistance to plasma leakage).
[0014] Therefore, the artificial lung produced by the method of the present invention can be suitably used not only as an artificial lung for use in ordinary surgery, but also as a circulatory and pulmonary assist device for patients with serious diseases.
[0015] Hereinafter, preferred embodiments of the present invention will be described. Note that the present invention is not limited to the following embodiments. Also, the dimensional ratios in the drawings are exaggerated for the convenience of explanation and may differ from the actual ratios.
[0016] In this specification, the term "X to Y" indicating a range includes X and Y and means "X or more and Y or less." Furthermore, unless otherwise specified, the operations and measurements of physical properties are performed under the conditions of room temperature (20 to 25°C) and relative humidity of 40 to 50% RH. "A and / or B" means at least one of A and B, and includes "A", "B", and "a combination of A and B."
[0017] The method for producing an artificial lung of the present invention will be described in detail below. For the sake of convenience, the present specification will first describe an artificial lung that can be obtained by the method for producing an artificial lung of the present invention, and then describe the method for producing an artificial lung of the present invention.
[0018] <Artificial lung> The artificial lung according to one embodiment of the present invention is an artificial lung having a plurality of porous hollow fiber membranes for gas exchange, at least a portion of which is made of polypropylene, the hollow fiber membranes having an inner surface forming a lumen and an outer surface, and a polymer layer and an antithrombotic agent layer formed by the method of the present invention are disposed on at least one of the inner and outer surfaces in this order (i.e., the hollow fiber membrane, the polymer layer, and the antithrombotic agent layer). The artificial lung according to the present invention exhibits high plasma leakage resistance and the effect of the antithrombotic agent (e.g., antithrombotic properties), and can maintain its plasma leakage resistance and antithrombotic properties even when used for a long period of time, for example, more than one month (i.e., excellent plasma leakage resistance, antithrombotic properties, plasma leakage resistance maintenance, and antithrombotic maintenance properties). Therefore, the artificial lung according to the present invention can be particularly suitably used as an extracorporeal circulation device such as ECMO (Extra Corporeal Membrane Oxygenation) or PCPS (Percutaneous Cardio Pulmonary Support) for the purpose of supporting the respiration and circulation of patients suffering from circulatory failure due to pneumonia, severe respiratory failure, acute myocardial infarction, acute myocarditis, etc. In the following, the polymer layer formed by the method of the present invention will also be simply referred to as the "polymer layer according to the present invention" or "polymer layer".
[0019] The details of the prosthetic lung according to the present invention are explained below with reference to the drawings.
[0020] Fig. 1 is a cross-sectional view of a hollow fiber membrane external hemoperfusion type oxygenator according to one embodiment of the present invention. Fig. 2 is an enlarged cross-sectional view of a porous hollow fiber membrane for gas exchange used in the hollow fiber membrane external hemoperfusion type oxygenator according to one embodiment of the present invention.
[0021] In the embodiment shown in FIG. 1, the hollow fiber membrane external hemoperfusion type oxygenator 1 has a number of gas exchange porous hollow fiber membranes 3 housed in a housing 2. As shown in FIG. 2, the hollow fiber membrane 3 has a passage (lumen) 3d forming a gas chamber in the center. Here, when an oxygen-containing gas flows in the lumen 3d, blood flows on the outside (external surface 3a' side) of the hollow fiber membrane (hollow fiber membrane external hemoperfusion type oxygenator). Similarly, when blood flows in the lumen 3d, oxygen-containing gas flows on the outside (external surface 3a' side) of the hollow fiber membrane (hollow fiber membrane internal hemoperfusion type oxygenator). The present invention may be in any of the above forms, but preferably, oxygen-containing gas flows in the lumen 3d and blood flows on the outside (external surface 3a' side) of the hollow fiber membrane. In addition, the hollow fiber membrane 3 has openings 3e and 3f that communicate with its outer surface 3a' and inner surface 3c'. The polymer layer 16 and the antithrombotic agent layer 18 are formed in this order (i.e., the hollow fiber membrane, the polymer layer, and the antithrombotic agent layer) on at least one of the inner surface 3c' and the outer surface 3a' of the hollow fiber membrane 3. Here, the polymer layer 16 and the antithrombotic agent layer 18 are preferably formed at least on the side where blood flows. That is, the polymer layer 16 and the antithrombotic agent layer 18 are preferably formed at least on the outer surface 3a' of the hollow fiber membrane 3, and in consideration of the effect of further improving gas permeability, it is more preferable that they are formed only on the outer surface 3a' of the hollow fiber membrane 3. In FIG. 2, the polymer layer is disposed on the outer surface of the hollow fiber membrane, but the polymer layer may be disposed on the inner surface of the hollow fiber membrane. In FIG. 2, the polymer layer is disposed directly above the hollow fiber membrane, but the polymer layer may be disposed on the hollow fiber membrane via another layer. Preferably, the polymer layer is disposed on the outer surface of the hollow fiber membrane, and more preferably, the polymer layer is disposed directly above the outer surface of the hollow fiber membrane.
[0022] The polymer layer 16 and the antithrombotic agent layer 18 according to the present invention may be formed on at least a part of the inner surface 3c' and / or the outer surface 3a' of the hollow fiber membrane 3, but from the viewpoint of maintaining gas exchange performance during long-term use (improving plasma leakage resistance and suppressing wet rungs), it is preferable to form them on the entire inner surface 3c' and / or the outer surface 3a', and more preferably on the entire outer surface 3a'. In addition, the polymer layer 16 according to the present invention is preferably formed as a homogeneous membrane that blocks the pores of the hollow fiber membrane 3, as shown in FIG. 2. By adopting such a form, leakage of plasma through the pores of the hollow fiber membrane is suppressed, and the plasma leakage resistance of the oxygenator can be further improved. Therefore, an oxygenator having such a structure can be used for a longer period of time. Even when the form is adopted, the polymer layer 16 and the antithrombotic agent layer 18 have high gas permeability and can therefore have sufficient gas exchange performance.
[0023] The antithrombotic agent layer 18 containing the antithrombotic agent may be formed on at least a part of the polymer layer 16, but is preferably formed on the entire polymer layer 16 from the viewpoints of antithrombotic properties (inhibitory and preventative effects on adhesion / adhesion of platelets and inhibitory and preventative effects on activation of platelets), antithrombotic maintenance (durability), and plasma leakage resistance. In the embodiment shown in FIG. 2, the polymer layer 16 and the antithrombotic agent layer 18 may be present in the inner layer 3b (in some cases, the inner layer 3b and the inner surface layer 3c) of the hollow fiber membrane 3, but are preferably not substantially present in the inner layer 3b (in some cases, the inner layer 3b and the inner surface layer 3c) of the hollow fiber membrane 3. If the antithrombotic agent is not substantially present, the hydrophobic properties of the membrane base material itself are maintained in the inner layer 3b or the inner surface layer 3c of the hollow fiber membrane, and leakage (leakage) of plasma components can be effectively prevented. In this specification, "antithrombotic agent layer 18 containing an antithrombotic agent is substantially not present in inner layer 3b (in some cases, inner layer 3b and inner surface layer 3c) of hollow fiber membrane 3" means that the permeation of the antithrombotic agent is not observed near inner surface 3c' (surface on the side where oxygen-containing gas flows) of hollow fiber membrane 3. When a polymer layer is formed as described in a preferred embodiment of a method for producing an artificial lung to be described later, the polymer layer-forming compound can be substantially not present in inner layer 3b or inner surface layer 3c of hollow fiber membrane 3. Similarly, as described in a preferred embodiment of a method for producing an artificial lung to be described later, a coating is formed by applying a colloidal solution of an antithrombotic polymer compound, so that the antithrombotic polymer compound is substantially not present in inner layer 3b or inner surface layer 3c of hollow fiber membrane 3.
[0024] That is, according to a particularly preferred embodiment of the present invention, an oxygen-containing gas flows through the inner cavity of the hollow fiber membrane, blood flows on the outside (outer surface) of the hollow fiber membrane, and a polymer layer and an antithrombotic agent layer are formed in this order over the entire outer surface (blood contact portion) of the hollow fiber membrane (external perfusion type oxygenator).
[0025] The polymer layer 16 may contain other components in addition to the dopamine polymer (polydopamine). The other components are not particularly limited, but may include polyolefins, aliphatic hydrocarbons, inorganic fine particles, hydrophilic polymers, and the like. Preferably, the polymer layer 16 is substantially composed of a dopamine polymer (polydopamine), and more preferably, is composed only of a dopamine polymer (polydopamine). In this specification, "the polymer layer is substantially composed of a dopamine polymer (polydopamine)" means that the polymer layer contains components other than the dopamine polymer (polydopamine) (e.g., dopamine or a salt thereof) at a ratio of less than 5% by mass (solid content equivalent).
[0026] Similarly, the antithrombotic agent layer 18 may contain other components in addition to the antithrombotic agent (e.g., the antithrombotic polymer compound of formula (1), heparin). The other components are not particularly limited, but include crosslinkers, thickeners, preservatives, pH adjusters, amphipathic substances, and the like. Preferably, the antithrombotic agent layer 18 is substantially composed of an antithrombotic agent, and more preferably, is composed only of an antithrombotic agent. In this specification, "the antithrombotic agent layer is substantially composed of an antithrombotic agent" means that the antithrombotic agent layer contains components other than the antithrombotic agent in a proportion of less than 5% by mass (solid content equivalent).
[0027] The hollow fiber membrane oxygenator 1 of this embodiment has a housing 2 having a blood inlet 6 and a blood outlet 7, a hollow fiber membrane bundle consisting of a number of porous hollow fiber membranes 3 for gas exchange contained in the housing 2, and a pair of partitions 4, 5 that support both ends of the hollow fiber membrane bundle in a liquid-tight manner in the housing 2. The hollow fiber membrane oxygenator 1 has a blood chamber 12 formed between the partitions 4, 5 and the inner surface of the housing 2 and the outer surface of the hollow fiber membrane 3, a gas chamber formed inside the hollow fiber membrane 3, and a gas inlet 8 and a gas outlet 9 communicating with the gas chamber.
[0028] Specifically, the hollow fiber membrane oxygenator 1 of this embodiment has a cylindrical housing 2, an assembly of hollow fiber membranes 3 for gas exchange contained within the cylindrical housing 2, and partitions 4, 5 that hold both ends of the hollow fiber membranes 3 liquid-tightly to the housing 2, and the inside of the cylindrical housing 2 is partitioned into a blood chamber 12 which is a first fluid chamber and a gas chamber which is a second fluid chamber, and the cylindrical housing 2 is provided with a blood inlet 6 and a blood outlet 7 which communicate with the blood chamber 12.
[0029] A cap-shaped gas inlet header 10 having a gas inlet 8, which is a second fluid inlet, communicating with a gas chamber, which is the internal space of the hollow fiber membranes 3, is attached above the partition wall 4, which is the end of the cylindrical housing 2. Thus, a gas inlet chamber 13 is formed by the outer surface of the partition wall 4 and the inner surface of the gas inlet header 10. This gas inlet chamber 13 communicates with the gas chamber formed by the internal space of the hollow fiber membranes 3.
[0030] Similarly, a cap-shaped gas outlet header 11 is attached below the partition wall 5 and has a gas outlet 9, which is a second fluid outlet that communicates with the internal space of the hollow fiber membrane 3. Thus, a gas outlet chamber 14 is formed by the outer surface of the partition wall 5 and the inner surface of the gas outlet header 11.
[0031] The hollow fiber membrane 3 is a porous membrane at least partly made of polypropylene. Here, the hollow fiber membrane may be partly made of polypropylene and other parts made of materials other than polypropylene (other materials), or partly or entirely made of polypropylene and other materials. Preferably, the hollow fiber membrane is made of only polypropylene. As the other materials, the same materials as those used in known artificial lungs are used, and are not particularly limited. By making the hollow fiber membrane (particularly the inner surface of the hollow fiber membrane) of a hydrophobic polymer material, leakage of plasma components can be suppressed. As the material used for the porous membrane, the same hydrophobic polymer material as that used in known artificial lungs can be used. Specifically, polyolefin resins such as polyethylene and polymethylpentene, and polymer materials such as polysulfone, polyacrylonitrile, polytetrafluoroethylene, and cellulose acetate can be mentioned. Among these, polyolefin resins are preferably used, and polymethylpentene is more preferable. In addition, when the hollow fiber membrane is composed of polypropylene and other materials as described above, the content of polypropylene is usually more than 70 mass% (solid content equivalent) of all materials constituting the hollow fiber membrane, preferably 80 mass% or more (solid content equivalent), and more preferably 90 mass% or more (solid content equivalent) (upper limit: less than 100 mass%).
[0032] The inner diameter of the hollow fiber membrane is not particularly limited, but is preferably 50 to 300 μm, more preferably 80 to 200 μm. The outer diameter of the hollow fiber membrane is not particularly limited, but is preferably 100 to 400 μm, more preferably 130 to 200 μm. The thickness (membrane thickness) of the hollow fiber membrane is preferably 20 μm or more and less than 50 μm, more preferably 25 μm or more and less than 50 μm, even more preferably 25 to 45 μm, even more preferably 25 to 40 μm, even more preferably 25 to 35 μm, and particularly preferably 25 to 30 μm. In this specification, the "thickness (membrane thickness) of the hollow fiber membrane" refers to the thickness between the inner surface and the outer surface of the hollow fiber membrane, and is calculated by the formula: [(outer diameter of the hollow fiber membrane)-(inner diameter of the hollow fiber membrane)] / 2. By setting the lower limit of the thickness of the hollow fiber membrane as described above, the strength of the hollow fiber membrane can be sufficiently ensured. In addition, the manufacturing process is satisfactory in terms of labor and cost, and is also preferable from the viewpoint of mass production. The porosity of the hollow fiber membrane is preferably 5 to 90% by volume, more preferably 10 to 80% by volume, and particularly preferably 30 to 60% by volume. The pore size of the hollow fiber membrane is preferably 0.01 to 5 μm, more preferably 0.05 to 1 μm. There are no particular limitations on the manufacturing method of the hollow fiber membrane, and known manufacturing methods of hollow fiber membranes can be used in the same manner or with appropriate modifications. For example, the hollow fiber membrane is preferably one in which micropores are formed in the wall by a stretching method or a solid-liquid phase separation method.
[0033] In this specification, the "pore size of the hollow fiber membrane" refers to the average diameter of the openings on the side (outer surface side) covered with the antithrombotic agent. The pore size of the hollow fiber membrane is measured by the method described below.
[0034] First, the side (outer surface) of the hollow fiber membrane that is to be coated with the antithrombotic agent is photographed using a scanning electron microscope (SEM). Next, the obtained SEM image is processed to invert the pores (openings) to white and the rest to black, and the number of pixels in the white area is measured. The boundary level for binarization is set to the midpoint between the difference between the whitest and blackest areas.
[0035] Next, the number of pixels of the pores (openings) displayed in white is measured. The pore area is calculated based on the number of pixels of each pore thus obtained and the resolution (μm / pixel) of the SEM image. From the obtained pore area, the diameter of each pore is calculated assuming that the pores are circular, and a statistically significant number of diameters, for example, 500 pores, are randomly extracted, and the arithmetic average thereof is taken as the "pore diameter of the hollow fiber membrane."
[0036] The cylindrical housing 2 may be made of the same material as that used for the housing of known oxygenators. Specific examples include hydrophobic synthetic resins such as polycarbonate, acrylic-styrene copolymer, and acrylic-butylene-styrene copolymer. The shape of the housing 2 is not particularly limited, but is preferably cylindrical and transparent. By forming the housing from a transparent material, the inside can be easily checked.
[0037] The amount of hollow fiber membranes stored in this embodiment is not particularly limited, and the same amount as that of a known oxygenator can be applied. For example, about 5,000 to 100,000 porous hollow fiber membranes 3 are stored in parallel in the axial direction in the housing 2. Furthermore, the hollow fiber membranes 3 are fixed in a liquid-tight state by partition walls 4 and 5 with both ends of the hollow fiber membranes 3 open to both ends of the housing 2. The partition walls 4 and 5 are formed of a potting agent such as polyurethane or silicone rubber. The part of the housing 2 sandwiched between the partition walls 4 and 5 is divided into a gas chamber on the inside side of the hollow fiber membranes 3 and a blood chamber 12 on the outside of the hollow fiber membranes 3.
[0038] In this embodiment, a gas inlet header 10 having a gas inlet 8 and a gas outlet header 11 having a gas outlet 9 are attached to the housing 2 in a liquid-tight manner. These headers may also be made of any material, for example, the hydrophobic synthetic resin used for the housing described above. The headers may be attached to the housing 2 by any method, for example, by fusion using ultrasonic waves, high frequency waves, induction heating, or the like, adhesion using an adhesive, or mechanical fitting. Also, a clamping ring (not shown) may be used. It is preferable that all of the blood contact parts of the hollow fiber membrane oxygenator 1 (the inner surface of the housing 2 and the outer surface of the hollow fiber membrane 3) are made of a hydrophobic material.
[0039] In this embodiment, the antithrombotic agent layer is selectively formed on the outer surface (external perfusion type) of the hollow fiber membrane. Therefore, blood (particularly plasma components) is unlikely to penetrate into the pores of the hollow fiber membrane or does not penetrate at all. Therefore, leakage of blood (particularly plasma components) from the hollow fiber membrane can be effectively suppressed and prevented. In particular, when the antithrombotic agent is substantially absent in the inner layer 3b of the hollow fiber membrane and the inner surface layer 3c of the hollow fiber membrane, the inner layer 3b of the hollow fiber membrane and the inner surface layer 3c of the hollow fiber membrane maintain the hydrophobic state of the material, so that leakage (leak) of high blood (particularly plasma components) can be more effectively suppressed and prevented. Therefore, the artificial lung obtained by the method of the present invention can maintain high gas exchange capacity for a long period of time.
[0040] The coating of the antithrombotic agent according to the present embodiment (formation of an antithrombotic agent layer) is formed on the polymer layer on the inner and / or outer surface of the hollow fiber membrane of the artificial lung, but in addition to the above, it may be formed on other components (for example, the entire blood contact portion). By adopting this configuration, adhesion / attachment and activation of platelets can be more effectively suppressed and prevented in the entire blood contact portion of the artificial lung. In addition, the contact angle of the blood contact surface is reduced, making the priming operation easier. In this case, the coating of the antithrombotic agent according to the present invention is preferably formed on other components that come into contact with blood, but the hollow fiber membrane other than the blood contact portion or other parts of the hollow fiber membrane (for example, parts embedded in the partition wall) may not be coated with the antithrombotic agent. Since such parts do not come into contact with blood, it is not particularly problematic if they are not coated with the antithrombotic agent.
[0041] The artificial lung obtained by the method of the present invention may be of a type as shown in Fig. 3. Fig. 3 is a cross-sectional view showing another embodiment of the artificial lung obtained by the method of the present invention. Fig. 4 is a cross-sectional view taken along line AA in Fig. 3.
[0042] In Figure 3, an artificial lung (hollow fiber membrane external blood perfusion type artificial lung) 20 has an inner tubular member 31 having a blood flow opening 32 on the side, a tubular hollow fiber membrane bundle 22 consisting of a number of porous hollow fiber membranes 3 for gas exchange wrapped around the outer surface of the inner tubular member 31, a housing 23 that stores the tubular hollow fiber membrane bundle 22 together with the inner tubular member 31, partitions 25, 26 that fix both ends of the tubular hollow fiber membrane bundle 22 to the housing with both ends of the hollow fiber membrane 3 open, a blood inlet 28 and blood outlets 29a, 29b that communicate with a blood chamber 17 formed in the housing 23, and a gas inlet 24 and gas outlet 27 that communicate with the inside of the hollow fiber membranes 3.
[0043] As shown in Figures 3 and 4, in the oxygenator 20 of this embodiment, the housing 23 includes an outer tubular member 33 that houses an inner tubular member 31, and the tubular hollow fiber membrane bundle 22 is housed between the inner tubular member 31 and the outer tubular member 33. Furthermore, the housing 23 includes one of a blood inlet or a blood outlet that communicates with the inside of the inner tubular member, and the other of a blood inlet or a blood outlet that communicates with the inside of the outer tubular member.
[0044] Specifically, in the oxygenator 20 of this embodiment, the housing 23 is housed in an outer cylindrical member 33 and an inner cylindrical member 31, and includes an inner cylindrical body 35 whose tip opens inside the inner cylindrical member 31. A blood inlet 28 is formed at one end (lower end) of the inner cylindrical body 35, and two blood outlets 29a, 29b extending outward are formed on the side surface of the outer cylindrical member 33. The number of blood outlets may be one or more.
[0045] The tubular hollow fiber membrane bundle 22 is wound around the outer surface of the inner tubular member 31. In other words, the inner tubular member 31 serves as the core of the tubular hollow fiber membrane bundle 22. The inner cylinder 35 housed inside the inner tubular member 31 has an opening at its tip near the first partition wall 25. A blood inlet 28 is formed at the lower end protruding from the inner tubular member 31.
[0046] The inner cylinder 35, the inner tubular member 31 with the hollow fiber membrane bundle 22 wound around its outer surface, and the outer tubular member 33 are arranged approximately concentrically. The concentric positional relationship between one end (upper end) of the inner tubular member 31 with the hollow fiber membrane bundle 22 wound around its outer surface and one end (upper end) of the outer tubular member 33 is maintained by the first partition wall 25, and the space formed inside the inner tubular member and between the outer tubular member 33 and the outer surface of the hollow fiber membranes is liquid-tight and does not communicate with the outside.
[0047] In addition, the concentric positional relationship between the portion of the inner cylinder 35 slightly above the blood inlet 28, the other end (lower end) of the inner tubular member 31 around whose outer surface the hollow fiber membrane bundle 22 is wound, and the other end (lower end) of the outer tubular member 33 are maintained by the second partition 26, and the space formed between the inner cylinder 35 and the inner tubular member 31 and the space formed between the outer tubular member 33 and the outer surface of the hollow fiber membranes are liquid-tight and do not communicate with the outside. In addition, the partitions 25, 26 are formed of a potting agent such as polyurethane or silicone rubber.
[0048] Therefore, the artificial lung 20 of this embodiment is provided with a blood inlet 17a formed by the inside of the inner cylindrical body 35, a first blood chamber 17b which is essentially a cylindrical space formed between the inner cylindrical body 35 and the inner cylindrical member 31, and a second blood chamber 17c which is essentially a cylindrical space formed between the hollow fiber membrane bundle 22 and the outer cylindrical member 33, and these form the blood chamber 17.
[0049] Then, blood flowing in from blood inlet 28 flows into blood inlet 17a, rises inside inner cylinder 35 (blood inlet 17a), flows out from upper end 35a (open end) of inner cylinder 35, flows into first blood chamber 17b, passes through opening 32 formed in inner tubular member 31, comes into contact with the hollow fiber membrane, undergoes gas exchange, then flows into second blood chamber 17c, and flows out from blood outlets 29a, 29b.
[0050] A gas inflow member 41 having a gas inlet 24 is fixed to one end of the outer cylindrical member 33, and a gas outflow member 42 having a gas outlet 27 is fixed to the other end of the outer cylindrical member 33. The blood inflow port 28 of the inner cylindrical body 35 passes through the gas outflow member 42 and protrudes to the outside.
[0051] The outer cylindrical member 33 is not particularly limited, but may be a cylinder, a polygonal cylinder, or one having an elliptical cross section. A cylinder is preferable. The inner diameter of the outer cylindrical member is not particularly limited, and may be the same as the inner diameter of the outer cylindrical member used in known oxygenators, but is preferably about 32 to 164 mm. The effective length of the outer cylindrical member (the length of the part not buried in the bulkhead) is also not particularly limited, and may be the same as the effective length of the outer cylindrical member used in known oxygenators, but is preferably about 10 to 730 mm.
[0052] The shape of the inner cylindrical member 31 is not particularly limited, and may be, for example, a cylinder, a polygonal tube, or one having an elliptical cross section. A cylinder is preferable. The outer diameter of the inner cylindrical member is not particularly limited, and may be the same as the outer diameter of inner cylindrical members used in known artificial lungs, and is preferably about 20 to 100 mm. The effective length of the inner cylindrical member (the length of the part not buried in the bulkhead out of the total length) is also not particularly limited, and may be the same as the effective length of inner cylindrical members used in known artificial lungs, and is preferably about 10 to 730 mm.
[0053] The inner cylindrical member 31 has a number of openings 32 for blood circulation on its side surface. The size of the openings 32 is preferably large in total area as long as the necessary strength of the cylindrical member is maintained. As shown in FIG. 5, which is a front view, FIG. 6, which is a central vertical cross-sectional view of FIG. 5, and FIG. 7, which is a cross-sectional view along line BB of FIG. 5, an annularly arranged opening in which a plurality of openings 32 (for example, 4 to 24 openings, 8 openings in the longitudinal direction in the figure) are provided at equal angular intervals on the outer peripheral surface of the cylindrical member, and multiple sets of openings are provided at equal intervals in the axial direction of the cylindrical member (8 sets per circumference in the figure). Furthermore, the opening shape may be a circle, a polygon, an ellipse, etc., but an oval shape as shown in FIG. 5 is preferable.
[0054] The shape of the inner cylinder 35 is not particularly limited, and may be, for example, a cylinder, a polygonal cylinder, or one with an elliptical cross section. A cylinder is preferable. The distance between the tip opening of the inner cylinder 35 and the first partition wall 25 is not particularly limited, and may be the same as that used in known artificial lungs, with a preferred range being about 20 to 50 mm. The inner diameter of the inner cylinder 35 is also not particularly limited, and may be the same as that used in known artificial lungs, with a preferred range being about 10 to 30 mm.
[0055] The thickness of the cylindrical hollow fiber membrane bundle 22 is not particularly limited, and may be the same as the thickness of a cylindrical hollow fiber membrane bundle used in a known artificial lung, but is preferably 5 to 35 mm, and more preferably 10 to 28 mm. The filling rate of the hollow fiber membrane in the cylindrical space formed between the outer surface and the inner surface of the cylindrical hollow fiber membrane bundle 22 is also not particularly limited, and the filling rate in a known artificial lung can be applied in the same manner, but is preferably 40 to 85%, and more preferably 45 to 80%. The outer diameter of the hollow fiber membrane bundle 22 may be the same as the outer diameter of a hollow fiber membrane bundle used in a known artificial lung, but is preferably 30 to 170 mm, and more preferably 70 to 130 mm. The gas exchange membrane is the one described above.
[0056] The hollow fiber membrane bundle 22 can be formed by winding hollow fiber membranes around the inner tubular member 31, specifically, forming a hollow fiber membrane bobbin with the inner tubular member 31 as a core, fixing both ends of the formed hollow fiber membrane bobbin with partition walls, and then cutting both ends of the hollow fiber membrane bobbin together with the inner tubular member 31 as the core. Note that this cutting opens the hollow fiber membranes on the outer surface of the partition walls. Note that the method for forming the hollow fiber membranes is not limited to the above method, and other known methods for forming hollow fiber membranes may be used in the same manner or with appropriate modifications.
[0057] In particular, it is preferable that one or more hollow fiber membranes are wound around the inner tubular member 31 at the same time so that the hollow fiber membranes are substantially parallel and adjacent hollow fiber membranes are spaced at a substantially constant distance from each other. This makes it possible to more effectively suppress uneven flow of blood. Furthermore, the distance between adjacent hollow fiber membranes is preferably 1 / 10 to 1 / 1 of the outer diameter of the hollow fiber membrane, although this is not limited thereto. Furthermore, it is preferable that the distance between adjacent hollow fiber membranes is 30 to 200 μm.
[0058] Furthermore, the hollow fiber membrane bundle 22 is preferably formed by winding one or more (preferably 2 to 16) hollow fiber membranes simultaneously around the inner tubular member 31 such that all adjacent hollow fiber membranes are spaced substantially at a constant interval, and is preferably formed by winding the hollow fiber membranes around the inner tubular member 31 by moving a rotor for rotating the inner tubular member 31 and a winder for weaving the hollow fiber membranes under the conditions of the following formula (1) when winding the hollow fiber membranes around the inner tubular member.
[0059]
number
[0060] By satisfying the above conditions, the formation of blood drift can be reduced. In this case, n, which is the relationship between the number of revolutions of the winding rotor and the number of reciprocations of the winder, is not particularly limited, but is usually 1 to 5, and preferably 2 to 4.
[0061] Also, in the hollow fiber membrane oxygenator 20, as shown in FIG. 2, the polymer layer 16 and the antithrombotic agent layer 18 are formed in this order (i.e., in the order of the hollow fiber membrane, the polymer layer, and the antithrombotic agent layer) on at least one of the inner surface 3c' of the hollow fiber membrane 3 through which the oxygen-containing gas flows and the outer surface 3a' of the hollow fiber membrane 3 which is the blood contact portion (in some cases, the outer surface 3a' and the outer surface layer 3a). Here, the polymer layer 16 and the antithrombotic agent layer 18 are preferably formed at least on the side through which blood flows. That is, the polymer layer 16 and the antithrombotic agent layer 18 are preferably formed at least on the outer surface 3a' of the hollow fiber membrane 3, and in consideration of the effect of further improving gas permeability, it is more preferable that they are formed only on the outer surface 3a' of the hollow fiber membrane 3. Here, the preferred form of the hollow fiber membrane (inner diameter, outer diameter, wall thickness, porosity, pore size, etc.) is not particularly limited, but the same form as that described in FIG. 1 above can be adopted.
[0062] <Manufacturing method of artificial lung> Next, the method for producing an artificial lung of the present invention will be described in detail. The method is a method for producing an artificial lung having a plurality of porous hollow fiber membranes for gas exchange, at least a part of which is made of polypropylene, the hollow fiber membranes having an inner surface forming a lumen and an outer surface, and is characterized in that a coating liquid containing at least one compound selected from the group consisting of dopamine and its salts and oligomers is prepared, and while blowing oxygen gas into the coating liquid, the inner surface or the outer surface of the hollow fiber membrane is brought into contact with the coating liquid for less than 10 hours to form a polymer layer containing a polymer of the compound on the inner surface or the outer surface.
[0063] In the manufacturing method of this embodiment, first, a coating liquid containing at least one compound selected from the group consisting of dopamine and its salts and oligomers is prepared ((1) coating liquid preparation step). Then, while blowing oxygen gas into the coating liquid prepared above, the inner or outer surface of the hollow fiber membrane is brought into contact with the coating liquid for less than 10 hours ((2) coating liquid application step). Each step will be described below.
[0064] (1) Coating solution preparation process In this step, a coating liquid is prepared that contains at least one compound (polymer layer-forming compound) selected from the group consisting of dopamine and its salts (dopamine salts) and oligomers (dopamine oligomers). This coating liquid is used to apply to the inner or outer surface of the hollow fiber membrane (hereinafter also simply referred to as the "hollow fiber membrane surface"). The coating liquid contains at least one compound (polymer layer-forming compound) selected from the group consisting of dopamine and its salts and oligomers, and a solvent.
[0065] The polymer layer-forming compound is applied to the surface of the hollow fiber membrane in this step, and then the polymer layer is formed as a homogeneous membrane in the coating liquid application step (2) described below. This has the function of suppressing leakage of plasma from one side of the hollow fiber membrane to the other side (from the outer surface side to the inner surface side or from the inner surface side to the outer surface side) (hence, excellent plasma leakage resistance). In addition, it has the function of improving adhesion with the antithrombotic agent layer described in detail below (hence, antithrombotic properties and plasma leakage resistance can be maintained even under long-term use). Here, the polymer layer-forming compound is selected from the group consisting of dopamine and its salts and oligomers. The salt of dopamine is not particularly limited, but examples thereof include dopamine hydrochloride (2-(3,4-dihydroxyphenyl)ethylamine hydrochloride). As the oligomer of dopamine, for example, a polymer in which about 2 to 50 5,6-dihydroxyindoles are repeated can be used. Among these, from the viewpoint of further improving the plasma leakage resistance and the adhesion with the antithrombotic agent layer, it is preferable to use dopamine or a dopamine salt, it is more preferable to use dopamine or dopamine hydrochloride, and it is particularly preferable to use dopamine hydrochloride. That is, in a preferred embodiment of the present invention, the compound is dopamine or a dopamine salt. In a preferred embodiment of the present invention, the compound is dopamine or dopamine hydrochloride. In a particularly preferred embodiment of the present invention, the compound is dopamine hydrochloride.
[0066] The polymer layer-forming compound may be either a commercially available product or a synthetic product, and may be purchased from, for example, Towa Pharmaceutical Co., Ltd., Nacalai Tesque Inc., Sigma-Aldrich Japan LLC, or the like.
[0067] The polymer layer-forming compound may be used alone or in combination of two or more kinds.
[0068] In addition, the solvent used to prepare the coating liquid is not particularly limited as long as it can dissolve the polymer layer-forming compound, and is appropriately selected according to the type of polymer layer-forming compound.Specific examples include buffers such as phosphate buffer (PBS), carbonate buffer, Tris buffer, glycine buffer, and Tricine buffer; HEPES buffer, etc.
[0069] The concentration of the polymer layer-forming compound in the coating solution is not particularly limited, but is preferably 0.1 to 50 mg / mL, more preferably 0.5 to 10 mg / mL, from the viewpoints of improving the liquid permeability of the coating solution in the lumen of the hollow fiber membrane, costs, polymerization rate, etc. The pH of the coating solution is not particularly limited, but is preferably 5.0 to 10.0, more preferably near neutral (for example, 6.0 to 8.0, particularly 6.5 to 7.5), from the viewpoints of operability, reaction of the polymer layer-forming compound (particularly polymerization rate of dopamine), etc.
[0070] The coating liquid may contain additives, if necessary, in addition to the polymer layer-forming compound and the solvent, such as polyolefins, aliphatic hydrocarbons, inorganic fine particles, and water-soluble polymers.
[0071] (2) Coating liquid application process In this step, the coating liquid prepared above is blown through the coating liquid while the inner or outer surface of the hollow fiber membrane is brought into contact with the coating liquid for less than 10 hours, so that the coating liquid is applied (coated) to the outer or inner surface of the hollow fiber membrane. The form (material, inner diameter, outer diameter, wall thickness, porosity, pore size) of the hollow fiber membrane to be coated with the coating liquid is explained above in the section on <artificial lung>, so a detailed explanation is omitted here.
[0072] Specifically, after assembling an oxygenator (for example, one having a structure as shown in FIG. 1 or FIG. 3), the coating liquid prepared as described above is brought into contact with (or circulated through) at least one of the outer and inner surfaces of the hollow fiber membrane, and oxygen gas is circulated directly or through the openings of the hollow fiber membrane. As a result, a reaction of the polymer layer-forming compound (for example, oxidation and polymerization of dopamine) proceeds on the outer or inner surface of the hollow fiber membrane (i.e., the blood contact portion), and a coating film (polymer layer) containing a polymer of the polymer layer-forming compound is formed on the outer or inner surface of the hollow fiber membrane. The coating liquid may be applied to the hollow fiber membrane before assembling the oxygenator. From the viewpoint of productivity / mass production, it is preferable to bring the coating liquid into contact with (or circulate through) at least one of the outer and inner surfaces of the hollow fiber membrane while circulating oxygen gas after assembling the oxygenator (or hollow fiber membrane bundle).
[0073] As described above, a preferred embodiment of the oxygenator produced by the method according to the present invention is an external perfusion type oxygenator. Therefore, it is preferred to apply a coating liquid to the outer surface of the hollow fiber membrane. That is, in a preferred embodiment of the present invention, the outer surface of the hollow fiber membrane is contacted with a coating liquid containing a polymer layer-forming compound, and oxygen gas is passed through the lumen (inner surface) of the hollow fiber membrane via the opening.
[0074] It is preferable to inject oxygen gas into the coating liquid before contacting the hollow fiber membrane surface with the coating liquid. This allows the reaction of the polymer layer-forming compound (e.g., oxidation and polymerization of dopamine) to proceed more quickly and efficiently. The conditions for injecting oxygen gas are not particularly limited, but are preferably such that the oxygen concentration in the coating liquid (at 25°C) is about 0.5 to 1.5% by volume, particularly about 0.8 to 1.2% by volume.
[0075] The method for contacting the surface of the hollow fiber membrane with the coating liquid is not particularly limited. For example, a method of immersing the hollow fiber membrane in the coating liquid, a method of flowing (filling) the coating liquid into the cavity of the hollow fiber membrane, a method of applying the coating liquid to the outer surface of the hollow fiber membrane, etc. can be used. In addition, when the coating liquid is brought into contact with only one surface of the hollow fiber membrane, for example, methods such as immersing the hollow fiber membrane in the coating liquid and then passing oxygen gas through the hollow fiber membrane lumen (according to this embodiment, a polymer layer can be selectively formed on the outer surface of the hollow fiber membrane); inserting a wire having approximately the same inner diameter as the hollow fiber membrane lumen into the hollow fiber membrane lumen or blocking both ends of the hollow fiber membrane to prevent the coating liquid from entering the lumen, and then contacting the hollow fiber membrane with the coating liquid (according to this embodiment, a polymer layer can be selectively formed on the outer surface of the hollow fiber membrane); sealing the outer surface of the hollow fiber membrane with a film or the like, and then contacting the hollow fiber membrane with the coating liquid (according to this embodiment, a polymer layer can be selectively formed on the inner surface of the hollow fiber membrane); or contacting the hollow fiber membrane with the coating liquid in a state in which the lumen of the hollow fiber membrane has been filled with a nonpolar solvent in advance.
[0076] Next, oxygen gas is blown into the coating liquid. This causes the polymer layer-forming compound in the coating liquid to react (e.g., oxidation and polymerization of dopamine), and the reactant of the polymer layer-forming compound (e.g., polydopamine) is formed and deposited on the surface of the hollow fiber membrane to form a polymer layer. Here, the contact (blow) time of oxygen gas is less than 10 hours. If the coating liquid is contacted with the hollow fiber membrane for more than 10 hours, the reaction of the polymer layer-forming compound (e.g., oxidation and polymerization of dopamine) will proceed too much, the layer (e.g., dopamine polymer layer) will become thick, and the gas exchange capacity (gas permeation rate) will be excessively reduced, and the obtained hollow fiber membrane will not be suitable for an artificial lung. In addition, it is also disadvantageous and undesirable from the viewpoint of cost. From the viewpoint of adhesion to the hollow fiber membrane and the antithrombotic agent layer described in detail below, gas exchange ability (gas permeation rate), and further the balance between these, the contact (blow) time of oxygen gas is preferably 8 hours or less, more preferably less than 6 hours, even more preferably 5 hours or less, and particularly preferably 4 hours or less. The lower limit of the contact (blow) time of oxygen gas is preferably more than 15 minutes, more preferably more than 30 minutes, even more preferably 40 minutes or more, even more preferably 60 minutes or more, and particularly preferably 120 minutes or more, from the viewpoint of adhesion to the hollow fiber membrane and the antithrombotic agent layer described in detail below. Therefore, the contact (blow) time of oxygen gas is preferably more than 15 minutes and less than 10 hours, more preferably more than 30 minutes and less than 8 hours, even more preferably 40 minutes or more and less than 6 hours, even more preferably 60 minutes or more and less than 5 hours, and particularly preferably 120 minutes or more and less than 4 hours. Such a contact (inflation) time ensures sufficient plasma leakage resistance and gas exchange capacity (gas permeation rate) while allowing the hollow fiber membrane and the antithrombotic agent layer to adhere more firmly via the polymer layer.
[0077] The method of blowing oxygen gas is not particularly limited as long as the reaction proceeds efficiently. For example, there is a method of blowing oxygen gas into the cavity of the hollow fiber membrane by connecting one end of the hollow fiber membrane to an oxygen gas tank, or a method of bubbling oxygen gas into the coating liquid to bring the polymer layer-forming compound into contact with the oxygen gas.
[0078] The hollow fiber membrane surface may be contacted with the coating liquid while the cavity of the hollow fiber membrane is under negative pressure. This method allows the coating liquid to come into contact with the hollow fiber membrane surface (particularly the hollow fiber membrane cavity) more uniformly and reliably. In this embodiment, the degree of negative pressure is not particularly limited, but it is preferable that the cavity of the hollow fiber membrane is under a negative pressure of 50 hPa to 150 hPa, preferably 50 hPa to 100 hPa. Here, the method of making the cavity of the hollow fiber membrane under negative pressure is not particularly limited, but for example, a vacuum pump (e.g., a diaphragm pump) and one end of the hollow fiber membrane are airtightly connected, and the vacuum pump can be operated to make the cavity under negative pressure. In this specification, the "degree of negative pressure (atmospheric pressure)" is the value of the indicated pressure of the vacuum pump.
[0079] The oxygen gas may be pure oxygen gas or a mixed gas containing oxygen gas. Preferably, the oxygen gas is pure oxygen gas (content of other gases: substantially 0% by volume (less than 5% by volume relative to the total volume). Here, the other gases that can be used when using the mixed gas are not particularly limited as long as they do not impair the effects of the present invention. For example, inert gases such as nitrogen gas, argon gas, and helium gas can be used. From the viewpoint of efficient progress of the above reaction, the content of the other gases is preferably more than 0% by volume and less than 50% by volume, more preferably more than 0% by volume and less than 20% by volume, relative to the total circulation amount (volume) of the mixed gas.
[0080] Other conditions for blowing oxygen gas are not particularly limited. For example, the blowing temperature is preferably 10 to 60°C, more preferably 25 to 40°C. The blowing rate of oxygen gas is preferably 0.05 to 0.7 L / min, more preferably 0.25 to 0.5 L / min. Under such conditions, a sufficient amount of oxygen gas can be supplied to the polymer layer-forming compound, and the reaction of the polymer layer-forming compound (for example, oxidation and polymerization of dopamine) can be sufficiently carried out.
[0081] As a result, the polymer layer-forming compound reacts to form a layer (e.g., a dopamine polymer layer) on the surface of the hollow fiber membrane, and if necessary, this state may be maintained after blowing in oxygen gas. This operation allows the reaction of the polymer layer-forming compound to proceed further, and the polymer layer can be more efficiently formed on the surface of the hollow fiber membrane. The maintaining conditions are not particularly limited. For example, the maintaining temperature is preferably 10 to 60°C, more preferably 25 to 40°C. The maintaining time is preferably 30 minutes to 24 hours, more preferably 1 to 12 hours. Under these conditions, the reaction of the polymer layer-forming compound proceeds further sufficiently, and the polymer layer can be more efficiently formed on the surface of the hollow fiber membrane. The maintaining operation may be performed in the air or in an inert gas atmosphere.
[0082] Thereafter, the coating film is washed and dried as necessary. The washing method is not particularly limited, but for example, washing is performed with water, an alcohol-based solvent (e.g., ethanol), etc. This makes it possible to remove unreacted polymer layer-forming compounds. In addition, the drying method is not particularly limited, but for example, methods such as natural drying, drying under reduced pressure, and high-temperature drying at normal pressure can be used.
[0083] In this way, a polymer layer is formed on the surface of the hollow fiber membrane. The film thickness (dry film thickness) of the polymer layer is not particularly limited, but is preferably 10 to 500 nm, more preferably 100 to 400 nm, and even more preferably 150 to 300 nm. When the film thickness of the polymer layer is 10 nm or more, sufficient adhesion to the hollow fiber membrane surface and the antithrombotic agent layer and sufficient plasma leakage resistance can be obtained. When the film thickness of the polymer layer is 500 nm or less, a decrease in gas exchange performance can be prevented. In this specification, the film thickness of the polymer layer is a value measured by dividing the mass of the coated polymer from the mass change by thermogravimetry (TG measurement) by the density of the polymer to calculate the volume, and then dividing the volume by the surface area. When the polymer layer is composed of polydopamine (PDA) (it is a polydopamine layer), the mass of the coated PDA from the mass change by TG measurement is calculated by dividing the mass by the density of the PDA (1.00 g / cm 3) to calculate the volume, and the volume is divided by the surface area to obtain the thickness of the polymer layer.
[0084] The above steps (1) and (2) form a polymer layer on the surface of the hollow fiber membrane. The method for producing an artificial lung according to this embodiment may include other steps in addition to steps (1) and (2). Examples of other steps include the following (3) antithrombotic agent layer forming step. This step is preferably performed after steps (1) and (2).
[0085] (3) Antithrombotic agent layer formation process In this step, a coating (antithrombogenic agent layer) containing an antithrombogenic agent is formed on the polymer layer. In one embodiment, an aqueous coating liquid containing an antithrombogenic agent is prepared, and the aqueous coating liquid is applied to the polymer layer formed on the outer surface or inner surface of the hollow fiber membrane in (2) above. As described above, the polymer layer and the antithrombogenic agent layer are preferably formed on the outer surface of the hollow fiber membrane. That is, in a preferred embodiment of the present invention, the production method of the present invention further comprises forming a polymer layer on the outer surface of the hollow fiber membrane, and forming an antithrombogenic agent layer containing an antithrombogenic agent on the polymer layer. The method of forming the antithrombogenic agent and the antithrombogenic agent layer (coating) is not particularly limited, and known methods can be appropriately adopted.
[0086] The antithrombotic agent is a compound that imparts antithrombotic properties to the artificial lung by being applied to the polymer layer formed on the surface of the hollow fiber membrane (for example, the outer surface of the hollow fiber membrane), which is the part that comes into contact with blood.
[0087] The antithrombotic agent can be used without any particular limitation as long as it has antithrombotic properties and biocompatibility. In particular, from the viewpoint of excellent properties, it is preferable that the antithrombotic agent has a structural unit derived from an alkoxyalkyl (meth)acrylate represented by the following formula (1). That is, in a preferred embodiment of the present invention, the antithrombotic agent has a structural unit (1) represented by the following formula (1).
[0088] [ka]
[0089] In the above formula (1), R 1 represents an alkylene group having 1 to 4 carbon atoms; R 2 represents an alkyl group having 1 to 4 carbon atoms; and R 3 represents a hydrogen atom or a methyl group.
[0090] A compound having a structural unit represented by formula (1) has excellent antithrombotic biocompatibility (the effect of inhibiting and preventing platelet adhesion / adhesion, and the effect of inhibiting and preventing platelet activation), particularly the effect of inhibiting and preventing platelet adhesion / adhesion. Therefore, by using a compound having the above structural unit, it is possible to manufacture an artificial lung having excellent antithrombotic biocompatibility (the effect of inhibiting and preventing platelet adhesion / adhesion, and the effect of inhibiting and preventing platelet activation), particularly the effect of inhibiting and preventing platelet adhesion / adhesion.
[0091] In this specification, "(meth)acrylate" means "acrylate and / or methacrylate." In other words, "alkoxyalkyl (meth)acrylate" includes only alkoxyalkyl acrylate, only alkoxyalkyl methacrylate, and both alkoxyalkyl acrylate and alkoxyalkyl methacrylate.
[0092] In formula (1), R 1 R represents an alkylene group having 1 to 4 carbon atoms. The alkylene group having 1 to 4 carbon atoms is not particularly limited, and may be a straight or branched alkylene group such as a methylene group, an ethylene group, a trimethylene group, a tetramethylene group, or a propylene group. Of these, an ethylene group or a propylene group is preferred, and an ethylene group is particularly preferred in view of the effect of further improving antithrombotic properties and biocompatibility. 2R represents an alkyl group having 1 to 4 carbon atoms. The alkyl group having 1 to 4 carbon atoms is not particularly limited, and examples of the alkyl group having 1 to 4 carbon atoms include linear or branched alkyl groups such as methyl, ethyl, propyl, isopropyl, butyl, isobutyl, sec-butyl, and tert-butyl. Of these, methyl and ethyl groups are preferred, and in consideration of the effect of further improving antithrombotic properties and biocompatibility, methyl is particularly preferred. 3 represents a hydrogen atom or a methyl group.
[0093] When the antithrombotic agent has two or more types of constituent units derived from alkoxyalkyl (meth)acrylate, the respective constituent units may be the same or different.
[0094] Specific examples of the alkoxyalkyl (meth)acrylate include methoxymethyl acrylate, methoxyethyl acrylate, methoxypropyl acrylate, ethoxymethyl acrylate, ethoxyethyl acrylate, ethoxypropyl acrylate, ethoxybutyl acrylate, propoxymethyl acrylate, butoxyethyl acrylate, methoxybutyl acrylate, methoxymethyl methacrylate, methoxyethyl methacrylate, ethoxymethyl methacrylate, ethoxyethyl methacrylate, propoxymethyl methacrylate, butoxyethyl methacrylate, etc. Among these, from the viewpoint of further improving the antithrombotic and biocompatible properties, methoxyethyl (meth)acrylate and methoxybutyl acrylate are preferred, and methoxyethyl acrylate (MEA) is particularly preferred. That is, the antithrombotic agent is preferably polymethoxyethyl acrylate (PMEA). The above alkoxyalkyl (meth)acrylates may be used alone or in combination of two or more.
[0095] The antithrombotic agent according to the present invention preferably has a structural unit derived from an alkoxyalkyl (meth)acrylate, and may be a polymer (homopolymer) composed of one or more structural units derived from an alkoxyalkyl (meth)acrylate, or a polymer (copolymer) composed of one or more structural units derived from an alkoxyalkyl (meth)acrylate and one or more structural units (other structural units) derived from a monomer that can be copolymerized with the alkoxyalkyl (meth)acrylate. When the antithrombotic agent according to the present invention is composed of two or more structural units, the structure of the polymer (copolymer) is not particularly limited, and may be any of a random copolymer, an alternating copolymer, a periodic copolymer, and a block copolymer. In addition, the terminal of the polymer is not particularly limited and is appropriately specified depending on the type of raw material used, but is usually a hydrogen atom.
[0096] Here, in the case where the antithrombotic agent according to the present invention has other structural units in addition to the structural units derived from an alkoxyalkyl (meth)acrylate, the monomer (copolymerizable monomer) that can be copolymerized with the alkoxyalkyl (meth)acrylate is not particularly limited. Examples of the copolymerizable monomer include methyl acrylate, ethyl acrylate, propyl acrylate, butyl acrylate, 2-ethylhexyl acrylate, methyl methacrylate, ethyl methacrylate, propyl methacrylate, butyl methacrylate, 2-ethylhexyl methacrylate, hexyl acrylate, hexyl methacrylate, ethylene, propylene, acrylamide, N,N-dimethylacrylamide, N,N-diethylacrylamide, aminomethyl acrylate, aminoethyl acrylate, aminoisopropyl acrylate, diaminomethyl acrylate, diaminoethyl acrylate, diaminobutyl acrylate, methacrylamide, N,N-dimethylmethacrylamide, N,N-diethylmethacrylamide, aminomethyl methacrylate, aminoethyl methacrylate, diaminomethyl methacrylate, diaminoethyl methacrylate, etc. Among these, the copolymerizable monomer is preferably one having no hydroxyl group or cationic group in the molecule. The copolymer may be any of random copolymers, block copolymers, and graft copolymers, and can be synthesized by known methods such as radical polymerization, ionic polymerization, and polymerization using macromers. Here, the ratio of the constituent units derived from the copolymerizing monomer in the total constituent units of the copolymer is not particularly limited, but considering antithrombotic properties and biocompatibility, it is preferable that the constituent units derived from the copolymerizing monomer (other constituent units) are more than 0 mol% and 50 mol% or less in the total constituent units of the copolymer. If it exceeds 50 mol%, the effect of the alkoxyalkyl (meth)acrylate may be reduced.
[0097] Here, the weight average molecular weight of the antithrombotic agent is not particularly limited, but is preferably 80,000 or more. In the manufacturing method of the artificial lung according to this embodiment, the antithrombotic agent is applied to the polymer layer formed on the outer surface or inner surface of the hollow fiber membrane in the form of an aqueous coating liquid. Therefore, from the viewpoint of easy preparation of a desired aqueous coating liquid, the weight average molecular weight of the antithrombotic agent is preferably less than 800,000. By setting it within the above range, it is possible to suppress aggregation or precipitation of the compound in the solution containing the antithrombotic agent, and to prepare a stable aqueous coating liquid. Furthermore, the weight average molecular weight of the antithrombotic agent is preferably more than 200,000 and less than 800,000, more preferably 210,000 or more and 600,000 or less, even more preferably 220,000 or more and 500,000 or less, and particularly preferably 230,000 or more and 450,000 or less.
[0098] In this specification, the "weight average molecular weight" is measured by gel permeation chromatography (GPC) using polystyrene as a standard substance and tetrahydrofuran (THF) as a mobile phase. Specifically, the polymer to be analyzed is dissolved in THF to prepare a 10 mg / ml solution. For the polymer solution thus prepared, a GPC column LF-804 manufactured by Shodex Co., Ltd. is attached to a GPC system LC-20 manufactured by Shimadzu Corporation, THF is run as a mobile phase, and polystyrene is used as a standard substance to measure the GPC of the polymer to be analyzed. After preparing a calibration curve with standard polystyrene, the weight average molecular weight of the polymer to be analyzed is calculated based on this curve.
[0099] It is presumed that by increasing the molecular weight of the antithrombotic agent, the content of polymers with relatively small molecular weights contained in the coating can be reduced, and as a result, the effect of suppressing and preventing the relatively small molecular weight polymers from dissolving into the blood can be obtained. Therefore, when the weight-average molecular weight of the antithrombotic agent is within the above range, the dissolution of the coating (especially low molecular weight polymers) into the blood can be more effectively suppressed and prevented. It is also preferable in terms of antithrombotic properties and biocompatibility. In addition, in this specification, the "low molecular weight polymer" means a polymer with a weight-average molecular weight of less than 60,000. The method for measuring the weight-average molecular weight is as described above.
[0100] In addition, the antithrombotic agent containing the structural unit derived from the alkoxyalkyl (meth)acrylate represented by the above formula (1) can be produced by a known method. Specifically, a method is preferably used in which the alkoxyalkyl (meth)acrylate represented by the following formula (2) and one or more monomers (copolymerizable monomers) that can be copolymerized with the above alkoxyalkyl (meth)acrylate, which are added as needed, are stirred together with a polymerization initiator in a polymerization solvent to prepare a monomer solution, and the monomer solution is heated to (co)polymerize the alkoxyalkyl (meth)acrylate, or the alkoxyalkyl (meth)acrylate and the copolymerizable monomer that is added as needed.
[0101] [ka]
[0102] In the above formula (2), the substituent R 1 , R 2 and R 3 is defined in the same way as in formula (1) above, and therefore will not be described here.
[0103] The polymerization solvent that can be used in the preparation of the monomer solution is not particularly limited as long as it can dissolve the alkoxyalkyl (meth)acrylate of the above formula (2) used and the copolymerizable monomer added as necessary. For example, water, methanol, ethanol, propanol, isopropanol, and other alcohols, polyethylene glycols, and other aqueous solvents; toluene, xylene, tetralin, and other aromatic solvents; and chloroform, dichloroethane, chlorobenzene, dichlorobenzene, trichlorobenzene, and other halogenated solvents. Among these, methanol is preferred in consideration of the ease of dissolving the alkoxyalkyl (meth)acrylate and the ease of obtaining a polymer having the above-mentioned weight average molecular weight.
[0104] The monomer concentration in the monomer solution is not particularly limited, but by setting the concentration relatively high, the weight-average molecular weight of the obtained antithrombotic agent can be increased. Therefore, in consideration of the ease of obtaining a polymer having the above-mentioned weight-average molecular weight, the monomer concentration in the monomer solution is preferably less than 50% by mass, more preferably 15% by mass or more and less than 50% by mass. Furthermore, the monomer concentration in the monomer solution is more preferably 20% by mass or more and 48% by mass or less, and particularly preferably 25% by mass or more and 45% by mass or less. Note that, when two or more kinds of monomers are used, the above-mentioned monomer concentration means the total concentration of these monomers.
[0105] The polymerization initiator is not particularly limited, and a known initiator may be used. Preferably, it is a radical polymerization initiator, because it has excellent polymerization stability. Specifically, it is a persulfate such as potassium persulfate (KPS), sodium persulfate, or ammonium persulfate; a peroxide such as hydrogen peroxide, t-butyl peroxide, or methyl ethyl ketone peroxide; azobisisobutyronitrile (AIBN), 2,2'-azobis(4-methoxy-2,4-dimethylvaleronitrile), 2,2'-azobis(2,4-dimethylvaleronitrile), 2,2'-azobis[2-(2-imidazolin-2-yl)propane]dihydrochloride, 2,2'-azobis[2-(2-imidazolin-2-yl)propane]disulfate dihydrate, 2,2'-azobis(2-methylpropionamide), etc. Examples of the azo compounds include azo compounds such as 2,2'-azobis[N-(2-carboxyethyl)-2-methylpropionamidine] dihydrochloride, 2,2'-azobis[N-(2-carboxyethyl)-2-methylpropionamidine] hydrate, 3-hydroxy-1,1-dimethylbutyl peroxyneodecanoate, α-cumyl peroxyneodecanoate, 1,1,3,3-tetrabutyl peroxyneodecanoate, t-butyl peroxyneodecanoate, t-butyl peroxyneoheptanoate, t-butyl peroxypivalate, t-amyl peroxyneodecanoate, t-amyl peroxypivalate, di(2-ethylhexyl) peroxydicarbonate, di(secondary butyl) peroxydicarbonate, and azobiscyanovaleric acid. In addition, the above-mentioned radical polymerization initiator may be used as a redox initiator by combining with a reducing agent such as sodium sulfite, sodium hydrogen sulfite, or ascorbic acid. The amount of the polymerization initiator is preferably 0.0001 to 1 mol % relative to the total amount of the monomers (alkoxyalkyl (meth)acrylate and copolymerizable monomer added as required; the same applies below), more preferably 0.001 to 0.8 mol %, and particularly preferably 0.01 to 0.5 mol %. Alternatively, the amount of the polymerization initiator is preferably 0.005 to 2 parts by mass, more preferably 0.05 to 0.5 parts by mass, relative to 100 parts by mass of the monomer (when multiple types of monomers are used, the total amount). With such an amount of the polymerization initiator, a polymer having a desired weight average molecular weight can be produced more efficiently.
[0106] The polymerization initiator may be mixed with the monomer and the polymerization solvent as it is, or may be mixed with the monomer and the polymerization solvent in the form of a solution in which it is dissolved in another solvent beforehand. In the latter case, the other solvent is not particularly limited as long as it can dissolve the polymerization initiator, and examples thereof include the same solvent as the polymerization solvent. The other solvent may be the same as or different from the polymerization solvent, but is preferably the same solvent as the polymerization solvent in consideration of ease of control of polymerization. The concentration of the polymerization initiator in the other solvent in this case is not particularly limited, but is preferably 0.1 to 10 parts by mass, more preferably 0.15 to 5 parts by mass, and even more preferably 0.2 to 1.8 parts by mass, based on 100 parts by mass of the other solvent, in consideration of ease of mixing.
[0107] Next, the monomer solution is heated to (co)polymerize the alkoxyalkyl (meth)acrylate or the alkoxyalkyl (meth)acrylate and other monomers. Here, the polymerization method may be a known polymerization method such as radical polymerization, anionic polymerization, or cationic polymerization, and preferably radical polymerization is used because it is easy to produce.
[0108] The polymerization conditions are not particularly limited as long as the above-mentioned monomers (alkoxyalkyl (meth)acrylate or alkoxyalkyl (meth)acrylate and copolymerizable monomer) can be polymerized under these conditions. Specifically, the polymerization temperature is preferably 30 to 60°C, and more preferably 40 to 55°C. The polymerization time is preferably 1 to 24 hours, and preferably 3 to 12 hours. Under such conditions, the above-mentioned high molecular weight polymer can be produced more efficiently. Furthermore, gelation in the polymerization step can be effectively suppressed or prevented, and high production efficiency can be achieved.
[0109] If necessary, a chain transfer agent, a polymerization rate regulator, a surfactant, and other additives may be appropriately used during the polymerization.
[0110] The atmosphere in which the polymerization reaction is carried out is not particularly limited, and the polymerization reaction can be carried out in an air atmosphere or an inert gas atmosphere such as nitrogen gas or argon gas, etc. During the polymerization reaction, the reaction liquid may be stirred.
[0111] The polymer after polymerization can be purified by a general purification method such as reprecipitation, dialysis, ultrafiltration, extraction, etc. Among the above, purification by the reprecipitation method is preferred because it gives a (co)polymer suitable for preparation of an aqueous coating liquid. In this case, it is preferred to use ethanol as a poor solvent for reprecipitation.
[0112] The purified polymer can be dried by any method such as freeze-drying, vacuum drying, spray drying, or heat drying. From the viewpoint of having little effect on the physical properties of the polymer, freeze-drying or vacuum drying is preferred.
[0113] As described above, in one embodiment of the present invention, an aqueous coating liquid containing an antithrombotic agent is prepared, and the aqueous coating liquid is applied to the polymer layer formed on the outer surface or inner surface of the hollow fiber membrane in the above (2), thereby forming a coating containing an antithrombotic agent (antithrombotic agent layer) on the polymer layer.
[0114] (Preparation of aqueous coating liquid) Here, a method for preparing the aqueous coating liquid according to the present invention will be described.
[0115] The solvent used for preparing the solution (aqueous coating solution) containing the antithrombotic agent is not particularly limited as long as it can adequately disperse the antithrombotic agent to prepare the aqueous coating solution. From the viewpoint of more effectively preventing the aqueous coating solution from penetrating to the outer or inner surface (the surface on the side where the oxygen-containing gas flows) of the pores of the hollow fiber membrane, it is preferable that the solvent contains water. Here, the water is preferably pure water, ion-exchanged water, or distilled water, and among them, distilled water is preferable.
[0116] In addition, the solvent other than water used in the preparation of the aqueous coating liquid is not particularly limited, but is preferably methanol or acetone in consideration of ease of control of the dispersibility of the antithrombotic agent. The above-mentioned solvent other than water may be used alone or in the form of a mixture of two or more. Among these, methanol is preferable in consideration of ease of further control of the dispersibility of the antithrombotic agent. That is, the solvent is preferably composed of water and methanol. Here, the mixing ratio of water and methanol is not particularly limited, but in consideration of ease of further control of the dispersibility of the antithrombotic agent and the average particle size of the colloid, the mixing ratio (mass ratio) of water:methanol is preferably 6 to 32:1, and more preferably 10 to 25:1. That is, the solvent is preferably composed of water and methanol in a mixing ratio (mass ratio) of 6 to 32:1, and more preferably composed of water and methanol in a mixing ratio (mass ratio) of 10 to 25:1.
[0117] As described above, when preparing an aqueous coating liquid using a mixed solvent of water and a solvent other than water, the order of adding the solvent (e.g., water and methanol) and the antithrombotic agent is not particularly limited, but it is preferable to prepare the aqueous coating liquid by the following procedure. That is, it is preferable to prepare an aqueous coating liquid by adding an antithrombotic agent to a solvent other than water (preferably methanol) to prepare an antithrombotic agent-containing solution, and then adding the antithrombotic agent-containing solution to water. This method makes it easy to disperse the antithrombotic agent. In addition, the above method has the advantage that a colloid with a uniform particle size can be formed, making it easy to form a uniform coating.
[0118] In the above method, the rate at which the antithrombotic agent-containing solution is added to water is not particularly limited, but it is preferable to add the antithrombotic agent-containing solution to water at a rate of 5 to 100 g / min.
[0119] The stirring time and stirring temperature when preparing the aqueous coating liquid are not particularly limited, but from the viewpoint of easily forming a colloid with a uniform particle size and being able to uniformly disperse the colloid, it is preferable to stir for 1 to 30 minutes, more preferably 5 to 15 minutes, after adding the antithrombotic agent-containing solution to water. The stirring temperature is preferably 10 to 40°C, more preferably 20 to 30°C.
[0120] The concentration of the antithrombotic agent in the aqueous coating solution is not particularly limited, but is preferably 0.01% by mass or more from the viewpoint of facilitating an increase in the amount of coating. From the above viewpoint, the aqueous coating solution preferably contains the antithrombotic agent at a concentration of 0.05% by mass or more, and particularly preferably contains the antithrombotic agent at a concentration of 0.1% by mass or more. On the other hand, the upper limit of the concentration of the antithrombotic agent in the aqueous coating solution is not particularly limited, but is preferably 0.3% by mass or less, and more preferably 0.2% by mass or less, in consideration of the ease of forming a coating and the effect of reducing coating unevenness. In addition, within such a range, the decrease in gas exchange capacity due to the coating of the antithrombotic agent becoming too thick is also suppressed.
[0121] (Water-based coating liquid application process) Next, the aqueous coating liquid prepared as above is applied (coated) to the polymer layer formed on the outer or inner surface of the hollow fiber membrane in the above (2). Specifically, after assembling an artificial lung (for example, one with a structure as shown in FIG. 1 or FIG. 3), a polymer layer is formed on the inner or outer surface of the hollow fiber membrane, and the aqueous coating liquid is brought into contact with the polymer layer (or circulated to the side where the polymer layer is formed), thereby coating the polymer layer (preferably the polymer layer formed on the outer surface of the hollow fiber membrane (i.e., the blood contact portion)) with the antithrombotic agent. As a result, an antithrombotic agent layer is formed on the polymer layer. The aqueous coating liquid may be applied to the hollow fiber membrane before assembling the artificial lung.
[0122] The method for contacting the polymer layer with the aqueous coating solution containing the antithrombotic agent is not particularly limited, and any conventionally known method such as filling, dip coating (immersion method), etc. Among these, filling is preferred in order to increase the amount of antithrombotic agent coated.
[0123] When filling is used as a method for contacting the aqueous coating solution containing the antithrombotic agent with the polymer layer, the amount of the aqueous coating solution filled is determined based on the membrane area (m 2 ) for 50g / m 2 More preferably, 80 g / m 2 It is preferable that the amount is such that the loading amount is 50 g / m or more. 2 When the amount is more than 100, a coating (antithrombotic agent layer) containing a sufficient amount of antithrombotic agent can be formed on the surface of the hollow fiber membrane. On the other hand, the upper limit of the amount of the antithrombotic agent is not particularly limited, but it is preferable that the amount of the antithrombotic agent is less than 100, and the membrane area (m 2 ) for 200g / m 2 Less than 150 g / m 2 It is preferable that the amount is as follows:
[0124] In this specification, the term "membrane area" refers to the area of the outer surface of a hollow fiber membrane, and is calculated from the product of the outer diameter, pi, number, and effective length of the hollow fiber membrane.
[0125] The time for contacting the polymer layer with the aqueous coating liquid containing the antithrombotic agent is not particularly limited, but is preferably 0.5 to 70 minutes, more preferably 1 to 5 minutes, in consideration of the amount of coating, ease of forming a coating film, effect of reducing coating unevenness, etc. The contact temperature between the aqueous coating liquid and the polymer layer (flow temperature of the aqueous coating liquid) is preferably 5 to 40°C, more preferably 15 to 30°C, in consideration of the amount of coating, ease of forming a coating film, effect of reducing coating unevenness, etc.
[0126] After contact with the aqueous coating liquid, the coating film is dried to form a coating (antithrombogenic agent layer) of the antithrombogenic agent according to the present invention on the polymer layer. Here, the drying conditions are not particularly limited as long as the coating (antithrombogenic agent layer) of the antithrombogenic agent can be formed on the polymer layer. Specifically, the drying temperature is preferably 5 to 50°C, more preferably 15 to 40°C. The drying time is preferably 60 to 300 minutes, more preferably 120 to 240 minutes. Alternatively, the coating film may be dried by continuously or stepwise circulating a gas at preferably 5 to 40°C, more preferably 15 to 30°C, through the hollow fiber membrane. Here, the type of gas is not particularly limited as long as it has no effect on the coating film and can dry the coating film. Specifically, air, and inert gases such as nitrogen gas and argon gas can be mentioned. The amount of gas circulated is not particularly limited as long as it can sufficiently dry the coating film, but is preferably 5 to 150L, more preferably 30 to 100L.
[0127] The above steps provide an artificial lung in which a polymer layer and an antithrombogenic agent layer are formed on the inner or outer surface of the hollow fiber membrane. Thus, the manufacturing method according to this embodiment can provide an artificial lung having both the desired antithrombogenicity and plasma leakage resistance. Furthermore, the artificial lung manufactured by the method according to this embodiment can maintain its antithrombogenicity and plasma leakage resistance even when used for a long period of time, for example, more than one month (i.e., it is also excellent in durability (maintenance of antithrombogenicity and plasma leakage resistance)). Therefore, the artificial lung manufactured by the method according to this embodiment can be suitably used as a lung assisting device for patients with serious diseases, in addition to being used as an artificial lung for normal surgery, etc. EXAMPLES
[0128] The effects of the present invention will be described using the following examples. However, the technical scope of the present invention is not limited to the following examples. In the following examples, unless otherwise specified, the operations were performed at room temperature (25°C). Furthermore, unless otherwise specified, "%" and "parts" mean "% by mass" and "parts by mass", respectively.
[0129] Examples 1 to 4 Dopamine hydrochloride (Sigma-Aldrich Japan LLC) was added to a PBS solution (composition: 8 g / L NaCl, 0.2 g / L KCl, 1.15 g / L Na2HPO4, 0.2 g / L KH2PO4, pH 7.4) to a concentration of 2 mg / mL. This mixed solution was placed in a sealed container, and oxygen gas was sealed in to make the oxygen concentration (25°C) 1.12 vol% to prepare DA / PBS solution 1 (pH 7.4).
[0130] A polypropylene porous hollow fiber membrane 51 (outer diameter: 170 μm, inner diameter: 112 μm, thickness: 29 μm, pore size: 0.05 μm, porosity: 30 vol%, membrane area: 0.05 m 2 ) was immersed in the DA / PBS solution 1 prepared above. Next, one end of the hollow fiber membrane was potted in a polyvinyl chloride tube using urethane resin, and connected to an oxygen gas tank using an air hose and a joint. Oxygen gas was blown from the oxygen gas tank into the lumen of the hollow fiber membrane at a rate of 0.3 L / min for 240 minutes (Example 1), 120 minutes (Example 2), 60 minutes (Example 3), and 30 minutes (Example 4), and then the membrane was held in this state at 37°C for 1 hour. As a result, dopamine was oxidized and polymerized to form a dopamine polymer layer (polymer layer) on the surface of the hollow fiber membrane (holding hollow fiber membranes 1 to 4). Note that the above operations were performed at 25°C except for holding at 37°C for 1 hour. Holding hollow fiber membranes 1 to 4 were taken out of DA / PBS solution 1, washed with RO water, and naturally dried at room temperature (25°C) to obtain coated hollow fiber membranes 1 to 4.
[0131] In addition, a certain amount of DA / PBS solution 1 was taken out after removing the retaining hollow fiber membranes 1 to 4, and the absorbance of the solution was measured at a measurement wavelength (200 to 800 nm) using ultraviolet-visible spectroscopy (UV-vis). The results are shown in Figure 8. In Figure 8, the high absorbance (abs.) at 450 nm is an index of the degree of polymerization of dopamine in the solution, and suggests that the polymerization of dopamine is promoted by blowing oxygen (i.e., dopamine is also polymerized on the surface of the hollow fiber membrane, forming a dopamine layer more quickly than when it is retained in the air).
[0132] Comparative Example 1 Comparative coated hollow fiber membrane 1 was produced in the same manner as in Examples 1 to 4, except that oxygen gas was not blown in (that is, oxygen gas blowing time=0 min).
[0133] That is, in the same manner as in Examples 1 to 4, DA / PBS solution 1 (pH 7.4) was prepared.
[0134] Polypropylene porous hollow fiber membrane (outer diameter: 170 μm, inner diameter: 112 μm, thickness: 29 μm, pore size: 0.05 μm, porosity: 30 vol%, membrane area: 0.05 m 2 ) was immersed in the DA / PBS solution 1 prepared above to fill the lumen of the hollow fiber membrane with DA / PBS solution 1, and in this state, it was kept at 37°C for 1 hour. As a result, dopamine was oxidized and polymerized to form a dopamine polymer layer (polymer layer) on the surface of the hollow fiber membrane (comparative retained hollow fiber membrane 1). Furthermore, the comparative retained hollow fiber membrane 1 was taken out of the DA / PBS solution 1, washed with RO water, and naturally dried at room temperature (25°C) to obtain a comparative coated hollow fiber membrane 1.
[0135] After the comparative retaining hollow fiber membrane 1 was removed, the amount of dopamine in the DA / PBS solution 1 was measured in the same manner as in Examples 1 to 4. The results are shown in FIG.
[0136] Comparative Example 2 Dopamine hydrochloride (Sigma-Aldrich Japan, LLC) was added to a PBS solution (composition: 8 g / L NaCl, 0.2 g / L KCl, 1.15 g / L Na2HPO4, 0.2 g / L KH2PO4, pH 7.4) to a concentration of 2 mg / mL to prepare DA / PBS solution 2 (pH 7.4).
[0137] Polypropylene porous hollow fiber membrane (outer diameter: 170 μm, inner diameter: 112 μm, thickness: 29 μm, pore size: 0.05 μm, porosity: 30 vol%, membrane area: 0.05 m 2) was immersed in the DA / PBS solution 2 prepared above for 24 hours, filling the lumen of the hollow fiber membrane with the DA / PBS solution, and the dopamine was oxidized and polymerized to form a dopamine polymer layer (polymer layer) on the surface of the hollow fiber membrane, thereby obtaining a comparative coated hollow fiber membrane 2.
[0138] After the comparative retaining hollow fiber membrane 2 was removed, the amount of dopamine in the DA / PBS solution 2 was measured in the same manner as in Examples 1 to 4. The results are shown in FIG.
[0139] 8, it can be seen that by carrying out the oxidation and polymerization of dopamine while blowing in oxygen gas as in the present embodiment, the polymerization of dopamine proceeds more efficiently than in Comparative Example 1 in which oxygen gas was not blown in. Therefore, it is considered that when an antithrombotic agent layer containing an antithrombotic agent is formed on the dopamine polymer layer formed in the present embodiment, the antithrombotic agent layer adheres more closely to the dopamine polymer layer than the dopamine polymer layer in the Comparative Example (hence, the artificial lung can exhibit higher durability).
[0140] Moreover, a comparison between FIG. 8 and FIG. 9 reveals that according to the embodiment, a dopamine polymer layer can be formed in a shorter time to an equal or greater extent.
[0141] Comparative Example 3 Polypropylene porous hollow fiber membrane (outer diameter: 170 μm, inner diameter: 112 μm, thickness: 29 μm, pore size: 0.05 μm, porosity: 30 vol%, membrane area: 0.05 m 2 ) was prepared as an uncoated hollow fiber membrane.
[0142] <Evaluation> The gas permeability and plasma leakage resistance of the coated hollow fiber membrane 3 obtained in Example 3, the comparative coated hollow fiber membrane 1 obtained in Comparative Example 1, and the uncoated hollow fiber membrane were evaluated.
[0143] [Gas permeability] The coated hollow fiber membrane was potted with epoxy resin, and the outside of the hollow fiber membrane was filled with oxygen gas. A pressure of 50 mmHg was applied to the gas, and the amount of gas flowing from the outside of the hollow fiber membrane to the lumen was measured to evaluate the gas permeability. The gas permeability was also evaluated in the same manner for the comparative coated hollow fiber membrane 1 and the uncoated hollow fiber membrane. The results are shown in Figure 10. In Figure 10, the vertical axis indicates the gas flow rate (mL / m) per unit (area·time). 2 The higher the value on the vertical axis, the better the gas permeability.
[0144] As shown in FIG. 10, the coated hollow fiber membrane 3 has a lower gas permeability than the uncoated hollow fiber membrane ("uncoated" in FIG. 10) and the comparative coated hollow fiber membrane 1, but it still has the gas permeability (1.0 mL / m 2 It was confirmed that the blood flow to the splendid splenic area was adequately protected (≥ 100 m / s·min·mmHg).
[0145] [Plasma leak resistance] The coated hollow fiber membrane was potted with epoxy resin, and the outside of the hollow fiber membrane was filled with a solution (SDS / saline solution) in which sodium dodecyl sulfate (SDS) was dissolved in a 0.9 w / v% aqueous sodium chloride solution (saline solution) to a concentration of 1 mg / mL. A pressure of 760 mmHg was applied to the SDS / saline solution, and the amount of SDS / saline solution permeating from the outside of the hollow fiber membrane to the lumen was measured to evaluate the plasma leakage resistance. In addition, the plasma leakage resistance of the comparative coated hollow fiber membrane 1 and the uncoated hollow fiber membrane were evaluated in the same manner. The results are shown in Figure 11. Figure 11 is a graph in which the vertical axis represents the amount of SDS / saline solution permeated per unit (area·time) and the horizontal axis represents time. The smaller the value on the vertical axis, the better the plasma leakage resistance.
[0146] As shown in FIG. 11, the coated hollow fiber membrane 3 was shown to have significantly improved plasma leakage resistance compared to the uncoated hollow fiber membrane ("Uncoated" in FIG. 11) and the comparative coated hollow fiber membrane 1.
[0147] This application is based on Japanese Patent Application No. 2020-043497, filed on March 12, 2020, the disclosure of which is hereby incorporated by reference in its entirety. [Explanation of symbols]
[0148] 1, 20 Hollow fiber membrane external blood perfusion oxygenator, 2, 23 Housing, 3, 50 Porous hollow fiber membrane for gas exchange, 3a outer layer, 3a' outer surface, 3b inner layer, 3c inner layer, 3c' inner surface, 3D passage (lumen), 3e Opening on the outer surface side, 3f Opening on the inner surface side, 4,5 bulkhead, 6, 17a, 28 blood inlet; 7, 29a, 29b blood outlet; 8,24 Gas inlet, 9,27 Gas outlet, 10 Gas inlet header, 11 Gas outlet header, 12, 17 blood chamber, 13 Gas inlet chamber, 14 Gas escape chamber, 16 polymer layer, 17b First blood chamber, 17c First Blood Chamber, 18 Antithrombotic layer, 22 tubular hollow fiber membrane bundle, 25 First bulkhead, 26 Second bulkhead, 31 inner tubular member, 32 Blood circulation opening; 33 outer tubular member, 35 Inner cylinder, 35a top end; 41 Gas inlet member, 42 Gas outlet parts.
Claims
1. A method for producing an oxygenator having a plurality of porous hollow fiber membranes for gas exchange, at least a portion of which is made of polypropylene, comprising: The hollow fiber membrane has an inner surface forming a lumen and an outer surface, A coating liquid containing at least one compound selected from the group consisting of dopamine and its salts and oligomers is prepared; contacting the outer surface of the hollow fiber membrane with the coating liquid for less than 10 hours while blowing oxygen gas into the coating liquid, thereby forming a polymer layer containing a polymer of the compound on the outer surface, and forming an antithrombotic agent layer having an antithrombotic agent on the polymer layer.
2. The method of claim 1 , wherein the compound is dopamine or a dopamine salt.
3. The antithrombotic agent has the following formula (1): 【Chemistry 1】 However, R 1 represents an alkylene group having 1 to 4 carbon atoms; R 2 represents an alkyl group having 1 to 4 carbon atoms; and R 3 represents a hydrogen atom or a methyl group; The method according to claim 1 or 2, wherein the structural unit (1) is represented by the following formula:
Citation Information
Patent Citations
Modification method for preparing high-hydrophilic coating by dopamine-induced sol-gel process
CN104150787A
Preparation method of super hydrophobic and oleophobic film for dual-bionic film with photothermal effects
CN108722200A
Preparation method of Janus composite membrane