Method for manufacturing master mold for imprint
The method of controlling resist exposure through masks with specific light patterns allows for the precise formation of master molds with forward tapered shapes, addressing the challenge of complex taper angle control and ensuring accurate pattern transfer in imprinting processes.
Patent Information
- Application Number
- PCT/JP2023/016284
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-24
- Filing Date
- 2023-04-25
- Publication Date
- 2024-10-03
AI Technical Summary
Current methods for producing master molds for imprinting struggle to easily control the taper angle of the side surface shape, requiring complex and time-consuming processes, which can lead to deformation and improper pattern transfer during replica mold formation.
A method involving the use of a resist coated on a base material, exposed to light through a mask with controlled exposure amounts and mask types (binary or grayscale) to achieve a forward tapered shape with optimal taper angles, ensuring accurate pattern transfer and reducing deformation risks.
Enables the easy formation of master molds with precise taper angles, improving the yield and smoothness of replica mold production by preventing inverted tapered shapes during polymerization and pressurization, thus ensuring reliable pattern transfer.
Smart Images

Figure JP2023016284_03102024_PF_FP_ABST
Abstract
Description
Method for making an imprint master mold
[0001] The present invention relates to a method for producing an imprint master mold.
[0002] The present applicant has proposed a technique disclosed in Japanese Patent Application Laid-Open No. 2003-229999 (hereinafter referred to as "the prior art") regarding a wiring formation method using an imprint method.
[0003] As shown in Figure 13, this conventional technology involves filling a conductive paste 22 into the recesses 21 of a replica mold 20, which has recesses 21 formed in a pattern similar to the wiring pattern or bump pattern to be formed on a substrate 10, and then overlapping the replica mold 20 with the recesses 21 filled with the conductive paste 22 on the substrate 10 and applying pressure (pressure welding) to transfer the conductive paste 22 in the recesses 21 of the replica mold 20 to the substrate 10, thereby forming wiring 11 and bumps of a predetermined pattern on the substrate 10.
[0004] Incidentally, the replica mold 20 used in this prior art is produced using a master mold 30 (original plate) having structures (protrusions) that represent a wiring pattern or a bump pattern on a substrate, as shown in Figure 14. The structure of this master mold 30 is formed by etching the substrate 31 itself (see Figure 14(a)), or by patterning a resist 32 applied to the substrate 31 (see Figure 14(b)).
[0005] When the structure of this master mold is formed from a resist, the resist is conventionally exposed to a sufficient amount of light, so that the side shape of the structure is almost perpendicular to the substrate.
[0006] However, if the side shape of the structure is nearly perpendicular to the substrate, the structure of the master mold may temporarily deform into an inverted tapered shape during polymerization and pressure application to form the replica mold, which may prevent proper transfer.
[0007] Therefore, in order to produce replica molds smoothly and with a high yield, it is preferable that the side shape of the master mold structure relative to the base material be a forward tapered shape; however, the shape of the master mold structure is directly reflected in the shape of the recesses in the replica mold, and further, the shape of the recesses in the replica mold is directly reflected in the shapes of the wiring and bumps formed on the substrate; for example, if the taper angle is too large, it will hinder miniaturization and high aspect ratios. Therefore, rather than simply giving the shape a tapered shape, it is necessary to form a forward tapered shape with an appropriate taper angle that takes into account the size, pitch, aspect ratio, etc. of the desired pattern.
[0008] Japanese Patent Application Laid-Open No. 2021-111668
[0009] However, to date, no method has been established for easily controlling the taper angle of the side surface shape of the master mold structure, and currently, in order to make the side surface shape of the master mold structure a forward tapered shape with a desired taper angle, many complicated operations are required, which is labor-intensive and costly.
[0010] The present invention has been made in view of the above-described current situation, and has an object to provide a method for producing an imprint master mold that can easily form, on a substrate, a structure formed in a forward tapered shape with an optimal taper angle taking into consideration the size, pitch, aspect, etc. of the target pattern.
[0011] The gist of the present invention will be explained with reference to the accompanying drawings.
[0012] The method for producing an imprint master mold has structures 2 formed on a substrate 1 in a predetermined pattern such as a wiring pattern or a bump pattern, and includes the steps of: a coating step of coating a resist 3 of a predetermined thickness on the substrate 1; an exposure step of exposing the resist 3 coated on the substrate 1 to light through a mask 4; and a development step of developing the exposed resist 3, wherein the exposure step exposes predetermined portions of the resist 3 by setting the exposure amount to an exposure amount not greater than twice the following Df, so that the side surfaces of the structures 2 formed by the resist 3 through development in the development step have a forward tapered shape, where Df is the minimum exposure amount at which the entire thickness of the resist 3 coated on the substrate 1 is exposed.
[0013] The present invention also relates to a method for producing an imprint master mold according to claim 1, characterized in that in the exposure step, a binary mask consisting of light-transmitting portions 4a and light-shielding portions 4b is used as the mask 4, and the exposure dose is set to D0 to Df as follows: D0: exposure dose at which the resist 3 applied on the substrate 1 begins to be exposed to light.
[0014] The present invention also relates to a method for producing an imprint master mold as set forth in claim 1, characterized in that in the exposure step, a grayscale mask consisting of a light-transmitting portion 4a, a light-shielding portion 4b, and a grayscale portion 4c is used as the mask 4.
[0015] The present invention also relates to a method for producing an imprinting master mold according to a third aspect, wherein the gray scale portion 4 c is provided along an edge of an opening of the light-transmitting portion 4 a.
[0016] The present invention also relates to a method for producing an imprint master mold according to any one of claims 1 to 4, wherein the exposure dose is determined based on data relating to the relationship between the exposure dose for a predetermined thickness of the resist 3, which is determined in advance, and the taper angle of the forward taper.
[0017] The present invention also relates to a method for producing an imprint master mold according to any one of claims 1 to 4, wherein the substrate 1 is a light-transmitting material, the resist 3 is a negative resist 3, and the method further comprises a mask formation step of forming the mask 4 on the surface of the substrate 1, and the exposure step involves irradiating the back surface of the substrate 1 with light to expose the resist 3 via the mask 4 formed on the surface of the substrate 1.
[0018] The present invention also relates to a method for producing an imprint master mold as set forth in claim 5, wherein the substrate 1 is a light-transmitting material, the resist 3 is a negative resist 3, and the method further comprises a mask formation step of forming the mask 4 on the surface of the substrate 1, and the exposure step involves irradiating the back surface of the substrate 1 with light and exposing the resist 3 via the mask 4 formed on the surface of the substrate 1.
[0019] As described above, the present invention provides a method for producing an imprint master mold that can easily form, on a substrate, a structure made of resist formed in a forward tapered shape with an optimal taper angle taking into consideration the size, pitch, aspect, etc. of the target pattern.
[0020] FIG. 1 is a schematic explanatory diagram of an example of forming a structure in the present invention. FIG. 2 is an explanatory diagram of the photosensitivity characteristics of a resist in Example 1. FIG. 3 is an explanatory diagram of the process flow in Example 1. FIG. 4 is a graph showing the photosensitivity characteristics of a resist (SU-8) in Example 1. FIG. 5 is an SEM image of a structure exposed at different exposure doses at a predetermined film thickness when using a negative resist in Example 1. FIG. 6 is an SEM image of a structure exposed at different exposure doses at a predetermined film thickness when using a positive resist in Example 1. FIG. 7 is an explanatory diagram of the process flow in Example 2. FIG. 8 is a schematic diagram showing a mask (grayscale mask) when using a negative resist in Example 2. FIG. 9 is an explanatory diagram (explanation of the principle) showing the light intensity distribution during exposure when using a grayscale mask in Example 2. FIG. 10 is an explanatory diagram (actual distribution) showing the light intensity distribution during exposure when using a binary mask in Example 2. FIG. 11 is a schematic diagram showing a mask (grayscale mask) when using a positive resist in Example 2. 1A and 1B are schematic cross-sectional views showing a wiring formation method using a replica mold in a conventional example, a method for producing a master mold in a conventional example, and a method for producing a replica mold using the master mold in a conventional example.
[0021] A preferred embodiment of the present invention will be briefly described below, illustrating the operation of the present invention with reference to the drawings.
[0022] A resist 3 is applied onto a substrate 1, the resist 3 applied onto the substrate 1 is exposed through a mask 4, and the exposed resist 3 is developed to form a structure 2 made up of the resist 3.
[0023] In the present invention, in the above-described operation, the exposure dose when exposing the resist 3 is set to be equal to or less than twice Df (the minimum exposure dose at which the entire thickness of the resist 3 applied on the substrate 1 is exposed). Therefore, as shown in FIG. 1( a), the resist 3 near the edge (end) of the light-transmitting portion 4 a (opening) of the mask 4 is exposed under conditions (exposure dose smaller than Df) in which the amount of light attenuates in the film thickness direction of the resist 3. This makes it possible to easily form a structure 2 whose side shape is a forward tapered shape relative to the substrate 1 as shown in FIG. 1( b).
[0024] That is, for example, when the resist 3 is exposed through the mask 4, the amount of light near the edges of the light-transmitting portions 4 a of the mask 4 is weaker than that at the center due to the phenomenon of light diffraction, and this causes a phenomenon in which the photosensitivity decreases in the film thickness direction of the resist 3 near the edges of the light-transmitting portions 4 a of the mask 4. Therefore, by setting the exposure amount to be equal to or less than twice the minimum exposure amount (Df) at which the entire thickness of the resist 3 applied on the substrate 1 is exposed, as shown in Figure 2, the exposure amount decreases toward the edge near the edges of the light-transmitting portions 4 a of the mask 4, and accordingly the photosensitivity in the film thickness direction of the resist 3 also decreases toward the edge, making it possible to obtain a structure 2 having a forward tapered shape.
[0025] Furthermore, for example, by using a grayscale mask having grayscale portions 4c at the edges of the light-transmitting portions 4a of the mask 4, in addition to the above-mentioned light diffraction phenomenon, the exposure amount can be spatially changed by the action of the grayscale portions 4c, making it possible to obtain a structure 2 with a forward tapered shape having a larger taper angle.
[0026] A specific embodiment 1 of the present invention will be described with reference to FIGS. 1 to 6. FIG.
[0027] This example is a method for producing an imprint master mold having structures 2 formed in a predetermined pattern such as a wiring pattern or a bump pattern on a substrate 1.
[0028] Specifically, it includes a mask formation process for forming a mask 4 on a substrate 1, a coating process for coating the resist 3 on the mask 4, an exposure process for exposing the resist 3 coated on the mask 4 through the mask 4, and a development process for developing the exposed resist 3.
[0029] That is, in this embodiment, a photomask is not used in the exposure process, but a resist 3 is formed in a predetermined pattern through a mask 4 formed on a substrate 1, and a structure 2 composed of the resist 3 is formed.
[0030] In this example, a thick-film negative resist 3 is used as the resist 3. When this negative resist 3 is used, if light is irradiated from the surface side of the resist 3 during exposure, the structures 2 will have an inverse tapered shape relative to the substrate 1, and therefore the light is irradiated from the substrate 1 side. Therefore, a light-transmitting material is used for the substrate 1.
[0031] Specifically, in this example, SU-8 manufactured by Nippon Kayaku Co., Ltd. is used as the resist 3, and the substrate 1 is made of glass.
[0032] Hereinafter, each step in the method for producing an imprint master mold of this example using the above-mentioned substrate 1 and resist 3 will be described in detail.
[0033] First, in the mask forming step, a mask 4 having a predetermined pattern is formed on a glass substrate 1 .
[0034] Specifically, a mask film 5 for forming the mask 4 is formed on the substrate 1, and the mask film 5 is etched into a predetermined pattern. In this example, Cr is sputtered onto the substrate 1 as the mask film 5 (see FIG. 3(b)), and a resist (in this example, a positive resist OFPR manufactured by Tokyo Ohka Kogyo Co., Ltd.) is applied to the Cr film 5. After exposure and development through a predetermined photomask, the Cr film 5 is etched through the resist (see FIG. 3(c)). After the etching, the resist is removed to form a binary mask consisting of light-transmitting portions 4a (openings) and light-shielding portions 4b (see FIG. 3(d)).
[0035] The thickness of the mask film 5 may be any thickness that can exhibit light-shielding properties during exposure in the exposure step (in this embodiment, it is set to 60 nm to 120 nm (adjustable depending on the exposure conditions)).
[0036] Furthermore, the mask film 5 is not limited to Cr, and any other material that can achieve the same effects as those of this embodiment can be used.
[0037] Subsequently, in the coating step, a resist 3 for forming the structures 2, in other words, a resist 3 that will become the structures 2, is coated on the substrate 1.
[0038] Specifically, a resist 3 (SU-8) having a predetermined thickness is applied onto a mask 4 formed on a substrate 1 (see FIG. 3(e)).
[0039] The resist 3 for forming the structure 2 is not limited to the above.
[0040] Subsequently, in the exposure step, the resist 3 is exposed to light.
[0041] Specifically, light is irradiated from the rear side of the glass substrate 1, and the resist 3 is exposed through a mask 4 provided between the glass substrate 1 and the resist 3 (see FIG. 3(f)).
[0042] The exposure dose is set to be equal to or less than twice the Df below, preferably D0 to Df below, so that the side shape of the structure 2 formed by development relative to the substrate 1 is forward tapered. Note: D0: exposure dose at which the resist 3 applied on the substrate 1 begins to be exposed; Df: minimum exposure dose at which the entire thickness of the resist 3 applied on the substrate 1 is exposed.
[0043] More specifically, the exposure amount is set to within the above range according to the target taper angle based on the relationship data between the exposure amount at a predetermined thickness of the resist 3 and the taper angle of the forward taper, which is previously determined.
[0044] D0 and Df can be determined, for example, from a data sheet disclosed by a manufacturer. In this example, D0 and Df are determined from the data sheet for SU-8 from Kayaku Advanced Materials, Inc. (https: / / kayakuam.com / wp-content / uploads / 2020 / 09 / KAM-SU-8-2-25-Datasheet-9.3.20-final.pdf) shown in FIG.
[0045] In this embodiment, based on the determined D0 and Df, relationship data between the exposure dose at a predetermined film thickness of the resist 3 and the taper angle of the forward taper is obtained through experiments, and based on this relationship data, the exposure dose is set according to the target taper angle.
[0046] Specifically, in this example, a TEG pattern having bump patterns with different diameters and wiring patterns with different line widths was used, and samples were prepared by exposing the samples to different exposure doses at a predetermined film thickness, as shown in FIG. 5 , and the taper angle was determined from SEM images of the bump pattern and wiring pattern (FIG. 5 shows the bump pattern) in these samples, thereby obtaining data on the relationship between the exposure dose at a predetermined film thickness and the taper angle of the forward taper.
[0047] For example, from FIG. 5, it is possible to obtain data on the relationship between the exposure dose and the taper angle, as shown in Table 1 below, and the exposure dose can be set based on this data (taper angle), or a calculation formula for determining the exposure dose can be created and used to set the exposure dose.
[0048]
[0049] Finally, in the development step, the exposed resist 3 is developed.
[0050] In this example, a negative resist 3 is used, so that the resist 3 remains in the exposed portion, and this remaining resist 3 forms a structure 2 whose side surface has a desired tapered shape (taper angle), thereby completing the master mold (see FIG. 3(g)).
[0051] As described above, this embodiment uses a negative resist 3, but a positive resist 3 may also be used.
[0052] When a positive resist 3 is used, the mask forming step is not necessary, and a photomask is used in the exposure step.
[0053] In contrast to the negative resist 3, the positive resist 3 has no exposed portion, so that in the exposure step, the resist 3 is exposed from the surface side, and the remaining resist 3 becomes the structure 2, as shown in FIG.
[0054] FIG. 6 shows the shape of the structure 2 in a sample exposed to various exposure doses at a predetermined film thickness using PMER P-LA900 manufactured by Tokyo Ohka Kogyo Co., Ltd. as the resist 3 and the same TEG pattern as in the case of the negative resist 3.
[0055] As shown in FIG. 6, in the case of the positive resist 3, it can be confirmed that the taper angle of the structure 2 changes when the exposure dose is changed, just like in the case of the negative resist 3. The taper angle can be determined from SEM images of the bump pattern or wiring pattern of this sample, and data on the relationship between the exposure dose at a specified film thickness and the taper angle of the forward taper can be obtained.
[0056] As described above, this example provides a method for producing an imprint master mold that can easily form, on a substrate 1, structures 2 formed in a forward tapered shape with an optimal taper angle taking into consideration the size, pitch, aspect, etc. of the target pattern.
[0057] That is, in this embodiment, the exposure dose of the resist 3 forming the structure 2 is set to D0 (the exposure dose at which the resist 3 applied on the substrate 1 begins to be exposed to light) to Df (the minimum exposure dose at which the entire thickness of the resist 3 applied on the substrate 1 is exposed to light), so that the exposure dose decreases near the edge of the light-transmitting portion 4a of the mask 4 toward the edge, and accordingly the photosensitivity of the resist 3 in the film thickness direction also decreases toward the edge, making it possible to reliably form a structure 2 whose side surface has a forward tapered shape.
[0058] Therefore, even if the structure of the master mold is deformed during polymerization and pressure application to form the replica mold, the occurrence of an inverse tapered shape is prevented, and a master mold can be produced that allows pattern transfer to be performed smoothly and with high yield.
[0059] A specific second embodiment of the present invention will be described with reference to FIGS.
[0060] In this embodiment, a mask 4 different from that in the first embodiment is used.
[0061] Specifically, in this embodiment, a grayscale mask is used as the mask 4, and this grayscale mask is made up of a light-transmitting portion 4a, a light-shielding portion 4b, and a grayscale portion 4c.
[0062] This embodiment will be described in detail below, but the process flow of this embodiment is the same as that of the first embodiment except for the mask formation process, so a description of the processes other than the mask formation process will be omitted.
[0063] When a grayscale mask is used as the mask 4 as in this embodiment, there is no limit to the exposure amount, but it is desirable to use the exposure conditions in the exposure step of embodiment 1, that is, an exposure amount of not more than twice Df.
[0064] In the mask forming process of this embodiment, first, a light-shielding film 5a for forming the light-shielding portions 4b of the mask 4 is formed on the substrate 1, and then the light-shielding film 5a is etched into a predetermined pattern. In this embodiment, as in Example 1, Cr is formed on the substrate 1 by sputtering as the light-shielding film 5a (see FIG. 7(b)), and a resist 6 (in this embodiment, a positive resist OFPR manufactured by Tokyo Ohka Kogyo Co., Ltd.) is applied to the Cr film 5a. After exposure and development through a predetermined photomask, the Cr film 5a is etched through the resist 6 (see FIG. 7(c)). After the etching, the resist 6 is removed to form the light-shielding portions 4b made of the Cr film 5a on the substrate 1 (see FIG. 7(d)).
[0065] Next, a grayscale film 5b for forming the grayscale portion 4c of the mask 4 is formed on the substrate 1 including the light-shielding portion 4b, and the grayscale film 5b is etched to form a predetermined pattern. In this embodiment, the grayscale film 5b is made of CrO 3 was formed on the substrate 1 including the light-shielding portion 4b by sputtering (see FIG. 7(e)). 3 Resist 6 (in this example, a positive resist OFPR manufactured by Tokyo Ohka Kogyo Co., Ltd.) is applied onto the film 5b, and after exposure and development through a predetermined photomask (see FIG. 7(f)), CrO 3 The film 5b is etched (see FIG. 7(g)), and after the etching, the resist 6 is removed to form the light-transmitting portions 4a and the grayscale portions 4c on the substrate 1 (see FIG. 7(h)), thereby forming a grayscale mask on the substrate 1, which is composed of the light-transmitting portions 4a, the light-shielding portions 4b, and the grayscale portions 4c.
[0066] In this embodiment, in order to improve the adhesiveness of the resist 3, an adhesive film 5c (SiO 2 A film) is formed (see FIG. 7(i)).
[0067] Fig. 8 shows an example of the configuration of the mask 4 (grayscale mask) for the bump pattern formed as described above. As shown in Fig. 8, the mask 4 of this embodiment has grayscale portions 4c that are provided at the boundaries between the light-transmitting portions 4a and the light-shielding portions 4b and along the periphery of the light-transmitting portions 4a. The amount of exposure light passing through these grayscale portions 4c reduces, and the photosensitivity of the resist 3 in the film thickness direction also decreases. Due to the interaction with the diffraction effect of light, it is possible to easily form structures 2 that have a forward tapered shape with a larger taper angle than when a binary mask is used (see Figs. 7(k) and (j)).
[0068] The exposure mechanism when a grayscale mask is used will be described below.
[0069] FIG. 9 shows the intensity distribution (upper part) derived based on the Fresnel diffraction of light that has passed through the light-transmitting portion 4 a and the intensity distribution (lower part) derived based on the Fresnel diffraction of light that has passed through the grayscale portion 4 c in the grayscale mask of this embodiment.
[0070] In the configuration of the grayscale portion 4c as shown in FIG. 9, the grayscale portion 4c is located within the range where Fresnel diffraction occurs, and therefore it is possible to superimpose (combine) the intensity distribution derived based on the Fresnel diffraction of light that has passed through the light-transmitting portion 4a and the intensity distribution derived based on the Fresnel diffraction of light that has passed through the grayscale portion 4c. As a result, the grayscale mask of this embodiment results in a light intensity distribution as shown in FIG. 10.
[0071] The light intensity distribution when the grayscale mask shown in Fig. 10 is used corresponds to a light intensity distribution shifted toward the light-shielding portion 4b (to the left in the figure) by the area (width) of the grayscale portion 4c relative to the light intensity distribution when the binary mask shown in Fig. 11 is used. Therefore, by using the grayscale mask, the amount of recession of the side surface of the structure 2 increases by the amount of the grayscale portion 4c, and accordingly the taper angle of the side surface of the structure 2 also increases.
[0072] Table 2 below shows the results of measuring the side taper angle of a structure 2 with a bump diameter of 10 μm when a 40 μm-thick resist 3 was exposed using a binary mask and when it was exposed using a grayscale mask. The grayscale mask used had a region (width) of the grayscale portion 4c of 1.5 μm.
[0073]
[0074] The results shown in Table 2 also confirm that the use of a grayscale mask makes it possible to increase the taper angle of the side surface of the structure 2.
[0075] As described above, this embodiment uses a negative resist 3, but a positive resist 3 (for example, PMER P-LA900 manufactured by Tokyo Ohka Kogyo Co., Ltd.) may also be used.
[0076] When a positive resist 3 is used, the mask forming step is not necessary, and a photomask is used in the exposure step.
[0077] A suitable photomask is one having a mask configuration as shown in FIG. 12 (in the figure, reference numeral 4a denotes a light-transmitting portion, 4b denotes a light-shielding portion, and 4c denotes a grayscale portion).
[0078] The present invention is not limited to the present embodiment, and the specific configuration of each component can be designed as appropriate.
Claims
1. A method for producing a master mold for imprinting having a structure formed on a substrate in a predetermined pattern such as a wiring pattern or a bump pattern, comprising a coating step of coating a resist of a predetermined thickness on the substrate, an exposure step of exposing the resist coated on the substrate through a mask, and a development step of developing the exposed resist, characterized in that the exposure step exposes a predetermined portion of the resist by setting the exposure amount to an exposure amount not greater than twice the following Df so that the side shape of the structure formed by the resist formed by development in the development step has a forward taper. Df: minimum exposure amount at which the entire thickness of the resist coated on the substrate is exposed.
2. A method for producing a master mold for imprinting according to claim 1, characterized in that in the exposure step, a binary mask consisting of a light-transmitting portion and a light-shielding portion is used as the mask, and the exposure dose is set to D0 to Df as follows: D0: Exposure dose at which the resist applied to the substrate begins to be exposed to light 3. A method for producing an imprinting master mold according to claim 1, characterized in that in the exposure step, a grayscale mask consisting of a light-transmitting portion, a light-shielding portion and a grayscale portion is used as the mask.
4. A method for producing a master mold for imprinting according to claim 3, characterized in that the gray scale portion is provided along the edge of an opening of the light transmitting portion.
5. A method for producing a master mold for imprinting according to any one of claims 1 to 4, characterized in that the exposure dose is determined based on data relating to the relationship between the exposure dose for a predetermined thickness of the resist and the taper angle of the forward taper.
6. A method for producing a master mold for imprinting according to any one of claims 1 to 4, comprising the steps of: using a light-transmitting substrate as the substrate; using a negative resist as the resist; and including a mask formation step of forming the mask on the surface of the substrate; and exposing the resist to light by irradiating the substrate from the rear surface side through the mask formed on the surface of the substrate.
7. A method for producing a master mold for imprinting according to claim 5, comprising the steps of: using a light-transmitting substrate as the substrate; using a negative resist as the resist; and including a mask formation step of forming the mask on the surface of the substrate; and exposing the resist to light by irradiating the substrate from the rear surface side through the mask formed on the surface of the substrate.
Citation Information
Patent Citations
Forming method of conductive portion forming pattern on substrate
JP2021111668A
Exposure mask and method for manufacturing mask pattern
JP2005258387A
Pattern forming template, pattern forming method and nano-imprinter
JP2008091782A
Method for manufacturing master plate for making stamp for micro contact printing, master plate for making stamp for micro contact printing, and method for making stamp for micro contact printing