Jetting method or coating method for fluid, method for producing secondary battery or all-solid-state battery, method for producing solar cell, and nozzle assembly
The nozzle assembly with thin plates and grooves efficiently coats secondary batteries and solar cells by atomizing fluids, addressing drying time and adhesion issues, and enhancing performance and efficiency in the manufacturing process.
Patent Information
- Application Number
- PCT/JP2024/014470
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-12
- Filing Date
- 2024-04-10
- Publication Date
- 2024-10-17
AI Technical Summary
The existing methods for manufacturing secondary batteries and solar cells face challenges such as prolonged drying times, inefficient coating processes, precipitation of slurry, and difficulty in maintaining film thickness and adhesion at high line speeds, particularly for next-generation batteries like all-solid-state batteries and perovskite solar cells.
A nozzle assembly with multiple thin plates and grooves is used to eject a fluid, combining a slurry with compressed gas or supercritical fluids to stretch and atomize the fluid into fine particles, allowing for efficient coating over wide surfaces at high speeds, reducing solvent evaporation time, and preventing slurry precipitation.
This method significantly shortens drying times, improves coating efficiency, and ensures uniform film thickness, enhancing the adhesion and performance of electrode layers in secondary batteries and solar cells, while reducing equipment size and environmental impact.
Smart Images

Figure JP2024014470_17102024_PF_FP_ABST
Abstract
Description
Fluid ejection or application method, secondary battery or all-solid-state battery manufacturing method, solar cell manufacturing method, and nozzle assembly
[0001] The present invention relates to a fluid ejection method, a fluid application method, a method for manufacturing a secondary battery or an all-solid-state battery, a method for manufacturing a solar cell, and a nozzle assembly.
[0002] With the rise in electric vehicles (EVs), the production volume of lithium-ion batteries (LIBs) is rapidly increasing. This, in turn, has led to an increase in the production volume of LIB electrode forms. However, the LIB electrode formation process requires large drying equipment due to the high line speed, posing a problem of carbon dioxide emissions. Furthermore, the manufacture of all-solid-state batteries using sulfide-based electrolytes, the leading candidate for next-generation secondary batteries, requires a dehumidified environment, which requires even larger equipment. Therefore, space-saving equipment was required while maintaining or improving performance. Furthermore, the formation of electrode layers in other fields, such as solar cell power generation layers, fuel cells, water electrolysis, and carbon dioxide electrolysis, also contributes to carbon neutrality, and as each process speeds up, there has been a strong demand for space-saving manufacturing processes.
[0003] The present invention is applicable to any type of secondary battery, including lithium-ion batteries (LIBs), potassium- or sodium-ion batteries, all-solid-state batteries, and semi-solid-state batteries. Solar cells include organic thin-film solar cells and dye-sensitized solar cells, as well as perovskite solar cells and perovskite-on-silicon tandem solar cells, regardless of their structure or type. The fluid can be selected from liquids, melts, powders, supercritical fluids, and compressed gases, and can be a single fluid or a mixture of these fluids, including short fibers.
[0004] Furthermore, the present invention can be applied to the production and formation of granulation, capsules, short fibers, webs, etc. using multiple fluids using a fluid spraying method. The coating method involves applying a fluid to an object and is effective for the general production of MLCCs, capacitors, and batteries of various shapes, and is suitable for electrode formation in fuel cells, water electrolysis, gas electrolysis, capacitors, etc. It can also be applied to other fields such as electronics and chemicals, and general painting and adhesive processes, contributing to the manufacturing process of these objects, particularly to high-speed production lines.
[0005] Traditionally, the slot die method has been commonly used to coat electrode slurries and other liquids on wide, fast-moving targets, such as secondary batteries, due to its simplicity and ability to accommodate high speeds. Drying equipment has also become available at high speeds, such as current collector coating speeds of over 60 meters per minute. Meanwhile, solvents such as normal methylpyrrolidone (NMP) are commonly used to dissolve the fluorine-based binder in electrode slurries, but their high boiling points require bulky drying equipment. To address this issue, attempts have been made to heat the back roll to high temperatures. However, because the heated roll and the tip of the slot die contact the target via a liquid film, the temperature and deformation of the slot die tip over time due to heat transfer from the heated roll cause gap changes, making it difficult to maintain a consistent coating shape. On the other hand, electrode formation using catalyst ink on thin, instantaneously swelling fuel cell electrolyte membranes, which require thin electrodes, is extremely difficult because the electrolyte membrane must be heated and adsorbed. Furthermore, the formation of photovoltaic layers for perovskite solar cells, which require ultrathin nanometer-level films, has been problematic due to micron-scale gap changes between the heated target and slot die heads or surface tension-based coating heads. Not only was the straightness of the slot die problematic, but the flatness of the heated tables and conveyors used to transport sheets was also an issue, for example when heating sheet-like objects to temperatures above 60°C. The general spray method, which uses a wide gap and a wide angle for spraying, is simple but has extremely poor coating efficiency, making it unsuitable for the secondary battery field, which requires wide widths and high speeds.
[0006] On the other hand, the electrode coating thickness after drying was around 100 micrometers, and only the surface of the coating was in contact with the outside air. Therefore, in order to prevent cracks, the drying temperature was set low and the coating moved at high speed, which resulted in the drying equipment becoming huge and becoming a source of CO2 emissions. As a result, the solvent recovery equipment also became large.
[0007] The secondary battery industry has long sought a method to shorten the drying time during electrode formation and improve electrode performance. To address this issue, some researchers have proposed solvent-free electrode powder formation methods to eliminate the need for drying equipment and solvent recovery equipment. However, unlike previous methods, these methods require binders in amounts of less than a few percent, resulting in poor powder adhesion to current collectors and other components. Furthermore, conductive additives, such as carbon nanofibers and carbon nanotubes (CNTs), also present in trace amounts of less than a few percent, must be efficiently attached to the active material particles. Sulfide-based all-solid-state batteries, considered promising next-generation secondary batteries, require a dehumidified atmosphere, and large dryers and other equipment require significant initial and running costs. Therefore, a more compact electrode formation system was needed. Rapid evaporation of the electrode slurry solvent can be achieved by heating the target material, switching to a low-bottom solvent, using the azeotropic effect of a low-boiling-point solvent in the desired ratio, increasing gas contact, drying in a vacuum, or a combination of these methods.
[0008] When applying a coating to an object, general spraying, which increases contact with gas, particularly the air spray method known as the two-fluid spray method, can quickly evaporate the solvent. However, as mentioned above, when spraying at a wide angle and from a large distance to the object to cover a wide area, the coating efficiency is extremely poor, at around 30%. Furthermore, spray efficiency on secondary battery objects moving at high speeds, such as 60 m / min or more, is further reduced by the influence of wind currents generated above the object. Furthermore, even if multiple spray nozzles are arranged in a horizontal row, the film thickness distribution across the width is extremely poor. Due to these numerous fundamental issues, spraying methods have been avoided, especially for high-speed secondary battery production equipment.
[0009] Furthermore, with the spray method, unless the viscosity is low, for example, below 200 mPascal seconds, the spray particles become coarse, resulting in large variations in coating distribution. On the other hand, slurries with low viscosity and high specific gravity, especially those containing particles such as positive electrode active material, suffer from significant particle settling in the flow path. This is particularly true when there is no circulation, for example, in the flow path downstream of the coating head's on-off valve, where the internal volume is large and the flow rate is slow, or when operation is stopped, resulting in the fatal problem of particle settling. The present invention was made to solve these problems, and it solves each of these individual issues.
[0010] Cited Document 1 discloses a method for forming a flow path by sandwiching a shim with narrow grooves for a viscous fluid between blocks, allowing a viscous fluid such as a hot melt adhesive to seep out of the flow path outlet, and then spraying heated compressed air into the viscous fluid from two directions to produce particles or fibers, which are then applied to a substrate. Cited Document 2, a method invented by the present inventor, proposes a method for spraying a fluid selected from liquid, molten material, powder, supercritical fluid, and gas in a divergent direction from multiple nozzles, even for wide substrates, with the timing staggered to prevent adjacent spray patterns from interfering with each other in the air or on the substrate. In the method of Cited Document 1, the viscous fluid is divided into thin streams by multiple narrow grooves, but heated air is collided with the stream from two directions at a certain angle through wide slit grooves to produce particles or fibers. However, even if a highly cohesive viscous fluid such as hot melt is successfully divided into thin streams, surface tension pulls it toward the wall or surface of the head tip the moment it seeps out, forming a continuous film or large droplets. Because hot melt is a high-temperature molten material (around 180°C), heated air is required to prevent the temperature from dropping. However, simply impacting the droplets from two directions does not achieve a sufficient stretching effect, and surface tension causes the viscous fluid to adhere to metal and other surfaces, spreading into a liquid film or droplets. Therefore, even when heated, impacting the droplets with compressed air alone results in a collection of coarse particles or extremely thick fibers. As a result, the desired small particle size cannot be achieved. The mechanism of finely dividing the liquid using multiple slot grooves and injecting air from air grooves into the liquid is easily understood from the diagram in JP 06-154691, which has a similar structure. This method aims to form a sharp-edged coating film on the desired location on a target object moving relatively at high speed. For this reason, highly viscous or viscous liquids cannot be stretched by simply colliding with compressed air from two directions, resulting in coarse particles, and other issues such as air bubbles remaining in the viscous fluid coating, so a detailed explanation will be omitted. Applications requiring adhesive properties rarely require functions other than adhesion, so atomization or ultrafine short fibers are not necessarily required. Furthermore, even if a thin, wide film of viscous liquid is extruded through a slot die, as per T-die theory, the moment it leaves the edge of the opening, it begins to agglomerate and transitions into a thick, rod-shaped flow toward the center in the air.Because the higher the viscosity, the stronger the cohesive force, making it impossible to break down a thick, cohesive stream into small particles or thin, short fibers using compressed gas. In other words, to achieve atomization or fine, short fibers, it was necessary to narrow, thin, and small the opening, and then, at the moment the liquid or melt separates from the opening edge, a high-speed flow of compressed gas was used from all around the opening to stretch the viscous fluid into fibers, tearing them apart, and then atomizing them using surface tension. Before the short fibers could be transformed into particles by surface tension, solvents with particularly low boiling points evaporate in the air, and resins, for example, become solid, thin, short fibers. Furthermore, when the temperature of low-viscosity heated melts, such as hot melts, drops below their melting point and forms a short-fiber aggregate without forming particles. This is commonly known as angel hair and is used in web manufacturing. In other words, high-viscosity fluids require sufficient or effective stretching or tearing force from all around the opening at the beginning. Furthermore, to achieve finer particles, compressed gas had to be collided with the flow at high speed.
[0011] Patent Publication No. 8-501974, Patent Publication No. 2018-089543
[0012] Therefore, the present invention aims to solve the following problems. Conventional secondary battery manufacturing has faced the following challenges. Similar challenges exist in the electrode formation of next-generation solar cells, such as perovskite solar cells, fuel cells, water electrolysis, and carbon dioxide electrolysis. 1. Shortening drying time: particularly for secondary batteries. 2. Wide-width coating compatibility: general. 3. High-speed line speed compatibility: general. 4. Preventing slurry precipitation: general, particularly for secondary batteries including all-solid-state batteries. 5. Formation of thin to thick films: general. 6. Improved coating film performance: general. The present invention was developed to solve these challenges, and provides a structure that facilitates solvent volatility to accelerate drying. Furthermore, it can be applied to wide widths and accommodates high-speed object movement. It supports both thin and thick films. It provides a structure that prevents or makes precipitation difficult for slurries containing solid particles. It aims to maintain at least conventional coating performance while seeking to improve it. It also aims to bring usage efficiency, including the coating efficiency of slurries, closer to that of conventional die head systems.
[0013] 1. Short-time drying: By stretching and tearing the slurry into particles with compressed gas, the contact area with the gas increases, promoting solvent evaporation. Heating the target object also impacts the spray particles, crushing them and thinning them, promoting solvent evaporation. Furthermore, by layering multiple thin films, a high-solids coating is formed immediately after application. In other words, with this invention, even if the solids concentration before application is low, a high-solids coating, known as a "higher solids," can be formed immediately after application, which is difficult to apply normally. Regardless of viscosity, viscous fluids can be extruded at low flow rates through thin, narrow grooves, e.g., 0.2 mm wide, per pitch of 1 mm to 10 mm, and then stretched and torn into fine particles with compressed gas for application. Furthermore, by pulse-opening and closing the upstream on-off valve on a millisecond basis, even lower flow rates, e.g., 1 / 10th the normal rate, can be achieved, enabling even thinner films. Increasing the flow rate is easily controlled by widening the automatic on-off valve or increasing the hydraulic pressure, enabling thicker coatings. The fluid flow path can also be made as large as desired. Furthermore, even for narrow grooves, thin film deposition with a desired film thickness is possible by arranging multiple nozzle assemblies in the direction of movement of the object and applying the layers. The thickness of the thin plate of the present invention can be selected from 0.05 to 1 mm, and more preferably from 0.05 to 0.5 mm. Therefore, there is no limit to the amount of liquid or the like that can be pumped in the present invention.
[0014] 2. Wide-Width Coating Capability: By selecting the number of nozzle assemblies with 1 to 1,500 nozzle openings for ejecting fluids such as slurry, coating widths ranging from narrow to wide can be accommodated. For example, for slow line speeds of 100 mm per minute, a nozzle assembly with one or fewer openings can be used to traverse perpendicular to the direction of object movement. For wide, slow-moving objects, even a wide-width head with a 1,500-opening nozzle assembly can be used to deposit thin films by adjusting the pulse interval. For wide, fast-moving objects, a fixed wide-width nozzle assembly can be used to coat, while a nozzle assembly with fewer openings can be swung in a short traverse. For example, a nozzle assembly with 1,500 openings and a 1 mm opening pitch can be used to coat a wide width of approximately 1,500 mm. Even when using a smaller number of openings and a wider pitch, multiple nozzle assemblies can be installed in the direction of object movement to narrow the overall fluid opening pitch. Five sets of nozzle assemblies with a fluid opening pitch of 5 mm are roughly equivalent to a 1 mm pitch. The number of layers can be increased by increasing the number of nozzle assemblies. Therefore, when forming LIB electrodes, a conductive additive, such as a desired low-solids dispersion of carbon nanofibers, can be mixed from around the active material particle slurry, stretched from the periphery by compressed gas, and then atomized and applied. Because it is layered, it is possible to disperse and mix a small amount of conductive additive with the desired distribution. The flow paths of the active material and conductive additive can be reversed. Furthermore, by improving electrode performance and increasing contact with compressed gas, drying time can be significantly reduced.
[0015] 3. High-speed line speed compatibility: The distance between the nozzle assembly opening and the target can be selected, for example, from 1 to 70 mm, more preferably from 5 to 50 mm. This allows for negligible effects of wind disturbances that can adversely affect particles caused by targets moving at high speeds. Furthermore, the opening pitch can be shortened, allowing particles to travel in a nearly straight line toward the target, resulting in a high impact, dense particle adhesion, and reduced rebound. In other words, by narrowing the nozzle opening pitch to, for example, 1 to 6 mm and arranging multiple nozzle assemblies in rows, for example, six rows, a system can be created that also achieves the effect of thin-film deposition.
[0016] 4. Slurry Settling Countermeasures: High-viscosity slurry is made resistant to settling and transported to the channel opening. Even with high viscosity, the slurry volume can be divided by multiple long, thin, comb-like grooves, reducing the flow rate from each opening. The thin slurry stream can be stretched from the entire periphery by compressed gas or compressed gas containing solvent particles, resulting in fiber-like fragmentation. A further method for further atomizing high-viscosity slurry is to merge the solvent from the periphery downstream of the slurry opening, swelling the high-viscosity slurry with the surrounding solvent to reduce its viscosity, thereby forming fine particles through the stretching and tearing effect of the compressed gas from the entire periphery. If desired, the above two methods can be combined to further refine the combined fluid or particles by using the collision energy of a compressed gas impinging stream from close proximity. Another option in the present invention is to mix an inert gas into the high-viscosity slurry upstream of the channel, dispersing it into a foam, which then shrinks the bubbles under hydraulic pressure. The foam then forms when it is ejected from the opening, making it easier to tear the slurry apart through the foaming force and the stretching force of the compressed gas from the surroundings. In this invention, the desired flow path can be formed using multiple thin plates, so the volume of the flow path downstream of the on-off valve can be made as small as possible, even for foamed viscous fluids. The timing of application is such that the compressed gas is ejected faster than the slurry ejection speed and can be ejected until after the slurry ejection has finished, allowing for clean cutting of a pulsed application pattern, including foamed liquids.
[0017] 5. Thin and Thick Films: Reducing the liquid fluid supply flow rate automatically results in a thin coating film, while increasing the supply rate results in a thick coating. To save energy, the amount of compressed gas can be increased or decreased according to the flow rate of the liquid fluid. Furthermore, regardless of viscosity, a viscous fluid can be divided into thin, thin layers (e.g., 50 to 300 μm) using elongated grooves in a thin plate, and then stretched and atomized by compressed gas or other means from the periphery, creating a nozzle assembly capable of coating thin to thick films. Multiple nozzle assemblies, for example, 10 rows, can be arranged in the direction of object movement. Since the present invention allows for the placement of any desired number of nozzle assemblies, there is no limit to the amount of liquid or other material pumped. The nozzle assembly and the object can move relative to each other. This invention allows for the same liquid film coating as a slot die. Since the gap between the nozzle assembly tip and the object can be wider than the liquid coating thickness, there is no need to worry about damage to the coating film, such as streaks caused by debris, which is a problem with slot dies. Therefore, this invention allows for the application of a liquid film to the object using a compressed gas-supported slot die by lowering the compressed gas pressure. A relatively high viscosity fluid can produce a narrow stripe coating, while a low viscosity fluid can be used with a narrow fluid opening pitch, allowing the fluid to flow over the target object, resulting in the formation of a continuous coating.
[0018] 7. Improved Coating Performance: The nozzle assembly of the present invention uses a thin plate structure that prevents viscous fluids from pooling on the wall of the nozzle opening due to surface tension, resulting in stable atomization of liquids and other materials. This allows for thin-film deposition, enabling dense deposition of electrode active material particles and other materials. Heating the target object to the desired temperature improves wetting after application and rapidly volatilizes the solvent. This allows for a well-dispersed composite slurry containing multiple particles and short fibers selected from active material particles, electrolyte particles, conductive additives, binders, etc., to be solidified immediately after application. The present invention achieves a nozzle assembly structure that allows for coating with minimal energy by combining multiple individual slurries or a selected number of composite slurries as they leave the nozzle opening, stretching and tearing them using compressed gas or other means to form fine particles, as needed, and applying them to a heated target object in a thin-film deposition process. In addition, in this invention, the electrode mixture is granulated to a powder with an average particle size of approximately 7 to 70 μm, and then mixed with a solvent to form a slurry, which serves as the first fluid and is then sprayed simultaneously with the second fluid, compressed gas, to form a powder layer by instantly volatilizing the solvent after application to the target object. Because the powder slurry has a low dynamic viscosity and is easy to form into spray particles, the pressure of the compressed gas can be kept low, at 0.2 MPa or less.
[0019] As described above, the present invention is effective for granulation and coating in general, and is particularly effective for high-speed production, which is in high demand, such as electrode formation for fuel cells such as SOFCs and PEFCs, and water electrolysis, MEA production, electrode formation for secondary batteries including all-solid-state batteries and semi-solid-state batteries, and capacitors, functional membrane and electrolyte layer formation for porous separators for secondary batteries, electrolyte layer formation for all-solid-state batteries, and power generation layers, functional membranes, and electrodes for organic solar cells.
[0020] Therefore, the present invention is as follows.
[0021] The present invention is a method for jetting a liquid fluid or applying it to an object, which comprises the steps of: aligning and stacking a plurality of thin plates and plates or blocks each having a thin groove formed therein for the fluid; forming a thin flow path for the fluid and one or more openings for jetting a first liquid fluid at the end of the thin plate; forming a jetting opening for a second fluid, which is a compressed gas or a compressed gas mixed with solvent particles, or a supercritical fluid, separated by a wall around the opening for jetting the liquid fluid; and forming a jetting opening for the first liquid fluid and the thin flow path via an upstream flow path. and connecting the elongated flow path for the second fluid to a first on-off valve that opens and closes the supply of the first liquid fluid via an upstream flow path; and stretching a discharge flow discharged from the opening of the first liquid fluid by opening the first and second on-off valves with a jet flow from the entire periphery of the jet outlet of the second fluid, and ejecting the discharged flow as fibers or particles, or applying the jetted fibers or particles to an object.
[0022] The present invention provides a method for ejecting or applying a liquid fluid, characterized in that the number of grooved thin plates is increased to make the number of fluids and openings three or more, the outermost openings are used as outlets for compressed gas or compressed gas containing solvent fine particles or supercritical fluid, the inside of which are used as openings for liquid fluid, and at least one of the openings for liquid fluid is used as an outlet for solvent.
[0023] The present invention provides a method for jetting or applying a fluid, characterized in that another compressed gas or a compressed gas containing solvent fine particles is collided with the jet flow of the jetted liquid fluid at an acute angle and from a close distance to finely atomize the fibers or particles and jet them out, or the finely atomized fibers or particles are applied to an object.
[0024] The present invention provides a method for producing a secondary battery or an all-solid-state battery, characterized in that the first fluid is selected from a slurry having a solid content of 25 to 75 weight percent, a slurry for a secondary battery electrode, a slurry for an all-solid-state battery electrode, or a slurry for an all-solid-state battery electrolyte, the second fluid is selected from a compressed gas, a mixture of solvent fine particles and a compressed gas, or a supercritical fluid, the two fluids are joined, the first fluid is stretched by the second fluid or the slurry is granulated by collision energy, and the slurry is applied to an object selected from a current collector, an electrolyte layer, an electrode layer, or a separator to form an electrode layer, an electrolyte layer, or a functional membrane layer.
[0025] The present invention provides a method for manufacturing a secondary battery or an all-solid-state battery, characterized in that after the two fluids are joined, a step is added in which a compressed gas or a compressed gas mixed with solvent fine particles is collided with the joined fluid at an acute angle, and the finely divided slurry is applied to an object selected from a heated current collector, an electrolyte layer, an electrode layer, and a separator to form an electrode layer, an electrolyte layer, or a functional film layer.
[0026] The present invention provides a method for producing a secondary battery or an all-solid-state battery, characterized in that the first fluid is selected from a slurry having a solid content of 50 to 85 weight percent, a slurry for a secondary battery electrode, a slurry for an all-solid-state battery electrode, and a slurry for an all-solid-state battery electrolyte, the second fluid is a solvent, and the third fluid is a compressed gas or a supercritical fluid, and the method further comprises the steps of: joining the three fluids; particleizing the slurry by the stretching or collision energy of the compressed gas or supercritical fluid; and atomizing the particles by colliding the compressed gas or compressed gas mixed with fine solvent particles with the particles at an acute angle of 30 degrees or less with respect to the ejection direction of the first fluid; and applying the fine particles to an object selected from a current collector, an electrolyte layer, an electrode layer, and a separator, which has been heated by impact, to form an electrode layer, an electrolyte layer, or a functional film layer.
[0027] The present invention provides a method for manufacturing solar cells, which involves moving a nozzle assembly that generates liquid droplets relative to an object and applying a liquid for a power generation layer or gas barrier layer in the form of droplets, the method comprising the steps of: manufacturing a nozzle assembly in which a plurality of thin plates, plates, or blocks with elongated grooves are stacked on both sides and 1 to 1,500 openings for a second fluid are arranged, separated by walls around the openings for a first fluid; and the first fluid is a transparent conductive layer, power generation layer, or gas barrier layer liquid, and the second fluid is a compressed gas or a supercritical fluid mixed with compressed gas or solvent particles, and the first fluid is stretched into fine particles by the surrounding compressed gas or supercritical fluid, and the fine particles are applied to an object selected from a heated silicon solar cell layer, transparent glass for a solar cell, and transparent plastic film, to form a transparent conductive film layer, power generation layer, or gas barrier layer.
[0028] The present invention provides a method for producing a perovskite solar cell, wherein the solar cell is a perovskite solar cell or a perovskite-on-silicon tandem solar cell.
[0029] The present invention provides a nozzle assembly for ejecting a liquid fluid, comprising: a first thin plate having one or more elongated grooves for a first fluid extending from the middle of the first thin plate to an end of one side of the plate; elongated grooves for a second fluid located on both sides of the first fluid groove and having a length from the end shorter than that of the first fluid groove; at least two second thin plates stacked in position on both sides of the first thin plate having elongated grooves connecting to a second flow path of the first thin plate; and a third thin plate having second fluid grooves formed thereon, the second fluid grooves being at least as wide as the ends of the elongated grooves for the first fluid of the first thin plate; or a second flow path at least wider than the width between centerlines of the elongated grooves for the second fluid located on both sides of the elongated groove for the first fluid of the first thin plate. a second thin plate is positioned on both outer sides of the first thin plate around the first thin plate as a center, and a third thin plate is positioned on both outer sides of the second thin plate; the second and third thin plates are formed with flow paths connected to elongated flow paths for selected fluids; plates or blocks having flow paths formed therein connected to one or more elongated grooves for the first fluid and the second fluid are superimposed to form one or more elongated flow paths and openings for the first fluid; an opening for the second fluid is provided on a wall surrounding the opening for the first fluid; the upstream of the opening for the first fluid is connected to an on-off valve that supplies the first fluid via the flow path, and the upstream of the opening for the second fluid is connected to an on-off valve that supplies the second fluid via the flow path.
[0030] The present invention provides a nozzle assembly in which, instead of the third thin plate, a plate or block having grooves for a second fluid is aligned and overlaps the second thin plate on both sides.
[0031] According to the present invention, as described above, thin grooves can be machined into multiple thin plates and stacked with blocks or the like to form one or more fluid flow paths and openings of the same shape. This eliminates the need to combine multiple parts with complex shapes, such as spray nozzles. Even with multiple nozzles, such as 1,500 nozzles, it is possible to form a nearly uniform jet flow without worrying about variations in the coating distribution of spray nozzles. Therefore, the present invention can also meet the desired requirements for wide-width objects.
[0032] Etching can be used to machine grooves in thin plates. Laser processing, such as with a femtosecond laser, has minimal temperature effects, allowing for processing even thin plates, such as 50 μm thick, without deformation. While the thickness of the plate is not particularly limited, a thickness of 0.05 to 1 mm is preferred, and 0.05 to 0.5 mm is more preferred. As described above, the present invention can accommodate desired fluid viscosities, coating widths, coating speeds, and coating thicknesses. It can be effectively applied in a wide range of fields, such as electrode layers and electrolyte layers for secondary batteries, including all-solid-state batteries, functional film coatings for separators, organic thin-film systems for forming power-generating layers, next-generation solar cells, including perovskite-on-silicon tandem solar cells and perovskite-on-perovskite tandem solar cells, fuel cells for electrode formation, water electrolysis, and carbon dioxide electrolysis. Perevskite-silicon tandem solar cells, in particular, require nano-level conductive oxide films and power-generating layers to be formed along the finely textured surfaces. However, conventional spray coatings cannot achieve uniform coating due to the inability to resolve air cushions. This is possible with the present invention, which allows for the deposition of thin films of fine particles with impact from close range. Ideally, the pulsed fine particles with impact can be deposited along the unevenness to form a thin film. Furthermore, nano-level ultrafine particles generated by the nozzle assembly of the present invention or by impacting an object can be electrostatically charged and deposited on a grounded object. Therefore, this method is effective for all objects in other fields that have fine unevenness.
[0033] The first thin plate of the nozzle assembly of the present invention can be selected from a thickness of approximately 50 to 300 micrometers, for example. While there is no restriction on thickness, thinner plates are preferable when considering that viscous fluids adhere to the end surface due to surface tension. The second and subsequent thin plates can be thin as described above, but when using supercritical fluids, a thickness of approximately 0.3 millimeters or more is desirable for strength. Furthermore, the protrusion level of the opening for the first liquid fluid can be the same as that of the other openings. However, if the wall end surface is thick, the liquid will easily wet due to surface tension and accumulate. Therefore, it is desirable for the end surface of the first opening to protrude approximately 0.1 to 2 mm beyond the end surface of the second opening to prevent accumulation on the wall of the second opening. Furthermore, by setting the timing of the compressed gas ejection longer before and after the liquid fluid ejection, liquid fluid accumulation on the end surface of the thin plate can be prevented, resulting in uniform liquid particles from the beginning to the end of ejection. For this reason, the thinner the wall thickness of the viscous fluid flow path, the better. Therefore, the thickness of the thin plate can be selected from a thickness of approximately 50 to 300 micrometers, for example. The smaller the first opening area, the thinner and narrower the opening, the more finely the viscous fluid can be divided. Furthermore, the thinner the wall, the better the stretching effect of the compressed gas, promoting atomization. Furthermore, since the present invention forms a three-dimensional flow path by aligning and stacking multiple thin plates with thin grooves, it can be easily disassembled. This means that each thin plate can be processed individually. After use, the flow path can be completely and easily cleaned by disassembly using ultrasound or other methods. Surface treatment is also possible. Surface modification treatments such as corrosion resistance and water repellency can be performed. For example, metal plates can be plated or ceramic coated. While it is extremely difficult to thoroughly treat and clean the inner surface of a thin, long, cylindrical flow path, such as a metal cylinder with an inner diameter of 0.1 mm and a length of 30 mm, such as a syringe needle, using the method of the present invention, this can be easily achieved.
[0034] The present invention allows particles to be sprayed onto an object at close range and at a narrow, nearly straight spray angle, for example, 20 degrees or less, or even 15 degrees or less, allowing for effective coating of objects moving at high speeds. This minimizes rebound, which occurs when the spray stream collides with the object, as occurs with a wide spray angle, resulting in high coating efficiency. High coating efficiency and high density at the object interface and between particles can be achieved by spraying with impact from close range. Pulsed spraying with impact is even more effective.
[0035] A slurry circulation circuit is formed upstream of the on-off valve of the coating head, allowing it to circulate at high speed. However, circulation is not possible in the flow path inside the head downstream of the on-off valve. As a result, slurries that settle particularly quickly settle inside the head. For this reason, it is preferable to reduce the internal volume of the head and increase the flow rate. The present invention increases the flow rate and minimizes cavities by forming narrow flow paths using thin plates. This makes it possible to solve the problem of precipitation by automatically periodically discharging a small amount of slurry inside the head downstream of the on-off valve using a solvent, etc., even when the line is stopped. The slurry can also be periodically discharged before it settles.
[0036] For secondary batteries, especially for the cathode slurry, fluorine-based materials such as PTFE and PVDF are often used as binders for their durability, so solvents with high boiling points have generally been used. Drying was then carried out in huge drying ovens. One of the goals of this invention is to shorten and downsize the drying process as much as possible.
[0037] The present invention enables space-saving production even with the high-speed line speeds required for forming electrodes in conventional secondary batteries. The solution dries immediately after application to the target object or in as short a time as possible. To achieve this, the solvent must be made more volatile. In the present invention, for the positive electrode of an all-solid-state battery, a thin film of a sulfide-based electrolyte or other electrolyte can be coated on the active material particles, for example, by dry mixing. The coated core-shell particles can then be dispersed in a solvent. A small amount of a binder, such as short fibers or fine particles, can be added to the solvent. Low-boiling point solvents and mixed solvents are preferable in terms of volatilization. Therefore, the solvent can be made to volatilize immediately after application to the target object. By forming a powder slurry by assembling multiple core-shell particles into a powder of 10 to several tens of micrometers, the solvent can be made to volatilize more easily. In this invention, regardless of the type of slurry, the flow path is divided into thin, comb-like segments, and the slurry is discharged from the opening. The compressed gas then stretches the slurry into finer, more fibrous lines or fragmented particles, which then collide with the heated object with an impact at the moment of application, spreading the solvent along with the flow path to a thin film, promoting solvent evaporation and forming a thin film. Therefore, the flow rate can be reduced by making the flow path and opening long enough to prevent solid particles from clogging. Furthermore, the fine particle application pattern from the nozzle assembly's liquid fluid openings can be achieved by arranging multiple nozzle assemblies in the direction of object movement so that the patterns overlap as much as possible on the object, and overlapping each pattern to achieve the desired distribution. Furthermore, in this invention, high-speed compressed gas impinges on the mixed flow of compressed gas that stretches or atomizes the slurry, etc., from as close as possible to form fine particles, further increasing the surface area of the slurry particles. This further promotes solvent evaporation and speeds drying. Increasing the number of layers allows for the formation of a more uniform coating film. In addition, by colliding slurry particles with the energy of speed against a heated object, the solvent contained in the slurry particles is crushed, increasing the surface area and accelerating solvent evaporation, resulting in an ultra-dense structure such as solid particles, which can improve adhesion. Since accelerating evaporation lowers the surface temperature of the object due to the heat of vaporization of the solvent vapor, it is important to vacuum-adsorb and heat the object via a heated adsorption drum or belt during application while simultaneously moving it. The heating temperature can be selected from 50 to 180°C.
[0038] In commercially available air spray systems, two-fluid sprays are atomized by stretching the liquid and colliding with compressed air, spreading the pattern and applying the spray stream to the target. However, the viscosity was generally relatively low. It was also not possible to manufacture spray nozzles with the same particle size distribution or spray pattern. For example, even if multiple nozzles were arranged in a horizontal row, it was not possible to obtain the same discharge volume, particle size, particle size distribution, spray pattern, etc. under the same settings. Therefore, even when multiple relatively uniform nozzles were selected from a large number of nozzles and lined up in a row, it was not possible to obtain a uniform coating, even with the adjustments of an experienced worker.
[0039] The liquid or melt is stretched or torn into fibers or a particle stream by a compressed gas or a supercritical fluid made from recovered carbon dioxide gas. If further atomization is desired, atomization can be achieved by colliding another compressed gas with the particle stream from close range at the desired angle. The distance between the liquid fluid opening and the target object is preferably 60 mm or less, and more preferably 30 mm or less, allowing the particles to impact and adhere to the target object. Coating with a nearly straight particle stream is advantageous in terms of improving the density of the coating film and coating efficiency.
[0040] As described above, the present invention significantly impacts the particles when they collide with the target, thereby improving particle adhesion at the target interface. Furthermore, the more linear the particle travel and the narrower the travel angle, the narrower the particle's angle of incidence with the target, resulting in less reflected flow and higher coating efficiency. The compressed gas can be from a single flow path or opening, or from multiple flow paths or openings. Multiple compressed gas streams are effective, for example, because they can stretch a high-viscosity fluid, enveloping it from both the inner and outer peripheries. Groups of solvent particles can be mixed into the compressed gas. Furthermore, atomization can be further enhanced by colliding compressed gas from another flow path at a close distance at a desired angle with the confluence of these streams. If coating film leveling is desired, solvent particles can be mixed into at least one compressed gas, or a separate opening can be used as a solvent stream.
[0041] The present invention is particularly suitable for battery applications requiring high speed, such as secondary batteries, including all-solid-state batteries, fuel cells, water electrolysis, and carbon dioxide gas electrolysis. In secondary battery applications, the fluid can be selected from electrode active material particles, electrolytes, conductive additives, conductive additive dispersions, binder particles or short fibers, binder solutions, composite powders for secondary batteries, all-solid-state batteries, and semi-solid batteries, electrode composite slurries, solvents, compressed gases, and supercritical fluids. The target object can be selected from current collectors, electrode layers, separators, and electrolyte layers, and the liquid fluid can be atomized and sprayed. Separators moving at high speeds can be coated with thin films of ceramic particles or electrolyte particles such as LLZ. For breathable separators, effective impregnation or coating with ceramic particles can be achieved by adsorbing or heating the separator using a roll or belt.
[0042] Furthermore, the compressed gas injected at the acute angle can be ejected from a close distance, e.g., 2 mm or less, before the speed energy decreases, thereby obtaining the desired fine particles. The compressed gas outlet for collision can be round, rectangular, or slit nozzle-shaped, but square or rectangular shapes are preferred due to their cost benefits. For example, shims with multiple narrow or wide grooves may be sandwiched between block surfaces or plates to form a long slit groove along the length of the nozzle assembly with a flow path approximately 100 micrometers thick. The slit groove may be wide enough to cover all fluid openings, and each opening can be as short as 1 mm or less. To increase the atomization and collision energy, collision from two directions at acute angles causes the particle distribution group after collision to move at a narrow angle, resulting in a high impact on the target object and the formation of a dense particle layer, thereby improving coating efficiency. On the other hand, obtuse angles result in a wider pattern but reduce coating efficiency. Because compressed gas undergoes adiabatic expansion and collision energy decreases with distance, the collision distance is preferably close, e.g., within 5 mm, more preferably within 2 mm, and is preferably as close as possible. The particle collision energy with the target object is preferably at a narrow angle, for example, an ejection angle of less than 30 degrees, preferably less than 20 degrees, and collision from close range, with the distance between targets after particle formation being less than 60 mm, more preferably less than 30 mm. The supercritical fluid obtained from the recovered carbon dioxide can be made to a high pressure of around 9 MPa, allowing it to collide with high-viscosity slurries at high speeds, which is effective in promoting the evaporation of high-boiling-point solvents contained in the slurry after collision through azeotropy. The evaporated carbon dioxide can be recovered.
[0043] The target object can be a long object such as a film or foil, or it can be a sheet or a three-dimensional structure. It can be silicon plates, glass plates, plastic films, etc. for next-generation solar cells, and there are no restrictions on size, shape, material, number, or mass. The fluid can be a supercritical fluid such as carbon dioxide gas, compressed gas, gas-powder mixture, liquid fluid or paste, or a heated melt material. Fluids with solid content can be used for particle granulation, short fiber, or web production in addition to film formation. Particles can also be applied directly to the target object.
[0044] Therefore, in addition to batteries, the material can be suitably used in capacitor manufacturing, multilayer ceramic capacitor manufacturing, and in the electronics, food, pharmaceutical, and chemical fields. It can also be favorably used to provide functional layers for fuel cells, secondary batteries, and all-solid-state batteries, to form electrodes and electrolyte layers, and to form functional films, power generation layers, and gas barrier layers for solar cells.
[0045] This method is particularly effective when increasing productivity in roll-to-roll or sheet-to-sheet applications, as it can accommodate a wide range of materials. It is also effective for composite materials that tend to separate even after mixing and dispersion, as it allows the materials to be mixed and dispersed at the moment of application. Furthermore, when forming thin, multi-layer coatings or mixing even more different fluids, multiple nozzle assemblies (coating devices) can be stacked in series along the direction of movement of the target object.
[0046] The present invention can spread a fluid such as a liquid and, if necessary, convert it into fine particles to apply a coating pattern of fine particles about 1 mm to an object. A desired number of spray patterns, such as 1 mm or 5 mm, can be arranged in a single row, for example, 1,500 particles, to apply a desired width to a wide object, even one with a coating width of 1 m or more. A pair of openings can apply a pattern of liquid fluid, and high-speed production can be achieved by moving the nozzle assembly, which uses a comb-shaped flow path for the wide liquid fluid, relative to the object.
[0047] Thin grooves or comb-like shapes in thin metal plates, for example, can be produced with high precision using exposure and etching. Fine comb-like shapes can be formed on thin plates such as ceramics using femtosecond laser processing, which is less affected by heat. The thin plate can be made of metal such as stainless steel (SUS), or it can also be a ceramic or plastic plate. Therefore, the present invention can produce multiple grooves with the same structure simultaneously with high precision, and since the assembly has the same structure, individual variations in multiple flow paths and openings can be ignored. Therefore, there is no variation like with commercially available air spray nozzles, and almost the same particle ejection quality can be achieved even over a wide width, maintaining coating quality.
[0048] The present invention combines multiple fluids with multiple nozzle assemblies, and even with combinations that utilize high-speed pulsed operation of the on-off valves of desired fluids. By managing individual conditions, such as the on-off or on-off time of each fluid, the pressure of each fluid, and the distance between the nozzle assembly and the target object, it is possible to achieve a composite distribution that cannot be achieved by conventional mixing of multiple fluids. It can also handle slurries containing particles that are impossible to achieve with inkjet printing, or highly viscous liquids. Furthermore, by using high-pressure compressed gas or recovered carbon dioxide gas to convert it into a supercritical fluid and spray it at high pressure, it is possible to generate fine particles even from highly viscous fluids. Furthermore, multiple fluids can be instantly mixed and dispensed outside the nozzle assembly, even in wide-area, high-speed production. The present invention also features the ability to easily and instantly change the flow rate ratio of multiple different fluids and the thin-film deposition of different mixed fluids through the above management. Flow rates can be changed by any suitable method, including pressure-based methods such as pumps, electrically driven positive displacement systems, or pulsed systems that rapidly open and close on-off valves. The deposition method is also not limited. The same liquid can be deposited, or different liquids or powders can be deposited in thin films as needed.
[0049] Traditionally, the slot die method has been widely used to apply liquids such as electrode slurry to wide, fast-moving targets, such as secondary batteries. Because the solvent used to dissolve the binder in the slurry has a high boiling point, a high-temperature back roll is ideal. However, because the heated roll and the tip of the slot die contact the target via a liquid film, the temperature and deformation of the slot die tip cause gap changes, making it difficult to achieve a consistent coating shape. On the other hand, applying a thin film of catalyst ink directly to the electrolyte membrane of a fuel cell requires a roll with a complex internal structure that combines both adsorption and heating functions, as the electrolyte membrane, approximately 10 micrometers in diameter, instantly swells with the solvent. However, even though this heated adsorption roll maintains low roundness at room temperature, it suffers from a fatal problem of roll deformation at high temperatures. This further changes the gap between the electrolyte membrane and the slot die, making thin film deposition impossible. The electrode layer of perovskite solar cells also requires a nanometer-level thin film, and this has not been possible to control. Therefore, while spraying with a wider gap is possible, wide-area application and extremely low coating efficiency have been issues.
[0050] The present invention was made to solve these problems, and is capable of coating over a wide area and is compatible with the high-speed movement of objects. It also prevents or makes it difficult for slurries containing particles that are particularly prone to settling to settle in the flow paths after the circulation circuit. It creates a coating system that makes it easy to volatilize the solvent from the moment it is sprayed. It is also compatible with high-speed production speeds. And when coating film performance is required for electrodes, etc., it forms an electrode layer with a high density of active material, etc.
[0051] For example, slurries containing particles of active materials are often used for electrode materials in batteries such as secondary batteries and all-solid-state batteries, as well as supercapacitors. Lowering the viscosity of a slurry improves its suitability for spraying. However, lowering the viscosity can lead to settling of particles, especially those with high specific gravity, in the flow path. For this reason, a method of circulating the flow path at high speed to prevent settling has been proposed. However, while settling can be prevented upstream of the valve, settling occurs downstream, clogging the nozzle. For example, in the case of a slurry containing a ternary active material with a solids content of 40% or less by weight, stopping application can cause particles to settle inside the nozzle within a few minutes, even with a nozzle diameter of 0.3 mm. Therefore, when production is stopped, it is necessary to constantly or automatically periodically discharge the desired amount of slurry from the nozzle. This invention increases the solids content of the slurry, reducing settling, thereby reducing the settling rate inside the nozzle. Furthermore, the slurry, including the inside of the nozzle downstream of the valve, can be replaced with solvent by pushing it through. At the start of production, production can be started simply by purging the flow path after the valve.
[0052] The present invention can be configured so that the slurry in the narrow flow path downstream of the on-off valve is washed away by the solvent flow from the upstream of the flow path.
[0053] The present invention is also effective for external mixing and coating of liquid fluids that react upon contact or mixing of two or more liquids. Therefore, a solvent opening can be provided between the openings of the two liquids to prevent reaction near the openings after coating. It can also be effectively applied to perovskite solar cells, in which two different liquids are layered or mixed and coated onto an object to form a power-generating layer. Perovskite solar cells require a method for accurately coating a thin film of a low-viscosity power-generating liquid, such as lead iodide, onto the object. Coating devices used so far include inkjet printers, slot dies, and devices that utilize surface tension to form thin films with a constant gap. However, all of these methods require controlling the gap between the object and the tip of a nozzle or other device to within a micron. Heating an object can cause subtle changes in the straightness of application heads such as slot die heads, which also alter the gap between the object and the coating, making it extremely difficult to maintain coating precision. The present invention allows for a wide gap between the object and the coating surface, and as described above, allows for wide coating widths of, for example, 1 m or more, making it suitable for high-speed production. The present invention also allows for high-speed application by impacting fine particles with pulsed impacts on the object. Therefore, even with uneven silicon substrates such as perovskite-on-silicon solar cells, a pulsed impact can be applied to prevent air cushions, allowing the fine particles to adhere to the finely uneven surface in a thin film. The particle size can be made finer than inkjet particles, and the number of particles per pulse per aperture can be several hundred times greater. Furthermore, up to 1,500 apertures can be installed, offering significant advantages in terms of high speed. On the other hand, it was previously impossible to use inkjet printing when electrode powder particles of approximately 5 to 70 μm used in dry printing were made into a powder slurry. However, the present invention can easily handle primary or aggregated particle diameters of less than one-third of the flow path.
[0054] In the present invention, a desired number of liquids can be merged and atomized with compressed gas for application. The liquid types can be one or more, for example, three or more. Furthermore, in the present invention, a solvent can be ejected from the openings surrounding a liquid fluid containing solids. At least one of a solvent, plasticizer, dispersant, or surfactant can be selected and mixed into the compressed gas at the outermost opening, forming fine particles, and then ejected from the opening. In particular, the solvent attached to the liquid fluid opening also has the effect of preventing the leading edge opening of the liquid fluid from drying out. The solvent can be a good solvent, a poor solvent, or a mixed solvent. In the case of a water-based liquid, water or a mixed solvent of water and alcohol can be used. The selected solvent, surfactant, etc. can also be attached to the atomized liquid particles to support leveling after application to the target object.
[0055] Furthermore, before or after applying powder to an object, a liquid material containing a solvent or solids can be applied by the method of the present invention.
[0056] As described above, the present invention is particularly effective for forming electrodes for secondary batteries including all-solid-state batteries, fuel cells, water electrolysis, etc., forming electrodes for capacitors, applying functional films to secondary battery separators, forming electrolyte layers for all-solid-state batteries, power generation layers for perovskite and organic solar cells, and moisture barrier functional films.
[0057] Fig. 1 is a schematic cross-sectional view and a plan view of a nozzle assembly according to an embodiment of the present invention; Fig. 2 is a schematic cross-sectional view of a nozzle assembly according to an embodiment of the present invention; Fig. 3 is a related schematic view of each thin plate groove machining of a nozzle assembly according to an embodiment of the present invention; Fig. 4 is a schematic view of a fluid machining groove of a block of a nozzle assembly according to an embodiment of the present invention; Fig. 5 is a schematic cross-sectional view of a nozzle assembly according to an embodiment of the present invention;
[0058] The following describes preferred embodiments of the present invention with reference to the drawings. Note that the following embodiments are merely examples for facilitating understanding of the invention, and do not exclude additions, substitutions, modifications, and the like that can be implemented by those skilled in the art within the scope of the technical concept of the present invention.
[0059] FIG. 1 shows a schematic plan view and a schematic cross-sectional view of a fluid opening of a nozzle assembly. One or more elongated first grooves are formed in a first thin plate 1, extending from the middle of the plate to the end of one side of the plate. The thin plate may be polygonal, but a rectangular shape is preferred. When there are one or several fluid grooves, a vertically long rectangular thin plate is preferred. When there are multiple fluid grooves, e.g., 100 or more, a horizontally long rectangular thin plate is preferred. A thin groove for the first fluid is formed in the middle of the rectangular first thin plate 1 and connects to the end of the desired side. Second thin plates 2 and 2' are stacked on both sides to form a first flow path 101 for the first fluid and a first opening 11 at its end. If multiple first grooves are formed, multiple first openings 11 can also be formed. The first groove becomes the first flow path 101, and the end of the first flow path 101 becomes the first fluid opening 11. Furthermore, on both sides of the first fluid groove in the first thin plate 1, elongated grooves for the second fluid are formed, shorter in length from the end than the first fluid groove. Grooves are formed in two second thin plates 2, 2' at substantially the same position and shape as the second grooves. Multiple thin plates, for example, four, may be used. The second thin plate is aligned with the first thin plate and stacked on both sides of the first thin plate. The first elongated groove forms one or more flow paths for the first fluid, with the second thin plate serving as walls 13, and one or more openings 11 for the first fluid at the ends of the thin plates. The first thin plate 1 and the second thin plates 2, 2' are aligned with each other, and third thin plates 3, 3' are stacked on both sides. Grooves of a width connecting to the two grooves for the second fluid formed on either side of the first flow path in the first thin plate are formed in the third thin plate 3, 3'. The third thin plates 3, 3' are aligned with the second thin plate and stacked. A selected thin plate 4, plate, or block 5 is aligned and stacked on the outside of the first, second, and third thin plates to form one or more flow paths and openings 11 for the first fluid, and a flow path 103 and opening 12 for the second fluid, separated by a wall 13 around the outer periphery of the flow path 101 and opening for the first fluid. The thin plate 4 can be omitted. The alignment method is not limited, but can be achieved, for example, by drilling holes in each thin plate and block and inserting knock pins. It is generally preferable to provide knock pins in two or more locations where they do not interfere with the flow paths. Upstream of the flow path 101 for the first fluid, a flow path 116 is formed in the thin plates 2, 3, and 4 and block 6, and is connected to an upstream open / close valve 126.Grooves 120 are formed in the end face of the block on the thin plate side, and are formed with a width that allows the first fluid to spread to multiple flow paths for the first fluid. Also, flow paths connected to the flow paths for the first fluid are formed at the same positions in each thin plate. Similarly, flow paths and grooves for the second fluid are formed in the thin plate and block, and the second fluid opening 12 is connected to an upstream open / close valve 127 via a flow path 117. Instead of forming grooves in the third thin plate, grooves can be formed on the inside of the block 5, thereby omitting the third and fourth thin plates.
[0060] In Figure 2, openings 214 and 215 are provided on the exterior of the blocks for ejecting another compressed gas or the like to collide with the fluid ejected by the nozzle assembly in Figure 1. The tapered surfaces of blocks 25 and 26 are extended to intersect with the extension of the first fluid flow path 201. The closer the distance to the intersection, the better; a distance of 2 mm or less is desirable to minimize deceleration of the compressed gas speed. The tapered surfaces of the blocks are preferably acute-angled to improve the linearity of particle movement, and a grooved thin plate 230 is fixed to a compressed gas block 240 to form a compressed gas flow path 250. While grooves may be machined in either block, machining grooves in the thin plate offers greater versatility, as the flow rate can be altered by changing the thickness of the thin plate and the shape of the compressed gas opening. The grooves in the thin plate 230 may have one or more widths 214 equal to the width of the second fluid opening 212, or may be wide-groove openings 215 covering multiple first fluid openings.
[0061] In Figure 3, one first thin plate 31, two second thin plates 32, and two third thin plates 33 are aligned and stacked to form a first flow path and an opening, and then plates, blocks, etc. (not shown) are stacked to form a second flow path and an opening around the first flow path. One or more elongated grooves 301 for the first fluid are formed in the first thin plate 31. Then, flow paths for the second fluid are processed in the first thin plate, second thin plate, and third thin plate according to the number of thin grooves for the first fluid, and thick plates or blocks (not shown) are stacked to form second fluid openings around the first fluid openings, separated by walls. The number of first and second openings can be selected from 1 to 1,500.
[0062] In Figure 4, one block 46 is formed with a flow path 416 for a liquid fluid (first fluid) connected to a first on-off valve (not shown), and a groove 420 that connects to the elongated thin plate flow path. A semicircular cross section of the groove 420 is preferable because it reduces resistance and allows for a smooth flow of slurry, etc. Also, a flow path 417 for a second fluid (compressed gas, etc.) and a groove 430 that connects to the second fluid are formed. The other block is formed with a flow path 417 for the compressed gas (second fluid) and a groove 430. The flow paths and grooves may be machined into a plate, such as a thick plate, instead of a block.
[0063] In FIG. 5 , the opening surface for the first fluid formed by the thin plates 51, 52, and 52' protrudes from the tip end surfaces of the blocks 55 and 56. A groove 501 for the first fluid flow path is formed in the thin plate 51, and the second thin plates 52 and 52' are stacked on both sides to form the opening for the first fluid. The nozzle assembly is formed by aligning the first, second, and third thin plates, each with grooves for the second fluid opening around the first fluid opening, with the blocks 55 and 56. A flow path 520 connecting to the first fluid groove 501 is formed in the block 56 and the thin plates 52 and 53 on one side. A flow path 530 connecting to the second fluid groove 502 is also formed in the block 56 on the other side. A similar flow path connecting to the second fluid groove is also formed in the block on the other side. In the figure, the tip surfaces of the third thin plates 52 and 52' are at the same level as the tip surfaces of the blocks 55 and 56, but they may be at the same level as the tip surfaces of the second thin plates or between them. Furthermore, a fourth thin plate with a channel processed therein may be laminated on both sides of two third thin plates, so that the openings for the first fluid and the openings for the second fluid are all protruded.
[0064] The present invention is suitable for methods of spraying or mixing multiple fluids and spreading them downstream. For example, it can be used to granulate multiple fluids while forming particles, encapsulate multiple fluids, or produce short fibers. While desired fluids can be combined and applied to a target object individually, it can also be used to extrude liquid fluids or heated melts through a die head or to apply powder to a target object by forming particles or fibers from the same or different liquid materials before and / or after the application of the liquid fluid or heated melt to a target object using a powder coating device. This allows for the production of granulated, encapsulated, or coated products in the food, pharmaceutical, and chemical industries, in addition to coating and adhesive applications. It is also suitable for the production of electrodes for fuel cells, water electrolysis, and CO2 electrolysis, secondary batteries including all-solid-state and semi-solid-state batteries, capacitor electrodes, electrolyte layers, and power-generating layers for solar cells. Furthermore, its increased productivity enables the production of new energy-related coating manufacturing processes with space-saving, energy-saving, low-cost, and high-quality results.
[0065] 1, 21, 31 First thin plate 2, 22, 32 Second thin plate 3, 23, 33 Third thin plate 5, 25, 45, 55 First block 6, 26, 46, 56 Second block 11, 211 First fluid opening 12, 212 Second fluid opening 13, 213 Wall 126, 216 First fluid opening / closing valve 127, 217 Second fluid opening / closing valve 101, 201 First flow path 103, 203 Second flow path 116, 416 First fluid supply flow path 117, 417 Second fluid supply flow path 120, 420 First fluid reservoir groove 130, 430 Second fluid reservoir groove 214 Second compressed gas opening 215 Second compressed gas opening 230 Second compressed gas thin plate 240 Second compressed gas block 270, 271 Part of second fluid opening 301 First fluid groove 302, 312, 380 Second fluid groove 311 First fluid groove opening 312, 370, 371 Second fluid groove opening
Claims
1. a step of forming an ejection opening for a second fluid, which is a compressed gas or a compressed gas mixed with solvent fine particles, or a supercritical fluid, on the side of a wall surrounding the opening for ejecting the liquid fluid; a step of connecting the opening and the elongated flow path for the first liquid fluid to a first opening / closing valve that opens and closes the supply of the first liquid fluid via an upstream flow path; a step of connecting the elongated flow path for the second fluid to a second opening / closing valve that opens and closes the supply of the second fluid via an upstream flow path; and a step of stretching the ejection flow from the opening for the first liquid fluid by opening the first and second opening / closing valves with an ejection flow from the entire periphery of the ejection port of the second fluid, and ejecting the first liquid fluid as fibers or particles, or applying the ejected fibers or particles to the object.
2. A method for spraying or applying a liquid fluid as described in claim 1, characterized in that the number of grooved thin plates is increased to make the number of fluids and openings three or more, the outermost openings are used as outlets for compressed gas or compressed gas containing solvent particles or supercritical fluid, the inside of which are openings for liquid fluid, and at least one of the openings for liquid fluid is used as an outlet for the solvent.
3. A method for spraying or applying a fluid as claimed in claim 1 or 2, characterized in that another compressed gas or a compressed gas containing solvent fine particles is collided with the jet of the jetted liquid fluid at an acute angle and from a close distance, thereby finely grinding the fibers or particles and spraying them out, or coating the fine fibers or particles on the target object.
4. A method for manufacturing a secondary battery or an all-solid-state battery, characterized in that the first fluid is selected from a slurry having a solid content of 25 to 75 weight percent, a slurry for a secondary battery electrode, a slurry for an all-solid-state battery electrode, or a slurry for an all-solid-state battery electrolyte, and the second fluid is selected from a compressed gas, a mixture of solvent fine particles and compressed gas, or a supercritical fluid, the two fluids are merged, the first fluid is stretched by the second fluid or the slurry is granulated by collision energy, and an object is selected from a current collector, an electrolyte layer, an electrode layer, or a separator, and the electrode layer, electrolyte layer, or functional membrane layer is formed by applying the slurry to the object.
5. A method for manufacturing a secondary battery or an all-solid-state battery according to claim 3 or 4, characterized in that after the at least two fluids are joined, a process is added in which a compressed gas or a compressed gas mixed with solvent fine particles is collided with the joined fluid at an acute angle, and the finely-particulated slurry is applied to an object selected from a heated current collector, an electrolyte layer, an electrode layer, and a separator to form an electrode layer, an electrolyte layer, or a functional membrane layer.
6. A method for producing a secondary battery or an all-solid-state battery according to claim 5, characterized in that the first fluid is selected from a slurry having a solid content of 50 to 85 weight percent, a slurry for a secondary battery electrode, a slurry for an all-solid-state battery electrode, or a slurry for an all-solid-state battery electrolyte, the second fluid is a solvent, and the third fluid is a compressed gas or a supercritical fluid, the three fluids are joined, the slurry is granulated by the stretching or collision energy of the compressed gas or the supercritical fluid, and the particles are collided with a compressed gas or a compressed gas mixed with fine solvent particles at an acute angle of 30 degrees or less with respect to the ejection direction of the first fluid to atomize the slurry, and the fine particles are heated by impact and applied to a target selected from a collector, an electrolyte layer, an electrode layer, or a separator to form an electrode layer, an electrolyte layer, or a functional film layer.
7. A method for manufacturing solar cells, comprising the steps of: manufacturing a nozzle assembly in which a nozzle assembly generating liquid particles and an object are moved relative to each other to coat the liquid for a power generation layer or gas barrier layer in the form of particles; and manufacturing a nozzle assembly in which a plurality of thin plates, plates or blocks with elongated grooves are stacked on both sides and 1 to 1,500 openings for a second fluid are arranged on the surfaces of the first fluid openings separated by walls around the openings for the first fluid; the first fluid being a transparent conductive layer, power generation layer or gas barrier layer liquid, and the second fluid being a compressed gas or a compressed gas or supercritical fluid mixed with a solvent fine particle; and the first fluid being stretched by the surrounding compressed gas or supercritical fluid to form fine particles, which are then coated on an object selected from a heated silicon solar cell layer, a transparent glass for a solar cell or a transparent plastic film to form a transparent conductive film layer, a power generation layer or a gas barrier layer.
8. The method for producing a perovskite solar cell according to claim 7, wherein the solar cell is a perovskite solar cell or a perovskite-on-silicon tandem solar cell.
9. A nozzle assembly for ejecting a liquid fluid, comprising: a first thin plate having one or more elongated grooves for a first fluid extending from the middle of the first thin plate to an end of one side of the thin plate; elongated grooves for a second fluid located on both sides of the first fluid groove and shorter in length from the end than the first fluid groove; at least two second thin plates are stacked in position from both sides of the first thin plate, and each second thin plate has an elongated groove connected to a second flow path of the first thin plate; and a third thin plate has a second fluid groove at least as wide as the two ends of the elongated grooves for the first fluid of the first thin plate, or a second fluid groove at least wider than the width between the centerlines of the elongated grooves for the second fluid located on both sides of the elongated groove for the first fluid of the first thin plate. a second thin plate is positioned on both outer sides of the first thin plate around the first thin plate, and a third thin plate is positioned on both outer sides of the second thin plate, the second and third thin plates are formed with flow paths connected to elongated flow paths for selected fluids, and plates or blocks having flow paths formed therein connected to one or more elongated grooves for the first fluid and the second fluid are superimposed to form one or more elongated flow paths and openings for the first fluid, an opening for the second fluid is provided separated by a wall surrounding the opening for the first fluid, the upstream of the opening for the first fluid is connected to an on-off valve for supplying the first fluid via the flow path, and the upstream of the opening for the second fluid is connected to an on-off valve for supplying the second fluid via the flow path.
10. A nozzle assembly as claimed in claim 9, characterized in that said third sheet is replaced by a plate or block having grooves for a second fluid aligned and overlapping said second sheet on both sides.
Citation Information
Patent Citations
Laminated nozzle with thick plate
JP2017535460A
High speed intermittent barrier nozzle
JP2018526214A
Nozzle, adhesive application head, adhesive application device, and diaper manufacturing method
JP2021154195A
Modular nozzle unit for web moistening
US20100224123A1
Cited By
nozzle
WO2026168118A1