Method for purifying crude ammonium fluoride product
The hydrogen fluoride impurity is removed in the preparation of ammonium fluoride through electrochemical exchange method, achieving high purity and high recovery rate of ammonium fluoride products, solving the problems of high energy consumption and low efficiency in traditional methods, and is suitable for industrial production.
Patent Information
- Application Number
- PCT/CN2024/090078
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-27
- Filing Date
- 2024-04-26
- Publication Date
- 2024-10-31
AI Technical Summary
There are hydrogen fluoride impurities that are difficult to remove in the existing ammonium fluoride preparation process, resulting in impure products, and traditional purification methods have high energy consumption and low efficiency.
An electrolytic cell is used for electrochemical exchange, and a cation exchange membrane is used to separate the cathode area and the anode area. The hydrogen fluoride in the crude ammonium fluoride solution is converted into sodium fluoride and potassium fluoride through electrolysis treatment, and then the water is removed in absolute ethanol. Dry and recrystallize to achieve high purity ammonium fluoride product.
It has achieved an ultra-high purity of over 99.6 wt% and a recovery rate of nearly 100% for ammonium fluoride products. Compared with traditional methods, it is simple, efficient and has low energy consumption, making it suitable for industrial production.
Smart Images

Figure PCTCN2024090078-APPB-I100001 
Figure PCTCN2024090078-APPB-I100002
Abstract
Description
Purification method of crude ammonium fluoride Technical Field
[0001] The invention belongs to the technical field of chemical industry, and in particular relates to a method for purifying crude ammonium fluoride. Background Art
[0002] Ammonium fluoride is a white crystal with the molecular formula NH4F. It is highly deliquescent and decomposes into ammonia and hydrogen fluoride when heated or exposed to hot water. It can corrode glass. Ammonium fluoride can be produced by neutralizing hydrofluoric acid and ammonia followed by concentrated crystallization.
[0003] In actual production and preparation, the properties of ammonium fluoride are extremely unstable, and relatively strict control of the reaction temperature and reaction materials is usually required. Usually, an excess of hydrogen fluoride and ammonia are reacted in a liquid phase or gas phase to prepare a mixture of ammonium fluoride and hydrogen fluoride. After that, a relatively high-purity ammonium fluoride product is prepared through multiple crystallization processes.
[0004] However, due to the actual existence of NH-F hydrogen bonds in ammonium fluoride, the hydrogen bonding effect causes a certain amount of unavoidable and almost difficult to remove hydrogen fluoride impurities to still exist in the purified product actually produced, which may exist in the form of ammonium bifluoride. Technical issues
[0005] In order to solve the problem that most existing ammonium fluoride preparation processes use excessive hydrofluoric acid to increase production and actual industrial benefits, resulting in the presence of difficult-to-remove hydrofluoric acid impurities in the ammonium fluoride product, the present invention provides a method for purifying crude ammonium fluoride.
[0006] The main objectives of the present invention are:
[0007] 1. It can efficiently and thoroughly remove the small amount of hydrogen fluoride remaining in the ammonium fluoride product;
[0008] 2. The removal effect is simple and efficient, and the energy consumption is relatively low. Technical Solutions
[0009] To achieve the above objectives, the present invention adopts the following technical solutions.
[0010] A method for purifying crude ammonium fluoride, comprising:
[0011] (1) An electrolytic cell is provided, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane, an inert cathode is provided in the cathode region, and an alkaline alkali metal compound aqueous solution and a copper electrode are provided in the anode region;
[0012] (2) placing the crude ammonium fluoride solution in the cathode region as the cathode electrolyte and applying power for electrolysis;
[0013] (3) The electrolysis process is continued until the potential reaches a threshold value, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0014] (4) The recovered cathode electrolyte is mixed with excess anhydrous ethanol and then calcium oxide is added to remove water and dry it. After filtering to remove the precipitate, it is crystallized under low temperature conditions to obtain the purified ammonium fluoride product.
[0015] The present invention uses a directional ion exchange method to fully convert the hydrogen fluoride in the crude ammonium fluoride solution. In the specific process, in the anode area, the selected alkaline alkali metal compound aqueous solution can generally be a sodium hydroxide aqueous solution and / or a potassium hydroxide aqueous solution. In actual industrial production, a saturated solution can be directly used or, based on the crude solution characterization results, an aqueous solution of sodium hydroxide and / or potassium hydroxide with a content of at least 1.3 times the hydrogen fluoride content in the crude solution can be prepared. During the electrolysis process, the copper electrode loses electrons and oxidizes into the alkaline alkali metal compound aqueous solution and forms a complex precipitate to prevent copper ions from entering the cathode area and causing loss of ammonium ions. During the electrolysis process, the hydrogen ions in the cathode area are reduced to hydrogen gas. To maintain the electrical neutrality of the electrolysis system, the cationic alkali metal ions in the anode area, namely sodium ions and / or potassium ions, are exchanged and enter the cathode area. After the electrolysis process is completed, the components of the recovered cathode electrolyte are converted into ammonium fluoride and sodium fluoride and / or potassium fluoride. Instead of the traditional method of removing hydrogen fluoride through multiple recrystallizations, the present invention uses solubility differences to directly separate sodium fluoride and potassium fluoride. In anhydrous ethanol, ammonium fluoride still maintains a certain solubility, but sodium fluoride and potassium fluoride are insoluble. Moreover, since the fluorine content in the solution increases after the dissolution of ammonium fluoride, it actually further limits the solubility of sodium fluoride and potassium fluoride. Therefore, after dehydration and drying, the present invention uses a special recrystallization method to directly, effectively and thoroughly remove excess fluoride impurities, thereby obtaining an ultra-high-purity ammonium fluoride product with a purity of more than 99.6 wt%. The recovery rate of ammonium fluoride is close to 100%, and no ammonium fluoride loss occurs.
[0016] As a preference,
[0017] In the step (1), the inert cathode is a carbon electrode.
[0018] The carbon electrode is inert in the system of the present invention and can avoid the introduction of impurities.
[0019] As a preference,
[0020] During the constant current electrolysis treatment in step (2), the starting voltage is controlled to be 1.23 V, and the potential voltage threshold in step (3) is 1.32 V.
[0021] During the constant current electrolysis process, as the solution systems in the anode and cathode regions change, the electrolysis potential will also change. In the actual production and preparation process, after rising to the above-mentioned voltage threshold, it can be basically determined that the hydrogen fluoride in the cathode electrolyte has been completely reacted.
[0022] As a preference,
[0023] When the cathode electrolyte recovered in step (4) is mixed with excess anhydrous ethanol, anhydrous ethanol in an amount of at least 48 times the volume of the cathode electrolyte is added to the cathode electrolyte.
[0024] A large amount of anhydrous ethanol is used to ensure that ammonium fluoride in the cathode electrolyte can be effectively recovered, so as to improve the recovery rate of the product.
[0025] As a preference,
[0026] The amount of calcium oxide used in step (4) is controlled so that its loose volume is at least 0.8 times the recovered cathode electrolyte.
[0027] The present invention uses excess calcium oxide to remove residual water in the cathode electrolyte because water and anhydrous ethanol are miscible and the presence of water will affect the impurity content in the final product.
[0028] As a preference,
[0029] The purified ammonium fluoride product obtained in step (4) is slowly dissolved in anhydrous ethanol until the purified ammonium fluoride product no longer dissolves, and solid matter is removed by solid-liquid separation. The anhydrous ethanol solution of ammonium fluoride is crystallized again to obtain an ultra-high-purity ammonium fluoride product.
[0030] The purified product is subjected to dropwise purification again to further remove a very small amount of residual impurities, thereby further improving the purity of the ammonium fluoride product. Beneficial effects
[0031] The beneficial effects of the present invention are:
[0032] (1) The present invention uses an electrochemical exchange method to directly and effectively remove impurities that are usually difficult to remove through crystallization or distillation processes, greatly improving the purity of the product;
[0033] (2) Compared with traditional purification methods, the present invention is simple, efficient and low in energy consumption, and is suitable for industrial production needs. Modes for Carrying Out the Invention
[0034] The present invention is further described in detail below with reference to specific embodiments. Those skilled in the art will be able to implement the present invention based on these descriptions. Furthermore, the embodiments of the present invention described below are generally only a portion of the embodiments of the present invention, rather than all of the embodiments. Therefore, all other embodiments derived by those skilled in the art based on the embodiments of the present invention without inventive effort should fall within the scope of protection of the present invention.
[0035] Unless otherwise specified, the raw materials used in the examples of the present invention are all commercially available or available to those skilled in the art; unless otherwise specified, the methods used in the examples of the present invention are all methods known to those skilled in the art.
[0036] Unless otherwise specified, the crude ammonium fluoride solution used in the embodiments of the present invention is prepared by dissolving currently industrially produced ammonium fluoride in water. The purity of the industrially produced ammonium fluoride is 93-95%, and the impurities are hydrogen fluoride and / or ammonium bifluoride.
[0037] Example 1: A method for purifying crude ammonium fluoride, comprising:
[0038] (1) An electrolytic cell is provided, which is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane). A carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region. The sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is approximately 2.0 Eq. A copper electrode is used as the anode electrode;
[0039] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0040] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0041] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0042] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0043] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0044] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.7%, and the recovery rate is accurate to one decimal place, and the calculated result is 100.0%.
[0045] Example 2: A method for purifying crude ammonium fluoride, comprising:
[0046] (1) An electrolytic cell is provided, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated potassium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region, wherein the potassium hydroxide equivalent in the saturated potassium hydroxide aqueous solution is approximately 2.1 Eq, and a copper electrode is used as the anode electrode;
[0047] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0048] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0049] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0050] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0051] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0052] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.6%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.
[0053] Example 3: A method for purifying crude ammonium fluoride, comprising:
[0054] (1) An electrolytic cell is provided, which is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane). A carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region. The sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is approximately 2.0 Eq. A copper electrode is used as the anode electrode;
[0055] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0056] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.35 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0057] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0058] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0059] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0060] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.6%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.
[0061] Example 4: A method for purifying crude ammonium fluoride, comprising:
[0062] (1) An electrolytic cell is provided, which is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane). A carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region. The sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is approximately 2.0 Eq. A copper electrode is used as the anode electrode;
[0063] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0064] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0065] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol, and then industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte was added to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 ° C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product;
[0066] (5) At least 50 kg of purified ammonium fluoride product is slowly dissolved in anhydrous ethanol. The rate of addition of anhydrous ethanol is controlled to be 15 mL of anhydrous ethanol per minute per gram of purified ammonium fluoride product. After the purified ammonium fluoride product no longer dissolves within 2 consecutive minutes, vacuum filtration is performed to separate and remove insoluble matter. The anhydrous ethanol solution of ammonium fluoride is placed at 20°C and evaporated under low pressure. The anhydrous ethanol is recovered and the crystalline product is recovered to obtain an ultra-high purity ammonium fluoride product.
[0067] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the ultra-high-purity ammonium fluoride product obtained in step (5) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.
[0068] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0069] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.9%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.
[0070] Example 5: A method for purifying crude ammonium fluoride, comprising:
[0071] (1) An electrolytic cell is provided, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated potassium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region, wherein the potassium hydroxide equivalent in the saturated potassium hydroxide aqueous solution is approximately 2.1 Eq, and a copper electrode is used as the anode electrode;
[0072] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0073] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0074] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol, and then industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte was added to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 ° C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product;
[0075] (5) At least 50 kg of purified ammonium fluoride product is slowly dissolved in anhydrous ethanol. The rate of addition of anhydrous ethanol is controlled to be 15 mL of anhydrous ethanol per minute per gram of purified ammonium fluoride product. After the purified ammonium fluoride product no longer dissolves within 2 consecutive minutes, vacuum filtration is performed to separate and remove insoluble matter. The anhydrous ethanol solution of ammonium fluoride is placed at 20°C and evaporated under low pressure. The anhydrous ethanol is recovered and the crystalline product is recovered to obtain an ultra-high purity ammonium fluoride product.
[0076] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the ultra-high-purity ammonium fluoride product obtained in step (5) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.
[0077] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0078] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.9%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.
[0079] Comparative Example 1: A method for purifying crude ammonium fluoride, comprising:
[0080] (1) An electrolytic cell is provided, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, a sodium hydroxide aqueous solution is provided in the anode region as the anode region electrolyte, and a copper electrode is used as the anode electrode;
[0081] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0082] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0083] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0084] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0085] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0086] The amount of sodium hydroxide in the sodium hydroxide aqueous solution in step (1) is expressed in equivalents (Eq), where 1 Eq is an aqueous solution prepared using sodium hydroxide having 1.0 times the hydrogen fluoride content of the crude product solution. The results of preparations with different equivalents are shown in the following table.
[0087]
[0088] In the table: Product recovery rate is the ammonium fluoride recovery rate.
[0089] The above characterization test results show that the equivalent amount of alkali metal hydroxide used in the anode electrolyte in the technical solution of the present invention has little practical effect on the recovery rate of ammonium fluoride, but has a significant impact on the purity. The use of a low equivalent amount of sodium hydroxide will limit the ion exchange process to a certain extent, resulting in a decrease in the removal of hydrogen fluoride. To ensure the production of ammonium fluoride product with a purity of 99.5%, a high industrial standard, at least 1.3 equivalents of sodium hydroxide or other alkali metal hydroxide should be used.
[0090] Comparative Example 2: A method for purifying crude ammonium fluoride, comprising:
[0091] (1) An electrolytic cell is provided, which is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane). A carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region. The sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is approximately 2.0 Eq. A copper electrode is used as the anode electrode;
[0092] (2) Place the crude ammonium fluoride solution in the cathode area as the cathode electrolyte, apply power for electrolysis, and control the starting voltage to 1.23 V;
[0093] (3) The electrolysis process was continued until the potential reached the threshold values of 1.30 V and 1.35 V, and two sets of experimental verifications were performed. The electrolysis process was terminated and the cathode electrolyte was recovered.
[0094] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0095] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0096] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0097] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.7%, and the recovery rate is accurate to one decimal place, and the calculated result is 100.0%.
[0098] Verification results showed that when the control threshold was 1.30 V, the purity of the resulting ammonium fluoride product was 99.3% and the recovery rate was 100.0%. When the control threshold was 1.35 V, the purity of the resulting ammonium fluoride product was 99.5% and the recovery rate was 100.0%. This indicates that lowering the threshold potential used to determine the electrolysis process resulted in a significant decrease in the purity of the ammonium fluoride product. Product characterization also revealed that this was due to incomplete removal of hydrogen fluoride. Increasing the threshold significantly increased energy consumption, but the actual product purity and recovery rate did not significantly improve. Compared to the 1.32 V threshold, the 1.35 V threshold increased electrolysis process energy consumption by approximately 12%. Therefore, to control costs, a 0.01 V gradient experiment was conducted, and the optimal threshold control range should be 1.32-1.34 V.
[0099] Comparative Example 3: Take the crude ammonium fluoride liquid, carry out 5 recrystallization processes with the existing conventional process, and characterize the purity and calculate the recovery rate of the product. The specific calculation formula of the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%, wherein the actual recovery amount is the actual recovery amount obtained by product characterization, and the theoretical maximum recovery amount is characterized and calculated according to the content of ammonium fluoride in the crude ammonium fluoride liquid. The characterization settlement results show that the product purity is 97.8% and the recovery rate is 96.3%. In addition, compared with the process of Example 1 of the present invention, the actual industrial production cycle of multiple recrystallization processes is extended by about 3 hours, and the energy consumption is increased by about 6%.
[0100] It can be seen that compared with the existing recrystallization process, the process of the present invention has been comprehensively improved in many aspects such as improving production efficiency, reducing energy consumption, and improving product quality and recovery rate.
[0101] Comparative Example 4: A method for purifying crude ammonium fluoride, comprising:
[0102] (1) An electrolytic cell is provided, which is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane). A carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the electrolyte of the anode region. The sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is approximately 2.0 Eq. A copper electrode is used as the anode electrode;
[0103] (2) Dissolve industrial ammonium fluoride crystals of different purities in water to prepare a crude solution, place it in the cathode area as the cathode electrolyte, and conduct electrolysis by applying power, controlling the starting voltage to 1.23 V;
[0104] (3) The electrolysis process is continued until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode electrolyte is recovered;
[0105] (4) The recovered cathode electrolyte was mixed with 48 times the volume of anhydrous ethanol and then added with industrial quicklime with a loose volume of 0.8 times that of the cathode electrolyte to remove water and dry. After filtering to remove the precipitate, the mixture was evaporated at low pressure at 20 °C and the anhydrous ethanol was recovered. The crystallized product was then recovered to obtain the purified ammonium fluoride product.
[0106] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery and the actual recovery.
[0107] The specific calculation formula for recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;
[0108] The corresponding preparation effects of industrial crystals of ammonium fluoride with different purities are shown in the following table.
[0109]
[0110] In the table: crystal purity refers to the purity of ammonium fluoride in the industrial crystal product of ammonium fluoride; product recovery rate refers to the recovery rate of ammonium fluoride.
[0111] Characterization of the industrial ammonium fluoride crystals used revealed that products with crystalline purities of 87.2% and 89.3% contained impurities primarily composed of hydrogen fluoride and / or ammonium bifluoride, but also contained other copper ion compound impurities, which the process of the present invention was unable to effectively and thoroughly remove. Therefore, the applicability of the purification method of the present invention is applicable to crude products whose primary impurities are hydrogen fluoride and / or ammonium bifluoride.
Claims
1. A method for purifying crude ammonium fluoride, characterized in that: The method comprises: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane, an inert cathode is provided in the cathode region, and an alkaline alkali metal compound aqueous solution and a copper electrode are provided in the anode region; (2) placing the crude ammonium fluoride solution in the cathode region as the cathode region electrolyte and applying power for electrolysis; (3) The electrolysis process is continued until the potential reaches a threshold value, the electrolysis process is terminated, and the cathode electrolyte is recovered; (4) The recovered cathode electrolyte is mixed with excess anhydrous ethanol, and then calcium oxide is added to remove water and dry. After filtering to remove the precipitate, the precipitate is crystallized under low temperature conditions to obtain the purified ammonium fluoride product.
2. A method for purifying crude ammonium fluoride according to claim 1, characterized in that: In the step (1), the inert cathode is a carbon electrode.
3. A method for purifying crude ammonium fluoride according to claim 1, characterized in that: During the constant current electrolysis treatment in step (2), the starting voltage is controlled to be 1.23 V, and the potential voltage threshold in step (3) is 1.32 V.
4. A method for purifying crude ammonium fluoride according to claim 1, characterized in that: When the cathode electrolyte recovered in step (4) is mixed with excess anhydrous ethanol, at least 48 times the volume of anhydrous ethanol is added to the anode electrolyte.
5. A method for purifying crude ammonium fluoride according to claim 1 or 5, characterized in that: The amount of calcium oxide used in step (4) is controlled so that its loose volume is at least 0.8 times the recovered anode electrolyte.
6. A method for purifying crude ammonium fluoride according to claim 1, characterized in that: The purified ammonium fluoride product obtained in step (4) is slowly dissolved in anhydrous ethanol until the purified ammonium fluoride product no longer dissolves, and then the solid matter is removed by solid-liquid separation. The anhydrous ethanol solution of ammonium fluoride is crystallized again to obtain an ultra-high purity ammonium fluoride product.
Citation Information
Patent Citations
Preparation method of etching and cleaning grade ammonium fluoride
CN110615447A
Production management control system for ammonium fluoride production and control method thereof
CN115453990A
Method for purifying ammonium fluoride crude product
CN117165960A
Preparation method of electronic-grade ammonium fluoride
CN117165961A
Process for the treatment and purification of dangerous wastes containing ammonium salts, particularly ammonium chloride, derived from pharmaceutical and chemical technologies
US20110044879A1